Special polypropylene material and preparation method thereof
By adding a formula of specific antioxidants, rigidity enhancers and friction coefficient reducers to polypropylene powder, combined with twin-screw extruder granulation, the problems of high processing costs and insufficient dynamic friction performance of polypropylene special materials are solved , prepared a special polypropylene material that meets the needs of the two-piece piston assembly, achieving high performance and low cost production results.
Patent Information
- Application Number
- CN202410878078.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-02
- Publication Date
- 2024-10-18
AI Technical Summary
It is difficult to prepare special polypropylene materials that meet the needs of two-piece piston components with the existing technology. There are problems such as high processing costs, complex processes, insufficient dynamic friction performance, and difficulty in recycling.
Use a high-speed mixer to stir at low speed and then add the main antioxidant, auxiliary antioxidant, rigidity enhancer and lubricant in order, then add the friction coefficient reducer, granulate with a twin-screw extruder, and process with a vacuum system. A special material for polypropylene was prepared, with a component mass percentage of 99% of polypropylene powder. .27%-99.76%, main antioxidant 0.05%-0.15%, auxiliary antioxidant 0.05%-0.15%, rigidity enhancer 0.08%-0.20%, lubricant 0.03%-0.08%, friction coefficient reducer 0.03% -0.15%.
It achieves the dual properties of low friction coefficient and high bending modulus of polypropylene special materials to meet the application requirements of two-piece disposable syringe piston components. The process is simple and the cost is low. The performance indicators meet the melt index, haze, density, Requirements for tensile yield stress, flexural modulus and dynamic coefficient of friction.
Smart Images

Figure BDA0004923703820000061
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of polyolefin materials, and in particular relates to a special polypropylene material for a disposable syringe piston assembly of the same material and a preparation method thereof. Background Art
[0002] Medical grade polypropylene has excellent transparency, gloss, balance of rigidity and toughness, good biocompatibility, multiple sterilization options, easy handling and environmental friendliness, and is widely used in disposable syringes.
[0003] The three-piece piston assembly is a combination accessory, which uses a variety of raw materials, has a complex manufacturing process, a high probability of secondary contamination during assembly, is restricted in use, and is relatively difficult to recycle. The two-piece piston assembly can effectively solve the above problems of the three-piece piston assembly. Due to the limitation of the special materials of the two-piece piston assembly, more than 85% of the disposable syringes in China are three-piece piston assemblies, and the two-piece piston assembly has a broad market application prospect.
[0004] Chinese patent CN107698826A discloses a piston material for a disposable syringe and a preparation method thereof. Since polyisoprene rubber is used as the matrix, the application scope is only applicable to the piston part of the piston assembly, and it cannot meet the use requirements in the application of the core rod part of a two-piece syringe. Chinese patent CN101584892A discloses an energy-saving and environmentally friendly syringe and its piston material, and provides a preparation method. The modified polyvinyl chloride provided by it for the manufacture of the piston part has the disadvantages of difficult processing, insufficient application strength and difficulty in recycling, and cannot be used for the manufacture of the core rod of the piston assembly of a two-piece syringe. Chinese patent CN101584893A discloses an energy-saving and environmentally friendly syringe and a material for its core rod and a preparation method thereof. The polypropylene material provided by it for the manufacture of the core rod assembly is easy to produce jams during the use of the disposable syringe due to the large lateral pressure resistance, making the drug intake unstable, and difficult to use in the two-piece piston assembly.
[0005] For special polypropylene materials, the problem of high processing costs and complex processes caused by too many additives needs to be solved. In terms of dynamic friction performance, under the same ring pressure force, in order to ensure the smoothness of the product injection process, the special polypropylene material needs to have a lower dynamic friction coefficient when used in the piston part, and a large number of tests are required to find the best additives and ratios. In terms of rigidity, in order to ensure that the special polypropylene material has high rigidity when used in the core rod part to provide stability in use, a large number of tests are required to find the best additives and ratios. Special materials need to ensure the dynamic friction performance of the core rod to ensure stable advancement. Summary of the invention
[0006] 1. Technical issues to be resolved
[0007] The invention provides a special polypropylene material and a preparation method thereof, so as to solve the technical problem of how to prepare the special polypropylene material which can be used for a two-piece piston assembly.
[0008] (II) Technical solution
[0009] In order to solve the above technical problems, the present invention provides a method for preparing a special polypropylene material, which comprises the following steps:
[0010] S1. Add the polypropylene powder raw material into a high-speed mixer and stir at a low speed;
[0011] S2. Add the primary antioxidant, the auxiliary antioxidant, and the rigidity enhancer in a high-speed mixer in order and stir at a low speed; add the lubricant and the friction coefficient reducer in a high-speed mixer in order and stir at a low speed to mix well to obtain a premix;
[0012] S3. The premix is fed into a twin-screw extruder for extrusion granulation, and a vacuum system is used to absorb excess odor and impurities to prepare a special polypropylene material.
[0013] Furthermore, the primary antioxidant is one or more of a phenolic antioxidant and a hindered amine stabilizer.
[0014] Furthermore, the auxiliary antioxidant is one or two of phosphites, phosphites or sulfur-containing synergists.
[0015] Furthermore, the lubricant is one or more of calcium stearate, pentaerythritol monostearate, glycerol monooleate, saponified montan ester wax and ethylene bisstearamide and their derivatives.
[0016] Furthermore, the friction coefficient reducer is one or a combination of an organic slip agent or an inorganic anti-sticking agent.
[0017] Furthermore, the rigidity enhancer is one or both of an aromatic carboxylate salt-based α-crystalline polypropylene nucleating agent and a substituted aromatic phosphate salt-based nucleating agent.
[0018] Furthermore, in step S3, the vacuum degree is -0.02 to 0.1 MPa.
[0019] Furthermore, in step S3, the temperature of the twin-screw extruder is 180-210°C.
[0020] Furthermore, in step S3, the main engine speed of the twin-screw extruder is 25-28 Hz.
[0021] In addition, the present invention also proposes a special material for polypropylene, which is prepared by the above method. The mass percentages of the components of the special material for polypropylene are as follows: 99.27% to 99.76% of polypropylene powder, 0.05% to 0.15% of a primary antioxidant, 0.05% to 0.15% of an auxiliary antioxidant, 0.08% to 0.20% of a rigidity enhancer, 0.03% to 0.08% of a lubricant, and 0.03% to 0.15% of a friction coefficient reducer.
[0022] (III) Beneficial effects
[0023] The present invention proposes a special polypropylene material and a preparation method thereof, comprising adding a polypropylene powder raw material to a high-speed mixer and stirring at a low speed; adding a main antioxidant, an auxiliary antioxidant, and a rigidity enhancer in the high-speed mixer in sequence and stirring at a low speed; adding a lubricant and a friction coefficient reducer in the high-speed mixer in sequence, stirring at a low speed, and mixing evenly to obtain a premix; putting the premix into a twin-screw extruder for extrusion granulation, and using a vacuum system to absorb excess odor and impurities to prepare a special polypropylene material. The present invention adopts the addition of a friction coefficient reducer and a rigidity enhancer to match the raw material basic additive formula, with a better ratio, and at the same time realizes that the special material has the dual properties of a low friction coefficient and a high bending modulus, and can produce a special polypropylene material that meets the application requirements of a two-piece disposable syringe piston assembly. The preparation process of the method is simple and easy to operate, and a small amount of additives can effectively reduce costs. The performance indicators of the product manufactured using the special polypropylene material of the present invention meet the following requirements: melt index 25.0±2.0g / 10min, haze ≤15%, density ≤0.91g / cm 3 , tensile yield stress ≥ 24Mpa, flexural modulus ≥ 1100Mpa, cantilever beam notched impact strength (23℃) ≥ 3.0KJ / m 3 , dynamic friction coefficient ≤0.35. DETAILED DESCRIPTION
[0024] In order to make the purpose, content and advantages of the present invention more clear, the specific implementation methods of the present invention are further described in detail below in conjunction with embodiments.
[0025] Example 1
[0026] A two-piece disposable syringe with the same material piston assembly polypropylene special material is weighed according to the following weight percentages of the components:
[0027] Polypropylene powder 99.85%, primary antioxidant 0.05%, auxiliary antioxidant 0.05%
[0028] Lubricant 0.05%, Friction reducer 0.00%, Rigidity enhancer 0.00%
[0029] Add the polypropylene powder raw material to the high-speed mixer, stir at low speed for 1 to 3 minutes, add the main antioxidant, auxiliary antioxidant, rigidity enhancer in order, stir at low speed for 1 to 3 minutes, add lubricant and friction coefficient reducer, ensure that the friction coefficient reducer is added last, stir at low speed for 2 minutes, and obtain a uniformly mixed premix. Put the premix into the 48-type extruder for extrusion and granulation, and use the vacuum system to absorb excess odor and impurities. The vacuum degree is controlled at -0.02 to 0.1MPa. The temperature of the twin-screw extruder is between 150 and 210°C. The main engine speed is controlled at 20 to 30Hz.
[0030] Example 2
[0031] Polypropylene powder 99.74%, primary antioxidant 0.05%, auxiliary antioxidant 0.05%
[0032] Lubricant 0.05%, Friction reducer 0.03%, Rigidity enhancer 0.08%
[0033] Add the polypropylene powder raw material to the high-speed mixer, stir at low speed for 1 to 3 minutes, add the main antioxidant, auxiliary antioxidant, rigidity enhancer in order, stir at low speed for 1 to 3 minutes, add lubricant and friction coefficient reducer, ensure that the friction coefficient reducer is added last, stir at low speed for 2 minutes, and obtain a uniformly mixed premix. Put the premix into the 48-type extruder for extrusion and granulation, and use the vacuum system to absorb excess odor and impurities. The vacuum degree is controlled at -0.02 to 0.1MPa. The temperature of the twin-screw extruder is between 150 and 210°C. The main engine speed is controlled at 20 to 30Hz.
[0034] Example 3
[0035] Polypropylene powder 99.67%, primary antioxidant 0.05%, auxiliary antioxidant 0.05%
[0036] Lubricant 0.05%, Friction reducer 0.06%, Rigidity enhancer 0.11%
[0037] Add the polypropylene powder raw material to the high-speed mixer, stir at low speed for 1 to 3 minutes, add the main antioxidant, auxiliary antioxidant, rigidity enhancer in order, stir at low speed for 1 to 3 minutes, add lubricant and friction coefficient reducer, ensure that the friction coefficient reducer is added last, stir at low speed for 2 minutes, and obtain a uniformly mixed premix. Put the premix into the 48-type extruder for extrusion and granulation, and use the vacuum system to absorb excess odor and impurities. The vacuum degree is controlled at -0.02 to 0.1MPa. The temperature of the twin-screw extruder is between 150 and 210°C. The main engine speed is controlled at 20 to 30Hz.
[0038] Example 4
[0039] Polypropylene powder 99.62%, primary antioxidant 0.05%, auxiliary antioxidant 0.05%
[0040] Lubricant 0.05%, Friction reducer 0.09%, Rigidity enhancer 0.14%
[0041] Add the polypropylene powder raw material to the high-speed mixer, stir at low speed for 1 to 3 minutes, add the main antioxidant, auxiliary antioxidant, rigidity enhancer in order, stir at low speed for 1 to 3 minutes, add lubricant and friction coefficient reducer, ensure that the friction coefficient reducer is added last, stir at low speed for 2 minutes, and obtain a uniformly mixed premix. Put the premix into the 48-type extruder for extrusion and granulation, and use the vacuum system to absorb excess odor and impurities. The vacuum degree is controlled at -0.02 to 0.1MPa. The temperature of the twin-screw extruder is between 150 and 210°C. The main engine speed is controlled at 20 to 30Hz.
[0042] Example 5
[0043] Polypropylene powder 99.57%, primary antioxidant 0.05%, auxiliary antioxidant 0.05%
[0044] Lubricant 0.05%, Friction reducer 0.12%, Rigidity enhancer 0.16%
[0045] Add the polypropylene powder raw material to the high-speed mixer, stir at low speed for 1 to 3 minutes, add the main antioxidant, auxiliary antioxidant, rigidity enhancer in order, stir at low speed for 1 to 3 minutes, add lubricant and friction coefficient reducer, ensure that the friction coefficient reducer is added last, stir at low speed for 2 minutes, and obtain a uniformly mixed premix. Put the premix into the 48-type extruder for extrusion and granulation, and use the vacuum system to absorb excess odor and impurities. The vacuum degree is controlled at -0.02 to 0.1MPa. The temperature of the twin-screw extruder is between 150 and 210°C. The main engine speed is controlled at 20 to -30Hz.
[0046] Example 6
[0047] Polypropylene powder 99.50%, primary antioxidant 0.05%, auxiliary antioxidant 0.05%
[0048] Lubricant 0.05%, Friction reducer 0.15%, Rigidity enhancer 0.20%
[0049] Add the polypropylene powder raw material to the high-speed mixer, stir at low speed for 1 to 3 minutes, add the main antioxidant, auxiliary antioxidant, rigidity enhancer in order, stir at low speed for 1 to 3 minutes, add lubricant and friction coefficient reducer, ensure that the friction coefficient reducer is added last, stir at low speed for 2 minutes, and obtain a uniformly mixed premix. Put the premix into the 48-type extruder for extrusion and granulation, and use the vacuum system to absorb excess odor and impurities. The vacuum degree is controlled at -0.02 to 0.1MPa. The temperature of the twin-screw extruder is between 150 and 210°C. The main engine speed is controlled at 20 to 30Hz.
[0050] Through experimental comparison, the performance index of the optimized product was tested, and the results are shown in the following table.
[0051]
[0052] It can be seen from the above table that the impact of all implementation cases on the conventional performance of raw materials is within the standard requirements, that is, the implementation cases have at least no unacceptable negative impact on the conventional performance of raw materials. In the investigation of the impact of formula changes on the key indicator dynamic friction coefficient, in the absence of film material coefficient reducer addition, the dynamic friction coefficient of the raw material is 1.19, which cannot meet the use requirements. When the friction coefficient reducer is added at a concentration of 0.09% (mass), the dynamic friction coefficient of the special material reaches 0.32, which is lower than the maximum dynamic friction coefficient of 0.35 required for use. In the investigation of the impact of formula changes on the key indicator bending modulus, in the absence of rigidity enhancer addition, the bending modulus of the raw material is 810Mpa, which cannot meet the use requirements. When the friction coefficient reducer is added at a concentration of 0.12% (mass), the bending modulus of the special material reaches 1100Mpa, which is higher than the minimum bending modulus of 1000Mpa required for use.
[0053] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the technical principles of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.
Claims
1. A method for preparing a special polypropylene material, characterized in that: The preparation method comprises the following steps: S1. Add the polypropylene powder raw material into a high-speed mixer and stir at a low speed; S2. Add the primary antioxidant, the auxiliary antioxidant, and the rigidity enhancer in a high-speed mixer in order and stir at a low speed; add the lubricant and the friction coefficient reducer in a high-speed mixer in order and stir at a low speed to mix well to obtain a premix; S3. The premix is fed into a twin-screw extruder for extrusion granulation, and a vacuum system is used to absorb excess odor and impurities to prepare a special polypropylene material.
2. The method for preparing a special polypropylene material according to claim 1, characterized in that: The main antioxidant is one or more of a phenolic antioxidant and a hindered amine stabilizer.
3. The method for preparing a special polypropylene material according to claim 1, characterized in that: The auxiliary antioxidant is one or two of phosphite, phosphite or sulfur-containing synergist.
4. The method for preparing a special polypropylene material according to claim 1, characterized in that: The lubricant is one or more of calcium stearate, pentaerythritol monostearate, glycerol monooleate, saponified montan ester wax and ethylene bisstearamide and their derivatives.
5. The method for preparing a special polypropylene material according to claim 1, characterized in that: The friction coefficient reducer is one of an organic slip agent and an inorganic anti-sticking agent or a combination of the two.
6. The method for preparing a special polypropylene material according to claim 1, characterized in that: The rigidity enhancer is one or both of an aromatic carboxylate salt type α-crystalline polypropylene nucleating agent and a substituted aromatic phosphate salt type nucleating agent.
7. The method for preparing a special polypropylene material according to claim 1, characterized in that: In step S3, the vacuum degree is -0.02 to 0.1 MPa.
8. The method for preparing a special polypropylene material according to claim 1, characterized in that: In step S3, the temperature of the twin-screw extruder is 180-210°C.
9. The method for preparing a special polypropylene material according to claim 1, characterized in that: In step S3, the main engine speed of the twin-screw extruder is 25 to 28 Hz.
10. A special material for polypropylene, characterized in that: The special polypropylene material is prepared by the method according to any one of claims 1 to 9, and the mass percentages of the components of the special polypropylene material are as follows: 99.27% to 99.76% polypropylene powder, 0.05% to 0.15% primary antioxidant, 0.05% to 0.15% auxiliary antioxidant, 0.08% to 0.20% rigidity enhancer, 0.03% to 0.08% lubricant, and 0.03% to 0.15% friction coefficient reducer.