Method and system for detecting void ratio of reinforced concrete column based on piezoelectric ceramic technology
By using piezoelectric ceramic sensors and wavelet packet analysis technology in Jingang concrete columns, the damage factor is calculated and three-dimensional imaging is performed, and the problem of detecting Jingang concrete columns in the existing technology is solved, achieving lossless, fast and accurate detection. Effect.
Patent Information
- Application Number
- CN202411284091.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-13
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2044-09-13
AI Technical Summary
The prior art is difficult to effectively detect peeling defects between concrete and steel ribs in steel columns and damage to large-size concrete structures, especially during construction, non-destructive testing cannot be carried out easily, and common methods are harmful to components.
Using a detection method based on piezoelectric ceramic technology, by burying piezoelectric ceramic sensors inside the components to be tested and imitated, using wavelet packet analysis and MATLAB for data processing, calculate the damage factor and perform three-dimensional imaging, and determine whether there is air on the detection path. gap or damage.
It realizes non-destructive, fast and convenient inspection of the steel concrete column, simple and efficient, and accurate detection results, avoiding damage to the components.
Smart Images

Figure CN118795026B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of hollowing rate detection of reinforced concrete columns, and in particular to a method and system for detecting hollowing rate of reinforced concrete columns based on piezoelectric ceramic technology. Background Art
[0002] With the acceleration of urbanization and the improvement of social and economic levels, in order to meet people's demand for the use of building space, the height of buildings is constantly rising. Reinforced concrete is widely used in the load-bearing part of super-high-rise buildings due to its high rigidity and strong deformation resistance. However, due to inadequate construction quality control and concrete material shrinkage, the interior, especially the blind area concrete under the steel ribs, may have peeling defects between concrete and steel ribs and webs, thereby reducing its mechanical properties. At present, the commonly used concrete damage detection methods are mainly core sampling and ultrasonic methods. Core sampling is detrimental to the component itself; the ultrasonic method is not suitable for the judgment of separation defects caused by poor bonding between concrete and steel ribs and holes under the stiffening ribs. At the same time, when detecting large-sized concrete structures, it may be necessary to change the orientation and detect multiple times to ensure that the signal emitted during the detection can pass through the damaged location, which increases the workload on site. To address this problem, it is necessary to design an effective detection method to facilitate the convenient and effective non-destructive detection of the poured reinforced concrete columns during the construction process. Summary of the invention
[0003] In view of the shortcomings of the prior art, the purpose of the present invention is to provide a method and system for detecting the void rate of reinforced concrete columns based on piezoelectric ceramic technology. The method and system can perform convenient and effective nondestructive testing on the cast reinforced concrete columns quickly and nondestructively.
[0004] In order to achieve the above object, the present invention provides the following technical solutions:
[0005] The method for detecting the void ratio of a reinforced concrete column based on piezoelectric ceramic technology comprises: S1, manufacturing a component to be tested, and burying a piezoelectric ceramic sensor inside the component to be tested; S2, using the piezoelectric ceramic sensor to obtain the voltage signal energy value of the component to be tested; S3, manufacturing a replica component with the same material, structure and size as the component to be tested, and burying a piezoelectric ceramic sensor inside the replica component; S4, using the piezoelectric ceramic sensor to obtain the voltage signal energy value of the replica component in a healthy state by means of a frequency sweep; S5, calculating the damage factor of the component to be tested according to the voltage signal energy value of the component to be tested and the voltage signal energy value of the replica component in a healthy state; S6, according to the damage factor, using a MATLAB data imaging method to perform three-dimensional imaging on the detection path of the component to be tested, comparing the damage factor with the damage factor threshold, if the damage factor is less than or equal to the damage factor threshold, it is determined that there is no air gap and damage on the detection path of the component to be tested, and if the damage factor is greater than the damage factor threshold, it is determined that there is an air gap or damage on the detection path of the component to be tested; the voltage signal energy value is calculated as follows:
[0006] The acquisition module collects the original signal S, and uses the wavelet packet analysis principle to decompose S into multiple component signals with equal width bands. The original signal is obtained by calling the wavelet packet tool script function in MATLAB to perform N-layer wavelet packet decomposition and reconstruction on the original signal. The corresponding wavelet packet energy.
[0007] (1) Wavelet packet decomposition
[0008] ;
[0009] Where T is the wavelet packet tree; is the original voltage signal collected in the i-th sampling period; N is the number of decomposition layers; Is the wavelet function type.
[0010] (2) Wavelet packet energy
[0011] ;
[0012] in, is the voltage signal energy value in the i-th sampling period, T is the wavelet packet tree after wavelet packet decomposition;
[0013] The calculation formula of the damage factor is:
[0014] ;
[0015] Among them, DI is the damage factor; is the voltage signal energy value of the detected path of the measured component within the sampling time i; is the voltage signal energy value of the simulated component in the healthy state within the sampling period i; , They respectively represent the average voltage signals of the tested component and the simulated component in a healthy state.
[0016] In the present invention, preferably, the damage factor threshold is 0.7.
[0017] In the present invention, preferably, the damage factor threshold is variable, and the steps of determining the damage factor threshold include: S1', setting a triggerable artificial damage on the imitation component; S2', triggering the artificial damage, using the piezoelectric ceramic sensor to obtain the voltage signal energy value of the imitation component in the damaged state; S3', calculating the damage factor threshold according to the voltage signal energy values of the imitation component in the healthy state and the damaged state, the formula is:
[0018] ;
[0019] in, is the damage factor threshold, is the voltage signal energy value of the simulated component in the damaged state within sampling period i; is the voltage signal energy value of the simulated component in the healthy state within the sampling period i, The average value of the voltage signal energy value of the simulated component under the damaged state, It represents the average value of the voltage signal energy value of the simulated component in a healthy state.
[0020] In the present invention, preferably, the piezoelectric ceramic sensor is buried inside the measured component and the piezoelectric ceramic sensor is buried inside the dummy component, and the piezoelectric ceramic sensor is buried in the concrete pouring blind area of the measured component and the dummy component.
[0021] The hollowing rate detection system of reinforced concrete columns based on piezoelectric ceramic technology includes: a first transmitting end piezoelectric ceramic sensor, which is buried inside the measured component and is used to transmit vibration signals; a first receiving end piezoelectric ceramic sensor, which is distributed around the outer wall of the measured component and is used to receive vibration signals; a first acquisition module, which is electrically connected to the first receiving end piezoelectric ceramic sensor and is used to obtain the voltage signal energy value of the measured component; a replica component, which has the same material, structure and size as the measured component and is used to imitate the internal and external environment of the measured component; a second transmitting end piezoelectric ceramic sensor, which is buried inside the replica component and is used to transmit vibration signals; a second receiving end piezoelectric ceramic sensor, which is distributed around the outer wall of the replica component and is used to receive vibration signals; a second acquisition module, which is electrically connected to the second receiving end piezoelectric ceramic sensor and is used to obtain the health status by scanning frequency. a damage factor calculation module, which is electrically connected to the first acquisition module and the second acquisition module respectively, and is used to calculate the damage factor of the measured component according to the voltage signal energy value of the measured component and the voltage signal energy value of the simulated component in the healthy state; an imaging and judgment module, which is electrically connected to the damage factor calculation module, and is used to perform three-dimensional imaging of the detection path of the measured component according to the damage factor, using the MATLAB data imaging method, and compare the damage factor with the damage factor threshold. If the damage factor is less than or equal to the damage factor threshold, it is determined that there is no air gap and damage on the detection path of the measured component. If the damage factor is greater than the damage factor threshold, it is determined that there is an air gap or damage on the detection path of the measured component; the calculation method of the voltage signal energy value is as follows:
[0022] The acquisition module collects the original signal S, and uses the wavelet packet analysis principle to decompose S into multiple component signals with equal width bands. The original signal is obtained by calling the wavelet packet tool script function in MATLAB to perform N-layer wavelet packet decomposition and reconstruction on the original signal. The corresponding wavelet packet energy.
[0023] (1) Wavelet packet decomposition
[0024] ;
[0025] Where T is the wavelet packet tree; is the original voltage signal collected in the i-th sampling period; N is the number of decomposition layers; Is the wavelet function type.
[0026] (2) Wavelet packet energy
[0027] ;
[0028] in, is the voltage signal energy value in the i-th sampling period, T is the wavelet packet tree after wavelet packet decomposition;
[0029] The calculation formula of the damage factor is:
[0030] ;
[0031] Among them, DI is the damage factor; is the voltage signal energy value of the detected path of the measured component within the sampling time i; is the voltage signal energy value of the simulated component in the healthy state within the sampling period i; , They respectively represent the average voltage signals of the tested component and the simulated component in a healthy state.
[0032] In the present invention, preferably, the damage factor threshold is 0.7.
[0033] In the present invention, preferably, the damage factor threshold is variable, and the piezoelectric ceramic technology-based steel concrete column void rate detection system further includes a threshold determination module, which is electrically connected to the second acquisition module and is used to calculate the damage factor threshold according to the voltage signal energy value of the simulated component in a healthy state and a damaged state, and the formula is:
[0034] ;
[0035] in, is the damage factor threshold, is the voltage signal energy value of the simulated component in the damaged state within sampling period i; is the voltage signal energy value of the simulated component in the healthy state within the sampling period i, The average value of the voltage signal energy value of the simulated component under the damaged state, It represents the average value of the voltage signal energy value of the simulated component in a healthy state.
[0036] In the present invention, preferably, the first transmitting end piezoelectric ceramic sensor is buried in a concrete casting blind area of the measured component, and the second transmitting end piezoelectric ceramic sensor is buried in a concrete casting blind area of the simulated component.
[0037] Compared with the prior art, the present invention has the following beneficial effects:
[0038] The method and system for detecting the void rate of a reinforced concrete column based on piezoelectric ceramic technology of the present invention arrange piezoelectric ceramic sensors inside and outside the reinforced concrete component to be tested, collect the voltage signal energy values of different detection paths, calculate the damage factors of different paths, and judge whether there are damages or air gaps on each detection path of the component to be tested based on the relationship between the damage factor and the damage factor threshold, thereby realizing non-destructive detection of the void rate of the reinforced concrete column. The detection process is simple and efficient, and the detection results are accurate. BRIEF DESCRIPTION OF THE DRAWINGS
[0039] Figure 1 The present invention is a flowchart of a method for detecting the void ratio of reinforced concrete columns based on piezoelectric ceramic technology according to an embodiment of the present invention.
[0040] Figure 2 The present invention is a flowchart of determining a damage factor threshold in a method for detecting a void ratio of a reinforced concrete column based on piezoelectric ceramic technology according to an embodiment of the present invention.
[0041] Figure 3 It is a structural schematic diagram of a system for detecting the void ratio of reinforced concrete columns based on piezoelectric ceramic technology according to another embodiment of the present invention.
[0042] Figure 4 It is a structural schematic diagram of a system for detecting the void ratio of reinforced concrete columns based on piezoelectric ceramic technology according to another embodiment of the present invention.
[0043] In the attached drawings: 1. Measured component; 2. First transmitting end piezoelectric ceramic sensor; 3. First receiving end piezoelectric ceramic sensor; 4. First acquisition module; 5. Imitation component; 6. Second transmitting end piezoelectric ceramic sensor; 7. Second receiving end piezoelectric ceramic sensor; 8. Second acquisition module; 9. Damage factor calculation module; 10. Imaging and judgment module; 11. Threshold determination module. DETAILED DESCRIPTION
[0044] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0045] It should be noted that when a component is referred to as being "fixed to" another component, it may be directly on the other component or there may also be a component centered. When a component is considered to be "connected to" another component, it may be directly connected to the other component or there may also be a component centered. When a component is considered to be "set on" another component, it may be directly set on the other component or there may also be a component centered. The terms "vertical", "horizontal", "left", "right" and similar expressions used herein are for illustrative purposes only.
[0046] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which the present invention belongs. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more of the related listed items.
[0047] See also Figure 1 A preferred embodiment of the present invention provides a method for detecting the void ratio of a reinforced concrete column based on piezoelectric ceramic technology, comprising:
[0048] S1, manufacturing a component to be measured, and embedding a piezoelectric ceramic sensor inside the component to be measured.
[0049] Here, manufacturing the measured component means making the measured component and placing it on the building, or directly building the measured component on the building. When manufacturing the measured component, the piezoelectric ceramic sensor needs to be buried inside the measured component, and the piezoelectric ceramic sensor leads the power line and signal line to the outside of the measured component to connect the power supply, control circuit and other components.
[0050] S2, using a piezoelectric ceramic sensor to obtain the voltage signal energy value of the measured component.
[0051] The energy value of the voltage signal of the measured component is obtained by a piezoelectric ceramic sensor arranged outside the measured component. The piezoelectric ceramic sensor inside the measured component is used to transmit the vibration signal, and the piezoelectric ceramic sensor outside the measured component is used to receive the vibration signal. The basic process is that the electrical energy is converted into the mechanical energy of the vibration of the internal piezoelectric ceramic sensor, and the external piezoelectric ceramic sensor converts the mechanical energy of the vibration into electrical energy, which is reflected in the waveform curve of the voltage signal changing with time. The area between the waveform curve and the time axis is calculated, which is the voltage signal energy value, that is, the function of the voltage signal changing with time is integrated. The calculation method of the voltage signal energy value is as follows:
[0052] The acquisition module collects the original signal S, and uses the wavelet packet analysis principle to decompose S into multiple component signals with equal width bands. The original signal is obtained by calling the wavelet packet tool script function in MATLAB to perform N-layer wavelet packet decomposition and reconstruction on the original signal. The corresponding wavelet packet energy.
[0053] (1) Wavelet packet decomposition
[0054] ;
[0055] Where T is the wavelet packet tree; is the original voltage signal collected in the i-th sampling period; N is the number of decomposition layers; Is the wavelet function type.
[0056] (2) Wavelet packet energy
[0057] ;
[0058] in, is the voltage signal energy value in the i-th sampling period, T is the wavelet packet tree after wavelet packet decomposition;
[0059] In order to ensure the detection of all directions of the measured component, it is necessary to arrange a circle of piezoelectric ceramic sensors on the outer wall of the measured component, that is, to surround the measured component with piezoelectric ceramic sensors, and the height of the piezoelectric ceramic sensors in this circle is equal, and then collect the electrical signals output by the piezoelectric ceramic sensors of each part on the outer wall of the measured component, calculate the voltage signal energy value, and then know the voltage signal energy value of each path of the measured component, and then continuously change the height of the external piezoelectric ceramic sensor, and then know the voltage signal energy value of all parts of the measured component. The following measurement of voltage signal energy value adopts such ideas and steps.
[0060] S3, manufacturing a replica component with the same material, structure and size as the component to be measured, and burying a piezoelectric ceramic sensor inside the replica component.
[0061] In order to obtain the voltage signal energy value of a healthy and undamaged component under the same conditions, a replica component is manufactured and a piezoelectric ceramic sensor is also buried in the same position as the piezoelectric ceramic sensor is buried inside the component being tested.
[0062] According to the strong steel concrete columns used in actual structural engineering, the same raw materials as the structure are selected to make components of the same size in the laboratory. When making the components, piezoelectric ceramics are arranged in the blind area of concrete pouring.
[0063] S4, using a piezoelectric ceramic sensor to obtain the voltage signal energy value of the replica component in a healthy state through a frequency sweep method.
[0064] In the laboratory, the concrete is cured and the components are tested. The voltage signal energy value of the simulated component obtained by the test is in the same form as the voltage signal energy value of the tested component.
[0065] S5, calculating the damage factor of the component under test according to the voltage signal energy value of the component under test and the voltage signal energy value of the simulated component in a healthy state.
[0066] The damage factor DI is defined for the voltage signal collected by the piezoelectric ceramic sensor. The calculation formula of the damage factor is:
[0067] The calculation formula of the damage factor is:
[0068] ;
[0069] Among them, DI is the damage factor; is the voltage signal energy value of the detected path of the measured component within the sampling time i; is the voltage signal energy value of the simulated component in the healthy state within the sampling period i; , Respectively represent the average voltage signals of the measured component and the simulated component.
[0070] By converting the voltage signal into energy, the cross-correlation deviation between the damaged energy value sample and the healthy steel concrete signal energy value is calculated to obtain the damage factor DI on the detection path. The larger the DI value, the greater the degree of damage on the detection path.
[0071] S6. According to the damage factor, the detection path of the measured component is imaged in three dimensions using the MATLAB data imaging method, and the damage factor is compared with the damage factor threshold. If the damage factor is less than or equal to the damage factor threshold, it is determined that there are no air gaps and damages on the detection path of the measured component. If the damage factor is greater than the damage factor threshold, it is determined that there are air gaps or damages on the detection path of the measured component.
[0072] On the detection path of the component under test, the damage factors at different positions are different. Damage factors of different values are associated with different colors, that is, different colors can represent different degrees of damage on the detection path, and the observer can intuitively see the damage status on the detection path of the component under test. Furthermore, different colors can also set different three-dimensional image thicknesses, and the different colors and thicknesses at each position of the detection path of the component under test are combined to form a three-dimensional image. In the present invention, the method of data imaging using MATLAB is used to perform three-dimensional imaging on the detection path of the component under test.
[0073] During the on-site construction process, the internal damage detection of the reinforced concrete column is carried out in real time by combining theoretical analysis data with on-site measurement results. Preferably, the condition for judging whether there are defects inside the reinforced concrete column is: the damage factor DI should satisfy ,like This reflects that there is an air gap or damage on the detection path, that is, the damage factor threshold is 0.7. This value is obtained through experimental verification and can usually be used as a standard for judging whether there is damage or air gap.
[0074] In a preferred embodiment of the present invention, the damage factor threshold is variable. This is because as the on-site environment of the component under test changes, the damage factor threshold may also change to a certain extent. In order to more accurately and finely determine whether the component under test is damaged, the damage factor threshold can be re-determined during each test. Figure 2 As shown, the steps for determining the damage factor threshold include:
[0075] S1', setting triggerable artificial damage on the replica component.
[0076] When the laboratory makes replica components, artificial damage is pre-set. For example, a part of a specific size and that can be easily removed is added when manufacturing the replica components. Once the part is removed, damage of a specific size will be left on the replica components.
[0077] S2', triggering artificial damage, using piezoelectric ceramic sensors to obtain the voltage signal energy value of the replica component in the damaged state.
[0078] After the component maintenance is completed, damage is triggered (such as removal of specific components), and the same type of piezoelectric ceramic sensor is used to collect electrical signals for the artificial damage set.
[0079] S3', calculate the damage factor threshold according to the voltage signal energy value of the simulated component in the healthy state and the damaged state, the formula is:
[0080] It is used to calculate the damage factor threshold according to the voltage signal energy value of the simulated component in the healthy state and the damaged state. The formula is:
[0081] ;
[0082] in, is the damage factor threshold, is the voltage signal energy value of the simulated component in the damaged state within sampling period i; is the voltage signal energy value of the simulated component in the healthy state within the sampling period i, The average value of the voltage signal energy value of the simulated component under the damaged state, It represents the average value of the voltage signal energy value of the simulated component in a healthy state.
[0083] In the present invention, preferably, a piezoelectric ceramic sensor is buried inside the measured component and a piezoelectric ceramic sensor is buried inside the imitation component, and the piezoelectric ceramic sensor is buried in the concrete casting blind area of the measured component and the imitation component. Because there is a high possibility of damage or air gaps in the concrete casting blind area, burying the piezoelectric ceramic sensor in the concrete casting blind area will be more conducive to quickly discovering damage and air gaps.
[0084] The embodiment of the present invention also provides a system for detecting the void ratio of reinforced concrete columns based on piezoelectric ceramic technology. Figure 3 As shown, it includes: a first transmitting end piezoelectric ceramic sensor 2, buried in the measured component 1, for transmitting vibration signals; a first receiving end piezoelectric ceramic sensor 3, which is distributed all around the outer wall of the measured component 1, for receiving vibration signals; a first acquisition module 4, which is electrically connected to the first receiving end piezoelectric ceramic sensor 3, for acquiring the voltage signal energy value of the measured component 1; an imitation component 5, which has the same material, structure, and size as the measured component 1, and is used to imitate the internal and external environment of the measured component 1; a second transmitting end piezoelectric ceramic sensor 6, which is buried in the imitation component 5, for transmitting vibration signals; a second receiving end piezoelectric ceramic sensor 7, which is fixed to the outer wall of the imitation component 5, for receiving vibration signals; a second acquisition module 8, which is electrically connected to the second receiving end piezoelectric ceramic sensor 7, for acquiring the simulated voltage signal energy value in a healthy state and in an injured state by a frequency sweeping method. The voltage signal energy value of the simulated component 5; the damage factor calculation module 9 is electrically connected to the first acquisition module 4 and the second acquisition module 8 respectively, and is used to calculate the damage factor of the measured component 1 according to the voltage signal energy value of the measured component 1 and the voltage signal energy value of the simulated component 5 in a healthy state; the imaging and judgment module 10 is electrically connected to the damage factor calculation module 9, and is used to perform three-dimensional imaging of the detection path of the measured component according to the damage factor, using the MATLAB data imaging method, and compare the damage factor with the damage factor threshold. If the damage factor is greater than or equal to the damage factor threshold, it is determined that the measured component 1 does not have air gaps and damage on the detection path. If the damage factor is less than the damage factor threshold, it is determined that the measured component 1 has air gaps or damage on the detection path; the calculation method of the voltage signal energy value is as follows:
[0085] The acquisition module collects the original signal S, and uses the wavelet packet analysis principle to decompose S into multiple component signals with equal width bands. The original signal is obtained by calling the wavelet packet tool script function in MATLAB to perform N-layer wavelet packet decomposition and reconstruction on the original signal. The corresponding wavelet packet energy.
[0086] (1) Wavelet packet decomposition
[0087] ;
[0088] Where T is the wavelet packet tree; is the original voltage signal collected in the i-th sampling period; N is the number of decomposition layers; Is the wavelet function type.
[0089] (2) Wavelet packet energy
[0090] ;
[0091] in, is the voltage signal energy value in the i-th sampling period, T is the wavelet packet tree after wavelet packet decomposition;
[0092] The calculation formula of the damage factor is:
[0093] ;
[0094] Among them, DI is the damage factor; The voltage signal energy value of the detected path of the measured component 1 within the sampling time i; Imitation component 5 in a healthy state within the voltage signal energy value of the sampling period i; , They respectively represent the average voltage signals of the tested component and the simulated component in a healthy state.
[0095] Specifically, the damage factor threshold may be 0.7.
[0096] In a preferred embodiment of the present invention, the damage factor threshold is variable, such as Figure 4 As shown, the steel concrete column void rate detection system based on piezoelectric ceramic technology also includes a threshold determination module 11, which is electrically connected to the second acquisition module 8 and is used to calculate the damage factor threshold according to the voltage signal energy value of the imitation component 5 in the healthy state and the damaged state. The formula is:
[0097] ;
[0098] in, is the damage factor threshold, is the voltage signal energy value of the imitation component 5 in the damaged state within the sampling period i; is the voltage signal energy value of the replica component 5 in the healthy state within the sampling period i, , Both represent the average value of the voltage signal energy value of the imitation component.
[0099] In a preferred embodiment of the present invention, the first transmitting end piezoelectric ceramic sensor 2 is buried in the concrete casting blind area of the measured component 1, and the second transmitting end piezoelectric ceramic sensor 6 is buried in the concrete casting blind area of the simulated component 5.
[0100] The method and system for detecting the void ratio of a reinforced concrete column based on piezoelectric ceramic technology of the present invention arrange piezoelectric ceramic sensors inside and outside the tested component 1 of the reinforced concrete, collect the voltage signal energy values of different detection paths, calculate the damage factors of different paths, and judge whether there are damages or air gaps on each detection path of the tested component 1 according to the relationship between the damage factor and the damage factor threshold, thereby realizing non-destructive detection of the void ratio of the reinforced concrete column. The detection process is simple and efficient, and the detection results are accurate.
[0101] The above description is a detailed description of the preferred feasible embodiments of the present invention, but the embodiments are not intended to limit the scope of the patent application of the present invention. All equivalent changes or modified changes completed under the technical spirit suggested by the present invention should fall within the patent scope covered by the present invention.
Claims
1. A method for detecting the void ratio of reinforced concrete columns based on piezoelectric ceramic technology, characterized in that: include: S1, manufacturing a component to be tested, and burying a piezoelectric ceramic sensor inside the component to be tested; S2, using a piezoelectric ceramic sensor to obtain a voltage signal energy value of the component under test; S3, manufacturing a replica component with the same material, structure and size as the component to be measured, and burying a piezoelectric ceramic sensor inside the replica component; S4, using a piezoelectric ceramic sensor to obtain a voltage signal energy value of the replica component in a healthy state by means of a frequency sweep; S5, calculating the damage factor of the component under test according to the voltage signal energy value of the component under test and the voltage signal energy value of the simulated component in a healthy state; S6, according to the damage factor, using the MATLAB data imaging method, three-dimensionally imaging the detection path of the measured component, comparing the damage factor with the damage factor threshold, if the damage factor is less than or equal to the damage factor threshold, it is determined that there is no air gap and damage on the detection path of the measured component, if the damage factor is greater than the damage factor threshold, it is determined that there is an air gap or damage on the detection path of the measured component; The voltage signal energy value is calculated as follows: The original signal is collected through the acquisition module, and the original signal is decomposed into several component signals of equal width bands using the wavelet packet analysis principle. The wavelet packet tool script function in MATLAB is called to perform N-layer wavelet packet decomposition and reconstruction on the original signal to obtain the wavelet packet energy corresponding to the original signal. Wavelet packet decomposition is expressed as: ; Where T is the wavelet packet tree, is the original voltage signal collected in the i-th sampling period, N is the number of decomposition layers, is the wavelet function type, The function is the wavelet packet decomposition function; The wavelet packet energy is expressed as: ; in, is the voltage signal energy value in the i-th sampling period, T is the wavelet packet tree after wavelet packet decomposition, The function is the wavelet coefficient energy function; The calculation formula of the damage factor is: ; Where DI is the damage factor, is the voltage signal energy value of the detection path of the measured component within the sampling time i, is the voltage signal energy value of the simulated component in the healthy state within the sampling period i, Indicates the average voltage signal of the measured component. Represents the average value of the voltage signal of the replica component.
2. The method for detecting the void ratio of reinforced concrete columns based on piezoelectric ceramic technology according to claim 1 is characterized in that: The damage factor threshold is 0.
7.
3. The method for detecting the void ratio of reinforced concrete columns based on piezoelectric ceramic technology according to claim 1 is characterized in that: The damage factor threshold is variable, and the step of determining the damage factor threshold comprises: S1', setting triggerable artificial damage on the imitation component; S2', triggering artificial damage, using piezoelectric ceramic sensors to obtain the voltage signal energy value of the replica component in the damaged state; S3', calculate the damage factor threshold according to the voltage signal energy value of the simulated component in the healthy state and the damaged state, the formula is: ; in, is the damage factor threshold, is the voltage signal energy value of the simulated component in the damaged state within sampling period i; is the voltage signal energy value of the simulated component in the healthy state within the sampling period i, The average value of the voltage signal energy value of the simulated component under the damaged state, It represents the average value of the voltage signal energy value of the simulated component in a healthy state, and N is the number of decomposition layers.
4. The method for detecting the void ratio of reinforced concrete columns based on piezoelectric ceramic technology according to claim 1 is characterized in that: The piezoelectric ceramic sensor is buried inside the measured component and the piezoelectric ceramic sensor is buried inside the imitation component. The piezoelectric ceramic sensor is buried in the concrete pouring blind area of the measured component and the imitation component.
5. The hollow rate detection system of reinforced concrete column based on piezoelectric ceramic technology is characterized by: include: The first transmitting end piezoelectric ceramic sensor is buried inside the measured component and is used to transmit a vibration signal; The first receiving end piezoelectric ceramic sensor is distributed all around the outer wall of the measured component and is used to receive the vibration signal; A first acquisition module, electrically connected to the first receiving end piezoelectric ceramic sensor, for acquiring a voltage signal energy value of the measured component; The imitation component has the same material, structure and size as the component to be tested and is used to simulate the internal and external environment of the component to be tested; The second transmitting end piezoelectric ceramic sensor is buried inside the imitation component and is used to transmit a vibration signal; The second receiving end piezoelectric ceramic sensor is distributed all around the outer wall of the imitation component and is used to receive the vibration signal; A second acquisition module, electrically connected to the second receiving end piezoelectric ceramic sensor, for acquiring voltage signal energy values of the imitation component in a healthy state and in a damaged state by means of frequency sweeping; A damage factor calculation module, electrically connected to the first acquisition module and the second acquisition module, respectively, for calculating the damage factor of the measured component according to the voltage signal energy value of the measured component and the voltage signal energy value of the simulated component in a healthy state; An imaging and judgment module is electrically connected to the damage factor calculation module, and is used to perform three-dimensional imaging of the detection path of the component under test according to the damage factor by using a data imaging method using MATLAB, and compare the damage factor with a damage factor threshold. If the damage factor is less than or equal to the damage factor threshold, it is determined that there are no air gaps and damages on the detection path of the component under test; if the damage factor is greater than the damage factor threshold, it is determined that there are air gaps or damages on the detection path of the component under test; The voltage signal energy value is calculated as follows: The original signal is collected through the acquisition module, and the original signal is decomposed into several component signals of equal width bands using the wavelet packet analysis principle. The wavelet packet tool script function in MATLAB is called to perform N-layer wavelet packet decomposition and reconstruction on the original signal to obtain the wavelet packet energy corresponding to the original signal. Wavelet packet decomposition is expressed as: ; Where T is the wavelet packet tree; is the original voltage signal collected in the i-th sampling period; N is the number of decomposition layers; is the wavelet function type, The function is the wavelet packet decomposition function; The wavelet packet energy is expressed as: ; in, is the voltage signal energy value in the i-th sampling period, T is the wavelet packet tree after wavelet packet decomposition, The function is the wavelet coefficient energy function; The calculation formula of the damage factor is: ; Where DI is the damage factor, is the voltage signal energy value of the detection path of the measured component within the sampling time i, is the voltage signal energy value of the simulated component in the healthy state within the sampling period i, The average value of the voltage signal of the measured component, Represents the average voltage signal of the simulated component, and N is the number of decomposition layers.
6. The piezoelectric ceramic technology-based steel-concrete column void rate detection system according to claim 5 is characterized in that: The damage factor threshold is 0.
7.
7. The piezoelectric ceramic technology-based steel-concrete column void rate detection system according to claim 5 is characterized in that: The damage factor threshold is variable. The piezoelectric ceramic technology-based steel concrete column void rate detection system also includes a threshold determination module, which is electrically connected to the second acquisition module and is used to calculate the damage factor threshold according to the voltage signal energy value of the imitation component in the healthy state and the damaged state. The formula is: ; in, is the damage factor threshold, is the voltage signal energy value of the simulated component in the damaged state within sampling period i; is the voltage signal energy value of the simulated component in the healthy state within the sampling period i, It represents the average value of the voltage signal energy value of the simulated component under the damaged state. It represents the average value of the voltage signal energy value of the simulated component in a healthy state, and N is the number of decomposition layers.
8. The piezoelectric ceramic technology-based steel-concrete column void ratio detection system according to claim 5 is characterized in that: The first transmitting end piezoelectric ceramic sensor is buried in a blind area of concrete casting of the measured component, and the second transmitting end piezoelectric ceramic sensor is buried in a blind area of concrete casting of the simulated component.