Article, method of producing an article and use thereof
By using an incompletely cured protective paint layer and printing layer in the injection mold, and performing partial curing during the imprinting process, the problem of difficult to balance product surface structure and resistance is solved, and high-efficiency, low-cost products are achieved. Production.
Patent Information
- Application Number
- CN202380024594.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-03
- Filing Date
- 2023-03-01
- Publication Date
- 2024-10-18
AI Technical Summary
Existing technologies struggle to provide localized surface structuring of articles cost-effectively and efficiently while ensuring resistance and flexible design, especially in the face of mechanical and chemical influences.
Using an incompletely cured protective paint layer and printing layer, a local relief structure is formed through post-injection molding and embossing technology in the injection mold, and a cross-linkable polymer is used for local curing during the embossing process.
It achieves high mechanical and chemical resistance of the product while allowing flexible surface design and three-dimensional forming, reducing production costs and avoiding the problem of unsatisfied optical requirements.
Smart Images

Figure CN118804832A_ABST
Abstract
Description
[0001] The present invention relates to a method for producing an article, as well as to the article and the use of the article.
[0002] The film is used for the surface decoration of articles. Articles decorated in this way are used, for example, in automobile manufacturing for automobile interior parts, such as door frames, instrument frames and center console visors, in the field of consumer electronics for decorative frames on televisions, or in the field of electronics and telecommunications for housings of portable devices such as mobile phones or laptops, or other covering elements, covering elements or control elements in household appliances, for example.
[0003] To produce these articles, it is known to carry out post-injection molding of an IMD transfer film (IMD = in-mold decoration) with a plastic composition in an injection mold. In order to ensure the resistance of the articles produced in this way, the IMD transfer film usually has a protective lacquer layer, which forms the outer side of the article after the carrier ply of the IMD transfer film has been peeled off.
[0004] In addition, the surface decoration of articles by means of insert molding processes is also known. This involves a combined method of hot stamping or cold embossing, vacuum forming and injection molding, wherein a transfer film is first applied to a substrate by means of hot stamping or cold embossing, and after peeling off the carrier film of the transfer film, the substrate is deformed in three dimensions or 2.5 dimensions, in particular by deep drawing, and then the substrate is post-injected. After deformation (in particular deep drawing), it can be seen that the decorated substrate, in particular its outer layer such as a protective lacquer layer, is directly cured. This curing is carried out, for example, by means of high-energy radiation, for example by means of UV radiation, and preferably by means of irradiation on the decorated substrate side. Curing can be carried out alternatively or additionally by means of thermal curing, and / or can be achieved alternatively or additionally by means of reactive curing inside the layer involved and / or between adjacent layers. Preferably, after curing, post-injection molding is carried out with a plastic composition, in particular.
[0005] Furthermore, it is also known to decorate the surface of articles by means of wet painting. This involves the application of liquid paint or ink by known methods such as spray painting, screen printing, inkjet printing, pad printing, etc. In this case, before the wet painting, the article is at least partially already provided with a coating, which is selected from wet painting, transfer coating by hot stamping, transfer coating by cold stamping, transfer coating by IMD method, coating by insert molding, lamination, coextrusion, labeling, alone or in combination.
[0006] Although it is also known to provide articles with a surface structure that occupies the entire surface of the article (e.g. with a matte transfer film), it is desirable to provide the surface structure only locally, so it is necessary to use transfer films that are locally structured before they are provided for the process of producing the article. However, this leads to challenges in the subsequent production of the article, especially when it is desired to register the local surface structuring with the graphics, background color or other decorative elements of the transfer film and / or with specific areas of functional areas such as control areas and displays or 3D geometries of decorative parts. In addition, transfer films that can be locally post-structured usually have insufficient resistance to mechanical or chemical loads precisely because of this structurability.
[0007] However, if the surface is to be very strong, post-processing of the surface is complex and cost-intensive due to its nature, and there is a risk that the molding is at least partially carried out but not all optical requirements are met. Thus, for example, the result of post-processing of a lacquer layer that has been completely cured and / or crosslinked by means of embossing may appear uneven and spotty. In addition, the strongness of the lacquer layer often also leads to brittleness or low stretchability, which limits the formability of the lacquer layer and thus its use in IMD methods and in-mold methods.
[0008] It is therefore unknown to provide a cost-effective and efficient surface which only partially has a surface structure, which on the one hand is very resistant to external influences such as UV radiation, hand creams, solvents, abrasion or scratches and on the other hand allows flexible surface design and the production of three-dimensional or 2.5-dimensional articles.
[0009] It is now an object of the present invention to provide an improved method for producing articles and to provide improved articles and their use.
[0010] This object is achieved by a method for producing an article, in particular according to one of claims 1 to 31, wherein the method comprises at least one of the steps A1) or A2) or A3),
[0011] Wherein step A1) comprises the following steps:
[0012] a1) providing a transfer film, wherein the transfer film has a carrier layer and a transfer layer, wherein the carrier layer is releasable from the transfer layer, wherein the carrier layer comprises a carrier layer, wherein the transfer layer comprises a protective lacquer layer, wherein the protective lacquer layer is at least partially not yet fully cured or is thermoplastic, and wherein the protective lacquer layer is arranged such that it is in contact with the carrier layer;
[0013] b1) arranging the transfer film, in particular the transfer layer, in an injection mold;
[0014] c1) post-injection molding of a transfer film (in particular a transfer layer) with a plastic composition, wherein the plastic composition forms the matrix;
[0015] d) peeling the carrier layer from the transfer layer;
[0016] Wherein step A2) comprises the following steps:
[0017] a2) providing an insert, wherein the insert comprises a substrate and a transfer ply arranged on the substrate and / or a print layer arranged, wherein the transfer ply comprises a protective lacquer layer;
[0018] b2) arranging the insert in the injection mold;
[0019] c2) post-injection molding of the insert with a plastic composition, wherein the plastic composition forms the matrix;
[0020] Wherein step A3) comprises the following steps:
[0021] a3) providing a transfer film, wherein the transfer film has a carrier layer and a transfer layer, wherein the carrier layer is peelable from the transfer layer, wherein the carrier layer comprises a carrier layer, wherein the transfer layer comprises a protective lacquer layer, and wherein the protective lacquer layer is arranged such that it is in contact with the carrier layer,
[0022] and providing a base body separately from the transfer film, said base body being produced in particular by means of injection molding;
[0023] k3) arranging a transfer film, in particular a transfer layer, on the surface of the substrate, and hot stamping the transfer film onto the surface of the substrate;
[0024] d) peeling the carrier layer from the transfer layer;
[0025] wherein the protective lacquer layer and / or the printed layer is at least partially not yet completely cured or is thermoplastic in step A1) or A2) or A3),
[0026] And wherein in addition to at least one of step A1) or A2) or A3), the method further comprises the following steps:
[0027] e) forming at least one first region and at least one second region in the protective lacquer layer and / or the printed layer by means of embossing, wherein the at least one first region has a relief structure;
[0028] f) optionally curing the protective lacquer layer and / or the printed layer which has not yet been fully cured at least in places, wherein the protective lacquer layer is at least partially fully cured;
[0029] g) obtaining an article, wherein the article comprises a substrate and a protective lacquer layer and / or a printed layer, wherein the protective lacquer layer and / or the printed layer is at least partially cured or thermoplastic, wherein the protective lacquer layer and / or the printed layer has at least one first area and at least one second area, wherein the relief structure is arranged in the at least one first area.
[0030] This task is also accomplished with the aid of an article, preferably according to claim 32, wherein the article has a substrate and a protective lacquer layer and / or a printed layer, wherein the protective lacquer layer and / or the printed layer is at least partially fully cured or is thermoplastic, wherein the protective lacquer layer and / or the printed layer has at least one first area and at least one second area, wherein the relief structure is arranged in at least one first area, and wherein the article is produced according to one of claims 1 to 31.
[0031] This object is further achieved in particular by claim 33, by the use of an article according to claim 32 or an article produced by a method according to any one of claims 1 to 31, alone or in combination as a display window, touch screen panel, panel, visor, covering, covering, functional element, electronic article and housing part or outer part, in particular for white goods and / or household appliances and / or for the interior area and / or exterior area of a vehicle.
[0032] A region is understood here to be a defined surface of a layer, film or ply, in particular when viewed perpendicularly to the plane formed by the transfer film of the substrate and / or base, in particular by the transfer ply, protective lacquer layer, print layer. Thus, for example, at least one protective lacquer layer and / or print layer of the obtained article has at least one first region and at least one second region, wherein each of the two or more regions has a defined surface in each case when viewed perpendicularly to the plane formed by the protective lacquer layer and / or print layer, in particular in all layers arranged in the protective lacquer layer and / or print layer and in the layers arranged above and / or below the protective lacquer layer and / or print layer, in particular in all layers of the transfer ply.
[0033] Forming at least one region is understood in the context of the present invention in particular as an operation on a layer, ply or lacquer (e.g. a protective lacquer layer and / or a printed layer), wherein the surface structure of the original layer, ply or lacquer, e.g. a protective lacquer layer and / or a printed layer, is different from the surface structure, in particular the relief structure, of the operated region. The region is formed in particular in the layer, ply or lacquer (e.g. a protective lacquer layer and / or a printed layer), wherein the surface structure of the layer, ply or lacquer is more structured in particular in the operated region. Therefore, it is possible that before forming at least one region, there is no surface structure, in particular the relief structure, in the layer, ply or lacquer (e.g. in a protective lacquer layer and / or a printed layer), and after forming the surface structure (in particular the relief structure), at least one operated region is formed. It is therefore possible that at least two formed regions may be optically different. This difference is particularly perceptible to the human eye and / or measurable for a sensor. The formation of the region is preferably achieved by means of embossing.
[0034] "Not yet fully cured" preferably describes a layer (in particular a protective lacquer layer and / or a printed layer) when its hardness and / or resistance has not yet reached a determined minimum value. The determined minimum value of hardness and / or resistance is preferably a function of the final intended use of the layer (for example as a protective lacquer layer and / or a printed layer). Therefore, "fully cured" in the meaning of the present invention describes a layer when its hardness and / or resistance has reached a determined minimum value.
[0035] The above minimum value can be determined such that a layer is described as not yet fully cured within the meaning of the present invention when no more than 95% of the crosslinkable polymer components in the layer are crosslinked. Thus, within the meaning of the present invention, a layer is described as fully cured when more than 95% of the crosslinkable polymer components in the layer are crosslinked. A fully cured layer exists when its polymer components have achieved complete (>95%) crosslinking.
[0036] The method according to the invention makes it possible to provide a transfer film which only partially has a relief structure by means of embossing only after the injection molding process. This offers several advantages. Thus, during the production of the article, it is not necessary to provide a film which already has a relief structure locally. Thus, the method also does not risk obtaining an unintended offset of the local relief structure relative to the decorative element or functional element.
[0037] The invention makes it possible to provide articles which have a surface which is resistant to mechanical and chemical influences and which are nevertheless locally structured with a relief structure. This can be achieved by virtue of the fact that the locally structured layer acquires its intended strength during the process. This further makes it possible to produce three-dimensional or 2.5-dimensional shaped articles, since the transfer film has sufficient flexibility during the shaping process. However, the transfer film can also be unshaped or only very slightly shaped and applied to flat (2D, two-dimensional) areas.
[0038] Furthermore, due to the use of different and replaceable embossing tools or carriers containing the master structure, individual layouts can be created for the articles. Thus, the production of small quantities or even individual articles is also associated with much lower additional costs when compared to having to produce a specific, already structured transfer film. Furthermore, the layout can also be changed temporarily. Thus, the transfer film does not need to be discarded if its layout is no longer current after a short period of time.
[0039] Another great advantage compared to the known prior art is that the structures and / or patterns in the article and / or transfer film, which can optionally be backlit, are not affected or only slightly affected by the post-structuring. The post-structuring affects the transparency present only to a small extent locally. Therefore, the scattering effects introduced by the relief structure are so low that they can be neglected in the transmitted light. Thus, optical diffraction structures for transmitted lighting can be embossed. If the article has a backlight, additional optical effects, such as anti-glare effects, can also be achieved by the relief structure introduced only locally.
[0040] Further advantageous embodiments of the invention are described in the dependent claims.
[0041] The steps A1) and A2) and A3) describe in particular an equivalent alternative for obtaining and / or providing a substrate on which a transfer layer and / or a printed layer has been arranged, wherein the protective lacquer layer and / or the printed layer are at least partially not fully cured or are thermoplastic. Step A1) comprises at least steps a1), b1), c1) and d). Step A2) comprises at least steps a2), b2) and c2). Step A3) comprises at least steps a3), k3) and d).
[0042] In particular, in steps e), f) and g), it is described how, preferably after steps A1) and / or A2) and / or A3), an article is obtained from a substrate on which a transfer ply and / or a print layer is arranged. The article comprises a substrate and a protective lacquer layer and / or a print layer, wherein the protective lacquer layer and / or the print layer is at least partially cured or thermoplastic, and wherein the protective lacquer layer and / or the print layer comprises at least one first region and at least one second region, wherein a relief structure is arranged in the at least one first region.
[0043] Step a) refers to step a1), a2) and / or a3). Furthermore, step b) refers to step b1) and / or b2). Furthermore, step c) refers to step c1) and / or step c2).
[0044] Step a) is preferably the first step of the method, in particular carried out before steps b) to g). In step a), the transfer film can be provided as a roll. In addition, the transfer film can be provided as a hot stamping film or an IMD film. In addition, an insert can also be provided. The article is preferably produced by the IMD method or the insert molding method. The article can also be produced in an injection molding method using a downstream hot stamping method, wherein the transfer layer is arranged on a substrate in the hot stamping method. In particular, in step a3), in addition to the transfer film, a substrate is also provided, which can preferably be designed as a substrate as described for step c).
[0045] The transfer film provided in step a) or the insert provided can have a transfer ply which is already structured in multiple layers.
[0046] The provided insert can have a multi-layer transfer ply and / or a multi-layer print layer. The print layer is preferably arranged partially or over the entire surface of the insert. The print layer is in particular formed as a screen print layer, a gravure print layer, an inkjet print layer or a combination thereof. The insert preferably has a gravure print layer and a screen print layer. The individual layers of the print layer can overlap at least partially. The insert can have a transfer ply on which one or more print layers have been partially printed.
[0047] The transfer layer preferably has a layer thickness selected from the range of 0.1 μm to 100 μm, preferably 0.5 μm to 75 μm, further preferably 1 μm to 50 μm.
[0048] The protective lacquer layer and / or printed layer protects the article in particular from external influences, such as UV radiation, mechanical influences (e.g. abrasion) or chemical influences (e.g. creams or solvents). The protective lacquer layer and / or printed layer therefore has a particularly high resistance to mechanical and chemical loads, in particular compared to the layers, matrix and / or optional substrate located therebelow.
[0049] The protective lacquer layer preferably has a layer thickness selected from the range of 1 μm to 15 μm, preferably 2 μm to 8 μm, further preferably 2 μm to 5 μm. With such a layer thickness of the protective lacquer layer, the protective lacquer layer can have the necessary resistance in the finished product.
[0050] Furthermore, the protective lacquer layer has a transmittance of at least 70%, preferably at least 85%, for the wavelength range perceptible to the human eye, preferably for the range of 400 nm to 700 nm. The above transmittance means that the protective lacquer layer is transparent. The decoration, decorative element or substrate located thereunder is thus clearly recognizable.
[0051] In particular, the protective lacquer layer is at least partially not yet fully cured. Preferably, the protective lacquer layer is at least partially precured chemically and / or by means of radiation, preferably UV radiation, and / or is at least partially fully curable by means of radiation, preferably UV radiation. For this purpose, the protective lacquer layer comprises at least one UV-crosslinkable polymer. Within the meaning of the present invention, a UV-crosslinkable polymer preferably has at least one, preferably two or more, ethylenically unsaturated double bond.
[0052] The term "ethylenically unsaturated double bond" preferably means a mono-, di- or tri-substituted C=C double bond which is not keyed into the aromatic electron system. The ethylenically unsaturated double bond is preferably not conjugated with other double bonds.
[0053] Preferably, the partially uncured protective lacquer layer is preferably prepared based on at least one UV-crosslinkable or at least one chemically crosslinkable polymer, alone or in combination. In addition, the protective lacquer layer can be prepared from a thermoplastic polymer.
[0054] The protective lacquer layer can also comprise at least one chemically crosslinkable polymer, which is further preferably selected from the group consisting of polymers containing isocyanate groups, polymers containing melamine groups, polymers containing hydroxyl groups and mixtures thereof.
[0055] The protective lacquer layer preferably has at least one chemically crosslinkable polymer combination, which contains or is a polymer and / or copolymer having at least one, preferably two or more isocyanate groups, and at least one polymer and / or copolymer having at least one, preferably two or more hydroxyl groups, and / or at least one melamine resin and at least one polymer and / or copolymer having at least one, preferably two or more hydroxyl groups.
[0056] The at least one UV-crosslinkable polymer of the protective lacquer layer may also have, in each case independently of one another, at least one chemically crosslinkable functional group, wherein the chemically crosslinkable functional group is preferably selected from hydroxyl groups, isocyanate groups, melamine groups, epoxy groups and combinations thereof.
[0057] Preferably, the at least one UV-crosslinkable polymer also has at least one hydroxyl group.
[0058] Suitable UV-crosslinkable polymers containing hydroxyl groups are known in the prior art and include, for example, at least one diacrylate monomer, an aliphatic polyether polyurethane diacrylate, an aliphatic polyester polyurethane diacrylate, an aromatic polyether polyurethane diacrylate, an aromatic polyester polyurethane diacrylate, a polyester diacrylate, a polyether diacrylate, an epoxy diacrylate, an acrylated acrylic diacrylate, a polyacrylate monomer, an aliphatic polyether polyurethane polyacrylate, an aliphatic polyester polyurethane polyacrylate, an aromatic polyether polyurethane polyacrylate, an aromatic polyester polyurethane polyacrylate, a polyester polyacrylate, a polyether polyacrylate, an epoxy polyacrylate, an acrylated acrylic polyacrylate or mixtures thereof and / or at least one hydroxy monoacrylate, a hydroxy diacrylate, a hydroxy polyacrylate, a hydroxy functionalized aliphatic polyether polyurethane monoacrylate, a hydroxy functionalized aliphatic polyester polyurethane monoacrylate, a hydroxy functionalized aromatic polyether polyurethane monoacrylate, a hydroxy functionalized aromatic polyester polyurethane monoacrylate. acrylates, hydroxy-functional polyester monoacrylates, hydroxy-functional polyether monoacrylates, hydroxy-functional epoxy monoacrylates, hydroxy-functional acrylated acrylic monoacrylates, hydroxy-functional aliphatic polyether urethane diacrylates, hydroxy-functional aliphatic polyester urethane diacrylates, hydroxy-functional aromatic polyether urethane diacrylates, hydroxy-functional aromatic polyester urethane diacrylates, hydroxy-functional polyester diacrylates, hydroxy-functional polyether diacrylates, hydroxy-functional epoxy diacrylates, hydroxy-functional acrylated acrylic diacrylates, hydroxy-functional aliphatic polyether urethane polyacrylates, hydroxy-functional aliphatic polyester urethane polyacrylates, hydroxy-functional aromatic polyether urethane polyacrylates, hydroxy-functional aromatic polyester urethane polyacrylates, hydroxy-functional polyester polyacrylates, hydroxy-functional polyether polyacrylates, hydroxy-functional epoxy polyacrylates, hydroxy-functional acrylated acrylates, or mixtures thereof.
[0059] Suitable melamine resins are in particular those which are obtainable by reaction of melamine with aldehydes and which may optionally be partially or completely modified.
[0060] In particular, formaldehyde, acetaldehyde, isobutyraldehyde and glyoxal are suitable as aldehydes.
[0061] The melamine formaldehyde resin is preferably a reaction product of melamine with aldehydes, such as the abovementioned aldehydes, in particular formaldehyde. The methylol groups obtained are preferably modified by etherification with monohydric or polyhydric alcohols.
[0062] The protective lacquer layer can also be a precured system and / or a hybrid system. In particular, the protective lacquer layer can have at least one UV-curable component consisting of UV-curable monomers and / or UV-curable oligomers or mixtures thereof, and can also have at least one binder selected from the group consisting of polyurethanes, polyacrylates, polymethacrylates, polyester resins, polycarbonates, phenolic resins, epoxy resins, polyureas, melamine resins, preferably polymethyl methacrylate (PMMA), polyesters, polycarbonates (PC) and mixtures thereof.
[0063] The protective lacquer layer may also preferably comprise at least one polyisocyanate. The term polyisocyanate preferably describes an organic compound having two or more isocyanate groups, including triisocyanates and isocyanates of higher functionality. In a specific embodiment, at least one polyisocyanate is selected from the group consisting of diisocyanate monomers, diisocyanate oligomers, diisocyanate-terminated prepolymers, diisocyanate-terminated polymers, polyisocyanate monomers, polyisocyanate oligomers, polyisocyanate-terminated prepolymers, polyisocyanate-terminated polymers, polyisocyanate-terminated polymers and mixtures thereof.
[0064] Further preferably, the at least one polyisocyanate comprises or is at least one diisocyanate-containing component, which preferably comprises at least one diisocyanate-containing polyurethane oligomer, diisocyanate-containing polyurea oligomer, prepolymers thereof, polymers thereof or mixtures thereof.
[0065] In a specific embodiment, the at least one polyisocyanate comprises or is at least one diisocyanate-containing component, which is preferably selected from the group consisting of: hexamethylene diisocyanate (HDI), isophorone diisocyanate (IPDI), diphenylmethane diisocyanate (MDI), toluene diisocyanate (TDI), phenylene diisocyanate, naphthalene diisocyanate, diphenyl sulfone diisocyanate, ethylene diisocyanate, propylene diisocyanate, dimers of these diisocyanates, trimers of these diisocyanates, triphenylmethane triisocyanate, polyphenylmethane polyisocyanate (polymeric MDI) and mixtures thereof.
[0066] The protective lacquer layer is preferably or comprises a dual-cure system (preferably, for example, based on hydroxyl-containing polyacrylic acid esters crosslinked with melamine resins). Dual-cure systems can be cured in two curing steps, based on a combination of chemical crosslinking and curing of UV-crosslinkable polymers.
[0067] In particular, the protective lacquer layer can be produced based on a system that is physically drying and chemically crosslinkable and / or crosslinkable by UV radiation. The protective lacquer layer of the transfer film (preferably the transfer ply) is preferably cured in the process for producing the article by chemically crosslinking and / or crosslinking the protective lacquer layer.
[0068] The protective lacquer layer may preferably have additives, for example selected from pigments, initiators, crosslinking agents or catalysts, alone or in combination. In particular, the initiator is a photoinitiator. This can start, support and / or control the curing of the protective lacquer layer.
[0069] The protective lacquer layer of the transfer film (preferably the transfer ply) may be based on a thermoplastic polymer and / or a thermoplastic resin. Thus, the protective lacquer layer may preferably not be chemically crosslinkable or not chemically crosslinked and / or not be crosslinkable or not crosslinked by UV radiation. The thermoplastic polymer and / or thermoplastic resin may, for example, be selected from the group consisting of polyurethanes, polyacrylates, polymethacrylates, polyester resins, polycarbonates, styrene-butadiene copolymers, either alone or in combination, preferably from the group consisting of polymethyl methacrylate (PMMA), polyesters, polycarbonates (PC), polycarbonate / acrylonitrile butadiene styrene (PC / ABS), either alone or in combination.
[0070] In a preferred embodiment, the protective lacquer layer is formed as a printed layer, in particular a screen-printed layer, a gravure-printed layer, an inkjet-printed layer or a combination thereof. Here, the protective lacquer layer preferably has a transmittance of at most 30%, preferably at most 15%, for the wavelength range perceptible to the human eye, preferably for the range of 400 nm to 700 nm. The above transmittance means that the protective lacquer layer is opaque. Thus, the protective lacquer layer can be perceived as a decoration and / or decorative element, preferably, the protective lacquer layer can form a decoration and / or decorative element.
[0071] The protective lacquer layer can be arranged in the transfer ply partially or over the entire surface, preferably over the entire surface. The protective lacquer layer can be formed in multiple layers, in particular, wherein the layers of the protective lacquer layer at least partially overlap. This is particularly advantageous when the protective lacquer layer is already formed as a printed layer, since interesting designs can be created thereby.
[0072] The printed layer, in particular the additional printed layer and / or the above-mentioned printed layer of the insert, can be arranged and / or will be arranged on the protective lacquer layer, in particular wherein the printed layer is not yet fully cured at least in places. The printed layer, in particular the additional printed layer and / or the above-mentioned printed layer of the insert, has been and / or will be arranged on the protective lacquer layer, preferably partially or over the entire surface. Furthermore, the printed layer, in particular the additional printed layer and / or the above-mentioned printed layer of the insert, is in particular formed as a screen printed layer, a gravure printed layer, an inkjet printed layer or a combination thereof, preferably as a screen printed layer.
[0073] The transfer ply has, in particular, at least one decorative layer which preferably comprises at least one decorative element on the side of the protective lacquer layer facing away from the carrier ply.
[0074] Furthermore, the at least one decorative element comprised by the at least one decorative layer is preferably selected from the group consisting of transparent and / or colored lacquer layers (in particular comprising one or more dyes and / or pigments), replication layers with a molded, optically active surface structure, reflective layers (in particular opaque, transparent, metallic or dielectric reflective layers), optically variable layers, optically active layers, interference multilayer systems, volume hologram layers, liquid crystal layers (in particular cholesteric liquid crystal layers) and combinations thereof.
[0075] Alternatively or additionally, the transfer ply can have at least one functional layer comprising at least one functional element on the side of the protective lacquer layer facing away from the carrier ply. Here, the at least one functional layer can be arranged overlapping and / or adjacent to the at least one decorative layer. The at least one functional layer can also be arranged between at least two decorative layers or on the side of the functional layer of at least one decorative layer facing and / or facing away from the protective lacquer layer.
[0076] The at least one functional element is in particular selected from the group consisting of: at least one electronic component, in particular a strip conductor, a contact element, an LED, a sensor, in particular a touch sensor, a temperature sensor, a pressure sensor, an antenna (in particular an RFID element), a memory, a processor, a control element, a display, a capacitor, a resistor, a microfluidic element and combinations thereof.
[0077] For example, the functional layer may be designed as a conductive layer, an antenna layer, an electrode layer, a magnetic layer, a magnetic storage layer or a barrier layer, alone or in combination.
[0078] Preferably, the at least one decorative element is arranged in at least one decorative layer and / or the at least one functional element is arranged in at least one functional layer, which at least one functional layer in each case independently of one another comprises a UV-crosslinked lacquer or a chemically crosslinked lacquer or a thermoplastically deformable layer and in each case independently of one another are uncolored or colored or dyed.
[0079] It is also conceivable that the protective lacquer layer at least partially has preferably at least one decorative element and / or functional element, or is for example free of such elements.
[0080] An adhesion promoter layer is preferably arranged between the protective lacquer layer and at least one decorative element and / or at least one functional element. Here, the adhesion promoter layer can include at least one acrylic resin or consist of at least one acrylic resin. Furthermore, the adhesion promoter layer can preferably have a layer thickness selected from the range of 0.1 μm to 10 μm.
[0081] The transfer ply may also have at least one lacquer layer, preferably with a layer thickness selected from the range of 0.5 μm to 10 μm, which forms the surface of the transfer ply facing away from the carrier ply. The lacquer layer is preferably used for bonding to a substrate or a plastic composition. The at least one lacquer layer preferably comprises at least one adhesive or consists of at least one adhesive, the adhesive being selected from the group consisting of a physically curing adhesive, a chemically curing adhesive, a pressure-sensitive adhesive or a mixture thereof. In addition, the at least one lacquer layer may be a primer layer and / or a primer layer arranged instead of at least one lacquer layer and / or a primer layer arranged on the side of the at least one lacquer layer facing away from the protective lacquer layer, in particular wherein the primer layer comprises or consists of a PVC-copolymer and PMMA (PVC = polyvinyl chloride, PMMA = polymethyl methacrylate).
[0082] Furthermore, the transfer ply can have at least one or more of the following layers, in each case selected individually or in combination from: at least one colored lacquer layer, at least one metal layer, at least one oxide layer, at least one barrier layer, at least one receiving layer, at least one second protective lacquer layer, at least one laser protective lacquer layer. The layers can in each case be arranged over the entire surface or in each case partially in the transfer ply.
[0083] The carrier layer of the transfer film is provided with a carrier ply, which preferably comprises polyethylene terephthalate (PET), glycol-modified polyethylene terephthalate (PETG), polypropylene (PP), polycarbonate (PC), polyimide (PI) or polyamide (PA) and / or blends or copolymers thereof, either alone or in combination. The carrier ply (preferably the carrier layer) preferably has a layer thickness selected from the range of 10 μm to 100 μm, preferably 10 μm to 50 μm.
[0084] The carrier ply may have at least one release layer, which is preferably arranged between the carrier layer and the protective lacquer layer. The layer thickness of the release layer is in particular selected from the range of 0.1 nm to 100 nm. The release layer preferably contains or consists of at least one wax, for example a polyethylene wax. The release layer preferably has a melting temperature selected from the range of 80° C. to 100° C. The carrier ply is preferably arranged on the protective lacquer layer with an adhesion force in the range of 2 cN to 50 cN, preferably in the range of 5 cN to 35 cN, or this force needs to be overcome when the carrier ply is peeled off.
[0085] "In contact with the carrier ply" with respect to the protective lacquer layer means that the protective lacquer layer is in direct contact with the carrier layer of the carrier ply when no release layer is provided, or that the protective lacquer layer is in contact with the release layer of the carrier ply when a release layer is provided.
[0086] It is also conceivable that before step b), in particular before step d), the transfer film is arranged on a substrate, shaped, preferably pre-deformed and / or deep-drawn and / or trimmed. Here, it is particularly advantageous if the protective lacquer layer is at least partially not yet cured, since it has a much greater stretchability.
[0087] In other words, the method may further include at least one of the following steps h), i) and j):
[0088] h) placing a transfer film on a substrate;
[0089] i) forming the transfer film and / or substrate into a desired shape; and
[0090] j) Trimming the transfer film and / or substrate along defined contour lines.
[0091] In particular, steps h), i) and j) can be carried out after step a), preferably after step a1). Step h) is preferably carried out before step d). Steps i) and j) are preferably carried out after step d) and preferably before step b).
[0092] It is also suitable to carry out steps h), i) and j) before step d). This offers the advantage that in the case of post-injection moulding, in particular when only slight shaping is carried out in step i), the protective lacquer layer is still protected by the carrier ply.
[0093] In particular, steps h), i) and j) are carried out in an insert molding method, wherein the transfer film arranged on the substrate corresponds to an insert or can be used as an insert. The insert can be used as and / or corresponds to the insert provided in step a2). In other words, after step i), the insert provided in step a2) can be obtained. For this purpose, in subsequent method steps, in particular in step b), the insert can be placed in an injection mold and there, in particular, post-injection molding can be preferably carried out in step c).
[0094] In particular, the transfer film is arranged on the substrate by means of embossing, in particular hot stamping or cold embossing. The transfer film is preferably arranged by applying heat and / or pressure and / or by irradiation with UV radiation.
[0095] In particular, the substrate is selected from polycarbonate (PC), polycarbonate / acrylonitrile butadiene styrene (PC / ABS), polypropylene (PP), thermoplastic polyurethane (TPU), polymethyl methacrylate (PMMA), or blends and / or co-extruded products thereof, alone or in combination.
[0096] In particular, the forming can be carried out by deep drawing or vacuum forming, alone or in combination. The forming is preferably achieved by applying heat and / or pressure.
[0097] In particular, trimming can be achieved by means of water jet cutting, laser or punching, alone or in combination.
[0098] The transfer ply is arranged in step b) in an injection mold and in step c) is post-injected with a plastic composition. Step b) is preferably carried out after step a) or after step j), in particular before step c). Step c) is preferably carried out before step d) and / or after step b). In particular, step c) can be carried out once or more, in particular with the same or different plastic compositions.
[0099] The injection mold advantageously has the shape of the surface of the article and / or predetermines it. A rigid article can be obtained. Preferably, the surface of the article, in particular the surface with the protective lacquer layer, can be tortuous and / or curved.
[0100] Preferably, in the case of post-injection molding of the transfer ply, in particular in step c), the transfer ply or the optional substrate is at least partially covered with the plastic composition at least on at least one surface of the transfer ply of the transfer film facing away from the carrier ply. For this purpose, the transfer film is arranged in an injection mold and the injection mold is filled with at least the plastic composition. Furthermore, the injection mold can be formed from two mold halves, in particular the mold halves are opened before step b) and closed before step c), preferably forming the injection mold therein.
[0101] The substrate is formed of and includes a plastic composition. The plastic composition preferably includes a thermoplastic selected from polycarbonate (PC), polyethylene terephthalate (PET), polypropylene (PP), polymethyl methacrylate (PMMA), polyethylene naphthalate (PEN), polyamide (PA), acrylonitrile butadiene styrene copolymer (ABS), ABS / PC, PC / ABS and thermoplastic polyurethane (TPU) alone or in combination. The substrate can be formed as a single layer or multiple layers.
[0102] The substrate may also have a transmittance of at least 45%, preferably at least 70%, for the wavelength range perceptible to the human eye, preferably for the range from 400 nm to 700 nm. For example, a display or a light source can thus be perceived through the substrate. This provides the advantage that the produced article can be backlit.
[0103] After the plastic composition has cooled or after the substrate has been formed, the substrate and the transfer film are advantageously removed from the mold. In particular, the transfer film and / or the optional substrate are bonded to the substrate after step c). The transfer layer and / or the substrate can no longer be removed from the substrate in a non-destructive manner.
[0104] In step d), the carrier layer is peeled off from the transfer layer. Step d) is preferably performed before step e). In particular, step d) can be performed before step f) and before step g). In addition, step d) is preferably performed after step c). Step d) can be performed after step k3).
[0105] When the carrier layer is removed, the optional peeling layer can remain on the carrier layer or remain on the transfer layer. In addition, the peeling layer can also be separated in itself, so that after the carrier layer is removed, the residue of the peeling layer is arranged on the carrier layer and the transfer layer.
[0106] The post-injection molding of the transfer layer in step c) and the stripping of the carrier layer in step d) can also be carried out spatially separately. Here, the transfer layer bonded to the substrate can be temporarily stored and / or transported. In particular, the article can then be individualized by forming at least one first and / or second region at another production location.
[0107] In step k3) of step A3), the transfer film (in particular the transfer layer) is arranged on the surface of the substrate. In addition, the transfer film (preferably the transfer layer) is bonded to the surface of the substrate by means of hot stamping. Preferably, the transfer layer can no longer be removed from the substrate in a non-destructive manner. The transfer layer can also be arranged and / or arranged on the substrate partially or over the entire surface.
[0108] In step e), at least one first region and at least one second region are arranged in the protective lacquer layer and / or the printed layer. This is achieved by means of an embossing method (e.g. hot stamping, in particular roller embossing or piston embossing), preferably by contacting the protective lacquer layer and / or the printed layer with an embossing tool. For example, the embossing tool can have a primary structure on the surface that contacts the protective lacquer layer and / or the printed layer.
[0109] The primary structure on the surface of the embossing tool can be introduced, for example, by laser processing and / or by etching methods and / or by means of other known surface treatment methods.
[0110] In another embodiment variant, the carrier containing the main structure can be arranged at least partially between the embossing tool and the transfer layer and / or between the embossing tool and the printing layer. In other words, the embossing tool can have a carrier containing the main structure at least partially. In this case, the embossing tool preferably has no main structure and / or is smooth, and preferably only the contour of the embossing surface is predetermined as the outer contour, and one or more recesses within the outer contour may be predetermined as the inner contour of the embossing surface. Thus, the outer contour and preferably the inner contour of the embossing surface can be predetermined by the embossing tool.
[0111] Optionally, in addition to the main structure of the carrier, the embossing tool can have an additional main structure, wherein the main structure of the embossing tool and the main structure of the carrier then overlap in the protective lacquer layer and / or the printed layer, in particular in at least one first region. Here, the main structures of the embossing tool and the carrier are preferably different. For example, for this purpose, the main structure on the embossing tool has different dimensions than the main structure on the carrier. For example, the embossing tool predetermines a coarse structure in the millimeter to micrometer range and superimposes the main structure on the carrier as a fine structure in the micrometer to nanometer range, wherein the combined structure of the coarse structure and the fine structure is molded into the protective lacquer layer and / or the printed layer.
[0112] By bringing the embossing tool into contact with the protective lacquer layer and / or with the printed layer and / or with a carrier arranged therebetween, the main structure of the embossing tool or the carrier is at least partially molded in the protective lacquer layer and / or the printed layer, wherein a relief structure complementary to the main structure is formed in the protective lacquer layer and / or the printed layer, in particular in at least one first area.
[0113] In particular, the protective lacquer layer and / or the printed layer is in contact with the embossing tool or the carrier only in certain places, preferably only at those locations in the protective lacquer layer and / or the printed layer where the at least one first region is arranged.
[0114] The embossing tool and / or the carrier can also be designed such that the embossing tool and / or the carrier only partially has the primary structure, wherein the protective lacquer layer and / or the printed layer is in contact with the embossing tool and / or the carrier in such a way that the primary structure is in contact with the protective lacquer layer and / or the printed layer at the location where at least one first area is arranged in the protective lacquer layer and / or the printed layer. Alternatively or additionally, the area in the protective lacquer layer and / or the printed layer in which at least one second area is arranged can be covered with a particularly removable mask, for example a removable polymer film.
[0115] Step e) is preferably implemented using an embossing tool. For example, at least one embossing roller or at least one embossing wheel or at least one embossing punch and / or at least one carrier containing a primary structure can be used as an embossing tool.
[0116] On the surface in contact with the protective lacquer layer and / or the print layer, for example on its outer circumference, the embossing tool preferably has an elastomer coating, the layer thickness of which is selected from the range of 3 mm to 20 mm, preferably 5 mm to 15 mm. The elastomer is preferably silicone rubber. The elastomer preferably has a hardness selected from the range of 30 Shore A to 95 Shore A, preferably 60 Shore A to 90 Shore A. The optical properties of the relief structure of the at least one first area can be advantageously influenced by different Shore hardnesses.
[0117] Alternatively, the embossing tool can also have a surface made of metal, in particular a metal selected from the group of brass, copper, steel or titanium.
[0118] In each case, the embossing wheel preferably has a bevel on its circumference at the outer edge, wherein in particular, in each case the elastomer coating on the circumference at the outer edge has a bevel. The angle of the bevel relative to the surface normal of the circumference of the embossing wheel is preferably between 15° and 75°, more preferably between 25° and 65°. With such a bevel, a particularly clean embossed edge can be obtained. This means that for the naked human eye, the transition between a first region and an adjacent second region is largely smooth, largely straight and largely free of disruptive artifacts, in particular smooth, straight and largely free of disruptive artifacts.
[0119] The formation of the at least one first and second region is preferably effected at an embossing temperature (ie the temperature of the embossing tool) which is selected from the range of 125° C. to 250° C. This temperature range ensures a clear embossing of the relief structure without the layers of the carrier or transfer ply being damaged by the temperature.
[0120] Furthermore, the stamping speed, ie the advancing rate, has a value selected from the range of 1 m / min to 5 m / min.
[0121] The embossing pressure, in particular in the case of piston embossing, is preferably selected from the range of 0.1 kN to 25 kN, preferably 0.2 kN to 20 kN, particularly preferably 0.3 kN to 15 kN.
[0122] The embossing time, in particular in the case of piston embossing, is preferably selected from the range of 0.3 s to 2.5 s, preferably 0.5 s to 2.0 s, particularly preferably 1.0 s to 1.5 s, wherein the embossing time is preferably adapted to the layer thickness of the support.
[0123] Furthermore, the embossing pressure, in particular in the case of roller embossing, can also preferably be selected from the range of 10 kg / cm² to 50 kg / cm², preferably 15 kg / cm² to 30 kg / cm², particularly preferably 20 kg / cm² to 25 kg / cm².
[0124] In order to determine the embossing pressure of roller embossing, the embossing wheel or embossing roller is moved vertically downward onto the substrate (e.g., transfer layer). Then, the contact area formed there is measured, which is produced by squeezing the coating of the embossing wheel or embossing roller, such as silicone rubber. The contact area is affected by the hardness of the coating and the applied embossing pressure. In theory, in the case of very hard materials, the contact area only corresponds to the line contact between the embossing wheel or embossing roller and the substrate. The contact area thus produced is called "imprint". In the case of an embossing wheel or embossing roller with Shore A of 80, the preferred imprint is a strip of 20 mm to 25 mm width. In the case of Shore A of 60, the preferred imprint is a strip of 30 mm to 55 mm width. According to the width of the embossing wheel or embossing roller and the area thus produced, the force of the embossing wheel or embossing roller pressing on the substrate can be specified. The embossing pressure used is therefore advantageously given according to the load-bearing surface (especially in the case of roller embossing). If the load-bearing surface and the embossing pressure are known, they can also be converted into an embossing pressure in Newtons.
[0125] For example, if the width of the embossing wheel or roller is 100 mm and the width of the bearing surface is 25 mm, then you get 100 mm x 25 mm = 25 cm 2 For a target value of 25 kg / cm² and a load-bearing surface of 25 cm², this results in an embossing pressure of 625 N. The width of the embossing wheel is measured at its outermost circumference.
[0126] For example, in the case of embossing processes, in particular piston embossing, good results were obtained with a combination of an embossing temperature of 190° C., an embossing time of 1.5 s and an embossing pressure of 15 kN.
[0127] In the case of embossing processes, in particular by roller embossing, good results have been obtained, for example, with a combination of an embossing temperature of 185°C, an embossing speed of 2 m / min, an embossing pressure of 20 kg / cm² to 25 kg / cm² and using an embossing roller with a hardness of 80 Shore A.
[0128] In particular, the main structure has a structure depth selected from the range of 0.1 μm to 15 μm, preferably 0.1 μm to 10 μm, particularly preferably 0.1 μm to 5 μm. In particular, the main structure has an average structure spacing selected from the range of 0.05 μm to 1000 μm, preferably 0.1 μm to 100 μm, particularly preferably 0.1 μm to 50 μm.
[0129] The complementary relief structure can in particular have a smaller structure depth than the main structure. In particular, the complementary relief structure has a structure depth which preferably corresponds to 20% to 99%, particularly preferably to 40% to 95% of the structure depth of the main structure.
[0130] The structure depth is the distance between the maximum elevation and the minimum depression of the main structure when viewed perpendicularly to the plane spanned by the carrier with the main structure.
[0131] The structure spacing refers to the spacing between two adjacent minima of the depression when viewed perpendicular to the plane spanned by the carrier with the main structure.
[0132] The main structure or the complementary relief structure can have, alone or in combination, a regular one-dimensional grating, a regular two-dimensional grating, a random structure assembly or a pseudo-random structure assembly. In particular, the complementary relief structure can have an optical and / or functional effect.
[0133] Random relief structures can be produced, for example, with a support having an introduced surface roughness or introduced particles, for example with a matte or brushed support or with a support comprising a primary structure layer into which particles have been introduced. In particular, relatively undefined and rounded contour shapes are thereby produced.
[0134] A pseudo-random relief structure is understood to mean a relief structure which appears as a random relief structure in a partial view, but which can preferably be reproduced in a targeted manner at regular intervals and is therefore not recognizable as a random structure.
[0135] Preferred one-dimensional or two-dimensional gratings are non-random relief structures, which preferably have a precise and geometrically formed profile shape, such as a rectangular profile, a sinusoidal profile, a sawtooth profile, a hemispherical profile or a blazed structure. In addition, the one-dimensional or two-dimensional grating can have a binary profile or a profile whose profile depth is staggered in a stepped manner or a profile whose profile depth is constant.
[0136] It is advantageous if the primary structure is designed such that the complementary relief structure comprises microstructures, in particular microstructures having dimensions below the resolution limit of the human eye. The resolution limit of the human eye is preferably at structures having dimensions of at least 300 μm.
[0137] Furthermore, the primary structure can be designed such that the complementary relief structure comprises macrostructures, in particular macrostructures whose dimensions are above the resolution limit of the human eye.
[0138] Furthermore, the main structure can be designed such that the complementary relief structure is formed as a microstructure whose size is below the resolution limit of the human eye and additionally as a macrostructure visible to the human eye. The macrostructure can exist adjacent to the microstructure and / or can be superimposed with the microstructure.
[0139] Microstructures can advantageously have optical effects that simulate the presence of macrostructures.
[0140] The main structure can be designed so that the complementary relief structure is formed as a rough structure, a diffractive structure and / or a refractive structure and / or a macrostructure. In addition, several of the above structures can also exist adjacent to each other and / or overlap each other.
[0141] Diffractive structures are structures that form optical effects based on the diffraction of light, such as diffraction gratings or holograms. These can be conventional 2D / 3D or 3D holograms, which allow to present three-dimensional information based on the surface structure. From a local observation, the profile of a holographically generated hologram (e.g. a Fourier hologram) can be seen as approximately periodic, with a typical number of lines in the range of 300 lines / mm to 3000 lines / mm and a typical structure depth in the range of 50 nm to 1000 nm. However, for achromatic effects, very coarse grating structures with a line number in the range of 10 lines / mm to 300 lines / mm and a structure depth in the range of 0.5 µm to 10 µm can also be used.
[0142] Computer-generated holograms, such as so-called kinoform holograms, can create the impression of a random surface relief and have an asymmetric diffraction effect. The typical structure depth is half or a multiple of the wavelength of the incident light and is suitable for whether the kinoform hologram exerts its effect in transmission or reflection.
[0143] The rough structure is a diffraction structure with a random order, as a result of which the incident light is scattered in a random manner. The rough structure has fine relief structural elements on a microscopic scale, which determine the scattering power and can be described by statistical characteristic values. The average spacing, average roughness Ra and correlation length lc of the relief structural elements in the x and / or y directions of the plane spanned by the transfer film are examples of these characteristic values. The average spacing of the preferred rough structure is in the range of 300 nm to 5000 nm, and the average roughness Ra is in the range of 20 nm to 2000 nm, preferably in the range of 50 nm to 500 nm. The correlation length lc is preferably in the range of 200 nm to 50,000 nm, preferably in the range of 500 nm to 10,000 nm.
[0144] Refractive structures are structures that form optical effects based on light refraction and / or light reflection, such as microlenses or micromirrors. Such microlenses or micromirrors are not used alone, but are preferably arranged adjacent to each other in a regular or pseudo-random grid or pixel array.
[0145] The optically variable effect based on the aforementioned structure can be achieved, for example, by changing one or more structural parameters, such as by changing the grating period, the average structure pitch, the tilt angle of the micromirror, the structure depth and / or the azimuth angle.
[0146] Preferably, a support containing the master structure is used for a small number of imprints in the same area of the support surface, in particular selected from the range of 1 to 20, preferably 1 to 10. If the support is used for too many imprints, the accumulated contamination has a negative impact on the imprinting.
[0147] The advantage of using a regularly replaced carrier is that contamination of the master structure that accumulates during the imprinting process does not accumulate on the carrier, but rather, after a defined maximum number of imprints in the same area of the carrier surface, a new area of the carrier surface with an unused structure is immediately available. The new surface area is then, for example, cleaner and the master structure has the envisaged structure depth. This results in a consistently high-quality imprint.
[0148] When using embossing tools without carriers, it is important to remember that contamination can also accumulate over time, or that surfaces, such as elastomer surface coatings, can solidify over time. As a result, the quality of the relief structure introduced into the protective lacquer layer can also deteriorate here, and the embossing tool may need to be replaced, which is more expensive than replacing the carrier.
[0149] In particular, it is advantageous if at least 20%, preferably at least 40%, further preferably at least 50%, even further preferably at least 70% of the relief shape or surface structure of the primary structure (in particular the structure depth of the primary structure) is molded into and / or has been molded into the protective lacquer layer and / or printed layer. In the finished product, the envisaged relief structure thus has the desired optical properties.
[0150] A substrate can be provided and / or obtained, which has a surface facing or to face the transfer film and / or the optional substrate, and wherein at least one bevel (preferably a chamfer) has been arranged on this surface. At least one bevel (preferably a chamfer) has been arranged on at least one outer edge of the substrate.
[0151] The bevel preferably has an angle selected from the range of 15° to 75°, more preferably 25° to 65° relative to the surface normal of the plane formed by the surface of the substrate. The substrate preferably has bevels, preferably chamfers, on opposite edges.
[0152] When the transfer layer and / or the printing layer is arranged on the substrate, the transfer layer and / or the printing layer preferably adopts the contour of the substrate. The first area can be formed and / or has been formed on the inclined surface and on the plane formed by the surface of the substrate, in particular, in particular formed and / or has been formed without interruption.
[0153] The embossing tool, in particular the embossing wheel, can be made height-adjustable. The height adjustment of the embossing tool can be carried out by one or more servomotors or by pneumatic control. This provides the advantage of applying the same embossing pressure over the entire surface. Thus, a uniformly designed and interrupted first region can be formed.
[0154] Advantageously, the carrier containing the primary structure is provided in particular in a coil and can therefore be further transported as a carrier web. A particularly rapid change of the carrier surface area for embossing is possible here. It is also possible to provide and use a carrier comprising the primary structure in sheet form or as a plate. This can also be easily exchanged and can also be individualized as required. The carrier preferably consists of a polymer, for example PET, or comprises the polymer. The carrier preferably has a layer thickness selected from the range of 5 μm to 500 μm, preferably 20 μm to 50 μm.
[0155] Alternatively, the support may comprise or consist of a metal such as brass, copper, steel or titanium.
[0156] Preferably, the primary structure is introduced into the carrier during production of the carrier, in particular during extrusion of the carrier. This provides the advantage that the structure is able to withstand the temperatures of the embossing step.
[0157] For example, step e) may have at least one or more of the following sub-steps:
[0158] - Arrange and align the transfer film (preferably the transfer layer) and the substrate with respect to the embossing tool or the carrier;
[0159] -Heat the stamping tool to stamping temperature
[0160] - contacting the primary structure of the embossing tool or the carrier with the transfer layer, in particular the protective lacquer layer, in particular in at least one first region;
[0161] - Moving or rotating the imprinting tool or carrier.
[0162] Step e) is preferably carried out after step A1) and / or A2) and / or A3). Step e) is preferably carried out after step d), in particular before step f). Step e) can also be carried out multiple times, in particular using different or the same embossing tools or carriers containing the same or different primary structures.
[0163] In particular, in step e), at least one first region is formed such that the transfer ply has a relief structure in at least one first region, wherein the relief structure is preferably complementary to the primary structure of the embossing tool and / or the carrier used. The at least second region is preferably unstructured and is considered smooth and flat. In particular, the at least one first region differs from the at least one second region optically or functionally, in particular in its gloss or transmittance.
[0164] Preferably, at least one first region is formed only partially in the protective lacquer layer and / or printed layer when viewed perpendicularly to a plane spanned by the protective lacquer layer and / or printed layer. The protective lacquer layer and / or printed layer preferably has at least one first region only partially.
[0165] The at least one first region preferably consists of one or more regions that are adjacent and / or separated from one another, in particular when viewed perpendicularly to the plane spanned by the protective lacquer layer and / or the printed layer. For example, the at least one first region may completely surround the at least one second region, and / or the at least one first region may be completely surrounded by the at least one second region. The at least one first region and the at least one second region are arranged adjacent to one another and do not overlap, in particular when viewed perpendicularly to the plane spanned by the protective lacquer layer and / or the printed layer.
[0166] In particular, the design or shape of the at least one first area is selected from the group consisting of: graphics, letters, numbers, symbols, geometric figures, visually recognizable design elements, patterns, logos, codes and strip conductors, alone or in combination.
[0167] In particular, at least one first region is formed in the protective lacquer layer and / or the printed layer in exact register with respect to the transfer ply and / or the layer or element (preferably the decorative element and / or the functional element) of the substrate. For this purpose, for example, the protective lacquer layer and / or the printed layer can be masked so that the relief structure is formed only in the at least one first region which is not masked.
[0168] Registration accuracy refers to the position accuracy of two or more plies, components, areas and / or layers relative to each other. The registration accuracy is within a predetermined tolerance range, which should be as small as possible. At the same time, in order to improve process reliability and / or product quality, as well as to prevent counterfeiting, the registration accuracy of several plies, components, areas and / or layers relative to each other is an important feature. Position-accurate positioning can be achieved in particular by perceptible, preferably optically detectable registration marks. These registration marks can represent special individual plies, components, areas and / or layers, or they themselves are part of the plies, components, areas and / or layers to be positioned.
[0169] Furthermore, for the wavelength range perceptible to the human eye in at least one first region and / or at least one second region, preferably in the range of 400 nm to 700 nm, the transfer film and / or the printed layer and / or the protective lacquer layer of the article can have a transmittance of at least 45%, preferably at least 70%. For example, a display or a light source can thereby be perceived in at least one first region and / or at least one second region. This provides the advantage that the produced article can be backlit.
[0170] At least one first area of the print layer and / or insert and / or transfer film, in particular the protective lacquer layer or the article, can have a gloss value selected from the range of 1 GU to 59 GU, preferably 5 GU to 30 GU, or be designed in such a way.
[0171] At least one second area of the printed layer and / or insert and / or transfer film, in particular a second area of the protective lacquer layer or article, preferably without relief structure, can have a gloss value selected from the range of 31 GU to 98 GU, preferably 60 GU to 90 GU.
[0172] The gloss value can thus advantageously be set so that at least one first region and at least one second region differ from one another in an optically perceptible manner. In particular, due to the corresponding structure, very rough surfaces are thus also possible, which is not possible with other lacquers, in particular known structured protective lacquers.
[0173] The gloss value is measured with a "microgloss" meter from Byk-Gardener GmbH, Geretsried at a measuring angle of 60°. During the gloss measurement, a precisely defined directed light beam is directed, in particular, at an angle of 60°, for example, onto a paint surface such as a transfer film and / or a protective paint layer of an article, and an oppositely placed reflectometer measures how much light is reflected at an angle of 60° (grazing angle). The gloss is advantageously calibrated to 100 GU (gloss units) (= 100%) using a standard. The highest achievable gloss value is therefore preferably 100 GU. The gloss value is advantageously given in percentage (%). In this case, therefore, it is advantageous if the unit of the gloss value is a percentage (%). Therefore, the measured gloss value is preferably a value in the range of 0% to 100%. Therefore, the gloss unit is in particular a percentage value and the gloss unit represents in particular a percentage value.
[0174] Advantageously, said method for producing an article may conveniently further comprise the optional following step, which is particularly carried out after step e) and before step g):
[0175] f) curing the protective lacquer layer and / or the printed layer which has not yet been completely cured at least in places, wherein the protective lacquer layer and / or the printed layer is completely cured at least in places.
[0176] All curable components of the article are preferably completely cured in step f). Thus, after step f), the protective lacquer has a high chemical and mechanical resistance in all areas.
[0177] In particular, in step f), complete curing of the protective lacquer layer and / or the printed layer is carried out by means of high-energy electromagnetic radiation, in particular UV-irradiation, and / or by means of high-energy particle radiation, in particular electron beam radiation, and / or by curing the protective lacquer layer and / or the printed layer, preferably at a temperature in the range of 25°C to 180°C.
[0178] The irradiation is preferably carried out by means of high-energy electromagnetic radiation and / or high-energy particle radiation. The electromagnetic radiation is preferably UV radiation, in particular UV radiation in the wavelength range of 100 nm to 390 nm, preferably 200 nm to 380 nm, particularly preferably 200 nm to 300 nm. The particle radiation is preferably electron beam radiation.
[0179] For complete curing in step f), the protective lacquer layer and / or the printed layer is irradiated with an irradiation intensity selected from the range of 500 mW / cm² to 700 mW / cm². The UV dose is preferably selected from the range of 2000 mJ / cm² to 3500 mJ / cm². The irradiation is preferably carried out in a time selected from 1 s to 10 s, preferably 2 s to 6 s.
[0180] Due to the possibility of implementing step f) and / or due to the protective lacquer layer and / or printed layer which has not yet been completely cured, a number of advantages arise. Therefore, a transfer film (preferably a transfer ply) which has not yet been completely cured is more easily deformable than a transfer film (preferably a transfer ply) with a completely cured layer. Even in the case of bending, it is thus particularly ensured that the corresponding layer can be stretched without cracking and other adverse effects. If a deformation, in particular of the transfer film (preferably a transfer ply), has already been achieved, for example in an injection mold or during a deep-drawing process, the protective lacquer layer and / or printed layer can then be cured in order to achieve their final hardness and resistance.
[0181] The article produced using the method is obtained in step g), which comprises the transfer layer (especially the protective lacquer layer and / or the printed layer) and the base body, and optionally the substrate. Therefore, step g) is especially the last step of the method according to the invention and is preferably carried out according to step e) or after it.
[0182] The article preferably has a protective lacquer layer and / or a printed layer as the outermost surface. Preferably, no further layers are applied to the protective lacquer layer and / or the printed layer, wherein advantageously a high resistance of the outermost surface is ensured, in particular compared to the base body and / or the optional substrate.
[0183] The article preferably comprises (especially in the transfer film and / or the transfer ply of the insert) at least one decorative layer comprising at least one decorative element and / or at least one functional layer comprising (especially in the transfer film and / or the transfer ply of the insert) at least one functional element.
[0184] The articles produced according to the method of the invention can be used in a variety of fields. The articles produced can be used, for example, alone or in combination, as display windows, touch screen panels, panels, sunshades, coverings, covers, functional elements, electronic articles and housing parts or exterior parts, in particular for white goods and / or household appliances and / or automotive interiors and / or automotive exteriors.
[0185] The method steps can also be performed once or multiple times. In particular, the method steps can be repeated. Preferably, the method has at least the following steps: a), e) and g), optionally a), e), f) and g), wherein further steps can be inserted in particular between these steps.
[0186] For the IMD method, the method has in particular at least the following steps in the order: a1), b1), c1), d), e), g), optionally a1), b1), c1), d), e), f), g).
[0187] For the insert molding method, the method particularly has at least the steps in the following order: a2), b2, c2), e), g), optionally a2), b2, c2), e), f), g). Optionally, for the insert molding method, the method particularly has at least the steps in the following order: a1), h), d), b1), c1), e), g), optionally a1), h), d), b1), c1), e), f), g). The insert molding method may have at least the steps in the following order: a1), h), d), i), j), b1), c1), e), g), optionally a1), h), d), i), j), b1), c1), e), f), g).
[0188] For an injection molding process with a downstream hot stamping process, the method has in particular at least the following steps in the order: a3), k3), d), e), g), optionally a3), k3), d), e), f), g).
[0189] In particular, if the method for producing the article is an IMD method, it may comprise at least one or more of the following steps:
[0190] a1) providing a transfer film, wherein the transfer film comprises a carrier layer and a transfer layer, wherein the carrier layer is releasable from the transfer layer, wherein the carrier layer comprises a carrier layer, wherein the transfer layer comprises a protective lacquer layer, wherein the protective lacquer layer is at least partially not yet fully cured or is thermoplastic,
[0191] and wherein the protective lacquer layer has been arranged so that it is in contact with the carrier ply;
[0192] b1) arranging the transfer film, in particular the transfer layer, in an injection mold;
[0193] c1) post-injection molding of a transfer film, in particular a transfer layer, with the plastic composition, wherein the plastic composition forms the matrix;
[0194] d) peeling the carrier layer from the transfer layer;
[0195] e) forming at least one first region and at least one second region in the protective lacquer layer by means of embossing, wherein the at least one first region has a relief structure;
[0196] f) optionally curing the protective lacquer layer which has not yet been completely cured at least in places, wherein the protective lacquer layer is completely cured at least in places;
[0197] g) obtaining an article, wherein the article comprises a substrate and a protective lacquer layer, which is at least partially cured or thermoplastic, wherein the protective lacquer layer has at least one first region and at least one second region, wherein the relief structure is arranged in the at least one first region.
[0198] In particular, if the method for producing an article is an insert molding method, it may include at least one or more of the following steps:
[0199] a2) providing an insert, wherein the insert comprises a substrate and a transfer layer and / or a print layer arranged on the substrate, wherein the transfer layer comprises a protective lacquer layer, wherein the protective lacquer layer and / or the print layer is at least partially not yet fully cured or is thermoplastic;
[0200] b2) arranging the insert in the injection mold;
[0201] c2) post-injection molding of the insert with the plastic composition, wherein the plastic composition forms the matrix;
[0202] e) forming at least one first region and at least one second region in the protective lacquer layer and / or the printed layer by means of embossing, wherein the at least one first region has a relief structure;
[0203] f) optionally curing the protective lacquer layer which has not yet been completely cured at least in places, wherein the protective lacquer layer and / or the printed layer are completely cured at least in places;
[0204] g) obtaining an article, wherein the article comprises a substrate and a protective lacquer layer and / or a printed layer, wherein the protective lacquer layer and / or the printed layer is at least partially cured or thermoplastic, wherein the protective lacquer layer and / or the printed layer has at least one first area and at least one second area, wherein the relief structure is arranged in the at least one first area.
[0205] In particular, if the method for producing the article is an injection molding method with subsequent hot stamping, it may comprise at least one or more of the following steps:
[0206] a3) providing a transfer film, wherein the transfer film has a carrier layer and a transfer layer, wherein the carrier layer can be peeled off from the transfer layer, wherein the carrier layer comprises a carrier layer, wherein the transfer layer contains a protective lacquer layer, and wherein the protective lacquer layer has been arranged so that it is in contact with the carrier layer, wherein the protective lacquer layer is at least partially not yet fully cured or is thermoplastic.
[0207] and providing a base body separately from the transfer film, said base body being produced in particular by means of injection molding;
[0208] k3) arranging a transfer film, in particular a transfer layer, on the surface of the substrate, and hot stamping the transfer film onto the surface of the substrate;
[0209] d) peeling the carrier layer from the transfer layer;
[0210] e) forming at least one first region and at least one second region in the protective lacquer layer by means of embossing, wherein the at least one first region has a relief structure;
[0211] f) optionally curing the protective lacquer layer which has not yet been completely cured at least in places, wherein the protective lacquer layer is completely cured at least in places;
[0212] g) obtaining an article, wherein the article comprises a substrate and a protective lacquer layer, which is at least partially cured or thermoplastic, wherein the protective lacquer layer has at least one first region and at least one second region, wherein the relief structure is arranged in the at least one first region.
[0213] Of course, the above features can also be applied in a method in an equivalent manner, or the mentioned method features can also be applied in a product.
[0214] In the following, the invention is explained by reference to a number of embodiment examples with the aid of the accompanying drawings. Therefore, the embodiment examples shown should not be understood as limiting.
[0215] Figure 1 A schematic diagram of a transfer membrane suitable for use in this method is shown.
[0216] Figure 2 A schematic side view of an article obtained using this method is shown.
[0217] Figure 3a A schematic top view of an intermediate product obtained using this method is shown.
[0218] Figure 3b to Figure 3e A schematic top view of an article obtained using this method is shown.
[0219] Figure 1 An exemplary transfer film 2 is shown which is suitable for the method according to the invention and which can be provided in step a), preferably in step a1) and / or in step a3).
[0220] The transfer film 2 particularly comprises a transfer layer 3 and a carrier layer 4, wherein the transfer layer 3 can be peeled off from the carrier layer 4. The transfer layer 3 can be constructed as a single layer or multiple layers. Figure 1 The transfer ply 3 shown is single-layered and has a protective lacquer layer 8 which is preferably not yet completely cured at least in places or consists of a thermoplastic.
[0221] In step a), the transfer film 2 can be provided in the form of a roll. The transfer film 2 can also be provided as a hot stamping film or as an IMD film. The article 1 is preferably produced by an IMD method or an insert molding method.
[0222] Optionally, according to step a2), the insert can already be provided. In another alternative according to step a3), the substrate 9 can be provided separately. The provided insert can have a multi-layer transfer ply and / or a multi-layer printed layer. The printed layer is preferably arranged on the insert partially or over the entire surface. The printed layer is especially formed as a screen printing layer, a gravure printing layer, an inkjet printing layer or a combination thereof. The insert preferably has a gravure printing layer and a screen printing layer. The layers of the printed layer can at least partially overlap. The insert can have a transfer ply on which one or more printed layers have been partially printed.
[0223] The transfer ply 3 of the provided transfer film 2 preferably has a layer thickness selected from the range of 0.1 μm to 100 μm, preferably 0.5 μm to 75 μm, further preferably 1 μm to 50 μm.
[0224] The protective lacquer layer 8 protects the obtained article 1 in particular from external influences such as UV radiation, mechanical influences (such as scratches) or chemical influences (such as frost or solvents). The protective lacquer layer 8 thus has a particularly high resistance to mechanical and chemical stresses, in particular compared to the layers and / or substrate 9 located therebelow.
[0225] The protective lacquer layer 8 preferably has a layer thickness selected from the range of 1 μm to 15 μm, preferably 2 μm to 8 μm, further preferably 2 μm to 5 μm.
[0226] Furthermore, the protective lacquer layer 8 has in particular a transmittance of at least 70%, preferably at least 85%, for the wavelength range perceptible to the human eye, preferably for the range from 400 nm to 700 nm.
[0227] In particular, the protective lacquer layer 8 is at least partially not yet fully cured. Preferably, the protective lacquer layer 8 is at least partially already chemically precured and / or precured by radiation, preferably UV radiation, and / or is at least partially still fully curable by radiation, preferably UV radiation. For this purpose, the protective lacquer layer 8 comprises at least one UV-crosslinkable polymer. Within the meaning of the present invention, a UV-crosslinkable polymer preferably has at least one, preferably two or more, ethylenically unsaturated double bond.
[0228] The partially uncured protective lacquer layer 8 is preferably produced based on at least one UV-crosslinkable or at least one chemically crosslinkable polymer, alone or in combination. Furthermore, the protective lacquer layer 8 can be made of a thermoplastic polymer.
[0229] In a preferred embodiment, the protective lacquer layer 8 is formed as a printed layer, in particular a screen printed layer 8, a gravure printed layer, an inkjet printed layer or a combination thereof. Here, for the wavelength range perceptible to the human eye, preferably for the range of 400 nm to 700 nm, the protective lacquer layer 8 preferably has a transmittance of at most 30%, preferably at most 15%.
[0230] The protective lacquer layer is preferably arranged on the entire surface of the transfer ply 3. Alternatively, in an embodiment not shown here, the protective lacquer layer 8 can be arranged partially in the transfer ply 3. The protective lacquer layer 8 can have been formed as a multilayer, in particular wherein the layers of the protective lacquer layer 8 at least partially overlap.
[0231] In another embodiment not shown here, the printed layer can have been and / or will be arranged on the protective lacquer layer 8, in particular wherein the printed layer has not yet been fully cured at least in places. The printed layer is preferably already arranged partially or entirely on the surface on the protective lacquer layer and / or is preferably arranged partially or entirely on the surface on the protective lacquer layer. Furthermore, the printed layer, in particular the further printed layer, has been formed in particular as a screen printed layer, a gravure printed layer, an inkjet printed layer or a combination thereof, preferably as a screen printed layer.
[0232] The transfer ply 3 particularly preferably has at least one decorative layer comprising at least one decorative element 11 on that side of the protective lacquer layer 8 which faces away from the carrier ply 4 .
[0233] Furthermore, the at least one decorative element 11 comprised by the at least one decorative layer is preferably selected from the group consisting of: transparent and / or colored lacquer layers, in particular comprising one or more dyes and / or pigments, replication layers with a molded optically active surface structure, reflective layers (in particular opaque reflective layers, transparent reflective layers, metallic reflective layers or dielectric reflective layers), optically variable layers, optically active layers, interference multilayer systems, volume hologram layers, liquid crystal layers (in particular cholesteric liquid crystal layers), and combinations thereof.
[0234] Alternatively or additionally, the transfer ply 3 may have at least one functional layer comprising at least one functional element 10 on the side of the protective lacquer layer facing away from the carrier ply. Here, at least one functional layer may be arranged overlapping and / or adjacent to at least one decorative layer. At least one functional layer may also be arranged between at least two decorative layers, or at least one decorative layer may already be arranged on the side of the functional layer facing and / or facing away from the protective lacquer layer 8.
[0235] The at least one functional element 10 is in particular selected from the group comprising at least one electronic component (in particular a strip conductor, a contact element), an LED, a sensor (in particular a touch sensor, a temperature sensor, a pressure sensor), an antenna (in particular an RFID element), a memory, a control element, a display, a processor, a capacitor, a resistor, a microfluidic element and combinations thereof.
[0236] For example, the functional layer can be designed alone or in combination as a conductive layer, an antenna layer, an electrode layer, a magnetic layer, a magnetic storage layer or a barrier layer.
[0237] Preferably, at least one decorative element 11 has been arranged in at least one decorative layer and / or at least one functional element 10 has been arranged in at least one functional layer, which functional layers in each case independently of one another comprise a UV-crosslinked lacquer or a chemically crosslinked lacquer or a thermoplastically deformable layer and in each case independently of one another are uncolored or colored or dyed.
[0238] It is also conceivable that the protective lacquer layer 8 preferably has at least one decorative element 11 and / or functional element 10 , or is, for example, at least partially free of these elements.
[0239] Preferably, an adhesion promoter layer is arranged between the protective lacquer layer 8 and the at least one decorative element 11 and / or the at least one functional element 10. Here, the adhesion promoter layer can contain at least one acrylic resin or consist of at least one acrylic resin. The adhesion promoter layer can also preferably have a layer thickness in the range of 0.1 μm to 10 μm.
[0240] The transfer layer 3 may also have at least one lacquer layer, preferably with a layer thickness selected from the range of 0.5 μm to 10 μm, which forms the surface of the transfer layer 3 facing away from the carrier layer 4. The lacquer layer is preferably used for bonding to the substrate 9 or the plastic composition. The at least one lacquer layer preferably contains or consists of at least one adhesive selected from the group consisting of physically curing adhesives, chemically curing adhesives, pressure-sensitive adhesives or mixtures thereof. Furthermore, the at least one lacquer layer may be a primer layer and / or a primer layer arranged instead of the at least one lacquer layer and / or a primer layer arranged on the side of the at least one lacquer layer facing away from the protective lacquer layer 8, in particular wherein the primer layer comprises or consists of a PVC copolymer and PMMA.
[0241] Furthermore, the transfer ply 3 may have at least one or more of the following layers, selected in each case individually or in combination from: at least one colored lacquer layer, at least one metal layer, at least one oxide layer, at least one barrier layer, at least one receiving layer, at least one second protective lacquer layer, at least one replication layer, at least one laser protective lacquer layer. The layers may in each case be arranged over the entire surface or in each case partially in the transfer ply 3.
[0242] The carrier layer 7 of the transfer film 2 is provided with a carrier ply 4, which preferably consists of polyethylene terephthalate (PET), glycol-modified polyethylene terephthalate (PETG), polypropylene (PP), polycarbonate (PC), polyimide (PI) or polyamide (PA) and / or mixtures or copolymers thereof or contains said polymers, either alone or in combination. The carrier ply, preferably the carrier layer, preferably has a layer thickness selected from the range of 10 μm to 100 μm, preferably 10 μm to 50 μm.
[0243] The carrier layer 4 can have at least one release layer, which is preferably arranged between the carrier layer 7 and the protective lacquer layer 8. The layer thickness of the release layer is in particular in the range of 0.1 nm to 100 nm. The release layer preferably contains or consists of at least one wax, for example a polyethylene wax. The release layer preferably has a melting temperature in the range of 80° C. to 100° C. The carrier ply 4 is preferably arranged on the protective lacquer layer 8 with an adhesive force in the range of 2 cN to 50 cN, preferably in the range of 5 cN to 35 cN, or this force needs to be overcome when the carrier ply 4 is released.
[0244] In step a), preferably after the transfer film 2 has been provided in step a1), the next step of the method according to the invention is carried out, for example step b), in which the transfer ply 3 is arranged in an injection mold.
[0245] However, it is also conceivable that before step b), in particular before step d), the transfer film 2 is arranged on the substrate, shaped, preferably pre-deformed and / or deep-drawn and / or trimmed. Here, it is particularly advantageous if the protective lacquer layer 8 is at least partially not yet cured, since it has a much greater stretchability.
[0246] In other words, the method may further include at least one of the following steps h), i) and j):
[0247] h) arranging the transfer film 2 on the substrate;
[0248] i) forming the transfer film 2 and / or the substrate into a desired shape by applying heat and pressure; and
[0249] j) Trimming the transfer film 2 and / or the substrate along defined contour lines.
[0250] In particular, steps h), i) and j) can be carried out after step a), preferably step a1). Step h) is preferably carried out after step d). Steps i) and j) are preferably carried out after step d) and preferably before step b). It may also be appropriate to carry out steps i) and j) before step d), in particular if only slight shaping is carried out in step i).
[0251] In particular, the transfer film 2 is arranged on the substrate by means of embossing, in particular hot stamping or cold embossing. The transfer film 2 is preferably arranged by applying heat and / or pressure and / or irradiation with UV radiation.
[0252] In particular, the substrate is selected from polycarbonate (PC), polycarbonate / acrylonitrile butadiene styrene (PC / ABS), polypropylene (PP), thermoplastic polyurethane (TPU), polymethyl methacrylate (PMMA), or blends and / or co-extruded products thereof, alone or in combination.
[0253] In particular, the forming can be performed by deep drawing or vacuum forming, alone or in combination. The forming is preferably achieved by applying heat and / or pressure. In particular, the trimming can be performed by water jet cutting, laser or punching, alone or in combination.
[0254] The transfer ply 3 is arranged in an injection mold in step b) and is post-injected with a plastic composition in step c). Step b) is preferably carried out after step a) or after step j), in particular before step c). Step c) is preferably carried out before step d) and / or after step b). In particular, step c) can be carried out once or more, in particular with the same or different plastic compositions.
[0255] The injection mold advantageously has and / or predetermines the shape of the surface of the article 1. It is possible to obtain an article 1 which is a rigid body. The surface of the article 1, in particular the surface with the protective lacquer layer, can preferably be tortuous and / or curved.
[0256] In the case of post-injection molding of the transfer layer 3, in particular in step c), the transfer layer 3 or the optional substrate is preferably at least partially covered with a plastic composition at least on at least one surface of the transfer layer 3 of the transfer film 2 facing away from the carrier layer 4. For this purpose, the transfer film 2 is arranged in an injection mold and the injection mold is filled with at least the plastic composition. The injection mold can also be formed by two mold halves, in particular the two mold halves have been opened before step b) and closed before step c), preferably forming the injection mold therein.
[0257] The substrate 9 is formed of and includes a plastic composition. The plastic composition preferably includes a thermoplastic selected from polycarbonate (PC), polyethylene terephthalate (PET), polypropylene (PP), polymethyl methacrylate (PMMA), polyethylene naphthalate (PEN), polyamide (PA), acrylonitrile butadiene styrene copolymer (ABS), ABS / PC, PC / ABS, and thermoplastic polyurethane (TPU), either alone or in combination. The substrate 9 may be formed as a single layer or multiple layers.
[0258] The matrix 9 can also have a transmittance of at least 45%, preferably at least 70%, for the wavelength range perceptible to the human eye, preferably for the range from 400 nm to 700 nm. For example, a display or a light source can thus be perceived through the matrix 9.
[0259] After the plastic composition has cooled or after the base body 9 has been formed, the base body 9 and the transfer film 2 are advantageously removed from the mold. In particular, the transfer film 2 and / or the optional substrate are bonded to the base body 9 after step c). The transfer layer and / or the substrate can no longer be removed from the base body in a non-destructive manner.
[0260] In an alternative embodiment, step k3) is performed instead of step c). Here, the transfer film 2, in particular the transfer ply 3, is arranged on the surface of the substrate 9 provided in step a3). In addition, the transfer film 2, preferably the transfer ply 3, is bonded to the surface of the substrate 9 by means of hot stamping. Preferably, the transfer ply 3 can no longer be removed from the substrate 9 in a non-destructive manner. The transfer ply 3 can also be arranged and / or already arranged on the substrate 9 partially or over the entire surface.
[0261] In step d), the carrier layer is peeled off from the transfer layer. Step d) is preferably performed before step e). In particular, step d) can be performed before step f) and before step g). In addition, step d) is preferably performed after step c). Step d) can be performed after step k3).
[0262] When the carrier layer 4 is removed, the optional release layer can remain on the carrier layer 4 or on the transfer layer 3. In addition, the release layer can also separate internally, so that after the carrier layer 4 is removed, the remnants of the release layer are arranged on the carrier layer 4 and the transfer layer 3.
[0263] The post-injection molding of the transfer layer 3 in step c) and the peeling off of the carrier layer 4 in step d) can also be carried out spatially separately. Here, the transfer layer 3 combined with the base body 9 can be temporarily stored and / or transported. In particular, at another production location, the product 1 can be individualized by forming at least one first area 5 and at least one second area 6.
[0264] In step e), at least one first region 5 and at least one second region 6 are formed in the protective lacquer layer 8 and / or the printed layer. This is achieved by means of an embossing method, such as hot stamping, in particular roller embossing or piston embossing, preferably by contacting the protective lacquer layer 8 and / or the printed layer with an embossing tool 13. The embossing tool 13 can have a primary structure on the surface that is in contact with the protective lacquer layer 8 and / or the printed layer.
[0265] The primary structure on the surface of the embossing tool 13 can be introduced, for example, by laser machining and / or by etching methods and / or by other known surface treatment methods.
[0266] In another embodiment variant, the carrier containing the main structure can be arranged at least partially between the embossing tool 13 and the transfer layer 3 and / or between the embossing tool 13 and the printing layer. In other words, the embossing tool 13 can have a carrier containing the main structure at least partially. In this case, the embossing tool 13 preferably has no main structure and / or is smooth, and preferably only the contour of the embossing surface is predetermined as the outer contour, and one or more recesses inside the outer contour can be predetermined as the inner contour of the embossing surface.
[0267] Optionally, the embossing tool 13 may have an additional main structure in addition to the main structure of the carrier, wherein the main structure of the embossing tool 13 and the main structure of the carrier then overlap in the protective lacquer layer and / or the printed layer, in particular in at least one first region. Here, the main structures of the embossing tool 13 and the carrier are preferably different. For example, for this purpose, the main structure on the embossing tool 13 has different dimensions than the main structure on the carrier. For example, the embossing tool 13 predetermines a coarse structure in the millimeter to micrometer range and superimposes the main structure on the carrier as a fine structure in the micrometer to nanometer range, wherein the combined structure of the coarse structure and the fine structure is molded in the protective lacquer layer and / or in the printed layer.
[0268] By bringing the embossing tool 13 into contact with the protective lacquer layer 8 and / or the printed layer and / or the carrier arranged therebetween, the main structure of the embossing tool 13 or the carrier is at least partially molded in the protective lacquer layer 8 and / or the printed layer, wherein a relief structure complementary to the main structure is formed in the protective lacquer layer 8 and / or the printed layer, in particular in at least one first area 5.
[0269] In particular, the protective lacquer layer 8 and / or the printed layer is in contact with the embossing tool 13 or the carrier only in certain places, preferably only at those locations where the at least one first region 5 is arranged in the protective lacquer layer 8 and / or the printed layer.
[0270] The embossing tool 13 and / or the carrier can also be designed so that the embossing tool 13 and / or the carrier only partially has the main structure, wherein the protective lacquer layer 8 and / or the printed layer is brought into contact with the embossing tool 13 and / or the carrier, i.e. the main structure is brought into contact with the protective lacquer layer 8 and / or the printed layer at the location where at least one first area 5 is arranged in the protective lacquer layer 8 and / or the printed layer. Alternatively or additionally, the area in the protective lacquer layer 8 and / or the printed layer in which at least one second area 6 is arranged can be covered with a particularly removable mask, for example a removable polymer film.
[0271] Step e) is preferably carried out using an embossing tool 13. For example, at least one embossing roller or at least one embossing wheel or at least one embossing tool and / or at least one carrier containing a primary structure can be used as embossing tool 13.
[0272] On the surface in contact with the protective lacquer layer 8 and / or the print layer, for example on its outer circumference, the embossing tool 13 preferably has an elastomer coating with a layer thickness selected from the range of 3 mm to 20 mm, preferably 5 mm to 15 mm. The elastomer is preferably silicone rubber. The elastomer preferably has a hardness selected from the range of 30 Shore A to 95 Shore A, preferably 60 Shore A to 90 Shore A. The optical properties of the relief structure of the at least one first area 5 can be advantageously influenced by different Shore hardnesses.
[0273] Alternatively, the embossing tool 13 can also have a surface made of metal, in particular a metal selected from the group of brass, copper, steel or titanium.
[0274] In each case, the embossing wheel preferably has a bevel on its circumference at the outer edge, wherein in particular, in each case, the elastomer coating on the circumference at the outer edge has a bevel. The angle of the bevel relative to the surface normal of the circumference of the embossing wheel is preferably between 15° and 75°, more preferably between 25° and 65°. With such a bevel, a particularly clean embossed edge can be obtained. This means that, to the naked eye, the transition between the first region 5 and the adjacent second region 6 is largely smooth, largely straight and largely free of disruptive artifacts, in particular smooth, straight and largely free of disruptive artifacts.
[0275] The formation of the at least one first region 5 and the at least one second region 6 is preferably effected at an embossing temperature, ie the temperature of the embossing tool 13 , which is selected from the range of 125° C. to 250° C.
[0276] Furthermore, the stamping speed, ie the advancing speed, has a value selected from the range of 1 m / min to 5 m / min.
[0277] The embossing pressure, in particular in the case of piston embossing, is preferably selected from the range of 0.1 kN to 25 kN, preferably 0.2 kN to 20 kN, particularly preferably 0.3 kN to 15 kN.
[0278] The embossing time, in particular in the case of piston embossing, is preferably selected from the range of 0.3 s to 2.5 s, preferably 0.5 s to 2.0 s, particularly preferably 1.0 s to 1.5 s. In particular, the embossing time is preferably adapted to the layer thickness of the support.
[0279] Furthermore, the embossing pressure, in particular in the case of roller embossing, can also preferably be selected from the range of 10 kg / cm² to 50 kg / cm², preferably 15 kg / cm² to 30 kg / cm², particularly preferably 20 kg / cm² to 25 kg / cm².
[0280] For example, in the case of embossing processes, in particular piston embossing, good results were obtained with a combination of an embossing temperature of 190° C., an embossing time of 1.5 s and an embossing pressure of 15 kN.
[0281] In the case of embossing processes, in particular by roller embossing, good results have been obtained, for example, with a combination of an embossing temperature of 185°C, an embossing speed of 2 m / min, an embossing pressure of 20 kg / cm² to 25 kg / cm² and using an embossing roller with a hardness of 80 Shore A.
[0282] In particular, the main structure has a structure depth selected from the range of 0.1 μm to 15 μm, preferably 0.1 μm to 10 μm, particularly preferably 0.1 μm to 5 μm. In particular, the main structure has an average structure spacing selected from the range of 0.05 μm to 1000 μm, preferably 0.1 μm to 100 μm, particularly preferably 0.1 μm to 50 μm.
[0283] The complementary relief structure can in particular have a smaller structure depth than the main structure. In particular, the complementary relief structure has a structure depth which preferably corresponds to 20% to 99%, particularly preferably to 40% to 95% of the structure depth of the main structure.
[0284] The main structure or the complementary relief structure can have, alone or in combination, a regular one-dimensional grating, a regular two-dimensional grating, a random structure assembly or a pseudo-random structure assembly. In particular, the complementary relief structure can have an optical and / or functional effect.
[0285] Preferred one-dimensional or two-dimensional gratings are non-random relief structures, which preferably have a precise and geometrically formed profile shape, such as a rectangular profile, a sinusoidal profile, a sawtooth profile, a hemispherical profile or a blazed structure. In addition, the one-dimensional or two-dimensional grating can have a binary profile or a profile with a profile depth that is staggered in a stepped manner or a profile with a constant profile depth.
[0286] It is advantageous if the primary structure is designed such that the complementary relief structure comprises microstructures, in particular microstructures having dimensions below the resolution limit of the human eye. The resolution limit of the human eye is preferably at structures having dimensions of at least 300 μm.
[0287] Furthermore, the primary structure may be designed such that the complementary relief structure comprises large structures, in particular large structures having a size above the resolution limit of the human eye.
[0288] Furthermore, the main structure can be designed such that the complementary relief structure is formed as a microstructure whose size is below the resolution limit of the human eye and additionally as a macrostructure visible to the human eye. The macrostructure can exist adjacent to the microstructure and / or can be superimposed with the microstructure.
[0289] Microstructures can advantageously have optical effects that simulate the presence of macrostructures.
[0290] The main structure can be designed so that the complementary relief structure is formed as a rough structure, a diffractive structure and / or a refractive structure and / or a macrostructure. In addition, several of the above structures can also exist adjacent to each other and / or overlap each other.
[0291] The optically variable effect based on the aforementioned structure can be achieved, for example, by changing one or more structural parameters, such as by changing the grating period, the average structure pitch, the tilt angle of the micromirror, the structure depth and / or the azimuth angle.
[0292] Preferably, a small number of imprints (in particular selected from the range of 1 to 20, preferably 1 to 10) are carried out in the same area of the surface of the support using the support containing the master structure.
[0293] In particular, it is advantageous if at least 20%, preferably at least 40%, further preferably at least 50%, even further preferably at least 70% of the relief shape or surface structure of the primary structure (in particular the structure depth of the primary structure) is molded into and / or has been molded into the protective lacquer layer 8 and / or the printed layer. In the finished product, the envisaged relief structure thus has the desired optical properties.
[0294] Advantageously, the carrier containing the primary structure is provided in particular in a roll and can therefore be further transported as a carrier web. A particularly rapid change of the carrier surface area for embossing is possible here. It is also possible to provide and use a carrier comprising the primary structure in sheet form or as a plate. The carrier preferably consists of or comprises a polymer, for example PET. The carrier preferably has a layer thickness selected from the range of 5 μm to 500 μm, preferably 20 μm to 50 μm.
[0295] Alternatively, the support may comprise or consist of a metal such as brass, copper, steel or titanium.
[0296] For example, step e) may have at least one or more of the following sub-steps:
[0297] - Arrange and align the transfer film 2 (preferably the transfer layer 3 ) and the substrate 9 in relation to the embossing tool 13 or the carrier;
[0298] - Heating the embossing tool 13 to the embossing temperature
[0299] - bringing the embossing tool 13 or the main structure of the carrier into contact with the transfer ply 3 , in particular the protective lacquer layer 8 , in particular in at least one first region 5 ;
[0300] - Moving or rotating the embossing tool 13 or the carrier.
[0301] Step e) is preferably carried out after step d), in particular before step f). Step e) can also be carried out several times, in particular using different or the same embossing tools 13 or carriers comprising the same or different primary structures.
[0302] In particular, in step e), at least one first region 5 is formed such that the transfer ply 3 has a relief structure in at least one first region 5, wherein the relief structure is preferably complementary to the primary structure of the embossing tool 13 and / or the carrier used. At least the second region 6 is preferably unstructured and perceived as smooth and flat. In particular, the at least one first region 5 differs from the at least one second region optically or functionally, in particular in its gloss or transmittance.
[0303] When viewed perpendicularly to the plane spanned by the protective lacquer layer 8 and / or the printed layer, at least one first region 5 is preferably formed only partially in the protective lacquer layer 8 and / or the printed layer. The protective lacquer layer 8 and / or the printed layer preferably has at least one first region 5 only partially.
[0304] The at least one first region 5 preferably consists of one or more regions that are adjacent and / or separated from one another, in particular when viewed perpendicularly to the plane spanned by the protective lacquer layer 8 and / or the printed layer. For example, the at least one first region 5 may completely surround the at least one second region 6, and / or the at least one first region 5 may be completely surrounded by the at least one second region 6. The at least one first region 5 and the at least one second region 6 are arranged adjacent to one another and do not overlap, in particular when viewed perpendicularly to the plane spanned by the protective lacquer layer 8 and / or the printed layer.
[0305] In particular, the design or shape of the at least one first area 5 is selected, alone or in combination, from the group consisting of: graphics, letters, numbers, symbols, geometric figures, visually recognizable design elements, patterns, logos, codes and strip conductors.
[0306] In particular, at least one first region 5 is formed in the protective lacquer layer 8 and / or the printed layer in exact register with respect to layers or elements of the transfer ply 3 and / or the substrate 9, in particular in exact register with respect to the modifying elements 11 and / or the functional elements 10 arranged in the transfer ply 3 and / or the substrate 9. For this purpose, for example, the protective lacquer layer 8 and / or the printed layer can be masked so that the relief structure is formed only in the at least one first region 5 which is not masked.
[0307] The transfer film 2 and / or the protective lacquer layer 8 and / or the printed layer of the article 1 can also have a transmittance of at least 45%, preferably at least 70%, in at least one first region 5 and / or at least one second region 6 for a wavelength range perceptible to the human eye, preferably for a range of 400 nm to 700 nm.
[0308] The print layer, insert and / or transfer film 2 , in particular the protective lacquer layer 8 or the at least one first region 5 of the article 1 can have a gloss value selected from the range of 1 GU to 59 GU, preferably 5 GU to 30 GU, or be designed in this way.
[0309] Preferably, the at least one second area 6 of the printed layer, insert and / or transfer film 2 , in particular the protective lacquer layer 8 or the at least one second area 6 of the article 1 , without relief structure, may have a gloss value selected from the range of 31 GU to 98 GU, preferably 60 GU to 90 GU.
[0310] Advantageously, the method for producing the article 1 may also conveniently comprise the following optional steps, which are particularly carried out after step e) and before step g):
[0311] f) curing the protective lacquer layer 8 and / or the printed layer which has not yet been completely cured at least in places, wherein the protective lacquer layer 8 and / or the printed layer is completely cured at least in places.
[0312] All curable components of the article 1 are preferably completely cured in step f). Thus, after step f), the protective lacquer layer and / or the printed layer has a high chemical and mechanical resistance in all areas.
[0313] In particular, in step f), complete curing of the protective lacquer layer 8 and / or the printed layer is carried out by means of high-energy electromagnetic radiation, in particular UV radiation, and / or by means of high-energy particle radiation, in particular electron beam radiation, and / or by curing the protective lacquer layer 8 and / or the printed layer, preferably at a temperature in the range of 25°C to 180°C.
[0314] The irradiation is preferably carried out by means of high-energy electromagnetic radiation and / or high-energy particle radiation. The electromagnetic radiation is preferably UV radiation, in particular UV radiation in the wavelength range of 100 nm to 390 nm, preferably 200 nm to 380 nm, particularly preferably 200 nm to 300 nm. The particle radiation is preferably electron beam radiation.
[0315] For complete curing in step f), the protective lacquer layer 8 and / or the printed layer is irradiated with an irradiation intensity selected from the range of 500 mW / cm² to 700 mW / cm². The UV dose is preferably selected from the range of 2000 mJ / cm² to 3500 mJ / cm². The irradiation is preferably carried out for a time selected from 1 s to 10 s, preferably 2 s to 6 s.
[0316] In step g) the article 1 produced using the method is obtained. Step g) is therefore in particular the last step of the method according to the invention and is preferably carried out after one of steps e) or one of the other optional steps.
[0317] A schematic diagram of the layer structure of an exemplary article 1 is shown in Figure 2 The article 1 has a transfer film 2 (eg, according to Figure 1 At least one protective lacquer layer 8 and / or printed layer of the transfer layer sheet 3 of the transfer film).
[0318] Alternatively, the article 1 has an insert provided according to step a2), wherein the insert has a substrate and a transfer ply 3 arranged on the substrate and / or the print layer, and wherein the transfer ply 3 comprises a protective lacquer layer 8.
[0319] The protective lacquer layer 8 and / or the printed layer are preferably at least partially cured or thermoplastic and represent the surface of the article 1 facing the observer. The article 1 also has a substrate 9, which is formed in step c) by post-injection molding of the transfer ply 3 with a plastic composition. In an alternative embodiment, the substrate 9 is provided in step a2). The substrate 9 has been arranged on the side of the transfer ply 3 or the insert facing away from the observer. In addition, the protective lacquer layer 8 and / or the printed layer of the article 1 has at least one first area 5 and at least one second area 6, which are formed in the protective lacquer layer 8 and / or the printed layer in step e) of the method. A relief structure has been formed in at least one first area 5.
[0320] The article 1 may also preferably have at least one decorative layer comprising at least one decorative element 11, in particular in a transfer film 2 or a transfer layer 3 of an insert, and / or at least one functional layer comprising at least one functional element 10, in particular in a transfer film 2 or a transfer layer 3 of an insert.
[0321] The article 1 produced according to the method of the invention can be used in a large number of areas. The produced article 1 can be used, for example, alone or in combination as display windows, touch screen panels, panels, sunshades, coverings, covers, functional elements, electronic products and housing parts or exterior parts, in particular for white goods and / or household appliances and / or automotive interior areas and / or automotive exterior areas.
[0322] When carrying out the method according to the invention, the method steps can be carried out once or several times. In particular, the method steps can be repeated. Preferably, the method has at least the following steps: a), e) and g), preferably a), e), f) and g), wherein further steps can be inserted in particular between these steps.
[0323] For the IMD method, the method has in particular at least the following steps in the order: a1), b1), c1), d), e), g), optionally a1), b1), c1), d), e), f), g).
[0324] For the insert molding method, the method particularly has at least the steps in the following order: a2), b2, c2), e), g), optionally a2), b2, c2), e), f), g). Optionally, for the insert molding method, the method particularly has at least the steps in the following order: a1), h), d), b1), c1), e), g), optionally a1), h), d), b1), c1), e), f), g). The insert molding method may have at least the steps in the following order: a1), h), d), i), j), b1), c1), e), g), optionally a1), h), d), i), j), b1), c1), e), f), g).
[0325] For an injection molding method with downstream hot stamping, the method in particular has at least the following steps in the order: a3), k3), d), e), g), optionally a3), k3), d), e), f), g).
[0326] Figure 3a A schematic intermediate product of the method for producing the article 1 is shown, wherein the intermediate product is viewed perpendicularly to the plane spanned by the protective lacquer layer 8. The surface of the protective lacquer layer 8 thus faces the observer, wherein it is preferably at least partially not yet fully cured.
[0327] Figure 3a An intermediate product is shown in the method in which step e), i.e. the formation of at least one first region 5 and a second region 6, has not yet been carried out. The intermediate product preferably has a base body 9. In other words, step c) or step k3) of the method has already been carried out. The intermediate product has, for example, Figure 1 The transfer layer 3 and / or may have a layer structure such as the above with respect to Figure 2 The intermediate product may also have an insert.
[0328] In this embodiment example, for the production of an intermediate product, a transfer ply 3 is provided, which has a decorative element 11 in the form of two dotted circles on the left and a decorative element 11 in the form of a circle interrupted by a line in the upper left corner. Three further decorative elements 11 in the form of circles interrupted by a line have been arranged on the right side of the article 1. Functional elements 10 have been arranged in the transfer ply 3 or the substrate 9, preferably in precise registration with respect to the above-mentioned decorative elements 11. The functional element 10 can be designed as a control element, for example. Another functional element 10 in the form of a display is arranged on the right-hand side. The display can be arranged below the transparent protective lacquer layer 8, or has been arranged to replace the protective lacquer layer 8.
[0329] If step e) of the method is now carried out, at least one first region 5 and at least one second region 6 are formed, wherein the at least one first region 5 has a relief structure. In this connection, Figure 3b to Figure 3d Different articles 1 are shown, such as can be made using the method according to the invention according to Figure 2 In particular, a flexible layout design resulting from the method of the invention is presented hereby. All articles 1 have in common the fact that they have at least one first area 5 and at least one second area 6, wherein at least one first area 5 has a relief structure, for example a matte finish. Figure 3e of products using slightly modified intermediate products, which are Figure 3a The intermediate product of is different in that it does not have the design element 11 in the form of a dotted circle, but is otherwise designed identically.
[0330] according to Figure 3b to Figure 3e An embodiment variant of the article 1 is, for example, a control panel of a household appliance, which is preferably decorated with an IMD film in a high-gloss manner, preferably with a glossiness selected from the range of 85 GU to 95 GU. In at least one second area 6, in which no relief structure is replicated and / or in which a display window is arranged, the protective lacquer layer is therefore still high-gloss. At least the protective lacquer layer 8 and / or the substrate 9 of the obtained article 1 have been appropriately formed to be transparent. Due to the introduced relief structure, at least one first area 5 is preferably perceived as matte, preferably with a glossiness selected from the range of 1 GU to 30 GU. The entire protective lacquer layer 8 has a high chemical and mechanical resistance.
[0331] In accordance with Figure 3b In a variant embodiment of the article 1, the surface of the article is divided into at least one first area 5 and at least one second area 6 independently of the decorative element 11. As a result, a control area is formed on the left and a display area is formed on the right. The control area is composed of the at least one first area 5 and the display area is composed of the at least one second area 6.
[0332] In accordance with Figure 3c In the article 1 , by introducing a relief structure in at least one first area 5 , only a single decorative element 10 or functional element 11 of the transfer layer 3 is deposited, preferably in optically exact register relative to at least one second area 6 .
[0333] according to Figure 3d Products 1 and according to Figure 3c However, all design elements 11 of the transfer layer 3 are provided with at least one corresponding first area 5. The first area 5 is preferably arranged in exact register with respect to the design element 11 and is completely surrounded by at least one second area 6.
[0334] Another design variation of product 1 is as follows Figure 3e As shown. The product 1 is similar to Figure 3a to Figure 3dAn article of manufacture 1 having design elements 11 and functional elements 10, such as control elements and displays, arranged in a transfer film 3. However, the circular first area 5 has been arranged so that it is not arranged in precise registration relative to the design element 11, but only relative to the functional element 10. Due to this design, the functional element 10 of the article 1 can be optically emphasized and made recognizable to the observer without the presence of a corresponding decorative element 11 in the transfer layer 3. In addition, by a further step e), at least one further first area 5 can be arranged in the area in which the functional element 10 in the form of a display is arranged, the first area 5 having a further relief structure different from the first at least one first area 5. For example, the relief structure can provide an "anti-glare" effect to improve the readability of the display.
[0335] Another design variation of product 1 is as follows Figure 4a and Figure 4b As shown. The product 1 is similar to Figure 3a to Figure 3d An article 1 having design elements 11 and functional elements 10, such as control elements and displays, arranged in a transfer film 3. However, on two opposite sides, the article 1 has a bevel which is approximately 15° relative to the other (horizontal, flat) surface of the article 1 in the example shown. The boundary between the bevel and the other surface of the article 1 is indicated by a dotted line. The first area 5 has been arranged on the flat surface and the bevel 12 of the article 1 so that the first area 5 is arranged uninterruptedly between the opposite outer edges of the article 1. According to Figure 4a and Figure 4b A side view of the product 1 is shown in Figure 4c , in order to show by way of example how the first region 5 is arranged by means of an embossing tool 13. Corresponding to the contour of the article with the lower inclined surface 12 and the upper flat surface, the embossing tool 13, here an embossing wheel, is accordingly made height-adjustable, as a result of which approximately the same embossing pressure can be applied to all regions of the article 1 to produce uniformly produced and uninterrupted first regions 5. The height adjustment can be achieved by one or more servomotors or via pneumatic control. Figure 4c Schematically shown are the positions of the embossing tool 13 or its rotation axis during embossing of a flat surface of the article 1 and possible positions of the embossing tool 13 ′ or its rotation axis during embossing of an underlying inclined surface 12 depending on the contour of the article 1 .
[0336] Of course, the listed embodiment variants can be combined with one another as desired and do not represent a limitation.
[0337] Reference Number List
[0338] 1 product
[0339] 2. Transfer film
[0340] 3 transfer layers
[0341] 4 carrier layers
[0342] 5First Area
[0343] 6Second Area
[0344] 7 Carrier layer
[0345] 8 Protective paint layer
[0346] 9 Matrix
[0347] 10 Functional elements
[0348] 11Decorative elements
[0349] 12 bevels
[0350] 13,13′ embossing tool
Claims
1. A method for producing an article (1), wherein the method comprises at least one of steps A1) or A2) or A3), Step A1) The following steps are involved: a1) providing a transfer film (2), wherein the transfer film (2) comprises a carrier layer (4) and a transfer layer (3), wherein the carrier layer (4) is releasable from the transfer layer (3), wherein the carrier layer (4) comprises a carrier layer (7), wherein the transfer layer (3) comprises a protective lacquer layer (8), and wherein the protective lacquer layer (8) is arranged such that it is in contact with the carrier layer (4); b1) arranging the transfer film (2), in particular the transfer layer (3), in an injection mold; c1) post-injection molding of a transfer film (2), in particular the transfer layer (2), with a plastic composition, wherein the plastic composition forms a matrix (9); d) peeling the carrier layer (4) from the transfer layer (3); Wherein step A2) comprises the following steps: a2) providing an insert, wherein the insert comprises a substrate and a transfer ply (3) arranged on the substrate and / or a print layer arranged, wherein the transfer ply (3) comprises a protective lacquer layer (8); b2) arranging the insert in the injection mold; c2) post-injection molding of the insert with a plastic composition, wherein the plastic composition forms the base body (9); Wherein step A3) comprises the following steps: a3) providing a transfer film (2), wherein the transfer film (2) comprises a carrier layer (4) and a transfer layer (3), wherein the carrier layer (4) is releasable from the transfer layer (3), wherein the carrier layer (4) comprises a carrier layer (7), wherein the transfer layer (3) comprises a protective lacquer layer (8), and wherein the protective lacquer layer (8) is arranged such that it is in contact with the carrier layer (4), and providing a base body (9) separately from the transfer film (2), said base body being produced in particular by means of injection molding; k3) arranging a transfer film (2), in particular a transfer layer (3), on the surface of the substrate (9), and hot stamping the transfer film (2) onto the surface of the substrate (9); d) peeling the carrier layer (4) from the transfer layer (3); wherein the protective lacquer layer (8) and / or the printed layer is at least partially not yet fully cured or is thermoplastic in step A1) or A2) or A3), And wherein in addition to at least one of step A1) or A2) or A3), the method further comprises the following steps: e) forming at least one first region (5) and at least one second region (6) in the protective lacquer layer (8) and / or the printed layer by means of embossing, wherein the at least one first region (5) has a relief structure; f) optionally curing the protective lacquer layer (8) and / or the printed layer which has not yet been fully cured at least in places, wherein the protective lacquer layer (8) is at least partially fully cured; g) obtaining an article (1), wherein the article (1) comprises a substrate (9) and a protective lacquer layer (8) and / or a printed layer, wherein the protective lacquer layer (8) and / or the printed layer is at least partially cured or thermoplastic, wherein the protective lacquer layer (8) and / or the printed layer has at least one first region (5) and at least one second region (6), wherein a relief structure is arranged in the at least one first region (5).
2. The method according to claim 1, Features The method further comprises at least one of the following steps h), i) and j): h) arranging the transfer film (2) on a substrate; i) forming the transfer film (2) and / or the substrate into a desired shape; as well as j) trimming the transfer film (2) and / or the substrate along a defined contour line.
3. The method according to claim 1, Features In step f), the complete curing of the protective lacquer layer (8) and / or the printed layer is carried out by means of high-energy electromagnetic radiation, in particular UV radiation, and / or by means of high-energy particle radiation, in particular electron beam radiation, and / or by means of curing of the protective lacquer layer (8) and / or the printed layer, preferably at a temperature in the range of 25°C to 180°C.
4. The method according to claim 1, Features Step f) is selected from 500 mW / cm 2 Up to 700mW / cm 2 The irradiation intensity is carried out in the range of , and / or the UV dose is preferably selected from 2000 mJ / cm 2 Up to 3500mJ / cm 2 , and / or the irradiation is performed within a time period selected from the range of 1 s to 10 s, in particular 2 s to 6 s.
5. The method according to claim 1, Features The transfer ply ( 3 ) is provided in such a way that the protective lacquer layer ( 8 ) which has not yet been cured in places contains at least one UV-crosslinkable and / or at least chemically crosslinkable polymer.
6. The method according to claim 5, Features The at least one chemically cross-linkable polymer is selected from the group consisting of isocyanate group-containing polymers, melamine-containing polymers, hydroxyl group-containing polymers and mixtures thereof.
7. A method according to claim 5 or 6, Features The at least one chemically crosslinkable polymer has a polymer combination which contains or is a polymer and / or copolymer having at least one isocyanate group and at least one polymer and / or copolymer having at least one hydroxyl group and / or at least one melamine resin and at least one polymer and / or copolymer having at least one hydroxyl group.
8. A method according to claims 5 to 7, Features The at least one UV-crosslinkable polymer has at least one chemically crosslinkable functional group, wherein the chemically crosslinkable functional group is preferably selected from hydroxyl groups, isocyanate groups, melamine groups, epoxy groups, and combinations thereof.
9. The method according to claim 1, Features The transfer film (2), preferably the transfer ply (3) provided in step a), preferably step a1), a2) and / or a3), comprises at least one decorative layer containing at least one decorative element (11) and / or at least one functional layer comprising at least one functional element (10).
10. The method according to claim 9, Features The at least one decorative element (11) comprised by the at least one decorative layer is selected from the group consisting of: transparent and / or colored lacquer layers, in particular comprising one or more dyes and / or pigments, replication layers with a molded optically active surface structure, reflective layers, in particular opaque reflective layers, transparent reflective layers, metallic reflective layers or dielectric reflective layers, optically variable layers, optically active layers, interference multilayer systems, volume hologram layers, liquid crystal layers, in particular cholesteric liquid crystal layers, and combinations thereof.
11. The method according to claim 9, Features The at least one functional element (10) is selected from the group consisting of: at least one electronic component, in particular a strip conductor, a contact element, an LED, a sensor, in particular a touch sensor, a temperature sensor, a pressure sensor, an antenna, in particular an RFID element, a memory, a display, a control element, a processor, a capacitor, a resistor, a microfluidic element and a combination thereof.
12. The method according to claim 1, Features An adhesion promoter layer is arranged between the protective lacquer layer (8) and the at least one decorative element (11) and / or the at least one functional element (10), preferably wherein the adhesion promoter layer comprises or consists of at least one acrylic resin, and Preferably, the adhesion promoter layer preferably has a layer thickness selected from the range of 0.1 μm to 10 μm.
13. The method according to claim 1, Features The transfer ply (3) has at least one lacquer layer, preferably with a layer thickness selected from the range of 0.5 μm to 10 μm, which forms the surface of the transfer ply (3) facing away from the carrier ply (4), in particular wherein the at least one lacquer layer contains or consists of at least one adhesive selected from the group consisting of physically curing adhesives, chemically curing adhesives, pressure-sensitive adhesives or mixtures thereof.
14. The method according to any one of the preceding claims, Features The carrier ply (4) has at least one release layer, which is preferably arranged between the carrier layer (7) and the protective lacquer layer (8), wherein the release layer preferably contains at least one wax or consists thereof, and The release layer has a preferred melting temperature in the range of 80°C to 100°C.
15. The method according to any one of the preceding claims, Features Step e) is carried out by means of hot stamping, in particular roller stamping or piston stamping, wherein step e) comprises the use of an embossing tool (13), in particular wherein the embossing tool (13) is selected, alone or in combination, from at least one embossing roller, at least one embossing wheel, at least one embossing tool, at least one carrier containing a primary structure.
16. The method according to claim 15, Features A carrier having a primary structure is arranged at least partially between the embossing tool (13) and the transfer layer (3) and / or between the embossing tool (13) and the printing layer, in particular wherein the embossing tool (13) has no primary structure and / or is smooth.
17. The method according to claim 15, Features The embossing tool (13) has a primary structure.
18. A method according to claims 15 to 17, Features The protective lacquer layer (8) and / or the printed layer are in contact with the embossing tool (13).
19. The method according to any one of claims 15 to 18, Features The embossing tool (13) has no primary structure and / or is smooth.
20. The method according to any one of claims 16 to 19, It is characterized in that By bringing the embossing tool (13) into contact with the protective lacquer layer (8) and / or with the printed layer or the carrier arranged therebetween, the main structure of the embossing tool (13) or the carrier is at least partially molded in the protective lacquer layer (8) and / or the printed layer, wherein a relief structure complementary to the main structure is formed in the protective lacquer layer (8) and / or the printed layer, in particular in the at least one first area (5).
21. A method according to claims 16 to 20, Features The primary structure or the complementary relief structure is selected, alone or in combination, from a regular one-dimensional grating, a regular two-dimensional grating, a random structure assembly and a pseudo-random structure assembly.
22. The method of claims 16 to 21, Features The main structures have a structure depth selected from the range of 0.1 μm to 15 μm, preferably 0.1 μm to 10 μm, particularly preferably 0.1 μm to 5 μm, and / or the main structures have an average structure spacing selected from the range of 0.05 μm to 1000 μm, preferably 0.1 μm to 100 μm, particularly preferably 0.1 μm to 50 μm.
23. The method of claims 15 to 22, Features The complementary relief structure has a smaller structure depth than the main structure, in particular wherein the complementary relief structure has a structure depth which preferably corresponds to 20% to 99%, particularly preferably to 40% to 95%, of the structure depth of the main structure.
24. A method according to any one of claims 16 to 23, Features The carrier comprises or consists of a polymer, preferably PET, and preferably has a layer thickness selected from the range of 5 μm to 500 μm, preferably 20 μm to 50 μm.
25. The method according to any one of claims 16 to 24, Features The protective lacquer layer (8) and / or the printed layer is in contact with the embossing tool (13) or the carrier only in certain places, preferably only at the locations where at least one first region (5) is arranged in the protective lacquer layer (8) and / or the printed layer.
26. A method according to any one of claims 16 to 25, Features The embossing tool (13) and / or the carrier are designed so that the embossing tool (13) and / or the carrier only partially have a main structure, wherein the protective lacquer layer (8) and / or the printed layer are in contact with the embossing tool (13) and / or the carrier, so that the main structure is in contact with the protective lacquer layer (8) and / or the printed layer at a position where at least one first area (5) is arranged in the protective lacquer layer (8) and / or the printed layer.
27. A method according to any one of claims 16 to 26, Features A small number of embossings, in particular selected from the range of 1 to 20 times, preferably 1 to 10 times, are carried out in the same surface area of the carrier using the carrier containing the primary structure.
28. The method according to any one of the preceding claims, Features The at least one first region (5) and the at least one second region (6) are formed at an imprinting temperature selected from the range of 125°C to 250°C, and / or the imprinting speed has a value selected from the range of 1m / min to 5m / min.
29. The method according to any one of the preceding claims, Features In step e), the embossing pressure, in particular in the case of piston embossing, is selected from the range of 0.1 kN to 25 kN, preferably 0.2 kN to 20 kN, particularly preferably 0.3 kN to 15 kN, and / or the embossing pressure, in particular in the case of roller embossing, is selected from the range of 10 kg / cm 2 Up to 50kg / cm 2 , preferably 15kg / cm 2 Up to 30kg / cm 2 , particularly preferably 20kg / cm 2 Up to 25kg / cm 2 range.
30. The method according to any one of the preceding claims, Features The at least one first region (5) is formed in exact register with respect to layers or elements, in particular functional and / or decorative elements, of the transfer ply (3) and / or the substrate (9) in the protective lacquer layer (8) and / or the print layer.
31. The method according to any one of the preceding claims, Features The at least one first region (5) of the printed layer and / or the insert and / or the transfer film (2) is designed such that it has a gloss value in the range of 1 GU to 59 GU, preferably 5 GU to 30 GU.
32. Article (1), wherein the article (1) has a substrate (9) and a protective lacquer layer (8) and / or a printed layer, wherein the protective lacquer layer (8) and / or the printed layer are at least partially fully cured or thermoplastic, wherein the protective lacquer layer (8) and / or the printed layer have at least one first area (5) and at least one second area (6), wherein the relief structure is arranged in the at least one first area (5), and wherein the article (1) is produced according to one of claims 1 to 31.
33. Use of an article according to claim 32 or an article produced according to a method according to one of claims 1 to 31, alone or in combination, as display windows, touch screen panels, panels, sunshades, coverings, covers, functional elements, electronic products and housing parts or exterior parts, in particular for white goods and / or household appliances and / or automotive interior areas and / or automotive exterior areas.