Production method of metal powder
By mixing the metal compound with the binder, using non-metallic materials to cover the metal layer, and shearing and homogenizing emulsification in cold crucible vacuum suspension induction melting and hot oil, the high cost and uniformity of metal powder production in the existing technology is solved. This reduces the problem of temperature reduction and enables efficient, low-cost production of uniform metal powders suitable for high-performance electronic components.
Patent Information
- Application Number
- CN202410912468.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-09
- Publication Date
- 2024-10-22
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing metal powder production methods suffer from high costs, difficult quality control and reduced uniformity, especially in large-scale production, where it is difficult to effectively produce uniform tantalum and niobium powders.
It is formed by mixing a metal compound and a binder, using non-metallic materials as carriers to cover the surface with a metal layer, melting the metal rod through the cold crucible vacuum suspension induction melting method, and performing shearing and homogeneous emulsification in hot oil to form The spherical metal powder uses electromagnetic stirring and magnetic force to control the outflow of the melt, and is combined with a high-speed rotating shear homogenizing emulsifier for shearing and dispersion to ensure the uniformity and low oxygen content of the powder.
It achieves the uniformity and low oxygen content of metal powder in mass production, reduces production costs, improves the fineness and sphericity of the powder, and is suitable for the material requirements of high-performance electronic components.
Smart Images

Figure CN118808633A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of metal powder production, and more particularly to a method for producing metal powder. Background Art
[0002] Metal powder has a small size and a large specific surface area, so that the metal parts made of it have many properties different from conventional materials, such as excellent mechanical properties, special magnetic properties, high electrical conductivity and diffusivity, high reactivity and catalytic activity, etc. These special properties make it more and more widely used in aerospace, ships, automobiles, metallurgy, chemical industry and other fields. At present, there are many methods for preparing metal powder. Common methods include chemical reduction, electrolytic reduction and gas atomization. Tantalum or niobium capacitors usually have small size and high capacitance, and have become key components in mobile phones and personal computers. With the growing demand for electronic components with higher performance, higher reliability and lower cost, there is an inevitable demand for improving the quality of tantalum and / or niobium powder and more economical production methods. The existing production methods involve a large number of steps, resulting in very high costs and difficult quality control. At present, industrially produced tantalum powder and other high melting point rare metal powders are used as capacitor materials, and such powders are mainly produced by metal thermal reduction methods, in which active metals are used as reducing agents to reduce the raw materials. The advantage of using the metallothermic reduction method is that powdered tantalum can be produced directly through a reduction reaction. However, it is difficult to effectively produce a large amount of uniform powder through this reduction reaction, especially when the reaction scale is increased, which will lead to a disadvantage that the uniformity of the generated powder decreases. Summary of the invention
[0003] 1. Technical issues to be resolved
[0004] In view of the problems existing in the prior art, the present invention provides a method for producing metal powder to solve the technical problems mentioned in the background technology.
[0005] (II) Technical solution
[0006] To achieve the above object, the present invention provides the following technical solution: a method for producing metal powder, comprising the following steps:
[0007] Step 1: mixing the metal compound with a binder, forming, and sintering to produce a metal compound raw material molded body;
[0008] Step 2: Use a non-metallic material as a carrier and cover the metal layer on its surface by known physical, chemical or electrochemical methods;
[0009] Step 3: Use the cold crucible vacuum suspension induction melting method to put the metal rod into the cold crucible. The first inductor provides heat source and suspension force to melt the metal rod to form molten metal. The molten metal does not contact or elastically contacts the cold crucible. At the same time, there is an electromagnetic stirring effect to make the composition of different metals in the alloy more uniform.
[0010] Step 4: After the molten metal reaches a certain degree of superheat, the power of the first inductor and the second inductor is reduced, and the molten metal flows out from the bottom hole under gravity to form a molten metal flow. The molten metal flow is further heated by the magnetic force of the second inductor and the diameter of the molten metal flow is constrained, so that the molten metal flow flows out stably at a certain flow rate and a certain diameter.
[0011] Step 5: After the metal and its alloy are heated and melted, they are placed in hot oil higher than their liquidus temperature point, and appropriate corrosion inhibition emulsification aids are added. They are sheared and dispersed by a high-speed rotating shear homogenizer, so that the metal liquid is emulsified into droplets and suspended in the hot oil under the action of the shear homogenizer. The emulsified mixture of hot oil and metal is then cooled to below the solidus temperature of the alloy. The alloy droplets in the emulsified mixture solidify into spherical metal powder under the action of surface tension, with a particle size of 2-100um and an oxygen content of less than 80ppm.
[0012] The present invention is further configured that in step one, the metal compound raw material molded body is molded into a shape in which the distance from any position in the metal compound raw material molded body to the surface of the molded body is no longer than 10 mm, and the metal compound is a metal element compound selected from niobium, zirconium, titanium, hafnium, tantalum, rare earth metals and actinide metals.
[0013] The present invention is further configured such that the hot oil used in step five is a vegetable oil or mineral oil with a boiling point greater than 200°C, a viscosity E(20) greater than 14, and a temperature 5°C-50°C higher than the corresponding metal liquidus temperature.
[0014] The present invention is further configured such that the non-metallic material in step one includes: chemical fiber cloth, natural fiber cloth, organic polymer film and sponge; the prepared metal powder includes: single-phase metal powder of copper, nickel, iron, cobalt and zinc and two-phase or multi-phase metal powder.
[0015] The present invention is further configured such that the metal compound raw material molded body is molded by mixing a metal compound, a binder, and an active metal compound as a reactant.
[0016] The present invention further provides that at least one active metal selected from the group consisting of calcium, magnesium, sodium, barium and potassium is used as the reducing agent.
[0017] The present invention further provides that a compound of at least one active metal selected from the group consisting of calcium, magnesium, sodium, barium and potassium is used as the reactant.
[0018] The present invention is further configured that an oil-soluble corrosion inhibitor and an emulsifying aid can be added to the hot oil, which are petroleum sulfonate, undecenyl succinic acid or paraffin respectively, and the added amount is 1-10% of the weight of the metal and the hot oil.
[0019] (III) Beneficial effects
[0020] Compared with the prior art, the present invention provides a method for producing metal powder, which has the following beneficial effects:
[0021] The present invention performs high-temperature oxidation, reduction, and grinding processes on non-metallic materials, which are all relatively mature processes with simple reaction conditions and short cycles, and can be used for mass production. In addition, there are no special requirements for the shape of the raw materials, and there is an electromagnetic stirring effect, which makes the alloy composition more uniform and can increase the superheat of the molten metal. In the powder making process, the increase in the superheat of the molten metal can reduce the viscosity of the molten metal and make the metal powder finer. In addition, according to the production method of spherical low-temperature metal powder provided by the present invention, since the shear dispersion molding of the metal powder and the entire production process are completely free from contact with the air, and after the hot oil is separated from the metal powder, each powder surface is coated with vegetable oil or mineral oil with a corrosion inhibitor, so after appropriate packaging, the metal powder prepared by this production method has an extremely low oxygen content. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 The figure is an overall flow chart of a method for producing metal powder in the present invention. DETAILED DESCRIPTION
[0023] It should be noted that, in the absence of conflict, the embodiments and features in the embodiments of the present application may be combined with each other. The present invention will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.
[0024] It should be noted that, unless otherwise specified, all technical and scientific terms used in this application have the same meanings as commonly understood by ordinary technicians in the technical field to which this application belongs.
[0025] Embodiment 1: See also Figure 1 , a method for producing a metal powder, comprising the following steps:
[0026] Step 1: mixing the metal compound with a binder, forming, and sintering to produce a metal compound raw material molded body;
[0027] Step 2: Use a non-metallic material as a carrier and cover the metal layer on its surface by known physical, chemical or electrochemical methods;
[0028] Step 3: Use the cold crucible vacuum suspension induction melting method to put the metal rod into the cold crucible. The first inductor provides heat source and suspension force to melt the metal rod to form molten metal. The molten metal does not contact or elastically contacts the cold crucible. At the same time, there is an electromagnetic stirring effect to make the composition of different metals in the alloy more uniform.
[0029] Step 4: After the molten metal reaches a certain degree of superheat, the power of the first inductor and the second inductor is reduced, and the molten metal flows out from the bottom hole under gravity to form a molten metal flow. The molten metal flow is further heated by the magnetic force of the second inductor and the diameter of the molten metal flow is constrained, so that the molten metal flow flows out stably at a certain flow rate and a certain diameter.
[0030] Step 5: After the metal and its alloy are heated and melted, they are placed in hot oil higher than their liquidus temperature point, and appropriate corrosion inhibition emulsification aids are added. They are sheared and dispersed by a high-speed rotating shear homogenizer, so that the metal liquid is emulsified into droplets and suspended in the hot oil under the action of the shear homogenizer. The emulsified mixture of hot oil and metal is then cooled to below the solidus temperature of the alloy. The alloy droplets in the emulsified mixture solidify into spherical metal powder under the action of surface tension, with a particle size of 80um and an oxygen content of less than 80ppm.
[0031] Take 2kg of Sn63Pb37 tin-lead alloy and 20kg of castor oil, place them in a stainless steel tin furnace, heat to 230℃, vertically insert the shear head of a high-speed shearing emulsifying homogenizer for laboratory use into the furnace, adjust the speed to 18,000 rpm, and after working for 20 minutes, the metal and vegetable oil form an emulsified mixed liquid. After cooling to room temperature, filter out castor oil with a stainless steel mesh to obtain 1.98kg of Sn63Pb37 metal powder of 15-25um. 60% of the weight distribution is between 15-25um measured by a laser particle size distribution tester, and more than 98% of the weight of the powder particle size is less than 25um. The oxygen content is less than 66ppm when analyzed by a nitrogen oxygen analyzer, and the sphericity is more than 99% when measured by a high-power microscope.
[0032] In this embodiment, in step one, the metal compound raw material molded body is molded into a shape in which the distance from any position in the metal compound raw material molded body to the surface of the molded body is no longer than 10 mm, and the metal compound is a metal element compound selected from niobium, zirconium, titanium, hafnium, tantalum, rare earth metals and actinide metals.
[0033] In this embodiment, the hot oil used in step 5 is vegetable oil or mineral oil with a boiling point greater than 200°C, a viscosity E(20) greater than 14, and a temperature 30°C higher than the corresponding metal liquidus temperature.
[0034] In this embodiment, the non-metallic materials in step one include: chemical fiber cloth, natural fiber cloth, organic polymer film and sponge; the prepared metal powder includes: single-phase metal powder of copper, nickel, iron, cobalt, zinc and two-phase or multi-phase metal powder.
[0035] Embodiment 2:
[0036] A method for producing metal powder comprises the following steps:
[0037] Step 1: mixing the metal compound with a binder, forming, and sintering to produce a metal compound raw material molded body;
[0038] Step 2: Use a non-metallic material as a carrier and cover the metal layer on its surface by known physical, chemical or electrochemical methods;
[0039] Step 3: Use the cold crucible vacuum suspension induction melting method to put the metal rod into the cold crucible. The first inductor provides heat source and suspension force to melt the metal rod to form molten metal. The molten metal does not contact or elastically contacts the cold crucible. At the same time, there is an electromagnetic stirring effect to make the composition of different metals in the alloy more uniform.
[0040] Step 4: After the molten metal reaches a certain degree of superheat, the power of the first inductor and the second inductor is reduced, and the molten metal flows out from the bottom hole under gravity to form a molten metal flow. The molten metal flow is further heated by the magnetic force of the second inductor and the diameter of the molten metal flow is constrained, so that the molten metal flow flows out stably at a certain flow rate and a certain diameter.
[0041] Step 5: After the metal and its alloy are heated and melted, they are placed in hot oil higher than their liquidus temperature point, and appropriate corrosion inhibition emulsification aids are added. They are sheared and dispersed by a high-speed rotating shearing homogenizer, so that the metal liquid is emulsified into droplets and suspended in the hot oil under the action of the shearing homogenizer. The emulsified mixture of hot oil and metal is then cooled to below the solidus temperature of the alloy. The alloy droplets in the emulsified mixture solidify into spherical metal powder under the action of surface tension, with a particle size of 50um and an oxygen content of less than 80ppm.
[0042] Take 3 kg of Sn96.5Ag3Cu0.5 tin-silver-copper alloy and 30 kg of castor oil, place them in a stainless steel tin furnace and heat them to 270°C, add 310 g of paraffin wax as an emulsifying aid, and directly insert the shear head of a laboratory high-speed shearing emulsifying homogenizer into the furnace, adjust the speed to 26,000 rpm, and after working for 40 minutes, the metal and castor oil form an emulsified mixed liquid. After cooling to room temperature, filter out the castor oil with a stainless steel mesh to obtain 2.96 kg of lead-free alloy powder with a particle size of 5-15 um. Using a laser particle size distribution tester, it is measured that 62% of the weight distribution is between 5-15 um, and more than 97% of the powder particle size is less than 15 um. The oxygen content is analyzed by a nitrogen and oxygen analyzer and is less than 88 ppm. The sphericity can be measured under a high-power microscope to be more than 98.5%.
[0043] In this embodiment, the metal compound raw material molded body is molded by mixing a metal compound, a binder and an active metal compound as a reactant; at least one active metal selected from calcium, magnesium, sodium, barium and potassium is used as the reducing agent; at least one active metal compound selected from calcium, magnesium, sodium, barium and potassium is used as the reactant; an oil-soluble corrosion inhibitor and an emulsifying aid can be added to the hot oil, which are petroleum sulfonate, undecenyl succinic acid or paraffin respectively. The added amount is 1-10% of the weight of the metal and the hot oil.
[0044] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A method for producing metal powder, characterized in that: The following steps are involved: Step 1: mixing the metal compound with a binder, forming, and sintering to produce a metal compound raw material molded body; Step 2: Use a non-metallic material as a carrier and cover the metal layer on its surface by known physical, chemical or electrochemical methods; Step 3: Use the cold crucible vacuum suspension induction melting method to put the metal rod into the cold crucible. The first inductor provides heat source and suspension force to melt the metal rod to form molten metal. The molten metal does not contact or elastically contacts the cold crucible. At the same time, there is an electromagnetic stirring effect to make the composition of different metals in the alloy more uniform. Step 4: After the molten metal reaches a certain degree of superheat, the power of the first inductor and the second inductor is reduced, and the molten metal flows out from the bottom hole under gravity to form a molten metal flow. The molten metal flow is further heated by the magnetic force of the second inductor and the diameter of the molten metal flow is constrained, so that the molten metal flow flows out stably at a certain flow rate and a certain diameter. Step 5: After the metal and its alloy are heated and melted, they are placed in hot oil higher than their liquidus temperature point, and appropriate corrosion inhibition emulsification aids are added. They are sheared and dispersed by a high-speed rotating shear homogenizer, so that the metal liquid is emulsified into droplets and suspended in the hot oil under the action of the shear homogenizer. The emulsified mixture of hot oil and metal is then cooled to below the solidus temperature of the alloy. The alloy droplets in the emulsified mixture solidify into spherical metal powder under the action of surface tension, with a particle size of 2-100um and an oxygen content of less than 80ppm.
2. The method for producing a metal powder according to claim 1, characterized in that: In step one, the metal compound raw material molded body is molded into a shape in which the distance from any position in the metal compound raw material molded body to the surface of the molded body is no longer than 10 mm, and the metal compound is a metal element compound selected from niobium, zirconium, titanium, hafnium, tantalum, rare earth metals and actinide metals.
3. The method for producing a metal powder according to claim 2, characterized in that: The hot oil used in step 5 is a vegetable oil or mineral oil with a boiling point greater than 200° C., a viscosity E(20) greater than 14, and a temperature 5° C.-50° C. higher than the corresponding metal liquidus temperature.
4. The method for producing a metal powder according to claim 3, characterized in that: The non-metallic materials in step one include: chemical fiber cloth, natural fiber cloth, organic polymer film and sponge; the prepared metal powder includes: single-phase metal powder and two-phase or multi-phase metal powder of copper, nickel, iron, cobalt and zinc.
5. The method for producing a metal powder according to claim 4, characterized in that: The metal compound raw material molded body is molded by mixing a metal compound, a binder, and an active metal compound as a reactant.
6. The method for producing a metal powder according to claim 5, characterized in that: At least one active metal selected from the group consisting of calcium, magnesium, sodium, barium and potassium is used as the reducing agent.
7. The method for producing a metal powder according to claim 6, characterized in that: A compound of at least one active metal selected from the group consisting of calcium, magnesium, sodium, barium and potassium is used as the reactant.
8. The method for producing a metal powder according to claim 7, characterized in that: Oil-soluble corrosion inhibitors and emulsifying aids may be added to the hot oil, which are petroleum sulfonate, undecenyl succinic acid or paraffin, and the amount of the added agents is 1-10% of the weight of the metal and the hot oil.