Porous structure atmosphere protection device for titanium alloy laser cladding and laser cladding additive manufacturing system

By using a porous structure atmosphere protection device during the laser cladding process of titanium alloy, a local inert atmosphere is formed, which solves the problem of easy oxidation of titanium alloy at high temperatures and difficulty in forming large parts, improves material utilization and production efficiency, and ensures Quality of molded parts.

CN118808677APending Publication Date: 2024-10-22SUZHOU ZHONGKE INNOVATION INST OF LASER INTELLIGENT MFG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410828341.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-25
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

Traditional titanium alloy processing methods cannot form complex parts and have low material utilization. Moreover, titanium alloys are easily oxidized at high temperatures, resulting in a decrease in mechanical properties. It is especially difficult to form during laser cladding in an air environment. The existing atmosphere box cannot meet the requirements. Large component forming and repair needs.

Method used

A porous structure atmosphere protection device is designed, which forms a local inert atmosphere in the molten pool and the cladding area through the first and second protective gas flow channels. The first protective gas flow is used to form a first protective gas area on the surface of the molten pool. The protective gas flow forms a second protective gas area in the cladding area, ensuring that the entire molding area is covered by inert gas to avoid oxidation.

Benefits of technology

It achieves large-scale local atmosphere protection, saves the cost of argon gas filling and gas cleaning time of the atmosphere box, improves production efficiency, effectively avoids the impact of high temperature on the laser head, and ensures the quality of molded parts and the absence of oxidation layers.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118808677A_ABST
    Figure CN118808677A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of laser cladding, in particular to a porous structure atmosphere protection device for titanium alloy laser cladding and a laser cladding additive manufacturing system.The porous structure atmosphere protection device for titanium alloy laser cladding comprises a first shell, a second shell and a third shell, the first shell is constructed to be cylindrical and used for surrounding a powder path and a light path structure, and the first shell comprises an upper half part and a lower half part; the inner diameter of the lower half part of the first shell is gradually reduced, the lower half part of the first shell is provided with an arc-shaped inner surface, and a first air inlet is formed in the first end of the inner surface. According to the atmosphere protection device, a large-range local protection atmosphere can be formed, the argon filling cost of the laser cladding titanium alloy closed box body is saved, the gas washing time of the atmosphere box is saved, the production and processing efficiency is improved, the device is provided with a cooling loop, the influence of high temperature on a laser head can be effectively avoided, and the production efficiency is improved. According to the device, a molten pool is protected, and meanwhile, a cladded area can be protected.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of laser cladding, and in particular to a porous structure atmosphere protection device for laser cladding of titanium alloy and a laser cladding additive manufacturing system. Background Art

[0002] Titanium alloys have high specific strength, low density, good corrosion resistance, and good mechanical properties at high temperatures, so they are widely used in aerospace, medical, metallurgy and other fields. However, traditional processing methods such as forging, casting, and rolling cannot form complex parts, and the material utilization rate is not high. Traditional processing methods are difficult to meet the needs of aviation blade forming, impeller forming, and parts repair. The application of laser cladding technology can greatly improve the utilization rate of materials and the forming structure is not restricted.

[0003] However, titanium alloys are chemically active at high temperatures, absorbing hydrogen at 250°C, oxygen at 400°C, and nitrogen at 600°C. When laser cladding titanium alloys in an open environment, it is very easy for gas elements in the air to react, seriously affecting the mechanical properties and microstructure of titanium alloys. When the ambient oxygen concentration is below 20ppm, the formed sample is silvery white, proving that the degree of oxidation is small; when the oxygen content increases to 60ppm, the surface is white and a small amount of yellow; when the oxygen content is 1000ppm, a thick oxide film is formed on the surface, showing blue-purple and dark green, indicating a harsh oxidation environment. In an air environment, the oxygen content is as high as 21%, and titanium alloys cannot be formed. A large amount of oxides are easily generated during the forming process. Due to the different thermal expansion coefficients of the oxides and the titanium alloy itself, a large number of cracks will be generated in the titanium alloy during the forming process, and it may even be impossible to form.

[0004] Therefore, atmosphere protection is required during the titanium alloy forming process. Currently, most of the methods used are to use a closed atmosphere box filled with inert gas to form a local inert environment. However, when using an atmosphere box, large parts cannot be placed in the atmosphere box for forming and repairing; and in a closed box, it is not conducive to the heat dissipation of the parts during forming. Summary of the invention

[0005] In view of the technical problems existing in laser cladding in the prior art, the first aspect of the present invention proposes a porous structure atmosphere protection device for titanium alloy laser cladding, comprising:

[0006] The first shell is configured in a cylindrical shape and is used to surround the powder path and the optical path structure. The first shell includes an upper half and a lower half. The lower half of the first shell is configured to have a gradually decreasing inner diameter and has an arc-shaped inner surface. A first air inlet is provided at a first end of the inner surface. The extending direction of the first air inlet is tangent to the inner surface. A nozzle is provided at a second end of the inner surface. The nozzle is parallel to the central axis of the first shell.

[0007] a second shell, assembled to the upper half of the first shell, the second shell being provided with an exhaust passage;

[0008] A second gas circuit housing is connected to the outside of the nozzle, the second gas circuit housing is provided with a second gas inlet and a plurality of gas outlets, and a porous filling structure is provided between the second gas inlet and the plurality of gas outlets, so as to make the gas entering the second gas inlet flow out uniformly from the plurality of gas outlets;

[0009] Among them, when the workpiece to be processed is subjected to surface treatment, the powder path flows toward the workpiece to be processed along the axis of the nozzle, and is converged to the powder path by the light spot on the outside of the powder path and is melted onto the surface of the workpiece to be processed to form a molten pool. The area where the molten pool is located is defined as the first area, and the area around the molten pool is defined as the second area. The first protective gas flow entering from the first air inlet flows through the inner surface and flows out from the inner wall of the nozzle to form a first protective gas area on the surface of the first area. The second protective gas flow entering from the second air inlet flows out through multiple air outlets to form a second protective gas area on the surface of the second area. The air pressure in the first protective gas area is higher than the air pressure in the second protective gas area.

[0010] Preferably, the axis of the air outlet is parallel to the axis of the nozzle.

[0011] Preferably, the lower end surface of the second gas circuit housing is circular, the gas outlet comprises a plurality of circular holes of the same size, and the gas outlet is distributed in a circular array around the axis of the nozzle on the lower end surface of the second gas circuit housing.

[0012] Preferably, the sum of the flow rates of the first protective airflow and the second protective airflow is greater than or equal to 24 L / min.

[0013] Preferably, the second air circuit housing includes an upper shell and a lower shell, the upper shell is connected to the outer wall of the nozzle, the lower shell is detachably connected to the upper shell, an annular space is formed between the upper shell and the lower shell, the second air inlet is provided on the upper shell, the air outlet is provided on the lower shell, and the porous filling structure is constructed as an annular structure and filled in the annular space.

[0014] Preferably, the upper shell includes an annular first plate body and a first sleeve body extending downward from the edge of the first plate body, the first plate body is provided with a plurality of equally spaced second air inlets, the outer wall of the first sleeve body is provided with an external thread, the lower shell includes an annular second plate body and a second sleeve body extending upward from the edge of the second plate body, the second plate body is provided with a plurality of the air outlets, the inner wall of the second sleeve body is provided with an internal thread, the upper shell body is threadedly connected to the lower shell body, the thickness of the second plate body is greater than the thickness of the first plate body, and the porous filling structure includes foam copper.

[0015] Preferably, in the radial direction of the second gas circuit housing, the second air inlet is closer to the edge of the second gas circuit housing.

[0016] Preferably, the first shell is provided with a circulating cooling channel, the cooling channel is located outside the inner surface, and the circulating cooling channel is connected to a water cooler.

[0017] Preferably, the lower end surface of the nozzle coincides with the lower end surface of the gas outlet, the distance between the lower end surface of the nozzle and the surface of the workpiece to be processed is 15 mm, and the diameter of the lower end surface of the second gas path housing is 55 mm.

[0018] The second aspect of the present invention proposes a technical solution, a laser cladding additive manufacturing system, comprising:

[0019] A laser for emitting a laser beam;

[0020] A powder delivery component; comprising a connecting shaft, a pressure relief chamber and a quartz powder tube, wherein the first end of the connecting shaft is connected to the powder delivery tube, the second end is connected to the first end of the pressure relief chamber, the second end of the pressure relief chamber is connected to the quartz powder tube, and an air jacket is provided on the outside of the quartz powder tube;

[0021] The optical path structure includes a conical lens and an annular lens. The laser beam is split and reflected by the conical lens to the annular lens. The annular lens forms intersecting laser beams to form a light spot below the quartz powder tube. When the powder passes through the light spot, it is laser-clad on the surface of the workpiece to form a molten pool.

[0022] The above-mentioned porous structure atmosphere protection device for titanium alloy laser cladding;

[0023] Among them, a collimated air flow channel is formed between the gas sleeve and the quartz powder tube, a molten pool protection flow channel is formed between the gas sleeve and the inner surface, and the outlets of the plurality of second air inlets form a cladding area protection flow channel. The collimated air flow channel and the molten pool protection flow channel correspond to the first area, and the cladding area protection flow channel corresponds to the second area.

[0024] Compared with the prior art, the advantages of the present invention are:

[0025] The atmosphere protection device proposed in the present application includes a first protective gas flow channel and a second protective gas flow channel. The first protective gas forms a first protective gas area on the surface of the molten pool when flowing through the first protective gas flow channel, and the second protective gas forms a second protective gas area in the clad area around the molten pool when flowing through the second protective gas flow channel. The second protective gas flow will not affect the convergence of the powder. In this way, a large-scale local protective atmosphere can be formed, saving the cost of filling argon gas for the closed box of laser cladding titanium alloy, saving the gas washing time of the atmosphere box, and improving the efficiency of production and processing. The device has a cooling circuit, which can effectively avoid the influence of high temperature on the laser head. The device can protect the clad area while protecting the molten pool. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] The drawings are not intended to be drawn to scale. In the drawings, each identical or nearly identical component shown in various figures may be represented by the same reference numeral. For clarity, not every component is labeled in every figure. Embodiments of various aspects of the present invention will now be described by way of example and with reference to the accompanying drawings, in which:

[0027] Figure 1 It is a schematic structural diagram of a porous structure atmosphere protection device for titanium alloy laser cladding shown in the present invention;

[0028] Figure 2 It is a schematic cross-sectional structure diagram of a porous structure atmosphere protection device for titanium alloy laser cladding shown in the present invention;

[0029] Figure 3 It is a structural schematic diagram of the laser cladding additive manufacturing system shown in the present invention;

[0030] Figure 4 a is a cloud diagram of oxygen content distribution in the side section of a cone protection device in the prior art;

[0031] Figure 4 b is a cloud diagram of oxygen content distribution in the working plane of a cone protection device in the prior art;

[0032] Figure 5 a is a side profile oxygen content distribution cloud diagram of the atmosphere protection device shown in the present application;

[0033] Figure 5 b is a cloud diagram of oxygen content distribution in the working plane of the atmosphere protection device shown in the present application;

[0034] Figure 6 It is a comparison chart of the test results of single-pass laser cladding of the conical protection device in the prior art and the atmosphere protection device shown in the present application;

[0035] Figure 7This is a diagram showing the result of block forming printing using the atmosphere protection device shown in this application. DETAILED DESCRIPTION

[0036] In order to better understand the technical content of the present invention, specific embodiments are given and described as follows in conjunction with the accompanying drawings.

[0037] Since titanium alloys are chemically active at high temperatures, laser cladding of titanium alloys must be carried out in an inert gas protective atmosphere. The commonly used atmosphere protection boxes have the defects of long filling and discharging time and large gas usage. Therefore, it is more flexible and effective to form local atmosphere protection during laser cladding. It should be understood that in addition to forming atmosphere protection for the molten pool, it is also necessary to form atmosphere protection in the clad area around the molten pool until the temperature of the clad area drops below the temperature that is not easily oxidized, so that even if the part is exposed to air, it will not oxidize.

[0038] Therefore, the present application aims to propose an atmosphere protection device, which can form local atmosphere protection for the molten pool and the clad area around the molten pool during laser cladding, especially to overcome the problem that titanium alloy forming must be carried out in a closed atmosphere box; the problem that large parts and components cannot be placed in the atmosphere box when repairing; and the problem that the atmosphere box needs to be cleaned before cladding, which requires long preparation time and causes low production efficiency.

[0039] [Porous structure atmosphere protection device for titanium alloy laser cladding]

[0040] like Figure 1 As shown, the first aspect of the present invention provides a porous structure atmosphere protection device for titanium alloy laser cladding, comprising a first shell 11 , a second shell 12 and a second gas path shell 20 .

[0041] The first shell 11 and the second shell 12 are both cylindrical in shape. When the first shell 11 and the second shell 12 are connected together, a structure is formed to surround the internal powder feeding components and at the same time construct a protective gas flow channel for the molten pool. The second gas path shell 20 is intended to form a protective gas flow channel for the clad area around the molten pool. By controlling the flow rates of the two parts of the protective gas flow, a local atmosphere protection area can be formed in the molten pool and the clad area around the molten pool.

[0042] like Figure 2As shown, the first shell 11 is constructed in a cylindrical shape and is used to surround the powder path and optical path structure. The first shell 11 includes an upper half and a lower half. The lower half of the first shell 11 is constructed with a gradually decreasing inner diameter and has an arc-shaped inner surface 11a. A first air inlet 111 is provided at a first end of the inner surface 11a. The extension direction of the first air inlet 111 is tangent to the inner surface 11a. A nozzle 11b is provided at the second end of the inner surface 11a, and the nozzle 11b is parallel to the central axis of the first shell 11.

[0043] In this way, when an external gas source intervenes into the first air inlet 111, the airflow can enter along the tangent of the inner surface 11a, and flow toward the nozzle 11b along the surface of the inner surface 11a, forming a protective gas around the powder path. Since it flows along the inner surface 11a and the inner wall of the nozzle 11b, it will not interfere with the convergence of the powder, and can especially blow on the surface of the molten pool, forming an atmosphere protection for the molten pool.

[0044] Furthermore, the second shell 12 is assembled to the upper part of the first shell 11, and an exhaust channel is provided on the second shell 12. Since there is a large amount of air in the cavity of the laser optical path before cladding, in order to avoid the adverse effects of this part of air on cladding, an exhaust channel is designed to exhaust the air in the cavity. At the same time, when the air pressure or flow rate in the cavity changes, the exhaust channel can balance the air pressure, make the airflow more stable, and form a more stable local protective atmosphere.

[0045] Furthermore, the second gas circuit housing 20 is intended to provide an air flow channel for the clad area. The second gas circuit housing 20 is connected to the outside of the nozzle 11b. The second gas circuit housing 20 is provided with a second air inlet 211 and multiple air outlets 221. A porous filling structure 23 is provided between the second air inlet 211 and the multiple air outlets 221.

[0046] In this way, when the air flow enters the second air path housing 20 from the second air inlet 211, the gas entering the second air inlet 211 is diverted by the porous filling structure 23, so that the gas flowing out from the second air inlet 211 flows out evenly from the multiple air outlets 221. The multiple air outlets 221 correspond to different positions of the clad area respectively. By delivering protective air flow at different positions, local atmosphere protection is formed on the whole clad area, so that the surface will not be oxidized during the process of solidification and cooling from the molten pool to low temperature.

[0047] Among them, when the workpiece to be processed is subjected to surface treatment, the powder path flows toward the workpiece to be processed along the axis of the nozzle 11b, and is melted onto the surface of the workpiece to be processed by the light spot gathered to the powder path from the outside of the powder path to form a molten pool. The area where the molten pool is located is defined as the first area, and the area around the molten pool is defined as the second area. The first protective gas flow entering from the first air inlet 111 flows through the inner surface 11a and flows out from the inner wall of the nozzle 11b, forming a first protective gas area on the surface of the first area. The second protective gas flow entering from the second air inlet 211 flows out through multiple air outlets 221, forming a second protective gas area on the surface of the second area. The air pressure in the first protective gas area is higher than the air pressure in the second protective gas area.

[0048] In this way, the first protective gas flow forms an inert atmosphere protection on the surface of the molten pool, and the second protective gas flow forms an inert atmosphere protection in the area around the molten pool. After the first protective gas flow reaches the molten pool, it flows in the direction around the molten pool, keeping the surface around the molten pool always covered with inert gas, and oxygen cannot invade the surface of the second protective gas area. Therefore, the first area and the second area are completely covered by inert gas, forming local atmosphere protection.

[0049] Preferably, the axis of the gas outlet 221 is parallel to the axis of the nozzle 11b. In this way, the shielding gas flowing out of the gas outlet 221 will not flow to the first area, so that the flow of the powder remains stable and convergent, and the structure formed by cladding is uniform.

[0050] In an optional embodiment, the lower end surface of the second gas circuit housing 20 is circular, and the gas outlets 221 include multiple circular holes of the same size. The gas outlets 221 are distributed in a circular array around the axis of the nozzle 11 b on the lower end surface of the second gas circuit housing 20 .

[0051] In this way, a stable airflow field can be formed around the molten pool. The first protective gas flow flowing out of the nozzle 11b flows on the surface of the molten pool toward the direction around the molten pool, but the flow rate of the first protective gas flow alone cannot meet the atmosphere protection effect for the second area. Therefore, the second protective gas flow flowing out from the multiple gas outlets 221 forms a second protective gas area on the surface of the second area together with the first protective gas flow. The multiple gas outlets 221 arranged in a circular array can ensure that the second protective gas area is in a stable state.

[0052] Combination Figure 2 As shown, the second gas path housing 20 includes an upper housing 21 and a lower housing 22, the upper housing 21 is connected to the outer wall of the nozzle 11b, and the lower housing 22 is detachably connected to the upper housing 21, forming an annular space between the upper housing 21 and the lower housing 22, a second air inlet 211 is provided on the upper housing 21, and an air outlet 221 is provided on the lower housing 22, and the porous filling structure 23 is constructed as an annular structure and filled in the annular space.

[0053] In this way, when the second air inlet 211 is connected to the inert gas source, the inert gas flow enters the annular space from the second air inlet 211, is diverted by the porous filling structure, flows evenly in the annular space, and finally flows out evenly from multiple air outlets 221 parallel to the direction of powder flow, and flows from the surface of the second area to the outside of the second area together with the first protective gas flow flowing toward the outside of the molten pool, thereby forming a second protective gas area below the lower shell 22.

[0054] Specifically, the upper shell 21 includes an annular first plate body and a first sleeve body extending downward from the edge of the first plate body, the first plate body is provided with a plurality of equally spaced second air inlets 211, the outer wall of the first sleeve body is provided with an external thread, the lower shell 22 includes an annular second plate body and a second sleeve body extending upward from the edge of the second plate body, the second plate body is provided with a plurality of air outlets 221, the inner wall of the second sleeve body is provided with an internal thread, the upper shell 21 is threadedly connected to the lower shell 22, the thickness of the second plate body is greater than the thickness of the first plate body, and the porous filling structure 23 includes foam copper.

[0055] In this way, the lower shell 22 and the upper shell 21 can be disassembled and assembled by rotating the lower shell 22, so that the internal foam copper structure can be easily maintained and replaced.

[0056] Since the first protective gas flow gradually flows outward from the molten pool, the gas flow rate in the area away from the molten pool gradually decreases. Therefore, preferably, in the radial direction of the second gas circuit housing 20, the second air inlet 211 is closer to the edge position of the second gas circuit housing 20.

[0057] Thus, below the second gas circuit housing 20, the second protective gas flow rate outside the second gas circuit housing 20 is slightly greater than the flow rate inside, so that the second gas circuit housing 20 is filled with inert gas as a whole, so that the clad area will not be oxidized.

[0058] Furthermore, due to the serious heat accumulation phenomenon in the cladding process, a circulating cooling channel 112 is provided in the first shell 11 . The cooling channel is located outside the inner surface 11 a , and the circulating cooling channel 112 is connected to a water cooler.

[0059] In this way, by designing a water cooling structure, the high temperature maintained by the atmosphere protection device for a long time can be avoided, thereby improving the processing stability of the laser head.

[0060] In a preferred embodiment, the lower end surface of the nozzle 11b coincides with the lower end surface of the gas outlet 221, the distance between the lower end surface of the nozzle 11b and the surface of the workpiece to be processed is 15mm, and the diameter of the lower end surface of the second gas path housing 20 is 55mm. The sum of the flow rates of the first protective gas flow and the second protective gas flow is greater than or equal to 24L / min.

[0061] Combination Figure 5As shown in Figs. 5a and 5b, it can be seen from the oxygen content distribution cloud diagrams of the side profile and the working plane that a good low oxygen content area is formed on the molten pool surface and the surrounding area of ​​the molten pool, especially on the workpiece surface corresponding to the lower side of the second gas path housing 20.

[0062] Under the same protective gas flow rate, by comparing with the conical atmosphere protection device in the prior art, it can be seen that the oxygen content of the atmosphere protection device proposed in the present application in the working plane and the side section of the porous atmosphere protection device is significantly lower than that of the conical atmosphere protection device (such as Figure 4 a and 4b), which is more conducive to the forming of titanium alloy.

[0063]

Laser cladding additive manufacturing system

[0064] like Figure 3 As shown, the second aspect of the present invention proposes a technical solution, a laser cladding additive manufacturing system, comprising:

[0065] A laser for emitting a laser beam;

[0066] A powder delivery component; comprising a connecting shaft 41, a pressure relief chamber 42 and a quartz powder tube 44, wherein a first end of the connecting shaft 41 is connected to the powder delivery tube, a second end is connected to a first end of the pressure relief chamber 42, a second end of the pressure relief chamber 42 is connected to the quartz powder tube 44, and an air jacket 43 is provided outside the quartz powder tube 44;

[0067] The optical path structure includes a conical lens 31 and an annular lens 32. The laser beam is split and reflected by the conical lens 31 to the annular lens 32. The annular lens 32 forms an intersecting laser beam, forming a light spot below the quartz powder tube 43. When the powder passes through the light spot, it is laser-clad on the surface of the workpiece to form a molten pool.

[0068] The above-mentioned porous structure atmosphere protection device for titanium alloy laser cladding;

[0069] Among them, a collimated air flow channel is formed between the gas sleeve 43 and the quartz powder tube 44, a molten pool protection flow channel is formed between the gas sleeve 43 and the inner surface 11a, and the outlets of the multiple second air inlets 211 form a cladding area protection flow channel. The collimated air flow channel and the molten pool protection flow channel correspond to the first area, and the cladding area protection flow channel corresponds to the second area.

[0070] In this way, the collimated flow channel and the molten pool protection flow channel respectively protect the powder and the molten pool, and the outlets of the multiple second air inlets 211 form a cladding area protection flow channel to protect the second area, so that an inert gas flow flows through the surfaces of the first area and the second area. On the first hand, it can increase the cooling rate of the cladding area and shorten its oxidation window. On the second hand, it provides atmosphere protection in its oxidation window. Therefore, the structure formed by cladding has better quality and there is no oxide layer on the surface.

[0071] In an optional embodiment, a single-pass laser cladding test of titanium alloy was carried out under the conditions of laser beam scanning speed of 6.3 mm / s, defocusing amount of -2 mm, powder feeder powder plate speed of 1.0 r / min, powder feeding gas flow rate of 1.8 L / min, collimation gas flow rate of 7.1 L / min, and total protection gas flow rate of 24 L / min. The results are as follows: Figure 6 shown.

[0072] in, Figure 6 a~e in the figure are five cladding structures formed by the cone protection device when the laser power is 350~450W and the growth gradient is 25W. Figure 6 f~j in the figure are five cladding structures formed by the protection device proposed in this application when the laser power is 350~450W and the growth gradient is 25W.

[0073] It can be seen from the experimental results that when the conical protection device is used for single-pass cladding at a laser power of 350 to 450 W, the single pass appears bluish purple, indicating that the titanium alloy has undergone severe oxidation; while when the atmosphere protection device proposed in the present application is used for single-pass cladding at a laser power of 350 to 450 W, the single pass appears silver, indicating that the titanium alloy has not undergone severe oxidation.

[0074] In an optional embodiment, a block forming test of titanium alloy is carried out at a laser power of 400 W, a laser beam scanning speed of 6.3 mm / s, a defocusing amount of -2 mm, a powder feeder powder plate speed of 1.0 r / min, a powder feeding gas flow rate of 1.8 L / min, a collimation gas flow rate of 7.1 L / min, and a total protection gas flow rate of 24 L / min. The forming structure is as follows Figure 7 shown.

[0075] From the appearance, it can be seen that the molded part is silvery white, with no obvious oxidation color on the surface, no cracks and other defects. The oxygen content of the block was tested using the ELEMENTRAC ONHp oxygen and nitrogen analyzer, and the mass fraction of oxygen was between 0.14% and 0.16%, which meets the requirement of GB / T 3620.1-2016 that the oxygen element should not exceed 0.2%.

[0076] Therefore, the atmosphere protection device proposed in this application can realize the titanium alloy laser cladding forming process in an open environment.

[0077] Although the present invention has been disclosed as above with preferred embodiments, it is not intended to limit the present invention. A person with ordinary knowledge in the technical field to which the present invention belongs may make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be determined by the definition of the claims.

Claims

1. A porous structure atmosphere protection device for titanium alloy laser cladding, characterized in that: include: A first shell (11) is configured in a cylindrical shape and is used to surround a powder path and an optical path structure. The first shell (11) comprises an upper half and a lower half. The lower half of the first shell (11) is configured to have a gradually decreasing inner diameter and has an arc-shaped inner surface (11a). A first air inlet (111) is provided at a first end of the inner surface (11a). The extension direction of the first air inlet (111) is tangent to the inner surface (11a). A nozzle (11b) is provided at a second end of the inner surface (11a). The nozzle (11b) is parallel to the central axis of the first shell (11); A second shell (12) assembled to the upper half of the first shell (11), wherein the second shell (12) is provided with an exhaust passage; A second gas circuit housing (20) connected to the outside of the nozzle (11b), the second gas circuit housing (20) being provided with a second gas inlet (211) and a plurality of gas outlets (221), a porous filling structure (23) being provided between the second gas inlet (211) and the plurality of gas outlets (221) for allowing the gas entering through the second gas inlet (211) to flow out uniformly from the plurality of gas outlets (221); When the workpiece to be processed is subjected to surface treatment, the powder path flows toward the workpiece to be processed along the axis of the nozzle (11b), and is converged to the powder path by the light spot on the outside of the powder path and is clad on the surface of the workpiece to be processed to form a molten pool. The area where the molten pool is located is defined as the first area, and the area around the molten pool is defined as the second area. The first protective gas flow entering from the first air inlet (111) flows through the inner surface (11a) and flows out from the inner wall of the nozzle (11b), forming a first protective gas area on the surface of the first area. The second protective gas flow entering from the second air inlet (211) flows out through the plurality of air outlets (221), forming a second protective gas area on the surface of the second area. The air pressure in the first protective gas area is higher than the air pressure in the second protective gas area.

2. The porous structure atmosphere protection device for titanium alloy laser cladding according to claim 1 is characterized in that: The axis of the air outlet (221) is parallel to the axis of the nozzle (11b).

3. The porous structure atmosphere protection device for titanium alloy laser cladding according to claim 1 is characterized in that: The lower end surface of the second gas circuit housing (20) is constructed in a circular shape, the gas outlet (221) comprises a plurality of circular holes of the same size, and the gas outlets (221) are distributed in a circular array around the axis of the nozzle (11b) on the lower end surface of the second gas circuit housing (20).

4. The porous structure atmosphere protection device for titanium alloy laser cladding according to claim 1 is characterized in that: The sum of the flow rates of the first protective airflow and the second protective airflow is greater than or equal to 24 L / min.

5. The porous structure atmosphere protection device for titanium alloy laser cladding according to claim 1 is characterized in that: The second gas path housing (20) comprises an upper housing (21) and a lower housing (22), wherein the upper housing (21) is connected to the outer wall of the nozzle (11b), and the lower housing (22) is detachably connected to the upper housing (21), and an annular space is formed between the upper housing (21) and the lower housing (22), wherein the upper housing (21) is provided with the second air inlet (211), and the lower housing (22) is provided with the air outlet (221), and the porous filling structure (23) is constructed as an annular structure and is filled in the annular space.

6. The porous structure atmosphere protection device for titanium alloy laser cladding according to claim 5 is characterized in that: The upper shell (21) comprises an annular first plate body and a first sleeve body extending downward from the edge of the first plate body, the first plate body is provided with a plurality of second air inlets (211) at equal intervals, the outer wall of the first sleeve body is provided with external threads, the lower shell (22) comprises an annular second plate body and a second sleeve body extending upward from the edge of the second plate body, the second plate body is provided with a plurality of air outlets (221), the inner wall of the second sleeve body is provided with internal threads, the upper shell (21) is threadedly connected to the lower shell (22), the thickness of the second plate body is greater than the thickness of the first plate body, and the porous filling structure (23) comprises foam copper.

7. The porous structure atmosphere protection device for titanium alloy laser cladding according to claim 6 is characterized in that: In the radial direction of the second gas circuit housing (20), the second air inlet (211) is closer to the edge of the second gas circuit housing (20).

8. The porous structure atmosphere protection device for titanium alloy laser cladding according to any one of claims 1 to 7, characterized in that: The first shell (11) is provided with a circulating cooling channel (112), the cooling channel is located outside the inner surface (11a), and the circulating cooling channel (112) is connected to a water cooler.

9. The porous structure atmosphere protection device for titanium alloy laser cladding according to any one of claims 1 to 7, characterized in that: The lower end surface of the nozzle (11b) coincides with the lower end surface of the gas outlet (221), the distance between the lower end surface of the nozzle (11b) and the surface of the workpiece to be processed is 15 mm, and the diameter of the lower end surface of the second gas path housing (20) is 55 mm.

10. A laser cladding additive manufacturing system, characterized in that: include: A laser for emitting a laser beam; Powder feeding parts; It comprises a connecting shaft (41), a pressure relief chamber (42) and a quartz powder tube (44), wherein a first end of the connecting shaft (41) is connected to a powder conveying pipe, a second end is connected to a first end of the pressure relief chamber (42), a second end of the pressure relief chamber (42) is connected to the quartz powder tube (44), and an air jacket (43) is provided outside the quartz powder tube (44); An optical path structure comprises a conical lens (31) and an annular lens (32), wherein the laser beam is split and reflected by the conical lens (31) to the annular lens (32), wherein the annular lens (32) forms intersecting laser beams, and forms a light spot below the quartz powder tube (43), and when the powder passes through the light spot, it is laser-clad on the surface of the workpiece to form a molten pool; The porous structure atmosphere protection device for titanium alloy laser cladding according to any one of claims 1 to 9; A collimated flow channel is formed between the gas sleeve (43) and the quartz powder tube (44), a molten pool protection flow channel is formed between the gas sleeve (43) and the inner surface (11a), and outlets of the plurality of second gas inlets (211) form a cladding area protection flow channel, the collimated flow channel and the molten pool protection flow channel correspond to the first area, and the cladding area protection flow channel corresponds to the second area.