Formula and production process of bamboo fiber composite board
Through the formula and production process of bamboo fiber composite boards, the problems of excessive stiffness and insufficient resource utilization of wooden composite boards have been solved, the strength improvement and environmental benefits have been achieved, the resistance and pressure resistance of the boards have been improved, and the environmental performance of the products has been enhanced. .
Patent Information
- Application Number
- CN202411035157.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-31
- Publication Date
- 2024-10-22
AI Technical Summary
Existing wood composite panels have too high stiffness during use and are easily partially broken, and the waste wood scraps used in the production process are not fully utilized, resulting in environmental protection and cost-effectiveness issues.
Using the bamboo fiber composite board formula and production process, dry bamboo fiber raw materials are mixed with PET fibers and adhesives, and are formed in the mold cavity by the layering method. Combined with high temperature and high pressure processes, a fibrous traction structure is formed to strengthen the board. strength and reduce costs.
It improves the resistance and pressure resistance of the board and extends its service life. At the same time, because bamboo fiber is a recycled material, it has better environmental performance, increasing the recognition and environmental benefits of the product.
Smart Images

Figure CN118809745A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of board manufacturing, and in particular to a bamboo fiber composite board formula and production process. Background Art
[0002] In recent years, with the development of the material field, the requirements for the processing cost, strength, service life, etc. of wooden boards are getting higher and higher. Ordinary wooden boards often fail to meet the requirements, so composite wooden boards such as three-ply boards and five-ply boards have appeared. The existing patent (Announcement No.: CN202895370U) proposes a multi-layer composite wooden board, including a multi-layer composite wooden board body, which is characterized in that: the multi-layer composite wooden board body is composed of a plywood layer and a rubber layer, the plywood layer is formed by gluing three or more thin plates, the rubber layer is between the plywood layers, and further, the rubber layer is inlaid with evenly distributed solid wood blocks. A multi-layer composite wooden board with such a structure has the advantages of good moisture resistance, comfortable texture, low cost, and good sound insulation effect. The main raw materials of the existing wooden boards are discarded wooden product scraps, which need to be crushed and then coated with glue and pressed. The manufactured wooden board has too high rigidity and is easy to be partially broken when foreign objects are inserted, which is not conducive to practical use. Summary of the invention
[0003] The purpose of the present invention is to provide a bamboo fiber composite board formula and production process to solve the problems existing in the above-mentioned prior art.
[0004] The above technical objectives of the present invention are achieved through the following technical solutions:
[0005] A bamboo fiber composite board formula and production process, including 50-70 parts of bamboo fiber raw material, 20-30 parts of PET, 10-15 parts of adhesive and 1-2 parts of auxiliary materials;
[0006] It is made by the following steps:
[0007] Step 1: Dry the bamboo fiber raw material to a humidity of 0.05%-0.2%, manufacture the PET material into a fiber shape with a length of 38mm-76mm and a diameter of 0.08mm-0.2mm, and dry the bamboo fiber raw material to a humidity below 0.2%;
[0008] Step 2: Evenly mix the adhesive and auxiliary materials, and then evenly mix the bamboo fiber raw material, bamboo fiber raw material and PET;
[0009] Step 3, heat the mold cavity to 220 degrees Celsius, and then evenly layer the bamboo fiber raw material, bamboo fiber raw material, PET mixture, adhesive and auxiliary material mixture in the molding mold cavity by the layering method, maintain the pressure for 5S-30S, and evenly increase the temperature to 260 degrees Celsius in the first 5 seconds of pressure holding, and evenly increase the temperature to 280 degrees Celsius from the 5th to the 20th second, stop heating from the 20th to the 30th second, let the temperature drop naturally, and release the internal pressure of the mold cavity by 25%-35%.
[0010] By adopting the above technical scheme, the bamboo fiber raw material and PET fiber both have a certain fiber density. After molding, they can be used as a pulling structure to apply force inside the wooden board. When encountering foreign objects inserted, they will break first, but the bamboo fiber can withstand a large force, so the structure of the wooden board can be strengthened. Moreover, bamboo fiber is a recycled material. Compared with practical wood fiber, bamboo fiber has better environmental protection effects. While increasing the strength of the product, it also plays a role in saving wood and protecting the environment. Moreover, because the bamboo fiber raw material needs to be subjected to force internally, the bamboo fiber can be seen from the surface, which makes people more recognized for the modified product.
[0011] In a further embodiment, the ingredients of the auxiliary material include: 35 parts of sodium polymethacrylate, 2 parts of sodium hydroxide, 2 parts of defoaming agent, and 1 part of anti-settling agent. The 35 parts of sodium polymethacrylate are used to enhance the bonding force, the defoaming agent is used to eliminate bubbles that appear during the uniform mixing of the adhesive and the auxiliary materials and cavitations that are coated on the surface of the material after the bamboo fiber raw material, the bamboo fiber raw material, and the PET are uniformly mixed, and the anti-settling agent is used to prevent the sodium polymethacrylate, sodium hydroxide, and defoaming agent from settling before use after the mixing is completed.
[0012] In a further embodiment, the main components of the adhesive are: 50-70 parts of water, 1-2 parts of hydroxyethyl cellulose, 2-5 parts of polyvinyl alcohol, 5-10 parts of organic emulsion, 10-15 parts of inorganic sol, 1-5 parts of alkali metal salt of silicate, 1-5 parts of sulfuric acid, 1-5 parts of attapulgite, 1-3 parts of bentonite, 1-2 parts of magnesium aluminum silicate, 1-2 parts of hydroalophane, and 5-10 parts of low-melting-point glass.
[0013] In a further embodiment, the preparation method of the bamboo fiber raw material is:
[0014] Step 1: Obtain bamboo strips and break them;
[0015] Step 2: removing impurities from the raw materials;
[0016] Step 3: Store in a dry place at room temperature to remove moisture.
[0017] In a further embodiment, the method for preparing the bamboo fiber raw material is as follows: step S1, soaking in an acid solution for 2-4 hours, and circulately stirring during the soaking process;
[0018] Step S2, rinsing and decolorizing, removing the cytochrome by rinsing;
[0019] Step S3, pulling and forging, pulling the decolorized bamboo fiber by a comb-tooth roller to control the bamboo fiber to a length of 5mm-100mm.
[0020] In a further embodiment, the PET is modified PET, and 2%-5% of cooling masterbatch is added during the manufacturing process.
[0021] The invention also discloses a production process of a bamboo fiber composite board formulation, comprising the following steps:
[0022] Step 1, setting the hot pressing temperature to 220°C, the hot pressing pressure to 2.6MPa, the hot pressing time to 30s, the single-layer composite thickness to be between 1.15g / ml-1.32g / ml per cubic millimeter of the mass of the bamboo fiber raw material, the bamboo fiber raw material, and the PET mixed material, and the spraying amount of the adhesive and the auxiliary material mixture to be between 30g / mm-45g / mm;
[0023] Step 2: From the 20th to the 30th second of holding pressure, the temperature in the mold cavity is quickly cooled to below 220 degrees Celsius through the cooling water channel.
[0024] In summary, the present invention has the following beneficial effects:
[0025] 1. Bamboo fiber raw materials and PET fiber both have a certain fiber density. After molding, they can be used as a pulling structure to apply force inside the wooden board. When encountering foreign objects inserted, they will break first, but bamboo fiber can withstand greater force, so it can strengthen the structure of the wooden board. Bamboo fiber is a recycled material. Compared with practical wood fiber, bamboo fiber has better environmental protection effects. While increasing the strength of the product, it also plays a role in saving wood and protecting the environment. And because the bamboo fiber raw material needs to be subjected to force internally, the bamboo fiber can be seen from the surface, which makes people more recognized of the product. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 It is a schematic diagram of the surface of the composite bamboo fiberboard of the present invention;
[0027] Figure 2 It is a schematic diagram of the relationship between the holding time and temperature of the finished product of the present invention;
[0028] Figure 3 It is a schematic diagram of the tensile strength structure of the finished product of the present invention;
[0029] Figure 4 is a schematic diagram of the anti-bending structure of the present invention;
[0030] Figure 5 It is a schematic diagram of the microstructure of the present invention;
[0031] Figure 6 It is a schematic diagram of the microscopic structure of the bamboo fiberboard of the present invention. DETAILED DESCRIPTION
[0032] The present invention is further described in detail below in conjunction with the accompanying drawings.
[0033] The same parts are denoted by the same reference numerals. It should be noted that the words "front", "rear", "left", "right", "upper" and "lower" used in the following description refer to the attached Figure 1 In the description of this specification, the words "bottom" and "top", "inside" and "outside" refer to directions toward or away from a particular component geometry, respectively. In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of this specification, the meaning of "multiple" is two or more, unless otherwise clearly and specifically defined.
[0034] Embodiment 1:
[0035] like Figure 1-Figure 6 As shown, a bamboo fiber composite board formula includes 50 parts of bamboo fiber raw material, 20 parts of PET, 6 parts of bamboo fiber raw material, 10 parts of adhesive and 1 part of auxiliary material, the components of the auxiliary material include: 35 parts of sodium polymethacrylate, 2 parts of sodium hydroxide, 2 parts of defoamer, 1 part of anti-settling agent, the 35 parts of sodium polymethacrylate are used to enhance the bonding force, the defoamer is used to eliminate bubbles appearing in the process of mixing the adhesive and the auxiliary material and cavitations applied to the surface of the bamboo fiber raw material, the bamboo fiber raw material and PET after being mixed, the anti-settling agent is used to prevent the sodium polymethacrylate, sodium hydroxide and defoamer from settling before use after the mixing is completed, and the main components of the adhesive are: 50 parts of water, 1 part of hydroxyethyl cellulose, 2 parts of polyvinyl alcohol, 5 parts of organic emulsion, 10 parts of inorganic sol, 1 part of alkali metal salt of silicate, 1 part of sulfuric acid, 1 part of attapulgite, 1 part of bentonite, 1 part of magnesium aluminum silicate, 1 part of hydroalophane, and 5 parts of low-melting-point glass;
[0036] It is made by the following steps:
[0037] Step 1: Dry the bamboo fiber raw material to a humidity of 0.05%-0.2%, manufacture the PET material into a fiber shape with a length of 38mm-76mm and a diameter of 0.08mm-0.2mm, and dry the bamboo fiber raw material to a humidity below 0.2%;
[0038] Step 2: Evenly mix the adhesive and auxiliary materials, and then evenly mix the bamboo fiber raw material, bamboo fiber raw material and PET;
[0039] Step 3, heat the mold cavity to 220 degrees Celsius, and then evenly layer the bamboo fiber raw material, bamboo fiber raw material, PET mixture, adhesive and auxiliary material mixture in the molding mold cavity by the layering method, maintain the pressure for 5S-30S, and evenly increase the temperature to 260 degrees Celsius in the first 5 seconds of pressure holding, and evenly increase the temperature to 280 degrees Celsius from the 5th to the 20th second, stop heating from the 20th to the 30th second, let the temperature drop naturally, and release the internal pressure of the mold cavity by 25%-35%.
[0040] The preparation method of the bamboo fiber raw material is:
[0041] Step 1: Obtain bamboo strips and break them;
[0042] Step 2: removing impurities from the raw materials;
[0043] Step 3: Dry and store at room temperature to remove moisture. The preparation method of the bamboo fiber raw material is as follows: Step S1: soak in an acid solution for 2-4 hours, and stir cyclically during the soaking process;
[0044] Step S2, rinsing and decolorizing, removing the cytochrome by rinsing;
[0045] Step S3, pulling and forging, pulling the decolorized bamboo fiber by a comb roller, and controlling the length of the bamboo fiber to be 5mm-100mm, the PET is a modified PET, and 2%-5% of cooling masterbatch is added during the manufacturing process.
[0046] The invention also discloses a production process of a bamboo fiber composite board formulation, comprising the following steps:
[0047] Step 1, setting the hot pressing temperature to 220°C, the hot pressing pressure to 2.6MPa, the hot pressing time to 30s, the single-layer composite thickness to be between 1.15g / ml-1.32g / ml per cubic millimeter of the mass of the bamboo fiber raw material, the bamboo fiber raw material, and the PET mixed material, and the spraying amount of the adhesive and the auxiliary material mixture to be between 30g / mm-45g / mm;
[0048] Step 2: From the 20th to the 30th second of holding pressure, the temperature in the mold cavity is quickly cooled to below 220 degrees Celsius through the cooling water channel.
[0049] Specific implementation process: During the manufacturing process, all materials need to be mixed first and then layered according to the process requirements, and then the needle-punching process is used to connect them to form a density felt with a layer structure, and then different layers of density felt are stacked and molded through different processes. In this way, multiple layers of density felt with the same number of layers can be pressed to the same product thickness, and the density and hardness of the final product can be controlled. Multiple layers of the same number of density felts can also be pressed into products of different densities and qualities, making them more suitable for some fields that require lightweight materials.
[0050] Embodiment 2:
[0051] like Figure 1-Figure 6 As shown, a bamboo fiber composite board formula and production process, a bamboo fiber composite board formula, including 70 parts of bamboo fiber raw material, 30 parts of PET, 8 parts of bamboo fiber raw material, 15 parts of adhesive and 2 parts of auxiliary materials, the ingredients of the auxiliary materials include: 35 parts of sodium polymethacrylate, 2 parts of sodium hydroxide, 2 parts of defoaming agent, 1 part of anti-settling agent, the 35 parts of sodium polymethacrylate are used to enhance the bonding force, the defoaming agent is used to eliminate bubbles appearing in the process of mixing the adhesive and the auxiliary materials and cavitations applied to the surface of the bamboo fiber raw material, the bamboo fiber raw material and PET after mixing, the anti-settling agent is used to prevent the sodium polymethacrylate, sodium hydroxide and defoaming agent from settling before use after mixing, the main components of the adhesive are: 70 parts of water, 2 parts of hydroxyethyl cellulose, 5 parts of polyvinyl alcohol, 10 parts of organic emulsion, 15 parts of inorganic sol, 5 parts of alkali metal salt of silicate, 5 parts of sulfuric acid, 5 parts of attapulgite, 3 parts of bentonite, 2 parts of magnesium aluminum silicate, 2 parts of hydroalophane, and 10 parts of low melting point glass.
[0052] Embodiment 3:
[0053] like Figure 1-Figure 6 As shown, a formula for a bamboo fiber composite board includes 70 parts of bamboo fiber raw material, 30 parts of PET, 6 parts of bamboo fiber raw material, 15 parts of adhesive and 2 parts of auxiliary materials, wherein the ingredients of the auxiliary materials include: 35 parts of sodium polymethacrylate, 2 parts of sodium hydroxide, 2 parts of defoaming agent, and 1 part of anti-settling agent. The 35 parts of sodium polymethacrylate are used to enhance the bonding force, the defoaming agent is used to eliminate bubbles that appear during the uniform mixing of the adhesive and the auxiliary materials and cavitations that are coated on the surface of the bamboo fiber raw material, the bamboo fiber raw material, and the PET after the materials are uniformly mixed, the anti-settling agent is used to prevent the sodium polymethacrylate, sodium hydroxide, and defoaming agent from settling before use after the mixing is completed, and the main ingredients of the adhesive are: 50 parts of water, 1 part of hydroxyethyl cellulose, 2 parts of polyvinyl alcohol, 5 parts of organic emulsion, 10 parts of inorganic sol, 1 part of alkali metal salt of silicate, 1 part of sulfuric acid, 1 part of attapulgite, 1 part of bentonite, 1 part of magnesium aluminum silicate, 1 part of hydroalophane, and 5 parts of low-melting-point glass.
[0054] Embodiment 4:
[0055] like Figure 1-Figure 6 As shown, a formula for a bamboo fiber composite board includes 50 parts of bamboo fiber raw material, 20 parts of PET, 8 parts of bamboo fiber raw material, 10 parts of adhesive and 1 part of auxiliary material, wherein the ingredients of the auxiliary material include: 35 parts of sodium polymethacrylate, 2 parts of sodium hydroxide, 2 parts of defoaming agent, and 1 part of anti-settling agent. The 35 parts of sodium polymethacrylate are used to enhance the bonding force, the defoaming agent is used to eliminate bubbles that appear during the uniform mixing of the adhesive and the auxiliary materials and cavitations that are coated on the surface of the bamboo fiber raw material, the bamboo fiber raw material, and the PET after the mixture is uniformly mixed, and the anti-settling agent is used to prevent the sodium polymethacrylate, sodium hydroxide, and defoaming agent from settling before use after the mixture is completed. The main ingredients of the adhesive are: 2 parts, hydroxyethyl cellulose, 5 parts of polyvinyl alcohol, 10 parts of organic emulsion, 15 parts of inorganic sol, 5 parts of alkali metal salt of silicate, 5 parts of sulfuric acid, 5 parts of attapulgite, 3 parts of bentonite, 2 parts of magnesium aluminum silicate, 2 parts of hydroalophane, and 10 parts of low-melting-point glass.
[0056] In actual use, due to the presence of defoaming agent and the high pressure and high temperature inside the mold cavity, the bubbles attached to the surface will be eliminated, avoiding the existence of cavities inside the material. Cavities will reduce the overall strength of the material and easily cause uneven local shrinkage, resulting in surface deformation of the material when there is a large temperature change.
[0057] Embodiment 5:
[0058] like Figure 1 , Figure 5-Figure 6 As shown, it can be clearly seen that the PET fiber of the present invention obviously completely covers the bamboo fiber. Through this combination, the bamboo fiberboard manufactured by the scheme of the present invention has strong resistance. By controlling the pressure and force in the molding process, products of different thicknesses and densities can be obtained, achieving multi-purpose.
[0059] In the embodiments disclosed in the present invention, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense. For example, "connected" can be a fixed connection, a detachable connection, or an integral connection; "connected" can be a direct connection or an indirect connection through an intermediate medium. For those of ordinary skill in the art, the specific meanings of the above terms in the embodiments disclosed in the present invention can be understood according to specific circumstances.
[0060] This specific embodiment is merely an explanation of the present invention and is not a limitation of the present invention. After reading this specification, those skilled in the art may make non-creative modifications to the present embodiment as needed. However, as long as they are within the scope of the claims of the present invention, they are protected by the patent law.
Claims
1. A bamboo fiber composite board formula, characterized by: Including 50-70 parts of bamboo fiber raw materials, 20-30 parts of PET, 10-15 parts of adhesive and 1-2 parts of auxiliary materials; It is made by the following steps: Step 1: Dry the bamboo fiber raw material to a humidity of 0.05%-0.2%, manufacture the PET material into a fiber shape with a length of 38mm-76mm and a diameter of 0.08mm-0.2mm, and dry the bamboo fiber raw material to a humidity below 0.2%; Step 2, mixing the adhesive and the auxiliary materials evenly, and then mixing the bamboo fiber raw material, the bamboo fiber raw material, and PET evenly, wherein the PET is a modified low melting point PET; Step 3, heat the mold cavity to 220 degrees Celsius, and then evenly layer the bamboo fiber raw material, bamboo fiber raw material, PET mixture, adhesive and auxiliary material mixture in the molding mold cavity by the layering method, maintain the pressure for 5S-30S, and evenly increase the temperature to 260 degrees Celsius in the first 5 seconds of pressure holding, and evenly increase the temperature to 280 degrees Celsius from the 5th to the 20th second, stop heating from the 20th to the 30th second, let the temperature drop naturally, and release the internal pressure of the mold cavity by 25%-35%.
2. The bamboo fiber composite board formula according to claim 1, characterized in that: The ingredients of the auxiliary material include: 35 parts of sodium polymethacrylate, 2 parts of sodium hydroxide, 2 parts of defoaming agent, and 1 part of anti-settling agent. The 35 parts of sodium polymethacrylate are used to enhance the bonding force. The defoaming agent is used to eliminate bubbles that appear during the uniform mixing of the adhesive and the auxiliary material and cavitations that are coated on the surface of the bamboo fiber raw material, the bamboo fiber raw material, and the PET after being uniformly mixed. The anti-settling agent is used to prevent the sodium polymethacrylate, sodium hydroxide, and defoaming agent from settling before use after the mixture is completed.
3. The bamboo fiber composite board formula according to claim 1, characterized in that: The main components of the adhesive are: 50-70 parts of water, 1-2 parts of hydroxyethyl cellulose, 2-5 parts of polyvinyl alcohol, 5-10 parts of organic emulsion, 10-15 parts of inorganic sol, 1-5 parts of alkali metal salt of silicate, 1-5 parts of sulfuric acid, 1-5 parts of attapulgite, 1-3 parts of bentonite, 1-2 parts of magnesium aluminum silicate, 1-2 parts of hydroalophane, and 5-10 parts of low-melting-point glass.
4. The bamboo fiber composite board formula according to claim 1, characterized in that: The preparation method of the bamboo fiber raw material is: Step 1: Obtain bamboo strips and break them; Step 2: removing impurities from the raw materials; Step 3: Store in a dry place at room temperature to remove moisture.
5. The bamboo fiber composite board formula according to claim 1, characterized in that: The preparation method of the bamboo fiber raw material comprises: step S1, soaking in an acid solution for 2-4 hours, and circulately stirring during the soaking process; Step S2, rinsing and decolorizing, removing the cytochrome by rinsing; Step S3, pulling and forging, pulling the decolorized bamboo fiber by a comb-tooth roller to control the bamboo fiber to a length of 5mm-100mm.
6. The bamboo fiber composite board formula according to claim 1, characterized in that: The PET is a modified PET, and 2%-5% of cooling masterbatch is added during the manufacturing process.
7. A production process of the bamboo fiber composite board formulation according to any one of claims 1 to 6, characterized in that: The following steps are involved: Step 1, setting the hot pressing temperature to 220°C, the hot pressing pressure to 2.6MPa, the hot pressing time to 30s, the single-layer composite thickness to be between 1.15g / ml-1.32g / ml per cubic millimeter of the mass of the bamboo fiber raw material, the bamboo fiber raw material, and the PET mixed material, and the spraying amount of the adhesive and the auxiliary material mixture to be between 30g / mm-45g / mm; Step 2: From the 20th to the 30th second of holding pressure, the temperature in the mold cavity is quickly cooled to below 220 degrees Celsius through the cooling water channel.
Citation Information
Patent Citations
Multi-layer composite plank
CN202895370U
Thermoplastic bamboo fiber composite board and manufacturing method thereof
CN102145552A
Polyvinyl acetate emulsion paint and preparation method thereof
CN104387870A
Polymer composite for board modification and preparation method thereof
CN104926982A
Organic and inorganic composite adhesive