Injection-molded wood grain decorative plate and preparation method thereof

Through the injection molding process, composite nozzle technology is used to form wood grain decorative panels with high authenticity and excellent physical properties, which solves the problem of insufficient visual authenticity and physical properties of Polypropylene paper, and realizes environmentally friendly and economical decorative panel production.

CN118809941APending Publication Date: 2024-10-22NINGBO LISI HOUSEWARE CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202411038717.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-31
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

When existing polyester paper imitates natural wood, it suffers from poor visual authenticity and poor physical properties. It is difficult to replicate the delicate and complex texture and fiber structure of natural wood, and its service life and aesthetics are low.

Method used

Injection molding technology is used to form a decorative panel with a uniform background color and wood grain decorative stripes through one-piece injection molding of two colors of materials. The wood grain decorative stripes cover the uniform background color and are set in a curve. The materials are synchronized through the composite nozzle. Injected and molded to form decorative panels with high authenticity and excellent physical properties.

Benefits of technology

It achieves the effect of highly simulating the texture of natural wood, improves the visual beauty and durability, avoids the problem of delamination wear, conforms to the concept of environmental protection and reduces production costs, and adapts to the physical performance requirements of different application environments.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118809941A_ABST
    Figure CN118809941A_ABST
Patent Text Reader

Abstract

The invention discloses an injection-molded wood grain decorative plate and a preparation method thereof, and belongs to the technical field of decorative plate injection molding. Comprising a decorative plate body which is integrally formed by materials with at least two colors in an injection molding mode, and after forming, the decorative plate body has uniform ground color and wood-grain-shaped decorative stripes. S1, an injection gun barrel A and an injection gun barrel B are adopted to synchronously inject a material A and a material B into the same composite nozzle; s2, the composite nozzle comprises a spreader, a sharing chamber and a nozzle hole, the spreader is provided with an ejection hole A and an ejection hole B, the material A enters the sharing chamber through the ejection hole A, the material B enters the sharing chamber through the ejection hole B, and the two materials in the sharing chamber are ejected outwards through the nozzle hole; and S3, the two materials ejected from the nozzle holes are injected into a mold and molded into a decorative plate body. The decorative plate body can form a structure with uniform ground color and wood-grain-shaped decorative stripes in the one-time forming process, and the effect of highly simulating natural wood grains is achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of injection molding of decorative panels, and in particular relates to an injection-molded wood-grain decorative panel and a preparation method thereof. Background Art

[0002] With the improvement of environmental awareness and the pursuit of sustainable development, the architectural decoration and furniture manufacturing industries are increasingly using alternative materials to simulate the effects of natural wood to cope with the increasing scarcity of wood resources. Polaroid paper (or decorative paper) is a common wood texture imitation material. When manufacturing artificial boards, it is attached to the surface of the substrate by hot pressing and other methods to form a decorative panel similar to the effect of real wood.

[0003] Polaroid paper has the following disadvantages when imitating real wood grain:

[0004] Poor visual authenticity: Due to technical limitations, it is difficult to replicate the delicate and complex texture and fiber structure of natural wood, especially the natural pores and randomly distributed texture characteristics of wood, which makes the finished product lack real texture when observed up close;

[0005] Physical properties: The surface hardness, wear resistance and corrosion resistance of Polaroid board may not be as good as natural wood or some high-performance synthetic materials, which may reduce the service life and aesthetics in actual use. Summary of the invention

[0006] The present invention aims at the above problems existing in the prior art and proposes an injection-molded wood grain decorative board with low production cost, strong visual authenticity and high physical properties and a preparation method thereof.

[0007] The present invention can be achieved through the following technical solutions:

[0008] An injection-molded wood grain decorative board, comprising:

[0009] The decorative board body is integrally injection-molded from materials of at least two colors, and after molding, the decorative board body is formed to have a uniform base color and wood-grain decorative stripes.

[0010] As a further improvement of the present invention, the wood grain-like decorative stripes of the decorative board body are covered on its uniform base color.

[0011] As a further improvement of the present invention, the direction of the wood grain-like decorative stripes is arranged in a curved shape.

[0012] As a further improvement of the present invention, the decorative panel body has a single inlet gate, and the two colors of materials are injected and molded through the inlet gate.

[0013] A method for preparing an injection-molded wood-grain decorative board is also provided, comprising the following steps:

[0014] S1, using injection barrel A and injection barrel B to synchronously inject material A and material B into the same composite nozzle respectively;

[0015] S2, the composite nozzle includes a diverter shuttle, a shared chamber and a nozzle hole, wherein the diverter shuttle has an ejection hole A and an ejection hole B, material A enters the shared chamber through the ejection hole A, material B enters the shared chamber through the ejection hole B, and the two materials in the shared chamber are ejected outward through the nozzle hole;

[0016] S3. The two materials ejected from the nozzle hole are injected into the mold and formed into the decorative panel body.

[0017] As a further improvement of the present invention, in step S2, the injection speed of injection barrel B is controlled to be greater than the injection speed of injection barrel A.

[0018] As a further improvement of the present invention, the aperture of the nozzle hole is smaller than the diameter of the shared chamber, and a conical surface transition is provided between the two. When the material B enters the nozzle hole along the inner wall of the shared chamber and the conical surface wall, the injection speed of the ejection hole B is controlled to be greater than the injection speed of the ejection hole A, so that the material B is spirally wound around the outer peripheral surface of the material A.

[0019] As a further improvement of the present invention, in step S3, the two materials ejected from the nozzle hole can be split and injected into two molds at one time to form two decorative panel bodies.

[0020] Compared with the prior art, the present invention has the following beneficial effects:

[0021] 1. The decorative panel body is formed by one-piece injection molding, using a two-color material mixed injection molding process, which can form a structure with both uniform base color and wood grain-like decorative stripes in one molding process, achieving a highly simulated natural wood texture effect;

[0022] 2. Injection-molded decorative panels can better reproduce the three-dimensional texture and color gradient of wood, and their wood grain patterns are more realistic. Unlike traditional Polaroid veneers, which are limited to flat printing, they have more advantages in visual aesthetics;

[0023] 3. The injection molded decorative panel body has no delamination phenomenon, and there is no appearance damage caused by wear or peeling of the surface material. The service life is significantly extended, and it has excellent scratch and wear resistance;

[0024] 4. Environmental protection and cost-effectiveness: The injection molding process avoids the large consumption of natural wood, which is in line with the modern green environmental protection concept. In addition, the integrated production process simplifies the process steps, reduces production costs and improves economic benefits.

[0025] 5. The injection molded decorative panels can adjust the formula and process parameters as needed to accurately control the product's hardness, impact resistance, corrosion resistance and other physical properties to adapt to different application environments and needs. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 It is a flow chart of the method for preparing the injection-molded wood-grain decorative board of the present invention;

[0027] Figure 2 It is a schematic diagram of the structure of the composite nozzle of the present invention;

[0028] Figure 3 It is a cross-sectional view of the composite nozzle of the present invention.

[0029] In the figure, 100, compound nozzle; 110, split flow shuttle; 111, ejection hole A; 112, ejection hole B; 120, shared chamber; 130, nozzle hole; 140, cone surface. DETAILED DESCRIPTION

[0030] The following are specific embodiments of the present invention and the accompanying drawings to further describe the technical method of the present invention, but the present invention is not limited to these embodiments.

[0031] like Figure 1-3 As shown, the present invention provides an injection-molded wood grain decorative board, characterized in that it includes:

[0032] The decorative board body is integrally injection-molded from materials of at least two colors, and after molding, a decorative board body having a uniform base color and wood-grain decorative stripes is formed.

[0033] It should be noted that the decorative panel body in this embodiment is integrally formed by injection molding, and a two-color material mixed injection molding process is adopted, so that a structure with both a uniform base color and wood grain-like decorative stripes can be formed in a one-time molding process, achieving an effect of highly simulating the texture of natural wood. The advantages are:

[0034] 1. Visual effect: Injection-molded decorative panels can better reproduce the three-dimensional texture and color gradient of wood, and their wood grain patterns are more realistic. Unlike traditional Polaroid veneers that are limited to flat printing, they have more advantages in visual beauty;

[0035] 2. Durability and stability: The injection molded decorative panel body has no delamination phenomenon, and there is no appearance damage caused by wear or peeling of the surface material. The service life is significantly extended, and it has excellent scratch and wear resistance.

[0036] 3. Environmental protection and cost-effectiveness: The injection molding process avoids the large-scale consumption of natural wood, which is in line with the modern green environmental protection concept. In addition, the integrated production process simplifies the process steps, reduces production costs and improves economic benefits.

[0037] 4. Controllable performance: The injection molded decorative panels can adjust the formula and process parameters as needed to accurately control the product's hardness, impact resistance, corrosion resistance and other physical properties to adapt to different application environments and needs.

[0038] Preferably, the wood grain-like decorative stripes of the decorative board body are covered on its uniform base color, wherein, by flexibly matching raw materials of different tones, the color changes and texture characteristics of various woods can be accurately simulated, thereby achieving extremely high visual realism, making the final product look like a real wooden decorative board.

[0039] Preferably, the direction of the wood grain decorative stripes is arranged in a curved shape, deliberately simulating the grain curve of natural wood, just like the natural elements such as annual rings, knots, grain direction formed during the growth of trees, creating a strong three-dimensional visual effect and tactile experience. This curved wood grain arrangement greatly enhances the realism of the decorative board, making it almost comparable to natural wood in appearance, bringing users a sensory enjoyment closer to nature.

[0040] In addition, this curved wood grain design has a high artistic value and can add a unique charm and style to interior decoration. Compared with decorative panels with straight lines or regular patterns, its dynamic and smooth lines can better reflect the designer's deep understanding and careful interpretation of natural aesthetics, so that the decorative panels can meet functional requirements while also having the functions of artistic aesthetics and emotional expression, greatly enhancing the overall decorative effect and quality of the space.

[0041] Preferably, the decorative board body has a single inlet gate, and the two colors of materials are injected and molded through the inlet gate, thereby achieving the purpose of one-time injection molding of the product. This single-inlet two-color injection molding process not only simplifies the production process, reduces subsequent processing links, and effectively reduces production costs, but also can accurately manufacture a decorative board body with rich wood grain effects and uniform base color at one time, ensuring the consistency and stability of the product. More importantly, it successfully solves the problem of insufficient fidelity of the wood grain effect of traditional decorative boards, giving the product higher aesthetic value and market competitiveness.

[0042] The present invention also provides a method for preparing an injection-molded wood-grain decorative board, comprising the following steps:

[0043] S1. First, two independent injection barrels, namely, injection barrel A and injection barrel B, are used to load materials A and material B of different colors respectively. The two barrels work synchronously to melt the plastic particles of different colors carried by each barrel, and then precisely control the flow rate and pressure to deliver the molten materials to the same composite nozzle 100;

[0044] S2. The composite nozzle 100 includes a diverter shuttle 110, a shared chamber 120 and a nozzle hole 130, wherein the diverter shuttle 110 has an ejection hole A111 and an ejection hole B112, material A enters the shared chamber 120 through the ejection hole A111, material B enters the shared chamber 120 through the ejection hole B112, and the two materials in the shared chamber 120 are ejected outward through the nozzle hole 130;

[0045] S3. The two materials ejected from the nozzle hole 130 are injected into the mold and formed into a decorative panel body.

[0046] The entire injection molding process only requires one operation to complete the manufacturing of the decorative panel body, without the need for additional post-processing such as painting and veneer, which significantly improves production efficiency and saves a lot of time and cost. At the same time, due to the one-time molding process, compared with the traditional multi-step manufacturing method, the energy consumption is significantly reduced, which is more in line with the current concept of green manufacturing and sustainable development.

[0047] More importantly, the decorative panels formed by this method have excellent imitation wood grain effects, with clear and natural wood grain textures. Both the color transition and the texture are very close to natural wood, which greatly meets consumers' requirements for the aesthetics of home decoration materials.

[0048] In addition, since artificial synthetic materials are used instead of directly utilizing natural wood, the consumption of forest resources is reduced, the ecological environment is protected from the source, and the perfect combination of decorative effects and environmental protection properties is truly achieved.

[0049] Preferably, in step S2, the injection speed of injection barrel B is controlled to be greater than the injection speed of injection barrel A.

[0050] Furthermore, the aperture of the nozzle hole 130 is smaller than the diameter of the shared chamber 120, and the two are transitioned by a conical surface 140. When the material B enters the nozzle hole 130 along the inner wall of the shared chamber 120 and the wall of the conical surface 140, the injection speed of the injection hole B112 is controlled to be greater than the injection speed of the injection hole A111, so that the material B is spirally wound around the outer peripheral surface of the material A.

[0051] That is to say, as long as material B is spirally wound on the outer peripheral surface of material A in the shared chamber 120, after the two materials are sprayed outward from the nozzle hole 130 and injected into the cavity of the mold, a decorative panel body with wood grain-like decorative stripes can be formed. The internal structure of the decorative panel body formed in this way will show the characteristics of clear layers and interlaced colors similar to natural wood grain, thereby achieving a highly simulated decorative purpose.

[0052] Specifically, material A usually represents the base color or lighter color, which is equivalent to the background color of the wood grain, while material B is the dark part, which is used to simulate the texture of the wood grain. By precisely controlling the injection speed, the diameter of the nozzle hole 130, and the transition design of the cone surface 140 between the shared chamber 120 and the nozzle hole 130, it can be ensured that the two materials can maintain an ideal interweaving state at the moment of contact and in the subsequent cooling and curing process, and finally obtain a wood grain decorative board product with realistic appearance and excellent texture.

[0053] Preferably, in step S3, the two pre-mixed materials ejected from the nozzle hole 130 are not limited to being injected into one mold to form a decorative panel body, but the mixed molten materials can be injected into two independent molds at one time through an appropriate diversion device. In this way, two decorative panel bodies with the same wood grain decorative effect can be formed in the same time period, which greatly improves production efficiency and reduces the production time cost per unit product, which is particularly beneficial for mass production.

[0054] The technical means disclosed in the scheme of the present invention are not limited to the technical means disclosed in the above technical means, but also include technical schemes composed of any combination of the above technical features. The above is a specific implementation of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention, and these improvements and modifications are also regarded as the protection scope of the present invention.

[0055] It should be noted that all directional indications in the embodiments of the present invention (such as up, down, left, right, front, back, etc.) are only used to explain the relative position relationship, movement status, etc. between the components under a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication will also change accordingly.

[0056] In addition, in the present invention, descriptions such as "first", "second", "one", etc. are only used for descriptive purposes and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" or "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.

[0057] In the present invention, unless otherwise clearly specified and limited, the terms "connection", "fixation", etc. should be understood in a broad sense. For example, "fixation" can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0058] In addition, the technical solutions between the various embodiments of the present invention can be combined with each other, but it must be based on the fact that ordinary technicians in the field can implement it. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such combination of technical solutions does not exist and is not within the scope of protection required by the present invention.

Claims

1. An injection molded wood grain decorative board, characterized in that: include: The decorative board body is integrally injection-molded from materials of at least two colors, and after molding, the decorative board body is formed to have a uniform base color and wood-grain decorative stripes.

2. The injection molded wood grain decorative board according to claim 1, characterized in that: The wood grain-like decorative stripes of the decorative board body are covered on its uniform base color.

3. The injection molded wood grain decorative board according to claim 1, characterized in that: The direction of the wood grain-like decorative stripes is arranged in a curve shape.

4. The injection molded wood grain decorative board according to claim 1, characterized in that: The decorative panel body has a single inlet gate, and materials of two colors are injected and molded through the inlet gate.

5. A method for preparing an injection-molded wood-grain decorative board according to any one of claims 1 to 4, characterized in that: The steps include: S1, using injection barrel A and injection barrel B to synchronously inject material A and material B into the same composite nozzle respectively; S2, the composite nozzle includes a diverter shuttle, a shared chamber and a nozzle hole, wherein the diverter shuttle has an ejection hole A and an ejection hole B, material A enters the shared chamber through the ejection hole A, material B enters the shared chamber through the ejection hole B, and the two materials in the shared chamber are ejected outward through the nozzle hole; S3. The two materials ejected from the nozzle hole are injected into the mold and formed into the decorative panel body.

6. The method for preparing an injection-molded wood-grain decorative board according to claim 5, characterized in that: In step S2, the injection speed of injection barrel B is controlled to be greater than the injection speed of injection barrel A.

7. The method for preparing an injection-molded wood-grain decorative board according to claim 5, characterized in that: The aperture of the nozzle hole is smaller than the diameter of the shared chamber, and there is a conical transition between the two. When material B enters the nozzle hole along the inner wall of the shared chamber and the conical wall, the injection speed of the ejection hole B is controlled to be greater than the injection speed of the ejection hole A, so that material B is spirally wound around the outer peripheral surface of material A.

8. The method for preparing an injection-molded wood-grain decorative board according to claim 5, characterized in that: In step S3, the two materials ejected from the nozzle hole can be split and injected into two molds at one time to form two decorative board bodies.

Citation Information

Patent Citations

  • Double-color spiral curve thermal insulation double-layer cup and preparation method thereof

    CN116849499A

  • Nozzle, color mixing injection molding machine and gradient texture injection molding method

    CN117001937A