TPU color-changing film and processing technology thereof

Through the hot-melt compounding of low-temperature TPU masterbatch and high-temperature TPU base material, a transparent wear-resistant coating and color film are formed, which solves the problem of easy scratching and curling of the color-changing film, and achieves higher wear resistance and composite fastness. Spend.

CN118810089APending Publication Date: 2024-10-22JINJIANG YONGGU TEXTILE COATING CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202410908237.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-08
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

The color layer of the existing color-changing film is easily affected by scratches and impacts, causing marks to appear, and the peeling strength of the pressure-sensitive adhesive layer and the TPU substrate is insufficient, causing curling problems.

Method used

Low-temperature TPU masterbatch is cast on the surface of pearlescent paper to form compound A, and hot-melt compounded with high-temperature TPU base material through large-diameter heating rollers and rubber pressing rollers to form a transparent wear-resistant polyurethane coating and polyurethane color film, replacing The traditional pressure-sensitive adhesive layer enhances the composite fastness and flatness of the shelf.

Benefits of technology

It improves the wear resistance and composite fastness of the TPU color-changing film, prevents scratch marks, enhances the color durability of the color film, and effectively improves the curling problem.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118810089A_ABST
    Figure CN118810089A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of multilayer films, in particular to a TPU color-changing film and a processing technology thereof.The processing technology comprises the steps that a composite material A composed of pearlescent paper and a low-temperature hot-melt film is prepared through tape casting; preparing a composite material B with release paper, a transparent wear-resistant polyurethane coating, a polyurethane color film, a polyurethane adhesive layer and a high-temperature TPU (Thermoplastic Polyurethane) base material; and after the composite material A is attached to the outer wall face of the large-diameter heating roller to run for a certain distance, the composite material A and the composite material B are attached and pressed between the first rubber pressing roller and the large-diameter heating roller, and the composite material A and the composite material B which are attached together continue to run backwards in the mode of being attached to the roller till the composite material A and the composite material B are laminated again through the second rubber pressing roller. The surface wear resistance of the TPU color-changing film is improved through the transparent wear-resistant polyurethane coating, the heating area and the heating time of the low-temperature hot-melt film are greatly increased on the whole through improvement of the compounding process, the low-temperature hot-melt film obtains a better hot-melt bonding effect through sufficient and stable heating, the interlayer firmness is more stable, and the hemming problem is obviously solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of multilayer films, and in particular to a TPU color-changing film and a processing technology thereof. Background Art

[0002] Color-changing films are widely used in the fields of shoe uppers, decorative films, lettering films, etc. The conventional color-changing films use the following method to color the TPU substrate: a colorant and a polyurethane resin are used to configure a PU coating, and a layer of PU coating is evenly applied on the surface of the TPU substrate to form a color layer. Then, a pressure-sensitive adhesive layer is applied on the other side of the TPU substrate coated with the color layer, and a release layer is applied at the same time. The color layer of the color-changing film prepared in this way is directly exposed to the environment, and it is easy to produce obvious marks due to scratches or impacts during use, which affects the long-lasting beauty of the product, especially some brighter and more vivid colors, as well as silver, gold, and mirror color films. At the same time, the pressure-sensitive adhesive layer is used as a functional layer for the color-changing film to adhere to the carrier. It is difficult to achieve excellent peeling strength with the TPU substrate through conventional direct coating or transfer coating processes. Even after a heated lamination operation, conventional lamination only uses an upper and lower roller structure, and the heat and pressure are not sufficient and uniform, and curling is prone to occur. Summary of the invention

[0003] The object of the present invention is to provide a TPU color-changing film and a processing technology thereof, which can enhance the composite fastness of the layers and improve the curling problem.

[0004] To achieve the above object, the technical solution adopted by the present invention is: The processing technology of TPU color-changing film specifically includes the following steps: The low-temperature TPU masterbatch is melted on the machine and then cast on the surface of the pearl paper, cooled and rolled up for use, thereby obtaining a composite material A consisting of the pearl paper and the low-temperature hot-melt film on its surface; A polyurethane coating is coated on the surface of the release paper, and a transparent wear-resistant polyurethane coating is obtained after drying; then a polyurethane color glue is coated on the surface of the transparent wear-resistant polyurethane coating, and a polyurethane color film is obtained after drying on the surface of the transparent wear-resistant polyurethane coating; then a polyurethane adhesive is coated on the surface of the polyurethane color film, and a high-temperature TPU substrate is covered after drying until it is half dry, and finally drying, cooling, and winding for standby use, thereby obtaining a composite material B having a release paper, a transparent wear-resistant polyurethane coating, a polyurethane color film, a polyurethane adhesive layer, and a high-temperature TPU substrate; Composite material A and composite material B are unrolled and enter the composite unit respectively, and the composite unit includes a large-diameter heating roller, a first rubber pressing roller and a second rubber pressing roller. Composite material A adheres to the outer wall of the large-diameter heating roller and runs for a distance with the rotation of the large-diameter heating roller, and then is pressed tightly with composite material B between the first rubber pressing roller and the large-diameter heating roller. The low-temperature hot-melt film and the high-temperature TPU substrate are bonded to each other, and then the bonded composite material A and composite material B continue to adhere to the outer wall of the large-diameter heating roller and run backward with the rotation of the large-diameter heating roller until they are laminated again between the second rubber pressing roller and the large-diameter heating roller, and finally leave the large-diameter heating roller from the second rubber pressing roller, cool, and peel off the release paper to obtain the TPU color-changing film.

[0005] Preferably, the polyurethane color glue comprises the following components in parts by weight: 50-60 parts of aqueous polyurethane emulsion, 10-20 parts of aqueous color paste, 0.5-1.5 parts of defoaming agent, 0.5-1 parts of leveling agent, 0.2-0.6 parts of thickener, and 0.5-2 parts of wetting and dispersing agent.

[0006] Preferably, the polyurethane coating is a two-component polyurethane coating.

[0007] Preferably, the transparent wear-resistant polyurethane coating has a 100% modulus of elongation in the longitudinal direction at 23°C of 100 kg / cm 2 ~130kg / cm 2 .

[0008] Preferably, the melting point of the low-temperature hot melt film is 70°C to 100°C, the surface temperature of the large-diameter heating roller is 15°C to 25°C higher than the melting point of the low-temperature hot melt film; the melting point of the high-temperature TPU substrate is 160°C to 180°C.

[0009] Preferably, the pressing pressure of the first rubber pressing roller and the second rubber pressing roller on the laminated composite material A and composite material B is 1.5 kg / cm 2 ~3.0kg / cm 2 .

[0010] Preferably, the composite material B is subjected to plasma pretreatment on the bonding surface of the high-temperature TPU substrate before entering the large-diameter heated roller.

[0011] Preferably, the large-diameter heating roller has a diameter of 100 cm to 150 cm and a line speed of 15 m / min to 35 m / min.

[0012] Preferably, the distance that the composite material A runs along the outer wall of the large diameter heating roller as the large diameter heating roller rotates is 5 / 36 to 9 / 36 of the outer circumference of the large diameter heating roller, and the distance that the composite material A and the composite material B bonded together run along the outer wall of the large diameter heating roller as the large diameter heating roller rotates is 20 / 36 to 23 / 36 of the outer circumference of the large diameter heating roller.

[0013] The present invention also provides a TPU color-changing film made by the above-mentioned processing technology, comprising a high-temperature TPU substrate, a low-temperature hot-melt film is provided on the lower surface of the high-temperature TPU substrate, and pearlescent paper is provided on the side of the low-temperature hot-melt film away from the high-temperature TPU substrate; a polyurethane color film is bonded to the upper surface of the high-temperature TPU substrate through a polyurethane adhesive layer, and a transparent wear-resistant polyurethane coating is provided on the side of the polyurethane color film away from the high-temperature TPU substrate.

[0014] Compared with the prior art, the present invention has the following beneficial effects: The TPU color-changing film of the present invention comprises a high-temperature TPU substrate, a polyurethane color film, a transparent wear-resistant polyurethane coating and a low-temperature hot-melt film. The polyurethane color film is covered and sealed by the transparent wear-resistant polyurethane coating, thereby improving the surface wear resistance of the TPU color-changing film. When there are scratches, the color film will not be directly damaged, thereby protecting the color of the color film to remain as good as new for a long time. Under a pressure of 9KPa, there is no wear after grinding for 1000 revolutions.

[0015] At the same time, the present invention uses a low-temperature hot-melt film instead of conventional pressure-sensitive adhesive as the bonding medium layer between the TPU color-changing film and the carrier interface, and realizes hot-melt composite with the high-temperature TPU substrate through the low-temperature hot-melt film. Compared with the conventional cast composite process on the high-temperature TPU substrate and the conventional coating process of the pressure-sensitive adhesive, higher composite fastness can be obtained; and during the composite, the composite material A composed of the low-temperature hot-melt film and the pearlescent paper is first preheated and heated on the outer wall of the large-diameter heating roller, and then laminated with the composite material B containing the high-temperature TPU substrate and continues to be heated by the large-diameter heating roller. The diameter of the large-diameter heating roller is 100cm to 150cm. On the one hand, the bonding surface of the composite material A is softened so as to facilitate The composite material B can smoothly enter and fit the composite material A, which has a good effect on ensuring the flatness of the fit between the composite materials A and B and inhibiting local wrinkles. On the other hand, it greatly increases the heating area and heating time of the low-temperature hot melt film. After sufficient and stable heating, and in the process of being transmitted backward against the large-diameter heating roller for more than half a circle, the composite materials A and B themselves produce a tendency to squeeze the wrapping pressure of the large-diameter heating roller, so that the low-temperature hot melt film obtains a better hot melt bonding effect. Then, the rubber pressing roller is used to apply pressure to fit the various layers of the composite material B and the composite material A tightly together. The interlayer firmness is more stable and flat, and the curling problem is significantly improved. In addition, the roughness of the fitting surface of the high-temperature TPU substrate is increased through plasma pretreatment, which is conducive to enhancing the bonding firmness of the low-temperature hot melt film and the high-temperature TPU substrate, and it is not easy to fall off.

[0016] Furthermore, the transparent wear-resistant polyurethane coating of the present invention adopts a two-component polyurethane coating, which forms a coating with good transparency and wear resistance after drying, and strictly controls the modulus of the transparent wear-resistant polyurethane coating to ensure the wear resistance and flexibility of the TPU color-changing film. At the same time, the two-component polyurethane coating is cross-linked and cured during the preparation of the composite material B and is shaped. During compounding, it is no longer affected by the full heat of the large-diameter heating roller, thereby ensuring the lamination effect. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 Schematic diagram of the composite material A and the composite material B of the present invention.

[0018] Figure 2 It is a schematic diagram of the structure of the TPU color-changing film of the present invention. DETAILED DESCRIPTION

[0019] In order to make the above features and advantages of the present invention more obvious and easy to understand, embodiments are given below with reference to the accompanying drawings for detailed description as follows.

[0020] Example 1 like Figure 2 As shown, the present embodiment provides a TPU color changing film, including a high-temperature TPU substrate 10, a low-temperature hot-melt film 22 is provided on the lower surface of the high-temperature TPU substrate 10, and a pearlescent paper 21 is provided on the side of the low-temperature hot-melt film 22 away from the high-temperature TPU substrate 10; a polyurethane color film 31 is bonded to the upper surface of the high-temperature TPU substrate 10 through a polyurethane adhesive layer, and a transparent wear-resistant polyurethane coating 32 is provided on the side of the polyurethane color film 31 away from the high-temperature TPU substrate 10.

[0021] The processing technology of the TPU color-changing film specifically includes the following steps: S1. The low-temperature TPU masterbatch is melted on the machine and then cast on the surface of the pearl paper 21, cooled and rolled up for use, to obtain a composite material A consisting of the pearl paper 21 and the low-temperature hot-melt film 22 on its surface. The thickness of the low-temperature hot-melt film 22 is 15 μm and the melting point is 80° C.

[0022] S2, coating the surface of the release paper 33 with a polyurethane coating, wherein the polyurethane coating is a two-component polyurethane coating GPU401, and drying to obtain a transparent wear-resistant polyurethane coating 32, wherein the 100% modulus of elongation in the longitudinal direction at 23° C. after drying is 100 kg / cm 2; Then, a polyurethane color glue is applied on the surface of the transparent wear-resistant polyurethane coating 32. The polyurethane color glue includes the following components in parts by weight: 60 parts of an aqueous polyurethane emulsion with a solid content of 30%, 10 parts of an aqueous color paste, 1 part of a defoaming agent, 0.6 parts of a leveling agent, 0.4 parts of a thickener, and 1 part of a wetting and dispersing agent. After drying, a polyurethane color film 31 with a thickness of 30 μm on the surface of the transparent wear-resistant polyurethane coating 32 is obtained; then, a polyurethane adhesive is applied on the surface of the polyurethane color film 31, and after drying until semi-dry, a high-temperature TPU substrate 10 with a melting point of 165°C is covered thereon. Finally, the polyurethane color film 31 is dried, cooled, and rolled up for use, to obtain a composite material B having a release paper 33, a transparent wear-resistant polyurethane coating 32, a polyurethane color film 31, a polyurethane adhesive layer, and a high-temperature TPU substrate 10.

[0023] S3, composite material A and composite material B are unwound separately, and enter the composite unit after passing through the stenter roller, such as Figure 1 As shown, the composite unit includes a large-diameter heating roller 11, a first rubber pressing roller 12 and a second rubber pressing roller 13. The first rubber pressing roller 12 and the second rubber pressing roller 13 are arranged in sequence along the rotation direction of the large-diameter heating roller 11 and close to the large-diameter heating roller 11. The large-diameter heating roller 11 has a diameter of 100 cm and a line speed of 20 m / min. The large-diameter heating roller 11 is heated by an electric heating wire and its surface temperature is 15°C higher than the melting point of the low-temperature hot melt film 22. The diameters of the first rubber pressing roller 12 and the second rubber pressing roller 13 are both 50 cm.

[0024] The composite material A adheres to the outer wall of the large diameter heating roller 11 and rotates along the large diameter heating roller 11 for 5 / 36 of the outer circumference of the large diameter heating roller 11. Then, it is pressed against the composite material B between the first rubber pressing roller 12 and the large diameter heating roller 11. The pressing pressure is 2.5 kg / cm 2 The low-temperature hot-melt film 22 and the high-temperature TPU substrate 10 are laminated to each other, and then the laminated composite materials A and B continue to adhere to the outer wall of the large-diameter heating roller 11 and move backward along the rotation of the large-diameter heating roller 11 by 21 / 36 of the outer circumference of the large-diameter heating roller 11 until they are laminated again between the second rubber pressing roller 13 and the large-diameter heating roller 11. The pressing pressure is 2.0 kg / cm 2 Finally, the second rubber pressing roller 13 leaves the large-diameter heating roller 11, cools and peels off the release paper 33 to obtain the TPU color-changing film.

[0025] The composite material B is subjected to plasma pretreatment on the bonding surface of the high-temperature TPU substrate 10 before entering the large-diameter heating roller 11. Specifically, the plasma gas is 0.2% oxygen, the rest is argon, the discharge voltage is 2 kV, the discharge time is 150 seconds, and the bias source is 400V.

[0026] Example 2 like Figure 2 As shown, the present embodiment provides a TPU color changing film, including a high-temperature TPU substrate 10, a low-temperature hot-melt film 22 is provided on the lower surface of the high-temperature TPU substrate 10, and a pearlescent paper 21 is provided on the side of the low-temperature hot-melt film 22 away from the high-temperature TPU substrate 10; a polyurethane color film 31 is bonded to the upper surface of the high-temperature TPU substrate 10 through a polyurethane adhesive layer, and a transparent wear-resistant polyurethane coating 32 is provided on the side of the polyurethane color film 31 away from the high-temperature TPU substrate 10.

[0027] The processing technology of the TPU color-changing film specifically includes the following steps: S1. The low-temperature TPU masterbatch is melted on the machine and then cast on the surface of the pearl paper 21, cooled and rolled up for use, to obtain a composite material A consisting of the pearl paper 21 and the low-temperature hot-melt film 22 on its surface. The low-temperature hot-melt film 22 has a thickness of 20 μm and a melting point of 70°C.

[0028] S2, coating the surface of the release paper 33 with a polyurethane coating, wherein the polyurethane coating is a two-component polyurethane coating JG500-92, and drying to obtain a transparent wear-resistant polyurethane coating 32, wherein the 100% modulus of elongation in the longitudinal direction at 23° C. after drying is 120 kg / cm 2 ; Then, a polyurethane color glue is applied on the surface of the transparent wear-resistant polyurethane coating 32. The polyurethane color glue includes the following components in parts by weight: 55 parts of an aqueous polyurethane emulsion with a solid content of 30%, 12 parts of an aqueous color paste, 0.5 parts of a defoaming agent, 0.8 parts of a leveling agent, 0.5 parts of a thickener, and 1 part of a wetting and dispersing agent. After drying, a polyurethane color film 31 with a thickness of 40 μm on the surface of the transparent wear-resistant polyurethane coating 32 is obtained; then, a polyurethane adhesive is applied on the surface of the polyurethane color film 31, and after drying until semi-dry, a high-temperature TPU substrate 10 with a melting point of 180°C is covered thereon. Finally, the polyurethane color film 31 is dried, cooled, and rolled up for use, to obtain a composite material B having a release paper 33, a transparent wear-resistant polyurethane coating 32, a polyurethane color film 31, a polyurethane adhesive layer, and a high-temperature TPU substrate 10.

[0029] S3, composite material A and composite material B are unwound separately, and enter the composite unit after passing through the stenter roller, such as Figure 1 As shown, the composite unit includes a large-diameter heating roller 11, a first rubber pressing roller 12 and a second rubber pressing roller 13, and the first rubber pressing roller 12 and the second rubber pressing roller 13 are arranged in sequence along the rotation direction of the large-diameter heating roller 11 and close to the large-diameter heating roller 11. The large-diameter heating roller 11 has a diameter of 150 cm and a line speed of 30 m / min. The large-diameter heating roller 11 is heated by heat-conducting oil and its surface temperature is 20°C higher than the melting point of the low-temperature hot melt film 22, and the diameters of the first rubber pressing roller 12 and the second rubber pressing roller 13 are both 50 cm.

[0030] The composite material A adheres to the outer wall of the large diameter heating roller 11 and rotates along the large diameter heating roller 11 for 8 / 36 of the outer circumference of the large diameter heating roller 11. Then, it is pressed tightly with the composite material B between the first rubber pressing roller 12 and the large diameter heating roller 11. The pressing pressure is 2.0 kg / cm 2 The low-temperature hot-melt film 22 and the high-temperature TPU substrate 10 are laminated to each other, and then the laminated composite materials A and B continue to adhere to the outer wall of the large-diameter heating roller 11 and move backward along the rotation of the large-diameter heating roller 11 by 21 / 36 of the outer circumference of the large-diameter heating roller 11 until they are laminated again between the second rubber pressing roller 13 and the large-diameter heating roller 11. The pressing pressure is 1.5 kg / cm 2 Finally, the second rubber pressing roller 13 leaves the large-diameter heating roller 11, cools and peels off the release paper 33 to obtain the TPU color-changing film.

[0031] The composite material B is subjected to plasma pretreatment on the bonding surface of the high-temperature TPU substrate 10 before entering the large-diameter heating roller 11. Specifically, the plasma gas is 0.2% oxygen, the rest is argon, the discharge voltage is 2 kV, the discharge time is 150 seconds, and the bias source is 400V.

[0032] Comparative Example 1 The difference between this comparative example and the above-mentioned Example 1 is that the composite material B and the composite material A are introduced together and conveyed backward to the second rubber pressing roller 13 against the large-diameter heating roller 11. The peel strength between the low-temperature hot-melt film and the high-temperature TPU substrate of this comparative example 1 is reduced by 8.5% compared with that of Example 1, and wrinkles appear in a local area of ​​the comparative example 1.

[0033] The above shows and describes the basic principles, main features and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only for illustrating the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which shall fall within the scope of the present invention to be protected. The scope of protection of the present invention shall be defined by the attached claims and their equivalents.

Claims

1. TPU color changing film processing technology, It is characterized in that The specific steps include: The low-temperature TPU masterbatch is melted on the machine and then cast on the surface of the pearl paper, cooled and rolled up for use, thereby obtaining a composite material A consisting of the pearl paper and the low-temperature hot-melt film on its surface; A polyurethane coating is coated on the surface of the release paper, and a transparent wear-resistant polyurethane coating is obtained after drying; then a polyurethane color glue is coated on the surface of the transparent wear-resistant polyurethane coating, and a polyurethane color film is obtained after drying on the surface of the transparent wear-resistant polyurethane coating; then a polyurethane adhesive is coated on the surface of the polyurethane color film, and a high-temperature TPU substrate is covered after drying until it is half dry, and finally drying, cooling, and winding for standby use, thereby obtaining a composite material B having a release paper, a transparent wear-resistant polyurethane coating, a polyurethane color film, a polyurethane adhesive layer, and a high-temperature TPU substrate; Composite material A and composite material B are unrolled and enter the composite unit respectively, and the composite unit includes a large-diameter heating roller, a first rubber pressing roller and a second rubber pressing roller. Composite material A adheres to the outer wall of the large-diameter heating roller and runs for a distance with the rotation of the large-diameter heating roller, and then is pressed tightly with composite material B between the first rubber pressing roller and the large-diameter heating roller. The low-temperature hot-melt film and the high-temperature TPU substrate are bonded to each other, and then the bonded composite material A and composite material B continue to adhere to the outer wall of the large-diameter heating roller and run backward with the rotation of the large-diameter heating roller until they are laminated again between the second rubber pressing roller and the large-diameter heating roller, and finally leave the large-diameter heating roller from the second rubber pressing roller, cool, and peel off the release paper to obtain the TPU color-changing film.

2. The TPU color-changing film processing technology according to claim 1, Features: The polyurethane color glue comprises the following components in parts by weight: 50-60 parts of water-based polyurethane emulsion, 10-20 parts of water-based color paste, 0.5-1.5 parts of defoaming agent, 0.5-1 parts of leveling agent, 0.2-0.6 parts of thickener, and 0.5-2 parts of wetting and dispersing agent.

3. The TPU color-changing film processing technology according to claim 1, Features: The polyurethane coating is a two-component polyurethane coating.

4. The TPU color-changing film processing technology according to claim 5, Features: The transparent wear-resistant polyurethane coating has a 100% modulus of elongation in the longitudinal direction at 23°C of 100 kg / cm 2 ~130kg / cm 2 .

5. The TPU color-changing film processing technology according to claim 1, Features: The melting point of the low-temperature hot-melt film is 70°C to 100°C, the surface temperature of the large-diameter heating roller is 15°C to 25°C higher than the melting point of the low-temperature hot-melt film; the melting point of the high-temperature TPU substrate is 160°C to 180°C.

6. The TPU color-changing film processing technology according to claim 1, Features: The pressing pressure of the first rubber pressing roller and the second rubber pressing roller on the laminated composite material A and composite material B is 1.5 kg / cm 2 ~3.0kg / cm 2 .

7. The TPU color-changing film processing technology according to claim 1, Features: The composite material B is subjected to plasma pretreatment on the bonding surface of the high-temperature TPU substrate before entering the large-diameter heated roller.

8. The TPU color-changing film processing technology according to claim 1, Features: The large-diameter heating roller has a diameter of 100 cm to 150 cm and a line speed of 15 m / min to 35 m / min.

9. The TPU color-changing film processing technology according to claim 8, Features: The distance that the composite material A adheres to the outer wall of the large diameter heating roller as the large diameter heating roller rotates is 5 / 36 to 9 / 36 of the outer circumference of the large diameter heating roller. The distance that the composite material A and the composite material B bonded together adhere to the outer wall of the large diameter heating roller as the large diameter heating roller rotates is 20 / 36 to 23 / 36 of the outer circumference of the large diameter heating roller.

10. A TPU color-changing film, Features: It is made by the processing technology as described in any one of claims 1 to 9, comprising a high-temperature TPU substrate, a low-temperature hot-melt film is provided on the lower surface of the high-temperature TPU substrate, and pearl paper is provided on the side of the low-temperature hot-melt film away from the high-temperature TPU substrate; a polyurethane color film is bonded to the upper surface of the high-temperature TPU substrate through a polyurethane bonding layer, and a transparent wear-resistant polyurethane coating is provided on the side of the polyurethane color film away from the high-temperature TPU substrate.

Citation Information

Patent Citations

  • Sewing-free hot melt adhesive TPU-PU leather and preparation method thereof

    CN103437195A

  • TPU (thermoplastic polyurethane) high-low temperature film with repairing function and preparation method thereof

    CN115785834A

  • Washable soft metal heat transfer printing lettering film

    CN213501605U

  • Composite device for compounding reflective material

    CN213798583U

  • Self-repairing TPU (thermoplastic polyurethane) high-low temperature film

    CN219279781U