Etching stop layer preparation method and semiconductor structure
By using shielding layers and ultraviolet light irradiation technology in integrated circuit manufacturing, the problem of stress matching between NMOS and PMOS devices is solved, the performance of NMOS devices is improved without affecting the PMOS devices, and the best performance enhancement effect is achieved.
Patent Information
- Application Number
- CN202410804675.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-20
- Publication Date
- 2024-10-22
AI Technical Summary
In integrated circuit manufacturing, the working principles and structures of N-type MOS transistors (NMOS) and P-type MOS transistors (PMOS) devices are different, which makes it a challenge to use appropriate stress types to achieve optimal performance enhancement. It is difficult for existing technologies to simultaneously Improve the electrical performance of NMOS devices without affecting the performance of PMOS devices.
By forming spaced NMOS and PMOS devices on the substrate, and forming a shielding layer on the PMOS device, using ultraviolet light to irradiate the first stress etching stop layer on the NMOS device to convert it into a second stress etching stop layer , improve the channel mobility of the NMOS device, thereby improving its electrical performance, and the shielding effect of the shielding layer avoids affecting the PMOS device.
It achieves applying matching stress to PMOS and NMOS devices, improves the electrical performance of NMOS devices, while reducing the impact on the electrical performance of PMOS devices, ensuring optimal performance enhancement.
Smart Images

Figure CN118824945A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of integrated circuit manufacturing, and in particular to an etch stop layer preparation method and a semiconductor structure. Background Art
[0002] In integrated circuit manufacturing, as the requirements for device performance continue to increase, various new technical solutions emerge one after another.
[0003] Stress engineering is a widely used method to optimize channel mobility to improve the electrical performance of devices. For example, stress film can effectively improve the performance of PMOS transistors (PMOS).
[0004] However, since the working principles and structures of N-type MOS tubes (NMOS) and PMOS are different, it is a challenge to use the right stress type to achieve the best performance enhancement.
[0005] It should be noted that the information disclosed in the above background technology section is only used to enhance the understanding of the background of the present application, and therefore may include information that does not constitute prior art known to ordinary technicians in the field.
[0006] Application Contents
[0007] Based on this, the embodiments of the present application provide an etch stop layer preparation method and a semiconductor structure, which can improve the electrical performance of the NMOS device while avoiding affecting the electrical performance of the PMOS device, thereby applying matching stresses to the PMOS device and the NMOS device to achieve optimal performance enhancement.
[0008] According to some embodiments, the present application provides, on one hand, a method for preparing an etch stop layer, comprising:
[0009] Providing a substrate on which an NMOS device and a PMOS device are spaced apart are formed; and forming a first stress etch stop layer on the substrate, the NMOS device and the PMOS device;
[0010] forming a blocking layer on the first stress etch stop layer located on the PMOS device;
[0011] The first stress etch stop layer on the NMOS device is irradiated with ultraviolet light, so that the first stress etch stop layer on the NMOS device is converted into a second stress etch stop layer.
[0012] In some embodiments, the shielding layer includes a metal shielding layer.
[0013] In some embodiments, the metal shielding layer includes an aluminum shielding layer.
[0014] In some embodiments, before forming a blocking layer on the first stress etch stop layer on the PMOS device, the preparation method further includes:
[0015] forming a protective layer on a surface of the first stress etch stop layer away from the substrate;
[0016] The step of forming a blocking layer on the first stress etch stop layer located on the PMOS device comprises:
[0017] forming a shielding material layer on a surface of the protection layer away from the first stress etching stop layer;
[0018] The shielding material layer located on the NMOS device is removed, and the shielding material layer located on the PMOS device is retained as the shielding layer.
[0019] In some embodiments, the material of the protection layer includes silicon dioxide.
[0020] In some embodiments, after forming the second stress etching stop layer, the preparation method further includes:
[0021] The protective layer is removed.
[0022] In some embodiments, the material of the first stress etch stop layer includes silicon nitride.
[0023] In some embodiments, the second stress etch stop layer has a tensile stress of at least 1200 MPa.
[0024] In some embodiments, the first stress etch stop layer has a tensile stress ranging from 400 MPa to 600 MPa.
[0025] According to some embodiments, the present application provides a semiconductor structure on the other hand. The process of preparing the semiconductor structure includes the steps of the etch stop layer preparation method described in some of the above embodiments.
[0026] The etch stop layer preparation method and semiconductor structure provided in the present application can or at least have the following advantages:
[0027] In an embodiment of the present application, after forming the first stress etch stop layer, a shielding layer is used to shield the first stress etch stop layer located on the PMOS device, and the steps are simple and easy to implement. After shielding the first stress etch stop layer located on the PMOS device, the first stress etch stop layer located on the NMOS device is irradiated with ultraviolet light, so that this part of the first stress etch stop layer obtains high tensile stress, so as to improve the channel mobility of the NMOS device, thereby improving the electrical performance of the NMOS device. Due to the shielding effect of the shielding layer, the first stress etch stop layer located on the PMOS device will not be affected by ultraviolet light, and a low tensile stress level can be maintained. Therefore, the embodiment of the present application can reduce the impact on the electrical performance of the PMOS device, and apply matching stress to the PMOS device and the NMOS device, thereby achieving optimal performance enhancement.
[0028] In some embodiments, a metal shielding layer is used for shielding. The metal shielding layer not only has good light shielding performance, can effectively block most of the ultraviolet light, and achieve good shielding for the first stress etch stop layer on the PMOS device; it also has high reflectivity. The high reflectivity of the metal shielding layer can be used to reflect ultraviolet light to the first stress etch stop layer located on the side wall of the gate of the NMOS device, thereby effectively improving the defect of insufficient ultraviolet light irradiation at the side wall of the gate. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] Other features, objects and advantages of the present application will become more apparent by reading the detailed description of non-limiting embodiments made with reference to the following drawings.
[0030] Figure 1 A schematic diagram of a process for preparing an etch stop layer provided in some embodiments of the present application;
[0031] Figure 2 A schematic diagram of a process for forming a shielding layer in a method for preparing an etch stop layer provided in some embodiments of the present application;
[0032] Figure 3 A schematic cross-sectional view of a structure obtained after forming a first stress etch stop layer in a method for preparing an etch stop layer provided in some embodiments of the present application;
[0033] Figure 4 A schematic cross-sectional view of a structure obtained after forming a protective layer in a method for preparing an etch stop layer provided in some embodiments of the present application;
[0034] Figure 5 A schematic cross-sectional view of a structure obtained after a shielding material layer is formed in a method for preparing an etch stop layer provided in some embodiments of the present application;
[0035] Figure 6A schematic cross-sectional view of a structure obtained after a shielding layer is formed in a method for preparing an etch stop layer provided in some embodiments of the present application;
[0036] Figure 7 A cross-sectional schematic diagram of ultraviolet light irradiation in a method for preparing an etch stop layer provided in some embodiments of the present application;
[0037] Figure 8 A schematic cross-sectional view of a structure obtained after removing a shielding layer in a method for preparing an etch stop layer provided in some embodiments of the present application;
[0038] Fig. 9 A schematic cross-sectional view of a structure obtained after an interlayer dielectric layer is formed in a method for preparing an etch stop layer provided in some embodiments of the present application.
[0039] Reference numerals:
[0040] 110, substrate; 110a, NMOS device; 110b, PMOS device; 120, first stress etch stop layer; 220, protection layer; 200, shielding material layer; 210, shielding layer; 300, second stress etch stop layer; 400, interlayer dielectric layer. DETAILED DESCRIPTION
[0041] In order to facilitate understanding of the present application, the present application will be described more fully below with reference to the relevant drawings. The preferred embodiments of the present application are given in the drawings. However, the present application can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present application more thorough and comprehensive.
[0042] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which this application belongs. The terms used herein in the specification of this application are only for the purpose of describing specific embodiments and are not intended to limit this application.
[0043] It should be understood that although the terms first, second, etc. may be used to describe various elements, components, regions, layers, doping types and / or portions, these elements, components, regions, layers, doping types and / or portions should not be limited by these terms. These terms are only used to distinguish one element, component, region, layer, doping type or portion from another element, component, region, layer, doping type or portion. Therefore, without departing from the teachings of the present application, the first element, component, region, layer, doping type or portion discussed below may be represented as a second element, component, region, layer or portion; for example, a first stress etch stop layer may be referred to as a second stress etch stop layer, and similarly, a second stress etch stop layer may be referred to as a first stress etch stop layer; the first stress etch stop layer and the second stress etch stop layer are different stress etch stop layers.
[0044] Although the terms "on" and the like may be used in this specification to describe different exemplary features and elements of the present application, these terms are used herein for convenience only, for example, according to the directions of the examples described in the accompanying drawings. Nothing in this specification should be construed as requiring a specific three-dimensional orientation of the structure to fall within the scope of the present application. Furthermore, the illustrations provided in the present embodiment only illustrate the basic concept of the present disclosure in a schematic manner. Although the illustrations only show components related to the present disclosure rather than being drawn according to the number, shape, and size of components in actual implementation, the type, quantity, and proportion of each component in actual implementation may be a random change, and the component layout type may also be more complex.
[0045] When used herein, the singular forms "a", "an", and "said / the" may also include plural forms, unless the context clearly indicates otherwise. It should also be understood that when the terms "consisting of" and / or "comprising" are used in this specification, the presence of the features, integers, steps, operations, elements and / or parts can be determined, but the presence or addition of one or more other features, integers, steps, operations, elements, parts and / or groups is not excluded. At the same time, when used herein, the term "and / or" includes any and all combinations of the relevant listed items.
[0046] As a widely used method, stress engineering is used to optimize channel mobility to improve the electrical performance of devices. For example, stress film can effectively improve the performance of P-type MOS tubes (hereinafter referred to as PMOS). However, since the working principle and structure of N-type MOS tubes (hereinafter referred to as NMOS) are different from those of PMOS, it is a challenge to use the appropriate stress type to achieve the best performance enhancement.
[0047] Based on this, the embodiments of the present application provide an etch stop layer preparation method and a semiconductor structure, which can improve the electrical performance of the NMOS device while avoiding the impact on the electrical performance of the PMOS device, thereby applying matching stresses to the PMOS device and the NMOS device to achieve optimal performance enhancement. The details will be described in subsequent embodiments.
[0048] This application provides a method for preparing an etch stop layer. Figure 1 The method for preparing the etching stop layer may specifically include the following steps S100 to S300:
[0049] S100: providing a substrate on which an NMOS device and a PMOS device are spaced apart are formed; and forming a first stress etch stop layer on the substrate, the NMOS device and the PMOS device.
[0050] S200: forming a blocking layer on a first stress etch stop layer located on a PMOS device.
[0051] S300: irradiating a first stress etch stop layer on the NMOS device with ultraviolet light, so that the first stress etch stop layer on the NMOS device is converted into a second stress etch stop layer.
[0052] After forming the first stress etch stop layer, the embodiment of the present application uses a shielding layer to shield the first stress etch stop layer located on the PMOS device. The steps are simple and easy to implement, and can be well applied to process nodes such as 28nm and 40nm. After shielding the first stress etch stop layer located on the PMOS device, the first stress etch stop layer located on the NMOS device is irradiated with ultraviolet light, so that this part of the first stress etch stop layer obtains high tensile stress, so as to improve the channel mobility of the NMOS device, thereby improving the electrical performance of the NMOS device. Due to the shielding effect of the shielding layer, the first stress etch stop layer located on the PMOS device will not be affected by the ultraviolet light, and a low tensile stress level can be maintained.
[0053] In this way, the embodiments of the present application can reduce the impact on the electrical performance of the PMOS device, apply matching stresses to the PMOS device and the NMOS device, and thus achieve optimal performance enhancement.
[0054] In some embodiments, see Figure 2 Step S200 forms a blocking layer on the first stress etch stop layer located on the PMOS device, which may specifically include the following steps:
[0055] S210: forming a blocking material layer on a surface of the protection layer away from the first stress etching stop layer.
[0056] S220: removing the blocking material layer on the NMOS device, and retaining the blocking material layer on the PMOS device as a blocking layer.
[0057] The following combination Figures 3 to 9 The method for preparing the etch stop layer provided in the embodiment of the present application is described in more detail.
[0058] In step S100, refer to Figure 3 A substrate 110 is provided, on which an NMOS device 110a and a PMOS device 110b are formed at intervals; and a first stress etch stop layer 120 is formed on the substrate 110, the NMOS device 110a and the PMOS device 110b.
[0059] The embodiment of the present application does not specifically limit the material of the first stress etch stop layer 120. In some embodiments, the first stress etch stop layer 120 may include a silicon nitride (SiN) layer. SiN has excellent chemical corrosion resistance and high etching selectivity, which can ensure better effects in stress engineering. In other embodiments, the first stress etch stop layer 120 may also include a silicon carbide (SiC) layer, a silicon oxynitride (SiON) layer, or a film layer of other materials, and is not limited thereto.
[0060] The embodiment of the present application does not specifically limit the tensile stress of the first stress etch stop layer 120. In some embodiments, the tensile stress of the first stress etch stop layer 120 ranges from 400 MPa to 600 MPa; for example, the tensile stress of the first stress etch stop layer 120 may be 400 MPa, 450 MPa, 500 MPa, 550 MPa or 600 MPa, etc.
[0061] In some embodiments, see Figure 4 Before performing the subsequent step S200, a protective layer 220 may be formed on the surface of the first stress etch stop layer 120 away from the substrate 110. The protective layer 220 may be used to protect the first stress etch stop layer 120 and prevent the first stress etch stop layer 120 from being damaged in the subsequent etching process. The protective layer 220 may also serve as an etching stop layer of the shielding layer in the subsequent steps.
[0062] The present embodiment of the present application does not specifically limit the material of the protective layer 220. As an example, the material of the protective layer 220 may include silicon dioxide (SiO 2 ).SiO 2 It has good electrical insulation performance and chemical stability, and is compatible with the first stress etch stop layer 120 (eg, SiN layer). 2 The protective layer 220 of the material can provide excellent mechanical protection and prevent the first stress etching stop layer 120 from being subjected to additional chemical corrosion.
[0063] Exemplarily, the protection layer 220 may also include a passivation layer material, such as polyimide (PI), aluminum nitride (AlN), etc. The passivation layer material has good chemical stability and mechanical strength, and can prevent additional wet etching or plasma etching damage.
[0064] In step S200, refer to Figures 5 and 6 , a blocking layer 210 is formed on the first stress etch stop layer 120 located on the PMOS device 110 b.
[0065] In some embodiments, the shielding layer 210 may specifically include a metal shielding layer, but is not limited thereto.
[0066] The metal shielding layer not only has good light shielding performance, but can also effectively block most of the ultraviolet light, and can also provide good shielding for the first stress etch stop layer 120 on the PMOS device 110b, ensuring that the first stress etch stop layer 120 on the PMOS device 110b will not be affected by the ultraviolet light, thereby maintaining a low tensile stress level. In addition, the metal shielding layer also has a high reflectivity; therefore, the ultraviolet light can be reflected to the first stress etch stop layer 120 on the gate sidewall of the NMOS device 110a by utilizing the high reflectivity of the metal shielding layer, effectively improving the defect of insufficient ultraviolet light irradiation at the gate sidewall, so that the second stress etch stop layer formed in the subsequent steps has a more uniform stress distribution.
[0067] In addition, the metal shielding layer has good chemical corrosion resistance, can maintain stability in the subsequent etching process, reduce the corrosion of the etching solution on the shielding layer 210, and ensure the integrity and functionality of the shielding layer 210. The metal shielding layer also has good mechanical strength, and can provide effective physical protection in the subsequent semiconductor process to prevent external mechanical stress from having adverse effects on the structure obtained in step S100 and other underlying devices.
[0068] In some embodiments, the aforementioned metal shielding layer may include an aluminum (Al) shielding layer, a chromium (Cr) shielding layer and / or a titanium (Ti) shielding layer, but is not limited thereto.
[0069] The aluminum shielding layer has a high reflectivity, especially in the ultraviolet range, and can effectively block most of the light, with a transmittance close to 0. The high reflectivity of the aluminum shielding layer can not only protect the first stress etch stop layer 120 on the PMOS device 110b, but also effectively reflect ultraviolet light to improve the illumination effect at the gate sidewall of the NMOS device 110a. The chromium shielding layer not only has good light shielding performance, but also has good corrosion resistance, which is beneficial to improving the stability of the semiconductor process. The titanium shielding layer has good durability and mechanical strength, and can take into account both light shielding performance and mechanical performance.
[0070] The aluminum shielding layer has a high etching selectivity relative to the first stress etch stop layer 120 (e.g., SiN). Therefore, the aluminum shielding layer is used to shield the first stress etch stop layer 120 located on the PMOS device 110b, which can ensure that when the aluminum shielding layer is removed, the first stress etch stop layer 120 is slightly damaged, and the aluminum shielding layer can maintain integrity during the process, thereby improving the production yield of the etch stop layer preparation method.
[0071] In addition, aluminum has excellent thermal conductivity, so the aluminum shielding layer can effectively dissipate heat and reduce the heat accumulation generated during ultraviolet light irradiation, thereby reducing the impact of thermal stress on the semiconductor structure and protecting the structure obtained in step S100 and other underlying devices. In addition, aluminum is a common and low-cost metal material, so the use of an aluminum shielding layer is also economical. Aluminum has excellent processing performance and is easy to deposit and etch, so forming an aluminum shielding layer as a shielding layer 210 in the above steps also helps to reduce the manufacturing cost and process complexity of the semiconductor process.
[0072] In some embodiments, step S200 may be specifically performed as the following steps S210 to S220.
[0073] In step S210, Figure 5 As shown, a blocking material layer 200 is formed on a surface of the protection layer 220 away from the first stress etching stop layer 120 .
[0074] In step S220, Figure 6 As shown, the blocking material layer 200 located on the NMOS device 110 a is removed, and the blocking material layer 200 located on the PMOS device 110 b is retained as the blocking layer 210 .
[0075] In some embodiments, when removing the blocking material layer 200 on the NMOS device 110 a , the etching stops on the protection layer 220 .
[0076] In step S300, refer to Figure 7 , the first stress etch stop layer 120 on the NMOS device 110a is irradiated with ultraviolet light to convert the first stress etch stop layer 120 on the NMOS device 110a into a second stress etch stop layer 300, for example Figure 8 As shown.
[0077] In the above steps, the chemical bonds in the first stress etch stop layer 120 not shielded by the shielding layer 210 are rearranged by the ultraviolet light irradiation process, thereby changing its internal structure. The energy of the ultraviolet light can break the original silicon-hydrogen bonds and nitrogen-hydrogen bonds in the aforementioned first stress etch stop layer 120 (for example, SiN), forming stronger silicon-nitrogen bonds, causing the aforementioned first stress etch stop layer 120 to undergo microscopic deformation and generate tensile stress. For ease of description, in this application, the first stress etch stop layer 120 irradiated by ultraviolet light is defined as the second stress etch stop layer 300.
[0078] The embodiment of the present application does not specifically limit the tensile stress of the second stress etch stop layer 300. In some embodiments, the second stress etch stop layer 300 has a tensile stress of at least 1200 MPa. For example, after being irradiated with ultraviolet light, the first stress etch stop layer 120 that is not shielded by the shielding layer 210 can be increased from a lower tensile stress level (e.g., 400 MPa to 600 MPa) to at least 1200 MPa.
[0079] It should be noted that, at the same time, due to the shielding effect of the shielding layer 210 , the first stress etch stop layer 120 located on the PMOS device 110 b is not affected by the ultraviolet light, and thus is maintained at a relatively low tensile stress level.
[0080] The embodiment of the present application does not specifically limit the specific parameters for irradiating the first stress etch stop layer 120 located on the NMOS device 110 a with ultraviolet light in step S300 .
[0081] Among them, the ultraviolet light irradiation time can directly affect the conversion effect of the first stress etch stop layer 120. As an example, the ultraviolet light irradiation time range can be between 1 minute and 10 minutes; for example, the ultraviolet light irradiation time of the first stress etch stop layer 120 located on the NMOS device 110a can be 1 minute, 3 minutes, 5 minutes, 8 minutes or 10 minutes, etc. Too short irradiation time (for example, irradiation time less than 1 minute) may result in insufficient tensile stress of the converted second stress etch stop layer 300, and too long irradiation time (for example, irradiation time greater than 10 minutes) may cause material damage caused by excessive irradiation.
[0082] For example, a longer irradiation time (eg, irradiation time ranging from 7 minutes to 10 minutes) can help fully transform the first stress etch stop layer 120, and can avoid material damage caused by excessive irradiation while ensuring that the second stress etch stop layer 300 has sufficient tensile stress.
[0083] In step S300, the wavelength of the ultraviolet light will also have a significant impact on the stress conversion effect of the first stress etch stop layer 120. As an example, ultraviolet light with a wavelength in the range of 200nm to 400nm can be selected. Ultraviolet light with a wavelength in the range of 200nm to 400nm has high energy, which can effectively break silicon-hydrogen bonds and nitrogen-hydrogen bonds, promote the formation of silicon-nitrogen bonds, and thus ensure that the second stress etch stop layer 300 has sufficient tensile stress.
[0084] In addition, the power of the UV light needs to be selected to ensure effective conversion while avoiding damage to the material. As an example, the power of the UV light can be set at 10mW / cm 2 Up to 200mW / cm 2In this way, sufficient stress transformation can be achieved within a reasonable time without causing excessive thermal damage to the material.
[0085] As an example, see Figure 8 , the shielding layer 210 can be removed after the second stress etch stop layer 300 is formed. The embodiment of the present application does not specifically limit the method for removing the shielding layer 210, and the removal method can be adaptively selected according to the process requirements, equipment conditions, and materials to be protected in the actual embodiment. Exemplarily, the shielding layer 210 can be removed by, but not limited to, a wet etching process. The equipment required for the wet etching process is relatively simple, with a low process cost, and the wet etching process is easy to control. The shielding layer 210 can be accurately removed by adjusting the concentration of the etching solution, the process temperature and / or the process time.
[0086] In some embodiments, see Fig. 9 After the second stress etch stop layer 300 is formed and the shielding layer 210 is removed, the protective layer 220 can be removed. The embodiment of the present application does not specifically limit the method for removing the protective layer 220, and the removal method can be adaptively selected according to the process requirements, equipment conditions, and materials to be protected in the actual embodiment.
[0087] For example, the protective layer 220 can be removed by a wet etching process, which not only has a low process cost, but also is easy to control and can accurately remove the protective layer 220. The protective layer 220 can also be removed by a dry etching process, which can accurately control the etching rate and uniformity, and can achieve fine adjustment of the protective layer 220 removal process by adjusting process parameters (such as gas flow, power and pressure, etc.). In addition, the dry etching process also reduces the use of chemical reagents and avoids the problem of waste liquid treatment, thereby improving the cleanliness and environmental friendliness of the etching stop layer preparation method, making the etching stop layer preparation method more suitable for integration into complex multi-step semiconductor processes.
[0088] After removing the protective layer 220, as Fig. 9 As shown, subsequent processes such as forming an inter-level dielectric (ILD) layer 400 on the surface of the first stress etch stop layer 120 away from the substrate 110 may be performed. This is not the focus of the present application and will not be further described here.
[0089] Based on the same inventive concept, the present application also provides a semiconductor structure. In the process of preparing the semiconductor structure, the steps of the etching stop layer preparation method in some of the aforementioned embodiments are included. The display device is, for example, an LED display panel or an LED backplane. The technical effects that can be achieved by the aforementioned etching stop layer preparation method can also be achieved by the semiconductor structure, and will not be described in detail here.
[0090] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features of the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0091] The above-described embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be construed as limiting the scope of the patent application. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present application, and these all belong to the protection scope of the present application. Therefore, the protection scope of the patent application shall be subject to the attached claims.
Claims
1. A method for preparing an etch stop layer, characterized in that: include: Providing a substrate on which NMOS devices and PMOS devices arranged at intervals are formed; and forming a first stress etch stop layer on the substrate, the NMOS device and the PMOS device; forming a blocking layer on the first stress etch stop layer located on the PMOS device; The first stress etch stop layer on the NMOS device is irradiated with ultraviolet light, so that the first stress etch stop layer on the NMOS device is converted into a second stress etch stop layer.
2. The method for preparing an etch stop layer according to claim 1, characterized in that: The shielding layer includes a metal shielding layer.
3. The method for preparing an etch stop layer according to claim 2, characterized in that: The metal shielding layer includes an aluminum shielding layer.
4. The method for preparing an etch stop layer according to claim 1, characterized in that: Before forming a blocking layer on the first stress etch stop layer located on the PMOS device, the preparation method further includes: forming a protective layer on a surface of the first stress etch stop layer away from the substrate; The step of forming a blocking layer on the first stress etch stop layer located on the PMOS device comprises: forming a shielding material layer on a surface of the protection layer away from the first stress etching stop layer; The shielding material layer located on the NMOS device is removed, and the shielding material layer located on the PMOS device is retained as the shielding layer.
5. The method for preparing an etch stop layer according to claim 4, characterized in that: The material of the protective layer includes silicon dioxide.
6. The method for preparing an etch stop layer according to claim 4, characterized in that: After forming the second stress etching stop layer, the preparation method further includes: The protective layer is removed.
7. The method for preparing an etch stop layer according to claim 1, characterized in that: The material of the first stress etching stop layer includes silicon nitride.
8. The method for preparing an etch stop layer according to claim 1, characterized in that: The second stress etch stop layer has a tensile stress of at least 1200 MPa.
9. The method for preparing an etch stop layer according to claim 8, characterized in that: The first stress etch stop layer has a tensile stress in the range of 400 MPa to 600 MPa.
10. A semiconductor structure, characterized in that: The process of preparing the semiconductor structure includes the steps of the method for preparing an etch stop layer according to any one of claims 1 to 9.