Method for promoting co-fermentation of sludge and straw to produce acid and recycling blue iron ore through potassium ferrate pretreatment
Potassium ferrate promotes sludge-straw co-fermentation, which solves the problems of short-chain fatty acid accumulation and low blue iron ore recovery efficiency in sludge anaerobic fermentation, achieves efficient carbon source and phosphorus resource recovery, simplifies the treatment process and Reduced costs.
Patent Information
- Application Number
- CN202410839893.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-26
- Publication Date
- 2024-10-25
Smart Images

Figure CN118834919A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a method for promoting sludge-straw co-fermentation to produce acid and recover blue iron ore through potassium ferrate pretreatment, belongs to the field of water pollution control and resource recycling, and can be used to achieve sewage sludge treatment, disposal and resource utilization. Background Art
[0002] Excess sludge is the main byproduct produced during the biological treatment of sewage. It is rich in organic matter and nutrients, and its treatment and disposal has always been a concern. Anaerobic fermentation is an effective treatment method to achieve the stabilization and resource utilization of excess sludge, and can recover resources such as short-chain fatty acids and methane. Among them, short-chain fatty acids are widely used. They can not only be used to produce polyhydroxyalkanoates and bioenergy, but also serve as a supplementary carbon source for water plants to achieve the purpose of carbon emission reduction and promote carbon neutrality. However, due to the influence of sludge floc structure and extracellular polymers, hydrolysis often limits the progress of anaerobic fermentation. Therefore, physical, chemical or biological pretreatment is often used to promote the release of organic matter and improve the anaerobic fermentation performance of sludge. On the other hand, the low C / N in sludge will also limit the production of acid by anaerobic fermentation. Adding carbon-rich substances for co-fermentation is an effective way to solve this problem. Corn stover, as an agricultural waste, contains a large amount of hemicellulose, cellulose and lignin, which can be co-fermented with excess sludge to improve C / N, thereby increasing the production of short-chain fatty acids. However, corn stalks themselves have a compact structure and low bioavailability, and usually need to be pretreated separately before being co-fermented with sludge, which increases the processing cost.
[0003] In addition, phosphate rock, as a non-renewable resource, will be exhausted in the next few decades; at the same time, human activities have caused a large amount of phosphorus to enter water bodies, causing eutrophication problems. Residual sludge is one of the important phosphorus sinks produced by human activities. Recycling the phosphorus resources in it can solve the "phosphorus crisis" and "phosphorus pollution" problems. Studies have shown that iron-containing sludge or residual sludge with additional iron source can generate violet iron ore after anaerobic fermentation. Vitriol iron ore itself has magnetic properties and can be separated by magnetic separation, thereby achieving effective recovery of phosphorus. However, its generation is affected by the iron reduction rate and phosphorus release rate, which limits the efficiency of recovering violet iron ore from fermented sludge.
[0004] Therefore, it is necessary to develop a method to achieve efficient and rapid accumulation of short-chain fatty acids while reducing the use of chemical reagents, and to achieve the generation of cyanite to recover phosphorus resources. Potassium ferrate, as a highly oxidizing green water treatment agent, can achieve sludge solubilization while avoiding environmental problems that may be caused by other chemical pretreatments, and can also provide additional iron ions to promote the generation of cyanite. The Fe(VI) in it can generate active oxygen (OH, O2 - and 1O2), while increasing pH to destroy sludge floc structure and extracellular polymers. Oxidative pretreatment and alkaline pretreatment are also conventional means to improve the bioavailability of corn straw. Therefore, potassium ferrate pretreatment has great application potential in promoting sludge solubilization and improving straw bioavailability. It is feasible to develop a method to increase the accumulation of anaerobic fermentation acid production and simultaneously recover phosphorus resources by adding potassium ferrate.
[0005] The present invention is technically different from the prior art, mainly in the following two aspects:
[0006] (1) Different research objects: This invention first proposed to use potassium ferrate as a pretreatment method to improve the acid production fermentation performance of the residual sludge-corn straw co-fermentation system, successfully increasing the accumulation of short-chain fatty acids and shortening the time required for anaerobic fermentation. In addition, blue iron ore was detected in the residual sludge after fermentation, which proved that this method can not only achieve carbon source recovery, but also further recover phosphorus using rubidium magnets, which has extremely high application prospects and value.
[0007] (2) Different operation steps: Due to its dense structure, corn stalks usually require additional treatment, such as steam explosion, acid-base pretreatment, oxidation pretreatment, etc., before they can be effectively utilized, which increases the operation steps and costs. The present invention utilizes the strong oxidizing property of potassium ferrate itself and the strong alkaline environment generated by its hydrolysis to simultaneously achieve sludge solubilization and improve the bioavailability of corn stalks. While enhancing the accumulation of short-chain fatty acids, it simplifies the material preparation process and reduces the processing cost. Summary of the invention
[0008] The present invention aims to provide an efficient and economical method for recycling waste resources, which promotes sludge solubilization and simultaneously improves the bioavailability of straw by adding potassium ferrate, while minimizing the use of chemical reagents and realizing the recovery of carbon source and phosphorus resources. The method not only greatly improves the yield of short-chain fatty acids in the co-fermentation system, but also shortens the fermentation time, increases the phosphorus release rate, and promotes the formation of blue iron ore during anaerobic fermentation of sludge, and has broad application prospects.
[0009] A method for promoting acid production by co-fermentation of sludge and straw by potassium ferrate pretreatment and recovering blue iron ore, characterized in that: utilizing the strong oxidizing property of potassium ferrate itself and the characteristics of increasing environmental pH by hydrolysis, sludge solubilization and straw pretreatment are realized simultaneously, and efficient accumulation of short-chain fatty acids is achieved, and the generation of blue iron ore is promoted. The specific steps are as follows:
[0010] (1) Material preparation: Use a 40-mesh sieve to filter the residual sludge discharged from the sewage biological treatment system to remove large particles such as gravel, then let it settle naturally at room temperature for 1 hour, remove the supernatant, control the volatile suspended solids concentration in the concentrated sludge to 9-11 g / L, and store it in a refrigerator at 4°C for later use; wash the naturally air-dried corn stalks to remove the floating soil, cut them into 1-3 cm small pieces, dry them at 70°C for 48 hours until constant weight, crush them, pass them through a 1 mm sieve, and seal them in a cool and dry place; the weight of corn stalks mentioned below is the weight of volatile solids to reduce the interference of inactive ingredients;
[0011] (2) Anaerobic co-fermentation acid production: Use 1 mol / L NaOH solution to adjust the pH of the residual sludge to 10 to provide a stable alkaline environment and enhance the effect of potassium ferrate; control the volatile suspended solids concentration in the residual sludge to 9-11 g / L, the total suspended solids concentration to 10-13 g / L, and the total phosphorus concentration to 255-265 mg / L; add crushed corn stalks at a dosage of 0.5 g per gram of volatile suspended solids in the residual sludge, stir at 600 rpm / min for 5 minutes to fully mix the residual sludge and corn stalks; add 0.2-0.5 g of agent per gram of volatile suspended solids in the residual sludge. Potassium ferrate was added in large amounts to pretreat the mixture, and the mixture was stirred at 400 rpm / min for 30 minutes at room temperature to complete the pretreatment process; the pretreated residual sludge and corn straw mixture was put into a sequencing batch reactor, aerated with nitrogen for 10 minutes to remove dissolved oxygen in the mixed solution, and the reactor was completely sealed for anaerobic fermentation; a gas collecting port was provided on the top of the reactor, which was used to connect an air bag to collect the gas generated during the anaerobic fermentation process to balance the internal and external pressures and prevent oxygen from entering; the sequencing batch reactor was reacted at 180 rpm / min and 33°C ± 1°C for 6-8 days, and the pH was no longer adjusted during the process to obtain a fermentation liquid;
[0012] (3) Generation and recovery of violaceous iron ore: The mixed liquor after anaerobic fermentation is centrifuged and dehydrated, and the dehydrated sludge is freeze-dried until completely dry; the freeze-dried sample is subjected to X-ray diffraction analysis to determine the mineral composition and crystal structure of the sample, thereby determining the generation of violaceous iron ore in the product; a strongly magnetic rubidium magnet is used to separate violaceous iron ore from the freeze-dried sludge to achieve phosphorus recovery.
[0013] Beneficial results of the present invention
[0014] The unreasonable treatment and disposal of excess sludge may not only cause waste of resources but also cause secondary pollution. Therefore, promoting the resource utilization of excess sludge is an effective way to solve this problem. The present invention makes full use of the strong oxidizing property and alkalinity enhancement of potassium ferrate, and simultaneously realizes sludge solubilization and straw pretreatment, thereby significantly increasing the accumulation of short-chain fatty acids and successfully realizing the formation of blue iron ore. The results show that when the potassium ferrate addition amount is 0.2-0.5g / gVSS 污泥 When the soluble chemical oxygen demand, soluble protein and soluble polysaccharide in the co-fermentation system were compared with the non-dosing group, the release amount was increased by 6.97-9.92, 3.78-5.89 and 3.12-4.29 times, respectively, which greatly improved the hydrolysis rate and promoted the utilization of microorganisms. The efficient accumulation of short-chain fatty acids was successfully achieved, and the maximum accumulation amount of 6379.4-7343.3 mgCOD / L was reached in only 7 days, and the acid production rate was increased by 91.7-120.7%. At the same time, potassium ferrate also significantly promoted the release of phosphorus in the sludge, and successfully captured a large amount of soluble phosphorus to generate iron-phosphorus compounds. The XRD results showed that only blue iron ore existed in the sludge, without interference from other iron-containing impurities, and it could be recovered using a rubidium magnet. The present invention recovers the carbon and phosphorus resources in the residual sludge to the maximum extent, and simultaneously realizes the resource utilization of agricultural waste straw, which has broad application prospects.
[0015] Innovation of the present invention
[0016] (1) The present invention adds potassium ferrate to the sludge-straw co-fermentation system for the first time, successfully promoting the release of organic matter, significantly improving the utilization rate of microorganisms and increasing the accumulation of short-chain fatty acids. At the same time, it also promotes the release of phosphorus in the excess sludge and successfully converts it into blue iron ore, realizing phosphorus recovery.
[0017] (2) The present invention makes full use of the chemical action of potassium ferrate itself to achieve the simultaneous solubilization of sludge and pretreatment of straw. The pretreatment steps of straw are simplified, thereby reducing the processing cost, streamlining the operation process, and providing a method with more practical application value for the resource utilization of sludge and straw. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 Effects of different dosages of potassium ferrate on anaerobic digestion process in co-fermentation system
[0019] Figure 2 Effects of different doses of potassium ferrate on the production of short-chain fatty acids
[0020] Figure 3 Changes in iron during the reaction
[0021] Figure 4 Changes of phosphorus during the reaction
[0022] Figure 5 XRD analysis results of residual sludge after anaerobic fermentation DETAILED DESCRIPTION
[0023] Example: Potassium ferrate pretreatment promotes acid production and blue iron ore generation by co-fermentation of sludge and straw
[0024] 1) Take the residual sludge with biological phosphorus removal function, sieve to remove impurities, and remove the supernatant after natural sedimentation at room temperature for 1 hour. Control its volatile solid concentration at (10±1)g / L and store it in a refrigerator at 4℃; wash the straw, cut it into small pieces, dry it at 70℃ to constant weight, then crush it, and store it in a dry place in a sealed container without additional pretreatment;
[0025] 2) Adjust the pH of the remaining sludge to 10 and add 0.5g / g VSS WAS Then, the mixture was divided into 4 groups and different doses of potassium ferrate (0, 0.05, 0.2 and 0.5 g / g VSS) were added to each group. WAS ) and were named PF0, PF005, PF02 and PF05 respectively. After thorough mixing, the mixture was loaded into a sequencing batch reactor and aerated with nitrogen for 10 minutes to remove dissolved oxygen. Seal and place in an air bath shaker, react at 180rpm / min, 33℃±1℃ for 8 days, and the pH was no longer adjusted during the process. The concentrations of soluble polysaccharides, soluble proteins, soluble chemical oxygen demand (SCOD) and total short-chain fatty acids (TSCFAs) in the supernatant were measured during the fermentation process. The results showed that potassium ferrate pretreatment significantly promoted the release of organic matter in the co-fermentation system, such as Figure 1 As shown, after 1 day of reaction, the PF02 and PF05 groups released 5342.5 mg / L and 7787.5 mg / L of SCOD, respectively, which were 8.16 times and 11.90 times that of the PF0 group. The soluble protein and polysaccharide increased significantly with the increase of potassium ferrate dosage. The soluble protein reached 1.36, 3.67, and 5.89 times that of the PF0 group, respectively, and the soluble polysaccharide reached 1.9, 3.12 and 4.29 times that of the PF0 group, respectively. Correspondingly, the maximum accumulation of SCFAs increased significantly (PF0 = 3327.2 mg / L, PF005 = 4884.2 mg / L, PF02 = 6279.4 mg / L and PF05 = 7343.3 mg / L), and the PF02 and PF05 groups only took 7 days to reach the peak, shortening the fermentation time ( Figure 2 ).
[0026] 3) Monitoring of Fe and P during anaerobic fermentation: Figure 3As shown in the figure, within 3-5 days, the reduction rate of iron ions introduced into the system by potassium ferrate reached more than 90%, and the reduction rate was relatively fast. And with the increase of the dosage, TPO4 3- The content increased accordingly ( Figure 4 ), which indicates that the addition of PF promotes the release of phosphorus in sludge. When the dosage reaches 0.2-0.5gPF / gVSS WAS When almost all phosphorus is converted into PO4 3- The iron ions introduced by potassium ferrate reacted with soluble phosphorus (SP) to form a precipitate, which significantly reduced the proportion of SP in the supernatant (only 97.7% and 99.8% of TPO4 in the PF02 group). 3- The content of SP in the PF05 group was (6.99±0.82)%, and almost no SP was detected in the PF05 group. Most of the phosphorus was enriched in the residual sludge and did not flow out with the fermentation liquid, thus avoiding secondary pollution and improving the availability of the fermentation liquid as a supplementary carbon source for the water plant.
[0027] 4) The remaining sludge after anaerobic fermentation is freeze-dried and subjected to XRD analysis. Figure 5 As shown in the figure, cyanite crystals were generated in all systems with PF added, but the characteristic peak of cyanite in the PF005 group was very weak, and an amorphous peak was clearly seen in the range of 15-25°. In the PF02 and PF05 groups, the characteristic peak of cyanite was obvious and the amorphous peak was small, indicating that cyanite was generated well. The cyanite product was separated from the mixed sludge using a rubidium magnet, achieving the simultaneous recovery of phosphorus.
[0028] The present invention takes into account the treatment cost and treatment effect of potassium ferrate and believes that 0.2-0.5g / g VSS WAS The dosage of potassium ferrate is the best, which can promote the solubilization of sludge and the improvement of straw bioavailability, thereby achieving effective recovery of carbon sources. It can also effectively reduce the soluble phosphorus content in the fermentation liquid, promote the formation of blue iron ore in the residual sludge, and further achieve phosphorus recovery. Therefore, the dosage of potassium ferrate is set at 0.2-0.5g / g VSS WAS , anaerobic fermentation was carried out for 7 days to obtain a fermentation liquid rich in short-chain fatty acids, and cyanite was separated from the remaining sludge after fermentation using a rubidium magnet to achieve phosphorus recovery.
Claims
1. A method for promoting acid production by co-ferration of sludge and straw by potassium ferrate pretreatment and recovering blue iron ore, characterized in that The specific steps are as follows: (1) Material preparation: Use a 40-mesh sieve to filter the residual sludge discharged from the sewage biological treatment system to remove large particles of impurities, then let it settle naturally at room temperature for 1 hour, remove the supernatant, control the concentration of volatile suspended solids in the concentrated sludge to 9-11 g / L, and store it in a refrigerator at 4°C for later use; wash the naturally air-dried corn stalks to remove the floating soil, cut them into small pieces of 1-3 cm, dry them at 70°C for 48 hours until constant weight, crush them, pass them through a 1 mm sieve, and seal them in a cool and dry place; (2) Anaerobic co-fermentation acid production: Use 1 mol / L NaOH solution to adjust the pH of the residual sludge to 10; control the volatile suspended solids concentration in the residual sludge to 9-11 g / L, the total suspended solids concentration to 10-13 g / L, and the total phosphorus concentration to 255-265 mg / L; add crushed corn stalks at a dosage of 0.5 g per gram of volatile suspended solids in the residual sludge, and stir at 600 rpm / min for 5 minutes to fully mix the residual sludge and corn stalks; add potassium ferrate at a dosage of 0.2-0.5 g per gram of volatile suspended solids in the residual sludge to pretreat the mixture, and stir at 400 rpm / min for 30 minutes at room temperature to complete the pretreatment process; The pretreated residual sludge and corn straw mixture is put into a sequencing batch reactor, aerated with nitrogen for 10 minutes to remove dissolved oxygen in the mixed solution, and the reactor is completely sealed for anaerobic fermentation; a gas collecting port is provided on the top of the reactor, which is used to connect an air bag to collect the gas generated during the anaerobic fermentation process to balance the internal and external pressures and prevent oxygen from entering; the sequencing batch reactor is reacted at 180 rpm / min and 33°C ± 1°C for 6-8 days, and the pH is no longer adjusted during the process to obtain a fermentation liquid; (3) Generation and recovery of violaceous iron ore: The fermentation liquid is centrifuged and dehydrated, and the dehydrated sludge is freeze-dried until it is completely dry; the freeze-dried sample is subjected to X-ray diffraction analysis to determine the mineral composition and crystal structure of the sample, thereby determining the generation of violaceous iron ore in the product; a rubidium magnet is used to separate violaceous iron ore from the freeze-dried sludge to achieve phosphorus recovery.
Citation Information
Cited By
Method for gradient reinforcement of efficient release and recycling of carbon and phosphorus in sludge
CN120025053A
Method and system for strengthening sludge cracking and producing medium-chain fatty acid
CN121380222A
A method and system for enhancing sludge pyrolysis and producing medium-chain fatty acids
CN121380222B
Method for simultaneously recovering short-chain fatty acid and phosphorus in sludge anaerobic fermentation
CN121426398A
A method for simultaneously recovering short-chain fatty acids and phosphorus from anaerobic fermentation of sludge
CN121426398B