Display substrate, preparation method thereof and display device
By setting isolation grooves and barrier layers in the transition area of the OLED display, the problem of water vapor and oxygen penetration is solved, the reliability of the packaging is improved, and the stability of the display is ensured.
Patent Information
- Application Number
- CN202310486035.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-04-28
- Publication Date
- 2024-10-29
AI Technical Summary
During the thin-film packaging process of OLED displays, packaging reliability is affected by the permeability of the organic evaporated film layer after cutting, causing water vapor and oxygen to penetrate, affecting the reliability of the display.
A display substrate is designed, which includes a hole area, a transition area and a display area. The transition area is provided with an isolation structure, including an isolation groove and a barrier layer. The isolation groove penetrates the second structural layer and exposes the barrier layer to prevent water vapor and oxygen from penetrating.
It effectively blocks the organic light-emitting functional film layer in the transition area, prevents external water vapor and oxygen from intruding into the display area, and improves the reliability and isolation effect of the package.
Smart Images

Figure CN118870918A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to but is not limited to the field of display technology, and specifically to a display substrate and a preparation method thereof, and a display device. Background Art
[0002] As smartphones rapidly develop towards full-screen displays, the requirements for screen-to-body ratio are getting higher and higher, the market demand for perforated screens is increasing, and semiconductor packaging technology to meet this demand is also constantly developing. At present, thin film encapsulation (TFE) is a commonly used packaging technology for organic light-emitting diode (OLED) displays. Due to the packaging reliability requirements of TFE, no evaporated light-emitting functional film layer is allowed under the edge of the TFE layer. Otherwise, after cutting, water vapor, oxygen, etc. will penetrate into the interior of the OLED display through the organic evaporated film layer of the cut section, affecting the reliability of the OLED display packaging. Therefore, how to improve the packaging reliability of thin film encapsulation at the opening position in the OLED display has become an urgent problem to be solved. Summary of the invention
[0003] The embodiment of the present disclosure provides a display substrate, comprising a hole area, a transition area surrounding the hole area, and a display area surrounding the transition area; the transition area is provided with an isolation structure surrounding the hole area, and the isolation structure comprises at least one isolation groove;
[0004] The display substrate includes a base, the isolation groove includes a groove and a blocking edge arranged on a side of the groove away from the base; in a direction perpendicular to the base, the transition zone includes a first structural layer and a second structural layer stacked in sequence in a direction away from the base, the first structural layer includes a blocking layer, the groove penetrates the second structural layer and exposes at least a portion of the surface of the blocking layer, the blocking edge is arranged on a surface of the second structural layer away from the base, and a portion of the blocking edge extends in a direction parallel to the base and protrudes from the side wall of the groove.
[0005] The embodiment of the present disclosure also provides a display device, comprising the display substrate.
[0006] The present disclosure also provides a method for preparing the display substrate, comprising:
[0007] forming a first structural layer and a second structural layer on the substrate of the transition zone in sequence, wherein the first structural layer comprises a barrier layer, and the second structural layer is provided with a groove, wherein the groove penetrates the second structural layer and exposes at least a portion of the surface of the barrier layer;
[0008] forming a filling layer in the groove, wherein the filling layer fills the groove;
[0009] forming a stop edge on a surface of the second structural layer away from the substrate, wherein a portion of the stop edge extends in a direction parallel to the substrate to a surface of the filling layer away from the substrate;
[0010] The filling layer is removed.
[0011] The display substrate of the embodiment of the present disclosure can isolate the organic light-emitting functional film layer evaporated in the transition area by arranging an isolation structure around the hole area in the transition area, thereby preventing external water vapor and oxygen from invading the display area from the hole area through the organic light-emitting functional film layer, thereby ensuring the reliability of packaging. In addition, by arranging a barrier layer at the bottom of the isolation groove, it can help control the structural morphology of the groove formed during the etching process to improve the isolation effect of the isolation groove. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] The accompanying drawings are used to provide a further understanding of the technical solution of the present disclosure and constitute a part of the specification. Together with the embodiments of the present disclosure, they are used to explain the technical solution of the present disclosure and do not constitute a limitation on the technical solution of the present disclosure. The shapes and sizes of the components in the accompanying drawings do not reflect the actual proportions and are only intended to illustrate the contents of the present disclosure.
[0013] Figure 1 Schematic diagram of a planar structure of a display substrate of some exemplary embodiments;
[0014] Figure 2a In some exemplary embodiments Figure 1 AA section structure schematic diagram in;
[0015] Figure 2b In some other exemplary embodiments Figure 1 AA section structure schematic diagram in;
[0016] Figure 2c In some further exemplary embodiments Figure 1 AA section structure schematic diagram in;
[0017] Figure 3 In some further exemplary embodiments Figure 1 AA section structure schematic diagram in;
[0018] Figure 4 In some further exemplary embodiments Figure 1 AA section structure schematic diagram in;
[0019] Figure 5 In some further exemplary embodiments Figure 1 AA section structure schematic diagram in;
[0020] Figure 6 In some further exemplary embodiments Figure 1 AA section structure schematic diagram in;
[0021] Figure 7a is a schematic structural diagram of a display substrate after forming a second interlayer insulating layer according to some exemplary embodiments;
[0022] Figure 7b Schematic diagram of the structure of a display substrate after forming a first source-drain metal layer according to some exemplary embodiments;
[0023] Figure 7c is a schematic structural diagram of a display substrate after forming a first planar layer according to some exemplary embodiments;
[0024] Figure 7d Schematic diagram of the structure of the display substrate after forming the second source-drain metal layer of some exemplary embodiments;
[0025] Figure 7e Schematic diagram of the structure of a display substrate after forming a pixel defining layer according to some exemplary embodiments;
[0026] Figure 7f is a schematic structural diagram of a display substrate of some exemplary embodiments after a filling layer is removed;
[0027] Figure 8a is a schematic structural diagram of a display substrate after forming a third gate insulating layer according to some exemplary embodiments;
[0028] Figure 8b is a schematic structural diagram of a display substrate after forming a third gate metal layer according to some exemplary embodiments;
[0029] Figure 8c is a schematic structural diagram of a display substrate after forming a second interlayer insulating layer according to some exemplary embodiments;
[0030] Figure 8d Schematic diagram of the structure of a display substrate after forming a first source-drain metal layer according to some exemplary embodiments;
[0031] Figure 8e is a schematic structural diagram of a display substrate after forming a first planar layer according to some exemplary embodiments;
[0032] Figure 8f Schematic diagram of the structure of the display substrate after forming the second source-drain metal layer of some exemplary embodiments;
[0033] Figure 8g is a schematic structural diagram of a display substrate after forming a first electrode according to some exemplary embodiments;
[0034] Figure 8hSchematic diagram of the structure of a display substrate after forming a pixel defining layer according to some exemplary embodiments;
[0035] Figure 8i is a schematic structural diagram of a display substrate of some exemplary embodiments after a filling layer is removed;
[0036] Figure 9a is a schematic structural diagram of a display substrate after forming a second interlayer insulating layer according to some exemplary embodiments;
[0037] Figure 9b Schematic diagram of the structure of a display substrate after forming a first source-drain metal layer according to some exemplary embodiments;
[0038] Fig.9c is a schematic structural diagram of a display substrate after forming a first planar layer according to some exemplary embodiments;
[0039] Figure 9d Schematic diagram of the structure of the display substrate after forming the second source-drain metal layer of some exemplary embodiments;
[0040] Fig.9e is a schematic structural diagram of a display substrate after forming a first electrode according to some exemplary embodiments;
[0041] Figure 9f Schematic diagram of the structure of a display substrate after forming a pixel defining layer according to some exemplary embodiments;
[0042] Figure 9g Schematic diagram of the structure of the display substrate after the filling layer is removed according to some exemplary embodiments.
[0043] Figure numerals: 10, substrate, 20, driving structure layer, 21, first buffer layer, 22, first gate insulating layer, 23, second gate insulating layer, 24, first interlayer insulating layer, 25, third gate insulating layer, 26, second interlayer insulating layer, 27, first flat layer, 28, second flat layer, 30, light emitting structure layer, 31, first electrode, 32, pixel defining layer, 33, light emitting function layer, 34, second electrode layer, 40, packaging structure layer, 41, first packaging layer, 42, second packaging layer, 43, third packaging layer, 50, isolation structure, 51, isolation groove, 52, isolation column, 60, isolation dam, 71, first isolation layer, 72, retaining wall, 73, second isolation layer, 81, first groove, 82, second groove, 83, third groove, 84, first metal ring, 85, second metal ring, 86, first a blocking edge, 87, a second blocking edge, 91, a first convex ring, 92, a second convex ring, 100, a display area, 200, a hole area, 201, a first transistor, 202, a second transistor, 203, a storage capacitor, 204, a connecting electrode, 261, a first sublayer, 262, a second sublayer, 271, a filling layer, 300, a transition area, 511, a groove, 512, a blocking edge, 513, a blocking layer, 514, a convex ring, 521, a first isolation portion, 522, a second isolation portion, 523, a column base, 2011, a first active layer, 2012, a first gate electrode, 2013, a first source electrode, 2014, a first drain electrode, 2021, a second active layer, 2022, a second gate electrode, 2023, a second source electrode, 2024, a second drain electrode, 2031, a first electrode plate, 2032, a second electrode plate. DETAILED DESCRIPTION
[0044] Those skilled in the art should understand that the technical solutions of the embodiments of the present disclosure may be modified or replaced by equivalents without departing from the spirit and scope of the technical solutions of the embodiments of the present disclosure, and all should be included in the scope of the claims of the present disclosure.
[0045] like Figure 1 , Figure 2a and Figure 2b As shown, Figure 1 is a schematic diagram of a planar structure of a display substrate of some exemplary embodiments, Figure 2a In some exemplary embodiments Figure 1 AA section structure diagram in, Figure 2b In some other exemplary embodiments Figure 1 AA cross-sectional structural schematic diagram in , the display substrate includes a hole area 200, a transition area 300 surrounding the hole area 200, and a display area 100 surrounding the transition area 300.
[0046] Exemplarily, the display area 100 includes a driving structure layer 20 , a light emitting structure layer 30 and a packaging structure layer 40 which are sequentially stacked on the substrate 10 .
[0047] The driving structure layer 20 includes a plurality of pixel driving circuits, each of which includes a plurality of transistors (T) and a storage capacitor 203 (C). Figure 2a The diagram shows a first transistor 201. The pixel driving circuit may adopt a 3T1C, 4T1C, 5T1C, 5T2C, 6T1C or 7T1C structure, and the present disclosure does not limit this.
[0048] The light-emitting structure layer 30 includes a plurality of light-emitting elements, and the light-emitting element may be an OLED (organic light-emitting diode) or a QLED (quantum dot light-emitting diode) device. The light-emitting element includes a first electrode 31, a light-emitting functional layer 33, and a second electrode layer 34 stacked in sequence in a direction away from the substrate 10. The light-emitting functional layer 33 includes an organic light-emitting layer, and may also include any one or more film layers of a hole injection layer, a hole transport layer, and an electron blocking layer between the first electrode 31 and the organic light-emitting layer, and any one or more film layers of an electron injection layer, an electron transport layer, and a hole blocking layer between the second electrode layer 34 and the organic light-emitting layer. The first electrode 31 of the light-emitting element is connected to a pixel driving circuit, and the light-emitting element emits light under the drive of the pixel driving circuit. In a direction perpendicular to the substrate 10, the light-emitting structure layer 30 includes a first electrode layer, a pixel defining layer 32, a light-emitting functional layer 33 and a second electrode layer 34 which are arranged in sequence; the first electrode layer includes a plurality of first electrodes 31, the pixel defining layer 32 is arranged on a side of the plurality of first electrodes 31 away from the substrate 10 and is provided with a plurality of pixel openings, the pixel openings expose the first electrodes 31, and the light-emitting functional layer 33 and the second electrode layer 34 are stacked in sequence on a side of the first electrode 31 away from the substrate 10.
[0049] The encapsulation structure layer 40 may include a first encapsulation layer 41, a second encapsulation layer 42, and a third encapsulation layer 43 stacked in sequence in a direction away from the substrate 10. The main materials (the material with the largest component in the film layer) of the first encapsulation layer 41 and the third encapsulation layer 43 are inorganic materials, which may include silicon oxide (SiOx), silicon nitride (SiNx), and silicon oxynitride (SiO X N Y ), the main material of the second encapsulation layer 42 can be an organic material, such as epoxy resin, which helps to achieve encapsulation and avoid water vapor erosion. The first encapsulation layer 41 and the third encapsulation layer 43 can be formed by a chemical vapor deposition (CVD) process, and the second encapsulation layer 42 can be formed by an inkjet printing (IJP) process.
[0050] Exemplarily, the transition region 300 is provided with an isolation structure 50 surrounding the hole region 200, and the isolation structure 50 is configured to isolate the light-emitting functional layer 33 and the second electrode layer 34 of the transition region 300, so as to prevent water and oxygen from corroding from the hole region 200 along the light-emitting functional layer 33 and the second electrode layer 34 to the display region 100, and protect the light-emitting functional layer 33 and the second electrode layer 34 of the display region 100 from being corroded by water and oxygen. The isolation structure 50 may include at least one isolation groove 51 ( Figure 2b ) or / and at least one isolation column 52 ( Figure 2a As shown in FIG. 2 , the isolation column 52 and the isolation groove 51 are both arranged around the hole area 200. The number of the isolation structure 50 may be one or more, and the embodiment of the present disclosure does not limit the number of the isolation structure 50.
[0051] The transition area 300 may also be provided with an isolation dam 60, which is arranged around the hole area 200. In the process of forming the second encapsulation layer 42 of the encapsulation structure layer 40 by the inkjet printing process, the inkjet printing material may overflow, and the isolation dam 60 may prevent the inkjet printing material from overflowing. The surface of the isolation dam 60 away from the substrate 10 is higher than the surface of the isolation column 52 away from the substrate 10. The number of the isolation dams 60 may be one or more, and the embodiment of the present disclosure does not limit the number of the isolation dams 60. At least one of the isolation structures 50 may be located on the side of the isolation dam 60 facing the display area 100 or / and on the side of the isolation dam 60 facing the hole area 200.
[0052] In some exemplary embodiments, Figure 2a and Figure 2b As shown, in a direction perpendicular to the substrate 10, the driving structure layer 20 may include a first buffer layer 21, a first semiconductor layer, a first gate insulating layer 22, a first gate metal layer, a second gate insulating layer 23, a second gate metal layer, a first interlayer insulating layer 24, a first source-drain metal layer, a first flat layer 27, a second source-drain metal layer and a second flat layer 28, which are arranged in sequence along a direction away from the substrate 10; the first semiconductor layer may include a first active layer 2011 of a first transistor 201, the first gate metal layer may include a first gate electrode 2012 of the first transistor 201 and one plate of the storage capacitor 203, the second gate metal layer may include another plate of the storage capacitor 203, the first source-drain metal layer includes a first source electrode 2013 and a first drain electrode 2014 of the first transistor 201, and the second source-drain metal layer includes a connecting electrode 204 connected to the first source electrode 2013 or the first drain electrode 2014 of the first transistor 201, and the connecting electrode 204 is also connected to the first electrode 31.
[0053] In some examples of this embodiment, Figure 2aAs shown, the isolation structure 50 may include at least one isolation column 52, which is arranged around the hole area. The isolation column 52 may include a first isolation portion 521 and a second isolation portion 522 which are arranged in sequence along a direction away from the substrate 10. On the side of the isolation column 52 facing the display area 100 and / or the hole area 200, the second isolation portion 522 is protruding from the first isolation portion 521.
[0054] The material of the first isolation portion 521 may be an inorganic insulating material. The first isolation portion 521 may be disposed in the same layer as the first interlayer insulating layer 24, and the first interlayer insulating layer 24 may be a single-layer structure or a multi-layer structure. For example, the first interlayer insulating layer 24 may include a silicon oxide film layer and a silicon nitride film layer stacked in sequence in a direction away from the substrate 10, and the first isolation portion 521 includes a silicon oxide film layer and a silicon nitride film layer stacked in sequence in a direction away from the substrate 10, and the thickness of the silicon nitride film layer may be 0.5um to 1um (micrometer), for example, 0.8um.
[0055] The material of the second isolation portion 522 may be a metal material. The second isolation portion 522 may be disposed in the same layer as the first source electrode 2013 and the first drain electrode 2014 of the first transistor 201; or, the second isolation portion 522 may be disposed in the same layer as the connecting electrode 204; or, the second isolation portion 522 may include a first sub-isolation portion and a second sub-isolation portion sequentially stacked in a direction away from the substrate 10, the first sub-isolation portion may be disposed in the same layer as the first source electrode 2013 and the first drain electrode 2014 of the first transistor 201, and the second sub-isolation portion may be disposed in the same layer as the connecting electrode 204.
[0056] In this embodiment, the thickness of the first interlayer insulating layer 24 can be designed to be thicker (for example, in some examples, the thickness of the silicon nitride film layer in the first interlayer insulating layer 24 can be designed to be thicker), and accordingly, the thickness of the first isolation portion 521 is thicker, which is beneficial to improve the isolation effect of the isolation column 52 on the light-emitting functional layer 33 and the second electrode layer 34, and avoid the light-emitting functional layer 33 located on both sides of the isolation column 52 after being isolated by the isolation column 52 to be connected into a conductive path through the second isolation portion 522 with conductive function of the isolation column 52, thereby avoiding the resulting poor display.
[0057] Herein, "A and B are arranged in the same layer" means that the film layer of A and the film layer of B are from the same thin film, which can be a single-layer structure or a multi-layer composite structure, and the film layer of A and the film layer of B can be the same or different. "A and B are arranged in the same layer" can be understood as that the same thin film is subjected to the same patterning process to form A and B at the same time, or that the same thin film is subjected to the same patterning process to form A' and B' at the same time, and A' is further processed (such as etching, etc.) to obtain A, and B' is further processed (such as etching, etc.) to obtain B.
[0058] In some examples of this embodiment, Figure 2b As shown, the isolation structure 50 may include at least one isolation groove 51, which is arranged around the hole area. The isolation groove 51 includes a groove 511 and a blocking edge 512 arranged on the side of the groove 511 away from the substrate 10. In the direction perpendicular to the substrate 10, the transition zone 300 includes a first structural layer and a second structural layer stacked in sequence along the direction away from the substrate 10, the first structural layer includes a blocking layer 513, the groove 511 penetrates the second structural layer and exposes at least a portion of the surface of the blocking layer 513 (the surface away from the substrate 10), the blocking edge 512 is arranged on the surface of the second structural layer away from the substrate 10, and a portion of the blocking edge 512 extends in a direction parallel to the substrate 10 and protrudes from the side wall of the groove 511.
[0059] The blocking layer 513 may be disposed in the same layer as the first active layer 2011 (first semiconductor layer) of the first transistor 201. The second structural layer may include a plurality of stacked inorganic insulating layers, for example, may include a first inorganic insulating layer, a second inorganic insulating layer and a third inorganic insulating layer stacked in sequence in a direction away from the substrate 10, the first inorganic insulating layer and the first gate insulating layer 22 are disposed in the same layer, the second inorganic insulating layer and the second gate insulating layer 23 are disposed in the same layer, and the third inorganic insulating layer and the first interlayer insulating layer 24 are disposed in the same layer.
[0060] The dam 512 may be disposed in the same layer as the connection electrode 204. Alternatively, the dam 512 may be disposed in the same layer as the first source electrode 2013 and the first drain electrode 2014.
[0061] The orthographic projection of the blocking edge 512 on the substrate 10 may include the orthographic projection of the edge of the blocking layer 513 away from the groove 511 on the substrate 10. Alternatively, the orthographic projection of the blocking edge 512 on the substrate 10 may fall within the orthographic projection of the blocking layer 513 on the substrate 10. This is not limited in this embodiment.
[0062] In this embodiment, by providing an isolation groove 51 around the hole area 200 in the transition area 300, the organic light-emitting functional film layer evaporated in the transition area 300 can be isolated, thereby preventing external water vapor and oxygen from invading the display area 100 from the hole area 200 through the organic light-emitting functional film layer, thereby ensuring the reliability of packaging. In addition, the barrier layer 513 can help control the structural morphology of the groove 511 formed during the etching process of the groove 511. For example, the part of the side wall of the groove 511 close to the barrier layer 513 can be more concave in the direction away from the center of the groove 511, thereby improving the isolation effect of the isolation groove 51.
[0063] In some exemplary embodiments, Figure 2c As shown, Figure 2c In some further exemplary embodiments Figure 1 AA cross-sectional structural diagram in FIG. 1 , the isolation structure 50 may include a plurality of isolation grooves 51 ( Figure 2c 3. The three isolation grooves 51 are shown in the figure. The isolation grooves 51 are arranged around the hole area. The isolation grooves 51 include a groove 511 and a stop edge 512 arranged on the side of the groove 511 away from the substrate 10. In the direction perpendicular to the substrate 10, the transition zone 300 includes a first structural layer and a second structural layer stacked in sequence in the direction away from the substrate 10. The first structural layer includes a stop layer 513. The groove 511 penetrates the second structural layer and exposes at least part of the surface of the stop layer 513 (the surface away from the substrate 10). The stop edge 512 is arranged on the surface of the second structural layer away from the substrate 10, and a part of the stop edge 512 extends in a direction parallel to the substrate 10 and protrudes from the side wall of the groove 511. Each isolation groove 51 may include two stop edges 512, which are respectively located on both sides of the groove 511.
[0064] The isolation structure 50 may further include at least one isolation column 52; the isolation column 52 includes a first isolation portion 521 and a second isolation portion 522 arranged in sequence along a direction away from the substrate 10, and on the side of the isolation column 52 facing the display area 100 and / or the hole area 200, the second isolation portion 522 is protruded from the first isolation portion 521.
[0065] An isolation column 52 may be formed between two adjacent isolation grooves 51, the blocking edge 512 and the second isolation portion 522 may be provided in the same layer and made of the same material, and the second structural layer between two adjacent grooves 511 is the first isolation portion 521. The second isolation portion 522 of an isolation column 52 may serve as one of the blocking edges 512 of two adjacent isolation grooves 51.
[0066] The two adjacent barrier layers 513 may not be connected, and at least a portion of the orthographic projection of the second isolation portion 522 on the substrate 10 may not overlap with the orthographic projection of the two adjacent barrier layers 513 on the substrate 10 .
[0067] In other embodiments, at least two adjacent barrier layers 513 may be connected as one, and the orthographic projection of the at least two adjacent barrier layers 513 connected as one on the substrate 10 may include the orthographic projection of at least one isolation column 52 on the substrate 10. Figure 2c The multiple barrier layers 513 are connected as one.
[0068] In some exemplary embodiments, Figure 3 and Figure 4 As shown, Figure 3 In some further exemplary embodiments Figure 1 AA section structure diagram in, Figure 4 In some further exemplary embodiments Figure 1 AA cross-sectional structural diagram in the figure, in the direction perpendicular to the substrate 10, the driving structure layer 20 may include a first buffer layer 21, a first semiconductor layer, a first gate insulating layer 22, a first gate metal layer, a second gate insulating layer 23, a second gate metal layer, a first interlayer insulating layer 24, a second semiconductor layer, a third gate insulating layer 25, a third gate metal layer, a second interlayer insulating layer 26, a first source-drain metal layer, a first planarizing layer 27, a second source-drain metal layer and a second planarizing layer 28, which are sequentially arranged in a direction away from the substrate 10; the first semiconductor layer may include a first active layer 2011 of the first transistor 201, the first gate metal layer may include a first gate electrode 2012 of the first transistor 201 and the storage capacitor 20 3, the second gate metal layer may include another plate of the storage capacitor 203, the second semiconductor layer may include a second active layer 2021 of the second transistor 202, the third gate metal layer may include a second gate electrode 2022 of the second transistor 202, the first source-drain metal layer includes a first source electrode 2013 and a first drain electrode 2014 of the first transistor 201, and a second source electrode 2023 and a second drain electrode 2024 of the second transistor 202, the second source-drain metal layer includes a connecting electrode 204 connected to the first source electrode 2013 or the first drain electrode 2014 of the first transistor 201, and the connecting electrode 204 is also connected to the first electrode 31.
[0069] In some examples of this embodiment, the display substrate may be a low temperature polycrystalline oxide (LTPO) display substrate, and the multiple transistors of the pixel driving circuit may include a low temperature polycrystalline silicon (LTPS) thin film transistor and an oxide thin film transistor, and the oxide thin film transistor may be an indium gallium zinc oxide (IGZO) thin film transistor. The first transistor 201 may be a low temperature polycrystalline silicon thin film transistor, and the material of the first active layer 2011 is low temperature polycrystalline silicon. The second transistor 202 may be an indium gallium zinc oxide thin film transistor, and the material of the second active layer 2021 is indium gallium zinc oxide. In other embodiments, the display substrate may be a low temperature polycrystalline silicon display substrate, and the transistor of the display substrate is a low temperature polycrystalline silicon thin film transistor. The disclosed embodiments do not limit the type of display substrate and the type of transistor.
[0070] In some exemplary embodiments, the first buffer layer 21, the first gate insulating layer 22, the second gate insulating layer 23, the first interlayer insulating layer 24, the third gate insulating layer 25 and the second interlayer insulating layer 26 may be inorganic insulating layers, and may be made of silicon oxide (SiOx), silicon nitride (SiNx) and silicon oxynitride (SiO X N Y ), and may be a single-layer structure or a multi-layer composite structure. The first planar layer 27 and the second planar layer 28 may be organic insulating layers, and may be made of resin material. The materials of the first gate metal layer, the second gate metal layer, the third gate metal layer, the first source-drain metal layer and the second source-drain metal layer may be any one or more of silver (Ag), copper (Cu), aluminum (Al), titanium (Ti) and molybdenum (Mo), or alloy materials of the above metals, such as aluminum-neodymium alloy (AlNd) or molybdenum-niobium alloy (MoNb), and may be a single-layer structure or a multi-layer composite structure, such as Mo / Cu / Mo, Ti / Al / Ti, etc. The first semiconductor layer and the second semiconductor layer may be made of amorphous indium gallium zinc oxide material (a-IGZO), zinc oxynitride (ZnON), indium zinc tin oxide (IZTO), amorphous silicon (a-Si), polycrystalline silicon (p-Si), sexithiophene or polythiophene and the like.
[0071] In some exemplary embodiments, the substrate 10 may be a flexible substrate or a rigid substrate. The rigid substrate may be glass, quartz, etc., and the flexible substrate may include one or more of polyethylene terephthalate, polyethylene terephthalate, polyetheretherketone, polystyrene, polycarbonate, polyarylate, polyarylate, polyimide, polyvinyl chloride, polyethylene, and textile fibers.
[0072] In some exemplary embodiments, the first source-drain metal layer may include a first metal layer, a second metal layer, and a third metal layer sequentially arranged in a direction away from the substrate, the first metal layer and the third metal layer may be a titanium layer, and the second metal layer may be an aluminum layer. The second source-drain metal layer may include a fourth metal layer, a fifth metal layer, and a sixth metal layer sequentially arranged in a direction away from the substrate, the fourth metal layer and the sixth metal layer may be a titanium layer, and the fifth metal layer may be an aluminum layer. In other embodiments, the first source-drain metal layer and the second source-drain metal layer may be a single-layer structure.
[0073] In some examples of this embodiment, Figure 3 and Figure 4 As shown, the isolation structure 50 may include at least one isolation groove 51, which is arranged around the hole area. The isolation groove 51 includes a groove 511 and a blocking edge 512 arranged on the side of the groove 511 away from the substrate 10. In the direction perpendicular to the substrate 10, the transition zone 300 includes a first structural layer and a second structural layer stacked in sequence along the direction away from the substrate 10, the first structural layer includes a blocking layer 513, the groove 511 penetrates the second structural layer and exposes at least a portion of the surface of the blocking layer 513, the blocking edge 512 is arranged on the surface of the second structural layer away from the substrate 10, and a portion of the blocking edge 512 extends in a direction parallel to the substrate 10 and protrudes from the side wall of the groove 511.
[0074] For example, Figure 3 As shown, the blocking layer 513 can be disposed in the same layer as the second active layer 2021 (second semiconductor layer) of the second transistor 202; the second structural layer can include a plurality of stacked inorganic insulating layers, for example, can include a first inorganic insulating layer and a second inorganic insulating layer stacked in sequence in a direction away from the substrate 10, the first inorganic insulating layer is disposed in the same layer as the third gate insulating layer 25, and the second inorganic insulating layer is disposed in the same layer as the second interlayer insulating layer 26. The blocking edge 512 can be disposed in the same layer as the connecting electrode 204.
[0075] Or, if Figure 4As shown, the blocking layer 513 may be disposed in the same layer as the first active layer 2011 (first semiconductor layer) of the first transistor 201; the second structural layer may include a plurality of stacked inorganic insulating layers, for example, may include a first inorganic insulating layer, a second inorganic insulating layer, a third inorganic insulating layer, a fourth inorganic insulating layer and a fifth inorganic insulating layer stacked in sequence in a direction away from the substrate 10, the first inorganic insulating layer is disposed in the same layer as the first gate insulating layer 22, the second inorganic insulating layer is disposed in the same layer as the second gate insulating layer 23, the third inorganic insulating layer is disposed in the same layer as the first interlayer insulating layer 24, the fourth inorganic insulating layer is disposed in the same layer as the third gate insulating layer 25, and the fifth inorganic insulating layer is disposed in the same layer as the second interlayer insulating layer 26. The blocking edge 512 may be disposed in the same layer as the connecting electrode 204.
[0076] In other embodiments, the barrier layer 513 may be disposed in the same layer as the first gate metal layer, the second gate metal layer or the third gate metal layer; or, the barrier layer 513 may be an inorganic insulating layer, such as a SiOx layer. The second structural layer may include a plurality of stacked inorganic insulating layers; and the barrier edge 512 may be disposed in the same layer as the connecting electrode 204.
[0077] In some exemplary embodiments, Figure 5 As shown, Figure 5 In some further exemplary embodiments Figure 1 AA cross-sectional structural schematic diagram in the figure, the isolation structure 50 may include at least one isolation groove 51, the isolation groove 51 is arranged around the hole area, the isolation groove 51 includes a groove 511 and a blocking edge 512 arranged on the side of the groove 511 away from the substrate 10, in the direction perpendicular to the substrate 10, the transition zone 300 includes a first structural layer and a second structural layer stacked in sequence along the direction away from the substrate 10, the first structural layer includes a blocking layer 513, the groove 511 penetrates the second structural layer and exposes at least a portion of the surface of the blocking layer 513, the blocking edge 512 is arranged on the surface of the second structural layer away from the substrate 10, and a portion of the blocking edge 512 extends in a direction parallel to the substrate 10 and protrudes from the sidewall of the groove 511.
[0078] For example, Figure 5As shown, one or more convex rings 514 are provided on the side wall of the groove 511, and the multiple convex rings 514 are arranged in sequence along a direction perpendicular to the substrate 10. The groove 511 forms a groove between adjacent convex rings 514, and a groove is formed between the retaining edge 512 and the convex ring 514. Exemplarily, a first convex ring 91 and a second convex ring 92 are arranged in sequence on the side wall of the groove 511 along a direction perpendicular to the substrate 10. In this example, by providing one or more convex rings 514 on the side wall of the groove 511, the light-emitting functional layer 33 can be disconnected at the position of at least one convex ring 514, which can improve the isolation effect of the isolation groove 51; in addition, when the encapsulation layer of inorganic material is subsequently deposited, the encapsulation material can have a better climbing on the side wall of the groove 511, and the encapsulation is more dense, thereby improving the encapsulation effect.
[0079] For example, Figure 5 As shown, the retaining edge 512 can be arranged in the same layer as the connecting electrode 204 (second source-drain metal layer). The film layer of the retaining edge 512 can be the same as the film layer of the connecting electrode 204. The second source-drain metal layer can be a single-layer structure or a multi-layer structure, then, the retaining edge 512 and the connecting electrode 204 can be a single-layer structure or a multi-layer structure. Exemplarily, the second source-drain metal layer may include a fourth metal layer, a fifth metal layer and a sixth metal layer sequentially arranged in a direction away from the substrate 10, the fourth metal layer and the sixth metal layer may be a titanium layer, and the fifth metal layer may be an aluminum layer. Then, the retaining edge 512 and the connecting electrode 204 both include a fourth metal layer, a fifth metal layer and a sixth metal layer sequentially arranged in a direction away from the substrate 10. On the side of the retaining edge 512 close to the groove 511, the fifth metal layer can be set inward compared to the fourth metal layer and the sixth metal layer (that is, the fourth metal layer and the sixth metal layer are set protruding compared to the fifth metal layer).
[0080] For example, Figure 5 As shown, the second interlayer insulating layer 26 may include a first sublayer 261 and a second sublayer 262 sequentially arranged in a direction away from the substrate 10. The material of the first sublayer 261 may be silicon oxide, and the material of the second sublayer 262 may be silicon nitride. At least one of the convex rings 514 may be arranged in the same layer and the same material as the first sublayer 261.
[0081] For example, Figure 5 As shown, the barrier layer 513 may be disposed in the same layer as the second active layer 2021 of the second transistor 202. In other embodiments, the barrier layer 513 may be disposed in the same layer as the first active layer 2011 of the first transistor 201, the first gate metal layer, the second gate metal layer or the third gate metal layer.
[0082] For example, Figure 5 As shown, the second structural layer may include at least one inorganic insulating layer and at least one metal layer, and the metal layer in the second structural layer may be disposed in the same layer as the third gate metal layer. The convex ring 514 may be formed by the inorganic insulating layer in the second structural layer. In other embodiments, any metal layer in the second structural layer may be disposed in the same layer as the third gate metal layer, the second gate metal layer, or the first gate metal layer.
[0083] In some exemplary embodiments, Figure 6 As shown, Figure 6 In some further exemplary embodiments Figure 1 As shown in the AA cross-sectional structural schematic diagram, the isolation structure 50 may include at least one isolation column 52, and the isolation column 52 is arranged around the hole area. The isolation column 52 may include a first isolation portion 521 and a second isolation portion 522 arranged in sequence along a direction away from the substrate 10, and on the side of the isolation column 52 facing the display area 100 and / or the hole area 200, the second isolation portion 522 protrudes from the first isolation portion 521.
[0084] For example, Figure 6 As shown, the materials of the first isolation part 521 and the second isolation part 522 can both be metal materials. The first isolation part 521 may include a first metal layer, a second metal layer and a third metal layer arranged in sequence in a direction away from the substrate 10, and on the side of the isolation column 52 facing the display area 100 or / and the hole area 200, the second metal layer is set inward compared with the first metal layer and the third metal layer; or / and, the second isolation part 522 may include a fourth metal layer, a fifth metal layer and a sixth metal layer arranged in sequence in a direction away from the substrate 10, and on the side of the isolation column 52 facing the display area 100 or / and the hole area 200, the fifth metal layer is set inward compared with the fourth metal layer and the sixth metal layer. Compared with some technologies in which the isolation column 52 only includes the first isolation part 521 or the second isolation part 522, the isolation column 52 of this example can improve the isolation effect of the isolation column 52 by setting the first isolation part 521 and the second isolation part 522, and can improve the strength of the isolation column 52.
[0085] The fourth metal layer may be disposed on a surface of the third metal layer away from the substrate 10 , and on a side of the isolation column 52 facing the display area 100 and / or the hole area 200 , the fourth metal layer is disposed protruding compared to the third metal layer.
[0086] The first isolation portion 521 may be provided in the same layer as the first source electrode and the first drain electrode (the same layer as the first source-drain metal layer), and the second isolation portion 522 may be provided in the same layer as the connection electrode 204 (the second source-drain metal layer). The first metal layer and the third metal layer of the first isolation portion 521 may be titanium layers, the second metal layer may be an aluminum layer, the fourth metal layer and the sixth metal layer of the second isolation portion 522 may be titanium layers, and the fifth metal layer may be an aluminum layer.
[0087] For example, Figure 6 As shown, the isolation column 52 may further include a column base 523 disposed on the side of the first isolation portion 521 facing the substrate 10, and the column base 523 may include at least one inorganic insulating layer. For example, the column base 523 may include a plurality of stacked inorganic insulating layers, or the column base 523 may include at least one inorganic insulating layer and at least one metal layer, and the metal layer in the column base 523 may be covered by the inorganic insulating layer in the column base 523.
[0088] For example, Figure 6 As shown, the transition region 300 is further provided with a barrier layer 513, and the isolation column 52 is provided on the surface of the barrier layer 513 away from the substrate 10. The barrier layer 513 can be provided in the same layer as the first active layer 2011, the first gate electrode 2012, any plate of the storage capacitor 203, the second active layer 2021 or the second gate electrode 2022.
[0089] For example, Figure 6 As shown, the isolation structure 50 may include a plurality of isolation columns 52, and one isolation trench 51 may be formed between two adjacent isolation columns 52. Similarly, the isolation structure 50 may include a plurality of isolation trenches 51; and one isolation column 52 may be formed between two adjacent isolation trenches 51.
[0090] The structure of the display substrate is exemplified below by the preparation process of the display substrate. The "patterning process" mentioned in the present disclosure includes the processes of coating photoresist, mask exposure, development, etching, stripping photoresist, etc. for metal materials, inorganic materials or transparent conductive materials, and includes the processes of coating organic materials, mask exposure and development, etc. for organic materials. Deposition can be any one or more of sputtering, evaporation, and chemical vapor deposition, coating can be any one or more of spraying, spin coating and inkjet printing, and etching can be any one or more of dry etching and wet etching, which are not limited in the present disclosure. "Thin film" refers to a layer of thin film made by deposition, coating or other processes of a certain material on a substrate. If the "thin film" does not require a patterning process during the entire production process, the "thin film" can also be called a "layer". If the "thin film" requires a patterning process during the entire production process, it is called a "thin film" before the patterning process and a "layer" after the patterning process. The "layer" after the patterning process contains at least one "pattern". The "thickness" of the film layer is the size of the film layer in the direction perpendicular to the display substrate. In the exemplary embodiments of the present disclosure, "the orthographic projection of B is within the range of the orthographic projection of A" or "the orthographic projection of A contains the orthographic projection of B" means that the boundary of the orthographic projection of B falls within the boundary range of the orthographic projection of A, or the boundary of the orthographic projection of A overlaps with the boundary of the orthographic projection of B.
[0091] In some exemplary embodiments, Figure 3 Taking the display substrate as an example, illustratively, the preparation process of the display substrate may include the following operations:
[0092] (1) The driving structure layer 20 and the film layer of the isolation groove 51 are formed.
[0093] A first buffer film and a first semiconductor film are sequentially deposited on the substrate 10, and the first semiconductor film is patterned by a patterning process to form a first buffer layer 21 covering the substrate 10, and a first semiconductor layer pattern disposed on the first buffer layer 21, wherein the first semiconductor layer pattern includes a plurality of first active layers 2011 located in the display area 100. After this patterning process, the transition area 300 includes the first buffer layer 21 disposed on the substrate 10. Figure 7a shown.
[0094] Subsequently, a first gate insulating film and a first gate metal film are sequentially deposited, and the first gate metal film is patterned by a patterning process to form a first gate insulating layer 22 covering the first semiconductor layer pattern, and a first gate metal layer pattern disposed on the first gate insulating layer 22, wherein the first gate metal layer pattern includes a plurality of first gate electrodes 2012 and a plurality of first plates 2031 located in the display area 100. After this patterning process, the transition area 300 includes a first buffer layer 21 and a first gate insulating layer 22 sequentially stacked on the substrate 10. Figure 7a shown.
[0095] Subsequently, a second gate insulating film and a second gate metal film are sequentially deposited, and the second gate metal film is patterned by a patterning process to form a second gate insulating layer 23 covering the first gate metal layer, and a second gate metal layer pattern disposed on the second gate insulating layer 23, wherein the second gate metal layer pattern includes a plurality of second electrodes 2032 located in the display area 100. The plurality of second electrodes 2032 are disposed opposite to the plurality of first electrodes 2031 and form a plurality of storage capacitors 203. After this patterning process, the transition area 300 includes a first buffer layer 21, a first gate insulating layer 22, and a second gate insulating layer 23 sequentially stacked on the substrate 10. Figure 7a shown.
[0096] Subsequently, a first interlayer insulating film and a second semiconductor film are deposited, and the second semiconductor film is patterned by a patterning process to form a first interlayer insulating layer 24 covering the second gate metal layer pattern, and a second semiconductor layer pattern disposed on the first interlayer insulating layer 24, wherein the second semiconductor layer pattern includes a plurality of second active layers 2021 located in the display area 100 and a barrier layer 513 located in the transition area 300. After this patterning process, the transition area 300 includes a first buffer layer 21, a first gate insulating layer 22, a second gate insulating layer 23, a first interlayer insulating layer 24, and a barrier layer 513 disposed on the first interlayer insulating layer 24, which are sequentially stacked on the substrate 10. Figure 7a shown.
[0097] Subsequently, a third gate insulating film and a third gate metal film are sequentially deposited, and the third gate metal film is patterned by a patterning process to form a third gate insulating layer 25 covering the second semiconductor layer pattern, and a third gate metal layer pattern disposed on the third gate insulating layer 25, wherein the third gate metal layer pattern includes a plurality of second gate electrodes 2022 located in the display area 100. After this patterning process, the transition area 300 includes a first buffer layer 21, a first gate insulating layer 22, a second gate insulating layer 23, a first interlayer insulating layer 24, a barrier layer 513, and a third gate insulating layer 25 covering the barrier layer 513, which are sequentially stacked on the substrate 10. Figure 7a shown.
[0098] Subsequently, a second interlayer insulating film is deposited, and the second interlayer insulating film is patterned by a patterning process to form a second interlayer insulating layer 26 pattern covering the third gate metal layer pattern. The second interlayer insulating layer 26 of the display area 100 is provided with a plurality of first via holes V1, a plurality of second via holes V2, a plurality of third via holes V3, and a plurality of fourth via holes V4, wherein the plurality of first via holes V1 expose one end of the plurality of first active layers 2011, the plurality of second via holes V2 expose the other end of the plurality of first active layers 2011, the plurality of third via holes V3 expose one end of the plurality of second active layers 2021, and the plurality of fourth via holes V4 expose the other end of the plurality of second active layers 2021; the second interlayer insulating layer 26 of the transition area 300 is provided with a groove 511 penetrating the third gate insulating layer 25 and exposing the barrier layer 513. After this patterning process, the transition region 300 includes a first buffer layer 21, a first gate insulating layer 22, a second gate insulating layer 23, a first interlayer insulating layer 24, a barrier layer 513, a third gate insulating layer 25 covering the barrier layer 513, and a second interlayer insulating layer 26 disposed on the third gate insulating layer 25, which are sequentially stacked on the substrate 10; the second interlayer insulating layer 26 of the transition region 300 is provided with a groove 511 penetrating the third gate insulating layer 25 and exposing the barrier layer 513. Figure 7a shown.
[0099] Subsequently, a first source-drain metal film is deposited and patterned by a patterning process to form a first source-drain metal layer pattern on the second interlayer insulating layer 26, wherein the first source-drain metal layer pattern includes a plurality of first source electrodes 2013, a plurality of first drain electrodes 2014, a plurality of second source electrodes 2023 and a plurality of second drain electrodes 2024 located in the display area 100, the first source electrode 2013 is connected to one end of the first active layer 2011 through a first via hole V1, the first drain electrode 2014 is connected to the other end of the first active layer 2011 through a second via hole V2, the second source electrode 2023 is connected to one end of the second active layer 2021 through a third via hole V3, and the second drain electrode 2024 is connected to the other end of the second active layer 2021 through a fourth via hole V4. The plurality of first active layers 2011, the plurality of first gate electrodes 2012, the plurality of first source electrodes 2013 and the plurality of first drain electrodes 2014 of the display area 100 form a plurality of first transistors 201, and the plurality of second active layers 2021, the plurality of second gate electrodes 2022, the plurality of second source electrodes 2023 and the plurality of second drain electrodes 2024 form a plurality of second transistors 202. Figure 7b As shown, Figure 7b A first transistor 201 and a second transistor 202 are used as an example.
[0100] The first source-drain metal layer may include a first metal layer, a second metal layer, and a third metal layer stacked in sequence in a direction away from the substrate 10. For example, the first metal layer and the third metal layer may be titanium layers, and the second metal layer may be an aluminum layer. Then, the first source electrode 2013, the first drain electrode 2014, the second source electrode 2023, and the second drain electrode 2024 all include a first metal layer, a second metal layer, and a third metal layer stacked in sequence in a direction away from the substrate 10.
[0101] Subsequently, a first flat film is coated and patterned by a patterning process to form a first flat layer 27 pattern covering the first source-drain metal layer pattern. The first flat layer 27 is provided with a fifth via hole V5 in the display area 100. The first flat layer 27 in the fifth via hole V5 is removed and the surface of the first source electrode 2013 or the first drain electrode 2014 is exposed. The first flat layer 27 pattern includes a filling layer 271 located in the transition area 300 and filled in the groove 511. The filling layer 271 can fill the groove 511. Figure 7c shown.
[0102] Subsequently, a second source-drain metal film is deposited, and the second source-drain metal film is patterned by a patterning process to form a second source-drain metal layer pattern on the first flat layer 27. The second source-drain metal layer pattern includes a plurality of anode connection electrodes 204 located in the display area 100 and a plurality of retaining edges 512 located in the transition area 300. The anode connection electrode 204 is connected to the first source electrode 2013 or the first drain electrode 2014 through the fifth via hole V5. The plurality of retaining edges 512 may include a first retaining edge 86 and a second retaining edge 87. The first retaining edge 86 is located on the second interlayer insulating layer 26 on the side of the groove 511 facing the display area 100, and a portion of the first retaining edge 86 is located on the filling layer 271. The second retaining edge 87 is located on the second interlayer insulating layer 26 on the side of the groove 511 facing the hole area, and a portion of the second retaining edge 87 is located on the filling layer 271. The distance between the first retaining edge 86 and the second retaining edge 87 in a direction parallel to the substrate 10 is less than the width of the notch of the groove 511. Figure 7d shown.
[0103] Among them, the film layer structure and material of the second source-drain metal layer can be the same as the film layer structure and material of the first source-drain metal layer. For example, the second source-drain metal layer can include a fourth metal layer, a fifth metal layer and a sixth metal layer stacked in sequence in a direction away from the substrate 10. For example, the fourth metal layer and the sixth metal layer can be titanium layers, and the fifth metal layer can be an aluminum layer.
[0104] Subsequently, a second flat film is coated and patterned by a patterning process to form a second flat layer 28 pattern covering the second source-drain metal layer pattern of the display area 100. The second flat layer 28 exposes the plurality of baffles 512 of the transition area 300 and the filling layer 271 in the groove 511. The second flat layer 28 is formed with a plurality of sixth via holes located in the display area 100. The second flat layer 28 in the sixth via hole is removed and the surface of the anode connection electrode 204 is exposed. Figure 7e shown.
[0105] At this point, the driving structure layer 20 and the film layer of the isolation groove 51 are prepared.
[0106] (2) Forming the light emitting structure layer 30. In an exemplary embodiment, forming the light emitting structure layer 30 may include:
[0107] A first electrode 31 thin film is deposited on the substrate 10 formed with the aforementioned pattern, and the first electrode 31 thin film is patterned by a patterning process to form a first electrode layer pattern, wherein the first electrode layer pattern includes a plurality of first electrodes 31 (anodes) located in the display area 100, and the first electrode 31 is connected to the anode connection electrode 204 through the sixth via hole on the second flat layer 28, so that the first electrode 31 is connected to the first source electrode 2013 or the first drain electrode 2014 through the anode connection electrode 204. Figure 7e shown.
[0108] Subsequently, a pixel defining film is coated on the substrate 10 with the aforementioned pattern formed thereon, and the pixel defining film is patterned by a patterning process to form a pixel defining layer 32 pattern, wherein the pixel defining layer 32 is provided with a plurality of pixel openings, and the pixel openings expose the surface of the first electrode 31 of the display area 100. Figure 7e shown.
[0109] Then, an etching process is used to remove the filling layer 271 in the groove 511. For example, oxygen etching can be used. Figure 7f shown.
[0110] Subsequently, on the substrate 10 on which the aforementioned pattern is formed, a plurality of film layers of the light-emitting functional layer 33 may be sequentially formed by an evaporation process. The light-emitting functional layer 33 may include a hole injection layer, a hole transport layer, an electron blocking layer, an organic light-emitting layer, a hole blocking layer, an electron transport layer and an electron injection layer sequentially arranged in a direction away from the substrate 10. Except for the organic light-emitting layer, the remaining film layers of the light-emitting functional layer 33 may be an integrated whole-surface structure, that is, the remaining film layers of the light-emitting functional layer 33 may be common layers of sub-pixels of different colors, and these common layers may be formed in the display area 100 and the transition area 300 during evaporation. Since an isolation groove 51 is provided in the transition area 300, these common layers will be disconnected at the isolation groove 51, thereby blocking the path for water and oxygen to be transmitted from the hole area 200 through the light-emitting functional layer 33 to the display area 100, thereby preventing water and oxygen from corroding the light-emitting functional layer 33 in the display area 100. Figure 3 shown.
[0111] Subsequently, on the substrate 10 formed with the aforementioned pattern, a second electrode (cathode) layer is formed by an evaporation process. The second electrode layer 34 of sub-pixels of different colors is a common layer connected as an integrated structure. The second electrode layer 34 can be formed in the display area 100 and the transition area 300. The second electrode layer 34 can be disconnected at the isolation groove 51, blocking the path of water and oxygen from the hole area 200 through the second electrode layer 34 to the display area 100, thereby preventing water and oxygen from corroding the second electrode layer 34 in the display area 100. Figure 3 shown.
[0112] At this point, the light emitting structure layer 30 is completed.
[0113] (3) Forming the encapsulation structure layer 40. In an exemplary embodiment, forming the encapsulation structure layer 40 may include:
[0114] On the substrate 10 formed with the aforementioned pattern, a first encapsulation film is first deposited by a deposition method using an open mask to form a first encapsulation layer 41 located in the display area 100 and the transition area 300. Subsequently, a second encapsulation material is printed by an inkjet printing process using an open mask to form a second encapsulation layer 42 located in the display area 100 and the transition area 300, wherein the isolation dam 60 in the transition area 300 can prevent ink overflow during the inkjet printing process. Subsequently, a third encapsulation film is deposited by a deposition method using an open mask to form a third encapsulation layer 43 located in the display area 100 and the transition area 300. The materials of the first encapsulation layer 41 and the third encapsulation layer 43 can be inorganic materials, and the materials of the second encapsulation layer 42 can be organic materials. Figure 3 shown.
[0115] Subsequently, film layers such as a touch control structure layer and a color filter layer may be formed in sequence on the side of the encapsulation structure layer 40 away from the substrate 10 .
[0116] In some other exemplary embodiments, Figure 5 Taking the display substrate as an example, illustratively, the preparation process of the display substrate may include the following operations:
[0117] (1) The driving structure layer 20 and the film layer of the isolation groove 51 are formed.
[0118] A first buffer film and a first semiconductor film are sequentially deposited on the substrate 10, and the first semiconductor film is patterned by a patterning process to form a first buffer layer 21 covering the substrate 10, and a first semiconductor layer pattern disposed on the first buffer layer 21, wherein the first semiconductor layer pattern includes a plurality of first active layers 2011 located in the display area 100. After this patterning process, the transition area 300 includes the first buffer layer 21 disposed on the substrate 10. Figure 8a shown.
[0119] Subsequently, a first gate insulating film and a first gate metal film are sequentially deposited, and the first gate metal film is patterned by a patterning process to form a first gate insulating layer 22 covering the first semiconductor layer pattern, and a first gate metal layer pattern disposed on the first gate insulating layer 22, wherein the first gate metal layer pattern includes a plurality of first gate electrodes 2012 and a plurality of first plates 2031 located in the display area 100. After this patterning process, the transition area 300 includes a first buffer layer 21 and a first gate insulating layer 22 sequentially stacked on the substrate 10. Figure 8a shown.
[0120] Subsequently, a second gate insulating film and a second gate metal film are sequentially deposited, and the second gate metal film is patterned by a patterning process to form a second gate insulating layer 23 covering the first gate metal layer, and a second gate metal layer pattern disposed on the second gate insulating layer 23, wherein the second gate metal layer pattern includes a plurality of second electrodes 2032 located in the display area 100. The plurality of second electrodes 2032 are disposed opposite to the plurality of first electrodes 2031 and form a plurality of storage capacitors 203. After this patterning process, the transition area 300 includes a first buffer layer 21, a first gate insulating layer 22, and a second gate insulating layer 23 sequentially stacked on the substrate 10. Figure 8a shown.
[0121] Subsequently, a first interlayer insulating film and a second semiconductor film are deposited, and the second semiconductor film is patterned by a patterning process to form a first interlayer insulating layer 24 covering the second gate metal layer pattern, and a second semiconductor layer pattern disposed on the first interlayer insulating layer 24, wherein the second semiconductor layer pattern includes a plurality of second active layers 2021 located in the display area 100 and a barrier layer 513 located in the transition area 300. After this patterning process, the transition area 300 includes a first buffer layer 21, a first gate insulating layer 22, a second gate insulating layer 23, a first interlayer insulating layer 24, and a barrier layer 513 disposed on the first interlayer insulating layer 24, which are sequentially stacked on the substrate 10. Figure 8a shown.
[0122] Subsequently, a third gate insulating film is sequentially deposited and patterned by a patterning process to form a third gate insulating layer 25 pattern covering the second semiconductor layer pattern. The third gate insulating layer 25 in the transition region 300 is provided with a first groove 81 surrounding the hole region 200. The first groove 81 at least partially exposes the barrier layer 513. Figure 8a shown.
[0123] Subsequently, a third gate metal film is deposited, and the third gate metal film is patterned by a patterning process to form a third gate metal layer pattern located on the third gate insulating layer 25. The third gate metal layer pattern includes a plurality of second gate electrodes 2022 located in the display area 100, and a first metal ring 84 and a second metal ring 85 located in the transition area 300. The first metal ring 84 and the second metal ring 85 are located on the side of the first groove 81 close to the display area 100 and the side close to the hole area 200, respectively. The edges of the first metal ring 84 and the second metal ring 85 close to the first groove 81 are set inward compared to the sidewall of the first groove 81. The portion of the third gate insulating layer 25 protruding from the edge of the first metal ring 84 close to the first groove 81 forms a first convex ring 91, and the portion of the third gate insulating layer 25 protruding from the edge of the second metal ring 85 close to the first groove 81 forms another first convex ring 91. A second groove 82 is formed between the first metal ring 84 and the second metal ring 85. Figure 8b shown.
[0124] Subsequently, a second interlayer insulating film is deposited, and the second interlayer insulating film is patterned by a patterning process to form a second interlayer insulating layer 26 pattern covering the third gate metal layer pattern. The second interlayer insulating layer 26 may include a first sublayer 261 and a second sublayer 262 stacked in sequence in a direction away from the substrate 10. The material of the first sublayer 261 may be silicon oxide, and the material of the second sublayer 262 may be silicon nitride. The second interlayer insulating layer 26 of the display area 100 is provided with a plurality of first via holes V1, a plurality of second via holes V2, a plurality of third via holes V3, and a plurality of fourth via holes V4. The plurality of first via holes V1 expose one end of the plurality of first active layers 2011, the plurality of second via holes V2 expose the other end of the plurality of first active layers 2011, the plurality of third via holes V3 expose one end of the plurality of second active layers 2021, and the plurality of fourth via holes V4 expose the other end of the plurality of second active layers 2021; the second interlayer insulating layer 26 of the transition area 300 is provided with a first via hole V1 exposing the first groove 81 and the second groove 82. Three grooves 83, the first sub-layer 261 is protruding from the second sub-layer 262 on the side wall of the third groove 83 (the etching solution or etching gas has different selection ratios for the first sub-layer 261 and the second sub-layer 262 during the etching process, thereby forming a stepped side wall of the third groove 83), a second convex ring 92 is formed on the side wall of the third groove 83 near the display area 100, and another second convex ring 92 is formed on the side wall of the third groove 83 near the hole area 200, where the first sub-layer 261 protrudes from the second sub-layer 262. The two second convex rings 92 are also protruding from the first metal ring 84 and the second metal ring 85, respectively. Figure 8c shown.
[0125] Subsequently, a first source-drain metal film is deposited and patterned by a patterning process to form a first source-drain metal layer pattern on the second interlayer insulating layer 26, wherein the first source-drain metal layer pattern includes a plurality of first source electrodes 2013, a plurality of first drain electrodes 2014, a plurality of second source electrodes 2023 and a plurality of second drain electrodes 2024 located in the display area 100, the first source electrode 2013 is connected to one end of the first active layer 2011 through a first via hole V1, the first drain electrode 2014 is connected to the other end of the first active layer 2011 through a second via hole V2, the second source electrode 2023 is connected to one end of the second active layer 2021 through a third via hole V3, and the second drain electrode 2024 is connected to the other end of the second active layer 2021 through a fourth via hole V4. The plurality of first active layers 2011, the plurality of first gate electrodes 2012, the plurality of first source electrodes 2013 and the plurality of first drain electrodes 2014 of the display area 100 form a plurality of first transistors 201, and the plurality of second active layers 2021, the plurality of second gate electrodes 2022, the plurality of second source electrodes 2023 and the plurality of second drain electrodes 2024 form a plurality of second transistors 202. Figure 8d As shown, Figure 8d A first transistor 201 and a second transistor 202 are used as an example.
[0126] The first source-drain metal layer may include a first metal layer, a second metal layer, and a third metal layer stacked in sequence in a direction away from the substrate 10. For example, the first metal layer and the third metal layer may be titanium layers, and the second metal layer may be an aluminum layer. Then, the first source electrode 2013, the first drain electrode 2014, the second source electrode 2023, and the second drain electrode 2024 all include a first metal layer, a second metal layer, and a third metal layer stacked in sequence in a direction away from the substrate 10.
[0127] Subsequently, a first flat film is coated and patterned by a patterning process to form a first flat layer 27 pattern covering the first source-drain metal layer pattern. The first flat layer 27 is provided with a fifth via hole V5 in the display area 100. The first flat layer 27 in the fifth via hole V5 is removed and the surface of the first source electrode 2013 or the first drain electrode 2014 is exposed. The first flat layer 27 pattern includes a filling layer 271 located in the transition area 300 and filled in the third groove 83, the second groove 82 and the first groove 81. The filling layer 271 can fill the third groove 83. Figure 8e shown.
[0128] Subsequently, a second source-drain metal film is deposited, and the second source-drain metal film is patterned by a patterning process to form a second source-drain metal layer pattern on the first flat layer 27. The second source-drain metal layer pattern includes a plurality of anode connection electrodes 204 located in the display area 100 and a first stop edge 86 and a second stop edge 87 located in the transition area 300. The anode connection electrode 204 is connected to the first source electrode 2013 or the first drain electrode 2014 through a fifth via hole V5. The first stop edge 86 and the second stop edge 87 are respectively located on the side of the third groove 83 close to the display area 100 and the side close to the hole area 200. The first stop edge 86 and the second stop edge 87 are both partially located on the second interlayer insulating layer 26 and the other part is located on the filling layer 271. Among them, the third groove 83, the second groove 82 and the first groove 81 form the groove 511 of the isolation groove 51, and the first stop edge 86 and the second stop edge 87 are both partially located above the groove 511 (that is, the side of the groove 511 away from the substrate 10). As shown in FIG. Figure 8f shown.
[0129] The film structure and material of the second source-drain metal layer may be the same as those of the first source-drain metal layer. For example, the second source-drain metal layer may include a fourth metal layer, a fifth metal layer, and a sixth metal layer stacked in sequence in a direction away from the substrate 10. For example, the fourth metal layer and the sixth metal layer may be titanium layers, and the fifth metal layer may be aluminum layers. Then, the connecting electrode 204, the first stop edge 86, and the second stop edge 87 all include a fourth metal layer, a fifth metal layer, and a sixth metal layer stacked in sequence in a direction away from the substrate 10. Figure 8f shown.
[0130] Subsequently, a second flat film is coated and patterned using a patterning process to form a second flat layer 28 pattern covering the second source-drain metal layer pattern of the display area 100. The second flat layer 28 is formed with a plurality of sixth via holes located in the display area 100. The second flat layer 28 in the sixth via hole is removed to expose the surface of the anode connection electrode 204. Figure 8g shown.
[0131] At this point, the driving structure layer 20 and the film layer of the isolation groove 51 are prepared.
[0132] (2) Forming the light emitting structure layer 30. In an exemplary embodiment, forming the light emitting structure layer 30 may include:
[0133] A first electrode 31 thin film is deposited on the substrate 10 formed with the aforementioned pattern, and the first electrode 31 thin film is patterned by a patterning process to form a first electrode layer pattern, wherein the first electrode layer pattern includes a plurality of first electrodes 31 (anodes) located in the display area 100, and the first electrode 31 is connected to the anode connection electrode 204 through the sixth via hole on the second flat layer 28, so that the first electrode 31 is connected to the first source electrode 2013 or the first drain electrode 2014 through the anode connection electrode 204. Figure 8g shown.
[0134] In the process of patterning the first electrode 31 film (such as a wet etching process), the fifth metal layer of the first stop edge 86 and the second stop edge 87 can be etched laterally at the same time, so that the fifth metal layer of the first stop edge 86 and the second stop edge 87 is partially retracted compared to the fourth metal layer and the sixth metal layer (that is, the fourth metal layer and the sixth metal layer protrude compared to the fifth metal layer) on the side of the first stop edge 86 and the second stop edge 87 close to the groove 511 of the isolation groove 51, as shown in FIG. Figure 8gIn other embodiments, during the aforementioned patterning process (such as the development process) of the second flat film, the fifth metal layer of the first stop edge 86 and the second stop edge 87 can be etched laterally, so that the fifth metal layer of the first stop edge 86 and the second stop edge 87 is partially retracted compared to the fourth metal layer and the sixth metal layer on the side of the first stop edge 86 and the second stop edge 87 close to the groove 511 of the isolation groove 51.
[0135] Subsequently, a pixel defining film is coated on the substrate 10 with the aforementioned pattern formed thereon, and the pixel defining film is patterned by a patterning process to form a pixel defining layer 32 pattern, wherein the pixel defining layer 32 is provided with a plurality of pixel openings, and the pixel openings expose the surface of the first electrode 31 of the display area 100. Figure 8h shown.
[0136] Then, an etching process (dry etching or wet etching, such as etching using oxygen) is used to etch away the filling layer 271 in the groove 511 of the isolation trench 51. Figure 8i At this point, the isolation trench 51 structure is formed.
[0137] Subsequently, on the substrate 10 on which the aforementioned pattern is formed, a plurality of film layers of the light-emitting functional layer 33 may be sequentially formed by an evaporation process. The light-emitting functional layer 33 may include a hole injection layer, a hole transport layer, an electron blocking layer, an organic light-emitting layer, a hole blocking layer, an electron transport layer and an electron injection layer sequentially arranged in a direction away from the substrate 10. Except for the organic light-emitting layer, the remaining film layers of the light-emitting functional layer 33 may be an integrated whole-surface structure, that is, the remaining film layers of the light-emitting functional layer 33 may be common layers of sub-pixels of different colors, and these common layers may be formed in the display area 100 and the transition area 300 during evaporation. Since an isolation groove 51 is provided in the transition area 300, these common layers will be disconnected at the isolation groove 51, thereby blocking the path for water and oxygen to be transmitted from the hole area 200 through the light-emitting functional layer 33 to the display area 100, thereby preventing water and oxygen from corroding the light-emitting functional layer 33 in the display area 100. Figure 5 shown.
[0138] Subsequently, on the substrate 10 formed with the aforementioned pattern, a second electrode (cathode) layer is formed by an evaporation process. The second electrode layer 34 of sub-pixels of different colors is a common layer connected as an integrated structure. The second electrode layer 34 can be formed in the display area 100 and the transition area 300. The second electrode layer 34 can be disconnected at the isolation groove 51, blocking the path of water and oxygen from the hole area 200 through the second electrode layer 34 to the display area 100, thereby preventing water and oxygen from corroding the second electrode layer 34 in the display area 100. Figure 5 shown.
[0139] At this point, the light emitting structure layer 30 is completed.
[0140] (3) Forming the encapsulation structure layer 40. In an exemplary embodiment, forming the encapsulation structure layer 40 may include:
[0141] On the substrate 10 formed with the aforementioned pattern, a first encapsulation film is first deposited by a deposition method using an open mask to form a first encapsulation layer 41 located in the display area 100 and the transition area 300. Subsequently, a second encapsulation material is printed by an inkjet printing process using an open mask to form a second encapsulation layer 42 located in the display area 100 and the transition area 300, wherein the isolation dam 60 in the transition area 300 can prevent ink overflow during the inkjet printing process. Subsequently, a third encapsulation film is deposited by a deposition method using an open mask to form a third encapsulation layer 43 located in the display area 100 and the transition area 300. The materials of the first encapsulation layer 41 and the third encapsulation layer 43 can be inorganic materials, and the materials of the second encapsulation layer 42 can be organic materials. Figure 5 shown.
[0142] Subsequently, film layers such as a touch control structure layer and a color filter layer may be formed in sequence on the side of the encapsulation structure layer 40 away from the substrate 10 .
[0143] based on Figure 3 and Figure 5 The present disclosure also provides a method for preparing a display substrate. Figure 3 and Figure 5 An exemplary method of displaying a substrate includes:
[0144] forming a first structural layer and a second structural layer on the substrate of the transition zone in sequence, wherein the first structural layer comprises a barrier layer, and the second structural layer is provided with a groove, wherein the groove penetrates the second structural layer and exposes at least a portion of the surface of the barrier layer;
[0145] forming a filling layer in the groove, wherein the filling layer fills the groove;
[0146] forming a stop edge on a surface of the second structural layer away from the substrate, wherein a portion of the stop edge extends in a direction parallel to the substrate to a surface of the filling layer away from the substrate;
[0147] The filling layer is removed.
[0148] In some exemplary embodiments, the guard edge includes a fourth metal layer, a fifth metal layer, and a sixth metal layer stacked in sequence in a direction away from the substrate, and the method further includes etching the fifth metal layer of the guard edge so that the fifth metal layer is retracted inward compared to the fourth metal layer and the sixth metal layer on the side of the guard edge close to the groove.
[0149] In some further exemplary embodiments, Figure 6Taking the display substrate as an example, illustratively, the preparation process of the display substrate may include the following operations:
[0150] (1) The driving structure layer 20 and the film layer of the isolation column 52 are formed.
[0151] A first buffer film and a first semiconductor film are sequentially deposited on the substrate 10, and the first semiconductor film is patterned by a patterning process to form a first buffer layer 21 covering the substrate 10, and a first semiconductor layer pattern disposed on the first buffer layer 21, wherein the first semiconductor layer pattern includes a plurality of first active layers 2011 located in the display area 100. After this patterning process, the transition area 300 includes the first buffer layer 21 disposed on the substrate 10. Figure 9a shown.
[0152] Subsequently, a first gate insulating film and a first gate metal film are sequentially deposited, and the first gate metal film is patterned by a patterning process to form a first gate insulating layer 22 covering the first semiconductor layer pattern, and a first gate metal layer pattern disposed on the first gate insulating layer 22, wherein the first gate metal layer pattern includes a plurality of first gate electrodes 2012 and a plurality of first plates 2031 located in the display area 100. After this patterning process, the transition area 300 includes a first buffer layer 21 and a first gate insulating layer 22 sequentially stacked on the substrate 10. Figure 9a shown.
[0153] Subsequently, a second gate insulating film and a second gate metal film are sequentially deposited, and the second gate metal film is patterned by a patterning process to form a second gate insulating layer 23 covering the first gate metal layer, and a second gate metal layer pattern disposed on the second gate insulating layer 23, wherein the second gate metal layer pattern includes a plurality of second electrodes 2032 located in the display area 100. The plurality of second electrodes 2032 are disposed opposite to the plurality of first electrodes 2031 and form a plurality of storage capacitors 203. After this patterning process, the transition area 300 includes a first buffer layer 21, a first gate insulating layer 22, and a second gate insulating layer 23 sequentially stacked on the substrate 10. Figure 9a shown.
[0154] Subsequently, a first interlayer insulating film and a second semiconductor film are deposited, and the second semiconductor film is patterned by a patterning process to form a first interlayer insulating layer 24 covering the second gate metal layer pattern, and a second semiconductor layer pattern disposed on the first interlayer insulating layer 24, wherein the second semiconductor layer pattern includes a plurality of second active layers 2021 located in the display area 100 and a barrier layer 513 located in the transition area 300. After this patterning process, the transition area 300 includes a first buffer layer 21, a first gate insulating layer 22, a second gate insulating layer 23, a first interlayer insulating layer 24, and a barrier layer 513 disposed on the first interlayer insulating layer 24, which are sequentially stacked on the substrate 10. Figure 9a shown.
[0155] Subsequently, a third gate insulating film and a third gate metal film are sequentially deposited, and the third gate metal film is patterned by a patterning process to form a third gate insulating layer 25 covering the second semiconductor layer pattern, and a third gate metal layer pattern disposed on the third gate insulating layer 25, wherein the third gate metal layer pattern includes a plurality of second gate electrodes 2022 located in the display area 100. After this patterning process, the transition area 300 includes a first buffer layer 21, a first gate insulating layer 22, a second gate insulating layer 23, a first interlayer insulating layer 24, a barrier layer 513, and a third gate insulating layer 25 covering the barrier layer 513, which are sequentially stacked on the substrate 10. Figure 9a shown.
[0156] Subsequently, a second interlayer insulating film is deposited, and the second interlayer insulating film is patterned by a patterning process to form a second interlayer insulating layer 26 pattern covering the third gate metal layer pattern. The second interlayer insulating layer 26 of the display area 100 is provided with a plurality of first via holes V1, a plurality of second via holes V2, a plurality of third via holes V3, and a plurality of fourth via holes V4. The plurality of first via holes V1 expose one end of the plurality of first active layers 2011, the plurality of second via holes V2 expose the other end of the plurality of first active layers 2011, the plurality of third via holes V3 expose one end of the plurality of second active layers 2021, and the plurality of fourth via holes V4 expose the other end of the plurality of second active layers 2021. The second interlayer insulating layer 26 of the transition area 300 is provided with a plurality of grooves penetrating the third gate insulating layer 25 and exposing the barrier layer 513. A column base 523 of the isolation column 52 located on the barrier layer 513 is formed between adjacent grooves. The column base 523 includes the stacked third gate insulating layer 25 and the second interlayer insulating layer 26. Figure 9a shown.
[0157] Subsequently, a first source-drain metal film is deposited, and the first source-drain metal film is patterned by a patterning process to form a first source-drain metal layer pattern on the second interlayer insulating layer 26. The first source-drain metal layer pattern includes a plurality of first source electrodes 2013, a plurality of first drain electrodes 2014, a plurality of second source electrodes 2023, and a plurality of second drain electrodes 2024 located in the display area 100, and a first isolation layer 71 located on the column base 523 of the transition area 300 and a retaining wall 72 located on the second interlayer insulating layer 26. The side of the retaining wall 72 close to the groove may be flush with the side of the groove. The first source electrode 2013 is connected to one end of the first active layer 2011 through the first via hole V1, the first drain electrode 2014 is connected to the other end of the first active layer 2011 through the second via hole V2, the second source electrode 2023 is connected to one end of the second active layer 2021 through the third via hole V3, and the second drain electrode 2024 is connected to the other end of the second active layer 2021 through the fourth via hole V4. The plurality of first active layers 2011, the plurality of first gate electrodes 2012, the plurality of first source electrodes 2013 and the plurality of first drain electrodes 2014 of the display area 100 form a plurality of first transistors 201, and the plurality of second active layers 2021, the plurality of second gate electrodes 2022, the plurality of second source electrodes 2023 and the plurality of second drain electrodes 2024 form a plurality of second transistors 202. Figure 9b As shown, Figure 9b A first transistor 201 and a second transistor 202 are used as an example.
[0158] The first source-drain metal layer may include a first metal layer, a second metal layer, and a third metal layer stacked in sequence in a direction away from the substrate 10. For example, the first metal layer and the third metal layer may be titanium layers, and the second metal layer may be an aluminum layer. Then, the first source electrode 2013, the first drain electrode 2014, the second source electrode 2023, the second drain electrode 2024, the first isolation layer 71, and the retaining wall 72 all include a first metal layer, a second metal layer, and a third metal layer stacked in sequence in a direction away from the substrate 10.
[0159] Subsequently, a first flat film is coated and patterned by a patterning process to form a first flat layer 27 pattern covering the first source-drain metal layer pattern of the display area 100. The first flat layer 27 is provided with a fifth via hole V5 in the display area 100. The first flat layer 27 in the fifth via hole V5 is removed and the surface of the first source electrode 2013 or the first drain electrode 2014 is exposed. The first flat layer 27 pattern includes a filling layer 271 located in the transition area 300 and filled in the groove. The filling layer 271 can fill the groove, and the surface of the filling layer 271 away from the substrate 10 can be flush with the surface of the first isolation layer 71 and the retaining wall 72 away from the substrate 10. Fig.9c shown.
[0160] Subsequently, a second source-drain metal film is deposited, and the second source-drain metal film is patterned by a patterning process to form a second source-drain metal layer pattern on the first flat layer 27. The second source-drain metal layer pattern includes a plurality of anode connection electrodes 204 located in the display area 100 and a second isolation layer 73 located on the first isolation layer 71 in the transition area 300. The anode connection electrode 204 is connected to the first source electrode 2013 or the first drain electrode 2014 through the fifth via hole V5. The second isolation layer 73 is also partially located on the filling layer 271. The side of the second isolation layer 73 facing the display area 100 and / or the hole area 200 protrudes from the corresponding side of the first isolation layer 71. Figure 9d shown.
[0161] The film structure and material of the second source-drain metal layer may be the same as those of the first source-drain metal layer. For example, the second source-drain metal layer may include a fourth metal layer, a fifth metal layer, and a sixth metal layer stacked in sequence in a direction away from the substrate 10. For example, the fourth metal layer and the sixth metal layer may be titanium layers, and the fifth metal layer may be an aluminum layer. Then, the anode connection electrode 204 and the second isolation layer 73 both include a fourth metal layer, a fifth metal layer, and a sixth metal layer stacked in sequence in a direction away from the substrate 10.
[0162] Subsequently, a second flat film is coated and patterned using a patterning process to form a second flat layer 28 pattern covering the second source-drain metal layer pattern of the display area 100. The second flat layer 28 is formed with a plurality of sixth via holes located in the display area 100. The second flat layer 28 in the sixth via hole is removed to expose the surface of the anode connection electrode 204. Fig.9e shown.
[0163] At this point, the driving structure layer 20 and the film layer of the isolation column 52 are prepared.
[0164] (2) Forming the light emitting structure layer 30. In an exemplary embodiment, forming the light emitting structure layer 30 may include:
[0165] A first electrode 31 thin film is deposited on the substrate 10 on which the aforementioned pattern is formed, and the first electrode 31 thin film is patterned through a patterning process to form a first electrode layer pattern. The first electrode layer pattern includes a plurality of first electrodes 31 (anodes) located in the display area 100. The first electrode 31 is connected to the anode connecting electrode 204 through a sixth via hole on the second flat layer 28, so that the first electrode 31 is connected to the first source electrode 2013 or the first drain electrode 2014 through the anode connecting electrode 204.
[0166] In the process of patterning the first electrode 31 film (such as a wet etching process), the fifth metal layer of the second isolation layer 73 can be etched laterally at the same time, so that on the side of the second isolation layer 73 facing the display area 100 and the hole area 200, the fifth metal layer of the second isolation layer 73 is partially retracted compared to the fourth metal layer and the sixth metal layer, such as Fig.9e In other embodiments, during the aforementioned patterning process (such as the development process) of the second flat film, the fifth metal layer of the second isolation layer 73 can be laterally etched, so that the fifth metal layer of the second isolation layer 73 is partially retracted compared to the fourth metal layer and the sixth metal layer on the side of the second isolation layer 73 facing the display area 100 and the hole area 200.
[0167] Subsequently, a pixel defining film is coated on the substrate 10 with the aforementioned pattern formed thereon, and the pixel defining film is patterned by a patterning process to form a pixel defining layer 32 pattern, wherein the pixel defining layer 32 is provided with a plurality of pixel openings, and the pixel openings expose the surface of the first electrode 31 of the display area 100. Figure 9f shown.
[0168] Subsequently, an etching process (dry etching or wet etching, for example, oxygen can be used as an etching gas) is used to etch away the filling layer 271 in the groove. At the same time, a portion of the fifth metal layer of the second isolation layer 73 and the second metal layer of the first isolation layer 71 are both laterally etched, so that on the side of the second isolation layer 73 and the first isolation layer 71 facing the display area 100 and the hole area 200, a portion of the fifth metal layer of the second isolation layer 73 is retracted compared to the fourth metal layer and the sixth metal layer, and a portion of the second metal layer of the first isolation layer 71 is retracted compared to the first metal layer and the third metal layer, so that the first isolation layer 71 becomes the first isolation portion 521 of the isolation column 52, and the second isolation layer 73 becomes the second isolation portion 522 of the isolation column 52. The column base 523, the first isolation portion 521 and the second isolation portion 522 form the isolation column 52. Figure 9g shown.
[0169] Subsequently, on the substrate 10 on which the aforementioned pattern is formed, a plurality of film layers of the light-emitting functional layer 33 may be sequentially formed by an evaporation process. The light-emitting functional layer 33 may include a hole injection layer, a hole transport layer, an electron blocking layer, an organic light-emitting layer, a hole blocking layer, an electron transport layer and an electron injection layer sequentially arranged in a direction away from the substrate 10. Except for the organic light-emitting layer, the remaining film layers of the light-emitting functional layer 33 may be an integrated whole-surface structure, that is, the remaining film layers of the light-emitting functional layer 33 may be common layers of sub-pixels of different colors, and these common layers may be formed in the display area 100 and the transition area 300 during evaporation. Since the isolation columns 52 are provided in the transition area 300, these common layers will be disconnected at the isolation columns 52, thereby blocking the path for water and oxygen to be transmitted from the hole area 200 through the light-emitting functional layer 33 to the display area 100, thereby preventing water and oxygen from corroding the light-emitting functional layer 33 in the display area 100. Figure 6 shown.
[0170] Subsequently, a second electrode (cathode) layer is formed on the substrate 10 with the aforementioned pattern by an evaporation process. The second electrode layer 34 of sub-pixels of different colors is a common layer connected as an integrated structure. The second electrode layer 34 can be formed in the display area 100 and the transition area 300. The second electrode layer 34 can be disconnected at the isolation column 52, blocking the path for water and oxygen to be transmitted from the hole area 200 through the second electrode layer 34 to the display area 100, thereby preventing water and oxygen from corroding the second electrode layer 34 in the display area 100. Figure 6 shown.
[0171] At this point, the light emitting structure layer 30 is completed.
[0172] (3) Forming the encapsulation structure layer 40. In an exemplary embodiment, forming the encapsulation structure layer 40 may include:
[0173] On the substrate 10 formed with the aforementioned pattern, a first encapsulation film is first deposited by a deposition method using an open mask to form a first encapsulation layer 41 located in the display area 100 and the transition area 300. Subsequently, a second encapsulation material is printed by an inkjet printing process using an open mask to form a second encapsulation layer 42 located in the display area 100 and the transition area 300, wherein the isolation dam 60 in the transition area 300 can prevent ink overflow during the inkjet printing process. Subsequently, a third encapsulation film is deposited by a deposition method using an open mask to form a third encapsulation layer 43 located in the display area 100 and the transition area 300. The materials of the first encapsulation layer 41 and the third encapsulation layer 43 can be inorganic materials, and the materials of the second encapsulation layer 42 can be organic materials. Figure 6 shown.
[0174] Subsequently, film layers such as a touch control structure layer and a color filter layer may be formed in sequence on the side of the encapsulation structure layer 40 away from the substrate 10 .
[0175] The present disclosure also provides a display device, including the display substrate described in any of the above embodiments. The display device can be any product or component with a display function, such as a mobile phone, a tablet computer, a television, a monitor, a notebook computer, a digital photo frame, a navigator, etc.
[0176] In the drawings, the size of the components, the thickness of the layers, or the regions are sometimes exaggerated for the sake of clarity. Therefore, the embodiments of the present disclosure are not necessarily limited to the dimensions, and the shape and size of each component in the drawings do not reflect the true proportions. In addition, the drawings schematically show some examples, and the embodiments of the present disclosure are not limited to the shapes or values shown in the drawings.
[0177] In the description of this article, "parallel" refers to a state where the angle formed by two straight lines is greater than -10° and less than 10°, and therefore includes a state where the angle is greater than -5° and less than 5°. In addition, "perpendicular" refers to a state where the angle formed by two straight lines is greater than 80° and less than 100°, and therefore includes a state where the angle is greater than 85° and less than 95°.
[0178] In the description herein, the terms "upper", "lower", "left", "right", "top", "inside", "outside", "axial", "four corners", etc., indicating orientations or positional relationships are based on the orientations or positional relationships shown in the accompanying drawings, and are merely simplified descriptions for the convenience of describing the embodiments of the present disclosure, rather than indicating or implying that the referred structure has a specific orientation, is constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present disclosure.
[0179] In the description herein, unless otherwise clearly specified and limited, the terms "connection", "fixed connection", "installation", and "assembly" should be understood in a broad sense, for example, it can be a fixed connection, or a detachable connection, or an integral connection; the terms "installation", "connection", and "fixed connection" can be a direct connection, or an indirect connection through an intermediate medium, or the internal communication of two elements. For ordinary technicians in this field, the meanings of the above terms in the embodiments of the present disclosure can be understood according to the circumstances.
Claims
1. A display substrate, characterized in that: The device comprises a hole area, a transition area surrounding the hole area, and a display area surrounding the transition area; the transition area is provided with an isolation structure surrounding the hole area, and the isolation structure comprises at least one isolation groove; The display substrate includes a base, the isolation groove includes a groove and a blocking edge provided on the side of the groove away from the base; in a direction perpendicular to the base, the transition zone includes a first structural layer and a second structural layer stacked in sequence in a direction away from the base, the first structural layer includes a blocking layer, the groove penetrates the second structural layer and exposes at least a portion of the surface of the blocking layer, the blocking edge is provided on the surface of the second structural layer away from the base, and a portion of the blocking edge extends in a direction parallel to the base and protrudes from the sidewall of the groove.
2. The display substrate according to claim 1, wherein The retaining edge includes a fourth metal layer, a fifth metal layer and a sixth metal layer arranged in sequence along a direction away from the base. On the side of the retaining edge close to the groove, the fifth metal layer is set inward compared to the fourth metal layer and the sixth metal layer.
3. The display substrate according to claim 1, wherein The display area includes a driving structure layer and a light-emitting structure layer sequentially stacked on the substrate, the driving structure layer includes a pixel driving circuit, the pixel driving circuit includes a plurality of transistors and a storage capacitor, the light-emitting structure layer includes a plurality of light-emitting elements, and the light-emitting elements include a first electrode, a light-emitting functional layer, and a second electrode layer sequentially stacked in a direction away from the substrate; In a direction perpendicular to the substrate, the driving structure layer includes a first source-drain metal layer, a first planar layer, a second source-drain metal layer, and a second planar layer, which are sequentially arranged in a direction away from the substrate; the first source-drain metal layer includes a first source electrode and a first drain electrode of the first transistor; the second source-drain metal layer includes a connecting electrode connected to the first source electrode or the first drain electrode, and the connecting electrode is also connected to the first electrode; The blocking edge is provided in the same layer as the connecting electrode, or the blocking edge is provided in the same layer as the first source electrode and the first drain electrode.
4. The display substrate according to claim 3, wherein: In a direction perpendicular to the substrate, the driving structure layer further includes a first semiconductor layer, a first gate metal layer, and a second gate metal layer, which are arranged on a side of the first source / drain metal layer close to the substrate; the first semiconductor layer includes a first active layer of the first transistor, the first gate metal layer includes a first gate electrode of the first transistor and one plate of the storage capacitor, and the second gate metal layer includes the other plate of the storage capacitor; The barrier layer is provided in the same layer as the first active layer, the first gate metal layer or the second gate metal layer.
5. The display substrate according to claim 3, wherein: In a direction perpendicular to the substrate, the driving structure layer further includes a first semiconductor layer, a first gate metal layer, a second gate metal layer, a second semiconductor layer, and a third gate metal layer, which are arranged on a side of the first source-drain metal layer close to the substrate; the first semiconductor layer includes a first active layer of the first transistor, the first gate metal layer includes a first gate electrode of the first transistor and one plate of the storage capacitor, the second gate metal layer includes another plate of the storage capacitor, the second semiconductor layer includes a second active layer of the second transistor, and the third gate metal layer includes a second gate electrode of the second transistor; the first source-drain metal layer also includes a second source electrode and a second drain electrode of the second transistor; The barrier layer is provided in the same layer as any one of the first active layer, the first gate metal layer, the second gate metal layer, the second active layer and the third gate metal layer.
6. The display substrate according to claim 1, wherein The second structural layer includes a plurality of stacked inorganic insulating layers, or the second structural layer includes at least one inorganic insulating layer and at least one metal layer.
7. The display substrate according to claim 6, wherein: One or more convex rings are provided on the sidewall of the groove. The multiple convex rings are arranged in sequence along a direction perpendicular to the substrate. The convex rings are formed by the inorganic insulating layer.
8. The display substrate according to claim 3, wherein: The isolation structure further includes at least one isolation column; the isolation column includes a first isolation portion and a second isolation portion sequentially arranged in a direction away from the substrate, and the second isolation portion is protruding from the first isolation portion on a side of the isolation column facing the display area and / or the hole area; The material of the first isolation part is an inorganic insulating material, and the material of the second isolation part is a metal material; the second isolation part is arranged on the same layer as the first source electrode and the first drain electrode; or, the second isolation part is arranged on the same layer as the connecting electrode; or, the second isolation part includes a first sub-isolation part and a second sub-isolation part stacked in sequence along a direction away from the substrate, the first sub-isolation part is arranged on the same layer as the first source electrode and the first drain electrode, and the second sub-isolation part is arranged on the same layer as the connecting electrode.
9. The display substrate according to claim 8, wherein: An isolation column is formed between two adjacent isolation grooves. The blocking edge is provided in the same layer and made of the same material as the second isolation portion. The second structural layer between two adjacent grooves is the first isolation portion.
10. The display substrate according to claim 9, wherein The two adjacent barrier layers are not connected, and at least a portion of an orthographic projection of the second isolation portion on the substrate does not overlap with the orthographic projections of the two adjacent barrier layers on the substrate.
11. The display substrate according to claim 9, wherein At least two adjacent barrier layers are connected as one, and the orthographic projections of the at least two adjacent barrier layers connected as one on the substrate include the orthographic projection of at least one isolation column on the substrate.
12. The display substrate according to claim 3, wherein The isolation structure further includes at least one isolation column; the isolation column includes a first isolation portion and a second isolation portion sequentially arranged in a direction away from the substrate, and the second isolation portion is protruding from the first isolation portion on a side of the isolation column facing the display area and / or the hole area; The first isolation portion and the second isolation portion are both made of metal material, the first isolation portion is provided on the same layer as the first source electrode and the first drain electrode, and the second isolation portion is provided on the same layer as the connection electrode; The isolation column further includes a column base provided on a side of the first isolation portion facing the substrate, and the column base includes at least one inorganic insulating layer.
13. The display substrate according to claim 12, wherein: The first isolation portion includes a first metal layer, a second metal layer, and a third metal layer sequentially arranged in a direction away from the substrate, and on a side of the isolation column facing the display area and / or the hole area, the second metal layer is set back in comparison with the first metal layer and the third metal layer; Or / and, the second isolation portion includes a fourth metal layer, a fifth metal layer and a sixth metal layer arranged in sequence along a direction away from the substrate, and on the side of the isolation column facing the display area and / or the hole area, the fifth metal layer is retracted compared to the fourth metal layer and the sixth metal layer.
14. The display substrate according to claim 8, wherein The first isolation portion includes a silicon oxide film layer and a silicon nitride film layer stacked in sequence in a direction away from the substrate, and the thickness of the silicon nitride film layer is 0.5um to 1um.
15. A display device, characterized in that: The display substrate comprises the display substrate according to any one of claims 1 to 14.
16. A method for preparing the display substrate according to claim 1, characterized in that: include: forming a first structural layer and a second structural layer in sequence on the substrate of the transition region, wherein the first structural layer includes a barrier layer, and the second structural layer is provided with a groove, wherein the groove penetrates the second structural layer and exposes at least a portion of the surface of the barrier layer; forming a filling layer in the groove, wherein the filling layer fills the groove; forming a retaining edge on a surface of the second structural layer away from the substrate, wherein a portion of the retaining edge extends in a direction parallel to the substrate to a surface of the filling layer away from the substrate; The filling layer is removed.