Modified phenolic resin foaming grinding wheel and preparation method thereof

The grinding wheel prepared by modified phenolic resin and high-temperature foaming process solves the brittleness and toxicity problems of existing phenolic resin grinding wheels, achieving high strength, durability and simplified production effects.

CN118875980APending Publication Date: 2024-11-01BAIGE ABRASIVES CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202411376013.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-30
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

The existing phenolic foam resin grinding wheels have high brittleness, low strength, low elasticity, short service life, and complex low-temperature foaming methods, which are toxic and harmful, resulting in large mold corrosion and damage during the production process.

Method used

Modified phenolic resin is made of polyurethane modified phenolic resin, hexamethylenetetramine, surfactant, glass hollow microbeads, glycerin and diluent, etc. The grinding wheel is prepared through a high-temperature foaming and curing process to form uniform pores and High strength grinding wheel.

Benefits of technology

It realizes a non-toxic and harmless grinding wheel with high elasticity, high strength and uniform air pores, improves the durability and cutting force of the grinding wheel, simplifies the production process, and reduces the damage to the mold and production costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure FT_1
    Figure FT_1
  • Figure SMS_1
    Figure SMS_1
Patent Text Reader

Abstract

The invention relates to a modified phenolic resin foaming grinding wheel which is prepared from the following raw materials in percentage by weight: 30%-40% of modified phenolic resin, 2%-4% of hexamethylenetetramine, 2%-6% of a surfactant, 2%-5% of glass hollow microspheres, 2%-5% of glycerol, 2%-5% of a diluent and the balance of a green silicon carbide grinding material. The resin foaming grinding wheel is prepared by weighing the raw materials according to the weight ratio, stirring, mixing, curing and molding. The polishing solution has the characteristics of high elasticity and good polishing performance; pores are uniform and rich, and cutting force is strong; the grinding wheel is high in toughness and strength, simple and convenient in production process and operation and non-toxic.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of resin grinding wheels, and particularly relates to a modified phenolic resin foamed grinding wheel and a preparation method thereof. Background Art

[0002] Foamed resin grinding wheels are generally used for precision grinding of metals and non-metals with large cutting volumes. The workpieces have high requirements on surface quality, requiring no scratches or burns.

[0003] At present, ordinary phenolic foamed resin grinding wheels or polyvinyl alcohol acetal foamed grinding wheels are brittle, low in strength, low in elasticity, short in service life, easy to clog pores during grinding, and the low-temperature foaming method used is complicated and requires the use of acidic foaming agents, which are toxic and harmful, and cause great corrosion and damage to the mold during the production process. Therefore, it is urgent to use modified phenolic resin and high-temperature foaming methods for improvement.

[0004] Based on this, this application was developed. Summary of the invention

[0005] The purpose of the present invention is to overcome the defects of the prior art and provide a modified phenolic resin foamed grinding wheel, which has the characteristics of being non-toxic and harmless, high elasticity, high strength, uniform pores and convenient production.

[0006] The invention also provides a method for preparing the modified phenolic resin foamed grinding wheel.

[0007] To achieve the above object, the present invention is implemented through the following technical solutions: A modified phenolic resin foamed grinding wheel is made of the following raw materials in percentage by weight: Modified phenolic resin 30%-40%, hexamethylenetetramine 2%-4%, surfactant 2%-6%, glass hollow microspheres 2%-5%, glycerol 2%-5%, diluent 2%-5%, and the balance is green silicon carbide abrasive.

[0008] Specifically, the modified phenolic resin can be a polyurethane modified phenolic resin, etc. The weight percentage of the polyurethane modified phenolic resin is preferably 32% to 38%. The viscosity of the polyurethane modified phenolic resin is 900-1400 pc, preferably 1000-1200 pc. The core and innovation of the present invention lies in the formula of the foamed grinding wheel and its preparation method, and the polyurethane modified phenolic resin can be a common commercial product.

[0009] Furthermore, the surfactant may be Tween 80 surfactant or the like.

[0010] Specifically, the D of the hollow glass microspheres 50 The diameter is 25um-60um, preferably 30~50um.

[0011] Specifically, the diluent includes but is not limited to one or more of acetone, anhydrous ethanol, ethylene dichloride, etc., and anhydrous ethanol is more preferred.

[0012] Specifically, the particle size range of the green silicon carbide abrasive is F220-F800, preferably F320-F600. Further, the weight percentage of the green silicon carbide abrasive is preferably 44%-55%.

[0013] The present invention provides a method for preparing the modified phenolic resin foamed grinding wheel, which comprises the following steps: 1) Weigh the modified phenolic resin, surfactant, glycerin and diluent in proportion, add them into a container, and stir and mix them evenly to obtain system 1; 2) Weigh green silicon carbide abrasive and glass hollow microspheres according to a certain proportion, add them into the system 1 obtained in step 1), and stir and mix them evenly to obtain system 2; 3) Weigh hexamethylenetetramine according to the proportion, add it to the system 2 obtained in step 2) and stir and mix evenly to obtain system 3; 4) Pour the system 3 obtained in step 3) into a mold, and then put it into a curing furnace for foaming and curing.

[0014] Specifically, in step 4), the foaming and curing process can be: foaming at 130-140° C. for 0.5-1 hour, and then curing at 140-165° C. for 4-6 hours.

[0015] The present invention weighs each raw material according to weight percentage, stirs and mixes, and solidifies to obtain a resin foamed grinding wheel. The characteristics of the present invention are high elasticity, good polishing performance, uniform and abundant pores, strong cutting force, high toughness and strength of the grinding wheel, simple production process and operation, and non-toxicity. Compared with the prior art, the present invention has the following beneficial effects: The present invention adopts polyurethane modified phenolic resin, which mainly plays the role of holding abrasives, and forms uniform and abundant bubbles during the curing process; due to its excellent elasticity and toughness, the resin grinding wheel of the present invention has good elasticity and strength, and improves the durability, life and cutting force of the grinding wheel. Glass hollow microspheres can not only increase the porosity of the grinding wheel, but also participate in grinding and increase the cutting force of the grinding wheel; hexamethylenetetramine is used as a foaming agent, which can make the raw materials foam quickly and evenly at high temperature, and also participate in the curing process of the grinding wheel after foaming, so that the foamed grinding wheel has a certain strength. In addition, the preparation method of the present invention using high-temperature foaming of phenolic resin is simple to operate, selects non-toxic and non-corrosive materials, reduces damage to the mold, and greatly reduces production costs. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1The present invention is a flow chart of the preparation process of the modified phenolic resin foamed grinding wheel. DETAILED DESCRIPTION

[0017] The present invention is further described below in conjunction with specific embodiments, but the protection scope of the present invention is not limited thereto.

[0018] In the following examples, the raw materials used are all common commercial products that can be directly purchased or can be prepared according to conventional techniques in the art.

[0019] Example 1 This embodiment provides a method for preparing a modified phenolic resin foamed grinding wheel (process flow as shown in FIG. Figure 1 ), which comprises the following steps: 1) Weigh the raw materials of the grinding wheel: 10.6 kg of green silicon carbide micropowder abrasive F320, 6.4 kg of polyurethane modified phenolic resin with a viscosity of 1150 pc, 0.5 kg of hexamethylenetetramine, 0.5 kg of Tween 80 active agent, 0.5 kg of glass hollow microspheres with a D50 diameter of 45 um, 0.6 kg of glycerol, and 0.6 kg of diluent anhydrous ethanol; 2) Grinding wheel mixing: Add polyurethane modified phenolic resin, Tween 80 active agent, glycerin, and diluent anhydrous ethanol into a container and stir for 15 minutes to mix evenly. After mixing evenly, add green silicon carbide micropowder and hollow glass microspheres and stir for 20 minutes to mix evenly. Then add hexamethylenetetramine and stir for 5 minutes to mix evenly. Finally, pour the above mixture into the mold; 3) Foaming and curing of grinding wheel: Put the mold containing the semi-finished product into the curing oven and foam it at 140℃ for 50 minutes, and cure it at 165℃ for 5 hours.

[0020] Example 2 The present embodiment provides a method for preparing a modified phenolic resin foamed grinding wheel, which comprises the following steps: 1) Weigh the raw materials of the grinding wheel: 9.58kg of green silicon carbide micropowder abrasive F400, 6.8kg of polyurethane modified phenolic resin with a viscosity of 1100pc, 0.6kg of hexamethylenetetramine, 1.0kg of Tween 80 active agent, 0.52kg of hollow glass microspheres with a D50 diameter of 40um, 0.7kg of glycerol, and 0.8kg of anhydrous ethanol; 2) Grinding wheel mixing: Add polyurethane modified phenolic resin, Tween 80 surfactant, glycerin and anhydrous ethanol into a container and stir for 15 minutes. After mixing evenly, add green silicon carbide micropowder and hollow glass microspheres and stir for 30 minutes. Then add hexamethylenetetramine and stir for 7 minutes. Finally, pour the above mixture into the mold. 3) Foaming and curing of grinding wheel: Put the mold containing the semi-finished product into the curing oven for foaming at 138℃ for 50 minutes and curing at 160℃ for 5.5 hours.

[0021] Example 3 The present embodiment provides a method for preparing a modified phenolic resin foamed grinding wheel, which comprises the following steps: 1) Weigh the raw materials of the grinding wheel: 8.96kg of green silicon carbide micropowder abrasive F600, 7.0kg of polyurethane modified phenolic resin with a viscosity of 1050pc, 0.7kg of hexamethylenetetramine, 1.1kg of Tween 80 active agent, 0.54kg of hollow glass microspheres with a D50 diameter of 36um, 0.8kg of glycerol, and 0.9kg of anhydrous ethanol; 2) Grinding wheel mixing: Add polyurethane modified phenolic resin, Tween 80 surfactant, glycerin and anhydrous ethanol into a container and stir for 15 minutes. After mixing evenly, add green silicon carbide micropowder and hollow glass microspheres and stir for 35 minutes. Then add hexamethylenetetramine and stir for 9 minutes. Finally, pour the above mixture into the mold. 3) Foaming and curing of grinding wheels: Place the mold containing the semi-finished product into a curing oven and foam it at 135°C for 45 minutes, and then cure it at 155°C for 6 hours.

[0022] Comparative Example 1 This comparative example provides a method for preparing a foamed grinding wheel, which comprises the following steps: 1) Weigh the raw materials of the grinding wheel: 10.6 kg of green silicon carbide micropowder abrasive F320, 6.4 kg of epoxy modified phenolic resin with a viscosity of 1150 pc, 0.5 kg of hexamethylenetetramine, 0.5 kg of Tween 80 active agent, 0.5 kg of hollow glass microspheres with a D50 diameter of 45 um, 0.6 kg of glycerol, and 0.6 kg of anhydrous ethanol; 2) Grinding wheel mixing: Add epoxy modified phenolic resin, Tween 80 surfactant, glycerin and anhydrous ethanol into a container and stir for 15 minutes. After mixing evenly, add green silicon carbide micropowder and hollow glass microspheres and stir for 20 minutes. Then add hexamethylenetetramine and stir for 5 minutes. Finally, pour the above mixture into the mold. 3) Foaming and curing of grinding wheel: Put the mold containing the semi-finished product into the curing oven and foam it at 140℃ for 50 minutes, and cure it at 165℃ for 5 hours.

[0023] Comparative Example 2 This comparative example provides a method for preparing a foamed grinding wheel, which comprises the following steps: 1) Weigh the raw materials of the grinding wheel: 10.6 kg of green silicon carbide micropowder abrasive F320, 6.4 kg of epoxy modified phenolic resin with a viscosity of 1150 pc, 0.5 kg of hexamethylenetetramine, 0.5 kg of Tween 80 active agent, 0.5 kg of hollow glass microspheres with a D50 diameter of 65 um, 0.6 kg of glycerol, and 0.6 kg of anhydrous ethanol; 2) Grinding wheel mixing: Add epoxy modified phenolic resin, Tween 80 surfactant, glycerin and anhydrous ethanol into a container and stir for 15 minutes. After mixing evenly, add green silicon carbide micropowder and hollow glass microspheres and stir for 20 minutes. Then add hexamethylenetetramine and stir for 5 minutes. Finally, pour the above mixture into the mold. 3) Foaming and curing of grinding wheel: Put the mold containing the semi-finished product into the curing oven and foam it at 140℃ for 50 minutes, and cure it at 165℃ for 5 hours.

[0024] Grinding test The titanium alloy workpiece was polished using the grinding wheels prepared in the above embodiments and comparative examples. A titanium alloy round tube was used as the grinding object with a specification of 30×60 mm. The roughness after grinding was required to be ≤0.06 um, and the surface was required to be free of spiral marks and scratches. The surface roughness of the polished workpiece was tested, and the grinding performance comparison results are shown in Table 1.

[0025] Table 1 Comparison of grinding performance of grinding wheel products in different embodiments It can be seen from Table 1 that the surface roughness of the workpiece after polishing is less than 0.06 μm for the grinding wheel prepared by the embodiment of the present invention, the service life is more than 4000 pieces, and there are no scratches and spiral lines on the surface of the workpiece after polishing. However, the grinding wheel prepared by epoxy modified phenolic resin in Comparative Example 1 has a rough surface and scratches on the workpiece after polishing, and spiral lines appear when the diameter of the hollow glass microsphere D50 is greater than 60 μm. This shows that the use of polyurethane modified phenolic resin to prepare grinding wheels can greatly improve the processing quality of workpieces.

[0026] The above is a detailed description of the embodiment process, but it does not limit the technical solution of the present invention. Ordinary technicians in this field should understand that any modifications, partial replacements and variations can be made to the above-mentioned embodiments within the scope of the present invention, which should all be included in the required scope of the present invention.

Claims

1. A modified phenolic resin foamed grinding wheel, characterized in that: Made from the following raw materials in weight percentage: Modified phenolic resin 30%-40%, hexamethylenetetramine 2%-4%, surfactant 2%-6%, glass hollow microspheres 2%-5%, glycerol 2%-5%, diluent 2%-5%, and the balance is green silicon carbide abrasive.

2. The modified phenolic resin foamed grinding wheel according to claim 1, characterized in that: The modified phenolic resin is polyurethane modified phenolic resin.

3. The modified phenolic resin foamed grinding wheel according to claim 2, characterized in that: The viscosity of the polyurethane modified phenolic resin is 900-1400 pc.

4. The modified phenolic resin foamed grinding wheel according to claim 1, characterized in that: The surfactant is Tween 80.

5. The modified phenolic resin foamed grinding wheel according to claim 1, characterized in that: The D of the hollow glass microspheres 50 The diameter is 25um-60um.

6. The modified phenolic resin foamed grinding wheel according to claim 1, characterized in that: The diluent is one or more of acetone, anhydrous ethanol and ethylene dichloride.

7. The modified phenolic resin foamed grinding wheel according to claim 1, characterized in that: The particle size range of the green silicon carbide abrasive is F220-F800.

8. The method for preparing the modified phenolic resin foamed grinding wheel according to any one of claims 1 to 7, characterized in that: The following steps are involved: 1) Weigh the modified phenolic resin, surfactant, glycerin and diluent in proportion and mix them evenly to obtain system 1; 2) weighing green silicon carbide abrasive and glass hollow microspheres according to a certain proportion, adding them to the system 1 obtained in step 1), and mixing them evenly to obtain system 2; 3) Weigh hexamethylenetetramine according to the proportion, add it to the system 2 obtained in step 2), and mix them evenly to obtain system 3; 4) Pour the system 3 obtained in step 3) into a mold, and then put it into a curing furnace for foaming and curing.

9. The method for preparing a modified phenolic resin foamed grinding wheel according to claim 8, characterized in that: In step 4), the foaming and curing process is: foaming at 130-140°C for 0.5-1 hour, and then curing at 140-165°C for 4-6 hours.

Citation Information

Patent Citations

  • Phenolic resin composition and foaming material and moulding material prepared therefrom

    CN105482243A

  • Method for preparing foaming resin sanding wheel

    CN107775547A

  • Modified resin grinding wheel and manufacturing method thereof

    CN107953275A

  • Phenolic foam material for polishing as well as preparation method and application thereof

    CN109401183A

  • High-porosity resin grinding wheel and preparation method thereof

    CN110524439A