Forming method of automobile injection molding part mold, forming method of automobile injection molding part and luminous automobile injection molding part

By reserving suture marks on the automotive injection molding part mold and combining the injection molding process of hard glue and soft glue materials, the existing automotive cover part molding problems are solved, and the direct injection molding of suture parts is achieved. and enhancement of design freedom.

CN118876296APending Publication Date: 2024-11-01DONGFENG MOTOR GRP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411006067.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-25
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

The forming production process of existing automotive cladding parts is long and costly, and the design freedom is limited. In particular, the production of suture cladding parts has complex processes and high costs.

Method used

The molding method of automobile injection molding parts is adopted. By reserving the suture mark processing allowance in the initial mold and using laser engraving and other technologies to form the suture mark mold. Combining the injection molding process of hard glue and soft glue materials, the suture mark is directly formed. Injection molded parts simplify the process and increase the design freedom.

Benefits of technology

Direct injection molding of suture parts is achieved, reducing production process and costs, while improving the design freedom and ornamentality of the cladding parts.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118876296A_ABST
    Figure CN118876296A_ABST
Patent Text Reader

Abstract

The invention relates to a forming method of an automobile injection molding part mold, a forming method of an automobile injection molding part and a light-emitting automobile injection molding part, and the forming method comprises the following steps that an initial mold needed by the automobile injection molding part is manufactured, and the initial mold reserves sewing line machining allowance; sewing lines are machined on the sewing line machining allowance reserved by the initial mold; and textures of the decoration area are machined in the mold where the sewing line textures are machined, and the injection mold is formed. By manufacturing the injection mold with the suture lines, the part with the suture lines in the vehicle can be directly formed through injection molding of the injection mold, and the technical problems that in the related technology, the forming production process of the covering part with the suture lines is long, the cost is relatively high, and the design freedom degree of the covering part is limited to a certain degree are solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of automobile parts, and in particular to a molding method of an automobile injection molding mold, a molding method of an automobile injection molding part, and a luminous automobile injection molding part. Background Art

[0002] At present, in order to improve the decorative effect of the interior of the car, soft materials such as fabric, artificial leather, and genuine leather are generally used to cover the surface of the plastic frame. In the related technology, the soft material is usually bonded to the surface of the plastic frame to form a covering, which can achieve a good surface tactile effect. Furthermore, before the soft material is covered and bonded to the frame, sewing threads of different colors or shapes can be sewn on the surface of the soft material, and the soft material can be cut and then spliced, folded, and then sewn to further improve the layering of the surface of the covering.

[0003] However, the cover with seams formed by the above method needs to go through the processes of frame injection molding, soft material cutting and sewing, glue spraying, heating, and coating, which has a long production process and leads to a relatively high cost of the cover. At the same time, because the soft material needs to fit the plastic frame completely, there are certain requirements for the flange height, minimum fillet, and concave surface of the cover, which greatly limits the design freedom of the cover. Summary of the invention

[0004] The present application provides a molding method for an automobile injection molding mold, a molding method for an automobile injection molding part, and a luminous automobile injection molding part, which can solve the technical problems in the related art that the molding production process of the suture covering part is long, the manufacturing cost is relatively high, and the design freedom of the covering part is limited to a certain extent.

[0005] In a first aspect, an embodiment of the present application provides a molding method for an automobile injection molding mold, which comprises the following steps: manufacturing an initial mold required for an automobile injection molding part, wherein the initial mold has a reserved seam pattern processing allowance; processing the seam pattern on the seam pattern processing allowance reserved in the initial mold; processing the texture of the decorative area in the mold after the seam pattern is processed, to form an injection mold.

[0006] In combination with the first aspect, in one embodiment, before processing the seam lines on the initial mold, it includes: rendering the seam lines on a car injection molded part product drawing marked with the seam line center lines according to the seam line pattern diagram; and designing the injection mold drawing according to the car injection molded part product drawing.

[0007] In combination with the first aspect, in one embodiment, the minimum demolding angle required for the processing of the seam pattern in the seam pattern diagram is α1; and the demolding angle of the injection molded part in the seam pattern area rendered in the automotive injection molded part product diagram is α2; wherein α2 is not less than α1.

[0008] In combination with the first aspect, in one embodiment, processing the seam pattern on the initial mold includes: using a laser to engrave the eyelet area of ​​the seam pattern and an area with the same depth as the eyelet area; and continuing to use the laser engraving to reach the final depth of the seam pattern.

[0009] In combination with the first aspect, in one embodiment, before processing the seam lines on the initial mold, it includes: separately processing the cavity and the core of the initial mold; polishing the side of the cavity with the seam line processing allowance reserved to a state with texture processing conditions for the seam lines and the decorative area.

[0010] In combination with the first aspect, in one embodiment, the texture of the decorative area is processed in the mold with processed seam lines to form an injection mold, including: coating the area of ​​the injection mold with processed seam lines with anti-corrosion glue; and using chemical corrosion to form the texture of the decorative area in the area not coated with the anti-corrosion glue.

[0011] In combination with the first aspect, in one embodiment, before processing the seam pattern on the initial mold, it includes: using a laser engraving device to perform a trial engraving of the seam pattern on a steel material of the same material as the initial mold; obtaining parameter data such as the output power of different areas in the seam pattern structure, the engraving depth at one time, and the total number of engraving times for each equal depth point through the trial engraving.

[0012] In a second aspect, an embodiment of the present application provides a molding method for an automotive injection molded part, which comprises the following steps: forming the automotive injection molded part by injection molding using an injection mold, wherein the injection mold is formed by the molding method for the automotive injection molded part mold as described above.

[0013] In combination with the second aspect, in one embodiment, the injection mold includes a core and a first cavity and a second cavity respectively matched with the core, and the use of the injection mold to form an automotive injection molded part by injection molding includes: matching the core with the first cavity, and injecting hard rubber material into the core and the first cavity to form an initial injection molded part with seam lines; placing the initial injection molded part between the core and the second cavity; injecting soft rubber material into the cavity of the core and the second cavity accommodating the initial injection molded part to form an automotive injection molded part with a soft rubber layer, wherein the soft rubber layer is located outside the seam lines.

[0014] In a third aspect, an embodiment of the present application provides a luminous automobile injection molded part, characterized in that it comprises: an automobile injection molded part, the automobile injection molded part is formed by the above-mentioned automobile injection molded part molding method, and the hard plastic material is a light-transmitting material;

[0015] A light-emitting component is fixed on a side of the soft adhesive layer corresponding to the stitching pattern.

[0016] The beneficial effects brought by the technical solution provided by the embodiments of the present application include:

[0017] By manufacturing an injection mold with seam patterns, parts with seams in the vehicle can be directly formed by injection molding through the injection mold, solving the technical problems in the related technology that the molding production process of seam-covered parts is long, the cost is relatively high, and the design freedom of the covering parts is limited to a certain extent. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0019] Figure 1 A schematic diagram of a process for forming a mold for an automobile injection mold provided in an embodiment of the present application;

[0020] Figure 2 A schematic diagram of the main structure of an automotive injection molded part provided in an embodiment of the present application;

[0021] Figure 3 A schematic diagram of the positions of the seam lines and fold lines in the automotive injection molded product diagram provided in the embodiment of the present application;

[0022] Figure 4 A schematic diagram of the position of the center line of the seam pattern in the automotive injection molded product diagram provided in the embodiment of the present application;

[0023] Figure 5 A schematic diagram of the structure of the reserved seam pattern processing allowance in the cavity provided in an embodiment of the present application.

[0024] In the figure:

[0025] 1. Automobile injection molding parts; 11. Soft rubber layer;

[0026] 2. Product image of automobile injection molding; 21. Center line of seam pattern;

[0027] 3. Cavity; 31. Processing allowance for seam pattern; 32. Processing allowance for fold pattern;

[0028] 4. Stitching pattern diagram. DETAILED DESCRIPTION

[0029] In order to enable those skilled in the art to better understand the solution of the present application, the technical solution in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.

[0030] The embodiment of the present application provides a molding method for an automobile injection molding mold, which can solve the technical problems in the related art that the molding production process of the covering parts with seam patterns is long, the manufacturing cost is relatively high, and the design freedom of the covering parts is limited to a certain extent.

[0031] See also Figure 1 As shown, a molding method of an automobile injection mold provided by an embodiment of the present application may include the following steps:

[0032] S1: An initial mold required for manufacturing an automobile injection molded part 1, wherein the initial mold reserves a seam processing allowance 31, and the seam processing allowance 31 can have a wider width along a direction perpendicular to the extension direction of the seam, so as to facilitate the subsequent processing of seams of different sizes on the seam processing allowance 31. The size of the seam refers not only to its width along a direction perpendicular to the extension direction of the seam, but also to the line diameter and stitch length of the seam.

[0033] S2: Processing the seam pattern on the seam pattern processing allowance 31 reserved in the initial mold, that is, processing the seam pattern on the seam pattern processing allowance 31 of the initial mold. The seam pattern can be processed by laser engraving or chemical corrosion. In order to achieve a better simulation effect, laser engraving is preferably used.

[0034] S3: Processing the texture of the decorative area in the mold after processing the seam lines to form an injection mold. In the embodiment of the present application, in addition to processing the seam lines, textures can also be processed in the decorative area outside the seam lines, so that the produced automobile injection molding part 1 can have imitation cloth texture, imitation leather texture or other imitation texture styles, making the injection molded automobile injection molding part 1 more ornamental. In addition, processing the texture in the decorative area outside the seam lines can also include processing to form folding lines.

[0035] The embodiment of the present application manufactures an injection mold with seam lines, so that parts with seams in the vehicle can be directly formed by injection molding the injection mold. The injection mold can have seam lines and other decorative textures. By setting the texture, imitation cloth texture, imitation leather texture or other profiling texture styles can be injection molded, thereby enhancing the ornamental value of the automobile injection molded part 1. In addition, the automobile injection molded part 1 with seam lines formed by injection molding can reduce the processing flow, save production time, and the cost can be relatively low compared to the covering parts with seams.

[0036] In some optional embodiments, before processing the stitching pattern on the initial mold, the following steps may be included: Figure 4 Automobile injection molded products with seam center line 21 on the logo Figure 2 Rendering stitching on the top, that is, on automotive injection molded parts Figure 2 Before rendering the stitching pattern, you can first design the stitching pattern you want to use. The stitching pattern in the template is considered the stitching pattern. Figure 4 , the stitching pattern Figure 4 After confirmation, the stitching pattern Figure 4 Rendering on automotive injection molding products Figure 2 Above, see Figure 4 As shown, automotive injection molding products Figure 2 Rendering stitch patterns Figure 4 The stitch pattern center line 21 may be marked beforehand, and the stitch pattern may be determined according to the stitch pattern center line 21 during rendering. Figure 4 Injection molding products for automobiles Figure 2 In some other embodiments, the stitch pattern Figure 4 Rendering to automotive injection molded products Figure 2 When it is installed, it can also be done by pre-injection molding of automotive parts. Figure 2 Other marks made on the surface to determine its position; according to the automotive injection molding products Figure 2 Design the mold drawing for injection molding, and understand that the injection mold can be manufactured according to the mold drawing for injection molding. Figure 3 As shown, in the embodiment of the present application, in order to enhance the ornamental effect of the stitching lines on the automobile injection molded part 1, folding lines are further provided on one side of the stitching lines, and the correlation between the stitching lines and the folding lines is enhanced so that the appearance effect after the folding lines and the stitching lines are matched can be as harmonious as possible.

[0037] Preferably, the stitching pattern Figure 4After rendering to the injection molded product drawing and defining and marking the fold lines according to the position of the seam lines, you can analyze whether the settings of the seam lines and fold lines are appropriate. If there is any inconsistency, you can make corresponding adjustments. The seam lines can be processed on the seam line processing allowance 31 reserved in the initial mold, and the fold lines can also be processed on the processing allowance reserved in the initial mold. The fold line processing position can also be separately reserved with a fold line processing allowance 32, that is, the initial mold synchronously reserves a fold line processing allowance 32 and a seam line processing allowance 31, and the processing allowances of the seam lines and fold lines can be directly and synchronously formed during the mold milling process. Since the actual positions of the seam lines and fold lines may be adjusted after rendering to the injection molded product drawing, refer to Figure 5 As shown, the stitching line machining allowance 31 and the folding line machining allowance 32 can both be set to a wider width, so that the folding lines and the stitching line can still be engraved on the folding line machining allowance 32 and the stitching line machining allowance 31 after adjustment.

[0038] In some optional embodiments, the seam processing allowance 31 and the folding processing allowance 32 can be reserved in the form of a boss, wherein the boss can have a certain height along the extension direction perpendicular to the seam, and the height H1 of the boss can be set to be greater than the maximum depth H2 of the seam and fold on the automotive injection molded part 1. In the embodiment of the present application, the height of the boss is preferably 1.5mm-2.0mm. The width of the boss can be based on the style of the seam, preferably 5-8mm for a single seam, and 10-15mm for a double seam. In some other embodiments, in addition to the seam, folds are further provided, and the folding processing allowance 32 and the seam processing allowance 31 can be reserved on a boss. At this time, if a single seam is provided, the width of the boss should be greater than 15mm, and if a double seam is provided, the width of the boss should be greater than 30mm. It should be understood that two adjacent eyelet patterns and a single stitch pattern between them can be regarded as a stitch pattern unit, and the overall stitch pattern is composed of several continuous stitch pattern units. The style of the stitch pattern unit can be designed according to the wire diameter and stitch length of the single stitch pattern, the length of the eyelet pattern, the number of strands on the single stitch pattern, the depth, direction, sinking amount, whether there are folding patterns on the outside of the stitch pattern, the width, height, gradient form of the folding pattern, and the texture style of the decorative area outside the stitch pattern. In the embodiment of the present application, combined with the conventional size of the suture, the width of a single stitch pattern is preferably 0.6-1mm, and the length is preferably 4.5-5.5mm; the length of the eyelet pattern is preferably 1mm-1.5mm; the number of strands on a single stitch pattern is preferably 6-8, and its value is proportional to the length of the single stitch pattern, and is evenly and obliquely arranged on each stitch pattern; the stitch pattern can be single or double, and the height from the stitch pattern to the highest point of the fold pattern should vary evenly; the main texture of the area outside the stitch pattern is preferably imitation cloth or imitation leather.

[0039] In some optional embodiments, the stitching pattern Figure 4 The minimum demoulding angle required for the processing and molding of the center seam pattern is α1, and the demoulding angle of the injection molded part in the seam pattern area rendered in the automotive injection molded part product diagram is α2, that is, the demoulding angle of the seam pattern area on the injection molded part is α2, and the setting value of α2 should be based on the required value of α1; wherein, α2 is not less than α1, and the injection molded part meets the demoulding angle requirements to ensure that the texture of the injection molded part will not be destroyed due to insufficient angle when demoulding after injection cooling. Therefore, the automotive injection molded part 1 should reserve a demoulding angle when using the injection mold to mold it, so that the automotive injection molded part 1 can be easily and intactly removed from the injection mold. In the embodiment of the present application, the depth of the seam pattern in the injection mold is deeper than that in other positions, so the demoulding angle α1 required for the processing and molding of the seam pattern can be regarded as the lower limit of the reserved demoulding angle α2 of the injection molded part; in the embodiment of the present application, the minimum demoulding angle α1 does not mean that the demoulding angle α2 needs to be not less than α1 for demoulding, but that the demoulding angle is not less than α1, so that the seam pattern can maintain its appearance intact after demoulding. Therefore, in the embodiment of the present application, the seam pattern area α2 ≥ α1 on the main viewing surface of the automobile injection molded part 1, and the seam pattern area α2 ≥ α1 on the non-main viewing surface of the automobile injection molded part 1 Line area α2 ≥ 75% α1, the main view surface is regarded as the position that the driver can directly observe when the automobile injection molding part 1 is installed in the vehicle, that is, the position that the co-pilot and the main driver can directly observe when riding is regarded as the main view surface, and the position that the co-pilot and the main driver need to change the angle to see when riding is regarded as the non-main view surface. In the embodiment of the present application, although the main view surface and the non-main view surface are set with different demoulding angles, the final effects presented by the main view surface and the non-main view surface can be basically consistent. Usually, the appearance requirements of the main view surface are set higher, so the demoulding of the main view surface is set higher. The angle is set to α2≥α1 to make the seam lines present a better effect. On the non-main viewing surface, the processing depth of the seam lines can be appropriately weakened based on the design requirements of the injection molded part profile. The minimum demolding angle of the seam lines with weakened depth is also reduced synchronously. Therefore, the demolding angle of the seam line area of ​​the injection molded part on the non-main viewing surface is set to α2≥75%α1 to make the automotive injection molded part 1 easier to demold. It should be understood that the 75% here is based on the premise of being easier to demold the automotive injection molded part 1 after multiple verifications, and it is also a value that can make the decorative effects of all appearance areas of the automotive injection molded part 1 have no obvious differences.

[0040] In some optional embodiments, the processing of the stitch lines on the initial mold includes: using laser to engrave the stitch line pinhole area and the area with the same depth as the area. In the embodiment of the present application, considering the design requirements of the automobile injection molded part 1, the mold material and the production process, etc., the stitch lines are formed by laser engraving. In some other embodiments, the stitch lines can also be formed by other feasible methods. It should be understood that among the stitch lines on the automobile injection molded part 1, the depth of the pinhole position should be the deepest. According to the opposite of the mold and the part concave and convex, the depth of the stitch lines should be the deepest. According to the principle, in the injection mold, the engraving depth at the eye of the seam pattern should be the shallower or even the shallowest area in the seam pattern. Therefore, in the embodiment of the present application, the seam pattern is processed by engraving from shallow to deep step by step. After the shallower part of the seam pattern in the injection mold is processed, laser engraving is continued to reach the final depth of the seam pattern, that is, the most prominent position of the seam pattern on the automobile injection molded part 1. When the seam pattern in the injection mold is engraved from shallow to deep, the thread strand pattern on the seam pattern will gradually form to achieve the final seam pattern display effect. It should be noted that when engraving from shallow to deep in the injection mold, the deeper the engraving position, the more engraving times are required. Therefore, after the seam pattern is engraved, when the folding pattern is engraved, the engraving times of each area of ​​the folding pattern will also increase gradually from shallow to deep.

[0041] In some optional embodiments, before processing the seam lines on the initial mold, the process may include: processing the cavity 3 and the core of the initial mold separately, that is, in the embodiment of the present application, polishing the side of the cavity 3 with the seam line processing allowance 31 to a state that meets the seam line processing conditions, dividing the initial mold into the core and the cavity 3 for manufacturing, and the seam lines in the injection mold are finally formed in the cavity 3. The cavity 3 can be formed by milling, punching and other equipment, and the surface of the cavity 3 can be polished with oilstone, sandpaper and other materials, preferably, the polishing degree can reach 600-800 mesh.

[0042] In some optional embodiments, the texture of the decorative area is processed in the mold after the stitching is processed to form the injection mold, which may include: coating the area of ​​the injection mold after the stitching is processed with anti-corrosion glue; using the method of chemical corrosion to form the texture of the decorative area in the area not coated with anti-corrosion glue. In the embodiment of the present application, after the stitching and folding are processed in the injection mold, when the texture of the decorative area is subsequently processed, in order to not affect the texture of the stitching during the processing, the stitching is coated with anti-corrosion glue for protection, and the folding may not be coated with anti-corrosion glue, so that the folding can also have the above-mentioned texture effect. In addition, in some other embodiments, in addition to using the method of chemical corrosion, laser engraving and other methods can be used to form the texture of the automobile injection molded part 1, which can eventually form the texture of imitation leather or imitation cloth on the automobile injection molded part 1 to enhance the ornamental and texture of the automobile injection molded part 1. After the above-mentioned texture is processed, the surface of the injection mold is sandblasted for gloss treatment to achieve the coordination and unity of the gloss of the stitching and the surrounding main texture.

[0043] In some optional embodiments, before processing the seam pattern on the initial mold, it includes: using laser engraving equipment to perform trial engraving of the seam pattern on the steel of the same material as the initial mold; obtaining parameter data such as the output power of different areas in the seam pattern structure, the engraving depth at one time, and the total number of engraving times at each equal depth point through trial engraving. In addition to the parameters of the number of engraving layers, the depth of one engraving can also be obtained. During the trial engraving, several seam pattern units can be engraved. The seam pattern unit should include two adjacent eye patterns and a single seam pattern between them. If folding patterns are set on the outside of the seam pattern, when trial engraving the seam pattern, folding patterns of the same length are trial engraved simultaneously. The purpose of trial engraving is to guide the formal engraving based on the parameters such as the output power of different areas obtained during the trial engraving, the engraving depth at one time, and the total number of engraving times at each equal depth point. In the embodiment of the present application, after the trial engraving, the power of the laser is set at about 20W, and the depth of one engraving is set to 1.5-2.0μm. If the engraving is too deep at one time, steps may appear, affecting the smoothing effect of the seam lines and fold lines; however, if the engraving is too shallow at one time, it will affect the processing time of the mold. Therefore, the 1.5-2.0μm set in the embodiment of the present application can improve the engraving efficiency as much as possible and meet the engraving effect.

[0044] The present application also provides a method for forming an automobile injection molded part, which may include the following steps: using an injection mold to form an automobile injection molded part 1 by injection molding, wherein the injection mold is formed by the molding method of the automobile injection molded part described in any of the above embodiments, and the automobile injection molded part 1 formed by the above molding method of the automobile injection molded part may have seam lines and fold lines, and may also have a texture imitating cloth lines or leather lines, so that the automobile injection molded part 1 has a better decorative effect and touch. Using the injection mold in the above embodiment to perform injection molding of the automobile injection molded part 1, since the manufacturing process is shortened, the automobile injection molded part 1 can be quickly injection molded, and the seam lines on the automobile injection molded part 1 can have a greater degree of design freedom, so that the automobile injection molded part 1 has a better visual effect.

[0045] In some optional embodiments, the injection mold includes a core and a first cavity and a second cavity respectively matched with the core, and the injection mold is used to form an automotive injection molded part 1 by injection molding, including: matching the core and the first cavity, and injecting hard glue material into the core and the first cavity to form an injection molded initial part with seam lines, that is, forming an injection molded skeleton with seam lines; placing the injection molded initial part between the core and the second cavity, the thickness of the injection molded initial part can be determined according to the design value, and the setting in the embodiment of the present application is 2.0mm-2.5mm, and the second cavity should be filled with the seam lines of the injection molded initial part at the non-pinhole lines of the seam lines, so that when the soft glue material is injected later, even if the injection molded initial part is placed in the mold Between the core and the second cavity, the core and the second cavity still have cavities in the pinhole pattern and decorative area; soft glue material is injected into the cavity of the core and the second cavity containing the initial injection molded part to form an automobile injection molded part 1 with a soft glue layer 11, wherein the soft glue layer 11 is located at the periphery of the stitch pattern, that is, it can be located in the decorative area and the pinhole pattern area. Since the stitch pattern of the second cavity is filled with the non-pinhole pattern of the initial injection molded part, that is, the first cavity and the second cavity are in contact with each other in the stitch pattern area except the pinhole, when the soft glue material is subsequently injected into the cavity of the core and the second cavity, the soft glue material will not enter the non-pinhole pattern area of ​​the stitch pattern of the second cavity, that is, the soft glue layer 11 will be located in the decorative area and the pinhole pattern area, see Figure 2As shown, the automobile injection molded part 1 formed at this time has both a hard skeleton and a soft rubber layer 11, which can make the outer surface of the automobile injection molded part 1 have a soft touch. In this application, the thickness of the soft rubber layer 11 can be set to 0.8-1.2mm, and the thickness of the initial injection molded part and the thickness of the soft rubber layer 11 can be designed according to actual needs. The decorative area and the pinhole pattern area of ​​the initial injection molded part are covered by injecting soft rubber material on the outside of the initial injection molded part, so that the automobile injection molded part 1 can have the smooth touch of the soft material surface while forming the seam pattern on the surface of the automobile injection molded part 1. Preferably, the first cavity may not have the texture of the decorative area, and the texture of the decorative area can be set only in the second cavity to save the manufacturing time of the injection mold as a whole. In some other embodiments, the injection mold may also include only a core and a second cavity. The automobile injection molded part 1 can be formed by injecting a hard rubber material once during injection molding. This method can save the manufacturing cost of the automobile injection molded part 1, and it can be formed by one injection, which can make the molding of the automobile injection molded part 1 faster.

[0046] The embodiment of the present application also provides a luminous automobile injection molded part, which may include: an automobile injection molded part 1, the automobile injection molded part 1 is formed by the molding method of the automobile injection molded part as described in the above embodiment, and the hard plastic material is a light-transmitting material. Preferably, the hard plastic can be selected from dyed and light-transmitting ABS and PC / ABS materials, wherein the ABS and PC / ABS materials can be selected from high light-transmitting or high light-transmitting and light-diffusing materials; a light-emitting component, the light-emitting component is fixed to the side away from the soft plastic layer 11 corresponding to the seam pattern, and the soft plastic layer 11 can be selected from non-light-transmitting materials, that is, in the embodiment of the present application, since the hard plastic uses a high light-transmitting material, and the soft plastic layer 11 is located in the decorative area of ​​the outer periphery of the seam pattern and the pinhole pattern area of ​​the seam pattern, therefore, at the seam pattern, the light-emitting component is fixed on the side away from the soft plastic layer 11 to make the non-pinhole pattern of the seam pattern transparent, the high light-transmitting material can make the transmitted light more brilliant, and the high light-transmitting and light-diffusing material can make the transmitted light softer. And when the colors of the hard plastic and the soft plastic are different, the effect of the seam pattern can also be highlighted. In the embodiment of the present application, an automobile injection molded part 1 with a light-transmitting effect is designed, wherein the hard rubber material and the light-emitting component are designed in coordination to meet the light-emitting effect, and the difference in color between the hard rubber material and the soft rubber material can highlight the display requirements of the seam lines. Since the soft rubber layer 11 is made of a light-proof soft rubber material, the installation position of the light-emitting component does not need to be very precise, and the automobile injection molded part 1 can also be light-proof except for the seam lines. This setting method can speed up the installation efficiency. In addition, the injection molded part used in the embodiment of the present application is co-molded with a soft rubber material and a hard rubber material, which can make the non-pinhole pattern area of ​​the seam lines have a light-transmitting effect while avoiding the phenomenon that the light-transmitting ability of the light-transmitting seams of the covering part gradually decays over time.

[0047] In the description of the present application, it should be noted that the terms "upper", "lower", etc. indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present application. Unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be an indirect connection through an intermediate medium, or it can be a connection between the two elements. For those of ordinary skill in the art, the specific meanings of the above terms in the present application can be understood according to the specific circumstances.

[0048] It should be noted that, in this application, relational terms such as "first" and "second" are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the sentence "comprise a ..." do not exclude the presence of other identical elements in the process, method, article or device including the elements.

[0049] The above description is only a specific implementation of the present application, so that those skilled in the art can understand or implement the present application. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein can be implemented in other embodiments without departing from the spirit or scope of the present application. Therefore, the present application will not be limited to the embodiments shown herein, but will conform to the widest range consistent with the principles and novel features applied for herein.

Claims

1. A molding method for an automobile injection mold, characterized in that: It includes the following steps: An initial mold required for manufacturing an automobile injection molded part (1), wherein the initial mold has a seam pattern processing allowance (31) reserved; Processing the seam pattern on the seam pattern processing allowance (31) reserved in the initial mold; The texture of the decorative area is processed in the mold after the stitching pattern is processed to form an injection mold.

2. The molding method of automobile injection mold according to claim 1, characterized in that: Before processing the seam lines on the initial mold, the method includes: According to the stitch pattern diagram (4), stitch patterns are rendered on an automobile injection molded product diagram (2) marked with a stitch pattern center line (21); and according to the automobile injection molded product diagram (2), an injection molded product diagram is designed.

3. The molding method of the automotive injection mold according to claim 2, characterized in that: The minimum demoulding angle required for the processing of the seam pattern in the seam pattern diagram (4) is α1, and the demoulding angle of the injection molded part in the seam pattern area rendered in the automotive injection molded part product diagram is α2; Among them, α2 is not less than α1.

4. The molding method of automobile injection mold according to claim 1, characterized in that: The processing of seam lines on the initial mold comprises: Use laser to engrave the eyelet area of ​​the stitching and the area with the same depth; Continue laser engraving to reach the final depth of the seam pattern.

5. The molding method of automobile injection mold according to claim 4, characterized in that: Before processing the seam lines on the initial mold, the method includes: Processing the cavity (3) and the core of the initial mold respectively; The side of the mold cavity (3) where the seam pattern processing allowance (31) is reserved is polished to a state where the seam pattern and the texture processing conditions of the decorative area are met.

6. The molding method of automobile injection mold according to claim 1, characterized in that: The method of processing the texture of the decorative area in the mold after processing the stitching pattern to form the injection mold comprises: Apply anti-corrosion glue to the area where the seam lines are processed in the injection mold; The texture of the decorative area is formed in the area not coated with anti-corrosion glue by using chemical corrosion.

7. The molding method of automobile injection mold according to claim 1, characterized in that: Before processing the seam lines on the initial mold, the method includes: Use laser engraving equipment to test engrave the seam pattern on the same steel material as the initial mold; The parameter data of output power in different areas of the seam pattern, engraving depth at one time and total engraving times at each point with the same depth were obtained through trial engraving.

8. A method for molding automobile injection molded parts, characterized in that: It includes the following steps: An automobile injection molded part (1) is formed by injection molding using an injection mold, wherein the injection mold is formed by a molding method for an automobile injection molded part mold according to any one of claims 1 to 7.

9. The method for molding an automobile injection molded part according to claim 8, characterized in that: The injection mold comprises a core and a first cavity and a second cavity respectively matched with the core. The automobile injection molded part (1) is formed by injection molding using the injection mold, comprising: Matching the core with the first cavity, and injecting hard plastic material into the core and the first cavity to form an injection-molded initial part with seam lines; placing the injection molded initial part between the core and the second cavity; A soft rubber material is injected into the core containing the initial injection molded part and the cavity of the second cavity to form an automobile injection molded part (1) having a soft rubber layer (11), wherein the soft rubber layer (11) is located at the periphery of the seam pattern.

10. A luminous automobile injection molded part, characterized in that: It includes: Automobile Injection molded part (1), the automobile injection molded part (1) is formed by the molding method of automobile injection molded part as described in claim 9, and the hard plastic material is a light-transmitting material; A light-emitting component is fixed to a side of the soft rubber layer (11) corresponding to the stitching pattern.