Production method of three-layer co-extrusion polypropylene sheet suitable for electroplating

Through the three-layer coextruded polypropylene sheet production method, the anchor hole is formed by etching by water treatment, which solves the problem of insufficient surface roughness and hydrophilicity of PP plastic electroplating, and achieves superior metal adhesion and environmentally friendly electroplating effect. Reduce costs and weight and meet environmental protection requirements.

CN118876384APending Publication Date: 2024-11-01NINGBO SUZHIHUA PLASTIC & CHEM CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410907859.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-08
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

PP plastic electroplating has problems such as too smooth surface, fewer functional groups on the surface, and low metal adhesion, which affects the plating quality, and the existing chemical roughening liquid causes harm to the environment.

Method used

The production method of three-layer coextruded polypropylene sheets is adopted to form microscopic irregular anchor holes through water treatment and etching, which improves the surface roughness and hydrophilicity of the polypropylene sheets, and uses polyether block polyamide and polyvinylpyrrolidone. Water-soluble macromolecules such as polyethylene glycol dissolve in water to form anchor holes to enhance metal adhesion.

Benefits of technology

It achieves superior metal adhesion, improves electroplating quality, and uses water treatment to avoid environmental pollution. The coating bonding force is consistent with ABS, reducing material cost and weight, while meeting environmental protection requirements.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
  • Figure SMS_3
    Figure SMS_3
Patent Text Reader

Abstract

The invention discloses a production method of a three-layer co-extrusion polypropylene sheet suitable for electroplating. The production method comprises the following steps: feeding: feeding different ingredients to a first extruder, a second extruder and a third extruder through corresponding feeding systems; extruding: simultaneously extruding three layers of sheets in a three-layer co-extrusion die opening, extruding an upper-layer easily-water-etched polypropylene sheet by a first extruder, extruding a middle-layer polypropylene sheet by a second extruder, and extruding a lower-layer easily-water-etched polypropylene sheet by a third extruder; and calendering the sheet by using a calender, cooling the three-layer polypropylene sheet, cutting the cooled sheet into a required size, performing water treatment, soaking and etching on the sheet to form an anchor hole, and drying. The polypropylene sheet has the advantages that a three-layer composite structure is prepared by adopting a three-layer co-extrusion technology, and microscopic irregular anchor holes are formed in the surface of the composite material through water treatment etching, so that the polypropylene sheet has proper surface roughness and hydrophilicity, excellent metal adhesion is provided, and the polypropylene sheet is suitable for electroplating.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of plastic electroplating, in particular to a production method of a three-layer co-extruded polypropylene sheet suitable for electroplating. Background Art

[0002] In recent years, with the development of my country's automobile and related decoration industries, plastic electroplating technology has been widely used, which can not only significantly improve the durability, corrosion resistance and impact resistance of parts, but also beautify the appearance to meet the needs of consumers. At present, ABS materials are the most commonly used plastic products for electroplating. ABS electroplated plastic has the advantages of easy access to raw materials and easy rough processing. ABS plastic particles of the same size are nearly 50% more expensive than PP plastic particles.

[0003] For PP plastic electroplating, there are usually problems such as too smooth surface, few surface grafted functional groups, and low metal adhesion, which affect the electroplating quality, especially the bonding strength between PP plastic and electroplated metal. Therefore, the improvement of roughening method is the key factor to improve the electroplating quality. The roughening methods of general non-metallic materials include mechanical roughening and chemical roughening. Chemical roughening is to etch the PP surface with high sulfuric acid type, high chromic acid type, phosphoric acid type and hydrochloric acid type roughening liquid, but such roughening liquid will cause great harm to the environment. Summary of the invention

[0004] The purpose of the present invention is to make up for the above-mentioned deficiencies and disclose to the public a production method of a three-layer co-extruded polypropylene sheet suitable for electroplating. The production method is green and environmentally friendly. Water treatment is used to etch the polypropylene composite material. After etching, microscopic irregular anchor holes appear on its surface, so that the polypropylene sheet has suitable surface roughness and hydrophilicity to provide excellent metal adhesion and is suitable for electroplating.

[0005] The technical solution of the present invention is achieved in this way:

[0006] A method for producing a three-layer co-extruded polypropylene sheet suitable for electroplating comprises the following steps:

[0007] Step 1: Loading: After being mixed by a high-speed mixer, different ingredients are delivered to the first extruder, the second extruder, and the third extruder through corresponding feeding systems;

[0008] Step 2, extrusion: the first extruder and the third extruder are used to extrude the upper and lower layers of water-etchable polypropylene sheets respectively, and the second extruder is used to extrude the middle layer of polypropylene sheet. After the raw materials are continuously added to the extruder barrel, the heated and molten materials are continuously extruded from the three-layer co-extrusion die under pressure.

[0009] The temperature setting of the first extruder is 150℃~190℃;

[0010] The temperature setting of the second extruder is 140℃~200℃;

[0011] The temperature setting of the third extruder is 150℃~190℃;

[0012] The first extruder extrude the upper layer of the easily water-etched polypropylene sheet, the second extruder extrude the middle layer of the polypropylene sheet, and the third extruder extrude the lower layer of the easily water-etched polypropylene sheet;

[0013] Step 3, calendering: calendering the extruded sheet using a calender;

[0014] Step 4: Cooling: placing the calendered three-layer polypropylene sheet into a cooling water tank for cooling;

[0015] Step 5: Cutting: Cut the cooled sheet into required sizes;

[0016] Step 6: Etching: The cooled sheet is soaked and etched by water to form anchor holes, and then dried.

[0017] The measures to further optimize this technical solution are:

[0018] Preferably, the raw material formula of the water-etchable polypropylene sheet is, by weight percentage:

[0019]

[0020] Preferably, the polyether block polyamide, polyvinyl pyrrolidone and polyethylene glycol are all water-soluble macromolecules, and the molecular weight of the polyether block polyamide is 2000-20000, and the molecular weight of the polyethylene glycol is 700-900.

[0021] As an improvement, the raw material formula of the polypropylene sheet of the middle layer is, by weight percentage:

[0022] Random copolymer polypropylene 75-80%;

[0023] Calcium carbonate 10-20%;

[0024] Maleic anhydride grafted polypropylene 3-11%.

[0025] Preferably, in the step three, the calendering temperature is controlled at 130°C to 180°C.

[0026] Preferably, in step three, the rolling thickness is controlled at 0.3 mm-5 mm.

[0027] Preferably, in step five, the water treatment immersion etching time is controlled within 2h-4h.

[0028] The advantages of the present invention compared with the prior art are:

[0029] The present invention adopts three-layer co-extrusion technology to prepare a three-layer composite structure, wherein the upper and lower layers are water-etchable polypropylene sheets, and microscopic irregular anchor holes appear on the surface of the composite material through water treatment etching, so that the polypropylene sheet has suitable surface roughness and hydrophilicity, so as to provide excellent metal adhesion and be suitable for electroplating.

[0030] The polypropylene in the present invention is random copolymer polypropylene, and its crystallinity is usually lower than that of homopolymer polypropylene. Therefore, the copolymer polypropylene has good toughness and impact resistance, low shrinkage and good dimensional stability.

[0031] The invention adds maleic anhydride grafted polypropylene in the formula, which not only increases the compatibility between the raw materials, but also improves the interface bonding force between the three-layer sheets.

[0032] The polyether block polyamide, polyvinyl pyrrolidone and polyethylene glycol selected in the present invention are all water-soluble macromolecules, which can not only etch microscopic anchor holes under water treatment conditions to form appropriate surface roughness, but also improve the hydrophilicity of the material, which is beneficial to the subsequent electroplating coating bonding. DETAILED DESCRIPTION

[0033] The present invention is further described in detail below:

[0034] A method for producing a three-layer co-extruded polypropylene sheet suitable for electroplating comprises the following steps:

[0035] Step 1: Loading: After being mixed by a high-speed mixer, different ingredients reach the first extruder, the second extruder, and the third extruder through corresponding feeding systems.

[0036] Step 2, extrusion: the first extruder and the third extruder are used to extrude the upper and lower layers of water-etchable polypropylene sheets respectively, and the second extruder is used to extrude the middle layer of polypropylene sheet. After the raw materials are continuously added to the extruder barrel, the heated and molten materials are continuously extruded from the three-layer co-extrusion die under pressure.

[0037] The temperature setting of the first extruder is 150℃~190℃;

[0038] The temperature setting of the second extruder is 140℃~200℃;

[0039] The temperature setting of the third extruder is 150℃~190℃;

[0040] The first extruder extrude the upper layer of the easily water-etched polypropylene sheet, the second extruder extrude the middle layer of the polypropylene sheet, and the third extruder extrude the lower layer of the easily water-etched polypropylene sheet.

[0041] The raw material formula of the above-mentioned water-etchable polypropylene sheet is, by weight percentage:

[0042]

[0043] The polyether block polyamide, polyvinyl pyrrolidone and polyethylene glycol are all water-soluble macromolecules. The molecular weight of the polyether block polyamide is 2000-20000, and the molecular weight of the polyethylene glycol is 700-900.

[0044] The raw material formula of the polypropylene sheet of the above-mentioned middle layer is, by weight percentage:

[0045] Random copolymer polypropylene 75-80%;

[0046] Calcium carbonate 10-20%;

[0047] Maleic anhydride grafted polypropylene 3-11%.

[0048] The three extruders are set at different temperatures according to the material formula characteristics, and use a three-layer co-extrusion die to extrude three layers of sheets at the same time to form a composite material. The three-layer co-extrusion technology is an existing technology and will not be elaborated here.

[0049] Step 3, calendering: calender the extruded sheet using a calender; the calendering temperature is controlled at 130°C to 180°C, and the calendering thickness is controlled at 0.3mm-5mm.

[0050] Step 4: Cooling: Place the calendered three-layer polypropylene sheet into a cooling water tank for cooling.

[0051] Step 5: Cutting: Cut the cooled sheet into required sizes.

[0052] Step 6, etching: The cooled sheet is soaked and etched by water treatment to form anchor holes, and then dried. The soaking and etching time of water treatment is controlled within 2h-4h.

[0053] In the formula of the present invention, polypropylene is random copolymer polypropylene, and its melt index at a temperature of 230°C and a test load of 2.16Kg is 2-20g / 10min. Processing conditions and compatibility issues will affect the dispersion and agglomeration behavior of polar macromolecules such as polyether block polyamide, polyvinyl pyrrolidone, and polyethylene glycol in polypropylene melt. The method of forming anchor holes is mainly to dissolve polyether block polyamide, polyvinyl pyrrolidone, and polyethylene glycol in water, so that anchor holes exist on the surface and the surface roughness is improved. The polyether block polyamide, polyvinyl pyrrolidone, and polyethylene glycol used in the formula are all water-soluble macromolecules. The molecular weight of the selected polyether block polyamide is 2000-20000, and the polyether block polyamide of this molecular weight is partially dissolved in water; the molecular weight of polyethylene glycol is 700-900, and the polyethylene glycol of this molecular weight is semi-solid and has good solubility in water; polyvinyl pyrrolidone is very soluble in water.

[0054] The polypropylene in the present invention is random copolymer polypropylene, and its crystallinity is usually lower than that of homopolymer polypropylene. Therefore, the copolymer polypropylene has good toughness and impact resistance, low shrinkage and good dimensional stability.

[0055] The invention adds maleic anhydride grafted polypropylene in the formula, which not only increases the compatibility between the raw materials, but also improves the interface bonding force between the three-layer sheets.

[0056] The polyether block polyamide, polyvinyl pyrrolidone and polyethylene glycol selected by the present invention are all water-soluble macromolecules. When immersed in water, they can increase the surface roughness and etch microscopic anchor holes, so that the surface has a suitable surface roughness, improves the hydrophilicity of the material, and is conducive to the subsequent electroplating coating bonding. The anchor holes are formed by water treatment etching, which is safe and environmentally friendly, and avoids the environmental pollution risks that may be caused by the conventionally used roughening liquids such as hexavalent chromium and concentrated sulfuric acid. At the same time, the hydrophilicity of the surface can be increased, and the glossiness and adhesion strength of the coating after electroplating are also improved.

[0057] The test shows that the bonding strength of the PP plastic coating after electroplating is 0.7-3.6N·cm -1 Its bonding strength is equivalent to that of ABS plastic electroplating.

[0058] Compared with ABS plastic electroplating, PP plastic electroplating has the following advantages:

[0059] (1) Cost-effectiveness: PP materials are generally cheaper than ABS. Using PP can reduce material costs, especially in large-scale production.

[0060] (2) Light weight: The density of PP is lower than that of ABS. Using PP can reduce the weight of electroplated products, which is of great significance in certain application scenarios (such as automobiles, aerospace, etc.). The relative density of ABS is 1.05g / cm 3 PP is a crystalline polymer. Among commonly used plastics, PP is the lightest, with a density of only 0.91g / cm 3 (Smaller than water).

[0061] (3) Environmental requirements: PP materials are considered more environmentally friendly and have less impact on the environment during production and recycling. As environmental regulations become increasingly stringent, using PP materials can help companies meet these requirements.

[0062] (4) Thermal performance: PP's heat resistance is generally better than ABS, and its performance is more stable in high temperature environments. Therefore, in applications that require high heat tolerance, PP may be a better choice. Among general-purpose plastics, PP has the best heat resistance, with a heat deformation temperature of 80-100°C.

[0063] (5) Mechanical properties: ABS has high impact strength and rigidity, good wear resistance, but is relatively brittle. PP has lower impact strength and rigidity, higher softness, but its toughness and tensile strength are better than ABS.

[0064] The following is an experimental comparison of the embodiment and the comparative example:

[0065] In each embodiment and comparative example, the raw material formula of the polypropylene sheet of the middle layer is the same, which is 80 kg of random copolymer polypropylene, 15 kg of calcium carbonate, and 5 kg of maleic anhydride grafted polypropylene. Only the formula of the upper and lower layers is changed.

[0066] Table 1 Specific formulations of Examples 1-5 and Comparative Examples 1-2 (in kilograms)

[0067]

[0068] The above formula was processed according to the production method of the present invention to obtain material samples, which were then tested. The test results are shown in Table 2.

[0069] Table 2 Test results of various embodiments and comparative examples

[0070]

[0071] From the test results of Examples 1-5 and Comparative Examples 1-2, it can be seen that because the formula of the polypropylene sheet in the middle layer remains unchanged, the tensile strength, bending strength and simply supported beam notched impact performance change little. After adding polyether block polyamide, polyvinyl pyrrolidone and polyethylene glycol to the upper and lower layer formulas, anchor holes are formed on the surface of the material after water treatment and etching, so that the polypropylene sheet has a suitable surface roughness, thereby improving the glossiness and adhesion of the coating after electroplating. Generally speaking, the requirement of the electroplating process for the surface roughness of plastics is that the Ra value is between 0.4μm and 1.2μm. In the electroplating process, too high a surface roughness will lead to poor adhesion of the electroplated layer, while too low a surface roughness will easily lead to problems such as bubbles and cracks in the electroplated layer.

[0072] From the test results of Examples 1 to 5 and Comparative Examples 1 to 2, it can be seen that adding polyether block polyamide, polyvinyl pyrrolidone and polyethylene glycol to the formula can improve the hydrophilicity of the material surface (the smaller the contact angle, the better the hydrophilicity), and the glossiness and adhesion strength of the coating after electroplating are also improved.

[0073] The above are only preferred embodiments of the present invention, and are not intended to limit the implementation methods and protection scope of the present invention. Those skilled in the art should be aware that all solutions obtained by equivalent substitutions and obvious changes made using the specification of the present invention should be included in the protection scope of the present invention.

Claims

1. A method for producing a three-layer co-extruded polypropylene sheet suitable for electroplating, characterized in that: The following steps are involved: Step 1: Loading: After being mixed by a high-speed mixer, different ingredients are delivered to the first extruder, the second extruder, and the third extruder through corresponding feeding systems; Step 2, extrusion: the first extruder and the third extruder are used to extrude the upper and lower layers of water-etchable polypropylene sheets respectively, and the second extruder is used to extrude the middle layer of polypropylene sheet. After the raw materials are continuously added to the extruder barrel, the heated and molten materials are continuously extruded from the three-layer co-extrusion die under pressure. The temperature setting of the first extruder is 150℃~190℃; The temperature setting of the second extruder is 140℃~200℃; The temperature setting of the third extruder is 150℃~190℃; The first extruder extrude the upper layer of the easily water-etched polypropylene sheet, the second extruder extrude the middle layer of the polypropylene sheet, and the third extruder extrude the lower layer of the easily water-etched polypropylene sheet; Step 3, calendering: calendering the extruded sheet using a calender; Step 4: Cooling: placing the calendered three-layer polypropylene sheet into a cooling water tank for cooling; Step 5: Cutting: Cut the cooled sheet into required sizes; Step 6: Etching: The cooled sheet is soaked and etched by water to form anchor holes, and then dried.

2. The method for producing a three-layer co-extruded polypropylene sheet suitable for electroplating according to claim 1, characterized in that: The raw material formula of the water-etchable polypropylene sheet is as follows, by weight percentage: Random copolymer polypropylene 55-80%; Polyvinylpyrrolidone 8-20%; Polyether block polyamide 4-15%; Polyethylene glycol 3-8%; Maleic anhydride grafted polypropylene 3-6%; Copper powder 2%.

3. The method for producing a three-layer co-extruded polypropylene sheet suitable for electroplating according to claim 2, characterized in that: The polyether block polyamide, polyvinyl pyrrolidone and polyethylene glycol are all water-soluble macromolecules. The molecular weight of the polyether block polyamide is 2000-20000, and the molecular weight of the polyethylene glycol is 700-900.

4. The method for producing a three-layer co-extruded polypropylene sheet suitable for electroplating according to claim 1, characterized in that: The raw material formula of the polypropylene sheet of the middle layer is, by weight percentage: Random copolymer polypropylene 75-80%; Calcium carbonate 10-20%; Maleic anhydride grafted polypropylene 3-11%.

5. The method for producing a three-layer co-extruded polypropylene sheet suitable for electroplating according to claim 1, characterized in that: In the step 3, the calendering temperature is controlled at 130°C to 180°C.

6. The method for producing a three-layer co-extruded polypropylene sheet suitable for electroplating according to claim 1, characterized in that: In the step 3, the rolling thickness is controlled at 0.3 mm-5 mm.

7. The method for producing a three-layer co-extruded polypropylene sheet suitable for electroplating according to claim 1, characterized in that: In the step 5, the water treatment immersion etching time is controlled within 2h-4h.