Cross net film and forming process and equipment thereof
By unidirectional stretching and online composite of the omentum, the cross mesh structure is formed, which solves the problems of easy damage and significant grammation of existing mesh bags, and achieves higher tear resistance and lightweight, suitable for multiple and reduce costs and environmental impacts.
Patent Information
- Application Number
- CN202410943499.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-15
- Publication Date
- 2024-11-01
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing mesh bags are prone to damage and are of great importance. The traditional glass fiber reinforced mesh is harmful to the environment and cannot meet the thickness and strength requirements.
By stretching the cut web film in one direction, a quadrilateral structure with longitudinal and transverse stretching is formed, and composited online to form an interlaced mesh structure to improve product performance.
It achieves higher tear resistance, dimensional stability and lightweight, and is suitable for packaging, construction and other fields. It has low cost, is recyclable and pollution-free, and has better performance in replacing traditional products.
Smart Images

Figure CN118876543A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of cross membranes, and in particular relates to a cross mesh membrane and a molding process and equipment thereof. Background Art
[0002] The mesh bags currently available on the market are basically made by weaving, which is very easy to damage and has a higher gram weight. The reinforced products are all square mesh products made by extrusion process, and the thinnest thickness of the product is about 0.2mm. This thickness does not meet the requirements of some paper composites or products with thickness requirements. In addition, the product has cross nodes, which are more likely to be damaged and broken under stress.
[0003] The wall coating and composite reinforcement mesh products currently used in the construction industry are all made of glass fiber, which is not only harmful to construction workers but also detrimental to environmental protection. Summary of the invention
[0004] In order to overcome the shortcomings of the prior art, the present invention provides a cross mesh and its forming process and equipment. The present invention mainly enhances the performance of the cut mesh in one direction by stretching, and then composites the two layers of stretched mesh online to form a cross mesh structure to obtain a higher performance product.
[0005] The above object of the present invention is achieved through the following technical solutions:
[0006] A cross composite mesh product consists of two layers, the upper layer is a longitudinally stretched layer, and the lower layer is a transversely stretched layer. The longitudinally stretched layer is a quadrilateral composed of longitudinal thick ribs and longitudinal thin ribs after longitudinal stretching, which is approximately a parallelogram. The transversely stretched layer is a quadrilateral composed of transverse thick ribs and transverse thin ribs after transverse stretching, which is approximately a parallelogram.
[0007] Furthermore, the transverse thick ribs and the longitudinal thick ribs are placed perpendicular to each other with an angle of 90 degrees.
[0008] Furthermore, the thickness of the cross-composite mesh product is between 0.05-0.5 mm, and the width is preferably 2 m. The product thickness can be adjusted according to the thickness of the original film used, and then slitting is performed according to demand.
[0009] Furthermore, the cross-laminated web product has a grammage of 15-47 g / m 2 .
[0010] The shape of the product can be changed by cutting the size, so that the side length and height of the quadrilateral of the transverse and longitudinal pulling layers can be changed, so that the style of the composite product can be changed.
[0011] A forming process of a cross composite mesh product comprises the following steps:
[0012] The prepared transverse film and longitudinal film are placed on the transverse film unwinding device and the longitudinal film unwinding device respectively. The transverse film passes through the entrance of the transverse stretching device, is supported by the chain clip, and enters the transverse stretching oven at a uniform speed. It first passes through the preheating section to preheat the film material, and then passes through the stretching section for stretching; the longitudinal film enters the longitudinal stretching device for longitudinal stretching, and the transverse and longitudinal films simultaneously enter the multi-roller composite device. The multi-roller composite device uses a rubber roller on the top and an electrically heated steel roller on the bottom. The two layers of film are composited by applying pressure from a cylinder. After the composite is completed, the product is removed from the chain clip and enters the shaping roller. It is folded back and shaped through multiple water-temperature heated rollers. The shaped web directly enters the winding and trimming equipment to cut off the waste edges and collect the rolled cross web products.
[0013] Furthermore, the transverse stretching ratio is between 3 and 8 times.
[0014] Furthermore, the longitudinal stretching ratio is between 3 and 10 times.
[0015] Furthermore, the speed of the transverse stretching is the same as that of the longitudinal stretching.
[0016] Furthermore, the multi-roll composite equipment is placed in an insulated box, and an infrared heating device is provided inside the insulated box to control the temperature.
[0017] Furthermore, the temperature of the shaping roller is between 70° and 90° to ensure the flatness of the composite web.
[0018] The beneficial effects of the present invention compared with the prior art are:
[0019] The product of the present invention is mainly used in the fields of packaging, construction, agriculture, automobiles, etc. The product has many characteristics, such as good tear resistance, larger contact area under porous conditions, better dimensional stability, light weight and thin appearance.
[0020] This product can be made of olefin raw materials, is recyclable, pollution-free, and has strength that meets requirements. Therefore, it can better replace many existing products, has better performance, low cost, and has broad market prospects. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 It is a schematic diagram of the product of the present invention;
[0022] Figure 2 This is a schematic diagram of the product's horizontal pulling layer;
[0023] Figure 3 This is a schematic diagram of the longitudinal pulling layer of the product;
[0024] Figure 4 This is the effect diagram of the film after passing through the molding equipment, and the black line represents the cutting line;
[0025] Figure 5 This is a cross-retina product picture;
[0026] Figure 6 Strengthen the existing rib products in the market;
[0027] Figure 7 For existing packaging net products;
[0028] Figure 8 It is a schematic diagram of the transverse film and longitudinal film forming equipment;
[0029] Fig. 9 This is a schematic diagram of the membrane material stretching and laminating process equipment;
[0030] Fig.10 This is a process flow chart for preparing cross-membrane.
[0031] Among them, 1. transverse thick ribs, 2. transverse thin ribs, 3. longitudinal thick ribs, 4. longitudinal thin ribs, 5. unwinding equipment, 6. forming rollers, 7. winding equipment, 8. transverse film unwinding equipment, 9. longitudinal film unwinding equipment, 10. longitudinal stretching equipment, 11. multi-roller composite equipment, 12. shaping rollers, 13. winding and trimming equipment, 14. transverse stretching equipment. DETAILED DESCRIPTION
[0032] The present invention is described in detail below by specific examples, but the protection scope of the present invention is not limited. Unless otherwise specified, the experimental methods used in the present invention are all conventional methods, and the experimental equipment, materials, reagents, etc. used can be obtained from commercial channels.
[0033] Cross-membrane products are a brand-new product. Through process adjustment, cross-membrane products of various specifications can be prepared.
[0034] The key points of the present invention are:
[0035] (1) Initial film forming and cutting.
[0036] (2) Preparation of single-layer reticular structure.
[0037] (3) A method of cross-compounding two layers of mesh.
[0038] The present invention mainly uses stretching to orient the macromolecules of the material and increase the intermolecular force. The composite product has reinforcing ribs in multiple directions in the structure, so the strength of the product is much higher than other types of products, and the surface of the product is flat, which is more conducive to composite use.
[0039] In the field of packaging, the existing products are basically woven products, such as Figure 7As shown, this type of product is made by cross-weaving plastic strips. Because there is no fixation between the strips, it is easy to deform and damage. The product of the present invention not only has a more complex structure, but also has a strong composite between the horizontal and vertical strips. The horizontal thick ribs 1 and the vertical thick ribs 3 are placed perpendicular to each other, so that the angle is 90 degrees, the shape is not easy to change, and the strength is higher.
[0040] In the field of reinforcing ribs, the traditional reinforcing materials are now made of extruded mesh, such as Figure 6 As shown, this extruded mesh is made by rotating extruded plastic strips. Because of the node structure, it has the disadvantages of low strength, heavy weight, large thickness, and difficulty in compounding. However, the product of the present invention increases its strength by stretching the film while reducing the thickness of the film material itself, reducing the gram weight of the product and saving costs. In addition, compared with this product or existing extruded mesh reinforcement products, it has a larger surface area and no nodes, making it easier to compound with other products.
[0041] The resin used in the present invention includes: polyolefins such as polypropylene and polyethylene and their copolymers, polyamide copolymers such as nylon 6 and nylon 66, polyvinyl chloride, etc.
[0042] Example 1
[0043] The rolled cast film of a specific width is placed on the unwinding device 5, and the film material passes through the correction device and enters the transverse forming roller to complete the initial cutting process of the film, and then is rewound by the transverse rewinding device. The cutting speed of this process can reach 50-80 meters / minute.
[0044] According to the processing procedure of the transverse film, the longitudinal forming roller is replaced, and the processing and winding of the longitudinal film is completed to obtain a rolled longitudinal film material.
[0045] The prepared transverse film and longitudinal film are placed on the transverse film unwinding device 8 and the longitudinal film unwinding device 9 respectively. The two unwinding devices use magnetic powder brakes and tension sensors to control constant tension so that the processed transverse and longitudinal films will not be stretched and damaged.
[0046] The transverse film passes through the entrance of the transverse stretching device 14, is supported by the chain clip, and enters the interior of the transverse stretching oven at a uniform speed. It first passes through the preheating section to preheat the film material, and then passes through the stretching section for stretching. According to product requirements, the transverse stretching ratio can be controlled between 3-8 times. (The larger the stretching ratio, the larger the product gap, the lighter the weight, and the thinner the thickness. However, when the stretching ratio is less than 3 times, the mechanical strength is not significantly improved. If it exceeds 8 times, it is difficult for ordinary equipment to complete, and high equipment costs are required.) Then the film is shaped in the shaping section to prevent the film material from shrinking after leaving the oven. The oven temperature setting is determined according to the material and thickness of the film and the stretching speed.
[0047] (When the stretching speed of 0.1mm thick PP film is 30M / min, the temperature of the preheating section is 110-120℃, the stretching section is 120-130℃, and the shaping section is 110-120℃.)
[0048] The longitudinally stretched film enters the longitudinal stretching device 10. The longitudinal stretching device 10 adopts electric heating / oil heating, uses 3 variable frequency motors, and stretches through 3 sets of hot roller speed differences. The stretching ratio is generally between 3-10 times. The stretching temperature is between 90-150 degrees, and different temperatures are set according to different materials. (PP film is generally set between 100-110 degrees). The longitudinal stretching device 10 can adjust different speeds, and the normal production speed is above 50M / minute. During the production process, the horizontal stretching speed and the longitudinal stretching speed must be adjusted to be consistent.
[0049] The horizontally stretched film and the vertically stretched film are simultaneously fed into the multi-roller composite device 11. The multi-roller composite device 11 uses a rubber roller on the top and a heated steel roller on the bottom. The two layers of film are composited by applying pressure from a cylinder. The multi-roller composite device 11 is placed in an insulated box. The insulated box is equipped with an infrared heating device to control the temperature. The composite process needs to ensure that the temperature of the horizontal and vertical films is kept between the softening temperature and the melting temperature to ensure the bonding strength of the two layers. During the composite process, the horizontal film is still in a chain clip stretching state to facilitate the flatness of the composite product.
[0050] After the lamination is completed, the product is removed from the chain clip and enters the shaping roller 12, and is returned to the shaping roller 12 through multiple water-heated rollers. The temperature of the shaping roller 12 is between 70-90° to ensure the flatness of the composite web.
[0051] The shaped web directly enters the winding and trimming device 13, where the waste edges are cut off and a rolled cross web product is obtained.
[0052] The final product consists of two layers, the upper layer is the longitudinal pulling layer, and the lower layer is the transverse pulling layer. The longitudinal pulling layer is a quadrilateral composed of longitudinal thick ribs and longitudinal thin ribs after longitudinal stretching, and the transverse pulling layer is a quadrilateral composed of transverse thick ribs and transverse thin ribs after transverse stretching.
[0053] The thickness of the cross-composite mesh product is between 0.05-0.5mm, and the width is preferably 2m. The product thickness can be adjusted according to the thickness of the original film used, and then slit according to demand.
[0054] The weight of cross-laminated web products is 15-47g / m 2 .
[0055] The shape of the product can be changed by cutting the unstretched original film to a different size, which can change the side length and height of the quadrilaterals of the transverse and longitudinal layers, thereby changing the style of the composite product.
[0056] Example 2
[0057] Three samples of the product of the present invention and three samples of Figure 6 The product samples, and the two samples have the same gram weight, are subjected to composite tests. The six samples are respectively composited with paper to obtain composite products, and then the products are subjected to tensile strength tests and peel strength tests. The tensile strength of the product of the present invention is Figure 6 The peel strength is more than twice that of the product. Figure 6 1.5 times the product.
[0058] Then select three samples of the product of the present invention and three Figure 7 The product samples were made, and the weight of the two products was ensured to be the same. The tensile strength test was performed on 6 samples respectively, and the average tensile strength of the product of the present invention was obtained. Figure 7 More than 3 times the product.
[0059] The above-described embodiments are only preferred embodiments of the present invention, but not all feasible embodiments of the present invention. For those skilled in the art, any obvious changes made thereto without departing from the principles and spirit of the present invention should be considered to be included in the scope of protection of the claims of the present invention.
Claims
1. A forming process for a cross-composite mesh product, Its characteristics are: The following steps are involved: The prepared transverse film and longitudinal film are placed on the transverse film unwinding device (8) and the longitudinal film unwinding device (9) respectively. The transverse film passes through the entrance of the transverse stretching device (14), is supported by the chain clip, and enters the interior of the transverse stretching oven at a uniform speed. It first passes through the preheating section to preheat the film material, and then passes through the stretching section to stretch it. The longitudinal film enters the longitudinal stretching device (10) for longitudinal stretching, and the transverse and longitudinal stretching films simultaneously enter the multi-roller composite device (11). The multi-roller composite device (11) uses a rubber roller on the top and an electrically heated steel roller on the bottom, and applies pressure from a cylinder to composite the two layers of film. After the composite is completed, the product is removed from the chain clip and enters the shaping roller (12), and is folded back and shaped by multiple water-heated rollers. The shaped web directly enters the winding and trimming device (13), where the waste edges are cut off and a rolled cross web product is obtained.
2. The forming process of the cross-composite web product according to claim 1, Its characteristics are: The transverse stretching ratio is between 3-8 times.
3. The forming process of the cross-composite web product according to claim 1, Its characteristics are: The longitudinal stretching ratio is between 3-10 times.
4. The forming process of the cross-composite web product according to claim 1, Its characteristics are: The speed of transverse stretching and longitudinal stretching is the same.
5. The forming process of the cross-composite web product according to claim 1, Its characteristics are: The multi-roller composite device (11) is placed in a heat preservation box, and an infrared heating device is provided inside the heat preservation box to control the temperature.
6. The forming process of the cross-composite web product according to claim 1, Its characteristics are: The temperature of the shaping roller (12) is between 70-90°.
7. A cross composite mesh product, Its characteristics are: The upper layer is a longitudinally stretched layer and the lower layer is a transversely stretched layer. The longitudinally stretched layer is a quadrilateral formed by longitudinal thick ribs (3) and longitudinal thin ribs (4) after longitudinal stretching, and the transversely stretched layer is a quadrilateral formed by transverse thick ribs (1) and transverse thin ribs (2) after transverse stretching.
8. The cross-composite web product according to claim 7, Its characteristics are: The transverse thick ribs (1) and the longitudinal thick ribs (3) are placed perpendicular to each other, with an angle of 90 degrees.
9. The cross-composite web product according to claim 7, Its characteristics are: The thickness of the cross-laminated mesh product is between 0.05-0.5mm.
10. The cross-composite web product according to claim 7, Its characteristics are: The weight of cross-laminated web products is 15-47g / m 2 .
Citation Information
Patent Citations
Mining plastic stretching net
CN2869325Y
Method and machine for cross-laying of non-weaving plastic cloth
CN85104384A
Plastic netting extrusion molding and its manufacture
JP1978049170A
Cited By
Method and system for preparing film having built-in mesh
WO2026118374A1