Iodhexol amorphous substance and preparation method thereof
The preparation of iodhell amorphous substance by heating reflux and spray drying in primary and secondary solvents was solved, and the literature missing problem of iodhell polycrystalline form was achieved, and industrial production and research applications were achieved with good stability , meets market demand.
Patent Information
- Application Number
- CN202410937313.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-12
- Publication Date
- 2024-11-01
AI Technical Summary
Up to now, there is no document that the polycrystalline form of iodhellol raw materials exists. It is very necessary to develop an iodhellol amorphous substance and its preparation method, especially to meet its medicinal value and industrial production needs.
通过将任意晶型的碘海醇粗品在一级溶剂中加热回流搅拌至完全溶解,冷却析晶,然后在二级溶剂中进行喷雾干燥,制得碘海醇无定型物,优选一级溶剂为乙醇,二级溶剂为水,控制喷雾干燥温度和搅拌时间以提高无定型物的收率和稳定性。
The stability of the iodine-hell amorphous substance is achieved, suitable for industrial production, and it is convenient for further research on different crystal forms. The crystal form of the sample has not changed after 6 months of storage under accelerated conditions, indicating that its stability is good.
Smart Images

Figure CN118878438A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of drug synthesis, and in particular to an iohexol amorphous substance and a preparation method thereof. Background Art
[0002] Iohexol, trade name: Omnipaque, English name: Iohexol, is a second-generation non-ionic monomeric iodine contrast agent. It is suitable for angiography, urinary system, spinal cord and hip joint, lymphatic system angiography. The structural formula is as follows:
[0003] Iohexol injection is a second-generation non-ionic monomeric iodine contrast agent developed by Nycomed of Norway. Its working principle combines the absorption of X-rays by iodine in blood vessels and tissues to produce image display. It was officially launched in the Norwegian and Swedish markets in 1982, and was approved by the US FDA for marketing in the United States in 1985 and mass-produced. According to CHEMISTRYREVIEW(S) information disclosed by the FDA, the dosage form of this product is injection, with five specifications of 140mgI / ml, 180mgI / ml, 240mgI / ml, 300mgI / ml and 350mgI / ml.
[0004] So far, there is no literature reporting the existence of polymorphic forms of iohexol API, including crystalline forms. In view of the crystalline form and medicinal value of iohexol, it is very necessary to develop an iohexol amorphous substance and a preparation method thereof. Summary of the invention
[0005] In view of the above problems, the present invention aims to provide an amorphous iohexol having good stability and suitable for industrial production and a preparation method thereof.
[0006] In order to achieve the above object, the technical scheme adopted by the present invention is as follows: an iohexol amorphous substance, the amorphous substance having Figure 1 The X-ray powder diffraction pattern and diffraction peaks shown; Figure 4 As shown, its DSC scan has endothermic peaks at 293.4°C to 298.4°C and a maximum endothermic peak at 295.0°C.
[0007] A method for preparing an iohexol amorphous substance comprises the following steps: 1) adding crude iohexol of any crystal form into a primary solvent, heating under reflux and stirring until completely dissolved, refluxing for reaction, cooling for crystallization, and filtering to obtain wet iohexol; 2) adding the wet iohexol obtained in step 1) into a secondary solvent, stirring until completely dissolved, and spray drying at a certain temperature to obtain an iohexol amorphous substance.
[0008] In the preparation method of the present invention, the primary solvent is selected from any one of ethanol, methanol, isopropanol, tetrahydrofuran, acetonitrile or dichloromethane, preferably ethanol.
[0009] In the preparation method of the present invention, the time for heating under reflux and stirring until complete dissolution in step 1) is ≤ 60 min; by controlling the complete dissolution time, rapid crystallization of the iohexol wet product is facilitated, and ultimately the yield of the iohexol amorphous product is improved.
[0010] In the preparation method of the present invention, the secondary solvent in step 2) is water; the concentration of the dissolved iohexol in water is 0.005 g / ml to 15 g / ml; the preferred concentration is 0.5 g / ml.
[0011] In the preparation method of the present invention, the stirring time in step 2) is 1 h to 96 h, preferably 10 h to 16 h.
[0012] In the preparation method of the present invention, the spray drying air inlet temperature of step 2) is 210°C to 240°C, and the air outlet temperature is 105°C to 135°C.
[0013] The advantages of the present invention are as follows: the present invention provides a method for preparing an amorphous iohexol; the amorphous crystals produced by the present invention have good stability and high application value; the overall process is suitable for industrial and industrialized production and meets market demand; and it is convenient to further study different crystal forms of iohexol. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 The X-ray powder diffraction pattern of the iohexol amorphous substance at day 0 in Example 1 of the present invention; Figure 2 is an infrared spectrum of the iohexol amorphous substance in Example 1 of the present invention; Figure 3 The TGA spectrum of the iohexol amorphous substance in Example 1 of the present invention; Figure 4 The DSC spectrum of the iohexol amorphous substance in Example 1 of the present invention; Figure 5 This is the X-ray powder diffraction pattern of the iohexol amorphous substance accelerated for 6 months in Example 4 of the present invention. DETAILED DESCRIPTION
[0015] The present invention is further described in detail below in conjunction with the accompanying drawings and specific implementation methods.
[0016] The test instruments used in the experiments in the embodiments of the present invention are as follows: 1. X-ray diffraction spectrum Instrument model: Bruker D8 Advance X-ray powder diffractometer; Ray: monochromatic Cu-Kα ray (λ=1.5406Å); Scanning mode: θ / 2θ, scanning range: 3~40°.
[0017] 2. Infrared spectroscopy Instrument model: Bruker Tensor 27 infrared spectrometer; Determination conditions: solid KBr pellet.
[0018] 3. Differential thermal analysis (DSC) Instrument model: NETZSCH DSC3500; Purge gas: nitrogen; Heating rate: 10.0℃ / min; Temperature range: 25~320℃.
[0019] 4. Thermogravimetric analysis (TGA) Instrument model: Perkin-Elmer TGA4000; Purge gas: nitrogen; Heating rate: 10.0℃ / min; Temperature range: 30~335℃. Embodiment 1:
[0020] 200.0 g of crude iohexol of any crystal form was added to 800 ml of ethanol, stirred and refluxed for 30 min, the reaction solution was clarified, stirred and refluxed for 12 hours, the iohexol solution was cooled to 25° C., crystallized for 2 hours, and filtered to obtain 216.8 g of wet iohexol.
[0021] 216.8 g of the obtained iohexol wet product was added to 400 ml of water to obtain an iohexol aqueous solution. The iohexol aqueous solution was passed through a 0.22 μm filter element and then spray-dried with an inlet air temperature of 220° C. and an outlet air temperature of 110° C.
[0022] 187.6 g of iohexol amorphous material was collected, with a yield of 93.8%. The X-ray powder diffraction pattern of iohexol amorphous material is as follows: Figure 1 As shown (test time: April 25, 2022).
[0023] The infrared spectrum of iohexol amorphous substance is as follows Figure 2 As shown, the detection time is April 25, 2022; the infrared spectrum of the sample shows the presence of hydroxyl, amine, aromatic, saturated alkane and amide groups. The main absorption peak of the infrared spectrum is consistent with the structure of the amorphous iohexol.
[0024] The TGA spectrum of iohexol amorphous substance is as follows Figure 3 As shown, the detection time is April 27, 2022; the sample loses 0.74% weight from 30°C to 120°C, indicating that the sample contains free water; there is almost no weight loss from 120°C to 250°C, indicating that the sample does not contain adsorbed water or residual solvent; then the sample begins to lose weight, loses weight dramatically at 290°C, and loses about 56% at 335°C.
[0025] The DSC spectrum of iohexol amorphous substance is as follows Figure 4 As shown, the detection time is April 27, 2022; the sample DSC scan has an endothermic peak at 293.4℃~298.4℃; and the maximum endothermic peak is at 295.0℃. Embodiment 2:
[0026] Add 200.0 g of any crystalline form of iohexol to 800 ml of isopropanol, stir and reflux for 30 min, the reaction solution is clarified, stir and reflux for 12 hours, cool the iohexol solution to 25° C., crystallize for 2 hours, and filter to obtain 123.6 g of iohexol wet product.
[0027] 123.6 g of the obtained iohexol wet product was added to 400 ml of water to obtain an iohexol aqueous solution. The iohexol aqueous solution was passed through a 0.22 μm filter element and then spray-dried with an inlet air temperature of 220° C. and an outlet air temperature of 110° C.
[0028] 106.8 g of iohexol amorphous substance was collected, with a yield of 53.4%.
[0029] (The detailed X-ray powder diffraction pattern is similar to Figure 1 ). Embodiment 3:
[0030] Add 200.0 g of any crystalline form of iohexol to 800 ml of methanol, stir and reflux for 30 min, the reaction solution is clarified, stir and reflux for 12 hours, cool the iohexol solution to 25° C., crystallize for 2 hours, and filter to obtain 46.0 g of iohexol wet product.
[0031] 46.0 g of the obtained iohexol wet product was added to 400 ml of water to obtain an iohexol aqueous solution. The iohexol aqueous solution was passed through a 0.22 μm filter element and then spray-dried. The inlet air temperature was 220° C. and the outlet air temperature was 110° C.
[0032] 39.6 g of iohexol amorphous substance was collected, with a yield of 19.8%. The detailed X-ray powder diffraction pattern of the substance is similar to Figure 1 The vertical table is exactly the same. The amorphous iohexol crystals produced in January 2022 were placed under accelerated conditions (40°C ± 2°C, 75% ± 5% RH) to investigate the stability of the iohexol sample. The sampling period was 6 months. The X-ray powder diffraction pattern of the iohexol amorphous material accelerated for 6 months is as follows: Figure 5 As shown (test time: August 19, 2022).
[0033] The results of the stability study showed that after the amorphous iohexol crystals were stored at 40℃±2℃, 75%±5%RH for 6 months, the crystal form of the sample did not change. This indicates that the amorphous iohexol crystals are stable during the accelerated storage process (40℃±2℃, 75%±5%RH).
[0034] It should be noted that the above are merely preferred embodiments of the present invention and are not intended to limit the protection scope of the present invention. Any combination or equivalent transformation made on the basis of the above embodiments shall fall within the protection scope of the present invention.
Claims
1. An iohexol amorphous substance, characterized in that: The amorphous substance has an X-ray powder diffraction pattern and diffraction peaks as shown in FIG1 ; its DSC scanning has an endothermic peak at 293.4° C. to 298.4° C.
2. The iohexol amorphous substance according to claim 1, characterized in that Its DSC scan has a maximum endothermic peak at 295.0°C.
3. A method for preparing the iohexol amorphous substance as claimed in claim 1-2, characterized in that: The preparation method comprises the following steps: 1) adding crude iohexol of any crystal form into a primary solvent, heating under reflux and stirring until completely dissolved, refluxing for reaction, cooling for crystallization, and filtering to obtain wet iohexol; 2) adding the wet iohexol obtained in step 1) into a secondary solvent, stirring until completely dissolved, and spray drying at a certain temperature to obtain an iohexol amorphous substance.
4. The preparation method according to claim 3, characterized in that: The primary solvent is selected from any one of ethanol, methanol, isopropanol, tetrahydrofuran, acetonitrile or dichloromethane.
5. The preparation method according to claim 3, characterized in that: In the step 1), the time for heating under reflux and stirring until complete dissolution is ≤ 60 min.
6. The preparation method according to claim 3, characterized in that: In the step 2), the secondary solvent is water, and the concentration of the dissolved iohexol in water is 0.005 g / ml to 15 g / ml.
7. The preparation method according to claim 6, characterized in that: The concentration of the dissolved iohexol in water is 0.5 g / ml.
8. The preparation method according to claim 3, characterized in that: In the step 2), the stirring time is 1 h to 96 h.
9. The preparation method according to claim 8, characterized in that: The stirring time is 10h~16h.
10. The preparation method according to claim 3, characterized in that: In the step 2), the spray drying air inlet temperature is 210°C to 240°C, and the air outlet temperature is 105°C to 135°C.
Citation Information
Patent Citations
Method for industrially producing iohexol refined product
CN116178204A
Iohexol powder and method of using the same
US20150251993A1
Procedure for obtaining high purity iohexol
WO2022106715A1