Preparation method of wear-resistant soot dispersant

By introducing aromatic phosphoric acid and polyisobutylene succinimide and boric acid into the phosphorus boronized ashless dispersant, the problem of degradation of fume dispersion in traditional dispersants is solved, and better fume dispersion performance and resistance are achieved Grinding performance, meet the needs of high-spec oil products.

CN118878723APending Publication Date: 2024-11-01XINXIANG RICHFUL LUBE ADDITIVE CO LTD
0 Cites 1 Cited by

Patent Information

Application Number
CN202410915837.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-09
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

Traditional phosphorus boronized ashless dispersant will reduce the soot dispersion during the preparation process and cannot meet the requirements of high-specification diesel engine oil for soot dispersion performance.

Method used

Aromatic phosphoric acid reacts with polyisobutylene succinimide and boric acid under the action of accelerator to prepare a phosphorus bored ashless dispersant, introduce aromatic groups and phosphorus elements, and improve the soot dispersion and wear resistance of the dispersant .

Benefits of technology

The obtained phosphorus boronized ashless dispersant not only maintains the antioxidant and anti-wear properties of the traditional dispersant, but also significantly improves the soot dispersion performance, and is even better than polyisobutylene succinimide before phosphorus boronation. Dispersant meets the needs of high-standard oil products for dispersion and wear resistance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118878723A_ABST
    Figure CN118878723A_ABST
Patent Text Reader

Abstract

The invention discloses a preparation method of a wear-resistant soot dispersant. The preparation method comprises the following steps: preparing polyisobutylene succinimide; the preparation method comprises the following steps: reacting polyisobutylene succinimide, boric acid and aromatic phosphoric acid under the action of an accelerant to prepare a phosphorus boronized ashless dispersant; wherein the aromatic phosphoric acid is a phosphoric acid compound which is formed by directly connecting phosphorus atoms and aromatic rings and contains aromatic groups. Aromatic phosphoric acid is selected in the preparation process of the phosphorus boronized ashless dispersant, and phosphorus and aromatic groups are introduced into molecules at the same time, so that the prepared phosphorus boronized ashless dispersant has soot dispersing performance more excellent than that of traditional phosphorus boronized polyisobutylene succinimide; the soot dispersibility of the phosphorus boronizing ashless dispersant is even superior to that of a polyisobutylene succinimide dispersant before phosphorus boronizing, and meanwhile, the phosphorus boronizing ashless dispersant has good wear resistance, friction reduction and oxidation resistance.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of lubricating oil additives, and in particular to a method for preparing an anti-wear soot dispersant. Background Art

[0002] Polyisobutylene succinimide, with its lipophilic group (polyisobutylene molecular chain) and polar group in the molecule, can show a strong solubilizing effect on the soot produced by fuel combustion and the sludge generated by lubricating oil oxidation. It can well wrap these particles and suspend them in the oil, avoiding problems such as filter clogging caused by the deposition of these solid substances.

[0003] As an important lubricant additive, the main types of dispersants include polyisobutylene succinimide, polyisobutylene succinate, ashless phosphate, benzylamine, etc. Among them, polyisobutylene succinimide is more widely used and commonly used in engine lubricants, such as diesel / gasoline engine lubricants, medium-speed cylinder piston engine lubricants, two-stroke gasoline engine lubricants, etc. The amount of dispersants used in engine lubricants accounts for about 80% of the total amount of dispersants used. In addition to engine oil, dispersants are also used in ATF, gear oil, hydraulic oil, etc.

[0004] But it is worth noting that although polyisobutylene succinimide has excellent dispersibility, due to the presence of low molecular weight compounds, such as low molecular weight polyisobutylene succinimide, low molecular weight polyisobutylene succinamide, unstable free amines, etc., these small molecules can diffuse into the sealing material during contact with the sealing material, causing changes in the physical and mechanical properties of the sealing material, resulting in sealing failure. Later, researchers found that the product obtained by using boric acid to react with polyisobutylene succinimide has good rubber compatibility and can improve the phenomenon of dispersant damage to rubber material sealing.

[0005] With the continuous improvement of internal combustion engine manufacturing technology and increasingly stringent requirements for energy conservation and environmental protection, the specifications of internal combustion engine lubricants are also constantly improving, and the requirements for ashless dispersants are also getting higher and higher. Traditional ashless dispersants can no longer meet the requirements of high-specification oils for soot dispersibility. The introduction of aromatic groups, heteroatom cyclic compounds, etc., effectively improves the soot dispersibility of dispersants. At the same time, ashless dispersants are also expected to have more additional functions to achieve multiple uses, such as boration and phosphoboration reactions on polyisobutylene succinimide, which gives the dispersant certain antioxidant and wear resistance on the basis of dispersibility.

[0006] As oil specifications are improved, the requirements for metal content in oil products are becoming more stringent. The use of traditional anti-wear agent ZDDP (zinc dialkyl dithiophosphate) is strictly restricted, and ashless anti-wear additives that do not contain metals are becoming more and more popular. Adding elements such as phosphorus, boron, sulfur, and molybdenum to ashless dispersants can improve their anti-wear properties while maintaining their own sludge dispersibility. This has become an important research direction for many researchers.

[0007] The boron-containing compounds used in traditional boron-phosphorus ashless dispersants are usually inorganic boron-containing compounds such as boric acid and boron trioxide, or organic boric acid esters such as tributyl borate and boron nitrogen ester compounds; the phosphorus-containing compounds used are usually phosphoric acid, phosphorous acid, phosphorus pentoxide, phosphite, etc. Introducing these boron-containing and phosphorus-containing compounds into traditional ashless dispersants can keep the dispersant's sludge dispersing performance, but will reduce the dispersant's ability to disperse soot to a certain extent.

[0008] As we all know, in high-specification diesel engine oils, traditional ashless dispersants can no longer meet the oil's requirements for soot dispersion performance. If you want to use this anti-wear type of traditional boron phosphide ashless dispersant in conjunction with ZDDP to achieve a better anti-wear effect, or reduce the amount of ZDDP used, it will be even more difficult to meet the requirements for soot dispersion performance. Summary of the invention

[0009] In view of the shortcoming that the soot dispersibility of the above-mentioned boron phosphide ashless dispersant will be reduced during the preparation process, the present invention provides a method for preparing an anti-wear soot dispersant. The anti-wear soot dispersant is a boron phosphide ashless dispersant with excellent antioxidant and anti-wear properties and excellent soot dispersibility. While providing good anti-wear properties, extreme pressure properties and antioxidant properties, the soot dispersibility is not only not reduced, but improved.

[0010] The present invention discloses a method for preparing an anti-wear soot dispersant, comprising:

[0011] Preparation of polyisobutylene succinimide;

[0012] Under the action of a promoter, polyisobutylene succinimide, boric acid and aromatic phosphoric acid are reacted to obtain a boronized ashless dispersant.

[0013] As a further improvement of the present invention, the accelerator includes one or more of water, ethanol, isobutanol, n-butanol, isopropanol, and n-propanol, and the amount of the accelerator is 30% to 150% of the total mass of the boric acid and the aromatic phosphoric acid.

[0014] As a further improvement of the present invention, the amount of the accelerator is 50% to 110% of the total mass of the boric acid and the aromatic phosphoric acid.

[0015] As a further improvement of the present invention, the aromatic phosphoric acid is a phosphoric acid compound containing an aromatic group in which a phosphorus atom is directly connected to an aromatic ring, including one or more of phenyl phosphoric acid, p-methylphenyl phosphoric acid, m-methylphenyl phosphoric acid, and 1-naphthyl phosphoric acid.

[0016] As a further improvement of the present invention, the boron content of the prepared boronized ashless dispersant is 0.3-1.5 wt %, and the phosphorus content is 0.3-1.0 wt %.

[0017] As a further improvement of the present invention, the reaction conditions for the reaction of polyisobutylene succinimide, boric acid and aromatic phosphoric acid are:

[0018] First react at 70-120°C for 2-8h, then heat to 150-160°C, introduce nitrogen to purge and react for 1.5-5h to obtain a boron phosphide ashless dispersant.

[0019] As a further improvement of the present invention, the preparation method of the polyisobutylene succinimide comprises:

[0020] The polyisobutylene succinic anhydride is reacted with polyene polyamine to obtain polyisobutylene succinimide.

[0021] As a further improvement of the present invention, the preparation method of the polyisobutylene succinimide specifically comprises:

[0022] After polyisobutylene succinic anhydride is mixed and diluted with base oil, polyethylene polyamine is added dropwise at 60-120° C., and then nitrogen is introduced, and the temperature is raised to 150-160° C. for reaction for 1-3 hours (preferably 2 hours) to obtain a polyisobutylene succinimide ashless dispersant.

[0023] As a further improvement of the present invention, the average molecular weight of the polyisobutylene succinic anhydride is 500-5000, preferably 750-3000, further preferably 900-3000, and more preferably 900-1500; the degree of substitution is 1.1-1.2.

[0024] As a further improvement of the present invention, the polyene polyamine includes one or more of diethylenetriamine, triethylenetetramine, tetraethylenepentamine, and heavy polyethylene polyamine, and the molar ratio of the polyisobutylene succinic anhydride to the polyethylene polyamine is 1.3:1 to 3:1, preferably 1.5:1 to 2.5:1.

[0025] Compared with the prior art, the present invention has the following beneficial effects:

[0026] The present invention selects aromatic phosphoric acid in the preparation process of the phosphoborated ashless dispersant, and simultaneously introduces phosphorus element and aromatic group into the molecule, which not only gives the dispersant certain anti-wear performance, but also improves the soot dispersing performance of the dispersant through the introduction of aromatic group; the prepared phosphoborated ashless dispersant has better soot dispersing performance than traditional phosphoborated polyisobutylene succinimide, and its soot dispersibility is even better than that of the polyisobutylene succinimide dispersant before phosphoboration; and the phosphoborated ashless dispersant has good anti-wear, friction reduction and antioxidant performance. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] Figure 1 The present invention is a flow chart of a method for preparing the anti-wear soot dispersant disclosed in the present invention. DETAILED DESCRIPTION

[0028] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0029] The present invention is further described in detail below in conjunction with the accompanying drawings:

[0030] like Figure 1 As shown, the present invention provides a method for preparing an anti-wear soot dispersant, comprising:

[0031] Step 1, preparation of polyisobutylene succinimide:

[0032] Specifically include:

[0033] After polyisobutylene succinic anhydride is mixed and diluted with base oil, polyethylene polyamine is added dropwise at 60-120° C., and then nitrogen is introduced, and the temperature is raised to 150-160° C. for reaction for 1-3 hours (preferably 2 hours) to obtain a polyisobutylene succinimide ashless dispersant;

[0034] Among them, the average molecular weight of polyisobutylene succinic anhydride is 500-5000, preferably 750-3000, further preferably 900-3000, and more preferably 900-1500; the degree of substitution is 1.1-1.2; the polyene polyamine includes one or more of diethylenetriamine, triethylenetetramine, tetraethylenepentamine, and heavy polyethylene polyamine (heavy polyethylene polyamine refers to a mixture of triethylenetetramine, tetraethylenepentamine, pentaethylenehexamine, hexaethyleneheptamine, etc., a common name in the industry, and the trade names include POLY-7 of Tosoh of Japan, EA300 and E-100 of Huntsman, etc.); the molar ratio of polyisobutylene succinic anhydride to polyethylene polyamine is 1.3:1 to 3:1, preferably 1.5:1 to 2.5:1.

[0035] Step 2: Under the action of a promoter, polyisobutylene succinimide, boric acid, and aromatic phosphoric acid are reacted to obtain a boronized ashless dispersant:

[0036] Specifically include:

[0037] Under the action of a promoter, polyisobutylene succinimide, boric acid and aromatic phosphoric acid are first reacted at 70-120°C for 2-8 hours, then the temperature is raised to 150-160°C, nitrogen is introduced for purging and the reaction is carried out for 1.5-5 hours to obtain a boronized ashless dispersant.

[0038] Wherein, the promoter includes one or more of water, ethanol, isobutanol, n-butanol, isopropanol, and n-propanol, and the amount of the promoter is 30% to 150% of the total mass of boric acid and aromatic phosphoric acid, preferably 50% to 110%. Aromatic phosphoric acid is a phosphoric acid compound containing aromatic groups composed of phosphorus atoms and aromatic rings directly connected, including one or more of phenylphosphoric acid, p-methylphenylphosphoric acid, m-methylphenylphosphoric acid, and 1-naphthylphosphoric acid. During the preparation process, the amount of boric acid and aromatic phosphoric acid is selected according to the requirements for the content of phosphorus and boron in the dispersant; preferably, the boron content in the prepared boronized ashless dispersant is 0.3 to 1.5wt%, more preferably 0.35 to 1.3wt%; the phosphorus content is 0.3 to 1.0wt%, more preferably 0.5 to 0.9wt%.

[0039] Embodiment 1:

[0040] In a 500ml four-necked glass bottle, add 150.0g of polyisobutylene succinic anhydride (PIB number average molecular weight 1300, degree of substitution 1.1-1.2) and 149.4g of 150N hydrogenated base oil, stir and heat to 70-80°C, add 15.9g of polyethylene polyamine, slowly heat to 150-160°C, pass nitrogen to purge for 2 hours, blow away the water generated by the reaction, and obtain polyisobutylene succinimide ashless dispersant.

[0041] Example 2

[0042] In a 500ml four-necked glass bottle, add 200.0g of the product of Example 1, 11.0g of boric acid, 12.0g of 1-naphthylphosphoric acid, and 18.0g of isobutanol, stir and slowly heat to 95-105°C, keep warm for 3 hours, then introduce nitrogen, slowly heat to 150-160°C, keep warm for 3 hours, and obtain a reaction product-phosphorus boronized ashless dispersant. After testing, the reaction product has a nitrogen content of 1.55wt%, a boron content of 0.79wt%, and a phosphorus content of 0.72wt%.

[0043] Example 3

[0044] In a 500ml four-necked glass bottle, add 150.0g of polyisobutylene succinic anhydride (PIB number average molecular weight 1300, degree of substitution 1.1-1.2) and 151.4g of 150N hydrogenated base oil, stir and heat to 70-80°C, add 18.2g of polyethylene polyamine, slowly heat to 150-160°C, pass nitrogen to purge for 2 hours, blow away the water generated by the reaction, and obtain polyisobutylene succinimide ashless dispersant.

[0045] Example 4

[0046] In a 500ml four-necked glass bottle, add 200.0g of the product of Example 3, 14.5g of boric acid, 14.5g of 1-naphthylphosphoric acid, and 25.0g of isobutanol, stir and slowly heat to 95-105°C, keep warm for 3 hours, then introduce nitrogen, slowly heat to 150-160°C, keep warm for 4 hours, and obtain the reaction product-phosphorus boronized ashless dispersant. After testing, the reaction product has a nitrogen content of 1.72wt%, a boron content of 1.03wt%, and a phosphorus content of 0.80wt%.

[0047] Embodiment 5:

[0048] In a 500ml four-necked glass bottle, add 150.0g of polyisobutylene succinic anhydride (PIB number average molecular weight 1300, degree of substitution 1.1-1.2) and 146.5g of 150N hydrogenated base oil, stir and heat to 70-80°C, add 12.8g of polyethylene polyamine, slowly heat to 150-160°C, pass nitrogen to purge for 2 hours, blow away the water generated by the reaction, and obtain polyisobutylene succinimide ashless dispersant.

[0049] Example 6

[0050] In a 500ml four-necked glass bottle, add 200.0g of the product of Example 5, 5.3g of boric acid, 8g of 1-naphthylphosphoric acid, and 7.0g of n-propanol, stir and slowly heat to 95-105°C, keep warm for 2 hours, then introduce nitrogen, slowly heat to 150-160°C, keep warm for 2 hours, and obtain the reaction product-phosphorus boronized ashless dispersant. After testing, the reaction product has a nitrogen content of 1.30wt%, a boron content of 0.42wt%, and a phosphorus content of 0.48wt%.

[0051] Example 7

[0052] In a 500ml four-necked glass bottle, add 150.0g of polyisobutylene succinic anhydride (PIB number average molecular weight 1000, degree of substitution 1.1-1.2) and 151.3g of 150N hydrogenated base oil, stir and heat to 70-80°C, add 18.6g of tetraethylene pentamine, slowly heat to 150-160°C, pass nitrogen to purge for 2 hours, blow away the water generated by the reaction, and obtain polyisobutylene succinimide ashless dispersant.

[0053] Example 8

[0054] In a 500ml four-necked glass bottle, add 200.0g of the product of Example 7, 17.0g of boric acid, 10.0g of phenyl phosphoric acid, and 27.0g of n-butanol, stir and slowly heat to 105-115°C, keep warm for 3 hours, then introduce nitrogen, slowly heat to 150-160°C, keep warm for 4.5 hours, and obtain the reaction product-phosphorus boronized ashless dispersant. After testing, the reaction product has a nitrogen content of 1.69wt%, a boron content of 1.28wt%, and a phosphorus content of 0.81wt%.

[0055] Example 9

[0056] In a 500ml four-necked glass bottle, add 150.0g of polyisobutylene succinic anhydride (PIB number average molecular weight 1000, degree of substitution 1.1-1.2) and 148.5g of 150N hydrogenated base oil, stir and heat to 70-80°C, add 15.5g of tetraethylene pentamine, slowly heat to 150-160°C, pass nitrogen to purge for 2 hours, blow away the water generated by the reaction, and obtain polyisobutylene succinimide ashless dispersant.

[0057] Example 10

[0058] In a 500ml four-necked glass bottle, add 200.0g of the product of Example 9, 12.5g of boric acid, 8.0g of phenylphosphoric acid, and 16.5g of isobutanol, stir and slowly heat to 95-105°C, keep warm for 3 hours, then introduce nitrogen, slowly heat to 150-160°C, keep warm for 3 hours, and obtain the reaction product-phosphorus boronized ashless dispersant. After testing, the reaction product has a nitrogen content of 1.45wt%, a boron content of 0.94wt%, and a phosphorus content of 0.69wt%.

[0059] Embodiment 11

[0060] In a 500ml four-necked glass bottle, add 150.0g of polyisobutylene succinic anhydride (PIB number average molecular weight 1000, degree of substitution 1.1-1.2) and 147.1g of 150N hydrogenated base oil, stir and heat to 70-80°C, add 13.9g of tetraethylene pentamine, slowly heat to 150-160°C, pass nitrogen to purge for 2 hours, blow away the water generated by the reaction, and obtain polyisobutylene succinimide ashless dispersant.

[0061] Example 12

[0062] In a 500ml four-necked glass bottle, add 200.0g of the product of Example 11, 7.0g of boric acid, 6.0g of phenylphosphoric acid, and 6.5g of isobutanol, stir and slowly heat to 95-105°C, keep warm for 3 hours, then introduce nitrogen, slowly heat to 150-160°C, keep warm for 3 hours, and obtain the reaction product-phosphorus boronized ashless dispersant. After testing, the reaction product has a nitrogen content of 1.38wt%, a boron content of 0.50wt%, and a phosphorus content of 0.50wt%.

[0063] Comparative Example 1:

[0064] In a 500ml four-necked glass bottle, add 200.0g of the product of Example 3, 13.8g of boric acid, 4.4g of phosphorus pentoxide, and 16.4g of isobutanol, stir and slowly heat to 95-105°C, keep warm for 3 hours, then introduce nitrogen, slowly heat to 150-160°C, keep warm for 4 hours to obtain a reaction product. After testing, the reaction product has a nitrogen content of 1.79wt%, a boron content of 1.02wt%, and a phosphorus content of 0.82wt%.

[0065] Comparative Example 2

[0066] In a 500ml four-necked glass bottle, add 200.0g of the product of Example 7, 16.5g of boric acid, 4.4g of phosphorus pentoxide, and 21.0g of n-butanol, stir and slowly heat to 105-115°C, keep warm for 3 hours, then introduce nitrogen, slowly heat to 150-160°C, keep warm for 4.5 hours to obtain a reaction product. After testing, the reaction product has a nitrogen content of 1.70wt%, a boron content of 1.25wt%, and a phosphorus content of 0.83wt%.

[0067] test:

[0068] The final products obtained from the above 12 embodiments and 2 comparative examples were evaluated for their low-temperature sludge dispersibility according to the industry standard (SH / T0623 Appendix A Ashless Dispersant Low-Temperature Dispersibility Evaluation Method); during the analysis and evaluation process, the additives used were the same; the evaluation results are shown in Table 1.

[0069] Table 1

[0070]

[0071]

[0072] According to the sludge dispersibility evaluation data in Table 1 (the higher the dispersion index, the better the sludge dispersibility), it can be seen that the new boron phosphide ashless dispersants prepared in the embodiments of the present invention (Example 2, Example 4, Example 6, Example 8, Example 10, Example 12) are compared with the corresponding traditional ashless dispersants (Example 1, Example 3, Example 5, Example 7, Example 9, Example 11), and the sludge dispersibility is equivalent, that is, within ±0.5; the traditional boron phosphide ashless dispersants (Comparative Example 1, Comparative Example 2) are compared with the corresponding traditional ashless dispersants (Example 3, Example 7), and the sludge dispersibility is equivalent; the new boron phosphide ashless dispersants (Example 4, Example 8) with equivalent nitrogen, boron and phosphorus contents are compared with the traditional boron phosphide ashless dispersants (Comparative Example 1, Comparative Example 2), and the sludge dispersibility is also equivalent.

[0073] The final products obtained from the above 12 examples and 2 comparative examples were added into the engine bench test used oil at a dosage of 1.0wt%. The soot content in the oil was 5.5wt% according to TGA analysis, and the kinematic viscosity at 100℃ was 49.65mm 2 / s. After the old oil with added dispersant was stirred at 100℃ for 2 hours, the kinematic viscosity at 100℃ was tested and the viscosity reduction rate was calculated. The lower the kinematic viscosity and the greater the reduction rate, the stronger the ability of the added dispersant to prevent the oil from thickening and the better the soot dispersion performance. The test results are shown in Table 2.

[0074] Table 2

[0075]

[0076]

[0077] According to the soot dispersibility evaluation data in Table 2, the traditional phosphoborated ashless dispersants (Comparative Example 1 and Comparative Example 2) have significantly lower dispersibility than the traditional ashless dispersants (corresponding to Example 3 and Example 7, respectively) due to the use of inorganic phosphorus-containing compounds as phosphating agents; and the use of phosphoric acid compounds containing aromatic groups as phosphating agents, the obtained new phosphoborated ashless dispersants (Example 2, Example 4, Example 6, Example 8, Example 10, Example 12) have significantly improved dispersibility than the traditional ashless dispersants (corresponding to Example 1, Example 3, Example 5, Example 7, Example 9, Example 11, respectively).

[0078] The final products obtained from the 12 embodiments and 2 comparative examples were evaluated for anti-wear performance according to the industry standard (SH / T0189-2017 Lubricant Anti-wear Performance Determination Method-Four-Ball Method). During the analysis and evaluation process, the amount of additives used was the same; the smaller the wear spot diameter, the better the anti-wear performance; the evaluation results are shown in Table 3. The final products obtained from the 12 embodiments and 2 comparative examples were evaluated for extreme pressure performance according to the industry standard (GB / T3142-2019 Lubricant Load Capacity Determination Method-Four-Ball Method). During the analysis and evaluation process, the amount of additives used was the same; the evaluation results are shown in Table 3.

[0079] Table 3

[0080]

[0081] It can be seen from the evaluation data in Table 3 that the new phosphoborated ashless dispersants prepared in the embodiments of the present invention (Example 2, Example 4, Example 6, Example 8, Example 10, Example 12) are significantly better in anti-wear performance than the traditional ashless dispersants (Example 1, Example 3, Example 5, Example 7, Example 9, Example 11) that have not been phosphoborated. The new phosphoborated ashless dispersants (Example 4, Example 8) obtained using phosphate compounds containing aromatic groups have equivalent anti-wear properties to the traditional phosphoborated ashless dispersants (Comparative Example 1, Comparative Example 2) obtained using inorganic phosphorus-containing compounds, and both have good anti-wear effects.

[0082] It can be seen from the evaluation data in Table 3 that the maximum no-seizure load and sintering load of the new boronized ashless dispersants prepared in the embodiments of the present invention (Example 2, Example 4, Example 6, Example 8, Example 10, Example 12) are significantly improved compared with the traditional ashless dispersants (Example 1, Example 3, Example 5, Example 7, Example 9, Example 11); the maximum no-seizure load and sintering load of the new boronized ashless dispersants (Example 4, Example 8) obtained by using aromatic group-containing phosphoric acid compounds are equivalent to the maximum no-seizure load and sintering load of the traditional boronized ashless dispersants (Comparative Example 1, Comparative Example 2) obtained by using inorganic phosphorus-containing compounds. The developed new boronized ashless dispersants have the same extreme pressure performance as the traditional boronized ashless dispersants, and both have good extreme pressure performance.

[0083] in conclusion:

[0084] The present invention uses a phosphoric acid compound containing an aromatic group to replace the traditional inorganic phosphorus-containing reagent and a phosphate ester compound as the phosphorus-containing reagent. The obtained new boronized phosphorus ashless dispersant is still equivalent to the traditional boronized phosphorus ashless dispersant in terms of anti-wear performance and extreme pressure performance; and the introduction of the aromatic group gives the boronized phosphorus ashless dispersant a more excellent soot dispersibility. In application, the new boronized phosphorus ashless dispersant can simultaneously exhibit excellent soot dispersibility, good anti-wear performance, and extreme pressure performance, and can better meet the requirements of high-specification internal combustion engine oils for dispersibility and anti-wear performance.

[0085] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. A method for preparing an anti-wear soot dispersant, characterized in that: include: Preparation of polyisobutylene succinimide; Under the action of a promoter, polyisobutylene succinimide, boric acid and aromatic phosphoric acid are reacted to obtain a boronized ashless dispersant.

2. The method for preparing the anti-wear soot dispersant according to claim 1, characterized in that: The accelerator comprises one or more of water, ethanol, isobutanol, n-butanol, isopropanol and n-propanol, and the amount of the accelerator is 30% to 150% of the total mass of the boric acid and the aromatic phosphoric acid.

3. The method for preparing the anti-wear soot dispersant according to claim 2, characterized in that: The amount of the accelerator used is 50% to 110% of the total mass of the boric acid and the aromatic phosphoric acid.

4. The method for preparing the anti-wear soot dispersant according to claim 1, characterized in that: The aromatic phosphoric acid is a phosphoric acid compound containing an aromatic group, which is composed of a phosphorus atom and an aromatic ring directly connected, and includes one or more of phenylphosphonic acid, p-methylphenylphosphonic acid, m-methylphenylphosphonic acid, and 1-naphthylphosphonic acid.

5. The method for preparing the anti-wear soot dispersant according to claim 1, characterized in that: The boron content of the prepared boronized ashless dispersant is 0.3-1.5wt%, and the phosphorus content is 0.3-1.0wt%.

6. The method for preparing the anti-wear soot dispersant according to claim 1, characterized in that: The reaction conditions for the reaction of polyisobutylene succinimide, boric acid and aromatic phosphoric acid are: First react at 70-120°C for 2-8h, then heat to 150-160°C, introduce nitrogen to purge and react for 1.5-5h to obtain a boron phosphide ashless dispersant.

7. The method for preparing the anti-wear soot dispersant according to claim 1, characterized in that: The preparation method of the polyisobutylene succinimide comprises: The polyisobutylene succinic anhydride is reacted with polyene polyamine to obtain polyisobutylene succinimide.

8. The method for preparing the anti-wear soot dispersant according to claim 7, characterized in that: The preparation method of the polyisobutylene succinimide specifically comprises: After polyisobutylene succinic anhydride is mixed and diluted with base oil, polyethylene polyamine is added dropwise at 60-120° C., and then nitrogen is introduced, and the temperature is raised to 150-160° C. for reaction for 1-3 hours (preferably 2 hours) to obtain polyisobutylene succinimide.

9. The method for preparing the anti-wear soot dispersant according to claim 7 or 8, characterized in that: The average molecular weight of the polyisobutylene succinic anhydride is 500-5000, and the degree of substitution is 1.1-1.

2.

10. The method for preparing the anti-wear soot dispersant according to claim 7 or 8, characterized in that: The polyene polyamine includes one or more of diethylenetriamine, triethylenetetramine, tetraethylenepentamine and heavy polyethylene polyamine. The molar ratio of the polyisobutylene succinic anhydride to the polyethylene polyamine is 1.3:1 to 3:1.

Citation Information

Cited By

  • Polyisobutylene succinimide dispersing agent as well as preparation method and application thereof

    CN122344284A