Flexible dual-mode sensor and manufacturing method thereof
By using a hollow structure flexible substrate layer and PVDF copolymer piezoelectric layer in a flexible piezoelectric/pyroelectric dual-mode sensor, combined with the etching technology of the indium tin oxide layer, the problems of complexity of sensor layout and poor breathability are solved. It achieves efficient production and both piezoelectric and pyroelectric effects.
Patent Information
- Application Number
- CN202410813911.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-21
- Publication Date
- 2024-11-01
AI Technical Summary
Existing flexible piezoelectric/pyroelectric dual-mode sensors are complex and have poor breathability when arranging sensing pixel points, making it difficult to reduce layout difficulty and simplify the production process.
A combined structure of a flexible substrate layer, a PVDF copolymer piezoelectric layer and an indium tin oxide layer is adopted to form a hollow array area through etching technology to ensure the breathability of each layer of the sensor and simplify the production process.
It realizes the improvement of the air permeability of the sensor and the simplification of the production process, reduces the difficulty of arranging pixel points, and ensures the combination of piezoelectric and pyroelectric effects of the sensor.
Smart Images

Figure CN118882871A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of sensors, and in particular to a flexible dual-mode sensor and a manufacturing method thereof. Background Art
[0002] In recent years, thanks to the progress of flexible material science, the in-depth application of piezoelectric technology, and the continuous improvement of micro-nano processing and electronic technology, flexible piezoelectric sensor arrays have shown broad application prospects in biomedicine, robot tactile perception, wearable devices, smart homes and other fields.
[0003] Compared with traditional silicon-based MEMS pressure sensors, flexible piezoelectric / pyroelectric dual-mode sensors have lower system dependence and stronger adaptability. However, the sensing pixels in the current flexible piezoelectric / pyroelectric dual-mode sensors are divided into two types: piezoelectric pixels and temperature pixels. The process of arranging the sensing pixels is relatively complicated, and the manufactured dual-mode sensors have poor air permeability.
[0004] Therefore, how to reduce the difficulty of arranging sensor pixels while ensuring the air permeability of dual-mode sensors and simplify the manufacturing process has become a technical problem that the industry urgently needs to solve. Summary of the invention
[0005] The present invention provides a flexible dual-mode sensor and a manufacturing method thereof, which solves the technical problem of how to reduce the difficulty of arranging sensing pixels while ensuring the air permeability of the dual-mode sensor and having a simple manufacturing process.
[0006] According to a first aspect of the present invention, there is provided a flexible dual-mode sensor, comprising:
[0007] A flexible substrate layer, the flexible substrate layer comprising an array area and a lead-out area adjacent to the array area, the array area comprising a plurality of sensing areas arranged in an array and separated from each other, and an interconnection area connected between adjacent sensing areas, with gaps between adjacent interconnection areas, and the interconnection area being a straight line parallel to the central axis of the surface of the flexible substrate layer;
[0008] a lower electrode located on the flexible substrate layer, the lower electrode comprising a plurality of first electrode portions arranged in an array and separated from each other, and first interconnection lines connected between adjacent first electrode portions along a first direction, the first electrode portions having a first projection pattern on the surface of the flexible substrate layer, the first projection pattern overlapping the sensing area, the first interconnection line having a second projection pattern on the surface of the flexible substrate layer, the second projection pattern partially overlapping the lead-out area;
[0009] A PVDF copolymer piezoelectric layer located on the lower electrode, the PVDF copolymer piezoelectric layer comprising a piezoelectric array area and a piezoelectric lead-out area adjacent to the piezoelectric array area, the piezoelectric array area having a third projection pattern on the surface of the flexible substrate layer, the third projection pattern overlapping the sensing area, the piezoelectric lead-out area having a fourth projection pattern on the surface of the flexible substrate layer, the fourth projection pattern partially overlapping the lead-out area;
[0010] an upper electrode located on the PVDF copolymer piezoelectric layer, the upper electrode comprising a plurality of second electrode portions arranged in an array and separated from each other, and second interconnecting lines connected between adjacent second electrode portions along a second direction, the second electrode portions having a fifth projection pattern on the surface of the flexible substrate layer, the fifth projection pattern overlapping the sensing area, the second interconnecting lines having a sixth projection pattern on the surface of the flexible substrate layer, the sixth projection pattern partially overlapping the lead-out area;
[0011] The encapsulation layer is located on the upper electrode, and an eighth projection pattern of the encapsulation layer on the surface of the flexible substrate layer overlaps with the flexible substrate layer.
[0012] Optionally, the first direction and the second direction are perpendicular to each other.
[0013] Optionally, the flexible substrate layer includes a flexible base and a buffer layer located on the flexible base.
[0014] Optionally, the materials of the upper electrode and the lower electrode are both composite electrodes of metal material and indium tin oxide.
[0015] According to a second aspect of the present invention, there is provided a method for manufacturing a flexible dual-mode sensor, comprising:
[0016] providing a first substrate;
[0017] forming a flexible substrate layer on the first substrate, wherein the flexible substrate layer comprises an array area and a lead-out area adjacent to the array area;
[0018] forming a first patterned lower electrode on the flexible substrate layer, wherein the lower electrode comprises a plurality of first electrode portions arranged in an array and separated from each other, and first interconnecting lines connected between adjacent first electrode portions along a first direction;
[0019] forming a PVDF copolymer piezoelectric layer on the lower electrode, wherein the PVDF copolymer piezoelectric layer comprises a piezoelectric array region and a piezoelectric lead-out region adjacent to the piezoelectric array region;
[0020] forming a second patterned upper electrode on the PVDF copolymer piezoelectric layer, wherein the upper electrode comprises a plurality of second electrode portions arranged in an array and separated from each other, and second interconnecting lines connected between adjacent second electrode portions along a second direction;
[0021] forming an insulating layer and a third patterned indium tin oxide layer in sequence on the upper electrode;
[0022] Using the indium tin oxide layer as a mask, the insulating layer, the PVDF copolymer piezoelectric layer and the flexible substrate layer are etched until the surface of the first substrate, so that the array area includes a plurality of sensing areas arranged in an array and separated from each other, and an interconnection area connected between adjacent sensing areas, and there is a gap between adjacent interconnection areas, and the interconnection area is a straight line parallel to the central axis of the surface of the flexible substrate layer; the first projection pattern of the first electrode part on the surface of the flexible substrate layer overlaps with the sensing area, and the second projection pattern of the first interconnection line on the surface of the flexible substrate layer overlaps partially with the lead-out area; the third projection pattern of the piezoelectric array area on the surface of the flexible substrate layer overlaps with the sensing area, and the fourth projection pattern of the piezoelectric lead-out area on the surface of the flexible substrate layer overlaps partially with the lead-out area; the fifth projection pattern of the second electrode part on the surface of the flexible substrate layer overlaps with the sensing area, and the sixth projection pattern of the second interconnection line on the surface of the flexible substrate layer overlaps partially with the lead-out area;
[0023] removing the insulating layer and the indium tin oxide layer;
[0024] forming a packaging layer on the upper electrode, wherein an eighth projection pattern of the packaging layer on the surface of the flexible substrate layer overlaps with the flexible substrate layer;
[0025] The first substrate is removed.
[0026] Optionally, forming a flexible substrate layer on the first substrate includes:
[0027] spin coating a flexible solution on the substrate;
[0028] After spin coating the flexible solution, annealing the flexible solution to obtain a flexible substrate;
[0029] A buffer layer is deposited on the flexible substrate to form the flexible substrate layer.
[0030] Optionally, a pattern of a first patterned mask for forming a first patterned lower electrode is perpendicular to a pattern of a second patterned mask for forming a second patterned lower electrode.
[0031] Optionally, an insulating layer and a third patterned indium tin oxide layer are sequentially formed on the upper electrode, comprising:
[0032] depositing the insulating layer on the upper electrode;
[0033] forming the indium tin oxide layer on the insulating layer by a magnetron sputtering process;
[0034] The indium tin oxide layer is photolithographically processed using a third patterned mask to form the third patterned indium tin oxide layer.
[0035] Optionally, using the insulating indium tin oxide layer as a mask, etching the PVDF copolymer piezoelectric layer and the flexible substrate layer until the surface of the first substrate comprises:
[0036] Using the third patterned indium tin oxide layer as a mask, the insulating layer, the PVDF copolymer piezoelectric layer and the flexible substrate layer are etched in sequence until the surface of the first substrate is reached.
[0037] Optionally, forming a packaging layer on the insulating layer and the indium tin oxide layer includes:
[0038] providing a second substrate;
[0039] forming a second flexible substrate layer on the second substrate;
[0040] depositing a second indium tin oxide layer on the second flexible substrate layer;
[0041] Using a patterned mask, photolithography is performed on the second indium tin oxide layer to form a fourth patterned second indium tin oxide layer on the second flexible substrate layer;
[0042] Using the fourth patterned second indium tin oxide layer as a mask, etching the second flexible substrate layer;
[0043] removing the fourth patterned second indium tin oxide layer and the second substrate to obtain the encapsulation layer;
[0044] The encapsulation layer is adhered to the surface of the upper electrode.
[0045] Compared with the prior art, the technical solution of the embodiment of the present invention has the following beneficial effects:
[0046] In the flexible dual-mode sensor of the technical solution of the present invention, the flexible substrate layer includes an array area and a lead-out area adjacent to the array area, the array area includes a plurality of sensing areas and interconnection areas, the interconnection area is a straight line and there is a gap between adjacent interconnection areas; the first electrode portion of the lower electrode overlaps with the pattern of the sensing area, and the first interconnection line overlaps with part of the pattern of the lead-out area; the piezoelectric array area of the PVDF copolymer piezoelectric layer overlaps with the pattern of the sensing area, and the piezoelectric lead-out area overlaps with part of the pattern of the lead-out area, and the PVDF copolymer material has both piezoelectric effect and pyroelectric effect, and there is no need to design the type of each pixel point in the piezoelectric array area; the second electrode portion of the upper electrode overlaps with the pattern of the sensing area, and the second interconnection line overlaps with part of the pattern of the lead-out area; the packaging layer overlaps with the pattern of the flexible substrate layer. Therefore, the present invention ensures the air permeability of the sensor by ensuring that each layer corresponding to the array area of the sensor is hollow.
[0047] In the manufacturing method of the flexible dual-mode sensor of the technical solution of the present invention, a flexible substrate layer is formed on a first substrate, a first patterned lower electrode is formed on the flexible substrate layer, a PVDF copolymer piezoelectric layer is formed on the lower electrode, a second patterned upper electrode is formed on the PVDF copolymer piezoelectric layer, an insulating layer and a third patterned indium tin oxide layer are sequentially formed on the upper electrode, and the indium tin oxide layer is used as a mask to etch the insulating layer, the flexible piezoelectric layer and the flexible substrate layer until the surface of the substrate, thereby ensuring that each layer corresponding to the sensor array area is hollowed out through two etchings, the manufacturing process is relatively simple, and the insulating layer and the indium tin oxide layer are subsequently removed. Each pixel point in the piezoelectric array area has both piezoelectric effect and pyroelectric effect, and a packaging layer is formed on the upper electrode. The eighth projection pattern of the packaging layer projected on the flexible substrate layer is the same as the flexible substrate layer, ensuring that each layer of the flexible dual-mode sensor is hollowed out and the air permeability of the sensor is ensured. BRIEF DESCRIPTION OF THE DRAWINGS
[0048] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0049] Figure 1 It is a schematic diagram of the device structure of the piezoelectric array area of the flexible dual-mode sensor in the prior art;
[0050] Figure 2 to Figure 23 This is a schematic diagram of a device structure formed by the main steps of manufacturing a flexible dual-mode sensor provided by an embodiment of the present invention;
[0051] Fig.24 is a disassembled diagram of each layer of a flexible dual-mode sensor provided by an embodiment of the present invention;
[0052] Description of reference numerals:
[0053] 10- a first substrate;
[0054] 20- flexible substrate layer;
[0055] 201- flexible substrate;
[0056] 202- buffer layer;
[0057] 30-lower electrode;
[0058] 301- first electrode portion;
[0059] 302-first interconnection line;
[0060] 31-a first patterned mask layer;
[0061] 40-PVDF copolymer piezoelectric layer;
[0062] 50-upper electrode;
[0063] 501- second electrode portion;
[0064] 502-second interconnection line;
[0065] 51-a second patterned mask layer;
[0066] 601-insulation layer;
[0067] 602-indium tin oxide layer;
[0068] 70- second substrate;
[0069] 80-a second flexible substrate layer;
[0070] 801-encapsulation layer;
[0071] 90-Second indium tin oxide layer. DETAILED DESCRIPTION
[0072] As described in the background art, how to reduce the difficulty of arranging sensor pixels while ensuring the air permeability of dual-mode sensors and simplifying the manufacturing process has become a technical problem that the industry urgently needs to solve. The following will be described in detail with reference to the accompanying drawings.
[0073] Before filing this application, the applicant has conducted a thorough study on the device structure and manufacturing method of the current flexible piezoelectric sensor.
[0074] The flexible dual-mode sensor is a new type of sensor that integrates piezoelectric effect and pyroelectric effect. Thanks to the complementary advantages of these two effects, the sensor can not only sense mechanical stress, but also temperature changes, thereby significantly improving its sensitivity and applicable scenarios. For example, in smart health monitoring, the dual-mode sensor can simultaneously monitor mechanical stress (such as pulse) and temperature changes (such as body temperature), providing more comprehensive data support for health monitoring.
[0075] Compared with traditional silicon-based MEMS pressure sensors, flexible piezoelectric / pyroelectric dual-mode sensors have lower system dependence and stronger adaptability. This is because traditional silicon-based sensors need to measure the change in the distance between the panel and the fixed position to measure the pressure, while flexible piezoelectric / pyroelectric dual-mode sensors do not require such tight support and can maintain stable performance under structural changes and external interference. Therefore, flexible piezoelectric / pyroelectric dual-mode sensors have lower requirements on the structure of other components of the system and the internal space structure when deployed, which makes them have greater advantages in applications such as folding screen devices and wearable devices with small internal space.
[0076] Existing flexible piezoelectric sensors are generally sandwich sensors, and the device structure is roughly substrate layer-lower electrode-piezoelectric layer-upper electrode-packaging layer. The manufacturing steps include using inkjet printing conductive paths, laser engraving substrates, preparing through holes, pouring conductive silver paste, and patch-mounting piezoelectric and temperature units to form a sandwich sensor structure.
[0077] The sensing pixels in dual-mode sensors are generally divided into two types: piezoelectric pixels and temperature pixels. Please refer to Figure 1 , Figure 1 The distribution diagram of sensing pixels in the flexible piezoelectric / pyroelectric dual-mode sensor is shown. Figure 1 In the figure, black island-shaped components (such as islands I(x1, y5), I(x2, y3), I(x3, y2), I(x3, y4), I(x4, y3), I(x5, y3)) and interconnected components indicate that the copper coating is retained on the surface of the components, and white (or hollow) island-shaped components (such as islands I(x1, y1), I(x1, y2), I(x5, y4), etc.) and interconnected components indicate that the copper coating on the surface of the components is removed. In addition, the island-shaped components with gray shades (for example, islands I(x2, y2), I(x3, y3), etc.) indicate that a waveguide signal acquisition unit or a temperature signal acquisition unit is carried on the island-shaped components. Specifically, patch type temperature sensors are respectively arranged on islands I(x1, y4), I(x3, y1), I(x3, y3), and I(x5, y2) to form an array of patch type temperature sensors; flexible piezoelectric sensors are respectively arranged on islands I(x2, y2), I(x2, y4), I(x4, y2), and I(x4, y4) to form an array of flexible piezoelectric sensors.
[0078] In actual implementation, the temperature pixel is a patch-type temperature sensor, and the piezoelectric pixel is a flexible piezoelectric sensor. Each sensing pixel requires an independent electrical connection and signal transmission path. Different levels of electrical conduction can only be achieved by preparing through holes and injecting conductive silver paste, which makes the process of preparing through holes more complicated. The placement of piezoelectric pixels and temperature pixels needs to be designed, which increases the complexity of the manufacturing process.
[0079] In addition, the packaging layer of the flexible piezoelectric sensor is usually a full-surface flexible film. Even if the substrate is laser engraved to remove unnecessary parts, when the sensor is attached to the human body, it will still be airtight, affecting comfort and use effect.
[0080] In order to solve the above problems, an embodiment of the present invention provides a method for manufacturing a flexible dual-mode sensor, comprising:
[0081] providing a first substrate;
[0082] forming a flexible substrate layer on the first substrate, wherein the flexible substrate layer comprises an array area and a lead-out area adjacent to the array area;
[0083] forming a first patterned lower electrode on the flexible substrate layer, wherein the lower electrode comprises a plurality of first electrode portions arranged in an array and separated from each other, and first interconnecting lines connected between adjacent first electrode portions along a first direction;
[0084] forming a PVDF copolymer piezoelectric layer on the lower electrode, wherein the PVDF copolymer piezoelectric layer comprises a piezoelectric array region and a piezoelectric lead-out region adjacent to the piezoelectric array region;
[0085] forming a second patterned upper electrode on the PVDF copolymer piezoelectric layer, wherein the upper electrode comprises a plurality of second electrode portions arranged in an array and separated from each other, and second interconnecting lines connected between adjacent second electrode portions along a second direction;
[0086] forming an insulating layer and a third patterned indium tin oxide layer in sequence on the upper electrode;
[0087] Using the indium tin oxide layer as a mask, the insulating layer, the PVDF copolymer piezoelectric layer and the flexible substrate layer are etched until the surface of the first substrate, so that the array area includes a plurality of sensing areas arranged in an array and separated from each other, and an interconnection area connected between adjacent sensing areas, and there is a gap between adjacent interconnection areas, and the interconnection area is a straight line parallel to the central axis of the surface of the flexible substrate layer; the first projection pattern of the first electrode part on the surface of the flexible substrate layer overlaps with the sensing area, and the second projection pattern of the first interconnection line on the surface of the flexible substrate layer overlaps partially with the lead-out area; the third projection pattern of the piezoelectric array area on the surface of the flexible substrate layer overlaps with the sensing area, and the fourth projection pattern of the piezoelectric lead-out area on the surface of the flexible substrate layer overlaps partially with the lead-out area; the fifth projection pattern of the second electrode part on the surface of the flexible substrate layer overlaps with the sensing area, and the sixth projection pattern of the second interconnection line on the surface of the flexible substrate layer overlaps partially with the lead-out area;
[0088] removing the insulating layer and the indium tin oxide layer;
[0089] forming a packaging layer on the upper electrode, wherein an eighth projection pattern of the packaging layer on the surface of the flexible substrate layer overlaps with the flexible substrate layer;
[0090] The first substrate is removed.
[0091] Thus, the manufacturing method provided by the present invention forms a flexible substrate layer on a first substrate, forms a first patterned lower electrode on the flexible substrate layer, forms a PVDF copolymer piezoelectric layer on the lower electrode, forms a second patterned upper electrode on the PVDF copolymer piezoelectric layer, forms an insulating layer and a third patterned indium tin oxide layer on the upper electrode in sequence, uses the indium tin oxide layer as a mask, etches the insulating layer, the flexible piezoelectric layer and the flexible substrate layer until the surface of the substrate, thereby ensuring that each layer corresponding to the sensor array area is hollowed out through two etchings, the manufacturing process is relatively simple, and the insulating layer and the indium tin oxide layer are subsequently removed. Each pixel point in the piezoelectric array area has both piezoelectric effect and pyroelectric effect, taking into account the advantage of being more convenient in arranging pixel points; forming a packaging layer on the upper electrode, the eighth projection pattern of the packaging layer projected on the flexible substrate layer is the same as the flexible substrate layer, ensuring that each layer of the flexible dual-mode sensor is hollowed out, and ensuring the air permeability of the sensor.
[0092] Figures 2 to 22 It is a structural schematic diagram of the flexible dual-mode sensor during the manufacturing process of an embodiment of the present invention.
[0093] Please refer to Figure 2 , providing a first substrate 10.
[0094] As an example, the first substrate 10 may be a glass substrate. Of course, the present invention is not limited to this. Of course, it may also be a metal substrate, a plastic substrate, etc. Those skilled in the art may select a suitable substrate material as needed.
[0095] Taking the example that the first substrate 10 can be a glass substrate, in actual work, before preparing subsequent processes on the first substrate 10, the glass substrate needs to be placed in a cleaning machine for water washing and water droplets are blown away.
[0096] In this embodiment, a flexible substrate layer 20 is subsequently formed on the first substrate 10. The flexible substrate layer 20 includes an array area and a lead-out area adjacent to the array area. For the process of forming the flexible substrate layer 20, please refer to Figure 3 to Figure 4 .
[0097] Please refer to Figure 3 , spin coating a flexible solution on the first substrate 10 ; after spin coating the flexible solution, annealing the flexible solution to obtain a flexible substrate 201 .
[0098] In a specific embodiment, the flexible solution is a polyimide solution. In this case, the flexible solution is subjected to an annealing treatment, comprising:
[0099] The polyimide solution is subjected to low temperature annealing treatment and high temperature annealing treatment in sequence to form a polyimide substrate;
[0100] In a preferred embodiment, after the polyimide solution is annealed, the method further comprises:
[0101] The polyimide substrate is subjected to ultraviolet light curing treatment.
[0102] In other embodiments, the flexible solution may also be a polyurethane (PU) solution, a polydimethylsiloxane (PDMS) solution, etc., and the present invention is not limited thereto.
[0103] Please refer to Figure 4 , a buffer layer 202 is deposited on the flexible substrate 201 to form the flexible substrate layer 20 .
[0104] In one embodiment, a buffer layer 202 is deposited on the flexible substrate 201 by a chemical vapor deposition process. As an example, the buffer layer 202 may be composed of silicon nitride and silicon dioxide, or may be replaced by silicon nitride or silicon dioxide alone. Of course, those skilled in the art may select a suitable material for the buffer layer 202 according to specific process requirements and conditions.
[0105] In this embodiment, a first patterned lower electrode is subsequently formed on the flexible substrate layer 20, wherein the lower electrode includes a plurality of first electrode portions arranged in an array and separated from each other, and first interconnects connected between adjacent first electrode portions along a first direction; the process of forming the lower electrode is described in detail in detail in the following. Figures 5 to 7 .
[0106] Please refer to Figure 5 , the lower electrode 30 is deposited on the flexible substrate layer 20 .
[0107] In a specific implementation manner, the lower electrode 30 is deposited on the flexible substrate layer 20 by a magnetron sputtering process. For example, the lower electrode 30 is a composite electrode of molybdenum and indium tin oxide. In this case, the method of depositing the lower electrode 30 on the flexible substrate layer 20 includes:
[0108] Depositing a molybdenum electrode layer on the flexible substrate layer 20 by a magnetron sputtering process;
[0109] An indium tin oxide electrode layer is deposited on the aluminum electrode layer by a magnetron sputtering process.
[0110] As an example, the thickness of the molybdenum electrode layer may be 150 nm, and the thickness of the indium tin oxide electrode layer may be 100 nm.
[0111] Of course, the present invention does not limit the electrode material of the lower electrode 30. For example, the aluminum electrode layer can be replaced by a metal material, such as aluminum, titanium, and the like.
[0112] Please refer to Figure 6 , based on the first patterned mask, a first patterned mask layer 31 is formed on the lower electrode 30 .
[0113] In a specific embodiment, the method of forming the first patterned mask layer 31 includes:
[0114] A photoresist is coated on the exposed lower electrode 30 , and the photoresist is exposed and developed to form a patterned photoresist.
[0115] In a preferred embodiment, when designing the mask layer, if an array area includes multiple arrays, the electrode patterns of each array are evenly oriented toward the four sides of the substrate as much as possible to facilitate subsequent scraping and spin coating photoresist processes.
[0116] Please refer to Figure 7, using the first patterned mask layer 31 as a mask, etching the lower electrode 30 to form a first patterned lower electrode 30, wherein the lower electrode 30 includes a plurality of first electrode portions 301 arranged in an array and separated from each other, and first interconnection lines 302 connected between adjacent first electrode portions 301 along a first direction; removing the first patterned mask layer 31.
[0117] In a specific implementation manner, the lower electrode 30 is etched by a wet etching process.
[0118] In a specific implementation, when the material of the mask layer is photoresist and the material of the piezoelectric layer in the subsequent process is polyvinylidene fluoride (PVDF copolymer), a photoresist stripping solution should be used for stripping the photoresist instead of an acetone solution.
[0119] Please refer to Figure 8 A PVDF copolymer piezoelectric layer 40 is formed on the lower electrode 30 , wherein the PVDF copolymer piezoelectric layer 40 includes a piezoelectric array region and a piezoelectric lead-out region adjacent to the piezoelectric array region.
[0120] In a specific embodiment, a PVDF copolymer piezoelectric layer 40 is formed on the lower electrode 30, comprising:
[0121] Scrape and coat the piezoelectric material on the lower electrode 30;
[0122] The piezoelectric material is polarized to form the PVDF copolymer piezoelectric layer 40 .
[0123] In a specific implementation, the polarization direction of the piezoelectric material is the Z-axis direction. Of course, the present invention is not limited to this, and those skilled in the art can select a suitable polarization direction according to application requirements.
[0124] In this embodiment, a second patterned upper electrode is subsequently formed on the PVDF copolymer piezoelectric layer, wherein the upper electrode includes a plurality of second electrode portions arranged in an array and separated from each other, and second interconnects connected between adjacent second electrode portions along a second direction; the process of forming the lower electrode is described in detail in detail in FIG. Figures 8 to 11 .
[0125] Please refer to Fig. 9 , the upper electrode 50 is deposited on the PVDF copolymer piezoelectric layer 40 .
[0126] In a specific implementation manner, the upper electrode 50 is deposited on the PVDF copolymer piezoelectric layer 40 by a magnetron sputtering process. For example, the upper electrode 50 is a composite electrode of a metal material and indium tin oxide.
[0127] Please refer to Fig.10 Based on the second patterned mask, a second patterned mask layer 51 is formed on the PVDF copolymer piezoelectric layer 40 .
[0128] Among them, the method of forming the second patterned mask layer 51 is similar to the method of forming the first patterned mask layer 31, which will not be repeated here. In actual implementation, unevenness may occur when spin coating photoresist on the PVDF copolymer piezoelectric layer 40, which can be solved by manual glue filling.
[0129] In a preferred embodiment, the pattern of the first patterned mask used to form the first patterned lower electrode 30 is perpendicular to the pattern of the second patterned mask used to form the second patterned lower electrode 30 .
[0130] Please refer to Fig.11 , using the second patterned mask layer 51 as a mask, etching the upper electrode 50 to form a second patterned upper electrode 50, wherein the upper electrode 50 includes a plurality of second electrode portions 501 arranged in an array and separated from each other, and second interconnection lines 502 connected between adjacent second electrode portions 501 along a second direction; removing the second patterned mask layer 51.
[0131] In this embodiment, an insulating layer and a third patterned indium tin oxide layer are subsequently formed on the upper electrode in sequence. For the process of forming the insulating layer and the indium tin oxide layer, please refer to Figure 12 to Figure 14 .
[0132] Please refer to Fig.12 , an insulating layer 601 is deposited on the upper electrode 50 .
[0133] In a specific implementation, the insulating layer 601 may be deposited on the patterned upper electrode 50 by a chemical vapor deposition process.
[0134] For example, the material of the insulating layer 601 can be silicon dioxide insulating layer, silicon nitride, etc. Taking the deposition of a 200nm silicon dioxide insulating layer on the patterned upper electrode 50 by chemical vapor deposition as an example, to ensure that the PVDF copolymer material can work properly, the temperature of the chemical vapor deposition process can be selected to be 80°C.
[0135] Please refer to Fig.13 , an indium tin oxide layer 602 is formed on the insulating layer 601 by a magnetron sputtering process.
[0136] In a specific implementation, the thickness of the indium tin oxide layer 602 may be 100 nm.
[0137] Please refer to Fig.14, using a third patterned mask, photolithography is performed on the indium tin oxide layer 602 to form the third patterned indium tin oxide layer 602 .
[0138] In a specific example, the indium tin oxide layer 602 is photolithographically processed to form the third patterned indium tin oxide layer 602 in a similar manner to the method of forming the first patterned mask layer 31 .
[0139] In this embodiment, the insulating layer, the PVDF copolymer piezoelectric layer and the flexible substrate layer are subsequently etched using the indium tin oxide layer as a mask until the surface of the first substrate, so that the array area includes a plurality of sensing areas arranged in an array and separated from each other, and an interconnection area connected between adjacent sensing areas, and there is a gap between adjacent interconnection areas, and the interconnection area is a straight line parallel to the central axis of the surface of the flexible substrate layer; the first projection pattern of the first electrode portion on the surface of the flexible substrate layer overlaps with the sensing area, and the second projection pattern of the first interconnection line on the surface of the flexible substrate layer partially overlaps with the lead-out area; the third projection pattern of the piezoelectric array area on the surface of the flexible substrate layer overlaps with the sensing area, and the fourth projection pattern of the piezoelectric lead-out area on the surface of the flexible substrate layer partially overlaps with the lead-out area; the fifth projection pattern of the second electrode portion on the surface of the flexible substrate layer overlaps with the sensing area, and the sixth projection pattern of the second interconnection line on the surface of the flexible substrate layer partially overlaps with the lead-out area.
[0140] Subsequent combination Fig.15 Provide explanation.
[0141] Please refer to Fig.15, using the third patterned indium tin oxide layer 602 as a mask, sequentially etching the insulating layer 601, the PVDF copolymer piezoelectric layer 40 and the flexible substrate layer 20 until the surface of the first substrate, so that the array area includes a plurality of sensing areas arranged in an array and separated from each other, and interconnection areas connected between adjacent sensing areas, and there are gaps between adjacent interconnection areas, and the interconnection area is a straight line parallel to the central axis of the surface of the flexible substrate layer 20; the first projection pattern of the first electrode portion 301 on the surface of the flexible substrate layer 20 overlaps with the sensing area, and the The first interconnection line 302 has a second projection pattern on the surface of the flexible substrate layer 20 that partially overlaps with the lead-out area; the piezoelectric array area has a third projection pattern on the surface of the flexible substrate layer 20 that overlaps with the sensing area, and the piezoelectric lead-out area has a fourth projection pattern on the surface of the flexible substrate layer 20 that partially overlaps with the lead-out area; the second electrode portion 501 has a fifth projection pattern on the surface of the flexible substrate layer 20 that overlaps with the sensing area, and the second interconnection line 502 has a sixth projection pattern on the surface of the flexible substrate layer 20 that partially overlaps with the lead-out area.
[0142] In a specific implementation manner, the insulating layer 601 , the PVDF copolymer piezoelectric layer 40 , and the flexible substrate layer 20 are sequentially etched through a dry etching process until the surface of the first substrate 10 .
[0143] It can be seen that when the hollow PVDF copolymer flexible piezoelectric / pyroelectric dual-mode array sensor of the present invention is attached to the body, the polyimide substrate is transformed from a surface shape to a hollow shape by a dry etching process, and the middle hollow part can allow air to circulate when attached, and has good air permeability.
[0144] In this embodiment, the insulating layer and the indium tin oxide layer are subsequently removed.
[0145] Subsequent combination Fig.16 Provide explanation.
[0146] Please refer to Fig.16 , and remove the indium tin oxide layer 602 and the insulating layer 601 in sequence.
[0147] In a specific implementation, the indium tin oxide layer 602 is removed by a wet etching process;
[0148] The insulating layer 601 is removed by dry etching process.
[0149] In this embodiment, a packaging layer is subsequently formed on the upper electrode, and the eighth projection pattern of the packaging layer on the surface of the flexible substrate layer overlaps with the flexible substrate layer. For the process of forming the packaging layer on the indium tin oxide layer, please refer to Figures 17 to 22 .
[0150] Please refer to Fig.17 , providing a second substrate 70.
[0151] As an example, the second substrate 70 may also be a glass substrate. Of course, the present invention is not limited to this. Of course, it may also be a metal substrate, a plastic substrate, etc. Those skilled in the art may select a suitable substrate material as needed.
[0152] Please refer to Fig.18 , a second flexible substrate layer 80 is formed on the second substrate 70 .
[0153] In a specific implementation manner, a method for forming the second flexible substrate layer 80 on the second substrate 70 is similar to a method for forming the first flexible substrate layer 20 , and will not be described in detail herein.
[0154] As an example, the material of the second flexible substrate layer 80 is also polyimide.
[0155] Please refer to Fig.19 , a second indium tin oxide layer 90 is deposited on the second flexible substrate layer 80 .
[0156] In a specific implementation manner, the second indium tin oxide layer 90 is deposited on the flexible substrate layer 20 by a magnetron sputtering process.
[0157] In actual operation, the thickness of the second indium tin oxide layer 90 may also be 100 nm.
[0158] Please refer to Fig. 20 , using a patterned mask, photolithography the second indium tin oxide layer 90 to form a fourth patterned second indium tin oxide layer 90 on the second flexible substrate layer 80; using the fourth patterned second indium tin oxide layer 90 as a mask, etching the second flexible substrate layer 80.
[0159] In a specific implementation manner, the second flexible substrate layer 80 is etched by a dry etching process.
[0160] Please refer to Fig.21 , remove the fourth patterned second indium tin oxide layer 90 and the second substrate 70 to obtain the packaging layer 801.
[0161] In a specific embodiment, the fourth patterned second indium tin oxide layer 90 is removed by a wet etching process;
[0162] The second flexible substrate layer 80 and the second base plate 70 are immersed in deionized water for demoulding to obtain the encapsulation layer 801 .
[0163] Please refer to Fig. 22 , the encapsulation layer 801 is pasted to the surface of the upper electrode 50 .
[0164] Please refer to Fig.23 , remove the first substrate 10. After completing this step, the flexible dual-mode sensor of the present invention is obtained.
[0165] Please refer to Fig.24 , Fig.24 The split diagram of each layer of the flexible dual-mode sensor is shown,
[0166] In summary, in the manufacturing method of the flexible dual-mode sensor provided by the present invention, a flexible substrate layer is formed on a first substrate, a first patterned lower electrode is formed on the flexible substrate layer, a PVDF copolymer piezoelectric layer is formed on the lower electrode, a second patterned upper electrode is formed on the PVDF copolymer piezoelectric layer, an insulating layer and a third patterned indium tin oxide layer are formed on the upper electrode in sequence, and the insulating layer and the indium tin oxide layer are used as masks to etch the flexible piezoelectric layer and the flexible substrate layer until the surface of the substrate, thereby ensuring that each layer corresponding to the sensor array area is hollowed out through two etchings, the manufacturing process is relatively simple, and the insulating layer and the indium tin oxide layer are subsequently removed. Each pixel point in the piezoelectric array area has both piezoelectric effect and pyroelectric effect, and a packaging layer is formed on the upper electrode. The eighth projection pattern of the packaging layer projected on the flexible substrate layer is the same as the flexible substrate layer, which ensures that each layer of the flexible dual-mode sensor is hollowed out and the air permeability of the sensor is ensured.
[0167] Accordingly, the embodiment of the present invention further provides a flexible dual-mode sensor, please continue to refer to Fig.24 ,include:
[0168] A flexible substrate layer 20, wherein the flexible substrate layer 20 includes an array area and a lead-out area adjacent to the array area, wherein the array area includes a plurality of sensing areas arranged in an array and separated from each other, and an interconnection area connected between adjacent sensing areas, and there is a gap between adjacent interconnection areas, and the interconnection area is a straight line parallel to the central axis of the surface of the flexible substrate layer 20;
[0169] A lower electrode 30 located on the flexible substrate layer 20, the lower electrode 30 comprising a plurality of first electrode portions 301 arranged in an array and separated from each other, and first interconnection lines 302 connected between adjacent first electrode portions 301 along a first direction, the first electrode portions 301 having a first projection pattern on the surface of the flexible substrate layer 20, the first projection pattern overlapping the sensing area, the first interconnection lines 302 having a second projection pattern on the surface of the flexible substrate layer 20, the second projection pattern partially overlapping the lead-out area;
[0170] A PVDF copolymer piezoelectric layer 40 located on the lower electrode 30, the PVDF copolymer piezoelectric layer 40 includes a piezoelectric array area and a piezoelectric lead-out area adjacent to the piezoelectric array area, the piezoelectric array area has a third projection pattern on the surface of the flexible substrate layer 20, the third projection pattern overlaps with the sensing area, and the piezoelectric lead-out area has a fourth projection pattern on the surface of the flexible substrate layer 20, the fourth projection pattern partially overlaps with the lead-out area;
[0171] An upper electrode 50 located on the PVDF copolymer piezoelectric layer 40, the upper electrode 50 comprising a plurality of second electrode portions 501 arranged in an array and separated from each other, and second interconnection lines 502 connected between adjacent second electrode portions 501 along a second direction, the second electrode portions 501 having a fifth projection pattern on the surface of the flexible substrate layer 20, the fifth projection pattern overlapping the sensing area, and the second interconnection lines 502 having a sixth projection pattern on the surface of the flexible substrate layer 20, the sixth projection pattern partially overlapping the lead-out area;
[0172] The encapsulation layer 801 is located on the upper electrode 50 , and an eighth projection pattern of the encapsulation layer 801 on the surface of the flexible substrate layer 20 overlaps with the flexible substrate layer 20 .
[0173] Furthermore, the present invention ensures the air permeability of the sensor by ensuring that each layer corresponding to the array area of the sensor is hollowed out.
[0174] In one implementation, please refer to Fig.24 The flexible substrate layer 20 includes a flexible substrate 201 and a buffer layer 202 located on the flexible substrate 201 .
[0175] exist Fig.24 In the example of , the first direction and the second direction are perpendicular to each other. Of course, the present invention is not limited thereto, and those skilled in the art can control the directions of the upper electrode 50 and the lower electrode 30 as needed.
[0176] As an example, the materials of the upper electrode 50 and the lower electrode 30 are both composite electrodes of metal material and indium tin oxide.
[0177] Thus, in the flexible dual-mode sensor provided by the present invention, the flexible substrate layer includes an array area and a lead-out area adjacent to the array area, the array area includes a plurality of sensing areas and interconnection areas, the interconnection area is a straight line and there is a gap between adjacent interconnection areas; the first electrode portion of the lower electrode overlaps with the pattern of the sensing area, and the first interconnection line overlaps with part of the pattern of the lead-out area; the piezoelectric array area of the PVDF copolymer piezoelectric layer overlaps with the pattern of the sensing area, and the piezoelectric lead-out area overlaps with part of the pattern of the lead-out area, and the PVDF copolymer material has both piezoelectric effect and pyroelectric effect, and there is no need to design the type of each pixel point in the piezoelectric array area; the second electrode portion of the upper electrode overlaps with the pattern of the sensing area, and the second interconnection line overlaps with part of the pattern of the lead-out area; the packaging layer overlaps with the pattern of the flexible substrate layer. Thus, the present invention ensures the air permeability of the sensor by ensuring that each layer corresponding to the array area of the sensor is hollowed out.
[0178] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.
Claims
1. A flexible dual-mode sensor, It is characterized in that include: A flexible substrate layer, the flexible substrate layer comprising an array area and a lead-out area adjacent to the array area, the array area comprising a plurality of sensing areas arranged in an array and separated from each other, and an interconnection area connected between adjacent sensing areas, with gaps between adjacent interconnection areas, and the interconnection area being a straight line parallel to the central axis of the surface of the flexible substrate layer; a lower electrode located on the flexible substrate layer, the lower electrode comprising a plurality of first electrode portions arranged in an array and separated from each other, and first interconnection lines connected between adjacent first electrode portions along a first direction, the first electrode portions having a first projection pattern on the surface of the flexible substrate layer, the first projection pattern overlapping the sensing area, the first interconnection line having a second projection pattern on the surface of the flexible substrate layer, the second projection pattern partially overlapping the lead-out area; A PVDF copolymer piezoelectric layer located on the lower electrode, the PVDF copolymer piezoelectric layer comprising a piezoelectric array area and a piezoelectric lead-out area adjacent to the piezoelectric array area, the piezoelectric array area having a third projection pattern on the surface of the flexible substrate layer, the third projection pattern overlapping the sensing area, the piezoelectric lead-out area having a fourth projection pattern on the surface of the flexible substrate layer, the fourth projection pattern partially overlapping the lead-out area; an upper electrode located on the PVDF copolymer piezoelectric layer, the upper electrode comprising a plurality of second electrode portions arranged in an array and separated from each other, and second interconnecting lines connected between adjacent second electrode portions along a second direction, the second electrode portions having a fifth projection pattern on the surface of the flexible substrate layer, the fifth projection pattern overlapping the sensing area, the second interconnecting lines having a sixth projection pattern on the surface of the flexible substrate layer, the sixth projection pattern partially overlapping the lead-out area; The encapsulation layer is located on the upper electrode, and an eighth projection pattern of the encapsulation layer on the surface of the flexible substrate layer overlaps with the flexible substrate layer.
2. The flexible dual-mode sensor according to claim 1, It is characterized in that The first direction and the second direction are perpendicular to each other.
3. The flexible dual-mode sensor according to claim 1, It is characterized in that The flexible substrate layer includes a flexible base and a buffer layer located on the flexible base.
4. The flexible dual-mode sensor according to claim 3, It is characterized in that The materials of the upper electrode and the lower electrode are both composite electrodes of metal material and indium tin oxide.
5. A method for manufacturing a flexible dual-mode sensor, It is characterized in that include: providing a first substrate; forming a flexible substrate layer on the first substrate, wherein the flexible substrate layer comprises an array area and a lead-out area adjacent to the array area; forming a first patterned lower electrode on the flexible substrate layer, wherein the lower electrode comprises a plurality of first electrode portions arranged in an array and separated from each other, and first interconnecting lines connected between adjacent first electrode portions along a first direction; forming a PVDF copolymer piezoelectric layer on the lower electrode, wherein the PVDF copolymer piezoelectric layer comprises a piezoelectric array region and a piezoelectric lead-out region adjacent to the piezoelectric array region; forming a second patterned upper electrode on the PVDF copolymer piezoelectric layer, wherein the upper electrode comprises a plurality of second electrode portions arranged in an array and separated from each other, and second interconnecting lines connected between adjacent second electrode portions along a second direction; forming an insulating layer and a third patterned indium tin oxide layer in sequence on the upper electrode; Using the indium tin oxide layer as a mask, etching the insulating layer, the PVDF copolymer piezoelectric layer and the flexible substrate layer until the surface of the first substrate, so that the array area includes a plurality of sensing areas arranged in an array and separated from each other, and interconnection areas connected between adjacent sensing areas, with gaps between adjacent interconnection areas, and the central axis of the interconnection area parallel to the surface of the flexible substrate layer is a straight line; The first projection pattern of the first electrode portion on the surface of the flexible substrate layer overlaps with the sensing area, and the second projection pattern of the first interconnection line on the surface of the flexible substrate layer overlaps partially with the lead-out area; The third projection pattern of the piezoelectric array area on the surface of the flexible substrate layer overlaps with the sensing area, and the fourth projection pattern of the piezoelectric lead-out area on the surface of the flexible substrate layer overlaps partially with the lead-out area; A fifth projection pattern of the second electrode portion on the surface of the flexible substrate layer overlaps with the sensing area, and a sixth projection pattern of the second interconnection line on the surface of the flexible substrate layer overlaps partially with the lead-out area; removing the insulating layer and the indium tin oxide layer; forming a packaging layer on the upper electrode, wherein an eighth projection pattern of the packaging layer on the surface of the flexible substrate layer overlaps with the flexible substrate layer; The first substrate is removed.
6. The method for manufacturing the flexible dual-mode sensor according to claim 5, It is characterized in that Forming a flexible substrate layer on the first substrate, comprising: spin coating a flexible solution on the substrate; After spin coating the flexible solution, annealing the flexible solution to obtain a flexible substrate; A buffer layer is deposited on the flexible substrate to form the flexible substrate layer.
7. The method for manufacturing the flexible dual-mode sensor according to claim 5, It is characterized in that The pattern of the first patterned mask for forming the first patterned lower electrode is perpendicular to the pattern of the second patterned mask for forming the second patterned lower electrode.
8. The method for manufacturing the flexible dual-mode sensor according to claim 5, It is characterized in that An insulating layer and a third patterned indium tin oxide layer are sequentially formed on the upper electrode, comprising: depositing the insulating layer on the upper electrode; forming the indium tin oxide layer on the insulating layer by a magnetron sputtering process; The indium tin oxide layer is photolithographically processed using a third patterned mask to form the third patterned indium tin oxide layer.
9. The method for manufacturing the flexible dual-mode sensor according to claim 5, It is characterized in that Using the insulating layer and the indium tin oxide layer as masks, etching the PVDF copolymer piezoelectric layer and the flexible substrate layer until the surface of the first substrate comprises: Using the third patterned indium tin oxide layer as a mask, the insulating layer, the PVDF copolymer piezoelectric layer and the flexible substrate layer are etched in sequence until the surface of the first substrate is reached.
10. The method for manufacturing the flexible dual-mode sensor according to claim 5, It is characterized in that Forming a packaging layer on the insulating layer and the indium tin oxide layer, comprising: providing a second substrate; forming a second flexible substrate layer on the second substrate; depositing a second indium tin oxide layer on the second flexible substrate layer; Using a patterned mask, photolithography is performed on the second indium tin oxide layer to form a fourth patterned second indium tin oxide layer on the second flexible substrate layer; Using the fourth patterned second indium tin oxide layer as a mask, etching the second flexible substrate layer; removing the fourth patterned second indium tin oxide layer and the second substrate to obtain the encapsulation layer; The encapsulation layer is adhered to the surface of the upper electrode.