Zinc oxide / hafnium oxide-based radio frequency switch and preparation method thereof

By adopting zinc oxide/hafnium oxide structure and simplified preparation process in RF switches, the complexity and high cost of traditional RF switches are solved, and the performance of RF switches with low insertion loss and high isolation is achieved, and the application field is expanded. .

CN118890956APending Publication Date: 2024-11-01NANJING UNIV OF POSTS & TELECOMM
View PDF 0 Cites 3 Cited by

Patent Information

Application Number
CN202410956325.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-17
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

The preparation process of traditional RF switches is complex, costly, and unstable. RF MEMS-based RF switches perform poorly in high-frequency applications, with large insertion loss and low linearity, and limited applications.

Method used

Using a radio frequency switch design based on zinc oxide/hafnium oxide, silicon-based wafers are used as carriers, and prepared by magnetron sputtering coating technology and optical lithography technology, including silicon substrate layer, aluminum nitride layer, nickel layer, platinum layer, and 2. The molybdenum sulfide layer/zinc oxide quantum dot layer, zinc oxide layer/hafnium oxide layer, silver layer, titanium nitride layer, nickel layer, and copper layer have simple structures, reducing the difficulty and cost of preparation.

Benefits of technology

The RF switch performance with low insertion loss, low power consumption, fast switching and high isolation is achieved, which simplifies the preparation process, reduces production costs, and expands the application field of RF switches.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118890956A_ABST
    Figure CN118890956A_ABST
Patent Text Reader

Abstract

The invention discloses a zinc oxide / hafnium oxide-based radio frequency switch and a preparation method thereof, and the radio frequency switch takes a silicon-based wafer as a carrier, takes metal platinum and metal silver as an electrode layer of a radio frequency switch device, and takes molybdenum disulfide and zinc oxide as resistive materials. Comprising a silicon substrate layer, an aluminum nitride layer, a nickel layer, a platinum layer, a molybdenum disulfide layer, a zinc oxide layer, a silver layer, a titanium nitride layer, a nickel layer and a copper layer which are sequentially arranged from bottom to top. The radio frequency switch is prepared on the silicon substrate by utilizing the photoetching process and the PVD magnetron sputtering coating process, and the preparation method is simple in process and low in cost. And the prepared radio frequency switch has excellent performance and good application prospect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of electronic devices, and in particular to a preparation method of a zinc oxide / hafnium oxide-based radio frequency switch. Background Art

[0002] With the development of semiconductor technology, many new RF switches have emerged, and the performance of RF control circuits has been optimized. However, the traditional RF switches have always had problems such as complex preparation process, high cost, and unstable performance; the current technical problems are: 1. Consider the specific parameters of the RF switch, such as the size of each part, and whether the ideal performance indicators can be achieved.

[0003] 2. During the preparation of the transmission line layer, it is difficult to strip copper.

[0004] 3. Solid-state field-effect transistor switches are mainly CMOS, GaAs, SiGe, and SOI. However, they have the disadvantages of high insertion loss, large variation, low linearity, and low power handling capability.

[0005] 4. RF switches based on RF micro-electromechanical systems (MEMS) can provide better RF performance, but RF MEMS are only implemented in very limited applications and only at low frequencies. Summary of the invention

[0006] To solve the above problems, the present invention discloses a preparation method of a radio frequency switch based on zinc oxide / hafnium oxide and the preparation method thereof. The present invention applies the non-volatility, low power consumption, fast switching, nanoscale size and other characteristics of a memristor to the design of a radio frequency switch, thereby obtaining a radio frequency switch based on zinc oxide with excellent performance such as low insertion loss and high isolation.

[0007] A zinc oxide / hafnium oxide based radio frequency switch, which uses a silicon-based wafer as a carrier and includes a silicon substrate layer, an aluminum nitride layer, a nickel layer, a platinum layer, a molybdenum disulfide layer / zinc oxide quantum dot layer, a zinc oxide layer / hafnium oxide layer, a silver layer, a titanium nitride layer, a nickel layer, and a copper layer arranged in sequence from bottom to top.

[0008] Furthermore, a switch structure of platinum-molybdenum disulfide-zinc oxide-silver or a switch structure of platinum-hafnium oxide-silver is adopted.

[0009] Furthermore, the aluminum nitride layer is deposited on the silicon substrate layer to play an insulating role.

[0010] Furthermore, a nickel layer is plated as an adhesion layer before plating the bottom electrode platinum layer.

[0011] Furthermore, in the radio frequency switch of the present invention, the aluminum nitride layer is deposited on the silicon substrate layer to play an insulating role.

[0012] Furthermore, in the radio frequency switch of the present invention, a nickel layer is first plated as an adhesion layer before plating the bottom electrode platinum layer.

[0013] Furthermore, in the radio frequency switch of the present invention, the size of the dielectric layer is larger than the size of the upper and lower electrodes to prevent the upper and lower electrodes from contacting each other and causing a short circuit during the preparation process.

[0014] Furthermore, in the radio frequency switch of the present invention, zinc oxide quantum dots are spin-coated on the surface of the molybdenum disulfide layer, which is beneficial to the formation of conductive filaments, or zinc oxide quantum dots are spin-coated on the surface of the platinum layer before plating hafnium oxide, which is beneficial to the formation of conductive filaments.

[0015] Furthermore, in the radio frequency switch of the present invention, the titanium nitride layer is deposited on the upper electrode silver layer to play an anti-oxidation role.

[0016] Furthermore, in the radio frequency switch of the present invention, a nickel layer is first plated as an adhesion layer before plating the copper layer of the transmission line to reduce the difficulty of stripping the transmission line.

[0017] Furthermore, in the radio frequency switch of the present invention, a copper layer around it is used as a ground wire structure; the hourglass shape in the middle is the signal transmission line, and the rectangular ring around it is the ground wire. A method for preparing a zinc oxide / hafnium oxide based radio frequency switch comprises the following steps: Step 1: Use magnetron sputtering coating technology to coat 40nm thick aluminum nitride on the silicon substrate layer as an insulating layer; Step 2: Spin-coat photoresist on the surface of the silicon-based wafer, and then use optical lithography technology to define the lower electrode pattern on the spin-coated photoresist layer; Step 3: Use magnetron sputtering coating technology to plate a nickel layer with a thickness of 10nm and a platinum layer with a thickness of 100nm on the surface, then put the wafer into an acetone solution for ultrasonic treatment, then put the wafer into ultrapure water for cleaning, and then put it into anhydrous ethanol and ultrapure water for cleaning in turn, and finally remove the residual photoresist to obtain the mask pattern of the platinum lower electrode; Step 4: Spin-coat photoresist on the surface of the silicon-based wafer, and then use optical lithography technology to define the dielectric layer pattern on the spin-coated photoresist layer; Step 5: using magnetron sputtering coating technology to coat a 5nm thick molybdenum disulfide layer on the surface, spin-coating zinc oxide quantum dots with a diameter of 80nm and then coating a 60nm thick zinc oxide layer, then placing the wafer in an acetone solution for ultrasonic treatment, then placing the wafer in ultrapure water for cleaning, then sequentially placing it in anhydrous ethanol and ultrapure water for cleaning, and finally removing the residual photoresist to obtain a mask pattern of the dielectric layer; or spin-coating a zinc oxide quantum dot layer with a diameter of 80nm on the surface of the platinum layer, using magnetron sputtering coating technology to coat a 60nm thick hafnium oxide layer on the surface, then placing the wafer in an acetone solution for ultrasonic treatment, then placing the wafer in ultrapure water for cleaning, then sequentially placing it in anhydrous ethanol and ultrapure water for cleaning, and finally removing the residual photoresist to obtain a mask pattern of the dielectric layer; Step 6: Spin-coat photoresist on the surface of the silicon-based wafer, and then use optical lithography technology to define the upper electrode pattern on the spin-coated photoresist layer; Step 7: Use magnetron sputtering coating technology to coat a 95nm thick silver layer and a 5nm thick titanium nitride layer on the surface, then put the wafer into an acetone solution for ultrasonic treatment, then put the wafer into ultrapure water for cleaning, and then put it into anhydrous ethanol and ultrapure water for cleaning in turn, and finally remove the residual photoresist to obtain the mask pattern of the dielectric layer; Step 8: Spin-coat photoresist on the surface of the silicon-based wafer, and then use optical lithography technology to define the transmission line pattern on the spin-coated photoresist layer; Step 9: Use magnetron sputtering coating technology to plate a 10nm thick nickel layer and a 100nm thick copper layer on the surface, then put the chip into acetone solution for ultrasonic treatment, then put the chip into ultrapure water for cleaning, and then put it into anhydrous ethanol and ultrapure water for cleaning, and finally remove the residual photoresist to obtain the mask pattern of the transmission line.

[0018] Beneficial effects of the present invention: The preparation process of a RF switch based on zinc oxide / hafnium oxide prepared by the present invention is simple, and only two processes, namely photolithography process and magnetron sputtering coating process, are used. The operation is simple and easy to mass produce. At the same time, the RF switch is low in cost, and the material cost, manufacturing equipment cost and labor cost are low, so that the product has better market competitiveness. The RF switch has a simple structure and has good turn-on and turn-off voltages, insertion loss and isolation. In addition, the application of the RF switch in the phase shifter further expands its application field and has broad application prospects. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 Side view of a zinc oxide memristor-based RF switch.

[0020] Figure 2 Top view of a zinc oxide memristor-based RF switch.

[0021] In the figure, there are: silicon substrate layer 1, aluminum nitride layer 2, nickel layer 3, platinum layer 4, molybdenum disulfide layer / zinc oxide quantum dot layer 5, zinc oxide layer / hafnium oxide layer 6, silver layer 7, titanium nitride layer 8, nickel layer 9, and copper layer 10.

[0022] Figure 3 Process flow chart of zinc oxide memristor-based RF switch.

[0023] Figure 4 Process flow diagram for hafnium oxide memristor-based RF switches.

[0024] Figure 5 (a) Hysteresis curve of the RF switch based on zinc oxide memristor in standard coordinate system (b) Hysteresis curve of the RF switch based on zinc oxide memristor in logarithmic coordinate system; Figure 5 (c) Set curves of the ZnO memristor-based RF switch after 40 cycles. Figure 5 (d) Reset curve of the ZnO memristor-based RF switch after 40 cycles. Figure 6 (a) The hysteresis curve of the RF switch based on hafnium oxide memristor in the standard coordinate system; (b) The hysteresis curve of the RF switch based on hafnium oxide memristor in the logarithmic coordinate system; Figure 6 (c) Set curves of the hafnium oxide memristor-based RF switch after 20 cycles. Figure 6 (d) Reset curves of the hafnium oxide memristor-based RF switch after 20 cycles.

[0025] Figure 7 Figure 2 shows the insertion loss curve dB (S (2, 1)) and isolation curve dB (S (4, 3) of the zinc oxide RF switch device. DETAILED DESCRIPTION

[0026] The present invention is further explained below in conjunction with the accompanying drawings and specific embodiments. It should be understood that the following specific embodiments are only used to illustrate the present invention and are not used to limit the scope of the present invention. It should be noted that the words "front", "rear", "left", "right", "upper" and "lower" used in the following description refer to directions in the accompanying drawings, and the words "inner" and "outer" refer to directions toward or away from the geometric center of a specific component, respectively. Example 1

[0027] like Figure 1 , 2As shown in Figure 3, the radio frequency switch of this embodiment uses a silicon-based wafer as a carrier, including a silicon substrate layer 1, an aluminum nitride layer 2, a nickel layer 3, a platinum layer 4, a molybdenum disulfide layer 5, a zinc oxide layer 6, a silver layer 7, a titanium nitride layer 8, a nickel layer 9, and a copper layer 10 arranged from bottom to top. The radio frequency switch adopts a special switch structure of platinum-molybdenum disulfide-zinc oxide-silver, and the aluminum nitride layer is deposited on the silicon substrate layer to play an insulating role. Before plating zinc oxide, zinc oxide quantum dots are spin-coated on the surface of the molybdenum disulfide layer, which is conducive to the formation of conductive filaments. The size of the dielectric layer is larger than the size of the upper and lower electrodes to prevent the upper and lower electrodes from contacting and causing a short circuit during the preparation process. The titanium nitride layer is deposited on the upper electrode silver layer to prevent oxidation. Before plating the copper layer of the transmission line, a nickel layer is first plated as an adhesion layer to reduce the difficulty of stripping the transmission line. And a circle of copper layer is plated around it as a ground wire structure.

[0028] The method for preparing a radio frequency switch based on zinc oxide memristor of the present invention takes the preparation of upper and lower electrodes of 50 μm×60 μm, a dielectric layer of 50 μm×50 μm, and a transmission line of 510 μm×100 μm as an example, and the preparation process is as follows: Step 1: Use nitrogen to blow away surface impurities from the purchased commercial silicon substrate, and use magnetron sputtering coating technology to coat 80nm thick aluminum nitride on the silicon substrate as an insulating layer; Step 2: The silicon substrate with the insulating layer was ultrasonically cleaned (5 min) with acetone, anhydrous ethanol and ultrapure water in sequence, and then dried with nitrogen; a photoresist was first spin-coated on the surface of the silicon substrate with the insulating layer using a coating machine at a speed of 600 rpm for 9 seconds, and then at a speed of 4000 rpm for 40 seconds. Then, optical lithography was used to define the lower electrode pattern on the spin-coated photoresist layer, and the lithography machine model was MA6.

[0029] Step 3: Use magnetron sputtering coating technology to plate 10nm thick nickel and 100nm thick platinum on the surface, then put the wafer into acetone solution for ultrasonic treatment, then put the wafer into ultrapure water for cleaning, and then put it into anhydrous ethanol and ultrapure water for cleaning in turn, and finally remove the residual photoresist to obtain the mask pattern of the platinum lower electrode; Step 4: After drying with nitrogen, use a coating machine to spin-coat the surface of the silicon substrate with an insulating layer at a speed of 600 rpm for 9 seconds, and then spin-coat the photoresist at a speed of 4000 rpm for 40 seconds. Then use optical lithography technology to define the dielectric layer pattern on the spin-coated photoresist layer; Step 5: Use magnetron sputtering coating technology to coat 5nm thick molybdenum disulfide on the surface, spin-coat zinc oxide quantum dots with a diameter of 80nm, and then coat zinc oxide with a thickness of 60nm. Then put the wafer into acetone solution for ultrasonic treatment, then put the wafer into ultrapure water for cleaning, and then put it into anhydrous ethanol and ultrapure water for cleaning in turn, and finally remove the residual photoresist to obtain the mask pattern of the dielectric layer; Step 6: After drying with nitrogen, use a coating machine to spin-coat the surface of the silicon substrate with an insulating layer at a speed of 600 rpm for 9 seconds, and then spin-coat the photoresist at a speed of 4000 rpm for 40 seconds. Then use optical lithography technology to define the upper electrode pattern on the spin-coated photoresist layer; Step 7: Use magnetron sputtering coating technology to coat 95nm thick metal silver and 5nm thick titanium nitride on the surface, then put the wafer into acetone solution for ultrasonic treatment, then put the wafer into ultrapure water for cleaning, and then put it into anhydrous ethanol and ultrapure water for cleaning in turn, and finally remove the residual photoresist to obtain the mask pattern of the dielectric layer; Step 8: After drying with nitrogen, use a coating machine to spin-coat the surface of the silicon substrate with an insulating layer at a speed of 600 rpm for 9 seconds, and then spin-coat the photoresist at a speed of 4000 rpm for 40 seconds. Then use optical lithography technology to define the transmission line pattern on the spin-coated photoresist layer; Step 9: Use magnetron sputtering coating technology to plate 10nm thick metal nickel and 100nm thick metal copper on the surface, then put the chip into acetone solution for ultrasonic treatment, then put the chip into ultrapure water for cleaning, and then put it into anhydrous ethanol and ultrapure water for cleaning, finally remove the residual photoresist to obtain the mask pattern of the transmission line. Example 2

[0030] like Figure 1 , 2 , as shown in 4. The radio frequency switch of this embodiment uses a silicon-based wafer as a carrier, including a silicon substrate layer 1, an aluminum nitride layer 2, a nickel layer 3, a platinum layer 4, a zinc oxide quantum dot layer 5, a hafnium oxide layer 6, a silver layer 7, a titanium nitride layer 8, a nickel layer 9, and a copper layer 10 arranged in sequence from bottom to top. The radio frequency switch adopts a special switch structure of platinum-hafnium oxide-silver, and the aluminum nitride layer is deposited on the silicon substrate layer to play an insulating role. To prevent the upper and lower electrodes from contacting and causing a short circuit during the preparation process. Spin coating zinc oxide quantum dots on the surface of the platinum layer is conducive to the formation of conductive filaments. The size of the dielectric layer is larger than the size of the upper and lower electrodes, and the titanium nitride layer is deposited on the upper electrode silver layer to play an anti-oxidation role. Before plating the copper layer of the transmission line, a nickel layer is first plated as an adhesion layer to reduce the difficulty of stripping the transmission line. And a circle of copper layer is plated around as a ground wire structure.

[0031] The method for preparing a radio frequency switch based on hafnium oxide memristor of the present invention takes the preparation of upper and lower electrodes of 50 μm×60 μm, a dielectric layer of 50 μm×50 μm, and a transmission line of 510 μm×100 μm as an example, and the preparation process is as follows: Step 1: Use nitrogen to blow off surface impurities from the purchased commercial silicon substrate, and use magnetron sputtering coating technology to coat an aluminum nitride layer 2 with a thickness of 80nm on the silicon substrate layer 1 as an insulating layer; Step 2: The silicon substrate with the insulating layer was ultrasonically cleaned (5 min) with acetone, anhydrous ethanol and ultrapure water in sequence, and then dried with nitrogen; a photoresist was first spin-coated on the surface of the silicon substrate with the insulating layer using a coating machine at a speed of 600 rpm for 9 seconds, and then at a speed of 4000 rpm for 40 seconds. Then, optical lithography was used to define the lower electrode pattern on the spin-coated photoresist layer, and the lithography machine model was MA6.

[0032] Step 3: A nickel layer with a thickness of 10 nm and a platinum layer with a thickness of 3100 nm are plated on the surface by magnetron sputtering coating technology, and then the wafer is placed in an acetone solution for ultrasonic treatment, and then the wafer is placed in ultrapure water for cleaning, and then placed in anhydrous ethanol and ultrapure water for cleaning in turn, and finally the residual photoresist is removed to obtain a mask pattern of the platinum lower electrode; Step 4: After drying with nitrogen, use a coating machine to spin-coat the surface of the silicon substrate with an insulating layer at a speed of 600 rpm for 9 seconds, and then spin-coat the photoresist at a speed of 4000 rpm for 40 seconds. Then use optical lithography technology to define the dielectric layer pattern on the spin-coated photoresist layer; Step 5: Spin-coat a zinc oxide quantum dot layer 5 with a diameter of 80 nm on the surface of the platinum layer 4, and use magnetron sputtering coating technology to coat a hafnium oxide layer 6 with a thickness of 60 nm on the surface, then put the wafer into an acetone solution for ultrasonic treatment, then put the wafer into ultrapure water for cleaning, and then put it into anhydrous ethanol and ultrapure water for cleaning in turn, and finally remove the residual photoresist to obtain a mask pattern of the dielectric layer; Step 6: After drying with nitrogen, use a coating machine to spin-coat the surface of the silicon substrate with an insulating layer at a speed of 600 rpm for 9 seconds, and then spin-coat the photoresist at a speed of 4000 rpm for 40 seconds. Then use optical lithography technology to define the upper electrode pattern on the spin-coated photoresist layer; Step 7: A 95nm thick silver layer 7 and a 5nm thick titanium nitride layer 8 are plated on the surface by magnetron sputtering coating technology, and then the wafer is placed in an acetone solution for ultrasonic treatment, and then the wafer is placed in ultrapure water for cleaning, and then placed in anhydrous ethanol and ultrapure water for cleaning in sequence, and finally the residual photoresist is removed to obtain a mask pattern of the dielectric layer; Step 8: After drying with nitrogen, use a coating machine to spin-coat the surface of the silicon substrate with an insulating layer at a speed of 600 rpm for 9 seconds, and then spin-coat the photoresist at a speed of 4000 rpm for 40 seconds. Then use optical lithography technology to define the transmission line pattern on the spin-coated photoresist layer; Step 9: Use magnetron sputtering technology to plate a 10nm thick nickel layer (9 and a 100nm thick copper layer 10 on the surface, then put the wafer into an acetone solution for ultrasonic treatment, then put the wafer into ultrapure water for cleaning, and then put it into anhydrous ethanol and ultrapure water for cleaning in turn, and finally remove the residual photoresist to obtain the mask pattern of the transmission line.

[0033] Combined with the products prepared in Examples 1 and 2, Figure 5 (a) Hysteresis curve of the RF switch based on zinc oxide memristor in the standard coordinate system (b) Hysteresis curve of the RF switch based on zinc oxide memristor in the logarithmic coordinate system (c) Set curve of the RF switch based on zinc oxide memristor after 40 cycles (d) Reset curve of the RF switch based on zinc oxide memristor after 40 cycles; The hysteresis curve of the device has been tested and obtained, and it can be found that the device has good resistance change characteristics. The zinc oxide-based device can achieve a change from on-state resistance of 14.470Ω to off-state resistance of 5.5616E+4Ω, and has good set voltage (1.32V) and reset voltage (-0.9V).

[0034] Figure 6 (a) Hysteresis curve of the RF switch based on hafnium oxide memristor in the standard coordinate system (b) Hysteresis curve of the RF switch based on hafnium oxide memristor in the logarithmic coordinate system (c) Set curve of the RF switch based on hafnium oxide memristor after 20 cycles (d) Reset curve of the RF switch based on hafnium oxide memristor after 20 cycles; The hafnium oxide-based device can achieve a change from an on-state resistance of 11.833Ω to an off-state resistance of 1.0971E+4Ω, and has a good set voltage (1V) and reset voltage (-0.5V). The RF switch can also be cycled multiple times with good stability. At the same time, the test shows that the device can achieve excellent RF performance with an insertion loss of less than 2dB and an isolation of more than 20dB.

[0035] Figure 7 Figure 2 shows the insertion loss curve dB (S (2, 1)) and isolation curve dB (S (4, 3) of the zinc oxide RF switch device.

[0036] The technical means disclosed in the solution of the present invention are not limited to the technical means disclosed in the above-mentioned implementation mode, but also include technical solutions composed of any combination of the above-mentioned technical features.

Claims

1. A radio frequency switch based on zinc oxide / hafnium oxide, characterized in that: The radio frequency switch uses a silicon-based wafer as a carrier, and comprises a silicon substrate layer (1), an aluminum nitride layer (2), a nickel layer (3), a platinum layer (4), a molybdenum disulfide layer / zinc oxide quantum dot layer (5), a zinc oxide layer / hafnium oxide layer (6), a silver layer (7), a titanium nitride layer (8), a nickel layer (9), and a copper layer (10) which are arranged in sequence from bottom to top.

2. The zinc oxide / hafnium oxide based radio frequency switch according to claim 1, characterized in that: A switching structure of platinum-molybdenum disulfide-zinc oxide-silver or a switching structure of platinum-hafnium oxide-silver is adopted.

3. The zinc oxide / hafnium oxide based radio frequency switch according to claim 1, characterized in that: The aluminum nitride layer (2) is deposited on the silicon substrate layer (1).

4. The zinc oxide / hafnium oxide based radio frequency switch according to claim 1, characterized in that: A zinc oxide quantum dot layer (5) with a diameter of 80 nm is spin-coated on the surface of the platinum layer (4).

5. The zinc oxide / hafnium oxide based radio frequency switch according to claim 1, characterized in that: The sizes of the molybdenum disulfide layer (5) and the zinc oxide layer (6) are larger than the sizes of the upper and lower electrodes, so as to prevent the upper and lower electrodes from contacting each other and causing a short circuit during the preparation process.

6. The zinc oxide / hafnium oxide based radio frequency switch according to claim 1, characterized in that: The size of the hafnium oxide layer (6) is larger than the size of the upper and lower electrodes.

7. The zinc oxide / hafnium oxide based radio frequency switch according to claim 1, characterized in that: Before plating the zinc oxide layer (6), zinc oxide quantum dots with a diameter of 80 nm are spin-coated on the surface of the molybdenum disulfide layer (5).

8. The zinc oxide / hafnium oxide based radio frequency switch according to claim 1, characterized in that: The titanium nitride layer (8) is deposited on the upper electrode silver layer (7).

9. The zinc oxide / hafnium oxide based radio frequency switch according to claim 1, characterized in that: A circle of copper layer (10) around the signal transmission line serves as a ground wire structure.

10. A zinc oxide / hafnium oxide based radio frequency switch prepared according to any one of claims 1 to 9, characterized in that: The method comprises the following steps: The first step: using magnetron sputtering coating technology to coat aluminum nitride (2) with a thickness of 40 nm on the silicon substrate layer (1) as an insulating layer; Step 2: Spin-coat photoresist on the surface of the silicon-based wafer, and then use optical lithography technology to define the lower electrode pattern on the spin-coated photoresist layer; Step 3: A nickel layer (3) with a thickness of 10 nm and a platinum layer (4) with a thickness of 100 nm are plated on the surface by magnetron sputtering coating technology, and then the wafer is placed in an acetone solution for ultrasonic treatment, and then the wafer is placed in ultrapure water for cleaning, and then placed in anhydrous ethanol and ultrapure water for cleaning in sequence, and finally the residual photoresist is removed to obtain a mask pattern of the platinum lower electrode; Step 4: Spin-coat photoresist on the surface of the silicon-based wafer, and then use optical lithography technology to define the dielectric layer pattern on the spin-coated photoresist layer; Step 5: using magnetron sputtering coating technology to coat a 5nm thick molybdenum disulfide layer (5) on the surface, spin-coating zinc oxide quantum dots with a diameter of 80nm and then coating a 60nm thick zinc oxide layer (6), then placing the wafer in an acetone solution for ultrasonic treatment, then placing the wafer in ultrapure water for cleaning, then sequentially placing it in anhydrous ethanol and ultrapure water for cleaning, and finally removing the residual photoresist to obtain a mask pattern of the dielectric layer; or spin-coating a zinc oxide quantum dot layer (5) with a diameter of 80nm on the surface of the platinum layer (4), using magnetron sputtering coating technology to coat a 60nm thick hafnium oxide layer (6) on the surface, then placing the wafer in an acetone solution for ultrasonic treatment, then placing the wafer in ultrapure water for cleaning, then sequentially placing it in anhydrous ethanol and ultrapure water for cleaning, and finally removing the residual photoresist to obtain a mask pattern of the dielectric layer; Step 6: Spin-coat photoresist on the surface of the silicon-based wafer, and then use optical lithography technology to define the upper electrode pattern on the spin-coated photoresist layer; Step 7: using magnetron sputtering coating technology to coat a 95 nm thick silver layer (7) and a 5 nm thick titanium nitride layer (8) on the surface, then placing the wafer in an acetone solution for ultrasonic treatment, then placing the wafer in ultrapure water for cleaning, and then placing it in anhydrous ethanol and ultrapure water for cleaning in sequence, and finally removing the residual photoresist to obtain a mask pattern of the dielectric layer; Step 8: Spin-coat photoresist on the surface of the silicon-based wafer, and then use optical lithography technology to define the transmission line pattern on the spin-coated photoresist layer; Step 9: A nickel layer (9) with a thickness of 10 nm and a copper layer (10) with a thickness of 100 nm are plated on the surface using magnetron sputtering technology, and then the wafer is placed in an acetone solution for ultrasonic treatment. The wafer is then placed in ultrapure water for cleaning, and then placed in anhydrous ethanol and ultrapure water for cleaning in turn. Finally, the residual photoresist is removed to obtain a mask pattern of the transmission line.

Citation Information

Cited By

  • Terahertz memristor radio frequency switch based on suspended nanoelectrode and preparation method thereof

    CN119562757A

  • Nonvolatile radio frequency switch chip for 5G radio frequency front end

    CN121036737A

  • A non-volatile radio frequency switch chip for 5G radio frequency front end

    CN121036737B