Manufacturing method of boiling type cooler and boiling type cooler

By forming boiling faces through layering and shapes, the complex processes in the prior art are solved, and the acquisition of efficient boiling heat transfer performance and the simplification of the manufacturing process are achieved.

CN118891485APending Publication Date: 2024-11-01SUMITOMO PRECISION PRODUCTS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380028354.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-03-31
Filing Date
2023-03-17
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

When the existing boiling coolers form boiling faces with high efficiency boiling heat transfer performance, the processes are complicated and it is difficult to achieve simple process operations.

Method used

The boiling face is formed by laminated shape, including laminated shape using metal powder and powder bed fusion, and a structure with gradually thicker protrusions and linear protrusions gradually thickened from the base end to the end, avoiding sandblasting treatment to simplify the process.

Benefits of technology

A boiling face that obtains efficient boiling heat transfer performance in a simple process is realized, which improves boiling heat transfer performance and simplifies the manufacturing process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118891485A_ABST
    Figure CN118891485A_ABST
Patent Text Reader

Abstract

A method for manufacturing a boiling type cooler (100) provided with a boiling section (10) for boiling a refrigerant by heat exchange with a heating element (HS), and a condensing section (20) for condensing the refrigerant boiled by the boiling section and returning the condensed refrigerant to the boiling section, the manufacturing method of the boiling type cooler (100) comprises a step of forming the condensation part and a step of forming the boiling part. The step for forming the boiling portion includes a step for forming, by means of a laminated molding, at least a portion of a boiling surface portion (13) that is provided on a surface (11b) of the heating element on the opposite side from the attachment surface (11a) and that is in contact with the refrigerant.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a method for manufacturing a boiling cooler and a boiling cooler, and in particular to a method for manufacturing a boiling cooler having a boiling section for boiling a refrigerant and a condensing section for condensing the refrigerant and returning it to the boiling section and a boiling cooler. Background Art

[0002] Conventionally, there is known a boiling type cooler including a boiling section for boiling a refrigerant and a condensing section for condensing the refrigerant and returning it to the boiling section. This type of boiling type cooler is disclosed in, for example, Japanese Patent No. 6744110.

[0003] The above-mentioned Japanese Patent Gazette No. 6744110 discloses a thermosyphon cooler (boiling cooler) having a boiling section for boiling a refrigerant and a condensing section for condensing the refrigerant and returning it to the boiling section. The boiling section includes a mounting surface for mounting a cooling object; and a boiling surface arranged on the back side of the mounting surface. A plurality of fins are formed on the boiling surface. The plurality of fins are formed by processing a plate-like member into a corrugated fin, cutting the processed corrugated fin and then joining it to the boiling surface, and removing the top of the joined corrugated fin by cutting.

[0004] Previous technical literature

[0005] Patent Literature

[0006] Patent Document 1: Japanese Patent No. 6744110 Summary of the invention

[0007] Technical issues to be solved by the invention

[0008] The thermosyphon cooler described in the Japanese Patent No. 6744110 has a plurality of fins formed on the boiling surface, so that a boiling surface with high boiling heat transfer performance can be obtained. On the other hand, forming the plurality of fins requires many individual processes, so the process is complicated. Therefore, it is desired to obtain a boiling surface with high boiling heat transfer performance by a simple process.

[0009] The present invention is made to solve the above-mentioned problems. One object of the present invention is to provide a method for manufacturing a boiling cooler and a boiling cooler capable of obtaining a boiling surface with high boiling heat transfer performance by a simple process.

[0010] Means for solving technical problems

[0011] In order to achieve the above-mentioned purpose, the inventors of the present application conducted in-depth research and found that a boiling surface with high boiling heat transfer performance can be obtained by forming a boiling surface by stacking molding, thereby completing the present invention. That is, based on the manufacturing method of a boiling type cooler of the first invention, the boiling type cooler has a boiling section that boils the refrigerant by heat exchange with a heating element and a condensation section that condenses the refrigerant boiled by the boiling section and returns it to the boiling section. The manufacturing method of the boiling type cooler includes: a step of forming a condensation section; and a step of forming a boiling section; the step of forming a boiling section includes: a step of forming at least a portion of a boiling surface that is provided on the side of the heating element opposite to the mounting surface and in contact with the refrigerant by stacking molding.

[0012] In the manufacturing method of the boiling cooler based on the first invention, as described above, at least a portion of the boiling surface portion that is provided on the surface of the heating element on the side opposite to the mounting surface and in contact with the refrigerant is formed by stacking molding. Therefore, a boiling surface portion having high boiling heat transfer performance can be obtained by stacking molding, and by using stacking molding, the boiling surface portion can be obtained by a simple process without going through many individual processes. As a result, a boiling surface portion having high boiling heat transfer performance can be obtained by a simple process. In addition, the inventors of the present application have confirmed in the experiments described later that a boiling surface portion having high boiling heat transfer performance can be obtained by stacking molding.

[0013] In the first invention, it is preferred that the step of forming at least a portion of the boiling face portion by stacking molding includes the step of forming at least a portion of the boiling face portion by stacking molding using metal powder. If configured in this manner, a boiling face portion having minute concave-convex portions on the surface can be obtained by stacking molding using metal powder. As a result, boiling can be promoted by the minute concave-convex portions on the surface, so that a boiling face portion having higher boiling heat transfer performance can be obtained.

[0014] At this time, it is preferred that the step of forming at least a portion of the boiling face portion by stacking molding includes the step of forming at least a portion of the boiling face portion by fusing a powder bed as a stacking molding. If configured in this manner, a boiling face portion having minute irregularities on the surface can be easily obtained by fusing the powder bed, and thus a boiling face portion having a higher boiling heat transfer performance can be easily obtained.

[0015] In the above-mentioned first invention, it is preferably as follows: the process of forming at least a part of the boiling face by stacking molding includes: the process of forming at least a part of the boiling face by stacking molding includes: the process of forming the protrusions by stacking molding in a manner of arranging a plurality of protrusions having a shape that gradually becomes thicker from the base end toward the terminal end. If constructed in this way, a boiling face having a space that can be filled with refrigerant between the protrusions can be obtained. As a result, when the refrigerant boils on the protrusions and the surroundings thereof, the refrigerant that fills the space between the protrusions can be quickly supplied, thereby suppressing the protrusions and the surroundings where the refrigerant boils from drying. Thus, a situation in which boiling is hindered due to drying of the protrusions and the surroundings thereof can be avoided, thereby improving the boiling heat transfer performance of the boiling face. Furthermore, although a plurality of protrusions having a shape that gradually becomes thicker from the base end toward the terminal end are difficult to form by mechanical processing such as cutting, they can be easily formed by stacking molding. Furthermore, the inventors of the present application have confirmed in experiments described below that a boiling surface with high boiling heat transfer performance can be obtained by forming the protrusions by stacking and molding in a manner that arranges a plurality of protrusions having a shape that gradually becomes thicker from the base end toward the tip end.

[0016] At this time, it is preferably as follows: the process of forming at least a part of the boiling face by stacking molding includes: the process of forming the protrusions by stacking molding in a manner of arranging a plurality of protrusions in a matrix in the first direction and the second direction, and the first direction and the second direction are approximately orthogonal to each other in a plane approximately parallel to the boiling face. If it is constructed in this way, a boiling face in which the protrusions are evenly arranged can be obtained. As a result, since the protrusions are not arranged eccentrically, the effect of improving the boiling heat transfer performance of the boiling face by filling the refrigerant between the protrusions can be equally exerted at any position on the boiling face.

[0017] In the structure in which a plurality of the above-mentioned protrusions are arranged, it is preferably as follows: the process of forming at least a part of the boiling face portion by stacking molding includes: a process of forming linear protrusions and protrusions by stacking molding in a manner in which a plurality of linear protrusions extending along a first direction in a plane substantially parallel to the boiling face portion are arranged in a second direction substantially orthogonal to the first direction in a plane substantially parallel to the boiling face portion, and a plurality of protrusions are arranged on the linear protrusions and between the linear protrusions in the second direction. If constructed in this manner, a boiling face portion that combines protrusions having a shape that gradually becomes thicker from the base end toward the tip and linear protrusions can be obtained. As a result, the heat transfer area can be increased by the linear protrusions, and the effect of improving the boiling heat transfer performance of the boiling face portion by filling the spaces between the protrusions with refrigerant can be obtained.

[0018] In the structure in which a plurality of the above-mentioned protrusions are arranged, it is preferably as follows: the process of forming at least a portion of the boiling face portion by stacking molding includes the process of forming the protrusions by stacking molding in a manner in which a plurality of protrusions are arranged at a pitch smaller than the width of the protrusions. Here, if the pitch of the protrusions becomes too large, the number of protrusions that can be arranged on the boiling face portion will decrease, and thus the boiling heat transfer performance of the boiling face portion will decrease. Therefore, if constructed in the above manner, it is possible to suppress the pitch of the protrusions from becoming too large, and thus it is possible to suppress the number of protrusions that can be arranged on the boiling face portion from being excessively reduced. As a result, the boiling heat transfer performance of the boiling face portion can be appropriately set.

[0019] In the above-mentioned first invention, it is preferably as follows: the process of forming at least a part of the boiling face portion by stacking molding includes: a process of forming linear protrusions by stacking molding in a manner that a plurality of linear protrusions extending along a first direction in a plane substantially parallel to the boiling face portion are arranged in a second direction substantially orthogonal to the first direction in a plane substantially parallel to the boiling face portion; or a process of forming a stacked molding body including pits by stacking molding in a manner that a plurality of pits having a shape that gradually becomes thicker from the opening toward the bottom are arranged. If constructed in this manner, a boiling face portion in which a plurality of linear protrusions are arranged or a boiling face portion in which a plurality of pits are arranged can be obtained. In the case of obtaining a boiling face portion in which a plurality of linear protrusions are arranged, the boiling face portion can be set to a simple shape. In addition, in the case of obtaining a boiling face portion in which a plurality of pits are arranged, since the pits easily generate bubbles due to boiling and have a shape that gradually becomes thicker from the opening toward the bottom, the boiling heat transfer performance of the boiling face portion can be improved. In addition, the inventors of the present application have confirmed in the experiments described later that a boiling face with high boiling heat transfer performance can be obtained by forming linear protrusions through stacking molding in the form of arranging multiple linear protrusions, or forming a stacked molding body including pits through stacking molding in the form of arranging multiple pits.

[0020] In the first invention, it is preferred that the step of forming at least a portion of the boiling face portion by stacking molding includes the step of forming the boiling face portion without sandblasting after the stacking molding. If configured in this manner, since sandblasting is not performed after the stacking molding, it is possible to avoid the removal of minute irregularities on the surface of the boiling face portion by sandblasting, thereby obtaining a boiling face portion with high boiling heat transfer performance. Furthermore, compared with the case of performing sandblasting, the manufacturing process of the boiling cooler can be simplified.

[0021] The boiling cooler based on the second invention comprises: a boiling section, which boils the refrigerant through heat exchange with the heat generating element; and a condensing section, which condenses the refrigerant boiled by the boiling section and returns it to the boiling section, wherein the boiling section includes: a mounting surface of the heat generating element; and a boiling surface portion, which is arranged on a surface opposite to the mounting surface and in contact with the refrigerant, at least a portion of which is formed by stacked molding.

[0022] In the boiling cooler based on the second invention, as described above, the boiling portion is formed in a manner that includes a surface provided on the side opposite to the mounting surface and in contact with the refrigerant and at least a portion of which is formed by stacking molding. Therefore, a boiling surface having high boiling heat transfer performance can be obtained by stacking molding, and the boiling surface can be obtained by stacking molding in a simple process. As a result, a boiling cooler can be provided that can obtain a boiling surface having high boiling heat transfer performance by a simple process.

[0023] The boiling cooler based on the third invention comprises: a boiling section, which boils the refrigerant through heat exchange with the heating element; and a condensing section, which condenses the refrigerant boiled by passing through the boiling section and returns it to the boiling section, the boiling section comprising: a mounting surface of the heating element; and a boiling surface section, which is arranged on the side opposite to the mounting surface and contacts the refrigerant, the boiling surface section being constituted by arranging a plurality of protrusions having a shape that gradually becomes thicker from the base end toward the tip.

[0024] In the boiling cooler based on the third invention, as described above, a plurality of protrusions having a shape that gradually becomes thicker from the base end toward the tip end are arranged to form a boiling surface. Thus, a boiling surface that can be filled with refrigerant between the protrusions can be obtained. As a result, when the refrigerant boils on the protrusions and the surroundings thereof, the refrigerant filled between the protrusions can be quickly supplied, thereby suppressing the protrusions and the surroundings where the refrigerant boils from drying out. Thus, a situation in which boiling cannot be performed due to drying out of the protrusions and the surroundings thereof can be avoided, thereby improving the boiling heat transfer performance of the boiling surface.

[0025] In the third invention, the boiling surface is preferably configured as follows: the boiling surface is configured by arranging a plurality of protrusions in a matrix in the first direction and the second direction, and the first direction and the second direction are substantially orthogonal to each other in a plane substantially parallel to the boiling surface. If configured in this manner, a boiling surface in which the protrusions are evenly arranged can be obtained. As a result, since the protrusions are not eccentrically arranged, the effect of improving the boiling heat transfer performance of the boiling surface by filling the protrusions with refrigerant can be equally exerted at any position of the boiling surface.

[0026] In the third invention, it is preferred that the boiling surface is configured as follows: the boiling surface is configured as a plurality of linear protrusions extending in the first direction in a plane roughly parallel to the boiling surface arranged in the second direction, and a plurality of protrusions are arranged on the linear protrusions and between the linear protrusions in the second direction, and the second direction is roughly orthogonal to the first direction in a plane roughly parallel to the boiling surface. If configured in this manner, a boiling surface can be obtained that combines protrusions having a shape that gradually becomes thicker from the base end toward the tip and linear protrusions. As a result, the heat transfer area can be increased by the linear protrusions, and the effect of improving the boiling heat transfer performance of the boiling surface by filling the spaces between the protrusions with refrigerant can be obtained.

[0027] In the third invention, the boiling face portion is preferably configured as follows: the boiling face portion is configured to arrange a plurality of protrusions at a pitch smaller than the width of the protrusion. If configured in this manner, if the pitch of the protrusions becomes too large, the number of protrusions that can be arranged on the boiling face portion is reduced, and thus the boiling heat transfer performance of the boiling face portion is reduced. Therefore, if configured in the above manner, it is possible to suppress the pitch of the protrusions from becoming too large, and thus it is possible to suppress the number of protrusions that can be arranged on the boiling face portion from being excessively reduced. As a result, the boiling heat transfer performance of the boiling face portion can be appropriately set.

[0028] Effects of the Invention

[0029] According to the present invention, as described above, a boiling surface portion having high boiling heat transfer performance can be obtained by a simple process. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] Figure 1 This is a schematic perspective view showing the boiling cooler according to the first embodiment.

[0031] Figure 2 This is a schematic exploded perspective view (1) showing a boiling cooler according to a first embodiment.

[0032] Figure 3 This is a schematic exploded perspective view (2) showing the boiling cooler according to the first embodiment.

[0033] Figure 4 This is a schematic perspective view showing a first example of a boiling surface.

[0034] Figure 5 yes Figure 4 Schematic partial cross-sectional view of the boiling face.

[0035] Figure 6 This is a schematic perspective view showing a second example of the boiling surface.

[0036] Figure 7 yes Figure 6 Schematic partial cross-sectional view of the boiling face.

[0037] Figure 8 This is a schematic perspective view showing a third example of the boiling surface.

[0038] Fig. 9 yes Figure 8 Schematic partial cross-sectional view of the boiling face.

[0039] Fig.10 It is a schematic stereoscopic diagram showing the fourth example of the boiling surface.

[0040] Fig.11 yes Fig.10 Schematic partial cross-sectional view of the boiling face.

[0041] Fig.12 This is a schematic perspective view showing the fifth example of the boiling surface.

[0042] Fig.13 yes Fig.12 Schematic partial cross-sectional view of the boiling face.

[0043] Fig.14 This is a diagram for explaining how to install the mounting portion of the boiling cooler based on the first embodiment to the condensing portion.

[0044] Fig.15 This is a diagram for explaining how the heat generating element of the boiling cooler according to the first embodiment is mounted on a mounting portion.

[0045] Fig.16 This is a diagram for explaining a state in which a heat generating element is mounted on the boiling cooler according to the first embodiment.

[0046] Fig.17 This is a schematic exploded perspective view showing a boiling cooler according to a first modification example of the first embodiment.

[0047] Fig.18 This is a schematic exploded perspective view showing a boiling cooler according to a second modification example of the first embodiment.

[0048] Fig.19 This is a schematic perspective view showing a boiling cooler according to the second embodiment.

[0049] Fig. 20 This is a schematic exploded perspective view (1) showing a boiling section of a boiling cooler according to a second embodiment.

[0050] Fig.21 This is a schematic exploded perspective view (2) showing a boiling section of a boiling cooler according to a second embodiment.

[0051] Fig. 22 This is a diagram for explaining how to attach the attachment portion of the ebullient cooler according to the second embodiment to the evaporator body.

[0052] Fig.23 This is a diagram for explaining how the evaporation section of the boiling cooler according to the second embodiment is mounted on the condensation section.

[0053] Fig.24 This is a diagram for explaining a state in which a heat generating element is mounted on a boiling cooler according to the second embodiment.

[0054] Fig.25 This is a schematic exploded perspective view showing an evaporation portion of an ebullient cooler according to a first modified example of the second embodiment.

[0055] Fig.26 This is a schematic exploded perspective view showing an evaporation portion of an ebullient cooler according to a second modification of the second embodiment.

[0056] Fig. 27 It is a graph showing the boiling heat transfer performance measurement results of the boiling surfaces of Example 1 and the comparative example.

[0057] Fig.28 It is a graph showing the boiling heat transfer performance measurement results of the boiling surfaces of Example 2 and the comparative example.

[0058] Fig.29 It is a graph showing the boiling heat transfer performance measurement results of the boiling surfaces of Example 3 and the comparative example.

[0059] Fig.30 It is a graph showing the boiling heat transfer performance measurement results of the boiling surfaces of Example 4 and the comparative example.

[0060] Fig.31 This is a graph showing the results of measuring the boiling heat transfer performance of the boiling surfaces of Examples 1 to 4. DETAILED DESCRIPTION

[0061] Hereinafter, embodiments of the present invention will be described with reference to the accompanying drawings.

[0062] [First embodiment]

[0063] refer to Figures 1 to 13 , the structure of the boiling cooler 100 (hereinafter referred to as cooler 100) based on the first embodiment is described. The cooler 100 is a cooler based on the boiling cooling method that utilizes the phase change (latent heat) of gasification and condensation of the refrigerant to absorb heat from the heating element HS and dissipate it to the outside. The heating element HS is, for example, a CPU (central processing unit). The heating element HS is not particularly limited. The refrigerant is, for example, a fluorocarbon, a hydrocarbon, or water. The refrigerant is not particularly limited.

[0064] Hereinafter, two directions substantially orthogonal to each other in a horizontal plane are referred to as the X direction and the Y direction. A vertical direction substantially orthogonal to the horizontal plane (XY plane) is referred to as the Z direction. In addition, the Z direction is a direction parallel to the direction of gravity and in which gravity acts downward.

[0065] like Figures 1 to 3 As shown, the cooler 100 includes a boiling section 10 and a condensing section 20. The boiling section 10 boils the refrigerant by heat exchange with the heating element HS. The condensing section 20 condenses the refrigerant that has boiled through the boiling section 10 and returns it to the boiling section 10. The boiling section 10 and the condensing section 20 in the first embodiment are integrated.

[0066] The boiling section 10 includes a mounting portion 11 and a receiving portion 12 (see Figure 3 ). The mounting portion 11 is in the shape of a plate extending in the horizontal direction. And, the surface on the lower side (Z2 direction side) of the mounting portion 11 is the mounting surface 11a of the heating element HS. In the mounting portion 11, a boiling surface portion 13 is provided on the surface 11b on the upper side (Z1 direction side) on the side opposite to the mounting surface 11a. The receiving portion 12 receives liquid refrigerant. The receiving portion 12 is divided by a hole portion 20a formed in the condensation portion 20 and a surface 11b of the mounting portion 11. The receiving portion 12 is provided as a recessed portion that is recessed downward (Z2 direction). In the receiving portion 12, the boiling surface portion 13 is in contact with the liquid refrigerant. In addition, details about the boiling surface portion 13 will be described later.

[0067] The condensation section 20 is composed of a plate-fin heat exchanger. The condensation section 20 includes a refrigerant channel 21 and an external channel 22. The refrigerant channel 21 and the external channel 22 are alternately arranged with a partition in between. The refrigerant channel 21 is a flow path for the refrigerant to flow. The refrigerant channel 21 is connected to the receiving section 12 of the boiling section 10. Specifically, the refrigerant channel 21 in the first section (closest to the Z2 direction side) is connected to the receiving section 12 of the boiling section 10, and the refrigerant channels 21 above the second section are also connected internally. The refrigerant flows in all the refrigerant channels 21. Corrugated fins 21a extending along the X direction are arranged in the refrigerant channel 21 (refer to Figure 3 ). The external channel 22 is a flow path for an external fluid to flow. The external fluid is a fluid that cools the refrigerant, such as air. The external fluid is not particularly limited. The external channel 22 opens to the outside. A corrugated fin 22a extending along the Y direction is arranged in the external channel 22.

[0068] When the heat of the heating element HS is transferred to the boiling surface portion 13 via the mounting portion 11, the liquid refrigerant in the receiving portion 12 is heated and boils. The refrigerant vaporized by boiling moves to the refrigerant channel 21 connected to the receiving portion 12, and is cooled and condensed by the external fluid flowing in the external channel 22. The refrigerant liquefied by condensation moves in the refrigerant channel 21 and returns to the receiving portion 12. In this way, the refrigerant sealed in the cooler 100 circulates between the boiling portion 10 and the condensing portion 20. As a result, the heating element HS is cooled.

[0069] (Structure of boiling face)

[0070] Here, in the first embodiment, at least a portion of the boiling face portion 13 is formed by stacking molding. Specifically, at least a portion of the boiling face portion 13 is formed by stacking molding using metal powder. More specifically, at least a portion of the boiling face portion 13 is formed by powder bed fusion (PBF: Powder Bed Fusion) as a stacking molding. Powder bed fusion is a stacking molding that forms a three-dimensional stacked molding body (such as the boiling face portion 13) by repeatedly performing a process of forming a metal powder layer and a process of irradiating a molding portion of the formed metal powder layer with a high-energy beam (laser, electron beam, etc.) to sinter (melt / harden) the metal powder of the molding portion. On the surface of the boiling face portion 13 formed by stacking molding, there are tiny bumps and depressions generated when the metal powder is sintered using a high-energy beam. In addition, the metal powder used in the stacking molding, that is, the material of the boiling face portion 13 is not particularly limited, and can be, for example, aluminum (including aluminum alloys). In the case of aluminum, for example, a silicon-based aluminum alloy called Al-Si10-Mg can be used.

[0071] refer to Figures 4 to 13 , a structural example of the boiling surface 13 is described. In addition, in the following, two directions approximately orthogonal to each other in a plane approximately parallel to the boiling surface 13 are respectively set as direction A and direction B. The direction approximately orthogonal to the plane approximately parallel to the boiling surface 13 is set as direction C. In the first embodiment, direction C is consistent with direction Z, direction C1 is consistent with direction Z1, and direction C2 is consistent with direction Z2. The portion of the boiling surface 13 on the C2 direction side is joined to the surface 11b of the mounting portion 11. In addition, direction A and direction B are examples of the "first direction" and "second direction" in the claims, respectively.

[0072] (The first case of boiling face)

[0073] Figure 4 and Figure 5 The first example is shown in FIG. In the first example, the boiling surface 13 is configured to arrange a plurality of linear protrusions 13a extending in the A direction in the B direction. The plurality of linear protrusions 13a are provided on the bottom plate 13b and protrude from the bottom plate 13b toward the C1 direction. Furthermore, by arranging a plurality of linear protrusions 13a extending in the A direction in the B direction, a plurality of grooves extending in the A direction and recessed toward the C2 direction are arranged in the B direction between each linear protrusion 13a in the B direction. The linear protrusions 13a are in the shape of a cube.

[0074] The linear protrusion 13a has a width W1 and a height H1. The width W1 is the length of the linear protrusion 13a in the B direction. The height H1 is the length of the linear protrusion 13a in the C direction. Furthermore, the linear protrusions 13a are arranged in the B direction at a pitch P1. The pitch P1 is the distance between adjacent linear protrusions 13a in the B direction. The pitch P1 is also the width of the groove in the B direction. Figure 4 and Figure 5 In the example shown, the width W1, the height H1, and the pitch P1 are the same length, but there is no particular limitation. For example, the width W1, the height H1, and the pitch P1 are approximately 2 mm.

[0075] (The second case of boiling face)

[0076] Figure 6 and Figure 7 The second example is shown. In the second example, the boiling surface 13 is constructed by arranging a plurality of protrusions 13c having a shape that gradually becomes thicker from the base end (C2 direction side) toward the tip end (C1 direction side). Specifically, the boiling surface 13 is constructed by arranging a plurality of protrusions 13c in a matrix in the A direction and the B direction. The plurality of protrusions 13c are provided on the bottom plate 13b and protrude from the bottom plate 13b toward the C1 direction side. Furthermore, by arranging the plurality of protrusions 13c in a matrix in the A direction and the B direction, a space that can be filled with refrigerant is formed between the protrusions 13c. The protrusion 13c is in the shape of a regular quadrangular pyramid that gradually becomes thicker from the C2 direction side toward the C1 direction side. The protrusion 13c has an upper bottom on the C2 direction side, a lower bottom on the C1 direction side, and four conical surfaces connecting the upper bottom and the lower bottom.

[0077] The protrusion 13c has a width W2 and a height H2. The width W2 is the length of the lower bottom of the protrusion 13c in the A direction and the B direction. The height H2 is the length of the protrusion 13c in the C direction. In addition, each conical surface (side surface) of the protrusion 13c is inclined at an angle θ2 relative to the AB plane. In addition, the protrusions 13c are arranged in the A direction and the B direction at a pitch P2. The pitch P2 is the distance between adjacent protrusions 13c in the A direction and the B direction. Figure 6 and Figure 7 In the example shown, the width W2 and the height H2 are the same length, but there is no particular limitation. Figure 6 and Figure 7 In the example shown, the pitch P2 is smaller than the width W2. Figure 6 and Figure 7 The boiling surface 13 shown is configured to arrange a plurality of protrusions 13c at a pitch P2 smaller than the width W2 of the protrusions 13c. However, the pitch P2 is not particularly limited. For example, the width W2 and the height H2 are approximately 0.5 mm, the pitch P2 is approximately 0.4 mm, and the inclination angle θ2 is approximately 70 degrees.

[0078] (The third case of boiling face)

[0079] Figure 8 and Fig. 9 The third example is shown. In the third example, the boiling surface portion 13 is configured to arrange a plurality of linear protrusions 13d extending in the A direction in the B direction, and to arrange a plurality of protrusions 13c on the linear protrusions 13d and between the linear protrusions 13d in the B direction (i.e., grooves). The plurality of linear protrusions 13d are provided on the bottom plate 13b, and protrude from the bottom plate 13b toward the C1 direction side. Furthermore, by arranging a plurality of linear protrusions 13d extending in the A direction in the B direction, a plurality of grooves extending in the A direction and recessed toward the C2 direction side are arranged in the B direction between each of the linear protrusions 13d in the B direction. The linear protrusions 13d are prism-shaped with a conical surface 13da in the C2 direction side portion. The conical surface 13da is provided corresponding to the protrusions 13c arranged in the grooves. Specifically, the tapered surface 13da is provided at a position opposite to the protrusion 13c disposed in the groove and closest to the tapered surface 13da in the B direction, and is inclined toward the side of the protrusion 13c opposite to the tapered surface. The protrusions 13c are arranged in a matrix in the A direction and the B direction on either the linear protrusion 13d or the groove (on the bottom plate 13b).

[0080] The linear protrusion 13d has a width W3 and a height H3. The width W3 is the length of the linear protrusion 13d in the B direction. The height H3 is the length of the linear protrusion 13d in the C direction. Furthermore, the linear protrusions 13d are arranged in the B direction at a pitch P3. The pitch P3 is the distance between adjacent linear protrusions 13d in the B direction. The pitch P3 is also the width of the groove in the B direction. Figure 8 and Fig. 9 In the example shown, the height H3 is smaller than the width W3, and the pitch P3 is larger than the height H3, but there is no particular limitation. In addition, each tapered surface 13da of the linear protrusion 13d is inclined at an angle θ3 relative to the AB plane. The angle θ3 is the same as the angle θ2. For example, the width W3 is about 2.0 mm, the height H3 is about 1.5 mm, the pitch P3 is about 2.0 mm, and the angle θ3 is about 70 degrees.

[0081] (Case 4 of boiling face)

[0082] Fig.10 and Fig.11The fourth example is shown. In the fourth example, the boiling surface 13 is constructed by arranging a plurality of pits 13e having a shape that gradually becomes thicker from the opening (C1 direction side) toward the bottom (C2 direction side). Specifically, the boiling surface 13 is constructed by arranging a plurality of pits 13e in a matrix in the A direction and the B direction. The plurality of pits 13e are recessed toward the C2 direction side in the plate-shaped main body 13f. The pits 13e are in the shape of a regular quadrangular pyramid that gradually becomes thicker from the C1 direction side toward the C2 direction side. The pits 13e have a bottom on the C2 direction side, an opening on the C1 direction side, and four conical surfaces connecting the bottom and the opening. In a shape such as the pits 13e, bubbles are easily generated (easy to become the starting point of boiling), and the boiling heat transfer performance is improved. In addition, Figures 6 to 9 The cross-sectional shape of the space between the projections 13 c shown has the same shape as the cross-sectional shape of the recesses 13 e .

[0083] The pit 13e has a width W4 and a height H4. The width W4 is the length of the opening of the pit 13e in the A direction and the B direction. The height H4 is the length of the pit 13e in the C direction. In addition, each conical surface (side surface) of the pit 13e is inclined at an angle θ4 relative to the AB plane. In addition, the pits 13e are arranged in the A direction and the B direction at a pitch P4. The pitch P4 is the distance between adjacent pits 13e in the A direction and the B direction. Fig.10 and Fig.11 In the example shown, the pitch P4 and the height H4 are the same length, but there is no particular limitation. Fig.10 and Fig.11 In the example shown, the width W4 is smaller than the pitch P4 and the height H4, but there is no particular limitation. For example, the width W4 is about 0.4 mm, the height H4 is about 0.5 mm, the pitch P4 is about 0.5 mm, and the inclination angle θ4 is about 70 degrees.

[0084] (Case 5 of Boiling Face)

[0085] Fig.12 and Fig.13 The fifth example is shown. The boiling surface portion 13 of the fifth example is formed by removing the bottom plate 12b of the boiling surface portion 13 of the second example. The boiling surface portion 13 of the fifth example is not provided with the bottom plate 12b, and other than this, it has the same structure as the boiling surface portion 13 of the second example. That is, the boiling surface portion 13 of the fifth example is configured to arrange a plurality of protrusions 13c having a shape that gradually becomes thicker from the base end (C2 direction side) toward the tip end (C1 direction side). Specifically, the boiling surface portion 13 is configured to arrange a plurality of protrusions 13c in a matrix shape in the A direction and the B direction. In addition, the protrusions 13c of the fifth example are directly joined to the surface 11b of the mounting portion 11 by stacking molding.

[0086] (Method for manufacturing a boiling cooler)

[0087] refer to Figures 14 to 16 , a method for manufacturing the cooler 100 according to the first embodiment will be described.

[0088] like Fig.14 As shown, the manufacturing method of the cooler 100 includes a step of forming the condensation unit 20. The step of forming the condensation unit 20 includes: forming the condensation unit 20 by joining the refrigerant channel forming portion 21b to be the refrigerant channel 21 and the external channel forming portion 22b to be the external channel 22. Fig.15 As shown, the manufacturing method of the cooler 100 includes a step of forming the boiling portion 10. The step of forming the boiling portion 10 includes: a step of forming the boiling surface portion 13; and a step of joining the mounting portion 11 to the condensing portion 20.

[0089] Here, in the first embodiment, the process of forming the boiling face portion 13 is a process of forming at least a portion of the boiling face portion 13 by stacking molding. Specifically, the process of forming the boiling face portion 13 includes: a process of forming at least a portion of the boiling face portion 13 by stacking molding using metal powder. More specifically, the process of forming the boiling face portion 13 includes: a process of forming at least a portion of the boiling face portion 13 by fusion of a powder bed as a stacking molding. That is, the process of forming the boiling face portion 13 includes: a process of forming at least a portion of the boiling face portion 13 by repeatedly performing a process of forming a metal powder layer and a process of irradiating a molding portion of the formed metal powder layer with a high-energy beam to sinter the metal powder of the molding portion. At this time, minute bumps and depressions generated when the metal powder is sintered by a high-energy beam are formed on the surface of the boiling face portion 13 as a stacked molding.

[0090] Furthermore, the process of forming the boiling surface 13 includes, in the case of the first example, a process of forming the linear protrusions 13a by stacking molding in a manner that a plurality of linear protrusions 13a extending along the A direction are arranged in the B direction. Furthermore, the process of forming the boiling surface 13 includes, in the case of the second, third and fifth examples, a process of forming the protrusions 13c by stacking molding in a manner that a plurality of protrusions 13c having a shape that gradually becomes thicker from the base end toward the tip end are arranged. Furthermore, the process of forming the boiling surface 13 includes, in the case of the second and fifth examples, a process of forming the protrusions 13c by stacking molding in a manner that a plurality of protrusions 13c are arranged in a matrix in the A direction and the B direction. In addition, in the case of the first, second and third examples, the bottom plate 13b is also formed by stacking molding, and in the case of the fifth example, the bottom plate 13b is not formed. Furthermore, the step of forming the boiling surface portion 13 in the second and fifth examples includes a step of forming the protrusions 13c by stacking molding in such a manner that a plurality of protrusions 13c are arranged at a pitch smaller than the width of the protrusions 13c.

[0091] Furthermore, the process of forming the boiling surface portion 13 in the case of the third example includes: a process of forming the linear protrusions 13d and the protrusions 13c by stacking molding in a manner that a plurality of linear protrusions 13d extending along the A direction are arranged in the B direction and a plurality of protrusions 13c are arranged on the linear protrusions 13d and between the linear protrusions 13d in the B direction. Furthermore, the process of forming the boiling surface portion 13 in the case of the fourth example includes: a process of forming a stacked molding body including the pits 13e by stacking molding in a manner that a plurality of pits 13e having a shape that gradually becomes thicker from the opening toward the bottom are arranged. In addition, in the first to fifth examples above, the entire boiling surface portion 13 is formed by stacking molding.

[0092] Furthermore, in the first embodiment, the process of forming the boiling surface portion 13 includes the process of forming the boiling surface portion 13 without performing sandblasting after the lamination molding. That is, the boiling surface portion 13 is not subjected to surface processing by sandblasting, but is used in the cooler 100 in the surface state formed by lamination molding. That is, the boiling surface portion 13 is used in the cooler 100 in a state where there are minute concavoconvexities generated by sintering the metal powder using a high-energy beam. In addition, the boiling surface portion 13 may also be subjected to heat treatment.

[0093] Furthermore, the process of forming the boiling surface portion 13 includes: a process of joining the boiling surface portion 13 to the surface 11b on the side opposite to the mounting surface 11a of the heating element HS of the mounting portion 11. The process of joining the boiling surface portion 13 to the surface 11b is not particularly limited, but includes: a process of directly joining the boiling surface portion 13 to the surface 11b by stacking molding, or a process of joining the boiling surface portion 13 as a stacked molding body formed by stacking molding to the surface 11b by a joining method such as welding, fusion or friction stir joining. In the cases of the first to fourth examples above, the boiling surface portion 13 may be joined to the surface 11b by any method. In the case of the fifth example above, the boiling surface portion 13 is directly joined to the surface 11b by stacking molding. After the boiling surface portion 13 is joined to the surface 11b, the process of joining the mounting portion 11 to the condensation portion 20 is performed.

[0094] The process of joining the mounting portion 11 to the condensation portion 20 includes: joining the mounting portion 11 to the condensation portion 20 by welding. At this time, for example, the four sides of the mounting portion 11 that are tangent to the condensation portion 20 are welded. And, by joining the mounting portion 11 to the condensation portion 20 by welding, the receiving portion 12 is formed. Thus, the boiling portion 10 is formed and the cooler 100 is completed. And, as Fig.16 As shown, a heat generating element HS is mounted on the mounting surface 11 a of the mounting portion 11 .

[0095] (Effects of the First Embodiment)

[0096] In the first embodiment, the following effects can be obtained.

[0097] Therefore, the boiling surface 13 with high boiling heat transfer performance can be obtained by stacking molding, and by using stacking molding, the boiling surface 13 can be obtained by a simple process without going through many individual processes. As a result, the boiling surface 13 with high boiling heat transfer performance can be obtained by a simple process.

[0098] Furthermore, in the first embodiment, by using the layered molding of metal powder, the boiling surface portion 13 having minute irregularities on the surface can be obtained. As a result, boiling can be promoted by the minute irregularities on the surface, so that the boiling surface portion 13 having higher boiling heat transfer performance can be obtained.

[0099] Furthermore, in the first embodiment, the boiling surface portion 13 having minute irregularities on the surface can be easily obtained by powder bed fusion, and thus the boiling surface portion 13 having higher boiling heat transfer performance can be easily obtained.

[0100] Furthermore, in the first embodiment, the protrusions 13c are formed by stacking the protrusions 13c in a manner of arranging a plurality of protrusions 13c having a shape that gradually becomes thicker from the base end toward the terminal end, thereby obtaining a boiling surface 13 having a space between the protrusions 13c that can be filled with refrigerant. As a result, when the refrigerant boils in the protrusions 13c and the surroundings thereof, the refrigerant that fills the space between the protrusions 13c can be quickly supplied, thereby suppressing the protrusions 13c and the surroundings where the refrigerant boils from drying out. Thus, a situation in which boiling is hindered due to drying out of the protrusions 13c and the surroundings thereof can be avoided, thereby improving the boiling heat transfer performance of the boiling surface 13. Furthermore, although the plurality of protrusions 13c having a shape that gradually becomes thicker from the base end toward the terminal end is difficult to be formed by machining such as cutting, they can be easily formed by stacking the protrusions 13c.

[0101] Furthermore, in the first embodiment, the protrusions 13c are formed by stacking the protrusions 13c in a matrix shape in the A direction and the B direction, and thus the boiling surface portion 13 in which the protrusions 13c are evenly arranged can be obtained, wherein the A direction and the B direction are substantially orthogonal to each other in a plane substantially parallel to the boiling surface portion 13. As a result, since the protrusions 13c are not eccentrically arranged, the effect of improving the boiling heat transfer performance of the boiling surface portion 13 by filling the spaces between the protrusions 13c with refrigerant can be equally exerted at any position of the boiling surface portion 13.

[0102] Furthermore, in the first embodiment, a plurality of linear protrusions 13d extending along the A direction within a plane approximately parallel to the boiling surface portion 13 are arranged in a B direction approximately orthogonal to the A direction within a plane approximately parallel to the boiling surface portion 13, and a plurality of protrusions 13c are arranged on the linear protrusions 13d and between the linear protrusions 13d in the B direction, and the linear protrusions 13d and the protrusions 13c are formed by stacking molding, thereby obtaining a boiling surface portion 13 that combines the protrusions 13c and the linear protrusions 13d having a shape that gradually becomes thicker from the base end toward the tip.

[0103] As a result, the heat transfer area can be increased by the linear protrusions 13d, and the boiling heat transfer performance of the boiling surface portion 13 can be improved by filling the space between the protrusions 13c with refrigerant.

[0104] Furthermore, in the first embodiment, a plurality of protrusions 13c are arranged at a pitch P2 that is smaller than a width W2 of the protrusion 13c. Here, when the pitch P2 of the protrusions 13c becomes too large, the number of protrusions 13c that can be arranged on the boiling surface portion 13 is reduced, and thus the boiling heat transfer performance of the boiling surface portion 13 is reduced. Therefore, if configured in the above manner, it is possible to suppress the pitch P2 of the protrusions 13c from becoming too large, and thus it is possible to suppress the number of protrusions 13c that can be arranged on the boiling surface portion 13 from being excessively reduced. As a result, the boiling heat transfer performance of the boiling surface portion 13 can be appropriately set.

[0105] Furthermore, in the first embodiment, when a boiling surface portion 13 having a plurality of linear protrusions 13a is obtained, the boiling surface portion 13 can be made into a simple shape. Furthermore, when a boiling surface portion 13 having a plurality of recesses 13e is obtained, since the recesses 13e are easy to generate bubbles due to boiling and have a shape that gradually becomes thicker from the opening toward the bottom, the boiling heat transfer performance of the boiling surface portion 13 can be improved.

[0106] Furthermore, in the first embodiment, by forming the boiling surface portion 13 without sandblasting after the stacking molding, it is possible to avoid the micro-concavities and convexities on the surface of the boiling surface portion 13 being removed by the sandblasting, thereby obtaining the boiling surface portion 13 with high boiling heat transfer performance. Furthermore, compared with the case where the sandblasting is performed after the stacking molding, the manufacturing process of the boiling cooler 100 can be simplified.

[0107] (First Modification of First Embodiment)

[0108] refer to Fig.17 , a first modification of the first embodiment described above will be described. In this first modification, unlike the first embodiment described above in which the mounting portion 11 is joined to the condensation portion 20 by welding, an example in which the mounting portion 11 is joined to the condensation portion 20 by welding will be described.

[0109] like Fig.17 As shown, the process of joining the mounting portion 11 to the condensation portion 20 includes: joining the mounting portion 11 to the condensation portion 20 by welding. At this time, a brazing plate 30 having a core material and solder provided on both sides of the core material is provided between the condensation portion 20 and the mounting portion 11. The mounting portion 11 is welded to the condensation portion 20 via the brazing plate 30. And, Fig.17 In the example shown, a recess 11c is provided in the mounting portion 11 instead of the hole 20a of the first embodiment. When the mounting portion 11 is welded to the condensation portion 20, the receiving portion 12 is formed by the recess 11c. Thus, the boiling portion 10 is formed and the cooler 100 is completed. In addition, a heating element HS is mounted on the mounting surface 11a of the mounting portion 11.

[0110] (Second Modification of First Embodiment)

[0111] refer to Fig.18 , a second modification of the first embodiment is described. In the second modification, unlike the first embodiment in which the mounting portion 11 is joined to the condensation portion 20 by welding, an example in which the mounting portion 11 is joined to the condensation portion 20 by screwing is described.

[0112] like Fig.18 As shown, the process of joining the mounting portion 11 to the condensing portion 20 includes: a process of joining the mounting portion 11 to the condensing portion 20 by screwing. At this time, a through hole for the screw 40 is provided in the mounting portion 11, and a threading hole for the screw 40 is provided in the condensing portion 20. In addition, a sealing component 50 such as an O-ring is provided between the condensing portion 20 and the mounting portion 11. With the sealing component 50 sandwiched in the middle, the mounting portion 11 is screwed to the condensing portion 20 by the screw 40. Thus, the housing portion 12 is formed to form the boiling portion 10, and the cooler 100 is completed. In addition, when fixing with screws, the refrigerant can also be sealed in the housing portion 12 by the sealing component 50. In addition, a heating element HS is installed on the mounting surface 11a of the mounting portion 11.

[0113] [Second embodiment]

[0114] Next, refer to Figures 19 to 21 , the structure of a boiling type cooler 200 (hereinafter referred to as cooler 200) based on the second embodiment of the present invention is described. In the second embodiment, unlike the first embodiment in which the boiling section 10 and the condensing section 20 are integrated, an example in which the boiling section 210 and the condensing section 220 are separated is described. In addition, for the same structure as the first embodiment, the same reference numerals are used and their descriptions are omitted.

[0115] like Figures 19 to 21As shown, the cooler 200 includes a boiling section 210, a condensing section 220 and a connecting section 260. The boiling section 210 boils the refrigerant by heat exchange with the heating element HS. The condensing section 220 condenses the refrigerant that has boiled through the boiling section 210 and returns it to the boiling section 210. The connecting section 260 is a connecting pipe that connects the boiling section 210 and the condensing section 220 and communicates them. In the second embodiment, the boiling section 210 and the condensing section 220 are separate types.

[0116] The boiling section 210 includes a mounting portion 11 and a receiving portion 212 (see Fig.21 ). The receiving portion 212 receives liquid refrigerant. The receiving portion 212 is divided by a recess 214a formed in the main body 214 of the boiling portion 210 and a surface 11b of the mounting portion 11. The receiving portion 212 is provided as a box-shaped space. In the receiving portion 212, the boiling surface portion 13 is in contact with the liquid refrigerant. In addition, the boiling surface portion 13 is the same as the first embodiment described above, and therefore will not be described in detail, but is formed by stacking molding.

[0117] The condensation section 220 is composed of a plate-fin heat exchanger. The condensation section 220 includes a refrigerant channel 221 and an external channel 222. The refrigerant channel 221 and the external channel 222 are alternately arranged with a partition in between. The refrigerant channel 221 is a flow path for the refrigerant to circulate. The refrigerant channel 221 is connected to the receiving section 212 of the boiling section 10 via the connecting section 260. Corrugated fins extending along the X direction are arranged in the refrigerant channel 221. The external channel 222 is a flow path for the external fluid to circulate. The external channel 222 opens to the outside. Corrugated fins 222a extending along the Y direction are arranged in the external channel 222.

[0118] When the heat of the heating element HS is transferred to the boiling surface portion 13 via the mounting portion 11, the liquid refrigerant in the receiving portion 212 is heated and boils. The refrigerant vaporized by boiling moves to the refrigerant channel 221 connected to the receiving portion 212 via the connecting portion 260, and is cooled and condensed by the external fluid flowing in the external channel 222. The refrigerant liquefied by condensation moves in the refrigerant channel 221 and the connecting portion 260 and returns to the receiving portion 212. In this way, the refrigerant sealed in the cooler 200 circulates between the boiling portion 210 and the condensing portion 220. As a result, the heating element HS is cooled.

[0119] (Method for manufacturing a boiling cooler)

[0120] refer to Figure 22 to Figure 24 , a method for manufacturing the cooler 200 according to the second embodiment will be described.

[0121] like Fig. 22As shown, the manufacturing method of the cooler 200 includes a process of forming a boiling portion 210. The process of forming the boiling portion 210 includes: a process of forming a boiling surface portion 13; and a process of joining the mounting portion 11 to the main body 214. The process of forming the boiling surface portion 13 is the same as that of the first embodiment described above, so it will not be described in detail, but it is a process of forming at least a part of the boiling surface portion 13 by stacking molding.

[0122] The process of joining the mounting portion 11 to the main body 214 includes: joining the mounting portion 11 to the main body 214 by welding. At this time, for example, the four sides of the mounting portion 11 that are tangent to the main body 214 are welded. And, by joining the mounting portion 11 to the main body 214 by welding, the receiving portion 212 is formed. Thus, the boiling portion 210 is formed. Fig.23 As shown, the manufacturing method of the cooler 200 includes a process of forming the condensation section 220. The process of forming the condensation section 220 includes: a process of forming the condensation section 220 by joining the refrigerant channel forming part 221b that will become the refrigerant channel 221 and the external channel forming part 222b that will become the external channel 222. In addition, the manufacturing method of the cooler 200 includes: a process of joining the boiling section 210 and the condensation section 220 via the connecting part 260. Thereafter, the cooler 200 is completed. In addition, as Fig.24 As shown, a heat generating element HS is mounted on the mounting surface 11 a of the mounting portion 11 .

[0123] The other structures of the second embodiment are the same as those of the above-mentioned first embodiment.

[0124] (Effects of the Second Embodiment)

[0125] In the manufacturing method of the boiling cooler 200 of the second embodiment, at least a portion of the boiling surface 13 which is provided on the surface 11b of the heating element HS on the opposite side to the mounting surface 11a and in contact with the refrigerant is formed by stacking molding, thereby, as in the above-mentioned first embodiment, a boiling surface 13 with high boiling heat transfer performance can be obtained by a simple process.

[0126] The other effects of the second embodiment are the same as those of the above-mentioned first embodiment.

[0127] (First Modification of Second Embodiment)

[0128] refer to Fig.25 , a first modification of the second embodiment will be described. Unlike the second embodiment in which the mounting portion 11 is joined to the main body 214 by welding, the first modification will be described in which the mounting portion 11 is joined to the main body 214 by welding.

[0129] like Fig.25As shown, the process of joining the mounting portion 11 to the main body 214 includes: a process of joining the mounting portion 11 to the main body 214 by welding. At this time, a brazing plate 230 having a core material and solder provided on both sides of the core material is provided between the main body 214 and the mounting portion 11. The mounting portion 11 is welded to the main body 214 via the brazing plate 230. When the mounting portion 11 is welded to the main body 214, the accommodating portion 212 is formed. Thus, the boiling portion 210 is formed and the cooler 200 is completed. In addition, a heating element HS is installed on the mounting surface 11a of the mounting portion 11.

[0130] (Second Modification of Second Embodiment)

[0131] refer to Fig.26 A second modification of the second embodiment will be described. In the second modification, unlike the first embodiment in which the mounting portion 11 is joined to the main body 214 by welding, an example in which the mounting portion 11 is joined to the main body 214 by screwing will be described.

[0132] like Fig.26 As shown, the process of joining the mounting portion 11 to the main body 214 includes: the process of joining the mounting portion 11 to the main body 214 by screwing. At this time, a through hole for the screw 240 is provided in the mounting portion 11, and a threaded hole for the screw 240 is provided in the main body 214. In addition, a sealing component 250 such as an O-ring is provided between the main body 214 and the mounting portion 11. With the sealing component 250 sandwiched in the middle, the mounting portion 11 is screwed to the main body 214 by the screw 240. Thus, the accommodating portion 212 is formed to form the boiling portion 210, and the cooler 200 is completed. In addition, when fixing with screws, the refrigerant can also be sealed in the accommodating portion 212 by the sealing component 250. In addition, a heating element HS is installed on the mounting surface 11a of the mounting portion 11.

[0133] [Example]

[0134] refer to Figures 27 to 31 , the measurement results of the boiling heat transfer performance of the boiling face are explained.

[0135] Figures 27 to 31 In the embodiment 1 to 4, each of the test coolers has a boiling surface in the shape of the above-mentioned 1st to 4th examples formed by stacking molding. The sizes of the protrusions, linear protrusions and pits on the boiling surface of the embodiments 1 to 4 are the values ​​described in the above-mentioned first embodiment. The boiling surfaces of the embodiments 1 to 4 are formed by powder bed fusion. The comparative example is a test cooler having a boiling surface in the same shape as the above-mentioned 1st example formed by extrusion molding. The material of the boiling surfaces of the embodiments 1 to 4 and the comparative example is common (aluminum). The refrigerant is a hydrofluorocarbon.

[0136] For the coolers of Examples 1 to 4 and the comparative example, the boiling heat transfer performance was measured under the condition of heating with a test heating element. At this time, air was supplied to the external passage of the condensation section at a specified air volume. The refrigerant temperature in the receiving section and the maximum temperature of the mounting surface were measured, and the temperature difference ΔT between the refrigerant temperature in the receiving section and the maximum temperature of the mounting surface was obtained as an indicator of the boiling heat transfer performance. The smaller the temperature difference ΔT, the higher the boiling thermal conductivity coefficient, and the higher the boiling heat transfer performance (cooling performance) of the boiling surface. In addition, the heat generation (heat flux) of the heating element is changed in stages to obtain the temperature difference ΔT in each heat flux.

[0137] Figures 27 to 30 A graph showing individual measurement results of Examples 1 to 4. Fig.31 A graph compiling the measurement results of Examples 1 to 4 is shown. Figures 27 to 31 In each graph, the horizontal axis represents the heat flux [W / cm2] of the heat generating element, and the vertical axis represents the temperature difference ΔT [K].

[0138] from Figures 27 to 30 As can be seen from the graph, according to the boiling faces of Examples 1 to 4, the temperature difference ΔT is reduced, and the boiling heat transfer performance (cooling performance) is improved compared to the existing boiling faces of the comparative example that are not subjected to stacking molding. Moreover, if we focus on the boiling face of Example 1 and the boiling face of the comparative example, even if the shapes are the same, the boiling heat transfer performance of the boiling face of Example 1 is higher. It is speculated that the reason for this is that the tiny bumps on the surface of the boiling face formed by stacking molding (powder bed fusion) help promote boiling. Specifically, it is speculated that the boiling heat transfer performance is improved because the bumps on the surface of the boiling face function as the generation point of bubbles (the starting point of boiling). From the measurement results, it can be seen that a boiling face with high boiling heat transfer performance can be obtained according to stacking molding.

[0139] And, from Fig.31 As can be seen from the graph, in the area with low heat flux, there is no significant difference in the temperature difference ΔT of any boiling surface in Examples 1 to 4, and there is no significant difference in boiling heat transfer performance. On the other hand, in the area with high heat flux, the boiling surfaces of Examples 2 to 4 have a lower temperature difference ΔT than the boiling surface of Example 1, and the boiling heat transfer performance (cooling performance) is improved. It is speculated that the reason is that in the area with high heat flux, the effect of the shape of the boiling surfaces of Examples 2 to 4 is exerted.

[0140] That is, for Examples 2 and 3, it is speculated that the reason is that the effect of arranging a plurality of protrusions having a shape that gradually becomes thicker from the base end toward the end is exerted. Specifically, the boiling surface of Examples 2 and 3 is a shape that can fill the space between the protrusions with refrigerant. Therefore, it is speculated that when the refrigerant boils on the protrusions and their surroundings, the refrigerant filling the space between the protrusions can be quickly supplied, so the protrusions and their surroundings are not easy to dry, and the boiling heat transfer performance is improved. And, with regard to Example 4, it is speculated that the reason is that the effect of arranging a plurality of pits having a shape that is easy to generate bubbles and gradually becomes thicker from the opening to the bottom is exerted. And, it is speculated that in areas with low heat flux, since the effects of these shapes do not have much influence, there is no significant difference in boiling heat transfer performance. From the measurement results, it can be seen that according to the boiling surface of arranging a plurality of protrusions having a shape that gradually becomes thicker from the base end to the end and the boiling surface of arranging a plurality of pits having a shape that gradually becomes thicker from the opening to the bottom, a boiling surface with higher boiling heat transfer performance can be obtained.

[0141] And, if Fig.31 As can be seen from the graph, in the area with high heat flux, the temperature difference ΔT of the boiling face of Example 2 is reduced compared to the boiling face of Example 3, and the boiling heat transfer performance (cooling performance) is improved. It can be inferred that the reason is that the boiling face of Example 2, which is provided with protrusions instead of linear protrusions, further exerts the above-mentioned effect of rapidly supplying refrigerant compared to the boiling face of Example 3, which is provided with both linear protrusions and protrusions. From the measurement results, it can be seen that according to the boiling face with multiple protrusions arranged instead of linear protrusions, a boiling face with higher boiling heat transfer performance is obtained.

[0142] [Modifications]

[0143] The embodiments disclosed herein are illustrative in all aspects and are not restrictive. The scope of the present invention is indicated by the technical claims rather than the description of the embodiments described above, and includes all modifications (variations) within the meaning and scope equivalent to the technical claims.

[0144] For example, although the first and second embodiments above illustrate a horizontal type boiling cooler with a horizontal boiling surface, the present invention is not limited thereto. The boiling surface of the boiling cooler of the present invention may also be a vertical type. Furthermore, the boiling cooler of the first and second embodiments above is only an example, and the shape or arrangement of each part of the boiling cooler is not particularly limited.

[0145] Furthermore, although the first and second embodiments described above illustrate an example in which the boiling surface portion is formed by powder bed fusion as a layered molding, the present invention is not limited thereto. The present invention may also form the boiling surface portion by layered molding other than powder bed fusion.

[0146] Furthermore, although the first and second embodiments illustrate an example in which a plurality of protrusions are arranged in a matrix and formed by stacking, the present invention is not limited thereto. The present invention can also form protrusions by arranging a plurality of protrusions in a houndstooth pattern (zigzag pattern) and stacking.

[0147] Furthermore, although the first and second embodiments above illustrate an example of forming a protrusion by stacking a plurality of protrusions at a pitch smaller than the width of the protrusion, the present invention is not limited thereto. The present invention can also form a protrusion by stacking a plurality of protrusions at a pitch greater than the width of the protrusion.

[0148] Furthermore, although the first and second embodiments above illustrate that the process of forming the boiling face portion includes an example of forming the boiling face portion without sandblasting after lamination, the present invention is not limited thereto. The process of forming the boiling face portion of the present invention may also include a process of forming the boiling face portion by sandblasting after lamination.

[0149] Furthermore, although the first and second embodiments described above illustrate an example of forming a boiling surface portion in which a plurality of protrusions having a shape gradually becoming thicker from the base end toward the terminal end are arranged by stacking molding, the present invention is not limited thereto. The present invention may also form a boiling surface portion in which a plurality of protrusions having a shape gradually becoming thicker from the base end toward the terminal end are arranged by machining or a combination of machining and stacking molding.

[0150] Furthermore, although the first and second embodiments above illustrate an example in which the protrusion having a shape gradually becoming thicker from the base end toward the terminal end is in the shape of a regular quadrangular pyramid, the present invention is not limited thereto. In the present invention, the protrusion having a shape gradually becoming thicker from the base end toward the terminal end may also be in the shape of a truncated pyramid (other truncated pyramids or circular truncated pyramids, etc.) other than a regular quadrangular pyramid.

[0151] Furthermore, although the first and second embodiments above illustrate an example in which the entire boiling face is formed by stacking molding, the present invention is not limited thereto. In the present invention, it is sufficient as long as at least a portion of the boiling face is formed by stacking molding. For example, a protrusion may be formed by stacking molding on a base plate formed by a method other than stacking molding, thereby forming a boiling face.

[0152] Explanation of symbols

[0153] 10, 210 - boiling part, 11a - mounting surface, 11b - surface opposite to the mounting surface, 13 - boiling surface part, 13a, 13d - linear protrusions, 13c - protrusions, 13e - pits, 20, 220 - condensation part, 100, 200 - cooler (boiling type cooler), HS - heating element.

Claims

1. A method for manufacturing a boiling cooler, the boiling cooler comprising a boiling section for boiling a refrigerant by heat exchange with a heating element and a condensing section for condensing the refrigerant that has been boiled by the boiling section and returning the refrigerant to the boiling section, the method comprising: forming the condensation portion; as well as The step of forming the boiling section, The step of forming the boiling portion includes the step of forming at least a portion of a boiling surface portion provided on a surface of the heat generating element opposite to a mounting surface and in contact with the refrigerant by lamination molding.

2. The method for manufacturing a boiling cooler according to claim 1, wherein: The step of forming at least a portion of the boiling surface portion by lamination molding includes the step of forming at least a portion of the boiling surface portion by lamination molding using metal powder.

3. The method for manufacturing a boiling cooler according to claim 2, wherein: The step of forming at least a portion of the boiling surface portion by lamination molding includes the step of forming at least a portion of the boiling surface portion by powder bed fusion as lamination molding.

4. The method for manufacturing a boiling cooler according to claim 1, wherein: The step of forming at least a portion of the boiling surface portion by lamination molding includes forming the protrusions by lamination molding in such a manner that a plurality of protrusions having a shape gradually becoming thicker from a base end toward a tip end are arranged.

5. The method for manufacturing a boiling cooler according to claim 4, wherein: The process of forming at least a portion of the boiling surface by stacking modeling includes: forming the protrusions by stacking modeling in a manner that a plurality of the protrusions are arranged in a matrix in a first direction and a second direction, wherein the first direction and the second direction are approximately orthogonal to each other in a plane approximately parallel to the boiling surface.

6. The method for manufacturing a boiling cooler according to claim 4, wherein: The process of forming at least a part of the boiling surface portion by stacking modeling includes: arranging a plurality of linear protrusions extending along a first direction within a plane substantially parallel to the boiling surface portion in a second direction substantially orthogonal to the first direction within a plane substantially parallel to the boiling surface portion, and arranging a plurality of the protrusions on the linear protrusions and between the linear protrusions in the second direction, thereby forming the linear protrusions and the protrusions by stacking modeling.

7. The method for manufacturing a boiling cooler according to claim 4, wherein: The step of forming at least a portion of the boiling surface portion by lamination molding includes the step of forming the protrusions by lamination molding in a manner that a plurality of the protrusions are arranged at a pitch smaller than a width of the protrusions.

8. The method for manufacturing a boiling cooler according to claim 1, wherein: The process of forming at least a part of the boiling surface by stacking molding includes: the process of forming the linear protrusions by stacking molding in a manner that a plurality of linear protrusions extending along a first direction within a plane approximately parallel to the boiling surface are arranged in a second direction approximately orthogonal to the first direction within a plane approximately parallel to the boiling surface; or the process of forming a stacked molding body including the pits by stacking molding in a manner that a plurality of pits having a shape that gradually becomes thicker from an opening toward a bottom are arranged.

9. The method for manufacturing a boiling cooler according to claim 1, wherein: The step of forming at least a portion of the boiling surface portion by lamination molding includes the step of forming the boiling surface portion without performing sandblasting after lamination molding.

10. A boiling cooler comprising: a boiling part that boils the refrigerant by exchanging heat with the heat generating element; and a condensing section that condenses the refrigerant that has been boiled by the boiling section and returns the refrigerant to the boiling section, The boiling section comprises: The installation surface of the heating element; and a boiling surface portion, which is provided on a surface opposite to the mounting surface and in contact with the refrigerant, and at least a portion of which is formed by stacking molding.

11. A boiling cooler comprising: a boiling part that boils the refrigerant by exchanging heat with the heat generating element; and a condensing section that condenses the refrigerant that has been boiled by the boiling section and returns the refrigerant to the boiling section, The boiling section comprises: The installation surface of the heating element; and a boiling surface portion provided on a surface opposite to the mounting surface and in contact with the refrigerant, The boiling surface portion is formed by arranging a plurality of protrusions having a shape that gradually becomes thicker from a base end toward a tip end.

12. The boiling cooler according to claim 11, wherein: The boiling surface portion is configured such that a plurality of the protrusions are arranged in a matrix in a first direction and a second direction, and the first direction and the second direction are substantially orthogonal to each other in a plane substantially parallel to the boiling surface portion.

13. The boiling cooler according to claim 11, wherein: The boiling surface portion is configured to arrange in a second direction a plurality of linear protrusions extending along a first direction within a plane substantially parallel to the boiling surface portion, and to arrange a plurality of the protrusions on the linear protrusions and between the linear protrusions in the second direction, wherein the second direction is substantially orthogonal to the first direction within a plane substantially parallel to the boiling surface portion.

14. The boiling cooler according to claim 11, wherein: The boiling surface portion is configured such that a plurality of the protrusions are arranged at a pitch smaller than a width of the protrusions.