Preparation method of multi-connecting-pipe continuous guiding assembly for reactor internals
Through laser selection melting additive manufacturing technology, the problems of low efficiency, long cycle and difficult accuracy in the manufacturing of continuous guide components in the reactor reactor are solved, and high-precision, short cycle and high-performance manufacturing is achieved, which meets the safety of nuclear reactors Require.
Patent Information
- Application Number
- CN202410860538.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-28
- Publication Date
- 2024-11-05
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The traditional manufacturing process of continuous guide components in the reactor reactor has low efficiency, long cycle, difficulty in control of precision and low material utilization, resulting in increased manufacturing difficulty and limited delivery efficiency.
Using laser selection melting additive manufacturing technology (SLM), metal powder is prepared through three-dimensional design and vacuum atomization method, and components are formed layer by layer using SLM equipment. Partition scanning strategy and appropriate grid support parameters are used to ensure high accuracy and high quality. Manufacturing of performance.
It realizes high-precision, high-performance, short-cycle manufacturing, reduces waste generation, simplifies manufacturing processes, shortens cycles, and improves economical and environmental protection, meeting the safe operation requirements of nuclear reactors.
Smart Images

Figure CN118893218A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of reactor internal component manufacturing, in particular to a method for preparing a multi-connected tube continuous guide assembly for reactor internal components. Background Art
[0002] In the core structure of a nuclear reactor, the control rod guide cylinder assembly plays a vital role, ensuring that the control rods can be accurately and quickly inserted into the core under various operating conditions, especially in emergency situations, to adjust or terminate the nuclear fission chain reaction and ensure the safe shutdown of the reactor. This assembly is divided into two parts, the upper and lower parts, of which the design of the lower guide cylinder assembly is particularly complex. It integrates key components such as continuous guide components, semi-square tube structures, precise guide plates, and middle flanges, which are combined into one through a precise welding process.
[0003] It is particularly noteworthy that the core of the lower guide cylinder assembly, the continuous guide assembly, is assembled from up to 26 independent parts through a high-precision welding process. This process not only requires extremely high manufacturing precision, but also faces complex assembly process challenges, especially in controlling welding deformation. Any slight deviation may cause the assembly to fail to meet stringent use requirements. Manual assembly is time-consuming and limited by the narrow welding space, which places extremely high demands on the professional skills of welders. In addition, the welding sequence must strictly follow a specific process, and the welder's operating habits must also be highly matched with it, which undoubtedly increases the difficulty of manufacturing.
[0004] Therefore, the continuous guide assembly is regarded as the component with the highest manufacturing precision and the most complicated process flow among the in-pile components, and its traditional manufacturing method has become a key bottleneck restricting the efficiency of product delivery. Summary of the invention
[0005] The technical problem to be solved by the present invention is to provide a method for preparing a multi-tube continuous guide assembly for reactor internals. By adopting laser selective melting additive manufacturing technology (SLM), the problems of low efficiency, long cycle, difficult precision control and low material utilization in the traditional manufacturing process of continuous guide assemblies for reactor internals are solved, and high-precision, high-performance and short-cycle manufacturing of continuous guide assemblies is achieved.
[0006] In order to solve the above technical problems, the technical solution adopted by the present invention is: a method for preparing a multi-tube continuous guide assembly for reactor internals, which mainly utilizes laser selective melting additive manufacturing technology (SLM) to produce the continuous guide assembly.
[0007] The preferred solution specifically includes the following steps: 1) Design and Modeling According to the final size requirements of the continuous guide component, a 3D model is created using 3D design software and converted into a file format suitable for SLM equipment. The model is then sliced and the process parameters are set according to the cross-section data of each layer. 2) Raw material preparation 304L stainless steel metal powder with a particle size of 15 μm to 53 μm was prepared by vacuum gas atomization and placed in a drying oven to remove moisture before printing; 3) Manufacturing process Using SLM equipment, continuous guide components are formed through the following cyclic steps: a) Use the powder spreading system to evenly spread the metal powder of the set thickness on the printing platform; b) The laser beam melts the powder according to preset parameters to form a layer of part cross section; c) Control the platform to descend to a certain height and apply powder again; d) Repeat the laser melting step, layer by layer, until the overall formation of the component is completed.
[0008] In a preferred solution, in step 1), specific process parameter settings include slice thickness, laser scanning path, and laser energy parameters.
[0009] In a preferred solution, in step 3), a partition scanning strategy is adopted to improve the forming accuracy and mechanical properties; At the same time, set appropriate mesh support parameters, including fill lines, fill teeth, cutting, boundaries and their tooth shape parameters to ensure the stability of the parts and reduce the workload of post-processing.
[0010] In a preferred embodiment, in step 3), during the forming process, argon gas is filled into the filling cavity as a protective atmosphere to prevent oxidation of the powder, and a gas circulation system is enabled to reduce splashing and the impact of impurities.
[0011] In a preferred solution, after the manufacturing is completed using the method, the chemical composition, mechanical properties, intergranular corrosion and microstructure analysis of the continuous guide assembly are performed to ensure that it meets the standard requirements of nuclear power equipment.
[0012] The present invention provides a method for preparing a multi-tube continuous guide assembly for reactor internals. By adopting the above method, the following beneficial effects are achieved: (1) SLM technology directly builds layer by layer based on the 3D model, avoiding the cumulative errors caused by traditional welding processes, ensuring that the continuous guide components have higher geometric accuracy and dimensional consistency, and meeting the strict requirements for the safe operation of nuclear reactors; (2) By precisely controlling material deposition, materials are added only where needed, effectively reducing waste generation. Compared with traditional processes, materials are saved by more than 60%, and the economic and environmental benefits are significantly enhanced; (3) The SLM process simplifies the manufacturing process, eliminating the need for multiple processing, welding, calibration and other complicated steps, greatly shortening the cycle from design to finished product, which is more than 70% faster than traditional methods and speeding up product delivery. (4) The continuous guide components formed by SLM have excellent mechanical properties and good corrosion resistance after carefully designed scanning strategies and support parameters. After testing, the mechanical properties and intergranular corrosion tests all meet high standards, ensuring the long-term safe and reliable operation of the in-core components. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] The present invention will be further described below in conjunction with the accompanying drawings and embodiments: Figure 1 It is a schematic diagram of the structure of the continuous guide assembly of the present invention.
[0014] Figure 2 It is a schematic diagram of the SLM equipment system of the present invention.
[0015] Figure 3 It is a schematic diagram of partition scanning during the SLM melting process of the present invention.
[0016] Figure 4-7 Microstructure analysis results of the present invention. DETAILED DESCRIPTION
[0017] Embodiment 1: like Figure 2 A method for preparing a multi-tube continuous guide assembly for reactor internals is disclosed, specifically, the continuous guide assembly is produced by using laser selective melting additive manufacturing technology (SLM).
[0018] The method for preparing the above-mentioned multi-tube continuous guide assembly for reactor internals comprises the following steps: 1) Design and Modeling According to the final size requirements of the continuous guide component, a 3D model is created using 3D design software and converted into a file format suitable for SLM equipment. The model is then sliced and the process parameters are set according to the cross-section data of each layer. 2) Raw material preparation 304L stainless steel metal powder with a particle size of 15 μm to 53 μm was prepared by vacuum gas atomization and placed in a drying oven to remove moisture before printing; 3) Manufacturing process Using SLM equipment, continuous guide components are formed through the following cyclic steps: a) Use the powder spreading system to evenly spread the metal powder of the set thickness on the printing platform; b) The laser beam melts the powder according to preset parameters to form a layer of part cross section; c) Control the platform to descend to a certain height and apply powder again; d) Repeat the laser melting step, layer by layer, until the overall formation of the component is completed.
[0019] In a preferred solution, in step 1), specific process parameter settings include slice thickness, laser scanning path, and laser energy parameters.
[0020] In a preferred embodiment, in step 3), during the forming process, argon gas is filled into the filling cavity as a protective atmosphere to prevent oxidation of the powder, and a gas circulation system is enabled to reduce splashing and the impact of impurities.
[0021] Embodiment 2: like Figure 3 As shown, based on Example 1, in step 3), a partition scanning strategy is adopted to improve the forming accuracy and mechanical properties; At the same time, set appropriate mesh support parameters, including fill lines, fill teeth, cutting, boundaries and their tooth shape parameters to ensure the stability of the parts and reduce the workload of post-processing.
[0022] In addition, the selection of the above grid support parameters is performed according to the following table:
[0023] Embodiment 3: On the basis of Example 1, after the manufacturing is completed by the method, the chemical composition, mechanical properties, intergranular corrosion and microstructure analysis of the continuous guide assembly are performed to ensure that it meets the standard requirements of nuclear power equipment.
[0024] The specific analysis results are as follows: 1) Chemical composition
[0025] 2) Mechanical properties
[0026] 3) Intergranular corrosion The intergranular corrosion test was carried out in accordance with the provisions of MC1310. The samples were sensitized using method B: heating to 700±10℃, keeping warm for 30 minutes, slowly cooling the sample to 500℃ in the furnace at a rate of 60±5℃ per hour, and then cooling in the air. The intergranular corrosion test results were all qualified.
[0027] 4) Microstructure After the samples were corroded by aqua regia, the microstructures were all typical austenite structures, as shown in the attached figure. Figure 4-7 shown.
[0028] This application adopts SLM to manufacture continuous guide components, which has high manufacturing accuracy, a wide range of suitable materials, good component performance, small machining amount, short manufacturing cycle and high degree of automation, and can meet the manufacturing requirements of precision metal components with complex shapes.
[0029] Compared with traditional processes for manufacturing continuous guide components, a single product saves more than 60% of materials and more than 70% of manufacturing cycle.
Claims
1. A method for preparing a multi-tube continuous guide assembly for reactor internals, characterized in that: The continuous guide component is produced using the additive manufacturing technology of selective laser melting (SLM).
2. The method for preparing a multi-tube continuous guide assembly for reactor internals according to claim 1, characterized in that The following steps are involved: 1) Design and Modeling According to the final size requirements of the continuous guide component, a 3D model is created using 3D design software and converted into a file format suitable for SLM equipment. The model is then sliced and the process parameters are set according to the cross-section data of each layer. 2) Raw material preparation 304L stainless steel metal powder with a particle size of 15 μm to 53 μm was prepared by vacuum gas atomization and placed in a drying oven to remove moisture before printing; 3) Manufacturing process Using SLM equipment, continuous guide components are formed through the following cyclic steps: a) Use the powder spreading system to evenly spread the metal powder of the set thickness on the printing platform; b) The laser beam melts the powder according to preset parameters to form a layer of part cross section; c) Control the platform to descend to a certain height and apply powder again; d) Repeat the laser melting step, layer by layer, until the overall formation of the component is completed.
3. The method for preparing a multi-connected tube continuous guide assembly for reactor internals according to claim 2, characterized in that: In the step 1), specific process parameter settings include slice thickness, laser scanning path, and laser energy parameters.
4. The method for preparing a multi-tube continuous guide assembly for reactor internals according to claim 2, characterized in that: In the step 3), a partition scanning strategy is adopted to improve the forming accuracy and mechanical properties; At the same time, set appropriate mesh support parameters, including fill lines, fill teeth, cutting, boundaries and their tooth shape parameters to ensure the stability of the parts and reduce the workload of post-processing.
5. The method for preparing a multi-connected tube continuous guide assembly for reactor internals according to claim 2, characterized in that: In the step 3), during the forming process, argon gas is filled into the filling cavity as a protective atmosphere to prevent oxidation of the powder, and a gas circulation system is enabled to reduce splashing and the impact of impurities.
6. The method for preparing a multi-tube continuous guide assembly for reactor internals according to claim 2, characterized in that: After the manufacturing is completed by the method, the chemical composition, mechanical properties, intergranular corrosion and microstructure analysis of the continuous guide component are carried out to ensure that it meets the standard requirements of nuclear power equipment.
Citation Information
Patent Citations
Hook provided with novel abrasion resistant layer structure and manufacturing method thereof
CN106903309A
Forming method of reactor internal integral type guide cylinder
CN108962412A
Nuclear fuel assembly and control rod
JP2015203636A
Universal inverted reactor and method for design and manufacture of universal inverted reactor
US20200027585A1
Improved corrosion resistance of additively-manufactured zirconium alloys
US20220184706A1