Method for efficiently using catalyst in production of oxidized trimellitic anhydride
By pre-adding part of the catalyst in the production of trimellitic anhydride and adding the remaining catalyst in the oxidation kettle at a constant speed, combined with the optimization of the stirring and heating structure, the problems of excessive catalyst consumption and low mixing efficiency are solved, and more efficient catalyst use and production are achieved Improve efficiency.
Patent Information
- Application Number
- CN202410939492.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-15
- Publication Date
- 2024-11-05
AI Technical Summary
The heating efficiency of the batching kettle in the production of existing trimellitic anhydride is not improved, resulting in the mixing efficiency being affected, the catalyst consumes excessively, and the catalyst forms a complex with the oxidation product, resulting in passivation of activity and self-inhibiting of reaction.
A part of the solution catalyst was added to the batching kettle in advance, and the oxidation gas was passed into the oxidation kettle, and the remaining solution catalyst was added continuously and at a constant speed after the initial reaction began. The catalyst mixing and heat were accelerated through a specific stirring mechanism and heating structure. Exchange, optimize the amount of catalyst used and reaction efficiency.
The catalyst usage amount is significantly reduced by 10%-15%, the production efficiency is improved by about 10%, and the mixing time of the catalyst is shortened through improved heating and mixing methods, reducing waste generation.
Smart Images

Figure CN118894824A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of plasticizer trimellitic anhydride, and in particular to a method for efficiently using a catalyst in the production of oxidized trimellitic anhydride. Background Art
[0002] The molecular structure of trimellitic anhydride contains carboxylic acid and anhydride structures, and has the chemical properties of benzoic acid and phthalic anhydride. It can react with alcohol to form esters or polyesters, react with alkali to form salts, react with ammonia (amine) to form amide-imide, and undergo condensation reactions with hydrocarbons under the action of catalysts, etc., making it widely used in the production of PVC resin plasticizers, polyimide resin paints, water-soluble alkyd resins, epoxy resin curing agents, impregnating agents for low-voltage and pulse power containers, movie films, water treatment agents, and surfactants.
[0003] At present, the main method for industrial production of trimellitic anhydride at home and abroad is the gas-phase air oxidation of trimellitic anhydride, which has the advantages of easy access to raw materials and low consumption of raw materials and utilities. The addition and proportioning of the catalyst are mainly two ways: adding all the catalyst before the reaction or adding the catalyst in batches by staged oxidation. Due to the self-inhibition effect of the catalyst activity passivation caused by the formation of complexes between the catalyst and the oxidation product in the middle and late stages of the oxidation reaction, it is necessary to add an excess of catalyst to ensure the full completion of the reaction; this results in the catalyst consumption being much higher than the theoretical consumption.
[0004] At the same time, since the preparation process of the catalyst requires the use of a batching kettle and an oxidation kettle for operation, the batching kettle is mainly used to mix the oxidant raw materials, and the existing batching kettle cannot improve its heating efficiency during the mixing process, which affects the mixing efficiency. Summary of the invention
[0005] The invention discloses a method for efficiently using a catalyst in the production of oxidized trimellitic anhydride, aiming to solve the technical problem that the heating efficiency of the existing batching kettle cannot be improved during the mixing process, thereby affecting the mixing efficiency.
[0006] In order to achieve the above object, the present invention adopts the following technical solutions:
[0007] A method for efficiently using a catalyst in the production of oxidized trimellitic anhydride comprises a water-carrying agent and a raw material, wherein the water-carrying agent is a low-unit aliphatic carboxylic acid, and the raw material is trimethylol. Part of the catalyst in solution is added to a batching kettle in advance, and then the catalyst is transferred to an oxidation kettle and an oxidizing gas is introduced for reaction. After the initial reaction begins, the remaining catalyst in solution is continuously added at a uniform rate. The batching kettle comprises a kettle body, and the kettle body is formed by connecting two cylinders. The outside of the kettle body is wrapped with a heating outer layer, and the two cylinders of the kettle body are respectively fixedly connected with inner branch pipes, and a heating rod is installed inside the inner branch pipe, and the heating rod is connected to the outer wall of the heating outer layer through a first bracket. An injection mechanism is tightly connected to the inner wall of one side of the kettle body, and a stirring mechanism is arranged inside the kettle body, and a discharge port is arranged at the bottom of the kettle body. The mixing mechanism includes two rotating clamping frames, the top ends of the two cylinders of the kettle body are respectively provided with annular slide grooves, and the two rotating clamping frames are respectively movably clamped in the annular slide grooves, and the bottom end of each rotating clamping frame is respectively fixedly connected with a plurality of first support rods, the plurality of first support rods pass through the annular slide groove, and a plurality of stirring blades are equidistantly arranged on the outer wall thereof; a gear ring is respectively fixedly arranged on the outer wall of each of the rotating clamping frames, and the two gear rings are simultaneously meshed with a first gear, one side of the first gear is connected with a first stepper motor, and the first stepper motor is fixed to the top end of the kettle body through a second bracket; the other side of the first gear is simultaneously meshed with a second gear, and the bottom end of the second gear is fixedly connected with a second support rod, the second support rod passes through the kettle body and is located at the connection of the two cylinders, and a plurality of guide blades are equidistantly arranged on the outer wall thereof.
[0008] By providing a stirring mechanism, the mixing effect of the catalyst can be accelerated under the action of multiple stirring blades, and a flow path of the liquid between the two cylinders can be established under the action of multiple guiding blades. At the same time, based on the same-direction rotation of multiple structures, the shear force between the three can be reduced to ensure that the liquid between the two cylinders can be better exchanged under the action of the guiding blades to complete the mixing of the catalyst. At the same time, when the catalyst enters the kettle body for mixing, rapid heat exchange is completed by expanding the heat contact area of the catalyst. Therefore, the heating efficiency can be further shortened while ensuring the mixing effect of the catalyst, and the mixing efficiency of the catalyst can be optimized.
[0009] In a preferred embodiment, the injection mechanism includes a conveying pipe, and the tail end of the conveying pipe is connected to the injection pipe, the injection pipe passes through the heating outer layer and is connected to the inner wall of the kettle body, the front end of the conveying pipe is provided with a second stepper motor, and the output end of the second stepper motor is connected to a third support rod, the outer wall of the third support rod is fixed with a spiral conveying fan blade, a plurality of elastic support plates are equidistantly fixedly connected to the outer wall of one side of the third support rod, and each elastic support plate is respectively provided with a plurality of U-shaped metal sheets, a multi-way pipe is connected to the inner wall of one side of the conveying pipe, and a plurality of through holes of the multi-way pipe are respectively connected to different material containers.
[0010] By providing a material injection mechanism, the spiral conveying blades can ensure that the material moves forward at a uniform speed in the conveying pipeline. When the liquid catalyst accumulates at different positions of the spiral conveying blades, a round of mixing can be performed. At the same time, under the rotation of multiple U-shaped metal sheets, the mixing effect of the liquid catalyst can be accelerated. When the catalyst after a round of mixing enters the kettle body for secondary mixing, the mixing efficiency can be more effectively improved.
[0011] In a preferred embodiment, the following specific steps are included:
[0012] S1: Raw material preparation: unsymmetrical trimethylbenzene and water-carrying agent are measured in proportion, and a reaction catalyst is added and mixed, wherein the catalyst is 30-60% of the total amount of the catalyst in an ionic cobalt solution, 30-60% of the total amount of the ionic manganese solution, and 30-80% of a solution of tetrabromoethane; the mixing temperature is controlled at 80-150°C;
[0013] S2: Initial oxidation: introduce oxidizing gas and control the pressure at 0.6-1.5 MPa. This is the initial oxidation stage. The reaction time is 0.5-1 h and the reaction temperature is 120-180 °C.
[0014] S3: Continuous oxidation: continuously introducing oxidizing gas and continuously adding the remaining liquid catalyst at a uniform rate, wherein the catalyst is 30-70% of the total amount of the catalyst in an ionic cobalt solution, 30-70% of the total amount of the manganese ion solution, and 30-80% of the liquid tetrabromoethane; controlling the pressure at 1.2-2.8Mpa, the reaction time at 0.5-2h, the reaction temperature at 150-280°C, and the oxidation reaction ends when the oxygen content of the tail gas reaches 3%-8%;
[0015] S4: Forming: After the oxidation, the material is subjected to anhydride formation, light removal, refining, and flake formation to obtain trimellitic anhydride product;
[0016] The catalyst in S1 is divided into two stages: adding the mixture in advance and adding the reaction solution at a uniform speed;
[0017] The catalyst described in S1 is a composite catalyst of a liquid cobalt ion catalyst, a liquid manganese ion catalyst, and a solution of tetrabromoethane;
[0018] The oxidant is one or more of air and oxygen, and the intake air volume is adjusted according to the process requirements and the oxygen content of the tail gas.
[0019] By targeting the self-inhibition effect of the catalyst being deactivated due to the formation of complexes between the catalyst and the oxidation product in the middle and late stages of the oxidation reaction, it is necessary to add an excess amount of catalyst to ensure the full completion of the reaction; by adjusting the ratio of new catalyst additions during the oxidation reaction, the amount of catalyst used can be significantly reduced by 10%-15%, effectively reducing the generation of waste; and after the initial oxidation of the trimethylolbenzene raw material, the remaining solution catalyst is continuously added at a uniform rate according to the progress of the reaction to produce trimethylolbenzene; compared with the two current domestic production processes of adding all the catalysts before the reaction or adding the catalysts in batches by staged oxidation, the self-inhibition effect of the catalyst being deactivated due to the formation of complexes between the catalyst and the oxidation product is reduced, thereby improving the production efficiency by about 10%.
[0020] From the above, it can be seen that a method for efficiently using a catalyst in the production of oxidized trimellitic anhydride includes a water-carrying agent and a raw material, wherein the water-carrying agent is a low-unit aliphatic carboxylic acid, and the raw material is trimethylol. A part of the solution catalyst is added to a batching kettle in advance, and an oxidizing gas is introduced into the oxidation kettle for reaction. After the initial reaction starts, the remaining solution catalyst is continuously added at a uniform rate; the batching kettle includes a kettle body, and the kettle body is formed by connecting two cylinders, the outside of the kettle body is wrapped with a heating outer layer, and the two cylinders of the kettle body are respectively fixedly connected with inner branches, and a heating rod is installed inside the inner branch, and the heating rod is connected to the outer wall of the heating outer layer through a first bracket, and an injection mechanism is tightly connected to the inner wall of one side of the kettle body, and a stirring mechanism is arranged inside the kettle body, and a discharge port is arranged at the bottom end of the kettle body; The stirring mechanism includes two rotating clamping frames, the top ends of the two cylinders of the kettle body are respectively provided with annular chutes, and the two rotating clamping frames are respectively movably clamped in the annular chutes, and the bottom end of each rotating clamping frame is respectively fixedly connected with a plurality of first support rods, the plurality of first support rods pass through the annular chutes, and a plurality of stirring blades are equidistantly arranged on the outer wall thereof; the outer wall of each rotating clamping frame is respectively fixed with a gear ring, and the two gear rings are simultaneously meshed with a first gear, one side of the first gear is connected with a first stepper motor, and the first stepper motor is fixed to the top end of the kettle body through a second bracket; the other side of the first gear is simultaneously meshed with a second gear, and the bottom end of the second gear is fixedly connected with a second support rod, the second support rod passes through the kettle body and is located at the connection of the two cylinders, and a plurality of guide blades are equidistantly arranged on the outer wall thereof. The method for efficiently using a catalyst in the production of oxidized trimellitic anhydride provided by the present invention has the technical effect that the heating efficiency can be further shortened while ensuring the mixing effect of the catalyst, and the mixing efficiency of the catalyst can be optimized. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 The present invention provides a schematic structural diagram of a batching kettle for a method for efficiently using a catalyst in the production of oxidized trimellitic anhydride.
[0022] Figure 2The present invention provides a schematic diagram of the internal structure of a batching kettle for a method for efficiently using a catalyst in the production of oxidized trimellitic anhydride.
[0023] Figure 3 The figure is a cross-sectional view of the interior of a batching kettle for a method for efficiently using a catalyst in the production of oxidized trimellitic anhydride proposed by the present invention.
[0024] Figure 4 The present invention provides a schematic structural diagram of the injection mechanism of a batching kettle for a method for efficiently using a catalyst in the production of oxidized trimellitic anhydride.
[0025] Figure 5 The present invention provides a flow chart of a method for efficiently using a catalyst in the production of oxidized trimellitic anhydride.
[0026] In the figure: 1, discharge port; 2, heating outer layer; 3, kettle body; 4, stirring mechanism; 5, heating rod; 6, first bracket; 7, injection mechanism; 8, inner branch pipe; 401, annular slide; 402, stirring blade; 403, first support rod; 404, rotating clamping frame; 405, gear ring; 406, first stepper motor; 407, first gear; 408, second bracket; 409, second gear; 410, second support rod; 411, guide blade; 701, injection pipe; 702, conveying pipeline; 703, multi-way pipe; 704, second stepper motor; 705, spiral conveying blade; 706, U-shaped metal sheet; 707, elastic support plate; 708, third support rod. DETAILED DESCRIPTION
[0027] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments.
[0028] The invention discloses a method for efficiently using a catalyst in the production of oxidized trimellitic anhydride, which is mainly applied to the production of oxidized trimellitic anhydride.
[0029] Reference Figure 1-Figure 3A method for efficiently using a catalyst in the production of oxidized trimellitic anhydride, comprising a water-carrying agent and a raw material, wherein the water-carrying agent is a low-unit aliphatic carboxylic acid, and the raw material is trimethylol. Part of the catalyst in solution is added to a batching kettle in advance, and then the catalyst is transferred to an oxidation kettle and an oxidizing gas is introduced for reaction. After the initial reaction begins, the remaining catalyst in solution is continuously added at a uniform rate. The batching kettle comprises a kettle body 3, and the kettle body 3 is formed by connecting two cylinders. The outside of the kettle body 3 is wrapped with a heating outer layer 2, and the two cylinders of the kettle body 3 are respectively fixedly connected with inner branch pipes 8, and a heating rod 5 is installed inside the inner branch pipe 8, and the heating rod 5 is connected to the outer wall of the heating outer layer 2 through a first bracket 6. The kettle body The inner wall of one side of the kettle body 3 is tightly connected with the injection mechanism 7, and the stirring mechanism 4 is arranged inside the kettle body 3, and the bottom end of the kettle body 3 is provided with a discharge port 1; the stirring mechanism 4 includes two rotating clamping frames 404, the top ends of the two cylinders of the kettle body 3 are respectively provided with annular slide grooves 401, and the two rotating clamping frames 404 are respectively movably clamped in the annular slide grooves 401, and the bottom end of each rotating clamping frame 404 is respectively fixedly connected with a plurality of first support rods 403, and the plurality of first support rods 403 pass through the annular slide grooves 401, and the outer wall thereof is equidistantly provided with a plurality of stirring blades 402; the outer wall of each rotating clamping frame 404 is respectively fixed with a toothed ring 405, and the two toothed rings 405 mesh simultaneously. A first gear 407 is coupled to the stirring mechanism 4, one side of the first gear 407 is connected to a first stepper motor 406, and the first stepper motor 406 is fixed to the top of the kettle body 3 through a second bracket 408; the other side of the first gear 407 is meshed with a second gear 409, and the bottom end of the second gear 409 is fixedly connected to a second support rod 410, the second support rod 410 passes through the kettle body 3 and is located at the connection between the two cylinders, and a plurality of guide blades 411 are equidistantly arranged on its outer wall. In the stirring mechanism 4, the first stepper motor 406 drives the first gear 407 to rotate, thereby driving the two gear rings 405 and the second gear 409 to rotate in the same direction at the same time, thereby, in the plurality of stirring blades 4 02 can accelerate the mixing effect of the catalyst, and a flow path of the liquid between the two cylinders can be established under the action of multiple guide blades 411. At the same time, based on the same-direction rotation of multiple structures, the shear force between the three can be reduced to ensure that the liquid between the two cylinders can be better exchanged under the action of the guide blades 411 to complete the mixing of the catalyst. At the same time, when the catalyst enters the kettle body 3 for mixing, the heat contact area of the catalyst can be expanded through the setting of the inner branch pipe 8, and the setting of the heating outer layer 2 and the heating rod 5 to complete rapid heat exchange. Therefore, the heating efficiency can be further shortened while ensuring the mixing effect of the catalyst, and the mixing efficiency of the catalyst can be optimized.
[0030] Reference Figure 4 In a preferred embodiment, the injection mechanism 7 includes a delivery pipe 702 , and the tail end of the delivery pipe 702 is connected to a injection pipe 701 , and the injection pipe 701 passes through the heating outer layer 2 and is connected to the inner wall of the kettle body 3 .
[0031] Reference Figure 4 In a preferred embodiment, a second stepper motor 704 is disposed at the front end of the conveying pipe 702 , and an output end of the second stepper motor 704 is connected to a third support rod 708 , and a spiral conveying blade 705 is fixed to an outer wall of the third support rod 708 .
[0032] Reference Figure 4 In a preferred embodiment, a plurality of elastic support plates 707 are equidistantly fixedly connected to the outer wall of one side of the third support rod 708, and a plurality of U-shaped metal sheets 706 are respectively arranged on each elastic support plate 707, a multi-way tube 703 is connected to the inner wall of one side of the conveying pipe 702, and a plurality of through holes of the multi-way tube 703 are respectively connected to different material containers, when different components of the liquid catalyst are conveyed into the conveying pipe 702 through the multi-way tube 703, the spiral conveying blades 705 can ensure that the material moves forward at a uniform speed in the conveying pipe 702 until it enters the interior of the kettle body 3, and under the rotation of the spiral conveying blades 705, when the liquid catalyst accumulates at different positions of the spiral conveying blades 705, a round of mixing can be performed, and at the same time, under the rotation of the plurality of U-shaped metal sheets 706, the mixing effect of the liquid catalyst can be accelerated, and when the catalyst after a round of mixing enters the kettle body 3 for secondary mixing, the mixing efficiency can be more effectively improved.
[0033] Reference Figure 5 In a preferred embodiment, the method comprises the following specific steps:
[0034] S1: Raw material preparation: unsymmetrical trimethylbenzene and water-carrying agent are measured in proportion, and reaction catalyst is added and mixed, wherein the catalyst is 30-60% of ionic cobalt solution of the total amount of catalyst, 30-60% of ionic manganese solution of the total amount, and 30-80% of liquid tetrabromoethane; the mixing temperature is controlled at 80-150°C;
[0035] S2: Initial oxidation: introduce oxidizing gas and control the pressure at 0.6-1.5 MPa. This is the initial oxidation stage. The reaction time is 0.5-1 h and the reaction temperature is 120-180 °C.
[0036] S3: Continuous oxidation: Continuously introduce oxidizing gas and continuously add the remaining liquid catalyst at a uniform rate. The catalyst is 30-70% of the total amount of catalyst, 30-70% of the total amount of ionic cobalt solution, 30-70% of the total amount of ionic manganese solution, and 30-80% of liquid tetrabromoethane; control the pressure at 1.2-2.8Mpa, the reaction time is 0.5-2h, the reaction temperature is 150-280°C, and the oxidation reaction ends when the oxygen content of the tail gas reaches 3%-8%;
[0037] S4: Forming: After the oxidation, the material is subjected to anhydride formation, light removal, refining, and flake formation to obtain trimellitic anhydride product.
[0038] Reference Figure 5 In a preferred embodiment, the catalyst in S1 is divided into two stages: adding the mixture in advance and adding the reaction solution at a uniform speed.
[0039] Reference Figure 5 In a preferred embodiment, the catalyst in S1 is a composite catalyst of a liquid cobalt ion catalyst, a liquid manganese ion catalyst, and a solution of tetrabromoethane.
[0040] Reference Figure 5 In a preferred embodiment, the oxidant is one or more of air and oxygen, and the intake air volume is adjusted according to the process requirements and the oxygen content of the tail gas.
[0041] Example 1
[0042] (1) Add 400 kg of trimethylol and 800 kg of acetic acid to the batching kettle, and then add 1.0 kg of ionic cobalt solution, 0.8 kg of ionic cobalt solution and 0.6 kg of liquid tetrabromoethane. Control the mixing temperature to 120 ° C, start stirring and mixing, and completely dissolve the catalyst. At the same time, use 20 kg of acetic acid, 1.0 kg of ionic cobalt solution, 1.2 kg of ionic cobalt solution and 0.8 kg of liquid tetrabromoethane to prepare a mixed solution and add it to the catalyst tank;
[0043] (2) The prepared reaction liquid is pressed into the reactor through the process pipeline, the temperature is continuously raised to 140° C., an inert gas is introduced to keep the system pressure at 0.8 MPa, and air is introduced for the initial oxidation reaction. The reaction temperature is controlled at 150-180° C., the pressure is controlled at 0.8-1.6 MPa, and the reaction time is 25-30 min. As the reaction temperature gradually stabilizes and approaches 170° C.-180° C., the catalyst is continuously added from the catalyst tank at a uniform speed and pressurized to raise the reaction pressure to 1.2-2.8 MPa, and the reaction temperature is controlled at 180-260° C., as the second stage of the oxidation reaction, and the reaction time is 35-50 min. The oxidation reaction ends when the oxygen content of the tail gas reaches 3%-8%.
[0044] (3) The oxide material is dehydrated to form a crude anhydride, and the crude anhydride is distilled under different pressure conditions to remove by-products to obtain finished anhydride and polyacid anhydride, which are further refined and purified, and finally cooled and flaked to obtain trimellitic anhydride product. The dilute acetic acid produced in the anhydride production process is sent to a distillation tower and reused after concentration.
[0045] Example 2
[0046] (1) Add 350 kg of trimethylol and 750 kg of acetic acid to the batching kettle, and then add 0.8 kg of ionic cobalt solution, 0.6 kg of ionic cobalt solution and 0.5 kg of liquid tetrabromoethane. Control the mixing temperature to 125 ° C, start stirring and mixing, and completely dissolve the catalyst. At the same time, use 30 kg of acetic acid, 1.0 kg of ionic cobalt solution, 1.2 kg of ionic cobalt solution and 0.8 kg of liquid tetrabromoethane to prepare a mixed solution and add it to the catalyst tank;
[0047] (2) The prepared reaction liquid is pressed into the reactor through the process pipeline, the temperature is continuously raised to 150° C., an inert gas is introduced to keep the system pressure at 0.8 MPa, and air is introduced for the initial oxidation reaction. The reaction temperature is controlled at 150-190° C., the pressure is controlled at 0.8-1.6 MPa, and the reaction time is 25-35 min. As the reaction temperature gradually stabilizes and approaches 170° C.-190° C., the catalyst is continuously added from the catalyst tank at a uniform speed and pressurized to raise the reaction pressure to 1.2-2.8 MPa, and the reaction temperature is controlled at 190-270° C., as the second stage of the oxidation reaction, the reaction time is 35-50 min. The oxidation reaction ends when the oxygen content of the tail gas reaches 3%-8%.
[0048] (3) The oxide material is dehydrated to form a crude anhydride, and the crude anhydride is distilled under different pressure conditions to remove by-products to obtain finished anhydride and polyacid anhydride, which are further refined and purified, and finally cooled to form flakes to obtain the trimellitic anhydride product. The dilute acetic acid produced in the anhydride forming process is sent to a distillation tower and recycled after concentration. After the initial oxidation of the trimellitic toluene raw material, the present invention continuously and uniformly adds the remaining solution catalyst according to the progress of the reaction to produce trimellitic acid. Compared with the two current domestic production processes of adding all the catalyst before the reaction or adding the catalyst in batches by staged oxidation, the self-inhibition effect of the catalyst activity being passivated due to the formation of a complex between the catalyst and the oxidation product is reduced, so that the production efficiency is improved by about 10%.
[0049] Working principle: In the stirring mechanism 4, the first gear 407 is driven to rotate by the first stepper motor 406, so as to simultaneously drive the two gear rings 405 and the second gear 409 to rotate in the same direction. Thus, the mixing effect of the catalyst can be accelerated under the action of the multiple stirring blades 402, and the flow path of the liquid between the two cylinders can be established under the action of the multiple guide blades 411. At the same time, based on the same-direction rotation of the multiple structures, the shear force between the three can be reduced to ensure that the liquid between the two cylinders can be better exchanged under the action of the guide blades 411 to complete the mixing of the catalyst. At the same time, when the catalyst enters the kettle body 3 for mixing, the heat contact surface of the catalyst can be expanded by setting the inner branch pipe 8, and the setting of the heating outer layer 2 and the heating rod 5. The accumulation can complete the rapid heat exchange, thereby, the heating efficiency can be further shortened while ensuring the catalyst mixing effect, and the catalyst mixing efficiency can be optimized. When different components of the liquid catalyst are transported to the conveying pipe 702 through the multi-way pipe 703, the spiral conveying blades 705 can ensure that the material moves forward at a uniform speed in the conveying pipe 702 until it enters the kettle body 3. Under the rotation of the spiral conveying blades 705, when the liquid catalyst accumulates at different positions of the spiral conveying blades 705, a round of mixing can be performed. At the same time, under the rotation of multiple U-shaped metal sheets 706, the mixing effect of the liquid catalyst can be accelerated. After a round of mixing, the catalyst can enter the kettle body 3 for secondary mixing, which can more effectively improve the mixing efficiency.
[0050] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A method for efficiently using a catalyst in the production of oxidized trimellitic anhydride, comprising a water-carrying agent and a raw material, characterized in that: The water-carrying agent is a low-unit aliphatic carboxylic acid, and the raw material is trimethylol. A portion of the catalyst in solution is added to the batching kettle in advance, and then the oxidation kettle is transferred to the oxidation kettle and the oxidizing gas is introduced to react. After the initial reaction starts, the remaining catalyst in solution is continuously added at a uniform rate. The batching kettle comprises a kettle body (3), and the kettle body (3) is formed by connecting two cylinders. The outside of the kettle body (3) is wrapped with a heating outer layer (2), and the two cylinders of the kettle body (3) are respectively fixedly connected with inner branch pipes (8), and the inner branch pipes (8) are installed with heating rods (5), and the heating rods (5) are connected to the outer wall of the heating outer layer (2) through a first bracket (6). The inner wall of one side of the kettle body (3) is tightly connected with a material injection mechanism (7), and the inside of the kettle body (3) is provided with a stirring mechanism (4), and the bottom end of the kettle body (3) is provided with a discharge port (1); The stirring mechanism (4) comprises two rotating clamping frames (404), the top ends of the two cylinders of the kettle body (3) are respectively provided with annular slide grooves (401), and the two rotating clamping frames (404) are respectively movably clamped in the annular slide grooves (401), and the bottom end of each rotating clamping frame (404) is respectively fixedly connected with a plurality of first support rods (403), and the plurality of first support rods (403) pass through the annular slide grooves (401), and the outer wall thereof is equidistantly provided with a plurality of stirring blades (402); A gear ring (405) is fixed to the outer wall of each rotating clamping frame (404), and the two gear rings (405) are simultaneously meshed with a first gear (407), one side of the first gear (407) is connected to a first stepper motor (406), and the first stepper motor (406) is fixed to the top of the kettle body (3) through a second bracket (408); The other side of the first gear (407) is meshed with a second gear (409), and the bottom end of the second gear (409) is fixedly connected to a second support rod (410), the second support rod (410) passes through the kettle body (3) and is located at the connection between the two cylinders, and a plurality of guide blades (411) are equidistantly arranged on its outer wall.
2. A method for efficiently using a catalyst in the production of oxidized trimellitic anhydride according to claim 1, characterized in that: The injection mechanism (7) comprises a conveying pipeline (702), and the tail end of the conveying pipeline (702) is connected to an injection pipe (701), and the injection pipe (701) passes through the heating outer layer (2) and is connected to the inner wall of the kettle body (3).
3. A method for efficiently using a catalyst in the production of oxidized trimellitic anhydride according to claim 2, characterized in that: A second stepping motor (704) is disposed at the front end of the conveying pipe (702), and the output end of the second stepping motor (704) is connected to a third support rod (708), and a spiral conveying blade (705) is fixed to the outer wall of the third support rod (708).
4. A method for efficiently using a catalyst in the production of oxidized trimellitic anhydride according to claim 3, characterized in that: A plurality of elastic support plates (707) are equidistantly fixedly connected to an outer wall of one side of the third support rod (708), and a plurality of U-shaped metal sheets (706) are respectively arranged on each elastic support plate (707). A multi-way pipe (703) is connected to an inner wall of one side of the conveying pipeline (702), and a plurality of through holes of the multi-way pipe (703) are respectively connected to different material containers.
5. A method for efficiently using a catalyst in the production of oxidized trimellitic anhydride according to claim 1, characterized in that: The specific steps include: S1: Raw material preparation: unsymmetrical trimethylbenzene and water-carrying agent are measured in proportion, and a reaction catalyst is added and mixed, wherein the catalyst is 30-60% of the total amount of the catalyst in an ionic cobalt solution, 30-60% of the total amount of the ionic manganese solution, and 30-80% of a solution of tetrabromoethane; the mixing temperature is controlled at 80-150°C; S2: Initial oxidation: introduce oxidizing gas and control the pressure at 0.6-1.5 MPa. This is the initial oxidation stage. The reaction time is 0.5-1 h and the reaction temperature is 120-180 °C. S3: Continuous oxidation: continuously introducing oxidizing gas and continuously adding the remaining liquid catalyst at a uniform rate, wherein the catalyst is 30-70% of the total amount of the catalyst in an ionic cobalt solution, 30-70% of the total amount of the manganese ion solution, and 30-80% of the liquid tetrabromoethane; controlling the pressure at 1.2-2.8Mpa, the reaction time at 0.5-2h, the reaction temperature at 150-280°C, and the oxidation reaction ends when the oxygen content of the tail gas reaches 3%-8%; S4: Forming: After the oxidation, the material is subjected to anhydride formation, light removal, refining, and flake formation to obtain trimellitic anhydride product.
6. A method for efficiently using a catalyst in the production of oxidized trimellitic anhydride according to claim 5, characterized in that: The catalyst in S1 is divided into two stages: adding the mixture in advance and adding the reaction solution at a uniform speed.
7. A method for efficiently using a catalyst in the production of oxidized trimellitic anhydride according to claim 5, characterized in that: The catalyst described in S1 is a composite catalyst of liquid cobalt ion catalyst, liquid manganese ion catalyst and liquid tetrabromoethane.
8. A method for efficiently using a catalyst in the production of oxidized trimellitic anhydride according to claim 5, characterized in that: The oxidant is one or more of air and oxygen, and the intake air volume is adjusted according to the process requirements and the oxygen content of the tail gas.