Method for detecting porosity of coating by adopting industrial CT (Computed Tomography)
Through industrial CT detection and hydraulic cylinder drive movement, combined with X-ray or gamma ray scanning, the problem of accuracy and human factors of coating porosity detection is solved, and the precise statistics of coating porosity and internal structure are achieved. Clear display.
Patent Information
- Application Number
- CN202410928957.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-11
- Publication Date
- 2024-11-05
AI Technical Summary
The existing coating porosity detection methods are influenced by human factors, which cannot achieve accurate statistics of the entire coating, and cannot clearly and intuitively display the internal structure and defect conditions.
Using industrial CT detection method, the correct shape processing of the Al2O3 coating and the movement of the hydraulic cylinder driven on the detection machine, combined with X-ray or gamma ray scanning, the precise statistics of the pore volume of the coating is realized, and the internal structure is displayed through image reconstruction. .
Accurate statistics on the porosity of the coating are achieved, the results are unique, and the internal structure and defect conditions of the coating can be clearly and intuitively displayed.
Smart Images

Figure CN118896890A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field related to coating porosity detection, and in particular to a method for detecting coating porosity by using industrial CT. Background Art
[0002] Thermal spraying refers to heating the coating material to a molten or semi-molten state and spraying its particles onto the surface of the part with a high-speed airflow to form a protective layer. It is a common surface strengthening technology that can form coatings with different properties such as high temperature resistance, corrosion resistance, oxidation resistance, wear resistance, heat insulation, and insulation according to needs. It can repair some damaged parts and strengthen and protect new products before installation. It has high economic value and practicality and is widely used in aerospace, metallurgical rolling, transportation and other industries.
[0003] Compared with traditional welding methods, thermal spraying has the characteristics of small heat input, small heat input to the workpiece, and not easy to deform. Because thermal spraying has little impact on the parent material, it is widely used in the repair and surface strengthening of some key aerospace components. Therefore, the final performance of the spray coating will affect the service life of the entire part and even the stability of the entire system.
[0004] The detection of coating performance mainly focuses on the following aspects: coating metallography, hardness, bonding strength, and coating porosity. There are various methods for detecting porosity, such as the standard metallographic pattern comparison method used in HB 20195. In addition, there is a method of using Image J software for black and white contrast adjustment detection. The metallographic contrast method does not have pore patterns of all coatings and has poor operability. The software statistics process is subject to the complex procedures in the sample preparation process and can only count a single cross-section coating, and cannot fully count the performance of the entire coating. In addition, there are human factors in the process of adjusting the image contrast. In short, there is no completely objective and unified method for detecting the coating porosity, and both of the above methods are affected by human factors. Therefore, we need a method for detecting the coating porosity using industrial CT.
[0005] However, the currently used method of detecting coating porosity using industrial CT cannot guarantee the accurate statistics of the porosity of the entire coating, the results are not unique, and it is unable to utilize the attenuation law and absorption characteristics of X-rays or gamma rays in the object being detected, and it is unable to clearly and intuitively display the internal structure, composition and internal defect status of the object being detected in the form of two-dimensional or three-dimensional images. Summary of the invention
[0006] The object of the present invention is to provide a method for detecting the porosity of a coating using industrial CT to solve the problems raised in the above background technology.
[0007] To achieve the above object, the present invention provides the following technical solutions:
[0008] A method for detecting the porosity of a coating by using industrial CT comprises a detection machine, operation frames are arranged on the left and right sides of the upper end of the detection machine, a movable frame is installed at one end of the operation frame, a workbench is installed at the upper end of the detection machine, a fixing groove is arranged at the upper end of the workbench, a load-bearing frame is installed at the upper end of the fixing groove, a detection device is arranged at the upper end of the load-bearing frame, a scanning head is installed at the lower end of the detection device, a slide rail is arranged at the upper end of the workbench, a first hydraulic cylinder is arranged at the left end of the workbench, a placing table is arranged at one end of the first hydraulic cylinder, a through hole is arranged on the surface of the placing table, a slot is arranged at one end of the through hole, a bottom plate is installed at the upper end of the slot, a second hydraulic cylinder is arranged at the right end of the workbench, a lifting plate is arranged at the upper end of the second hydraulic cylinder, and a shielding plate is arranged at the upper end of the lifting plate.
[0009] Preferably, the operating frame is movably connected to the movable frame, and the outer wall size of the movable frame is the same as the inner wall size of the operating frame.
[0010] Preferably, the load-bearing frame is snap-connected to the workbench via a fixing groove, and the load-bearing frame is embeddedly connected to the detection device.
[0011] Preferably, the placement table forms a sliding structure with the workbench through a slide rail, and the placement table forms a telescopic structure with the workbench through a first hydraulic cylinder.
[0012] Preferably, the bottom plate is connected to the placement table by a card slot, and the placement table is of open-hole design.
[0013] Preferably, the lifting plate forms a lifting structure with the detection mechanism through a second hydraulic cylinder, and the lifting plate and the shielding plate are in the same horizontal plane.
[0014] A method for detecting the porosity of a coating using industrial CT comprises the following steps:
[0015] S1. Open the movable frame in the device from the operation frame, spray the Al2O3 coating to be tested on the bottom plate, and wait for the Al2O3 coating to solidify after the Al2O3 coating is sprayed;
[0016] S2, completely peeling off the solidified Al2O3 coating on the bottom plate, and processing it into a piece of Al2O3 coating with regular shape through a machine for standby use;
[0017] S3, fixing the re-placed Al2O3 coated bottom plate with a regular shape to the placement table through a slot, and moving the placement table through a first hydraulic cylinder in cooperation with a slide rail on the workbench;
[0018] S4, when the placement table is moved to the bottom of the detection device, the Al2O3 coating on the bottom plate installed on the placement table is detected for pores by industrial CT, and the pore volume inside the Al2O3 coating is statistically analyzed after industrial CT scanning to calculate the volume ratio of the porosity;
[0019] S5. Finally, the Al2O3 coated bottom plate after the test is pushed forward to the rightmost end of the workbench, and the lifting plate is pushed upward by the second hydraulic cylinder to take the bottom plate out from the placement table through the penetration hole, so as to better perform accurate statistics of the porosity of different thermal spray coating layers.
[0020] Compared with the prior art, the present invention has the following beneficial effects:
[0021] 1. Use Al2O3 coating without primer layer to completely peel off the sprayed coating, and then machine a piece of Al2O3 coating with regular shape. After industrial CT scanning, count the internal pore volume and calculate the volume ratio of porosity. Use industrial CT to scan the same coating and give the value of coating porosity, so as to achieve accurate statistics of the porosity of the entire coating, and the result is unique.
[0022] 2. Adopting the attenuation law and absorption characteristics of X-rays or gamma rays in the object to be inspected, the object to be inspected is sliced and scanned, and finally the image is reconstructed using computer information processing technology to clearly and intuitively display the internal structure, composition and internal defect status of the object to be inspected in the form of two-dimensional or three-dimensional images. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 It is a schematic diagram of the vertical front view structure of a method for detecting coating porosity using industrial CT according to the present invention;
[0024] Figure 2 A schematic diagram of the internal structure of a method for detecting coating porosity using industrial CT according to the present invention;
[0025] Figure 3 It is a schematic diagram of the composition structure of a placing table, a bottom plate and a lifting plate of a method for detecting the porosity of a coating using industrial CT according to the present invention;
[0026] Figure 4 It is a schematic diagram of the component assembly structure of a detection machine, a detection device and a scanning head for a method of detecting coating porosity using industrial CT according to the present invention;
[0027] Figure 5 The present invention is a schematic flow chart of a method for detecting coating porosity using industrial CT.
[0028] In the figure: 1. detection machine; 2. operation frame; 3. movable frame; 4. workbench; 5. fixed groove; 6. load-bearing frame; 7. detection device; 8. scanning head; 9. slide rail; 10. first hydraulic cylinder; 11. placement table; 12. penetration hole; 13. card slot; 14. bottom plate; 15. second hydraulic cylinder; 16. lifting plate; 17. shielding plate. DETAILED DESCRIPTION
[0029] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0030] See also Figure 1-5 The present invention provides a method and technical solution for detecting the porosity of a coating using industrial CT:
[0031] A method for detecting the porosity of a coating by using industrial CT comprises a detection machine 1, an operation frame 2 is arranged on the left and right sides of the upper end of the detection machine 1, a movable frame 3 is installed at one end of the operation frame 2, a workbench 4 is installed at the upper end of the detection machine 1, a fixing groove 5 is arranged at the upper end of the workbench 4, a load-bearing frame 6 is installed at the upper end of the fixing groove 5, a detection device 7 is arranged at the upper end of the load-bearing frame 6, a scanning head 8 is installed at the lower end of the detection device 7, a slide rail 9 is arranged at the upper end of the workbench 4, a first hydraulic cylinder 10 is arranged at the left end of the workbench 4, a placing table 11 is arranged at one end of the first hydraulic cylinder 10, a penetration hole 12 is arranged on the surface of the placing table 11, a slot 13 is arranged at one end of the penetration hole 12, a bottom plate 14 is installed at the upper end of the slot 13, a second hydraulic cylinder 15 is arranged at the right end of the workbench 4, a lifting plate 16 is installed at the upper end of the second hydraulic cylinder 15, and a shielding plate 17 is installed at the upper end of the lifting plate 16.
[0032] The operating frame 2 is movably connected to the movable frame 3 , and the outer wall size of the movable frame 3 is the same as the inner wall size of the operating frame 2 .
[0033] The load-bearing frame 6 is connected to the workbench 4 by snapping together through the fixing groove 5 , and the load-bearing frame 6 is connected to the detection device 7 by embedding.
[0034] The placement table 11 forms a sliding structure with the workbench 4 through the slide rail 9 , and the placement table 11 forms a telescopic structure with the workbench 4 through the first hydraulic cylinder 10 .
[0035] The bottom plate 14 is connected to the placement platform 11 through the slot 13 , and the placement platform 11 is of an open hole design.
[0036] The lifting plate 16 forms a lifting structure with the detection machine 1 through the second hydraulic cylinder 15 , and the lifting plate 16 and the shielding plate 17 are in the same horizontal plane.
[0037] A method for detecting the porosity of a coating using industrial CT comprises the following steps:
[0038] S1, open the movable frame 3 in the device from the operation frame 2, spray the Al2O3 coating to be detected on the bottom plate 14, and wait for the Al2O3 coating to solidify after the Al2O3 coating is sprayed;
[0039] S2, completely peeling off the solidified Al2O3 coating on the bottom plate 14, and processing it into a piece of Al2O3 coating with regular shape through a machine for standby use;
[0040] S3, fix the re-placed Al2O3 coated bottom plate 14 with a regular shape to the placement table 11 through the slot 13, and move the placement table 11 through the first hydraulic cylinder 10 in cooperation with the slide rail 9 on the workbench 4;
[0041] S4, when the placement table 11 is moved to the bottom of the detection device 7, the Al2O3 coating on the bottom plate 14 installed on the placement table 11 is inspected for pores by industrial CT, and the pore volume inside the Al2O3 coating is statistically analyzed after industrial CT scanning to obtain the volume ratio of the porosity;
[0042] S5. Finally, the Al2O3 coated bottom plate 14 after the inspection is completed is pushed forward to the rightmost end of the workbench 4, and the lifting plate 16 is pushed upward by the second hydraulic cylinder 15, and the bottom plate 14 is taken out from the placement table 11 through the penetration hole 12, so as to better perform accurate statistics of the porosity of different thermal spray coating layers.
[0043] It should be noted that the present invention is a method for detecting the porosity of a coating using industrial CT. When in use, the movable frame 3 in the device is opened from the operating frame 2, and the Al2O3 coating to be detected is sprayed on the bottom plate 14. After the Al2O3 coating is sprayed, the Al2O3 coating is waited to solidify, and the solidified Al2O3 coating is completely peeled off on the bottom plate 14. After peeling, it is machined into a piece of Al2O3 coating with a regular shape for standby use, and the replaced bottom plate 14 with the Al2O3 coating with a regular shape is fixed to the placement table 11 through the card slot 13, and the placement table 11 is moved by the first hydraulic cylinder 10 in cooperation with the slide rail 9 on the workbench 4. When the placement table 11 is moved to the bottom of the detection device 7, the Al2O3 coating on the bottom plate 14 installed on the placement table 11 is detected for porosity by industrial CT, and the pore volume inside the Al2O3 coating is statistically analyzed after industrial CT scanning to calculate the volume ratio of the porosity. By utilizing the attenuation law and absorption characteristics of X-rays or gamma rays in the object to be inspected, the object to be inspected is sliced and scanned, and finally image reconstruction is performed using computer information processing technology to clearly and intuitively display the internal structure, composition and internal defect status of the object to be inspected in the form of a two-dimensional or three-dimensional image. Finally, the Al2O3 coated bottom plate 14 after the inspection is completed is pushed forward to the rightmost end of the workbench 4, and the lifting plate 16 is pushed upward by the second hydraulic cylinder 15, and the bottom plate 14 is taken out from the placement table 11 through the penetration hole 12, so as to better perform accurate statistics on the porosity of different thermal spray coating layers. In this way, a method for detecting coating porosity using industrial CT is completed.
[0044] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A method for detecting coating porosity using industrial CT. Features: The invention comprises a detection machine (1), wherein an operation frame (2) is mounted on the left and right sides of the upper end of the detection machine (1), a movable frame (3) is mounted on one end of the operation frame (2), a workbench (4) is mounted on the upper end of the detection machine (1), a fixing groove (5) is provided on the upper end of the workbench (4), a load-bearing frame (6) is mounted on the upper end of the fixing groove (5), a detection device (7) is mounted on the upper end of the load-bearing frame (6), a scanning head (8) is mounted on the lower end of the detection device (7), a slide rail (9) is provided on the upper end of the workbench (4), and the A first hydraulic cylinder (10) is installed at the left end of the workbench (4), a placing platform (11) is installed at one end of the first hydraulic cylinder (10), a through hole (12) is provided on the surface of the placing platform (11), a slot (13) is provided at one end of the through hole (12), a bottom plate (14) is installed at the upper end of the slot (13), a second hydraulic cylinder (15) is installed at the right end of the workbench (4), a lifting plate (16) is installed at the upper end of the second hydraulic cylinder (15), and a shielding plate (17) is installed at the upper end of the lifting plate (16).
2. A method for detecting coating porosity using industrial CT according to claim 1, Features: The operating frame (2) is movably connected to the movable frame (3), and the outer wall size of the movable frame (3) is the same as the inner wall size of the operating frame (2).
3. The method for detecting coating porosity using industrial CT according to claim 1, Features: The load-bearing frame (6) is snap-connected to the workbench (4) via a fixing groove (5), and the load-bearing frame (6) is embeddedly connected to the detection device (7).
4. The method for detecting coating porosity using industrial CT according to claim 1, Features: The placement platform (11) forms a sliding structure with the workbench (4) through a slide rail (9), and the placement platform (11) forms a telescopic structure with the workbench (4) through a first hydraulic cylinder (10).
5. The method for detecting coating porosity using industrial CT according to claim 1, Features: The bottom plate (14) is connected to the placement platform (11) by means of a card slot (13), and the placement platform (11) is of an open-hole design.
6. The method for detecting coating porosity using industrial CT according to claim 1, Features: The lifting plate (16) forms a lifting structure with the detection machine (1) through the second hydraulic cylinder (15), and the lifting plate (16) and the shielding plate (17) are on the same horizontal plane.
7. A method for detecting coating porosity using industrial CT. Features: The following steps are involved: S1, opening the movable frame (3) in the device from the operation frame (2), spraying the Al2O3 coating to be tested on the bottom plate (14), and after the Al2O3 coating is sprayed, waiting for the Al2O3 coating to solidify; S2, completely peeling off the solidified Al2O3 coating on the bottom plate (14), and processing it into a piece of Al2O3 coating with a regular shape through a machine for standby use; S3, fixing the re-placed Al2O3-coated bottom plate (14) with a regular shape to the placement table (11) through the clamping groove (13), and moving the placement table (11) through the first hydraulic cylinder (10) in cooperation with the slide rail (9) on the workbench (4); S4, when the placement table (11) is moved to the bottom of the detection device (7), the Al2O3 coating on the bottom plate (14) installed on the placement table (11) is inspected for pores by industrial CT, and the pore volume inside the Al2O3 coating is statistically analyzed after industrial CT scanning to calculate the volume percentage of the porosity; S5. Finally, the Al2O3 coated bottom plate (14) after the test is completed is pushed forward to the rightmost end of the workbench (4), and the lifting plate (16) is pushed upward by the second hydraulic cylinder (15), and the bottom plate (14) is taken out from the placement table (11) through the penetration hole (12), so as to better perform accurate statistics on the porosity of different thermal spray coating layers.