Inkjet recording method
By optimizing the circulation path and ink circulation conditions in the inkjet recording method, the problems of color consistency and ejection stability during long-term operation were solved, the opacity and color consistency of white images were improved, and ejection defects were reduced.
Patent Information
- Application Number
- CN202380029032.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-24
- Filing Date
- 2023-03-23
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2043-03-23
Smart Images

Figure CN118900779A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to an inkjet recording method. Background Art
[0002] In recent years, research on inkjet recording using white ink has been underway.
[0003] For example, Patent Document 1 discloses a white ink for inkjet recording as a white ink having good whiteness and excellent ejection stability, which contains a white pigment composed of a metal oxide having an average particle size of 200 nm to 400 nm and satisfies the following formula (1). 0.5×A≤V≤1.3×A…(1)
[0004] (In the above formula (1), A represents the content (mass %) of the white pigment contained in the white ink for inkjet recording. And V represents the ratio (%) of the volume of the white pigment to the total volume of the white ink for inkjet recording when the white pigment is completely precipitated in the white ink for inkjet recording.)
[0005] Patent Document 1: Japanese Patent Application Publication No. 2013-129708 Summary of the invention
[0006] Technical issues to be solved by the invention
[0007] Through research conducted by the present inventors, it was found that in an inkjet recording method using an ink containing water and a white pigment, which is titanium dioxide particles, during long-term operation (i.e., when continuous image recording is performed), the color constancy of the recorded image may be impaired (i.e., the color variation of the image becomes larger) and / or the ejection stability of the ink may be reduced.
[0008] An object of one embodiment of the present invention is to provide an inkjet recording method using ink containing water and a white pigment which is titanium dioxide particles, which has excellent color stability and ink ejection stability during long-term operation.
[0009] Means for solving technical problems
[0010] The present invention includes the following aspects.
[0011] <1> An inkjet recording method using an inkjet recording device, the inkjet recording device comprising:
[0012] An inkjet head that ejects ink; and
[0013] The circulation flow path is used to circulate the ink discharged from the inkjet head and return the ink to the inkjet head.
[0014] The inkjet recording method includes the steps of circulating ink in a circulation flow path and ejecting ink from an inkjet head to apply the ink to a recording medium.
[0015] The ink contains water and white pigment, which is titanium dioxide particles.
[0016] In the ink, the number of particles with a particle size of 0.8 μm to 5 μm in the white pigment, i.e., large white particles, is 1.00 × 10 4 Pieces / cm 3 above,
[0017] The circulation path includes a circulation pipe connected to the inkjet head for returning the ink to the inkjet head.
[0018] The speed ratio (1) defined by the following formula (1) is 5.0×10 3 Above and 1.4×10 5 the following.
[0019] Speed ratio (1) = Vc / (Vslp×log(Pn))…Formula (1)
[0020] Vslp={(ρ-ρw)gR 2} / (18η)…Formula (A)
[0021] In formula (1),
[0022] Vc is the circulation flow rate of the ink in the connection portion of the circulation pipe with the inkjet head in cm / s, Vslp is the sedimentation rate of the white macroparticles defined by formula (A) in cm / s,
[0023] Pn is the number of large white particles in the ink in pieces / cm 3 The number of units.
[0024] In formula (A),
[0025] ρ is 4.23,
[0026] ρw is the solvent in the ink in g / cm 3 The density of the unit is
[0027] g is in cm / s 2 is the unit of gravity acceleration,
[0028] R is the median particle size of the white macroparticles in cm.
[0029] η is the viscosity of the solvent in the ink at 30°C in g / cm·s.
[0030] <2> according to <1> The inkjet recording method, wherein the speed ratio (2) defined by the following formula (2) is 1.5×10 3 above.
[0031] Speed ratio (2) = speed ratio (1) × (1-cosθ) ... Formula (2)
[0032] In the formula (2), θ is the contact angle of the ink with respect to the inner surface of the circulation tube in degrees.
[0033] <3> according to <1> or <2> The inkjet recording method, wherein:
[0034] The ink is circulated through the ink tank.
[0035] The speed ratio (3) defined by the following formula (3) is 10.0 or more.
[0036] Speed ratio (3) = speed ratio (1) × (1 / L) ... Formula (3)
[0037] In the formula (3), L is the length of the circulation pipe from the ink tank to the inkjet head in cm.
[0038] Effects of the Invention
[0039] According to one embodiment of the present invention, there is provided an inkjet recording method using ink containing water and a white pigment which is titanium dioxide particles, which has excellent color stability and ink ejection stability during long-term operation. BRIEF DESCRIPTION OF THE DRAWINGS
[0040] Figure 1 This is a diagram conceptually showing an example of an inkjet recording apparatus for carrying out the inkjet recording method of the present invention. DETAILED DESCRIPTION
[0041] In the present specification, a numerical range expressed using "to" indicates a range including the numerical values described before and after "to" as the minimum value and the maximum value, respectively.
[0042] In the numerical ranges recorded in this specification, the upper limit or lower limit recorded in a certain numerical range may be replaced by the upper limit or lower limit of the numerical range recorded in other stages. In addition, in the numerical ranges recorded in this specification, the upper limit or lower limit recorded in a certain numerical range may be replaced by the value shown in the embodiments.
[0043] In the present specification, when a plurality of substances corresponding to each component are present in a composition, the amount of each component in the composition means the total amount of the plurality of substances present in the composition unless otherwise specified.
[0044] In the present specification, a combination of two or more preferred aspects is a more preferred aspect.
[0045] In the present specification, the term "process" includes not only an independent process but also a process that cannot be clearly distinguished from other processes as long as the intended purpose of the process can be achieved.
[0046] In this specification, “image” refers to the entire film formed by sequentially applying a pretreatment liquid and ink, “inkjet recording” refers to image recording by an inkjet recording method, and “image recording” refers to formation of an image (ie, film).
[0047] The concept of "image" in this specification also includes a solid image.
[0048] In this specification, unless otherwise specified, "amount applied" refers to g / m 2 In units, converted to per 1m 2 The given mass of the area (g).
[0049] In this specification, unless otherwise specified, the term "solvent" means an organic solvent.
[0050] In this specification, "(meth)acrylate" is a concept including both acrylate and methacrylate. Also, "(meth)acrylic acid" is a concept including both acrylic acid and methacrylic acid.
[0051] [Inkjet recording method]
[0052] The inkjet recording method of the present invention (hereinafter, also referred to as “recording method”) uses an inkjet recording device including:
[0053] An inkjet head that ejects ink; and
[0054] The circulation flow path is used to circulate the ink discharged from the inkjet head and return the ink to the inkjet head.
[0055] The inkjet recording method includes a step of circulating ink in a circulation flow path and ejecting ink from an inkjet head to apply the ink to a recording medium (hereinafter also referred to as an "ink applying step").
[0056] The ink contains water and a white pigment (hereinafter also referred to as "white pigment") which is titanium dioxide particles.
[0057] In the ink, the number of particles with a particle size of 0.8 μm to 5 μm in the white pigment, i.e., the number of large white particles (i.e., Pn in formula (1)) is 1.00×10 4 Pieces / cm 3 above,
[0058] The circulation path includes a circulation pipe connected to the inkjet head for returning the ink to the inkjet head.
[0059] The speed ratio (1) defined by the following formula (1) is 5.0×10 3 Above and 1.4×10 5 the following.
[0060] The recording method of the present invention may include other steps in addition to the ink applying step as necessary.
[0061] Speed ratio (1) = Vc / (Vslp×log(Pn))…Formula (1)
[0062] Vslp={(ρ-ρw)gR 2} / (18η)…Formula (A)
[0063] In formula (1),
[0064] Vc is the circulation flow rate of the ink in the connection portion of the circulation pipe with the inkjet head in cm / s, Vslp is the sedimentation rate of the white macroparticles defined by formula (A) in cm / s,
[0065] Pn is the number of large white particles in the ink in pieces / cm 3 The number of units.
[0066] In formula (A),
[0067] ρ is 4.23,
[0068] ρw is the solvent in the ink in g / cm 3 The density of the unit is
[0069] g is in cm / s 2 is the unit of gravity acceleration,
[0070] R is the median particle size of the white macroparticles in cm.
[0071] η is the viscosity of the solvent in the ink at 30°C in g / cm·s.
[0072] In the recording method of the present invention, in an inkjet recording method using ink containing water and a white pigment which is titanium dioxide particles, it is possible to improve color stability and ink ejection stability during long-term operation.
[0073] The reason why this effect can be exerted is presumed to be as follows.
[0074] Through the research of the present inventors, it was found that
[0075] In an inkjet recording method using an ink containing water and a white pigment, which is titanium dioxide particles, the color stability of the recorded image may be impaired (i.e., the color of the image changes greatly) during long-term operation (i.e., when continuous image recording is performed). The problem of color stability during long-term operation is that the number of white large particles in the ink is set to 1.00×10 4 Pieces / cm 3 This is particularly evident in the above case. That is, it is believed that the decrease in color stability during long-term operation is a problem caused by the precipitation of large white particles.
[0076] Therefore, in the recording method of the present invention, the ink is circulated during image recording, and the speed ratio (1) corresponding to the ratio of the circulation flow rate (Vc) of the ink to the precipitation rate (Vslp) of the white macroparticles defined by the formula (A) is set to 5.0×10 3 This is considered to suppress the precipitation of large white particles, and as a result, suppress the decrease in color stability during long-term operation.
[0077] On the other hand, the inventors have found that by limiting the speed ratio (1) to 1.4×10 5 As a result, it is possible to suppress a decrease in discharge stability during long-term operation.
[0078] As described above, it is considered that in the recording method of the present invention, by setting the speed ratio (1) to 5.0×10 3 Above and 1.4×10 5 As a result, the color stability and ink ejection stability during long-term operation can be improved.
[0079] <Inkjet Recording Device>
[0080] In the recording method of the present invention, an inkjet recording device is used, and the inkjet recording device includes:
[0081] an inkjet head that ejects ink containing water and a white pigment that is titanium dioxide particles; and
[0082] The circulation flow path is used to circulate the ink so that the ink discharged from the inkjet head flows and returns to the inkjet head.
[0083] (Inkjet Head)
[0084] The inkjet recording device in the present invention includes an inkjet head (for example, the inkjet recording device described below) for ejecting ink containing water and a white pigment as titanium dioxide particles. Figure 1 The inkjet head IJ1 in the apparatus.
[0085] As the inkjet head, a known inkjet head can be used without any particular limitation.
[0086] There is no particular limitation on the method of ejecting ink from the inkjet head, and it can be any of the known methods, for example, a charge control method that utilizes electrostatic induction force to eject ink, a drop-on-demand inkjet method (pressure pulse method) that utilizes the vibration pressure of a piezoelectric element, an acoustic inkjet method that converts an electrical signal into a sound beam and irradiates the beam onto the ink, and ejects the ink using radiation pressure, and a thermal inkjet method (Bubble Jet (registered trademark)) that heats the ink to form bubbles and uses the generated pressure to eject the ink.
[0087] As a recording method using an inkjet head, the method described in Japanese Patent Publication No. 54-59936 can be particularly effectively used, in which the ink subjected to thermal energy undergoes a rapid volume change, and the ink is ejected from the nozzle by the force of the state change. As a recording method using an inkjet head, the method described in paragraphs 0093 to 0105 of Japanese Patent Publication No. 2003-306623 can also be applied.
[0088] Inkjet head methods include: a reciprocating method in which a short strip-shaped serial head records while scanning in the width direction of a recording medium; and a linear method in which a linear head having recording elements arranged corresponding to the entire area of one side of a recording medium is used.
[0089] In the linear method, by scanning the recording medium in a direction intersecting the arrangement direction of the recording elements, it is possible to record an image on the entire surface of the recording medium. In the linear method, there is no need for a transport system such as a carriage for scanning a short strip of inkjet head in the reciprocating method. In addition, compared with the reciprocating method, in the linear method, there is no need for complex scanning control between the movement of the carriage and the recording medium, and only the movement of the recording medium is required. Therefore, according to the linear method, it is possible to achieve higher speed image recording than in the reciprocating method.
[0090] The resolution of the inkjet head is preferably 300 dpi or higher (more preferably 600 dpi or higher, and even more preferably 800 dpi or higher).
[0091] Among them, dpi is the abbreviation of dot per inch, and linch (1 inch) is 2.54cm.
[0092] From the viewpoint of obtaining a high-definition image, the amount of ink ejected from the inkjet head is preferably 1 pL (picoliter) to 10 pL, and more preferably 1.5 pL to 6 pL.
[0093] The inkjet head ejects ink from nozzles and discharges the ink for the purpose of circulating the ink.
[0094] The ink may be discharged from the inkjet head by returning the ink to the inkjet head through a circulation pipe and squeezing the ink from the inkjet head.
[0095] The ejection and discharge of ink may be performed simultaneously or at different times.
[0096] The inkjet head is connected to a circulation pipe (for example, Figure 1 Circulation pipes C1 and C2).
[0097] The circulation pipe connected to the inkjet head forms a circulation path for ink circulation alone or together with other components (for example, an ink tank, an infusion pump, a filter, a heat exchanger, a flow meter, etc.).
[0098] (Circulation Path)
[0099] The inkjet recording device in the present invention includes a circulation flow path for circulating ink, and the ink circulation allows ink discharged from the inkjet head to flow and return to the inkjet head.
[0100] The circulation flow path includes at least a circulation pipe (for example, a circulation pipe described below) connected to the inkjet head and returning the ink to the inkjet head. Figure 1 Circulation pipe C2 in the middle).
[0101] The circulation flow path may also include a circulation pipe (for example, a circulation pipe described below) connected to the inkjet head and discharging ink from the inkjet head. Figure 1 Circulation pipe C1).
[0102] Furthermore, the circulation flow path may be constituted by the circulation pipe and components other than the circulation pipe.
[0103] As components other than the circulation pipe, for example, there can be mentioned:
[0104] Ink tanks for storing ink (e.g., main tanks, buffer tanks, etc.);
[0105] Infusion pump for delivering ink;
[0106] Filters for removing foreign matter from ink;
[0107] Degassing module for degassing inks;
[0108] A heat exchanger for regulating the temperature of the ink;
[0109] A flow meter for measuring ink flow;
[0110] connectors; and
[0111] Valve; etc.
[0112] The inkjet recording device in the present invention may include an inkjet head and other components besides the circulation flow path.
[0113] As other components, any components provided in the inkjet recording apparatus can be appropriately applied without particular limitation.
[0114] (An example of an inkjet recording device)
[0115] Hereinafter, an example of an inkjet recording apparatus used in the recording method of the present invention will be described with reference to the drawings.
[0116] However, the inkjet recording apparatus used in the recording method of the present invention is not limited to the following example.
[0117] Figure 1 This is a diagram conceptually showing an example of an inkjet recording apparatus used in the inkjet recording method of the present invention.
[0118] like Figure 1 As shown, the inkjet recording device involved in this example is an example of an inkjet recording device having a conveying mechanism for conveying the recording medium in a roll-to-roll manner. The recording medium A1 in the shape of a long film in a roll is unwound by the unwinding device W1, and the wound recording medium A1 is conveyed along the direction of the hollow arrow, so that it passes through the pretreatment liquid imparting device P1, the pretreatment liquid drying area DP1, the inkjet head IJ1 and the drying area D1 in sequence, and is finally wound up by the winding device W2.
[0119] In this example, the pretreatment liquid is a liquid applied to the recording medium before applying the ink.
[0120] The pretreatment liquid contains, for example, water and a coagulant.
[0121] The pretreatment liquid will be described later.
[0122] The recording method of the present invention is not limited to the method using the pre-treatment liquid, and the ink may be applied to the recording medium without using the pre-treatment liquid.
[0123] In this case, the pre-treatment liquid applying device P1 and the pre-treatment liquid drying area DP1 can be omitted.
[0124] And, because Figure 1 This is a conceptual diagram, so the conveying path of the recording medium A1 is simplified in the diagram, and the recording medium A1 is conveyed in one direction. However, it goes without saying that in reality, the conveying path of the recording medium A1 can also be curved.
[0125] As a method of conveying the recording medium A1, various web conveying methods such as a barrel and a roller can be appropriately selected.
[0126] For the unwinding device W1 for unwinding the recording medium A1, a pretreatment liquid imparting device P1, a pretreatment liquid drying area DP1, an inkjet head IJ1 and a drying area D1 are arranged in sequence from the upstream side of the conveying direction of the recording medium A1 (hereinafter referred to as the "upstream side") on the downstream side of the conveying direction of the recording medium A1 (hereinafter referred to as the "downstream side").
[0127] The pretreatment liquid applying device P1 and the inkjet head IJ1 respectively apply the pretreatment liquid and the ink.
[0128] At this time, at least one of heating and drying the pre-treatment liquid in the pre-treatment liquid drying area DP1 and heating and drying the ink in the drying area D1 can be performed.
[0129] In the drying region D1 , in addition to the heating and drying of the ink, the heating and drying of the pretreatment liquid can be substantially performed.
[0130] Furthermore, if the recording medium is passed through each drying zone while the temperature of each drying zone is set to room temperature, heating and drying can be omitted.
[0131] A surface treatment unit (not shown) for performing a surface treatment (preferably a corona treatment) on the recording medium A1 may be provided on the upstream side of the pre-treatment liquid applying device P1.
[0132] Furthermore, a cooling region for cooling the recorded image may be provided on the downstream side of the drying region D1.
[0133] The inkjet head IJ1 may be a reciprocating type inkjet head, but is preferably a line head having a plurality of ejection ports (nozzles) arranged in the width direction of the long film-shaped recording medium A1 from the viewpoint of speeding up image recording.
[0134] One end of a circulation pipe C1 and one end of a circulation pipe C2 are connected to the inkjet head IJ1. The other ends of the circulation pipe C1 and the other ends of the circulation pipe C2 are connected to the ink tank IT1.
[0135] In the inkjet recording device of this example, these structures enable ink circulation, in which ink is discharged from the inkjet head IJ1 to the circulation pipe C1, and the discharged ink is circulated and returned to the inkjet head IJ1 through the circulation pipe C2 (see Figure 1 F1).
[0136] Although not shown in the figure, a degassing module for degassing ink, an infusion pump for infusing ink, a filter for removing foreign matter, a heat exchanger for adjusting the temperature of ink, and the like may be arranged in the middle of the circulation pipes C1 and C2.
[0137] Furthermore, the ink tank IT1 may be a main tank or a buffer tank. When the ink tank IT1 is a buffer tank, a main tank (not shown) is connected to the ink tank IT1 as a buffer tank.
[0138] Only one inkjet head IJ1 may be provided, or a plurality of inkjet heads IJ1 may be provided.
[0139] For example, a plurality of inkjet heads IJ1 may be arranged along the conveyance direction of the recording medium A1. This enables application of white ink (hereinafter also referred to as "white ink") and color ink.
[0140] Here, the color ink refers to an ink of a color other than white. The concept of the color ink includes not only color inks such as cyan ink, magenta ink, and yellow ink, but also achromatic inks such as black ink (hereinafter, also referred to as "black ink"). Similarly, the concept of the "color image" in the present invention includes not only color images but also black images (hereinafter, also referred to as "black images").
[0141] When a plurality of inkjet heads IJ1 are arranged, components for performing the above-described ink circulation (for example, circulation pipes C1 and C2 , ink tank IT1 , etc.) can be connected to each of the plurality of inkjet heads IJ1 .
[0142] In inkjet recording using the image recording apparatus according to this example:
[0143] First, the recording medium A1 in the form of a long film wound into a roll is unwound by the unwinding device W1;
[0144] The unrolled recording medium A1 is conveyed in the direction of arrow R1;
[0145] The pretreatment liquid is applied to the transported recording medium A1 by the pretreatment liquid applying device P1;
[0146] Next, the pretreatment liquid is dried in the pretreatment liquid drying area DP1 as needed;
[0147] Next, ink is ejected from a nozzle (not shown) in the inkjet head IJ1 onto the area to which the pretreatment liquid has been applied (see FIG. Figure 1 ), dashed arrow in the figure;
[0148] Next, the ink is dried in the drying area D1 as necessary.
[0149] Thus, an image recorded material in which an image derived from ink is recorded on the recording medium A1 (that is, the recording medium A1 with an image) can be obtained.
[0150] Next, the image is cooled as necessary, and finally the image recorded material (ie, the image-attached recording medium A1) is wound up by the winding device W2.
[0151] In the inkjet head IJ1, when the ink is ejected (reference Figure 1 At the same time, ink is discharged to the circulation pipe C1 (see the dotted arrow in the figure). Figure 1 arrow F1).
[0152] The ejection and discharge of ink may be performed simultaneously or at different times.
[0153] The ink discharged to the circulation pipe C1 is transferred via a path from the circulation pipe C1 to the ink tank IT1 and then to the circulation pipe C2, and then returns to the inkjet head IJ1 through the circulation pipe C2.
[0154] In this manner, in the inkjet recording apparatus, when ink is ejected from the inkjet head IJ1 (reference Figure 1 The ink is circulated (see Figure 1 arrow F1).
[0155] Ink ejection and ink circulation can be performed simultaneously or at different times.
[0156] The ink circulation can be continuous or intermittent.
[0157] Furthermore, the paths along which the ink circulates can be transferred alternately as required.
[0158] Furthermore, as described above, in the above example, the application and drying operations of the pretreatment liquid may be omitted.
[0159] In this case, in the inkjet recording apparatus according to the above example, the pre-treatment liquid applying device P1 and the pre-treatment liquid drying area DP1 may be omitted.
[0160] <Ink application process>
[0161] The recording method of the present invention includes an ink applying step.
[0162] The ink applying step is a step of circulating the ink through the circulation channel, ejecting the ink from the inkjet head, and applying the ink to the recording medium.
[0163] An image can be obtained by ejecting the ink onto a recording medium.
[0164] (Recording Medium)
[0165] The recording medium is not particularly limited, and a known recording medium such as a paper substrate and a resin substrate can be used without particular limitation.
[0166] As the paper substrate, for example, so-called coated paper generally used for offset printing, etc. As the coated paper, there can be mentioned paper having a coating material applied to the surface, such as high-quality paper and neutral paper which are generally not surface-treated and are mainly composed of cellulose.
[0167] The resin substrate is not particularly limited, but is preferably a resin substrate having a film shape (ie, a sheet shape).
[0168] The thickness of the resin substrate is preferably 12 μm to 200 μm, more preferably 12 μm to 100 μm, further preferably 12 μm to 60 μm, and further preferably 15 μm to 60 μm.
[0169] The shape of the resin substrate may be a long film shape (ie, a long sheet shape).
[0170] The length of the resin substrate in the form of a long film is not particularly limited, but is preferably 5 m or longer, more preferably 10 m or longer, and even more preferably 100 m or longer.
[0171] The upper limit of the length of the resin substrate in the case of a long film shape is also not particularly limited, and examples of the upper limit include 10000 m, 8000 m, and 5000 m.
[0172] Examples of the resin substrate include a polyester substrate, a polyethylene substrate, a polypropylene substrate, and a nylon substrate.
[0173] The resin substrate may be a stretched substrate or an unstretched substrate.
[0174] The resin substrate may be a transparent, non-permeable substrate.
[0175] Here, having transparency means that the transmittance of visible light with a wavelength of 400 nm to 700 nm is 80% or more (preferably 90% or more).
[0176] When the resin substrate is a transparent resin substrate, the image can be easily visually recognized through the resin substrate from the image non-recording surface side of the resin substrate.
[0177] For example, in the case where the resin substrate is a transparent resin substrate, when a pretreatment liquid, at least one coloring ink, and a white ink as the ink of the present invention are sequentially applied to the resin substrate to record an intermediate color image, a colored image (e.g., a pattern image of characters, graphics, etc.) with a white image (e.g., a solid image) as a background can be easily visually recognized through the resin substrate from the image non-recording surface side of the resin substrate.
[0178] The resin substrate may be surface treated.
[0179] Examples of the surface treatment include corona treatment, plasma treatment, frame treatment, heat treatment, abrasion treatment, light irradiation treatment (UV treatment), and flame treatment, but the surface treatment is not limited to these.
[0180] (Ink circulation and ink ejection)
[0181] The ink circulation and the ink discharge in the ink applying step are as described above.
[0182] (Ink)
[0183] The ink that is circulated and discharged in the ink applying step is an ink (for example, white ink) that is a white pigment containing water and titanium dioxide particles.
[0184] In the ink, the number of particles with a particle size of 0.8 μm to 5 μm in the white pigment, i.e., the number of large white particles (i.e., Pn in formula (1)) is 1.00×10 4 Pieces / cm 3 In other words, in the ink of the present invention, every 1 cm 3 The number of large white particles in the ink is 1.00×10 4 More than one.
[0185] The number of large white particles (i.e., Pn in formula (1)) is 1.00×10 4 Pieces / cm 3 The above helps to improve the concealment of the recorded image.
[0186] In the present invention, the hiding property refers to one of the properties of an image, and means a property of hiding a base (for example, a recording medium, a colored image recorded on a recording medium, etc.) on which the image is recorded.
[0187] Generally speaking, the number of large white particles is 1.00×10 4 Pieces / cm 3 In the above case, although it is advantageous for the hiding property, large white particles are easily precipitated in the ink, and as a result, the color stability is impaired during long-term operation.
[0188] However, according to the recording method of the present invention, the speed ratio (1) is set to 5.0×10 3 The above (in short, increasing the circulation rate of the ink relative to the sedimentation rate of the ink) can solve the sedimentation problem of large white particles, and as a result, can solve the problem of color stability during long-term operation.
[0189] In the present invention, the number of large white particles (ie, particles having a particle size of 0.8 μm to 5 μm in the white pigment) (ie, Pn in the formula (1)) refers to a value measured using a particle size distribution meter.
[0190] In the examples described below, a wet dispersion type injection type image analysis particle size distribution meter "IF-3200S" manufactured by JASCO Corporation was used as a particle size distribution meter. The number of white large particles in an aqueous solution obtained by diluting the ink 5000 times with water was measured, and the number of white large particles per 1 cm was calculated based on the measured value. 3 The number of large white particles in the ink (unit: pieces / cm 3 ).
[0191] Preferred embodiments of the ink in the present invention will be described later.
[0192] (Heating and drying of ink)
[0193] The ink applying step may include a step of heating and drying the applied ink on the recording medium.
[0194] The method of heat-drying the ink is not particularly limited, and examples thereof include infrared (IR) drying, warm air drying, and heat drying using a heating device (eg, a heater, a hot plate, a heating furnace, etc.).
[0195] As a method of heating and drying the ink, a method of combining two or more of these may be used.
[0196] Heat drying can be performed by heating the ink from at least one of the image recording surface side and the image non-recording surface side of the recording medium.
[0197] The heating temperature in heat drying of the ink is preferably 30°C to 100°C, more preferably 35°C to 90°C, and even more preferably 40°C to 80°C.
[0198] The heating time in the heat drying of the ink is not particularly limited, but is preferably 1 second to 180 seconds, more preferably 1 second to 120 seconds, and even more preferably 1 second to 60 seconds.
[0199] <Speed Ratio (1)>
[0200] In the recording method of the present invention, the speed ratio (1) defined by the following formula (1) is 5.0×10 3 Above and 1.4×10 5 the following.
[0201] Speed ratio (1) = Vc / (Vslp×log(Pn))…Formula (1)
[0202] Vslp={(ρ-ρw)gR 2} / (18η)…Formula (A)
[0203] In formula (1),
[0204] Vc is the circulation flow rate of the ink in the connection portion of the circulation pipe with the inkjet head in cm / s, Vslp is the sedimentation rate of the white macroparticles defined by formula (A) in cm / s,
[0205] Pn is the number of large white particles in the ink in pieces / cm 3 The number of units.
[0206] In formula (A),
[0207] ρ is 4.23,
[0208] ρw is the solvent in the ink in g / cm 3 The density of the unit is
[0209] g is in cm / s 2 is the unit of gravity acceleration,
[0210] R is the median particle size of the white macroparticles in cm.
[0211] η is the viscosity of the solvent in the ink at 30°C in g / cm·s.
[0212] In the formula (1) defining the speed ratio (1), the factor for improving the effect of color stability during long-term operation, namely "Vc" (circulation flow rate of ink), is configured in the numerator, and the factors for suppressing color stability during long-term operation, namely "Vslp" (precipitation rate of large white particles) and "log (Pn)" (Pn is the number of large white particles) are configured in the denominator.
[0213] The passing speed ratio (1) is 5.0×10 3 As described above, the effect of color stability during long-term operation can be obtained.
[0214] On the other hand, the passing speed ratio (1) is 1.4×10 5 Next, the effect of ink ejection stability during long-term operation can be obtained.
[0215] The speed ratio (1) is preferably 1.0×10 4 Above and 1.0×10 5 Below, more preferably 1.0×10 4 Above and 9.3×10 4 Below, more preferably 1.0×10 4 Above and 7.0×10 4 the following.
[0216] In the formula (1), Vc is the circulation flow rate of the ink in the connection portion with the inkjet head in the circulation pipe, expressed in cm / s.
[0217] Vc is calculated based on the flow rate of the ink in the connection portion and the flow path cross-sectional area of the circulation pipe in the connection portion.
[0218] Vc is preferably 5-100, more preferably 10-80.
[0219] In formula (1), Pn is the number of white macroparticles in the ink in pieces / cm 3 That is, Pn is the number of units per 1cm 3 The number of large white particles (i.e., particles with a particle size of 0.8 μm to 5 μm in the white pigment) in the ink.
[0220] The method for determining Pn was as described above.
[0221] As mentioned above, Pn satisfies 1.00×10 9 Pieces / cm 3 The above value.
[0222] Pn is preferably 1.00×10 9 Pieces / cm 3 Above and 1.00×10 13 Pieces / cm 3 The value is within the range below.
[0223] In formula (1), Vslp is the sedimentation velocity of the white macroparticles defined by formula (A) in cm / s.
[0224] Vslp is preferably 1.00×10 -6 Above and 1.00×10 -3 the following.
[0225] The formula (A) defining Vslp is a formula based on Stokes' theorem.
[0226] In formula (A), ρ is 4.23.
[0227] Here, "4.23" (=ρ) is the mass of rutile titanium dioxide in g / cm 3 The density of the unit.
[0228] In formula (A), ρw is the solvent in the ink in g / cm 3 The density in units.
[0229] Here, the solvent in the ink contains at least water.
[0230] In the case where the ink contains an organic solvent, the solvent in the ink contains water and the organic solvent.
[0231] ρw is measured by the following method.
[0232] By testing the ink under an acceleration of 10000G (Note: 1G = 9.80665m / s 2 ) for 60 minutes to separate the solvent from the ink, measure the mass and volume of the obtained solvent, and calculate the solvent's mass in g / cm 3 is the density of units (ρw).
[0233] ρw in the formula (A) is 0.70 to 1.30, preferably 0.80 to 1.20, and more preferably 0.90 to 1.10.
[0234] In formula (A), R is the median particle size (d50) of the white large particles in cm.
[0235] In the present invention, the median diameter (d50) in cm of white large particles (ie, particles having a particle diameter of 0.8 μm to 5 μm in white pigment) refers to a value measured using a particle size distribution analyzer.
[0236] In the examples described below, a wet dispersion type injection image analysis particle size distribution meter "IF-3200S" manufactured by Jasco Corporation was used as a particle size distribution meter to measure the median particle size (d50) in cm of white large particles in an aqueous solution obtained by diluting the ink 5000 times with water.
[0237] R in formula (A) is preferably 1.00×10 -5 Above and 1.00×10 -3 Below, more preferably 1.00×10 -4 Above and 1.00×10 -3 the following.
[0238] η in formula (A) is the viscosity of the solvent in the ink at 30° C. in units of g / cm·s.
[0239] The viscosity is a value measured with an E-type viscometer.
[0240] η in formula (A) is measured as follows.
[0241] By applying an acceleration of 10000G (Note: 1G = 9.80665m / s 2 ) for 60 minutes to separate the solvent from the ink, and the viscosity of the obtained solvent in g / cm·s at 30° C. was measured using an E-type viscometer.
[0242] The η in formula (A) is preferably 1.00×10 -2 Above and 1.00×10 -3 Below, more preferably 0.30×10-2 Above and 0.70×10 -2 the following.
[0243] <Speed Ratio (2)>
[0244] In the recording method of the present invention, the speed ratio (2) defined by the following formula (2) is preferably 1.2×10 3 More preferably, 1.5×10 3 above.
[0245] Speed ratio (2) = speed ratio (1) × (1-cosθ) ... Formula (2)
[0246] In the formula (2), θ is the contact angle of the ink with respect to the inner surface of the circulation pipe that returns the ink to the inkjet head in degrees.
[0247] θ is a contact angle (°) defined within a range of greater than 0 and less than 180, and a larger value within this range is more favorable to the effect of color stability during long-term operation.
[0248] That is, (1-cosθ) is a factor that increases the effect of color stability during long-term operation.
[0249] When the speed ratio (2) is 1.2×10 3 In the above case, the color stability during long-term operation is further improved.
[0250] (1-cosθ) itself is not particularly limited.
[0251] (1-cosθ) is, for example, not less than 0.05 and not more than 0.60, and preferably not less than 0.10 and not more than 0.20.
[0252] From the viewpoint of further improving the color stability during long-term operation and further improving the ink ejection stability during long-term operation, the speed ratio (2) is preferably 1.2×10 3 Above and 1.0×10 5 Below, more preferably 1.5×10 3 Above and 8.0×10 4 the following.
[0253] In the present invention, regarding θ, a contact angle measurement sample is prepared by cutting a connection portion of a circulation pipe for returning ink to the inkjet head with a cutter and stretching the pipe into a flat plate. The contact angle measurement sample is used for measurement.
[0254] Specifically, ink is dropped onto the surface of the contact angle measurement sample corresponding to the inner surface of the circulation tube, and the contact angle of the ink with respect to the inner surface of the circulation tube is measured.
[0255] The contact angle was measured using a contact angle measuring device under the conditions of 25° C., 50 RH%, an ink droplet size of 2 μL, and a waiting time of 1000 ms from droplet placement to measurement.
[0256] <Speed Ratio (3)>
[0257] In the recording method of the present invention, when the ink is circulated via the ink tank,
[0258] The speed ratio (3) defined by the following formula (3) is preferably 8.0 or more, and more preferably 10.0 or more.
[0259] Speed ratio (3) = speed ratio (1) × (1 / L) ... Formula (3)
[0260] In the formula (3), L is the length (cm) of the circulation pipe from the ink tank to the inkjet head (ie, the circulation pipe that returns the ink to the inkjet head).
[0261] The larger the value of L is, the more the effect of color stability during long-term operation is suppressed.
[0262] In the equation (3) defining the speed ratio (3), L is placed in the denominator.
[0263] Therefore, the larger the value of the speed ratio (3), specifically, when the speed ratio (3) is 8.0 or more, the effect of color stability during long-term operation is further improved.
[0264] From the viewpoint of further improving the effect of color stability during long-term operation, the speed ratio (3) is more preferably 10.0 or more.
[0265] From the viewpoint of further improving the color stability during long-term operation and further improving the ink ejection stability during long-term operation, the speed ratio (3) is preferably 8.0 to 120.0, more preferably 8.0 to 100.0, and even more preferably 8.0 to 80.0.
[0266] L itself in formula (3) is not particularly limited.
[0267] L is, for example, 200 or more and 5000 or less, preferably 300 or more and 3000 or less, more preferably 500 or more and 2400 or less, and further preferably 600 or more and 2000 or less.
[0268] <Preferred Mode of Ink>
[0269] The ink in the present invention contains water and a white pigment which is titanium dioxide particles.
[0270] Hereinafter, preferred embodiments of the ink in the present invention will be described.
[0271] (water)
[0272] The ink contains water.
[0273] The content of water is preferably 10% by mass or more, more preferably 20% by mass or more, further preferably 30% by mass or more, and particularly preferably 50% by mass or more, relative to the total amount of the ink.
[0274] The upper limit of the water content relative to the total amount of the ink can be appropriately determined according to the contents of other components, and is, for example, 99% by mass, preferably 95% by mass, and more preferably 90% by mass.
[0275] (Water-soluble organic solvent)
[0276] The ink contains a water-soluble organic solvent.
[0277] This ensures the stability of ejection from the inkjet head.
[0278] The water-soluble organic solvent contained in the ink may be one kind or two or more kinds.
[0279] In the present invention, "water-soluble" means a property of dissolving 1 g or more in 100 g of water at 25°C.
[0280] In the present invention, "water-insoluble" refers to a property that the amount of a compound that dissolves in 100 g of water at 25°C is less than 1 g.
[0281] The type of water-soluble organic solvent that can be contained in the ink is not limited, and examples thereof include:
[0282] Monoalcohols having 1 to 4 carbon atoms;
[0283] Diols such as 1,3-propylene glycol, 1,3-butylene glycol, 1,4-butylene glycol, 2-butene-1,4-diol, 2-ethyl-1,3-hexanediol, 2-methyl-2,4-pentanediol, 1,2-octanediol, 1,2-hexanediol, 1,2-pentanediol, and 4-methyl-1,2-pentanediol;
[0284] Triols such as propylene glycol, 1,2,6-hexanetriol, and trimethylolpropane;
[0285] Alkylene glycols such as ethylene glycol and propylene glycol;
[0286] Alkylene glycol monoalkyl ethers such as ethylene glycol monoalkyl ether and propylene glycol monoalkyl ether;
[0287] Polyalkylene glycols such as diethylene glycol, triethylene glycol, tetraethylene glycol, pentaethylene glycol, dipropylene glycol, polyoxyethylene polyoxypropylene glycol, etc.;
[0288] Polyalkylene glycol ethers such as diethylene glycol monoalkyl ether, triethylene glycol monoalkyl ether, tripropylene glycol monoalkyl ether, polyoxypropylene glycerol ether;
[0289] 2-pyrrolidone, N-methyl-2-pyrrolidone; etc.
[0290] From the viewpoint of discharge stability, the water-soluble organic solvent in the ink preferably contains at least one selected from the group consisting of alkylene glycols and alkylene glycol monoalkyl ethers.
[0291] The content of the water-soluble organic solvent is preferably 10% by mass to 40% by mass, and more preferably 15% by mass to 30% by mass, based on the total amount of the ink.
[0292] (white pigment)
[0293] The ink contains white pigment which is titanium dioxide particles.
[0294] The white pigment includes white macroparticles having a particle size of 0.8 μm to 5 μm.
[0295] The number of large white particles (Pn) is as described above.
[0296] The white pigment preferably contains rutile titanium dioxide.
[0297] The proportion of rutile titanium dioxide in the entire white pigment is preferably 50% by mass or more, more preferably 60% by mass or more, and further preferably 80% by mass or more. The proportion of rutile titanium dioxide in the entire white pigment may be 100% by mass or less.
[0298] From the viewpoint of hiding power, the average primary particle size of the white pigment is preferably 150 nm or more, more preferably 200 nm or more, and from the viewpoint of ink ejection properties, the average primary particle size of the white pigment is preferably 400 nm or less, more preferably 350 nm or less.
[0299] In the present invention, the average primary particle size of the white pigment is a value measured using a transmission electron microscope (TEM). Specifically, it is a value obtained by selecting any 50 white pigments present in the viewing angle observed by TEM, measuring 50 primary particle sizes, and averaging them. As a transmission electron microscope, a transmission electron microscope 1200EX manufactured by JEOL Ltd. can be used.
[0300] From the viewpoint of image density and ejection properties, the content of the white pigment in the ink is preferably 2 to 25% by mass, more preferably 5 to 25% by mass, and even more preferably 10 to 20% by mass, based on the total amount of the ink.
[0301] (Pigment dispersion resin)
[0302] The ink may contain at least one pigment dispersion resin.
[0303] In the present invention, the pigment dispersing resin refers to a resin having a function of dispersing a pigment.
[0304] The pigment dispersing resin may be a random copolymer or a block copolymer.
[0305] Furthermore, the pigment dispersion resin may have a cross-linked structure.
[0306] The ink can also be prepared using a pigment dispersion containing a pigment and a pigment dispersing resin.
[0307] As the pigment dispersion resin, for example, a known polymer dispersant such as the polymer dispersants described in paragraphs 0029 to 0106 of International Publication No. 2021 / 221069 can be used.
[0308] When the ink contains a pigment dispersion resin, the ratio of the content of the pigment to the content of the pigment dispersion resin in the ink is preferably 1:0.04 to 1:3, more preferably 1:0.05 to 1:1, and even more preferably 1:0.05 to 1:0.5 on a mass basis.
[0309] When the ink contains a pigment dispersion resin, the content of the pigment dispersion resin is preferably 0.1 to 10% by mass, more preferably 0.3 to 5% by mass, and even more preferably 0.5 to 2.5% by mass, based on the total amount of the ink.
[0310] (resin particles)
[0311] The ink may contain at least one type of resin particles.
[0312] Examples of the resin particles that may be contained in the ink include the same resin particles as those that may be contained in the pretreatment liquid.
[0313] However, the resin particles in the ink may be the same as or different from the resin particles in the pretreatment liquid.
[0314] When the ink contains a resin, it is preferred that the ink contain at least one type of resin particles.
[0315] The resin particles are preferably at least one selected from the group consisting of acrylic resin particles, ester resin particles, a mixture of acrylic resin particles and ester resin particles, composite particles containing acrylic resin and ester resin, and polyurethane resin particles.
[0316] The content of the resin particles in the ink is preferably 1% by mass to 20% by mass, more preferably 2% by mass to 15% by mass, and even more preferably 2% by mass to 10% by mass, based on the total amount of the ink.
[0317] (additive)
[0318] The ink may contain additives such as a surfactant, a water-soluble resin, a co-sensitizer, an ultraviolet absorber, an antioxidant, an anti-fading agent, a conductive salt, and an alkaline compound as required.
[0319] (physical properties)
[0320] From the viewpoint of improving discharge stability, the pH (25° C.) of the ink is preferably 7 to 10, and more preferably 7.5 to 9.5. The pH of the color ink can be measured by the same method as the pH of the pretreatment liquid.
[0321] The viscosity of the ink (25° C.) is preferably 0.5 to 30 mPa·s, more preferably 2 to 20 mPa·s, preferably 2 to 15 mPa·s, and further preferably 3 to 10 mPa·s. The viscosity of the ink can be measured by the same method as the viscosity of the pretreatment liquid.
[0322] The surface tension (25° C.) of the ink is preferably 60 mN / m or less, more preferably 20 mN / m to 50 mN / m, and even more preferably 30 mN / m to 45 mN / m.
[0323] The surface tension can be measured by the same method as in the case of the pretreatment liquid.
[0324] <Coloring ink>
[0325] In the recording method of the present invention, when white ink containing water and a white pigment is used as the ink in the present invention, a colored ink (for example, black ink and / or color ink) may be used in addition to the white ink.
[0326] The colored ink may be applied to the lower layer side relative to the white ink, may be applied to the upper layer side relative to the white ink, or may be applied to a portion different from the portion to which the white ink is applied.
[0327] <Pretreatment solution>
[0328] In the recording method of the present invention, as shown in the above example, not only ink but also a pre-treatment liquid can be used.
[0329] The pretreatment liquid preferably contains water and a coagulant.
[0330] (water)
[0331] The pretreatment liquid preferably contains water.
[0332] The content of water is preferably 50% by mass or more, more preferably 60% by mass or more, based on the total amount of the pretreatment liquid.
[0333] The upper limit of the water content also depends on the amounts of other components, but is preferably 90% by mass or less, more preferably 80% by mass or less, based on the total amount of the pretreatment liquid.
[0334] (Agglutinating agent)
[0335] The pretreatment liquid preferably contains at least one coagulant.
[0336] The coagulant in the pretreatment liquid aggregates the components in the ink on the recording medium, thereby improving the image quality of the image derived from the ink.
[0337] The coagulant is preferably at least one selected from the group consisting of organic acids, polyvalent metal compounds, metal complexes, and cationic polymers.
[0338] Preferred examples of the coagulant include those described in paragraphs 0122 to 0130 of International Publication No. 2020 / 195360.
[0339] Hereinafter, preferred embodiments of each of the organic acid, the polyvalent metal compound, the metal complex, and the cationic polymer that can be used as the coagulant will be described.
[0340] -Organic Acids-
[0341] Examples of the organic acid include organic compounds having an acidic group.
[0342] Examples of the acidic group include a phosphoric acid group, a phosphonic acid group, a phosphinic acid group, a sulfuric acid group, a sulfonic acid group, a sulfonic acid group, a sulfinic acid group, and a carboxyl group.
[0343] Among them, from the viewpoint of the aggregation speed of the ink, the acidic group is preferably a phosphoric acid group or a carboxyl group, and more preferably a carboxyl group.
[0344] It is preferred that at least a part of the acidic groups be dissociated in the pretreatment liquid.
[0345] Examples of the organic compound having a carboxyl group include (meth)acrylic acid, poly(meth)acrylic acid, acetic acid, formic acid, benzoic acid, glycolic acid, malonic acid, malic acid (preferably DL-malic acid), maleic acid, succinic acid, glutaric acid, pimelic acid, adipic acid, fumaric acid, citric acid, tartaric acid, phthalic acid, 4-methylphthalic acid, lactic acid, pyrrolidonecarboxylic acid, pyranonecarboxylic acid, pyrrolecarboxylic acid, furancarboxylic acid, pyridinecarboxylic acid, coumaric acid, thiophenecarboxylic acid and nicotinic acid.
[0346] Among them, from the viewpoint of the aggregation speed of the ink, the organic compound having a carboxyl group is preferably a divalent or higher-valent carboxylic acid (hereinafter also referred to as a polyvalent carboxylic acid), and more preferably a dicarboxylic acid.
[0347] Specifically, the polycarboxylic acid is preferably malonic acid, malic acid, maleic acid, succinic acid, glutaric acid, pimelic acid, adipic acid, fumaric acid, tartaric acid, 4-methylphthalic acid or citric acid, and more preferably malonic acid, malic acid, tartaric acid, succinic acid, glutaric acid, pimelic acid, adipic acid or citric acid.
[0348] The organic acid preferably has a low pKa (eg, 1.0 to 5.0). Thus, contact with an organic acid with a lower pKa can reduce the surface charge of particles such as pigments and resin particles in the ink dispersed and stabilized by weakly acidic functional groups such as carboxyl groups, thereby reducing dispersion stability.
[0349] The organic acid preferably has a low pKa, high solubility in water, and a valence of 2 or more. Furthermore, the organic acid more preferably has a high buffering capacity in a pH region lower than the pKa of the functional group (eg, carboxyl group) that stabilizes particle dispersion in the ink.
[0350] -Multivalent Metal Compounds-
[0351] Examples of the polyvalent metal compound include polyvalent metal salts.
[0352] Examples of the polyvalent metal salt include organic acid polyvalent metal salts and inorganic acid polyvalent metal salts.
[0353] As the organic acid polyvalent metal salt, polyvalent metal salts of the above-mentioned organic acids (for example, formic acid, acetic acid, benzoic acid, etc.) are preferred.
[0354] As the inorganic acid polyvalent metal salt, a nitrate polyvalent metal salt, a hydrochloride polyvalent metal salt or a thiocyanate polyvalent metal salt is preferred.
[0355] Examples of polyvalent metal salts include salts of alkaline earth metals of Group 2 of the periodic table (e.g., magnesium and calcium), salts of transition metals of Group 3 of the periodic table (e.g., lanthanum), salts of metals of Group 13 of the periodic table (e.g., aluminum), and salts of lanthanides (e.g., neodymium).
[0356] As the polyvalent metal salt, a calcium salt, a magnesium salt or an aluminum salt is preferred, and a calcium salt or a magnesium salt is more preferred.
[0357] As the polyvalent metal compound, an organic acid polyvalent metal salt is preferred, and an organic acid calcium salt or an organic acid magnesium salt is more preferred.
[0358] It is preferred that at least a part of the polyvalent metal compound is dissociated into polyvalent metal ions and counter ions in the pretreatment liquid.
[0359] -Metal Complex-
[0360] The metal complex preferably contains at least one selected from the group consisting of zirconium, aluminum, and titanium as a metal element.
[0361] The metal complex is preferably a metal complex containing as a ligand at least one selected from the group consisting of acetate, acetylacetone, methyl acetoacetate, ethyl acetoacetate, octanediol, butoxyacetylacetone, lactate, lactate ammonium salt and triethanolamine.
[0362] The metal complex may be a commercially available product. Various organic ligands (especially various multidentate ligands capable of forming metal chelate catalysts) are available on the market. Therefore, the metal complex may be a metal complex prepared by combining commercially available organic ligands and metals.
[0363] -Cationic polymer-
[0364] The cationic polymer is preferably a homopolymer of a cationic monomer having a primary to tertiary amino group or a quaternary ammonium salt group, a copolymer or a polycondensate of a cationic monomer and a non-cationic monomer. The cationic polymer may be used in the form of a water-soluble polymer or a water-insoluble polymer (ie, latex particles).
[0365] Examples of the cationic polymer include polyvinyl pyridinium salts, polyalkylaminoethyl acrylates, polyalkylaminoethyl methacrylates, polyvinylimidazoles, polyethyleneimine, polybiguanide, polyguanidine, polyallylamine, and derivatives thereof.
[0366] From the viewpoint of the viscosity of the pretreatment liquid, the weight average molecular weight of the cationic polymer is preferably small. In the case of imparting the pretreatment liquid to the resin substrate by inkjet recording, it is preferably 1,000 to 500,000, more preferably 1,500 to 200,000, and further preferably 2,000 to 100,000. If the weight average molecular weight is 1000 or more, it is advantageous from the viewpoint of agglomeration speed. If the weight average molecular weight is 500,000 or less, it is advantageous from the viewpoint of ejection reliability. However, in the case of imparting the pretreatment liquid to the resin substrate by a method other than inkjet recording, it is not limited thereto.
[0367] The content of the coagulant in the pretreatment liquid is preferably 0.1 to 40% by mass, more preferably 0.1 to 30% by mass, further preferably 1 to 20% by mass, and further preferably 1 to 10% by mass, based on the total amount of the pretreatment liquid.
[0368] (Water-soluble organic solvent)
[0369] The pretreatment liquid may contain at least one water-soluble organic solvent.
[0370] Examples of the water-soluble organic solvent that may be contained in the pretreatment liquid include the same water-soluble organic solvents as those contained in the ink described later.
[0371] However, in this case, the water-soluble organic solvent in the pretreatment liquid may be the same as or different from the water-soluble organic solvent in the ink.
[0372] The content of the water-soluble organic solvent is preferably 20% by mass or less, and more preferably 10% by mass or less, based on the total amount of the pretreatment liquid.
[0373] The content of the water-soluble organic solvent may be 0% by mass. That is, the pretreatment liquid may not contain a water-soluble organic solvent.
[0374] When the pretreatment liquid contains a water-soluble organic solvent, the content of the water-soluble organic solvent is preferably 1% by mass to 20% by mass, more preferably 3% by mass to 10% by mass, based on the total amount of the pretreatment liquid.
[0375] (Resin X)
[0376] The pretreatment liquid may contain at least one resin other than the cationic polymer (hereinafter also referred to as “resin X”).
[0377] Examples of the resin X include polyester resins, polyurethane resins, acrylic resins, polyamide resins, polyurea resins, polycarbonate resins, polyolefin resins, and polystyrene resins.
[0378] As the resin X, at least one of acrylic resin, polyester resin and polyurethane resin is preferred.
[0379] In the present invention, acrylic resin refers to a polymer (homopolymer or copolymer) containing at least one raw material monomer selected from the group consisting of acrylic acid, acrylic acid derivatives (such as acrylic acid esters), methacrylic acid and methacrylic acid derivatives (such as methacrylic acid esters).
[0380] The weight average molecular weight (Mw) of the resin X is preferably 1,000 to 300,000, more preferably 2,000 to 200,000, and even more preferably 5,000 to 100,000.
[0381] In the present invention, unless otherwise specified, the weight average molecular weight (Mw) refers to a value measured by gel permeation chromatography (GPC).
[0382] For the measurement by gel permeation chromatography (GPC), HLC (registered trademark)-8020GPC (TOSOH CORPORATION) was used as a measuring apparatus, three TSKgel (registered trademark) Super Multipore HZ-H (4.6 mmID×15 cm, TOSOH CORPORATION) columns were used as columns, and THF (tetrahydrofuran) was used as an eluent. Furthermore, as measurement conditions, the sample concentration was set to 0.45% by mass, the flow rate was set to 0.35 ml / min, the sample injection volume was set to 10 μl, and the measurement temperature was set to 40° C., and the RI detector was used for the measurement.
[0383] The calibration curve was prepared using eight samples of “standard sample TSK standard, polystyrene” manufactured by TOSOH Corporation: “F-40”, “F-20”, “F-4”, “F-1”, “A-5000”, “A-2500”, “A-1000” and “n-propylbenzene”.
[0384] As the form of the resin X in the pretreatment liquid, resin particles are preferred.
[0385] That is, the pretreatment liquid preferably contains resin particles as the resin X.
[0386] In this case, the resin X is preferably a water-insoluble resin.
[0387] The volume average particle size of the resin particles as the resin X is preferably 1 nm to 300 nm, more preferably 3 nm to 200 nm, and even more preferably 5 nm to 150 nm.
[0388] In the present invention, the volume average particle size refers to a value measured using a laser diffraction / scattering particle size distribution analyzer.
[0389] As a measuring apparatus, a particle size distribution measuring apparatus "Microtrac MT-3300II" (made by Nikkiso Co., Ltd.) is mentioned, for example.
[0390] As resin particles of resin X,
[0391] Preferred are acrylic resin particles, ester resin particles, a mixture of acrylic resin particles and ester resin particles, composite particles containing an acrylic resin and an ester resin, or polyurethane resin particles.
[0392] The content of the resin X in the pretreatment liquid is not particularly limited.
[0393] The content of the resin X relative to the total amount of the pretreatment liquid is preferably 0.5% by mass to 30% by mass, more preferably 1% by mass to 20% by mass, and particularly preferably 1% by mass to 15% by mass.
[0394] (Surfactant)
[0395] The pretreatment liquid may contain at least one surfactant.
[0396] The type of surfactant is not particularly limited, and may be any of anionic surfactants, cationic surfactants, betaine-based surfactants, and nonionic surfactants. Examples of surfactants include acrylic surfactants, fluorine-based surfactants, and silicone-based surfactants.
[0397] The content of the surfactant is preferably 0.1% by mass to 5% by mass, more preferably 0.2% by mass to 1% by mass, based on the total amount of the pretreatment liquid.
[0398] (Other ingredients)
[0399] The pretreatment liquid may contain other components besides the above-mentioned ones as necessary.
[0400] Other components that may be contained in the pretreatment liquid include solid wetting agents, colloidal silica, inorganic salts, anti-fading agents, emulsion stabilizers, penetration enhancers, ultraviolet absorbers, preservatives, mildew inhibitors, pH adjusters, viscosity adjusters, rust inhibitors, chelating agents, water-soluble polymer compounds (for example, the water-soluble polymer compounds described in paragraphs 0026 to 0080 of Japanese Patent Gazette No. 2013-001854) and other well-known additives.
[0401] (physical properties)
[0402] The pH of the pretreatment liquid is preferably 2.0 to 7.0, and more preferably 2.0 to 4.0. The pH is measured at 25° C. using a pH meter, for example, a pH meter manufactured by DKK-TOA Corporation (model “HM-31”).
[0403] From the viewpoint of the coating property of the pretreatment liquid, the viscosity of the pretreatment liquid is preferably 0.5 mPa·s to 10 mPa·s, and more preferably 1 mPa·s to 5 mPa·s. The viscosity is a value measured at 25° C. using a viscometer. The viscosity is measured at 25° C. using a viscometer, for example, a TV-22 viscometer manufactured by Toki Sangyo Co., Ltd.
[0404] The surface tension of the pretreatment liquid is preferably 60 mN / m or less, more preferably 20 mN / m to 50 mN / m, and further preferably 30 mN / m to 45 mN / m. The surface tension is a value measured at a temperature of 25° C. The surface tension is measured at 25° C. using a surface tensiometer, for example, using an automatic surface tensiometer manufactured by Kyowa Interface Science Co., Ltd. (product name “CBVP-Z”) by a plate method.
[0405] Example
[0406] Hereinafter, the present invention will be described in more detail with reference to Examples, but the present invention is not limited to the following Examples unless it departs from the gist of the present invention.
[0407] [Examples 1 to 9, Comparative Examples 1 to 6]
[0408] <Preparation of pretreatment solution>
[0409] The following components were mixed to prepare a pretreatment solution.
[0410] - Composition of pretreatment solution -
[0411] Glutaric acid (coagulant)
[0412] ...6.1% by mass
[0413] Propylene glycol (PG) [other water-soluble organic solvents]
[0414] ...20% by mass
[0415] ·OLFINE F1010: (manufactured by Nissin Chemical Co., Ltd.) [Surfactant]
[0416] ...0.5% by mass
[0417] SUPERFLEX 500M (manufactured by DKS Co., Ltd.) [Aqueous dispersion of urethane resin particles]
[0418] ...7.0% by mass
[0419] ·Triisopropanolamine (pH adjuster)
[0420] ...0.2% by mass
[0421] BYK024 (manufactured by BYK-Chemie GmbH)〔Defoaming agent〕
[0422] ...0.01% by mass
[0423] Ultrapure water
[0424] ...the remainder of 100% by mass in the entire pretreatment liquid
[0425] <Synthesis of Pigment Dispersant P1>
[0426] 965 g of dipropylene glycol was added to a 5000 mL three-necked flask equipped with a stirrer and a cooling tube, and the mixture was heated to 85° C. under a nitrogen atmosphere.
[0427] Separately prepare: Solution I, prepared by dissolving 640 g of benzyl methacrylate, 340 g of methacrylic acid and 19.94 g of 2-mercaptopropionic acid in 370.28 g of dipropylene glycol; and
[0428] Solution II was obtained by dissolving 17.69 g of tert-butyl peroxy-2-ethylhexanoate (product name: "PERBUTYL 0", manufactured by NOF CORPORATION) in 221.17 g of dipropylene glycol.
[0429] Solution I was added dropwise to the three-necked flask over 4 hours, and solution II was added dropwise over 5 hours. After the addition was completed, the mixture was allowed to react for 2 hours. 1 H-NMR confirmed the disappearance of the monomer.
[0430] The obtained reaction solution was heated to 70°C, and then 248.02 g of a 50% by mass potassium hydroxide aqueous solution was added thereto, and then 107.48 g of dipropylene glycol and 75.52 g of pure water were added and stirred to obtain a 37% by mass solution of a random polymer. This random polymer was used as a pigment dispersant P1.
[0431] pass 1 The structural units constituting the obtained random polymer were confirmed by H-NMR. The weight average molecular weight (Mw) was determined by GPC. The weight average molecular weight (Mw) of the obtained pigment dispersant P1 was 8400, and the acid value was 221.7 mgKOH / g.
[0432] <Preparation of White Pigment Dispersion (A)>
[0433] Pigment dispersant P1 (150 parts by mass) was dissolved in water to prepare a polymer solution having a concentration of pigment dispersant P1 of 25% by mass.
[0434] 96 parts by mass of the polymer solution, 300 parts by mass of CI Pigment White 6 (trade name "JR-405", rutile titanium dioxide particles, manufactured by TAYCAC RPORIZATION) as a white pigment, and 270 parts by mass of water were mixed to obtain a mixed solution. A potassium hydroxide aqueous solution was added to the obtained mixed solution to adjust the pH after neutralization to 8.7.
[0435] Next, the neutralized mixed solution was dispersed for 3 hours using a bead mill (bead diameter: 0.1 mmφ, zirconia beads). Thus, a white pigment dispersant P1 was obtained in which a white pigment was dispersed in a white pigment dispersion (non-crosslinked dispersion) PD1.
[0436] Next, the obtained white pigment dispersion (non-crosslinked dispersion) PD1 was ultrafiltered using an ultrafiltration device (cross-flow ultrafilter (UF), manufactured by Sartorius) by flowing ion exchange water at a flow rate of 600 mL per minute. The liquid temperature was maintained at 25° C., and ultrafiltration was performed three times with 1 times the volume of the added liquid as one pass. Ion exchange water was added to the ultrafiltered liquid to obtain an ultrafiltered dispersion having a white pigment concentration of 45% by mass and a pigment dispersant P1 concentration of 3.6% by mass.
[0437] 1.35 parts by mass of trimethylolpropane polyglycidyl ether (product name "Denacol EX-321", manufactured by Nagase ChemteX Corporation) and 14.5 parts by mass of an aqueous solution of boric acid (boric acid concentration: 4% by mass) were added as a crosslinking agent to 136 parts by mass of the above-mentioned dispersion after ultrafiltration, and the mixture was reacted at 70° C. for 6 hours, and then cooled to 25° C. Thus, the pigment dispersant P1 in the dispersion was crosslinked to form a pigment dispersant P1a as a crosslinked polymer dispersant, and a white pigment dispersion (crosslinked dispersion) in which a white pigment was dispersed in the pigment dispersant P1a was obtained.
[0438] Deionized water was added to the obtained cross-linked dispersion so that the concentration of the pigment became 15% by mass. The cross-linked dispersion to which deionized water was added was passed through an ultrafiltration device (cross-flow ultrafilter (UF), manufactured by Sartorius) equipped with a polyethersulfone (PESU) membrane (pore size: 0.1 μm) at a flow rate of 600 mL per minute, and ultrafiltration was performed. At this time, the liquid temperature was adjusted to 25° C., and ultrafiltration was performed three times at a volume ratio of 1 times the added liquid. Next, deionized water was added so that the concentration of the white pigment became 45% by mass. Thus, a white pigment dispersion (A) was obtained.
[0439] The acid value of the pigment dispersant P1a contained in the white pigment dispersion (A) was 144 mgKOH / g, and the concentration of the pigment dispersant P1a was 3.6% by mass.
[0440] <Preparation of White Pigment Dispersion (B)>
[0441] A white pigment dispersion (B) was obtained in the same manner as in the preparation of the white pigment dispersion (A) except that the diameter of the beads in the bead mill was changed to 0.3 mmφ.
[0442] <Preparation of white ink>
[0443] Inks W1 to W6 as white inks were prepared as follows.
[0444] (Preparation of ink W1)
[0445] The white pigment dispersion (A) was filtered through a 1-inch 0.5 μm filter (5EC4888389005J) manufactured by Japan Pore Corporation, and the filtered white pigment dispersion (A) and other components shown below were mixed. The obtained mixture was filtered through the above filter (5EC4888389005J) to obtain ink W1.
[0446] - Composition of ink W1 -
[0447] White pigment dispersion (A)
[0448] ...Content of white pigment is 10.0% by mass
[0449] Propylene glycol (PG) [other water-soluble organic solvents]
[0450] ...25.0% by mass
[0451] Propylene glycol monomethyl ether (PGmME) [water-soluble organic solvent]
[0452] ...2.0% by mass
[0453] · Neocryl A-1105 (manufactured by DSM Japan KK)〔Acrylic resin particle dispersion〕
[0454] ... as a content of resin particles is 5.0% by mass
[0455] ·OLFINE E1010 (manufactured by Nissin Chemical Co., Ltd.) [Acetylene glycol surfactant]
[0456] ...1.0% by mass
[0457] BYK3450 (manufactured by BYK-Chemie GmbH)〔Silicon-based surfactant〕
[0458] ...0.1% by mass
[0459] PVPK15 (Polyvinylpyrrolidone K15)
[0460] ...0.15% by mass
[0461] ·ST-XS (Nissan Chemical Corporation) [Colloidal silica dispersion]
[0462] ...The content of colloidal silica particles is 0.05% by mass
[0463] ·water
[0464] ...the remainder of 100% by mass in the total ink
[0465] <Preparation of Ink W2>
[0466] Ink W2 was obtained in the same manner as in the preparation of ink W1 except that the white pigment dispersion (A) was changed to the white pigment dispersion (B) of the same mass.
[0467] <Preparation of Ink W3>
[0468] Ink W3 was obtained in the same manner as in the preparation of ink W1 except that the amount of BYK3450 (0.1% by mass) was changed to 1.5% by mass.
[0469] <Preparation of Ink W4>
[0470] Ink W4 was obtained in the same manner as ink W1, except that the 1-inch-length 0.5-μm filter (5EC4888389005J) manufactured by Nippon Palls Co., Ltd. used in the filtration of the white pigment dispersion and the filtration of the mixture were respectively replaced with a 1-inch-length 1.0-μm filter (5EC4888389010J) manufactured by Nippon Palls Co., Ltd.
[0471] <Preparation of Ink W5>
[0472] The amount of propylene glycol (PG) (25.0 mass %) was changed to 20.0 mass %,
[0473] The amount of propylene glycol monomethyl ether (PGmME) (2.0 mass %) was changed to 5.0 mass %,
[0474] Propylene glycol monopropyl ether (PGmPE) (water-soluble organic solvent) (2.0% by mass) was further added.
[0475] In the same manner as in the preparation of ink W4 except for this, ink W5 was obtained.
[0476] <Preparation of Ink W6>
[0477] After the preparation of ink W1 (ie, after filtering the mixture with 5EC4888389005J), the obtained ink W1 was further filtered with 5EC4888389005J, thereby obtaining ink W6.
[0478] <Preparation of base material>
[0479] As a substrate (ie, recording medium), a polyethylene terephthalate (PET) substrate "FE2001 (thickness 23 μm)" manufactured by FUTAMURA CHEMICAL CO., Ltd. was prepared.
[0480] This "FE2001 (thickness 23 μm)" is a roll body in which a PET base material having a thickness of 23 μm, a width of 580 mm, and a length of 4000 m is wound up in a roll shape.
[0481] <Preparation of Inkjet Recording Apparatus>
[0482] As an inkjet recording device, Figure 1 In the inkjet recording apparatus shown, an inkjet recording apparatus having a structure in which six inkjet heads IJ1 are arranged along the conveyance direction of the recording medium is prepared.
[0483] As the pretreatment liquid applying device P1, a gravure coater was used.
[0484] The drying method in the pre-treatment liquid drying area DP1 is set to warm air drying.
[0485] The six inkjet heads IJ1 are connected to one end of the circulation pipe C1 and one end of the circulation pipe C2, respectively. The other ends of the circulation pipe C1 and the other ends of the circulation pipe C2 are connected to ink tanks IT1 corresponding to the inks of the respective colors.
[0486] Although not shown in the figure, a degassing module for degassing ink, an ink infusion pump, a foreign matter removal filter, an ink temperature regulating heat exchanger, and an ink flow meter are arranged in order from the ink tank IT1 side in the middle of each circulation pipe C2.
[0487] Although not shown in the figure, an ink infusion pump and a foreign matter removal filter are arranged in order from the inkjet head IJ1 side in the middle of each circulation pipe C1.
[0488] As the circulation pipes C1 and C2, the circulation pipes shown in Tables 1 and 2 were used.
[0489] The circulation pipes shown in Table 1 and Table 2 are as follows.
[0490] LDPE1…Low-density polyethylene tube (“6-608-6” manufactured by Azusa Scientific Co., Ltd., inner diameter 0.6 cm)
[0491] LDPE2…Low-density polyethylene tube (“6-608-10” manufactured by Azusa Techno Co., Ltd., inner diameter 1.0 cm)
[0492] LDPE3... low-density polyethylene tube ("6-608-4" manufactured by Azusa Techno Co., Ltd., inner diameter 0.4 cm)
[0493] LDPE4... low-density polyethylene tube ("6-608-15" manufactured by Azusa Techno Co., Ltd., inner diameter 2.1 cm)
[0494] ·Tygon…Tygon tube (“Tygon2001” manufactured by Saint-Gobain KK)
[0495] PP…polypropylene tube (“5-5666-44” manufactured by AZWAN, inner diameter 0.6 cm)
[0496] The length L of the circulation pipe C2 from the ink tank to the inkjet head was adjusted to the length shown in Table 1 ("length L of the circulation pipe C2 between the tank and the head").
[0497] Hereinafter, the six inkjet heads IJ1 may be referred to as the first head, the second head, the third head, the fourth head, the fifth head, and the sixth head in order from the upstream inkjet head. Also, the six inkjet heads IJ1 may be referred to as individual heads.
[0498] Each head is set to 1200dpi / 20inch width piezoelectric full line head. Wherein, dpi is the abbreviation of dot per inch.
[0499] Each head is a line head in which nozzles are arranged in a direction perpendicular to the conveyance direction of the substrate (that is, in the width direction of the substrate).
[0500] As each of the above heads, Samba G3L (manufactured by FUJIFILM DIMATIX, Inc.) was used.
[0501] <Inkjet Recording>
[0502] The substrate was surface treated by applying corona discharge using a corona treatment device (manufactured by Kasuga Denki Co., Ltd., corona surface modification evaluation device TEC-4AX) under the conditions of a discharge gap of 1 mm, 100 W, and 4 m / min.
[0503] The surface-treated substrate, pre-treatment liquid, and white ink (ie, any one of inks W1 to W6; see Table 1 and Table 2 for details) are set in the above-mentioned image recording apparatus.
[0504] The white ink is set to be ejected from the fifth head.
[0505] The pretreatment liquid was applied to the substrate using a wire bar coater while the substrate was moved at a constant speed of 50 m / min.
[0506] The applied mass of the pretreatment liquid was set to 1.5 g / m 2 .
[0507] Here, the applied mass of the pretreatment liquid is a value obtained by dividing the mass of the applied pretreatment liquid by the area of the region to which the pretreatment liquid is applied.
[0508] At the site where the application of the pretreatment liquid was completed, the pretreatment liquid was dried by the dryer 2 seconds after the application of the pretreatment liquid to the site was completed. The pretreatment liquid was dried at 60° C. for 3 seconds.
[0509] Next, while the substrate was moved at a constant speed of 50 m / min, white ink (i.e., any one of inks W1 to W6. For details, refer to Tables 1 and 2) was ejected from the fifth head to form a solid image on the surface of the substrate to which the pretreatment liquid was applied. At this time, the ink drop amount was set to 3.4 ng, the duty ratio was set to 100%, and the ejection frequency was set to 39.37 kHz.
[0510] The white ink is ejected by operating a liquid infusion pump (not shown) provided in the middle of the circulation pipe C1 and a liquid infusion pump (not shown) provided in the middle of the circulation pipe C2. Figure 1 As shown in FIG. 1 , the white ink is circulated in the path of ink tank IT1 → circulation pipe C2 → inkjet head IJ1 → circulation pipe C1 → ink tank IT1. At this time, the ink circulation flow rate (mL / s) is adjusted to the value shown in Table 1 and Table 2, thereby adjusting the ink circulation speed Vc in the circulation pipe (specifically, the connection part with the inkjet head) to the value shown in Table 1 and Table 2.
[0511] In addition, the white ink is degassed by a degassing module (not shown) disposed in the middle of the circulation pipe C2, and then passed through a filter (not shown), and after being adjusted to 30° C. by an ink temperature regulating heat exchanger (not shown) disposed in the middle of the circulation pipe C2, it is sprayed onto the substrate.
[0512] Next, with respect to the white ink applied to the substrate, 2 seconds after the ink application is completed, infrared (IR) drying is performed using an infrared (IR) irradiation device (PLC-328 manufactured by Noritake Co., Ltd.) under the condition that the surface temperature of the ink becomes 75°C, and then, warm air drying is performed using a dryer with warm air at 80°C for 20 seconds, thereby obtaining a solid image of white ink.
[0513] Through the above, an image recorded material including a substrate and a white ink solid image provided on the substrate was obtained.
[0514] <Contact angle θ of ink with respect to the inner surface of the circulation tube>
[0515] The circulation tube C2 was cut with a cutter and stretched into a flat plate to prepare a sample for contact angle measurement.
[0516] A corresponding white ink was dropped onto a surface of the contact angle measurement sample corresponding to the inner surface of the circulation tube, and the contact angle of the ink with respect to the inner surface of the circulation tube was measured.
[0517] The contact angle was measured using a contact angle measuring device (DM-
[0518] 500), and measured by a conventional method in an environment of 25°C and 50 RH% (the ink droplet size was 2 μL, and the waiting time from droplet placement to measurement was 1000 ms).
[0519] Tables 1 and 2 show the obtained contact angle θ (°) and “1-cos θ”.
[0520] <Speed Ratio (1), Speed Ratio (2) and Speed Ratio (3)>
[0521] According to equation (1), equation (2) and equation (3), speed ratio (1), speed ratio (2) and speed ratio (3) are obtained.
[0522] Tables 1 and 2 show the results.
[0523] <Evaluation>
[0524] The inkjet recording was subjected to the following evaluation.
[0525] Tables 1 and 2 show the results.
[0526] (Color stability over long periods of time)
[0527] The inkjet recording at a speed of 50 m / min was continued for 60 minutes to obtain an image recorded object. The opacity (hiding power) of the obtained image recorded object per a length of 1000 m was measured.
[0528] The hiding power was measured using x-rite eXact Advanced manufactured by X-Rite, Inc. according to the following procedure (see https: / / www.xrite.co.jp / allproduct / qa / 99-exact / 588-pqa0111.html).
[0529] First, the image recorded material was placed on the black portion of hiding power test paper (JIS qualified product) manufactured by TP TECHNICAL LAB. CO., Ltd. in a direction in which the image in the image recorded material was in contact with the black portion, and the hiding power was measured.
[0530] Next, the image recorded material whose hiding power on the black part was measured was placed on the white part of the hiding rate test paper in a direction in which the image in the image recorded material was in contact with the white part, and the hiding power at the same position as the position where the hiding power on the black part was measured was measured.
[0531] The obtained hiding powers every 1000 m (specifically, the hiding power of a portion with a length of 1000 m from the portion where image recording starts, the hiding power of a portion with a length of 2000 m from the portion where image recording starts, and the hiding power of a portion with a length of 3000 m from the portion where image recording starts) were compared, and color stability was evaluated.
[0532] The evaluation criteria are as follows.
[0533] In the following evaluation criteria, the most excellent grade in color stability during long-term operation was A.
[0534] -Evaluation criteria for color stability during long-term measurement-
[0535] A: The standard deviation of hiding power is 0.6% or less.
[0536] B: The standard deviation of hiding power is more than 0.6% and not more than 0.9%.
[0537] C: The standard deviation of hiding power is more than 0.9% and 1.5% or less.
[0538] D: The standard deviation of hiding power is greater than 1.5%.
[0539] (Image coverage)
[0540] In the evaluation of color stability during long-term operation, the hiding power of the image was evaluated based on the hiding power at a location 1000 m away from the location where image recording was started, according to the following evaluation criteria.
[0541] In the following evaluation criteria, the most excellent level of image covering property is AA.
[0542] -Evaluation criteria for image concealment-
[0543] AA: The hiding power is 58% or more.
[0544] A: The hiding power is 57% or more and less than 58%.
[0545] B: The hiding power is 56% or more and less than 55%.
[0546] C: The hiding power is 55% or more and less than 54%.
[0547] D: The hiding power is 54% or less.
[0548] (Discharge stability during long-term operation)
[0549] The image recorded material obtained in the evaluation of color stability during long-term operation was placed on the black portion of the above-mentioned coverage test paper in a direction in which the image in the image recorded material was in contact with the above-mentioned black portion, and the presence or absence of streaks in the image caused by poor ink ejection was observed.
[0550] Specifically, the number of streaks at the start position of image recording and the number of streaks at a position 3000 m away from the start position of image recording were compared, and the ejection stability during long-term operation was evaluated according to the following evaluation criteria.
[0551] In the following evaluation criteria, the most excellent discharge stability during long-term operation was rated as A.
[0552] -Evaluation criteria for discharge stability during long-term operation-
[0553] A: The increase rate of the number of streaks in a portion 3000 m away from the portion where image recording is started relative to the number of streaks in the portion where image recording is started is 10% or less.
[0554] B: The increase rate of the number of streaks in a portion 3000 m away from the portion where image recording is started relative to the number of streaks in the portion where image recording is started is more than 10% and less than 50%.
[0555] C: The increase rate of the number of streaks in a portion 3000 m away from the portion where image recording is started relative to the number of streaks in the portion where image recording is started is more than 50% and less than or equal to 100%.
[0556] D: The increase rate of the number of streaks in a portion 3000 m away from the portion where image recording is started relative to the number of streaks in the portion where image recording is started exceeds 100%.
[0557]
[0558]
[0559] In Table 1 and Table 2, the expression "aEb" means a×10 b For example, "1.64E-04" and "1.23E+09" represent 1.64×10 -4 and 1.23×10 9 .
[0560] As shown in Tables 1 and 2, the number of large white particles Pn is 1.00×10 4 Pieces / cm 3 Above and the speed ratio (1) is 5.0×10 3 Above and 1.4×10 5 In Examples 1 to 9 below, the color stability during long-term operation and the discharge stability during long-term operation were excellent.
[0561] The results of these Examples and Comparative Examples are as follows.
[0562] When the speed ratio (1) is less than 5.0×10 3 In Comparative Examples 1, 3 and 4, the color stability during long-term operation decreased.
[0563] At speed ratio (1) exceeding 1.4×10 5 In Comparative Examples 2, 5, and 6, the discharge stability during long-term operation was reduced.
[0564] The number of large particles in white Pn is less than 1.00×10 4 Pieces / cm 3 In Comparative Example 6, the hiding power of the image also decreased.
[0565] According to the results of Examples 5 and 9, when the speed ratio (2) is 1.5×10 3 In the above case (Example 9), the color stability during long-term operation is further improved.
[0566] From the results of Examples 6 and 9, it is understood that when the speed ratio (3) is 10.0 or more (Example 9), the color stability during long-term operation is further improved.
[0567] [Examples 101 to 109, Comparative Examples 101 to 106] (without pretreatment solution)
[0568] The same operations as those in Examples 1 to 9 and Comparative Examples 1 to 6 were performed except that the application of the pretreatment liquid and drying were not performed.
[0569] As a result, in each of Examples 101 to 109 and Comparative Examples 101 to 106 (without the pretreatment liquid), the same results as those in Examples 1 to 9 and Comparative Examples 1 to 6 were obtained.
[0570] The entire contents of the invention of Japanese Patent Application No. 2022-48837 filed on March 24, 2022 are incorporated herein by reference.
[0571] All documents, patent applications, and technical standards described in this specification are incorporated herein by reference to the same extent as if each individual document, patent application, or technical standard was specifically and individually described as being incorporated by reference.
Claims
1. An inkjet recording method using an inkjet recording device, wherein the inkjet recording device comprises: An inkjet head that ejects ink; and a circulation flow path for circulating the ink so that the ink discharged from the inkjet head flows and returns to the inkjet head; The inkjet recording method includes the steps of circulating the ink in the circulation flow path and ejecting the ink from the inkjet head to apply the ink to a recording medium. The ink contains water and white pigment which is titanium dioxide particles. In the ink, the number of particles with a particle size of 0.8 μm to 5 μm in the white pigment, i.e., large white particles, is 1.00×10 4 Pieces / cm 3 above, The circulation flow path includes a circulation pipe, which is connected to the inkjet head and is used to return the ink to the inkjet head. The speed ratio (1) defined by the following formula (1) is 5.0×10 3 Above and 1.4×10 5 the following, Speed ratio (1) = Vc / (Vslp×log(Pn)) Formula (1) Vslp={(ρ-ρw)gR 2 } / (18th)expression(A) In formula (1), Vc is the circulation flow rate of the ink in the connection portion of the circulation pipe with the inkjet head in cm / s, Vslp is the sedimentation velocity of the white macroparticles defined by formula (A) in cm / s, and Pn is the number of the white macroparticles in the ink in units of cm / s. 3 is the number of units, In formula (A), ρ is 4.23, ρw is the solvent in the ink in g / cm 3 The density of the unit is g is in cm / s 2 is the unit of gravity acceleration, R is the median particle size of the white large particles in cm, η is the viscosity of the solvent in the ink at 30°C in g / cm·s.
2. The inkjet recording method according to claim 1, in, The speed ratio (2) defined by the following formula (2) is 1.5×10 3 above, Speed ratio (2) = speed ratio (1) × (1-cosθ) Formula (2) In the formula (2), θ is the contact angle of the ink with respect to the inner surface of the circulation pipe in degrees.
3. The inkjet recording method according to claim 1 or 2, in, The ink is circulated through the ink tank. The speed ratio (3) defined by the following formula (3) is 10.0 or more, Speed ratio (3) = speed ratio (1) × (1 / L) Formula (3) In the formula (3), L is the length of the circulation pipe from the ink tank to the inkjet head in cm.
Citation Information
Patent Citations
Ink set and recording apparatus
CN103289471A
Ink circulation method and system thereof
CN109130523A
Ink jet recording medium for non-aqueous pigmented ink
JP2004230759A
Inkjet recording method / device
JP2006056234A
Emulsion white ink for inkjet, ink storing container, inkjet recording device, and inkjet recording method
JP2017193695A