Heating cigarette core and preparation method and application thereof
By adopting the quick-release sustained release coupling mechanism in the heating cigarette core and using a layered structure to regulate the smoke release, the problems of inconsistent release and insufficient fragrance holding of the heated cigarette cigarette are solved, and the sensory experience of consumers is improved.
Patent Information
- Application Number
- CN202411334423.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-24
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2044-09-24
AI Technical Summary
During the heating process, the existing heating cigarette cigarette cores cause the first flue gas to be released low due to the temperature conduction hysteresis, and the flue gas will attenuate the mouth by mouth, and the fragrance level added to the flavor components is insufficient, resulting in the consumer's inability to pump the senses. good.
Using the quick release sustained release coupling mechanism, the atomizer core, fragrance-generating layer and tobacco layer are designed in the tobacco core, and the atomizer hydrogel inner core, sustained release coat layer and quick release atomization are used. The agent layer regulates the flue gas release rate and stable amount, increases the initial heated flue gas aerosol release amount and reduces the sensory impact of the flue gas port-by-port decay.
The stability and consistency of the smoke release amount is achieved, the sensory experience of consumers is improved, and the outstandingness of tobacco fragrance and the durability of the flavor is ensured.
Smart Images

Figure CN118902163A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of heated cigarettes, and in particular relates to a heated cigarette core and a preparation method and application thereof. Background Art
[0002] With the improvement of people's quality of life and the strengthening of tobacco control, new requirements for "harm reduction" have been put forward for cigarette products, and new tobacco products have emerged. As one of the important categories of new tobacco, heated cigarettes are made by heating the core raw materials at 200-400℃, so that the core raw materials are heated to distill and pyrolyze to release nicotine and flavor components to meet the needs of consumers. Because the harmful or potentially harmful components in the smoke aerosol of the core raw materials are significantly reduced when heated at low temperatures, heated cigarettes have become an area of extensive concern for domestic and foreign tobacco companies and tobacco industry scientific research workers in recent years.
[0003] However, in the existing cigarette core materials, atomizers, aroma substances and tobacco substances are generally obtained by blending and forming tobacco particles, tobacco sheets, etc. The components in tobacco particles and tobacco sheets are relatively evenly distributed, but due to the different release temperatures of the components, there is a problem of inconsistent volatilization of atomizers, aroma substances and tobacco substances when heated. Since atomizers and aroma substances are easier to release due to their low volatilization temperature, while nicotine in tobacco and the original aroma components that escape from pyrolysis require a larger temperature range, consumers' puff-by-puff sensory consistency is poor and the original tobacco aroma is not prominent.
[0004] Obviously, compared with traditional cigarettes, the lag in temperature conduction during the heating process causes the amount of smoke released in the first puff of heated cigarettes to be lower than that in the second to fifth puffs, and the smoke decays puff by puff afterwards. In addition, since flavor components are added and the level of aroma retention needs to be improved, the aroma components in the product may not be retained enough, and the "aroma" and "taste" of the smoking senses may not be rich enough.
[0005] To solve at least one of the above problems, the present invention is proposed. Summary of the invention
[0006] The present invention prepares a heated cigarette core through a quick-release and slow-release coupling mechanism, increases the initial heated smoke aerosol release through a quick-release layer, regulates the smoke release rate and the puff-by-puff stable release amount through a slow-release layer, reduces the sensory impact caused by smoke puff-by-puff attenuation, and improves the sensory experience of consumers.
[0007] The first aspect of the present application provides a heated cigarette core, the core comprising: an atomizer core, a flavoring layer wrapped around the atomizer core, and a tobacco layer wrapped around the flavoring layer; the atomizer core contains a first atomizer;
[0008] The atomizer core comprises: an atomizer hydrogel inner core, which is a hydrogel containing the first atomizer and a first cross-linked network structure material.
[0009] Preferably, the aerosol core further comprises: a sustained-release coating layer wrapped around the outer periphery of the aerosol hydrogel core; the sustained-release coating layer is a membrane material that can form pores when heated, and the heating temperature is 60 to 200 degrees Celsius.
[0010] Preferably, the aerosol material core further comprises: a rapid-release aerosol gel layer located outside the sustained-release coating layer, and the rapid-release aerosol gel layer is a hydrogel containing a second aerosol and a second cross-linked network structure material.
[0011] Preferably, the first cross-linked network structure material is cellulose nanofibers, for example, one or more of cellulose nanocrystals CNC, cellulose nanofibrils CNF, and microcrystalline cellulose MCC. The material is in the form of particles, preferably with a diameter range of 5-50nm and a length range of 50nm-20um.
[0012] Preferably, the membrane material of the sustained-release coating layer that is easy to form pores when heated is selected from one or more of ethyl cellulose and its derivatives, cationic guar gum, and polyacrylic acid series polymers, with a size of 60-100 mesh and a thermal deformation temperature of 100-300 degrees Celsius.
[0013] The sustained-release coating layer is easily plastically deformed and thinned when heated, so that the internal atomizer small molecules break through the film and are released. The sustained-release coating layer material is selected from one or more of ethyl cellulose and its derivatives, cationic guar gum, and polyacrylic acid series polymers, and the thermal deformation temperature is 100-300 degrees Celsius.
[0014] Preferably, the second skeleton material is selected from one or more of sodium carboxymethyl cellulose, hydroxypropyl cellulose, and methyl cellulose, with a diameter ranging from 5 to 50 nm and a length ranging from 400 nm to 20 um.
[0015] Of course, the first cross-linked network structure material and the second cross-linked network structure material may also be selected from other materials that can form a gel with the atomizer.
[0016] Preferably, the second atomizer is the same as the first atomizer, or the boiling point of the second atomizer is lower than that of the first atomizer.
[0017] Preferably, the aerosol hydrogel core further contains aroma substances, and / or the rapid-release aerosol gel layer further contains aroma substances.
[0018] The first atomizer and the second atomizer are independently selected from polyols, such as one or more of glycerol, propylene glycol, etc.
[0019] The second aspect of the present application provides a method for preparing the heated cigarette core according to the first aspect, which comprises the following steps:
[0020] Step 1, mixing raw materials including a first atomizer, a first cross-linked network structure material and water to form the atomizer hydrogel inner core;
[0021] Step 2, wrapping the heat-sensitive plastic deformation material on the outer layer of the atomizer hydrogel inner core to form a sustained-release coating layer;
[0022] Step 3, mixing the raw materials including the second atomizer, the second cross-linked network structure material and water to form a hydrogel and wrapping the hydrogel outside the sustained-release coating layer to form a quick-release atomizer layer, and obtaining the whole particles as the atomizer material core;
[0023] Step 4, wrapping the aroma substance on the outside of the atomizer core to form an aroma layer;
[0024] Step 5: Wrap tobacco material on the outside of the aroma layer to form a tobacco layer, and the final whole particles obtained are the heated cigarette core.
[0025] Preferably, in step 1, the raw materials including the first atomizer, the first cross-linked network structure material and water are mixed and then subjected to high-pressure homogenization treatment, and the atomizer and the first cross-linked network structure material are cross-linked to form a three-dimensional network cross-linked structure by high-speed shearing under high pressure, that is, the atomizer hydrogel core is formed;
[0026] Step 2, wrapping a membrane material that is easy to form pores when heated around the outer layer of the atomizer hydrogel inner core to form a sustained-release coating layer;
[0027] Step 3, mixing the raw materials including the second atomizer, the second cross-linked network structure material and water, and then homogenizing under high pressure, forming a hydrogel by high-speed shearing under high pressure, and wrapping the hydrogel outside the sustained-release coating layer to form a rapid-release atomizer layer, so as to obtain the whole particles as the atomizer material core;
[0028] Step 4, wrapping the aroma substance on the outside of the atomizer core to form an aroma layer;
[0029] Step 5: Wrap tobacco material on the outside of the aroma layer to form a tobacco layer, and the final whole particles obtained are the heated cigarette core.
[0030] Preferably, in step 1, the mass ratio of the first atomizer to the first cross-linked network structure material is 1 to 15. The amount of water used is 0.1% to 5% of the first cross-linked network structure material.
[0031] Preferably, in step 2, the mass ratio of the sustained-release coating layer to the aerosol hydrogel core is 0.02-0.1.
[0032] Preferably, in step 3, the mass ratio of the quick-release aerosol gel layer to the aerosol hydrogel core is 0.05-0.1. The mass ratio of the second aerosol to the second cross-linked network structure material is 1 to 30. The amount of water used is 0.1% to 5% of the second cross-linked network structure material.
[0033] Preferably, in step 4, the mass fraction of the aroma layer in the entire heated cigarette core is 10%-30%.
[0034] Preferably, in step 5, the mass fraction of the tobacco layer in the entire heated cigarette core is 10%-20%.
[0035] The wrapping method may be spraying or rolling.
[0036] Preferably, the amount of the first atomizer is greater than that of the second atomizer.
[0037] Preferably, the aroma-generating substance may include tobacco substances, tobacco coating liquids and / or extracts.
[0038] Preferably, the tobacco material is tobacco powder, and the particle size of the tobacco powder ranges from 20 mesh to 400 mesh.
[0039] Preferably, the extract includes but is not limited to one or more extracts of herbal plants such as tobacco, cocoa, and chicory.
[0040] Preferably, the particle size of the general heated cigarette core is in the range of 0.3mm-5mm. Of course, large particle size heated cigarette cores can also be made and used in a heated cigarette alone or in multiples.
[0041] The third aspect of the present application provides a use of the heated cigarette core described in the first aspect for improving the consistency of the volatilization of atomizers, aroma substances and tobacco substances in the heated cigarette core.
[0042] Preferably, the purpose of controlling the amount of smoke released from each puff of the heated cigarette is achieved by regulating the atomizer content of the atomizer core and / or the quick-release atomizer gel layer.
[0043] Compared with the prior art, the present invention has the following beneficial effects:
[0044] 1. In the cigarette core material of the present application, the atomizer, the aroma substance and the tobacco substance are arranged from the inside to the outside in order from easy to difficult volatility. In this way, since the heat is transferred from the outside to the inside when the cigarette core material is heated, the tobacco substance that is least volatile on the outside can be pyrolyzed and volatilized at the same time as the aroma substance that is less volatile and the atomizer that is most volatile, thereby improving the problem of the atomizer, the aroma substance and the tobacco substance volatilizing in unison when heated.
[0045] 2. In the preferred technical solution, the atomizer hydrogel core is a hydrogel containing the first atomizer and the first cross-linked network structure material. This can solve the problem that the shape of the liquid atomizer is difficult to fix, and ensure that the atomizer can be well retained in the atomizer core.
[0046] 3. In the preferred technical solution, in the atomizer core, the outer periphery of the atomizer hydrogel core is wrapped with a sustained-release coating layer. The sustained-release layer is used to regulate the smoke release rate and the stable amount of smoke released puff by puff, and reduce the sensory impact caused by the attenuation of smoke release puff by puff.
[0047] Inside the atomizer hydrogel core, the atomizer is embedded in the first cross-linked network structure material structure by utilizing the interpenetrating network structure of the first cross-linked network structure material itself. The surface of the first cross-linked network structure material contains a large number of hydroxyl groups, and the hydroxyl groups form a large number of hydrogen bonds and other strong intermolecular forces with the atomizer, which firmly lock the atomizer inside the first cross-linked network structure material structure. When the atomizer particles are heated, the sustained-release coating layer wrapped around the outside of the atomizer hydrogel core is deformed by heat to form a pore channel, and the hydrogen bonds between the atomizer and the first cross-linked network structure material structure inside the sustained-release coating layer absorb energy by heat and break, and are gradually released through the pores. The present application can also control the porosity of the first cross-linked network structure material and the number of heated pores of the sustained-release coating layer by adjusting the amount of the first cross-linked network structure material and the loose skeleton material to control the stable release of the atomizer, thereby achieving the stable release of the overall smoke.
[0048] 4. In the preferred technical solution, the atomizer core also includes: a quick-release atomizer layer located outside the sustained-release coating layer, and the quick-release atomizer layer is a hydrogel containing a second atomizer and a second cross-linked network structure material. The surface of the second cross-linked network structure material contains a large number of hydroxyl groups, which can form a large number of hydrogen bonds with the atomizer molecules, thereby reducing the interaction force inside the atomizer molecules, and then changing large molecular clusters into small molecular clusters, which reduces the formation of large molecular clusters in the atomizer, so that the atomizer molecules exist mainly in small molecular clusters, and the atomizer of small molecular clusters is easy to release by heat. Secondly, the quick-release atomizer gel layer can be used to increase the initial heated smoke release because it is heated first on the outside. In this way, the stable release of aerosol can be achieved by regulating the quick release and sustained release of smoke-generating agents, aroma substances and atomizers. BRIEF DESCRIPTION OF THE DRAWINGS
[0049] Figure 1 This is a schematic diagram of the cigarette structure of Example 1.
[0050] Figure 2 This is a schematic diagram of the structure of the core particles of the medium-heated cigarette in Example 1.
[0051] Figure 3This is a photo of the hydrogel formed by the first atomizing agent glycerol, the first cross-linked network structure material cellulose nanofibrils CNF and water in Example 1 by a homogenizer.
[0052] Figure 4 This is a schematic diagram of the formation of pores in the hydrogel network structure of the sustained-release aerosol gel layer of the aerosol hydrogel core particles of Example 1 when heated.
[0053] Figure 5 This is a comparison chart of the puff-by-puff smoke release of the cigarette prepared in Example 1 and the existing heated cigarettes.
[0054] Figure 6 This is a comparison chart of the smoke release per puff of the cigarettes prepared in Example 1 and the cigarettes prepared in Comparative Examples 1-3.
[0055] 1. Atomizer hydrogel inner core particles, 2. Aroma layer, 3. Tobacco layer. DETAILED DESCRIPTION
[0056] The present invention is described below in conjunction with specific examples, but the embodiments of the present invention are not limited thereto. Experimental methods without specific conditions in the examples are usually carried out according to conventional conditions and conditions described in the manual, or according to conditions recommended by the manufacturer. The general equipment, materials, reagents, etc. used can be obtained from commercial channels unless otherwise specified. The raw materials required in the following examples and comparative examples can be obtained from cigarette factories.
[0057] Example 1
[0058] A method for preparing a heated cigarette core comprises the following steps:
[0059] 1. Preparation of aerosol hydrogel core: The first aerosol glycerol, the first cross-linked network structure material cellulose nanofibrils CNF (diameter 20 nm, length 400 nm) and water are mixed in a mass ratio of 3:1:0.01, and a homogenizer is used to perform low-temperature high-pressure treatment at a pressure of 100 MPa and a temperature of 5°C to generate hydrogel as the aerosol hydrogel core particles.
[0060] 2. Wrap the sustained-release coating layer around the aerosol hydrogel core:
[0061] The material of the sustained-release coating layer is ethyl cellulose (diameter 25nm, length 600nm). The method is: 3% of the mass of the atomizer hydrogel core is wrapped with ethyl cellulose on the outer layer of the atomizer hydrogel core by a spheronizer to form atomizer hydrogel core particles wrapped with a sustained-release coating layer.
[0062] 3. Wrap the rapid-release aerosol layer around the sustained-release coating layer:
[0063] The quick-release atomizer layer is a hydrogel containing a second atomizer and a second cross-linked network structure material. Hydroxypropyl cellulose (diameter 30nm, length 800nm) is selected as the second cross-linked network structure material, and the mass of the quick-release atomizer layer accounts for 5% of the mass of the atomizer hydrogel core particles. The second atomizer glycerol, hydroxypropyl cellulose and water are mixed in a mass ratio of 10:2:0.05 using a high-speed disperser (speed of 2000r / min) to form a hydrogel, and the hydrogel is wrapped around the outside of the sustained-release coating layer using a spheronizer to form a quick-release atomizer layer, thereby obtaining the overall particles as the atomizer core;
[0064] 4. Wrap the aroma layer on the outside of the atomizer core. The specific method is: place the atomizer core in a fluidized bed, and then use a peristaltic pump to slowly introduce 15% of the tobacco extract concentrate of the entire core particle mass into the fluidized bed as the aroma concentrate to complete the coating. The fluidized bed temperature is 50°C and dried for 5 minutes.
[0065] 5. Wrap the tobacco layer outside the aroma layer. The specific method is: put the particles coated by the fluidized bed into a spheronizer covered with 200-mesh tobacco powder for tobacco powder embedding. By controlling the spheronizer speed (15r / min) and the spheronization time of 3min, the heated cigarette core particles with a particle size of 2±0.2mm are obtained by spheronization.
[0066] The heated cigarette core particles are loaded into cigarette sticks to form complete cigarette sticks.
[0067] Example 2
[0068] 1. Preparation of atomizer hydrogel core: The first atomizer propylene glycol, the first cross-linked network structure material CNC (length 20 nm) and water are mixed in a mass ratio of 5:3:0.02, and a homogenizer is used to perform low-temperature high-pressure treatment at a pressure of 100 MPa and a temperature of 5°C to generate hydrogel as the atomizer hydrogel core particles.
[0069] 2. Wrap the sustained-release coating layer around the aerosol hydrogel core:
[0070] The material of the sustained-release coating layer is cationic guar gum (80 mesh). The method is as follows: cationic guar gum, which accounts for 2% of the mass of the atomizer hydrogel core, is wrapped on the outer layer of the atomizer hydrogel core by a spheronizer to form atomizer hydrogel core particles wrapped with a sustained-release coating layer.
[0071] 3. Wrap the rapid-release aerosol layer around the sustained-release coating layer:
[0072] The quick-release atomizer layer is a hydrogel containing a second atomizer and a second cross-linked network structure material. Sodium carboxymethyl cellulose (diameter 30nm, length 800nm) is selected as the second cross-linked network structure material, and the mass of the quick-release atomizer layer accounts for 6% of the mass of the atomizer hydrogel core particles. The second atomizer glycerol, sodium carboxymethyl cellulose and water are mixed in a mass ratio of 15:5:0.03 using a high-speed disperser (speed of 2000r / min) to form a hydrogel, and the hydrogel is wrapped around the outside of the sustained-release coating layer using a spheronizer to form a quick-release atomizer layer, thereby obtaining the overall particles as the atomizer core;
[0073] 4. Wrap the aroma layer on the outside of the atomizer core. The specific method is: place the atomizer core in a fluidized bed, and then use a peristaltic pump to slowly introduce 20% of the tobacco extract concentrate of the entire core particle mass into the fluidized bed as the aroma concentrate to complete the coating. The fluidized bed temperature is 70°C and dried for 5 minutes.
[0074] 5. Wrap the tobacco layer outside the aroma layer. The specific method is: put the particles coated by the fluidized bed into a spheronizer covered with 150 mesh tobacco powder for tobacco powder embedding. By controlling the spheronizer speed (10r / min) and the spheronization time of 3min, the heated cigarette core particles with a particle size of 3±0.2mm are obtained.
[0075] The heated cigarette core particles are loaded into cigarette sticks to form complete cigarette sticks.
[0076] Example 3
[0077] 1. Preparation of atomizer hydrogel core: The first atomizer propylene glycol, the first cross-linked network structure material MCC (diameter range is 50nm, length is 5um) and water are mixed in a mass ratio of 10:6:0.06, and a homogenizer is used to perform low-temperature high-pressure treatment at a pressure of 100MPa and a temperature of 5°C to generate hydrogel as the atomizer hydrogel core particles.
[0078] 2. Wrap the sustained-release coating layer around the aerosol hydrogel core:
[0079] The material of the sustained-release coating layer is polyacrylic acid (60 mesh). The method is as follows: polyacrylic acid, which accounts for 1.5% of the mass of the atomizer hydrogel core, is wrapped on the outer layer of the atomizer hydrogel core by a spray machine to form atomizer hydrogel core particles wrapped with a sustained-release coating layer.
[0080] 3. Wrap the rapid-release aerosol layer around the sustained-release coating layer:
[0081] The quick-release atomizer layer is a hydrogel containing a second atomizer and a second cross-linked network structure material. Methylcellulose (diameter 20nm, length 600nm) is selected as the second cross-linked network structure material, and the mass of the quick-release atomizer layer accounts for 10% of the mass of the atomizer hydrogel core particles. The second atomizer glycerol, methylcellulose and water are mixed in a mass ratio of 10:3:0.01 using a high-speed disperser (speed of 2000r / min) to form a hydrogel, and the hydrogel is wrapped around the outside of the sustained-release coating layer using a spheronizer to form a quick-release atomizer layer, thereby obtaining the overall particles as the atomizer core;
[0082] 4. Wrap the aroma layer on the outside of the atomizer core. The specific method is: place the atomizer core in a fluidized bed, and then use a peristaltic pump to slowly introduce 18% of the tobacco extract concentrate of the entire core particle mass into the fluidized bed as the aroma concentrate to complete the coating. The fluidized bed temperature is 65°C and dried for 6 minutes.
[0083] 5. Wrap the tobacco layer outside the aroma layer. The specific method is: put the particles coated by the fluidized bed into a spheronizer covered with 300-mesh tobacco powder for tobacco powder embedding. By controlling the spheronizer speed (15r / min) and the spheronization time of 3min, the heated cigarette core particles with a particle size of 1.5±0.2mm are obtained by spheronization.
[0084] The heated cigarette core particles are loaded into cigarette sticks to form complete cigarette sticks.
[0085] Comparative Example 1
[0086] The only difference from Example 1 is that the aerosol hydrogel core is not subsequently wrapped with a sustained-release coating layer and a rapid-release aerosol layer, and the aerosol hydrogel core is directly used as the aerosol material core, and the aroma layer and the tobacco layer are wrapped on the outside.
[0087] The obtained heated cigarette core particles are loaded into cigarettes in the manner of Example 1 to form comparative cigarette sample 1.
[0088] Comparative Example 2
[0089] The difference from Example 1 is that only the aerosol hydrogel inner core is wrapped with a sustained-release coating layer, and no quick-release aerosol layer is wrapped. Then, the aroma layer and the tobacco layer are wrapped outside the sustained-release coating layer.
[0090] The heated cigarette core particles are loaded into cigarettes in the manner of Example 1 to form comparative cigarette sample 2.
[0091] Comparative Example 3
[0092] The difference from Example 1 is that only the quick-release aerosol layer is directly wrapped on the aerosol hydrogel inner core, and no sustained-release coating layer is wrapped. Then, the aroma layer and the tobacco layer are wrapped outside the quick-release aerosol layer.
[0093] The heated cigarette core particles are loaded into cigarettes in the manner of Example 1 to form comparative cigarette sample 3.
[0094] Suction test 1:
[0095] The cigarettes of Example 1 were subjected to a Canadian deep smoking (HCI) experiment together with the existing IQOS heated cigarettes on the market. The experimental results are shown in Figure 5 . The "existing heated cigarette" in the figure is an IQOS heated cigarette, and the "regulated self-assembly raw materials" are the cigarettes shown in Example 1. The results show that the smoke release amount and the puff-by-puff stability of the cigarettes in Example 1 are better than those of existing heated cigarettes in the early stage of heating. Puff-by-puff smoke capture found that the maximum and minimum puff values of the existing heated cigarettes on the market differed by 0.83 mg, while the maximum and minimum puff values of Example 1 only differed by 0.39 mg. The variance of the smoke release of the first 7 puffs of heated cigarettes on the market is 0.026, and the variance of the smoke release of the first 7 puffs of Example 1 is 0.00274, indicating that the puff-by-puff release of Example 1 is closely clustered around the average value, and the data distribution is more consistent, further indicating that the puff-by-puff stability of smoke release in Example 1 is better.
[0096] Suction detection 2:
[0097] The cigarettes of Example 1 and comparative cigarette samples 1-3 were subjected to a Canadian high-intensity smoking (HCI) experiment to perform heated smoking.
[0098] The results are as follows Figure 6 As shown:
[0099] Comparison between Example 1 and Comparative Example 1 shows that without adding the quick-release and sustained-release layers, the aerosol hydrogel core alone cannot ensure that the aerosol carries smoke for stable release.
[0100] Comparison between Example 1 and Comparative Example 2 shows that when only the sustained-release layer exists, the smoke release in the first two puffs is less than that in the subsequent puffs, and the sustained-release layer plays a role in stabilizing the release in the subsequent puffs.
[0101] By comparing Example 1 with Comparative Example 3, it is found that the addition of the quick-release layer helps to ensure the initial release of smoke, but since no sustained-release layer is added, the smoke release increases first and then decreases.
[0102] Based on Example 1 and Comparative Examples 1-3, it is found that only the combination of rapid release and sustained release can regulate the stable release of smoke.
Claims
1. A heated cigarette core, characterized in that: The cigarette core comprises: an atomizer core, a flavoring layer wrapped around the atomizer core, and a tobacco layer wrapped around the flavoring layer; the atomizer core contains a first atomizer; The atomizer core comprises: an atomizer hydrogel inner core, which is a hydrogel containing the first atomizer and a first cross-linked network structure material.
2. The heated cigarette core according to claim 1, characterized in that: The atomizer core also includes: a sustained-release coating layer wrapped around the outer periphery of the atomizer hydrogel inner core; the sustained-release coating layer is a membrane material that can form pores when heated, and the heating temperature is 60 to 200 degrees Celsius.
3. The heated cigarette core according to claim 2, characterized in that: The aerosol material core further comprises: a quick-release aerosol gel layer located on the periphery of the sustained-release coating layer, wherein the quick-release aerosol gel layer is a hydrogel containing a second aerosol and a second cross-linked network structure material.
4. The heated cigarette core according to claim 3, characterized in that: The first cross-linked network structure material, the membrane material that is easily heated to form pores, and the second cross-linked network structure material are independently selected from: one or more of cellulose nanofibers, sodium carboxycellulose, hydroxy cellulose, methyl cellulose and its derivatives, ethyl cellulose and its derivatives, propyl cellulose and its derivatives, cationic guar gum, and polyacrylic acid series polymers.
5. The heated cigarette core according to claim 4, characterized in that: The first cross-linked network structure material is selected from cellulose nanofibers; The membrane material that is easy to form pores when heated is selected from: one or more of ethyl cellulose and its derivatives, cationic guar gum, and polyacrylic acid series polymers; The second cross-linked network structure material is selected from: one or more of sodium carboxymethyl cellulose, hydroxypropyl cellulose, and methyl cellulose.
6. The heated cigarette core according to claim 4, characterized in that: The boiling point of the second atomizer is the same as that of the first atomizer, or the boiling point of the second atomizer is lower than that of the first atomizer.
7. The heated cigarette core according to claim 4, characterized in that: The aerosol hydrogel inner core also contains aroma substances, and / or the rapid-release aerosol gel layer also contains aroma substances.
8. A method for preparing a heated cigarette core according to claim 3, characterized in that: The steps include: Step 1, mixing raw materials including a first atomizer, a first cross-linked network structure material and water to form the atomizer hydrogel inner core; Step 2, wrapping a membrane material capable of forming pores upon heating on the outer layer of the atomizer hydrogel inner core to form a sustained-release coating layer; Step 3, mixing the raw materials including the second atomizer, the second cross-linked network structure material and water to form a hydrogel and wrapping the hydrogel outside the sustained-release coating layer to form a quick-release atomizer layer, and obtaining the whole particles as the atomizer material core; Step 4, wrapping the aroma substance on the outside of the atomizer core to form an aroma layer; Step 5: Wrap tobacco material on the outside of the aroma layer to form a tobacco layer, and the final whole particles obtained are the heated cigarette core.
9. Use of the heated cigarette core according to claims 1 to 7 for improving the consistency of the volatilization of atomizers, aroma substances and tobacco substances in the heated cigarette core.
Citation Information
Patent Citations
Cigarette perfuming slow-release gel particles and preparation method thereof
CN111759001A
Tobacco particles, low-temperature smoke generating body, preparation method and heat-not-burn appliance
CN112438423A
Heating cigarette core material and preparation method thereof
CN116391900A