Coating device and using method thereof

By setting a second gasket of stacked flow paths on the slit type extrusion coating die head, the problem of lateral consistency adjustment of coating is solved, the uniform distribution of fluid flow is achieved, and the coating quality is improved. It is suitable for a variety of applications Coating application scenarios.

CN118904646APending Publication Date: 2024-11-08KAMIKAWA PRECISION TECH (WUXI) CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411182974.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-27
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The existing slit extrusion coating die is difficult to effectively adjust the lateral consistency of the coating in scenarios such as lithium batteries and photovoltaic perovskite films, especially when the gasket is too thin, it cannot be solved by thick on both sides or thin in the middle or The problem of thick middle and thin sides leads to the coating quality not meeting the standards.

Method used

A coating device is designed to form a stacked flow channel by providing a second gasket on the coating die head so that the flow resistance of the fluid in the intermediate route and the two side routes is the same, thereby improving the lateral consistency of the coating. The bottom wall of the second gasket is provided with a specific angle and geometric shape. By adjusting the angle and number of gaskets, the dry film thickness distribution trend can be corrected.

Benefits of technology

It achieves better lateral distribution consistency of fluid flow, improves lateral consistency of coating, simplifies the die head structure design, reduces cost and processing difficulty, and solves the problem of dry film thickness distribution in ultra-thin coating scenarios. It is suitable for In various application scenarios of coating die heads.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118904646A_ABST
    Figure CN118904646A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of coating, in particular to a coating device and a using method thereof.The coating device comprises a coating die head and a first gasket, the coating die head comprises an upper die and a lower die, the first gasket is arranged between the upper die and the lower die and provided with a first runner, the coating device further comprises a second gasket, and the second gasket is arranged between the upper die and the lower die and provided with a second runner. The second gasket and the first gasket are arranged in a stacked mode, the second gasket is provided with a second flow channel, and the second flow channel and the first flow channel form a stacked flow channel, so that the flow resistance borne by fluid is the same. According to the invention, the coating transverse consistency can be simply and effectively improved at low cost.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of coating technology, and in particular to a coating device and a use method thereof. Background Art

[0002] Slit extrusion coating dies are widely used in the production of optical films, plastic films, lithium battery pole pieces, hydrogen fuel cells, and photovoltaic perovskite film products. The coating industry often uses the dry film thickness or surface density consistency COV value as an important indicator to measure the quality of coating. The dry film consistency in the coating width direction is mainly affected by the rheological properties of the coating slurry, die flow channel design, die processing, installation and commissioning. The coating quality during the commissioning and acceptance stage can directly or indirectly indicate the application capabilities of the coating die manufacturer for the extrusion coating die.

[0003] In the lithium battery coating scenario, the target value of the lateral consistency of the coating is generally COV≤±0.5%~±1%. Due to the high viscosity of the coating slurry, thick coating and fast coating speed, in order to reduce the coating pressure and achieve stable and good coating, a gasket with a thickness of about 0.5~1.5mm is often used. Most of them use an adjustable slit extrusion coating die, such as a micrometer to adjust the coating die, a closed-loop motor to adjust the coating die, a push-pull rod to adjust the coating die, a sub-screw to adjust the coating die, and a locking bolt to adjust the coating die. In most cases, a good adjustment effect can be obtained, but there are also cases where adjustment cannot be made due to mechanical structure interference and other reasons.

[0004] In the ultra-thin coating scenario where the dry film thickness of photovoltaic perovskite films is between 0.5 and 1 μm, the target value of the lateral consistency of the coating is generally COV ≤ ±2% to ±5%. Due to the low viscosity of the coating slurry, thin coating and slow coating speed, thin gaskets of 0.05 to 0.15 mm are mostly used, and most of them use slit extrusion coating dies without adjustment mechanisms. Generally, the lateral distribution trend of the dry film thickness after stable film formation is thick in the middle and thin on both sides, or thick on both sides and thin in the middle. Since the gasket is too thin, the adjustment mechanism cannot be used. Generally speaking, if the middle is thick and the two sides are thin, it can be improved by replacing thin gaskets, and if the two sides are thick and the middle is thin, it can be improved by using thick gaskets. However, when the lateral consistency of the coating exceeds ±5%, the coating consistency does not meet the standard, and continuing to thicken the gasket still cannot achieve the expected lateral consistency of the coating. The final coating quality is poor, and because it cannot be adjusted, it ultimately affects the production progress.

[0005] In the existing technical solutions, such as CN216727951U, a sub-gasket is arranged in the middle of the gasket flow channel to improve the lateral consistency of coating by limiting the flow in the middle part. This structure has the following problems: (1) The sub-gasket can only adjust the problem of thick middle and thin sides, but cannot solve the problem of thin middle and thick sides; (2) When the mother gasket is very thin, the protrusions or grooves on the sub-gasket are difficult to process. Summary of the invention

[0006] The object of the present invention is to provide a coating device and a method for using the same, so that the fluid encounters the same flow resistance when flowing through the middle route and the two side routes, thereby making the lateral distribution consistency of the fluid flow better and improving the lateral consistency of the coating.

[0007] To achieve the above object, the present invention provides the following technical solutions:

[0008] A coating device includes a coating die and a first gasket, wherein the coating die includes an upper die and a lower die, the first gasket is arranged between the upper die and the lower die, the first gasket is provided with a first flow channel, and further includes a second gasket, the second gasket is stacked with the first gasket, the second gasket is provided with a second flow channel, the second flow channel and the first flow channel form a stacked flow channel so that the flow resistance to the fluid is the same.

[0009] Furthermore, the bottom wall of the second flow channel is provided with point A, point B and point C in sequence, wherein point A and point C are respectively located at the two ends of the bottom wall, point B is located in the middle of the bottom wall, straight line AC is parallel to the long side of the die head, and point B is located on the perpendicular bisector of straight line AC; the angles of ∠BAC and ∠BCA are both θ, if point B protrudes from the front end of the line connecting point A and point C, then θ<0, if point B is recessed from the rear end of the line connecting point A and point C, then θ>0; when only the first gasket is used, if the distribution trend of some film thickness or surface density is that the middle is greater than the two sides, then θ<0 is adopted, otherwise θ>0 is adopted.

[0010] Furthermore, the value of the angle θ is determined by the following formula:

[0011] θ=[57.29578·arctan(2·COV·L c / L b )]°;

[0012] Among them, COV is the coating transverse consistency value; L b is the length of the slit flow path, which is equal to the length of the straight line AC, that is, L b =L AC ; L c is the width of the slit choke flow channel.

[0013] Furthermore, the vertical distance between point B and the die lip is L m , L m The value range of is as follows:

[0014] When θ>0, 0.5·L b tanθ≤L m ≤L c ;

[0015] When θ<0, 0≤Lm ≤L c -0.5·L b ·tanθ.

[0016] Furthermore, the bottom wall of the second flow channel coincides with the hypotenuse AB and the hypotenuse BC.

[0017] Furthermore, the bottom wall of the second flow channel is arc-shaped, and point A, point B and point C are three points on the arc.

[0018] Furthermore, points A and B and points B and C form arcs AB and BC respectively, and points ABC are not cocircular, and the bottom wall of the second flow channel coincides with arcs AB and BC.

[0019] Furthermore, the arc AB and the arc BC are symmetrically arranged, and the radius R of the arc AB and the arc BC are the same, and the radius R is determined by the following formula:

[0020] R≥0.5·L b / sin(2θ / 57.29578°).

[0021] The present invention also provides a method for using the coating device, comprising the steps of:

[0022] S1: Installing the first gasket between the upper die head and the lower die head;

[0023] S2: Detect the dry film consistency value COV in the coating width direction. If it is higher than the target value, install the second gasket between the upper die head and the lower die head and overlap the first gasket;

[0024] S3: Detect the dry film consistency value COV in the coating width direction again. If it is higher than the target value, install another second gasket between the upper die head and the lower die head and overlap with the previous second gasket;

[0025] S4: Repeat step S3 until COV is lower than the target value and perform coating operation.

[0026] Furthermore, the bottom wall of the second flow channel of the second gasket is provided with point A, point B and point C in sequence, wherein point A and point C are located at the two ends of the bottom wall respectively, point B is located in the middle of the bottom wall, and the angles of ∠BAC and ∠BCA are both θ. If point B protrudes from the front end of the line connecting point A and point C, then θ<0; if point B is recessed from the rear end of the line connecting point A and point C, then θ>0. The value of angle θ is determined by the following formula:

[0027] θ=[57.29578·arctan(2·COV·L c / L b )]°;

[0028] Among them, L bis the length of the slit flow path, which is equal to the length of the straight line AC, that is, L b =

[0029] L AC ; L c is the width of the slit choke flow channel.

[0030] Compared with the prior art, the present invention has the following beneficial effects:

[0031] 1. After the slurry enters the distribution chamber through the feed port, it flows through the stacked flow channel formed by the first gasket and the second gasket. Through the stacked flow channel formed by one or more second gaskets and the first gasket, the flow resistance encountered by the fluid when flowing through the middle route and the routes on both sides is the same, thereby making the lateral distribution consistency of the fluid flow better and improving the lateral consistency of coating.

[0032] 2. Compared with the existing adjustment method or existing design, it avoids the use of bloated adjustment mechanism, greatly simplifies the structural design of the existing coating die head, and realizes the flexible adjustment of the lateral distribution trend of the coating dry film thickness. The structure is simple and the processing difficulty is low. The cost and use threshold of the second gasket are much lower than the conventional micrometer adjustment and die deformation adjustment, while the use effect is the same, achieving cost reduction and efficiency improvement.

[0033] 3. It solves the industry pain points and difficulties in scenarios such as ultra-thin coating of lithium batteries or ultra-thin coating of perovskites, where the dry film thickness distribution is thick on both sides and thin in the middle and cannot be adjusted when using thin gaskets for coating. A second gasket is superimposed on the original first gasket, and the trend of the dry film thickness distribution being thick on both sides and thin in the middle can be corrected by changing the number, geometry and parameters of the second gasket. In ultra-thin coating scenarios where the gasket thickness is less than 0.15mm, the second gasket adjustment method proposed in the present invention can effectively solve the trend of the dry film thickness distribution being thick on both sides and thin in the middle.

[0034] 4. The method proposed in the present invention can be adapted to the slit extrusion coating dies of all coating die manufacturers, and can be applied to slit extrusion coating die application scenarios including but not limited to lithium batteries, fuel cells, photovoltaic perovskite batteries, optical films, water treatment membranes, etc. The method proposed in the present invention only needs to be based on the distribution trend of the dry film thickness coated on site, and after a simple calculation, the corresponding second gasket can be superimposed or replaced to meet the needs.

[0035] In summary, the method proposed in the present invention can improve coating consistency simply, at low cost and effectively, and provide new ideas for the coating consistency adjustment method in the slot extrusion coating die industry. BRIEF DESCRIPTION OF THE DRAWINGS

[0036] Figure 1 This is a schematic diagram of the overall structure when the second gasket proposed in an embodiment of the present invention is used in combination with a conventional slot-type extrusion coating die head;

[0037] Figure 2 for Figure 1 Schematic diagram of the cross-section structure at 1 / 2 of the die length;

[0038] Figure 3 for Figure 1 The structure diagram of the conventional gasket placed on the lower mold;

[0039] Figure 4 It is a schematic diagram of the second gasket structure when θ>0 of scheme 1 when the distribution trend of the dry film thickness or surface density on site is that the two sides are greater than the middle;

[0040] Figure 5 This is a schematic diagram of the second gasket structure when θ>0 of Scheme 2 when the distribution trend of the dry film thickness on site is that the two sides are greater than the middle;

[0041] Figure 6 This is a schematic diagram of the second gasket structure when θ<0 of Scheme 1 when the distribution trend of the dry film thickness on site is that the thickness on both sides is smaller than that in the middle;

[0042] Figure 7 Comparison of the effects before and after using the second gasket on the slot extrusion coating die head at the photovoltaic perovskite cell coating production site;

[0043] Figure 8 Comparison of the effects before and after using the second gasket on the slot extrusion coating die head at the lithium battery coating production site;

[0044] Fig. 9 This is a comparison of the effects before and after using a second gasket on the slot extrusion coating die head at the optical film coating production site.

[0045] Among them, 100 is the upper mold; 101 is the clamping hole; 200 is the lower mold; 201 is the feed port; 202 is the distribution cavity; 203 is the slit flow blocking channel; 204 is the exhaust return port; 300 is the first gasket; 400 is the second gasket; L b ——Length of the slit choke flow channel; Lc——Width of the slit choke flow channel; L m ——vertical length from point B to the die lip; θ——θ angle. DETAILED DESCRIPTION

[0046] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Therefore, the following detailed description of the embodiments of the present invention provided in the drawings is not intended to limit the scope of the claimed invention, but merely represents selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0047] Example 1

[0048] See also Figures 1 to 4 The embodiment of the present invention provides a coating device. The coating device proposed by the present invention is not limited by the application scenarios of the coating die head, and can be applied to slit extrusion coating scenarios such as lithium battery coating, optical film coating, photovoltaic perovskite battery coating, and water treatment membrane coating; it is not affected by the number of coating layers, and can be applied to single-layer coating, double-layer coating, and multi-layer coating; it is not limited by the number and cross-sectional shape of the coating die head distribution cavity 202, and the distribution cavity 202 can be a single cavity, double cavity or multi-cavity design, and the cross-section of the distribution cavity 202 is a simple or complex geometric shape such as a rectangle, square, trapezoid, triangle, rhombus, semicircle, semi-teardrop, circle, teardrop, hanger, etc. The coating device proposed by the present invention is suitable for all slit extrusion coating dies with a sandwich structure mainly composed of an upper die 100, a lower die 200, and a conventional gasket 300.

[0049] The coating device includes a coating die head and a first gasket 300. The coating die head includes an upper die 100 and a lower die 200, and the first gasket 300 is disposed between the upper die 100 and the lower die 200.

[0050] The lower mold 200 is provided with a feed inlet 201 , a distribution cavity 202 , a slit flow-blocking channel 203 and an exhaust return port 204 . After the coating slurry is injected through the feed inlet 201 , it enters the distribution cavity 202 and flows out from the slit flow-blocking channel 203 .

[0051] See also Figure 3 The first gasket 300 is provided with a first flow channel. The first flow channel is communicated with the distribution cavity 202 and the slit flow-blocking flow channel 203, so as to limit the flow of the coating slurry passing through the slit flow-blocking flow channel 203.

[0052] It can be understood that the upper mold 100, the lower mold 200 and the first gasket 300 can adopt conventional design structures commonly used in the industry.

[0053] The coating device further includes a second gasket 400. The second gasket 400 is stacked with the first gasket 300. The second gasket 400 is provided with a second flow channel, and the second flow channel and the first flow channel form a stacked flow channel. This makes the flow resistance of the fluid the same. That is, the flow resistance of the fluid when flowing through the middle route and the two side routes is the same, thereby making the lateral distribution consistency of the fluid flow better and improving the lateral consistency of the coating.

[0054] It is understood that the number of the second gaskets 400 can be set to one or more as required. Specifically, the user can add the second gasket 400 according to the distribution of the coating dry film thickness until the final coating transverse consistency value COV meets the design requirements.

[0055] In addition, in the illustrated embodiment, the first gasket 300 is closer to the lower mold 200. In other embodiments, the second gasket 400 may be closer to the lower mold 200. There is no need to distinguish the order of stacking between the multiple second gaskets 400. The geometric shapes of the multiple second gaskets 400 can be the same or different. It is only necessary to make the stacked flow channel meet the desired lateral distribution of flow resistance.

[0056] By adjusting the geometric shape and size parameters of the second gasket 400, it is possible to suppress the middle flow or the flow on both sides in the overall trend, thereby regulating the overall trend of the dry film thickness distribution on site and improving the lateral consistency of coating.

[0057] In Example 1, the geometric shape of the second gasket 400 is as follows Figure 4 As shown, the bottom of the second flow channel of the second gasket 400 is symmetrically arranged with equal lengths of hypotenuse AB and hypotenuse BC. ABC forms an isosceles triangle, and the two base angles ∠BAC and ∠BCA are both angles θ. The AC line is parallel to the long side of the die head, because the hypotenuse AB and the hypotenuse BC are of equal length, so ∠BAC = ∠BCA, that is, point B is located on the perpendicular bisector of the straight line AC.

[0058] If point B is protruding from the front end of the line connecting point A and point C (the AC line of point B is closer to the outlet of the narrower slit blocking channel 203), then θ<0. If point B is recessed from the rear end of the line connecting point A and point C (the AC line of point B is farther away from the outlet of the narrower slit blocking channel 203), then θ>0.

[0059] By controlling the positive or negative value of the angle θ, the flow in the middle or on both sides can be suppressed. That is, the positive or negative value of the angle θ is determined according to the effect of using only the first gasket 300. If the dry film thickness or surface density distribution trend on site is thick in the middle and thin on both sides, θ<0 is used, otherwise θ>0 is used.

[0060] By controlling the size of the angle θ, the degree of flow suppression can be controlled.

[0061] Specifically, the size of the angle θ is determined by the COV value of the coating lateral consistency of different coating die heads, the length of the slit flow channel L b and the width of the slit choke channel L c Depends on the coating die head slit obstruction flow channel L c The larger the value, the larger θ; the higher the lateral consistency COV value, the larger θ; the slit flow path length L b The larger it is, the smaller the angle θ is.

[0062] The value of the angle θ is determined by the following formula:

[0063] θ=[57.29578·arctan(2·COV·L c / L b )]°;

[0064] Where 57.29578 is the conversion between radians and angles, 1 radian ≈ 57.29578°; arctan is the inverse tangent function operator; COV is the lateral consistency value of the coating; L b is the length of the slit flow path, which is equal to the length of the straight line AC, that is, L b =L AC ; L c is the width of the slit choke flow channel.

[0065] The vertical distance from point B to the die lip is L m , L m The value range of is as follows:

[0066] When θ>0, 0.5·L b tanθ≤L m ≤L c ;

[0067] When θ<0, 0≤L m ≤L c -0.5·L b tanθ;

[0068] Among them, tan is the tangent function operator.

[0069] Example 2

[0070] In Example 2, the geometry of the second gasket 400 is as follows Figure 5 As shown, the shape of the bottom of the second flow channel is: a three-point arc is formed by the left end point A, the center end point B and the right end point C of the bottom of the second flow channel.

[0071] As in Example 1, Example 2 can still make angles ∠BAC and ∠BCA, and their values ​​are both θ. The value of angle θ is the same as in Example 1. That is:

[0072] If point B is protruding from the front end of the line connecting point A and point C (the AC line of point B is closer to the outlet of the narrower slit blocking channel 203), then θ<0. If point B is recessed from the rear end of the line connecting point A and point C (the AC line of point B is farther away from the outlet of the narrower slit blocking channel 203), then θ>0.

[0073] By controlling the positive or negative value of the angle θ, the flow in the middle or on both sides can be suppressed. That is, the positive or negative value of the angle θ is determined according to the effect of using only the first gasket 300. If the dry film thickness or surface density distribution trend on site is thick in the middle and thin on both sides, θ<0 is used, otherwise θ>0 is used.

[0074] By controlling the size of the angle θ, the degree of flow suppression can be controlled.

[0075] Specifically, the size of the angle θ is determined by the COV value of the coating lateral consistency of different coating die heads, the length of the slit flow channel L b and the width of the slit choke channel L c Depends on the coating die head slit obstruction flow channel L c The larger the value, the larger θ; the higher the lateral consistency COV value, the larger θ; the slit flow path length L b The larger it is, the smaller the angle θ is.

[0076] The value of the angle θ is determined by the following formula:

[0077] θ=[57.29578·arctan(2·COV·L c / L b )]°;

[0078] Where 57.29578 is the conversion between radians and angles, 1 radian ≈ 57.29578°; arctan is the inverse tangent function operator; COV is the lateral consistency value of the coating; L b is the length of the slit flow path, which is equal to the length of the straight line AC, that is, L b =L AC ; L c is the width of the slit choke flow channel.

[0079] The vertical distance from point B to the die lip is L m , L m The value range of is as follows:

[0080] When θ>0, 0.5·L b tanθ≤L m ≤L c ;

[0081] When θ<0, 0≤L m ≤L c -0.5·L b tanθ;

[0082] Among them, tan is the tangent function operator.

[0083] Example 3

[0084] The shape of the bottom of the second flow channel in Example 3 is as follows: arc AB is formed through the left end point A and the center end point B of the bottom of the second flow channel, and arc BC is formed through the center end point B and the right end point C of the bottom of the second flow channel.

[0085] Arc AB and arc BC are set symmetrically, and the radius of arc AB and arc BC is the same. The radius R is determined by the following formula:

[0086] R≥0.5·L b / sin(2θ / 57.29578°).

[0087] Among them, when R = 0.5·L b sin(2θ / 57.29578°), three points ABC are in a circle. In this case, Example 3 is equivalent to Example 2.

[0088] Similarly, in Embodiment 3, angles ∠BAC and ∠BCA can still be made, and their values ​​are both θ. The value of angle θ is the same as that of Embodiment 1.

[0089] Example 4

[0090] In Example 4, the geometry of the second gasket 400 is as follows Figure 6 As shown, Example 4 is a schematic diagram of Example 1, where θ<0.

[0091] Example 5

[0092] This embodiment provides a method for using a coating device, comprising the steps of:

[0093] S1: Installing the first gasket 300 between the upper mold 100 and the lower mold 200;

[0094] S2: Detect the dry film consistency value COV in the coating width direction. If it is higher than the target value, install the second gasket 400 between the upper mold 100 and the lower mold 200 and overlap with the first gasket 300;

[0095] S3: Detect the dry film consistency value COV in the coating width direction again. If it is higher than the target value, install another second gasket 400 between the upper mold 100 and the lower mold 200 and overlap with the previous second gasket 400;

[0096] S4: Repeat S3 until COV is lower than the target value and perform coating operation.

[0097] The structure of the second gasket 400 is as described in Embodiments 1-4, and its angle θ meets the requirements of the above embodiments.

[0098] The design of the present invention is described below with reference to some specific embodiments.

[0099] Example 6

[0100] The method of the first gasket + a single second gasket proposed in the present invention is used on the slit extrusion coating die head at the photovoltaic perovskite cell coating production site, and the second gasket design of Example 1 is adopted. Figure 7 When only the first gasket is used, the lateral distribution trend of the dry film thickness on site is severely thick on both sides and thin in the middle, and the COV is as high as ±10.87%, which does not meet the coating consistency requirement of COV less than ±2.5%; since the die head does not have any adjustment mechanism and cannot be adjusted, it is considered to use the superimposed second gasket proposed by the present invention, and the second gasket adopts the geometric shape of Example 1, L c =25,L b =600, COV = 10.87%, according to the formula θ = [57.29578·arctan(2·COV·L c / L b )]°Calculation shows that the second gasket's θ=0.52°. After superimposing the second gasket, the distribution trend of the dry film thickness on site is slightly thick in the middle and thin on both sides, and the COV reaches ±0.40%, which meets the requirements.

[0101] Example 7

[0102] The method of the first gasket + a single second gasket proposed in the present invention is used on the slit extrusion coating die head at the lithium battery negative electrode coating production site, and the second gasket design of scheme 2 is adopted. Figure 8 When only the first gasket is used, the lateral distribution trend of the dry film surface density on site is heavy on both sides and light in the middle, and the COV is as high as ±2.20%, which does not meet the coating consistency requirement of COV less than ±1.00%. The effect is still poor after the micrometer is pressed down, and the micrometer is mechanically interfered, and the pressure has reached the limit and cannot be debugged further. Consider adding a second gasket and using Example 1. At this time, L c =55,L b =1500, COV = 2.20%, according to the formula θ = [57.29578·arctan(2·COV·L c / L b )]°Calculation shows that the second gasket's θ=0.09°. After superimposing the second gasket, the density trend of the dry film surface on site changes to a slight trend of heavy in the middle and light on both sides, and the COV reaches ±0.32%, meeting the requirements.

[0103] Example 8

[0104] The method of the first gasket + a single second gasket proposed by the present invention is used on the slot extrusion coating die head at the optical film coating production site, and the second gasket design of Example 3 is adopted. Fig. 9 When only the first gasket is used, the lateral distribution trend of the dry film surface density is heavy on both sides and light in the middle, and the COV is as high as ±3.83%, which does not meet the coating consistency requirement of COV less than ±2.00%. Due to cost reasons, the slot extrusion coating die head on site is not equipped with an adjustment mechanism, so it cannot be adjusted. So we considered adding a second gasket and using Example 3. At this time, L c =30, L b =1200, COV = 2.20%, according to the formula θ = [57.29578·arctan(2·COV·L c / L b )]°Calculation shows that the second gasket's θ=0.11°. After superimposing the second gasket, the trend of the dry film thickness on site changes to slightly thicker in the middle and thinner on both sides, and the COV reaches ±0.33%, meeting the requirements.

[0105] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A coating device, comprising a coating die head and a first gasket, wherein the coating die head comprises an upper die and a lower die, the first gasket is arranged between the upper die and the lower die, and the first gasket is provided with a first flow channel, characterized in that: It also includes a second gasket, which is stacked with the first gasket. The second gasket is provided with a second flow channel, and the second flow channel and the first flow channel form a stacked flow channel so that the flow resistance of the fluid is the same.

2. The coating device according to claim 1, characterized in that: The bottom wall of the second flow channel is provided with point A, point B and point C in sequence, wherein point A and point C are respectively located at the two ends of the bottom wall, point B is located in the middle of the bottom wall, straight line AC is parallel to the long side of the die head, and point B is located on the perpendicular bisector of straight line AC; the angles of ∠BAC and ∠BCA are both θ, if point B protrudes from the front end of the line connecting point A and point C, then θ<0, if point B is recessed from the rear end of the line connecting point A and point C, then θ>0; when only the first gasket is used, if the distribution trend of some film thickness or surface density is thick in the middle and thin on both sides, then θ<0 is adopted, otherwise θ>0 is adopted.

3. The coating device according to claim 2, characterized in that: The value of the angle θ is determined by the following formula: θ=[57.29578·arctan(2·COV·L c / L b )]°; Among them, COV is the coating lateral consistency value; L b is the length of the slit flow path, which is equal to the length of the straight line AC, that is, L b =L AC ; L c is the width of the slit choke flow channel.

4. The coating device according to claim 3, characterized in that: The vertical distance from point B to the die lip is L m , L m The value range of is as follows: When θ>0, 0.5·L b tanθ≤L m ≤L c ; When θ<0, 0≤L m ≤L c -0.5·L b ·tanθ.

5. The coating device according to claim 4, characterized in that: The bottom wall of the second flow channel coincides with the hypotenuse AB and the hypotenuse BC.

6. The coating device according to claim 4, characterized in that: The bottom wall of the second flow channel is arc-shaped, and point A, point B and point C are three points on the arc.

7. The coating device according to claim 4, characterized in that: Points A and B and points B and C form arcs AB and BC respectively, and the three points ABC are not cocircular. The bottom wall of the second flow channel coincides with the arcs AB and BC.

8. The coating device according to claim 7, characterized in that: The arc AB and the arc BC are set symmetrically, and the radius R of the arc AB and the arc BC are the same. The radius R is determined by the following formula: R≥0.5·L b / sin(2θ / 57.29578°)。 9. A method for using the coating device according to claim 1, characterized in that: Includes steps: S1: Installing a first gasket between the upper die and the lower die; S2: Detect the dry film consistency value COV in the coating width direction. If it is higher than the target value, install the second gasket between the upper mold and the lower mold and overlap the first gasket; S3: Detect the dry film consistency value COV in the coating width direction again. If it is higher than the target value, install another second gasket between the upper mold and the lower mold and overlap with the previous second gasket; S4: Repeat step S3 until COV is lower than the target value and perform coating operation.

10. The method for using the coating device according to claim 9, characterized in that: The bottom wall of the second flow channel of the second gasket is provided with point A, point B and point C in sequence, wherein point A and point C are located at the two ends of the bottom wall respectively, point B is located in the middle of the bottom wall, and the angles of ∠BAC and ∠BCA are both θ. If point B protrudes from the front end of the line connecting point A and point C, then θ<0; if point B is recessed from the rear end of the line connecting point A and point C, then θ>0. The value of angle θ is determined by the following formula: θ=[57.29578·arctan(2·COV·L c / L b )]°; Among them, L b is the length of the slit flow path, which is equal to the length of the straight line AC, that is, L b =L AC ; L c is the width of the slit choke flow channel.

Citation Information

Cited By

  • Uniform flow gasket for coating electrode of lithium ion battery and coating method of uniform flow gasket

    CN122252347A