Material mixing prevention method for metal target material component management

By burning component information on metal targets, X-ray fluorescence detection is used to ensure its accuracy, the mixing problem in metal target production is solved, the accuracy of product components and the traceability of supply chain are achieved, and the inspection and migration are avoided Ticket and label errors.

CN118904751APending Publication Date: 2024-11-08KONFOONG MATERIALS INTERNATIONAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410951806.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-16
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

In the production process of metal targets, the prior art is difficult to effectively prevent mixing, resulting in inaccurate product composition, and easy to be confused or fall off in the inspection and transfer tickets or labels, resulting in immeasurable losses.

Method used

X-ray fluorescence detection is used to detect the components of the metal target to ensure that it is consistent with the ticket inspection record, and then the component information is engraved on the surface of the target to ensure the accuracy of subsequent processing and supply chain, and avoid confusion and confusion inspection and ticket inspection Label error.

Benefits of technology

Through long-lasting and non-virulent surface burning, the accuracy of target components is ensured, the potential for mixing is completely eliminated, the traceability of production and supply chain is improved, and the mixing errors during product flow is avoided. It is suitable for large-scale application.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118904751A_ABST
    Figure CN118904751A_ABST
Patent Text Reader

Abstract

The invention provides an anti-mixing method for metal target component management, which comprises the following steps of: (1) detecting components of a metal target, and comparing the components with components recorded in a checking and moving ticket; (2) if the comparison result is consistent, the component information is carved on the surface of the metal target material, and the component information of the surface of the metal target material is taken as the criterion for subsequent processing; and if the comparison results are different, isolating the metal target material, and performing problem screening. According to the anti-mixing method provided by the invention, the component information of the metal target is directly carved on the surface of the target, so that the phenomena of checking and moving ticket confusion or wrong labeling and falling in the product flowing process are avoided, the accuracy of the component of the shipment target is ensured, the hidden danger of mixing is thoroughly eliminated, and large-scale popularization and application are facilitated.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of target material manufacturing, and relates to a material mixing prevention method, in particular to a material mixing prevention method for managing the components of metal target materials. Background Art

[0002] Sputtering targets are special raw materials used to generate thin film products under the bombardment of high-speed energetic particles. There are various types of targets, including metal targets, ceramic targets, etc., which are widely used in semiconductor integrated circuits, optical discs, flat panel displays, information storage, and surface coatings of workpieces.

[0003] The preparation and processing of target materials are relatively complicated. Taking metal targets as an example, they need to go through processes such as material collection, rough processing, welding, fine processing, size detection, helium leak detection, pre-cleaning, appearance inspection, cleaning, drying and packaging. The development trend of target materials is towards high sputtering rate, grain orientation control, large size and high purity. With the advancement of technology and the continuous expansion of application fields, the market demand and technical requirements for target materials are also constantly increasing.

[0004] The production and manufacturing process of metal targets involves the precise proportioning and processing of multiple metal components. Since the metal composition of the targets is relatively complex and may be very similar in appearance, it is impossible for humans to identify and judge them, which poses a huge challenge to material management and quality control in the production process. On the target production line, even a small mixing error can lead to extremely serious consequences. Once a mixing problem occurs, all the sputtered wafers on the client will be scrapped, causing immeasurable losses.

[0005] In order to prevent mixing, technicians generally use inspection and transfer tickets or labeling methods, but it is very easy for inspection and transfer tickets to be confused or labels to be mis-affixed or fall off during product flow, and this hidden danger is difficult to completely eliminate. Therefore, it is urgent to develop an anti-mixing method for metal target material composition management to ensure the accuracy of the composition of shipped target materials and completely eliminate the hidden danger of mixing. Summary of the invention

[0006] The purpose of the present invention is to provide a method for preventing mixing of metal target material components, which directly engraves the component information of the metal target material on the surface of the target material, thereby avoiding the phenomenon of confusion of inspection and transfer tickets or wrong labeling and falling off during the product flow process, ensuring the accuracy of the composition of the shipped target material, completely eliminating the hidden danger of mixing, and facilitating large-scale promotion and application.

[0007] In order to achieve the purpose of the invention, the present invention adopts the following technical solutions:

[0008] The present invention provides a method for preventing mixing of metal target components, the method comprising the following steps:

[0009] (1) Detect the composition of the metal target and compare it with the composition recorded in the inspection and transfer ticket;

[0010] (2) If the comparison results are consistent, the composition information is engraved on the surface of the metal target, and subsequent processing is based on the composition information on the surface of the metal target; if the comparison results are different, the metal target is isolated and problem screening is performed.

[0011] The anti-mixing method provided by the present invention first performs a composition test on the metal target material, and after ensuring that the composition is consistent with the composition recorded on the inspection and transfer ticket, the composition information is directly engraved on the surface of the metal target material. This durable and non-destructive marking method helps to ensure the traceability of the target material throughout the entire production and supply chain, while avoiding the phenomenon of confusion in the inspection and transfer ticket or mis-labeling and falling off during the product flow process. Potential mixing problems are identified in the early stages of production, and measures are taken to prevent the occurrence of mixing, thereby ensuring the accuracy of the composition of the shipped target material, completely eliminating the hidden dangers of mixing, and facilitating large-scale promotion and application.

[0012] Preferably, the material of the metal target in step (1) includes a metal element or an alloy, and more preferably an alloy.

[0013] Preferably, the alloy comprises aluminum-silicon-copper alloy or tungsten-titanium alloy.

[0014] Preferably, the component detection method in step (1) comprises X-ray fluorescence detection.

[0015] The present invention uses X-ray fluorescence to detect the composition of metal targets, and can perform composition analysis without damaging the target, which is crucial for maintaining the integrity of the target. In addition, the detection method can simultaneously analyze multiple elements in the target, including major elements and trace elements, which helps to comprehensively evaluate the composition of the target.

[0016] In addition, X-ray fluorescence detection can provide rapid component analysis results, which is suitable for rapid detection and process control on the production line, helping to improve production efficiency. Compared with other precision analysis technologies, this detection method has lower operating costs and maintenance requirements, does not require the use of harmful chemical reagents or sample preparation processes, and is an environmentally friendly detection method.

[0017] Preferably, the X-ray fluorescence detection comprises the following steps:

[0018] (1.1) Establish a composition curve database of target material standards;

[0019] (1.2) Establish the criteria for determining target material composition;

[0020] (1.3) Take samples of metal targets and conduct on-machine testing. Combine the composition curve database and judgment criteria to obtain the composition test results of the metal targets.

[0021] Preferably, the target material standard sample in step (1.1) includes an aluminum-silicon-copper target or a tungsten-titanium target.

[0022] Preferably, the component detection of the target material standard sample in step (1.1) comprises: first confirming with a glow discharge mass spectrometer or an optical emission spectrometer, and then detecting with an X-ray fluorescence detector.

[0023] Preferably, the determination criteria in step (1.2) include:

[0024] When the standard value of the target material component is ≥0.1wt%, for example, it can be 0.1wt%, 0.2wt%, 0.3wt%, 0.4wt%, 0.5wt%, 0.6wt%, 0.7wt%, 0.8wt%, 0.9wt% or 1wt%, and the relative error of the measured value is ≤40%, for example, it can be 5%, 10%, 15%, 20%, 25%, 30%, 35% or 40%, which means it is judged to be qualified.

[0025] In the present invention, the relative error of the measured value is specifically the difference between the measured value of the target material component and the standard value, and the specific calculation formula is as follows:

[0026]

[0027] When the standard value of the target material component is less than 0.1wt%, for example, it can be 0.01wt%, 0.02wt%, 0.03wt%, 0.04wt%, 0.05wt%, 0.06wt%, 0.07wt%, 0.08wt% or 0.09wt%, but is not 0, the measured value is ≤0.2wt%, for example, it can be 0.02wt%, 0.04wt%, 0.06wt%, 0.08wt%, 0.1wt%, 0.12wt%, 0.14wt%, 0.16wt%, 0.18wt% or 0.2wt%, and it is judged to be qualified.

[0028] When the standard value of the target material component is 0, the measured value is ≤0.1wt%, for example, it can be 0.01wt%, 0.02wt%, 0.03wt%, 0.04wt%, 0.05wt%, 0.06wt%, 0.07wt%, 0.08wt%, 0.09wt% or 0.1wt%, which is judged to be qualified.

[0029] Preferably, the determination criteria in step (1.2) include:

[0030] When the standard values ​​of the same target component of different metal targets differ by less than 0.2wt%, for example, it can be 0.02wt%, 0.04wt%, 0.06wt%, 0.08wt%, 0.1wt%, 0.12wt%, 0.14wt%, 0.16wt%, 0.18wt% or 0.2wt%, the metal target is subjected to at least 3 X-ray fluorescence tests, for example, 3 times, 4 times, 5 times, 6 times, 7 times, 8 times or 9 times, the middle value of the test results is taken as the measured value, and the obtained measured value and the corresponding standard value are subjected to correlation analysis.

[0031] Preferably, the on-machine detection method in step (1.3) includes spot inspection, specifically: performing targeted element detection on key points or specific areas of the target material.

[0032] Preferably, before the on-machine inspection in step (1.3), ensure that the purification cloth is in a clean state and the inspection hole is not blocked.

[0033] In the present invention, the purification cloth is in a clean state to avoid the introduction of new pollutants, thereby ensuring the accuracy of the detection results; the detection hole is not blocked to ensure that the X-rays act directly on the target surface, avoiding signal attenuation or scattering caused by obstructions, thereby improving the accuracy and reliability of detection.

[0034] Preferably, the composition information in step (2) is engraved on the non-sputtering surface of the metal target, and more preferably on the edge of the metal target.

[0035] Preferably, the composition information in step (2) is the standard value of the target material composition.

[0036] Preferably, the subsequent processing in step (2) includes pre-cleaning, appearance inspection, cleaning, drying and packaging performed in sequence.

[0037] Preferably, the pre-cleaning and cleaning each independently comprise ultrasonic cleaning.

[0038] As a preferred technical solution of the present invention, the anti-mixing method comprises the following steps:

[0039] (1) Detect the composition of the metal target and compare it with the composition recorded in the inspection and transfer ticket;

[0040] The component detection method includes X-ray fluorescence detection, specifically:

[0041] (1.1) Establishing a composition curve database of target material standard samples; the target material standard samples include aluminum-silicon-copper target materials or tungsten-titanium target materials; the composition detection of the target material standard samples includes: first confirming with a glow discharge mass spectrometer or an optical emission spectrometer, and then detecting with an X-ray fluorescence detector;

[0042] (1.2) Establish a target material composition determination standard; when the target material composition standard value is ≥0.1wt%, the relative error of the measured value is ≤40%, which means it is qualified; when the target material composition standard value is <0.1wt%, but not 0, the measured value is ≤0.2wt%, which means it is qualified; when the target material composition standard value is 0, the measured value is ≤0.1wt%, which means it is qualified; when the standard value of the same target material composition of different metal targets differs by less than 0.2wt%, perform at least 3 X-ray fluorescence tests on the metal target, take the middle value of the test results as the measured value, and perform correlation analysis on the obtained measured value and the corresponding standard value;

[0043] (1.3) Sampling the metal target and conducting on-machine testing, wherein the on-machine testing includes spot inspection, ensuring that the purification cloth is in a clean state and the detection hole is not blocked before the on-machine testing, and obtaining the composition test result of the metal target in combination with the composition curve database and the judgment standard;

[0044] (2) If the comparison results are consistent, the composition information is engraved on the edge of the metal target, and the subsequent pre-cleaning, appearance inspection, cleaning, drying and packaging are all based on the composition information on the surface of the metal target; if the comparison results are different, the metal target is isolated and problem screening is performed.

[0045] The numerical range described in the present invention not only includes the point values ​​listed above, but also includes any point values ​​between the above numerical ranges that are not listed. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the range.

[0046] Compared with the prior art, the present invention has the following beneficial effects:

[0047] The anti-mixing method provided by the present invention first performs a composition test on the metal target material, and after ensuring that the composition is consistent with the composition recorded on the inspection and transfer ticket, the composition information is directly engraved on the surface of the metal target material. This durable and non-destructive marking method helps to ensure the traceability of the target material throughout the entire production and supply chain, while avoiding the phenomenon of confusion in the inspection and transfer ticket or mis-labeling and falling off during the product flow process. Potential mixing problems are identified in the early stages of production, and measures are taken to prevent the occurrence of mixing, thereby ensuring the accuracy of the composition of the shipped target material, completely eliminating the hidden dangers of mixing, and facilitating large-scale promotion and application. BRIEF DESCRIPTION OF THE DRAWINGS

[0048] Figure 1 is a correlation diagram between the standard value and the measured value in the anti-mixing method provided in Example 1;

[0049] Figure 2 It is a ±3σ range diagram of the measured value of Al-1wt%Si-0.5wt%Cu in the anti-mixing method provided in Example 1;

[0050] Figure 3 This is a ±3σ range diagram of the measured values ​​of Al-0.8wt%Si-0.3wt%Cu in the anti-mixing method provided in Example 1. DETAILED DESCRIPTION

[0051] The technical solution of the present invention is further described below by specific implementation methods. It should be understood by those skilled in the art that the embodiments are only to help understand the present invention and should not be regarded as specific limitations of the present invention.

[0052] Example 1

[0053] This embodiment provides a method for preventing mixing of metal target material components, wherein the metal target material is made of aluminum-silicon-copper alloy, and the method for preventing mixing of metal target materials comprises the following steps:

[0054] (1) Detect the composition of the metal target and compare it with the composition recorded on the inspection ticket.

[0055] The component detection method includes X-ray fluorescence detection, specifically:

[0056] (1.1) Establishing a composition curve database of target material standard samples; the materials of the target material standard samples include Al-1wt%Si-0.5wt%Cu, Al-0.8wt%Si-0.3wt%Cu and Al-0.2wt%Si-0.5wt%Cu; the composition detection of the target material standard samples includes: first confirming with a glow discharge mass spectrometer and then detecting with an X-ray fluorescence detector.

[0057] (1.2) Establish a criterion for the target material composition; when the standard value of the target material composition is ≥0.1wt%, the relative error of the measured value is ≤40%, which means it is qualified; when the standard value of the target material composition is <0.1wt%, but not 0, the measured value is ≤0.2wt%, which means it is qualified; when the standard value of the target material composition is 0, the measured value is ≤0.1wt%, which means it is qualified; when the standard values ​​of the same target material component of different metal targets differ by less than 0.2wt%, perform three X-ray fluorescence tests on the metal target, take the middle value of the test results as the measured value, and perform correlation analysis on the obtained measured value and the corresponding standard value.

[0058] Specifically, the standard values ​​of silicon components in Al-1wt%Si-0.5wt%Cu and Al-0.8wt%Si-0.3wt%Cu differ by only 0.2wt%. By performing X-ray fluorescence detection on 10 targets of Al-1wt%Si-0.5wt%Cu and Al-0.8wt%Si-0.3wt%Cu respectively, and detecting each target three times, the middle value of the detection results was taken as the measured value, and a correlation diagram between the standard value and the measured value was formed (see Figure 1 ).

[0059] ① For Al-1wt%Si-0.5wt%Cu, the ±3σ range of the measured value is about 0.8-1.0 (see Figure 2 );

[0060] ② For Al-0.8wt%Si-0.3wt%Cu, the ±3σ range of the measured value is about 0.6-0.8 (see Figure 3 ).

[0061] After the determination criteria are established, if the actual measured value of the metal target is only slightly beyond the set range and is later judged as qualified by other testing methods, the test results of 30 products can be collected, the range can be reorganized, and adjustments can be made after being signed by relevant departments such as technology, quality, production, and technical services.

[0062] (1.3) Sampling the metal target and conducting on-machine testing, wherein the on-machine testing is performed by spot inspection. Before the on-machine testing, the purification cloth is ensured to be in a clean state and the testing hole is not blocked. The composition test result of the metal target is obtained by combining the composition curve database and the judgment standard.

[0063] (2) If the comparison results are consistent, the composition information is engraved on the edge of the metal target, and the subsequent pre-cleaning, appearance inspection, cleaning, drying and packaging are based on the composition information on the surface of the metal target; if the comparison results are different, the metal target is isolated and reported to the team leader for problem screening.

[0064] Example 2

[0065] This embodiment provides a method for preventing mixing of metal target material components, wherein the metal target material is made of tungsten-titanium alloy, and the method for preventing mixing of metal target material comprises the following steps:

[0066] (1) Detect the composition of the metal target and compare it with the composition recorded on the inspection ticket.

[0067] The component detection method includes X-ray fluorescence detection, specifically:

[0068] (1.1) Establishing a composition curve database of target material standard samples; the materials of the target material standard samples include Al-3wt%Ti, Al-10wt%Ti and Al-15wt%Ti; the composition detection of the target material standard samples includes: first confirming with an optical emission spectrometer and then detecting with an X-ray fluorescence detector.

[0069] (1.2) Establish a criterion for determining the target material composition; when the standard value of the target material composition is ≥0.1wt%, the relative error of the measured value is ≤40%, which means the target material is qualified; when the standard value of the target material composition is <0.1wt%, but not 0, the measured value is ≤0.2wt%, which means the target material is qualified; when the standard value of the target material composition is 0, the measured value is ≤0.1wt%, which means the target material is qualified.

[0070] After the determination criteria are established, if the actual measured value of the metal target is only slightly beyond the set range and is later judged as qualified by other testing methods, the test results of 30 products can be collected, the range can be reorganized, and adjustments can be made after being signed by relevant departments such as technology, quality, production, and technical services.

[0071] (1.3) Sampling the metal target and conducting on-machine testing, wherein the on-machine testing is performed by spot inspection. Before the on-machine testing, the purification cloth is ensured to be in a clean state and the testing hole is not blocked. The composition test result of the metal target is obtained by combining the composition curve database and the judgment standard.

[0072] (2) If the comparison results are consistent, the composition information is engraved on the edge of the metal target, and the subsequent pre-cleaning, appearance inspection, cleaning, drying and packaging are based on the composition information on the surface of the metal target; if the comparison results are different, the metal target is isolated and reported to the team leader for problem screening.

[0073] It can be seen that the anti-mixing method provided by the present invention first performs a composition test on the metal target material, and after ensuring that it is consistent with the composition recorded on the inspection and transfer ticket, the composition information is directly engraved on the surface of the metal target material. This durable and non-destructive marking method helps to ensure the traceability of the target material throughout the entire production and supply chain, while avoiding the phenomenon of confusion in inspection and transfer tickets or mis-labeling and falling off during the product flow process. Potential mixing problems are identified in the early stages of production, and measures are taken to prevent the occurrence of mixing, thereby ensuring the accuracy of the composition of the shipped target materials, completely eliminating the hidden dangers of mixing, and facilitating large-scale promotion and application.

[0074] The applicant declares that the above is only a specific implementation mode of the present invention, but the protection scope of the present invention is not limited thereto. Those skilled in the art should understand that any changes or substitutions that can be easily thought of by those skilled in the art within the technical scope disclosed by the present invention shall fall within the protection scope and disclosure scope of the present invention.

Claims

1. A method for preventing mixing of metal target components, characterized in that: The anti-mixing method comprises the following steps: (1) Detect the composition of the metal target and compare it with the composition recorded in the inspection and transfer ticket; (2) If the comparison results are consistent, the composition information is engraved on the surface of the metal target, and subsequent processing is based on the composition information on the surface of the metal target; if the comparison results are different, the metal target is isolated and problem screening is performed.

2. The anti-mixing method according to claim 1, characterized in that: The material of the metal target in step (1) includes a metal element or an alloy, and is more preferably an alloy; Preferably, the alloy comprises aluminum-silicon-copper alloy or tungsten-titanium alloy.

3. The anti-mixing method according to claim 1 or 2, characterized in that: The method of component detection in step (1) includes X-ray fluorescence detection; Preferably, the X-ray fluorescence detection comprises the following steps: (1.1) Establish a composition curve database of target material standards; (1.2) Establish the criteria for determining target material composition; (1.3) Take samples of metal targets and conduct on-machine testing. Combine the composition curve database and judgment criteria to obtain the composition test results of the metal targets.

4. The anti-mixing method according to claim 3, characterized in that: The target material standard sample in step (1.1) includes an aluminum-silicon-copper target material or a tungsten-titanium target material; Preferably, the component detection of the target material standard sample in step (1.1) comprises: first confirming with a glow discharge mass spectrometer or an optical emission spectrometer, and then detecting with an X-ray fluorescence detector.

5. The anti-mixing method according to claim 3 or 4, characterized in that: The determination criteria in step (1.2) include: When the target material component standard value is ≥0.1wt%, and the relative error of the measured value is ≤40%, it is considered qualified; When the target material component standard value is less than 0.1wt%, but not 0, the measured value is ≤0.2wt%, which means it is qualified; When the standard value of the target material component is 0, the measured value is ≤0.1wt%, which means it is judged to be qualified.

6. The anti-mixing method according to any one of claims 3 to 5, characterized in that: The determination criteria in step (1.2) include: When the standard values ​​of the same target material component of different metal targets differ by less than 0.2wt%, the metal target is subjected to at least three X-ray fluorescence tests, the middle value of the test results is taken as the measured value, and a correlation analysis is performed on the obtained measured value and the corresponding standard value.

7. The method for preventing mixing of materials according to any one of claims 3 to 6, characterized in that: The on-machine inspection method in step (1.3) includes spot inspection; Preferably, before the on-machine inspection in step (1.3), ensure that the purification cloth is in a clean state and the inspection hole is not blocked.

8. The method for preventing mixing of materials according to any one of claims 1 to 7, characterized in that: The composition information in step (2) is engraved on the non-sputtering surface of the metal target, and more preferably on the edge of the metal target; Preferably, the composition information in step (2) is the standard value of the target material composition.

9. The method for preventing mixing of materials according to any one of claims 1 to 8, characterized in that: The subsequent processing in step (2) includes pre-cleaning, appearance inspection, cleaning, drying and packaging in sequence; Preferably, the pre-cleaning and cleaning each independently comprise ultrasonic cleaning.

10. The method for preventing mixing of materials according to any one of claims 1 to 9, characterized in that: The anti-mixing method comprises the following steps: (1) Detect the composition of the metal target and compare it with the composition recorded in the inspection and transfer ticket; The component detection method includes X-ray fluorescence detection, specifically: (1.1) Establishing a composition curve database of target material standard samples; the target material standard samples include aluminum-silicon-copper target materials or tungsten-titanium target materials; the composition detection of the target material standard samples includes: first confirming with a glow discharge mass spectrometer or an optical emission spectrometer, and then detecting with an X-ray fluorescence detector; (1.2) Establish a target material composition determination standard; when the target material composition standard value is ≥0.1wt%, the relative error of the measured value is ≤40%, which means it is qualified; when the target material composition standard value is <0.1wt%, but not 0, the measured value is ≤0.2wt%, which means it is qualified; when the target material composition standard value is 0, the measured value is ≤0.1wt%, which means it is qualified; when the standard value of the same target material composition of different metal targets differs by less than 0.2wt%, perform at least 3 X-ray fluorescence tests on the metal target, take the middle value of the test results as the measured value, and perform correlation analysis on the obtained measured value and the corresponding standard value; (1.3) Sampling the metal target and conducting on-machine testing, wherein the on-machine testing includes spot inspection, ensuring that the purification cloth is in a clean state and the detection hole is not blocked before the on-machine testing, and obtaining the composition test result of the metal target in combination with the composition curve database and the judgment standard; (2) If the comparison results are consistent, the composition information is engraved on the edge of the metal target, and the subsequent pre-cleaning, appearance inspection, cleaning, drying and packaging are all based on the composition information on the surface of the metal target; if the comparison results are different, the metal target is isolated and problem screening is performed.