Resistance rivet welding method for aluminum steel heterogeneous material insulation weak rigidity structure

By opening through holes on the aluminum plate and using rotary feed equipment to pass through the rivets for resistance welding, the problem of connecting the heterogeneous insulation of aluminum steel is solved, and the riveting welding method of high reliability and automated production is realized, which improves manufacturing Quality and efficiency.

CN118905556APending Publication Date: 2024-11-08SHANGHAI ZHIRONG IND EQUIP CO LTD

Patent Information

Application Number
CN202410795713.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-19
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The existing technology is difficult to effectively connect the heterogeneous insulating weak rigid structure of aluminum steel, especially the hollow structure of aluminum plate with insulating layer and steel roll pressing parts with electrophoretic paint layer. The traditional resistance riveting welding process is not suitable for insulating materials, and the riveting method is complicated and Not suitable for automated production.

Method used

By opening through holes on the aluminum plate, using rotary feeding equipment to contact the single-sided double-spot welding rivets through the aluminum plate and contact the steel roller presses, forming a conductive path, and riveting is realized through resistance welding equipment to ensure self-consistent current path and high Reliable connection.

Benefits of technology

It realizes high-reliability connection of aluminum steel heterogeneous insulating weak rigid structures, simplifies processes, reduces assembly difficulty, is suitable for automated production, and improves manufacturing quality and efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118905556A_ABST
    Figure CN118905556A_ABST
Patent Text Reader

Abstract

A resistance rivet welding method for an aluminum steel heterogeneous material insulation weak rigidity structure comprises the steps that a plurality of through holes are formed in the outer surface of an aluminum plate of a hollow composite structure through mechanical cold machining and / or laser, a single-face double-spot-welding rivet penetrates through an upper-layer aluminum plate to make contact with a lower-layer steel profile through rotary feeding equipment, and a conductive path is formed; and finally, rivet welding of the penetrating aluminum plate and the steel rolling part is achieved through electric resistance welding equipment. According to the invention, the self-consistent current path of the insulation structure is realized by presetting the rivet so as to realize resistance welding, the limitation that the traditional resistance rivet welding process can only be used for a non-insulation strong-rigidity metal plate structure is solved, high-reliability connection on an insulation weak-rigidity structure is realized, the process is simple, the assembly difficulty is low, the method is suitable for automatic production, and the manufacturing quality and efficiency are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a technology in the field of metal structure connection, specifically a resistance riveting welding method for an aluminum-steel heterogeneous insulating weak rigidity structure, especially an aluminum plate with an insulating layer, a steel rolled part with an electrophoretic paint layer, and a sealant in the upper and lower structural gaps. Background Art

[0002] Aluminum-steel heterogeneous insulation weak rigid structure refers to a weak rigid structure with insulation characteristics composed of aluminum and steel parts, such as aluminum plate and steel roll-pressed parts, in which the surface of the aluminum plate has an insulation layer, and the surface of the steel roll-pressed parts has an electrophoretic layer and other insulating materials, for example Figure 1 The hollow structure shown. Existing mainstream SPR, FDS, FEW, and REW processes are limited by the location of the insulation layer, material strength, or low structural rigidity, making them incapable of joining dissimilar aluminum and steel materials in hollow structures. The only current industry-used method, pull riveting, is complex, difficult to assemble, and unsuitable for automated production. Summary of the Invention

[0003] In response to the above-mentioned deficiencies in the prior art, the present invention proposes a resistance riveting welding method for an insulating weak rigid structure of aluminum-steel heterogeneous materials. By pre-setting rivets, a self-consistent current path of the insulating structure is realized to achieve resistance welding, which solves the limitation that the traditional resistance riveting welding process can only be used for non-insulating strong support sheet metal structures, and realizes highly reliable connection on the insulating weak rigid structure. The process is simple, the assembly difficulty is low, and it is suitable for automated production, thereby improving manufacturing quality and efficiency.

[0004] The present invention is achieved through the following technical solutions:

[0005] The present invention relates to a resistance riveting method for an insulating weak-rigidity structure of aluminum-steel heterogeneous materials. A plurality of through holes are formed on the outer surface of an aluminum plate of a hollow composite structure by mechanical cold working and / or laser. A single-sided double-spot welding rivet is passed through the upper aluminum plate and contacts the lower steel profile by a rotary feeding device to form a conductive path. Finally, a resistance welding device is used to achieve riveting through the aluminum plate and the steel rolled part.

[0006] The diameter of the through hole is larger than the diameter of the rivet leg by more than 1 mm, preferably larger than 1.5 mm to 3 mm.

[0007] The plurality of through holes refers to at least two through holes provided on the upper aluminum plate of the same rolled steel piece, and each rivet corresponds to one through hole.

[0008] The single-sided double-spot-welded rivet is provided with a driving structure for rotary feeding, and a smooth transition is achieved between the cylindrical rivet body and the rivet head.

[0009] The end of the nail body is provided with a sharp corner, and the end of the sharp corner is provided with a protrusion or platform for contacting and rotating with the steel plate to prevent the rivet from tilting after riveting, which will affect the quality of subsequent spot welding, and the connection and conductive function are achieved with the steel plate through the sharp corner.

[0010] The diameter of the nail body is preferably 5-6 mm, and the sharp angle is greater than 10°.

[0011] The rotary feeding preferably adopts a rotation speed of 3000-6000 rad / min and a feed speed of 0.5-1.5 mm / s.

[0012] Further preferably, when the feed depth is about 1 mm and the rivet is fixed to the lower plate, the distance between the rivet head and the upper plate is within 1.5 mm.

[0013] The resistance welding equipment uses at least two riveting points as a group to form a self-consistent conductive path through the riveting points; the electrode pressure is less than 1.5kN, the current density is not less than 8kA, and the welding time is less than or equal to 150ms. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 Flowchart of the present invention;

[0015] Figure 2 This is a schematic diagram of a rivet in Example 1;

[0016] Figure 3 and Figure 4 This is the effect diagram of Example 1;

[0017] Figure 5 This is a schematic diagram of a rivet in Example 2;

[0018] Figure 6 This is the effect evaluation diagram of Example 1;

[0019] Figure 7 This is the effect evaluation diagram of Example 2;

[0020] Figure 8 This is the finished product rendering of Example 2. DETAILED DESCRIPTION Example 1

[0021] like Figure 1 As shown, the upper plate involved in this embodiment is a 2mm6xxx aluminum alloy with an insulating layer on the back, and the lower plate is a 1.4mmQP steel with a painted layer and a galvanized layer. Industrial structural adhesive is applied between the upper and lower plates. The resistance riveting welding method of the aluminum-steel heterogeneous insulation weak rigidity structure in this embodiment specifically includes:

[0022] Step 1: Use mechanical equipment to open a through hole with a diameter of 8mm on the upper plate;

[0023] Step 2: Place the upper plate on the lower plate and apply glue between the interfaces;

[0024] Step 3: Use self-piercing friction welding equipment to place multiple rivets in the through holes and implant them into the steel plate by rotating feed to a depth of 0.5 mm. Figure 3 As shown and a conductive path is formed, the rotation speed is 6000 rad / min and the feed speed is 0.5 mm / s;

[0025] The rivet is as follows Figure 2 As shown, in this embodiment, the diameter of the nail body is 6 mm, the end of the nail body is provided with a 10° sharp angle, and the end of the sharp angle is provided with a protrusion for contacting and rotating with the steel plate for positioning and connecting.

[0026] Step 4: resistance welding is performed using two rivets as a group to form an energized circuit, using strong standard parameters: current 12ka, time 30ms, and electrode pressure 0.8kN.

[0027] like Figure 4 As shown, in the scenario where the upper plate is 2mm aluminum alloy and the lower plate is 1.5mm coated DP steel, Figure 2 After the rivets are connected to the steel plate, the joint is completed by double-point spot welding. Figure 6 As shown in the figure, from the perspective of joint formation, a good molten core is formed. After the joint shear strength test, the maximum shear force reaches more than 7kN, and the failure mode is the base material or the nail, indicating that the rivet forms an effective connection with the lower plate and has considerable strength, and there is no splashing in the appearance, which can meet the joint reliability requirements in related fields. Example 2

[0028] The upper plate in this embodiment is a 2mm6xxx aluminum alloy with an insulating layer on the back, and the lower plate is a 1.4mmQP steel with a painted and galvanized layer. Industrial structural adhesive is applied between the upper and lower plates. The resistance riveting welding method of the aluminum-steel heterogeneous insulation weak rigidity structure in this embodiment specifically includes:

[0029] Step 1: Use mechanical equipment to open a through hole with a diameter of 8mm on the upper plate;

[0030] Step 2: Remove the galvanized layer on the steel structure surface of the lower plate with mechanical equipment or mask it during the electrophoretic painting process to expose the steel substrate and conduct electricity;

[0031] Step 3: Place the upper plate on the lower plate and apply glue between the interfaces;

[0032] Step 4: Use a single-sided double-point resistance welding device with a nail feeding device to Figure 5 The rivets shown are placed in each through hole, and two rivets are used as a group to form an electric circuit for resistance welding, with a current of 11ka, a time of 20ms, and an electrode pressure of 0.6kN.

[0033] like Figure 7 As shown in the figure, after the joint shear strength test, the maximum shear force reaches more than 8kN, and the failure mode is the nail, indicating that the rivet forms an effective connection with the lower plate; Figure 8 As shown, this embodiment can perform resistance welding on box-shaped hollow parts of different materials with good appearance.

[0034] The above-mentioned specific implementation can be partially adjusted in different ways by those skilled in the art without departing from the principles and purpose of the present invention. The scope of protection of the present invention shall be based on the claims and shall not be limited by the above-mentioned specific implementation. All implementation schemes within its scope shall be subject to the constraints of the present invention.

Claims

1. A resistance riveting welding method for an aluminum-steel heterogeneous material insulation weak rigidity structure, characterized in that: A plurality of through holes are made on the outer surface of the aluminum plate of the hollow composite structure by mechanical cold working and / or laser, and a single-sided double-spot welding rivet is passed through the upper aluminum plate to contact the lower steel profile by a rotary feeding device to form a conductive path, and finally a resistance welding device is used to achieve riveting through the aluminum plate and the steel rolled part.

2. The resistance riveting welding method for the aluminum-steel heterogeneous material insulation weak rigidity structure according to claim 1 is characterized by: The diameter of the through hole is greater than the diameter of the rivet leg by more than 1 mm.

3. The resistance riveting welding method for the aluminum-steel heterogeneous material insulation weak rigidity structure according to claim 1 is characterized by: The plurality of through holes refers to at least two through holes being arranged on the upper aluminum plate of the same steel rolled piece.

4. The resistance riveting welding method for the aluminum-steel heterogeneous material insulation weak rigidity structure according to claim 1 is characterized by: The single-sided double-spot-welded rivet is provided with a driving structure for rotary feeding, and a cylindrical rivet body and a rivet head have a smooth transition.

5. The resistance riveting welding method for the aluminum-steel heterogeneous material insulation weak rigidity structure according to claim 4 is characterized in that: The end of the nail body is provided with a sharp corner.

6. The resistance riveting welding method for the aluminum-steel heterogeneous material insulation weak rigidity structure according to claim 5 is characterized by: The tip end is provided with a protrusion or platform for contacting and rotating with the steel plate to prevent the rivet from tilting after riveting, affecting the spot welding quality, and at the same time plays a role of fixing and conducting electricity.

7. The resistance riveting welding method for the aluminum-steel heterogeneous material insulation weak rigidity structure according to claim 5 is characterized by: The diameter of the nail body is 5-6 mm, and the sharp angle is more than 10°.

8. The resistance riveting welding method for the aluminum-steel heterogeneous material insulation weak rigidity structure according to claim 1 is characterized by: The rotary feeding adopts a rotation speed of 3000-6000 rad / min and a feeding speed of 0.5-1.5 mm / s.

9. The resistance riveting welding method for the aluminum-steel heterogeneous material insulation weak rigidity structure according to claim 8 is characterized by: When the feed depth is about 1 mm and the rivet is fixed to the lower plate, the distance between the rivet head and the upper plate is within 1.5 mm.

10. The resistance riveting welding method for the aluminum-steel heterogeneous material insulation weak rigidity structure according to claim 1 is characterized by: The resistance welding equipment is composed of at least two riveting points as a group, the electrode pressure is less than 1.5 kN, the current density is at least 8 kA, and the welding time is less than or equal to 150 ms.

Citation Information

Patent Citations

  • Resistance plug welding method of aluminum alloy-high-strength steel

    CN105478982A

  • Aluminum alloy and steel welding method

    CN109202247A

  • Different material joined body, structure for different material joined body and rivet for different material joined body

    JP2014000580A

  • Dissimilar material joint body

    JP2016175128A

  • Arc stud weld method for jointing different materials, joint auxiliary member, and different materials weld joint

    JP2020062668A

Cited By

  • Composite connection manufacturing method for aluminum steel dissimilar materials

    CN121373787A