Modified copper silicate hollow microsphere material, preparation and application thereof, and method for detecting volatile sulfide in breath by colorimetric method
By combining modified copper silicate hollow microsphere material and colorimetric method, the sensitivity and cost problems of detection of volatile sulfides of periodontal disease pathogenic bacteria are solved, and high sensitivity and low cost detection effect is achieved. It is suitable for Periodontal disease monitoring.
Patent Information
- Application Number
- CN202411008528.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-26
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2044-07-26
AI Technical Summary
The prior art is difficult to achieve high sensitivity detection of volatile sulfides of periodontal disease pathogenic bacteria, and traditional methods have problems such as strong subjectivity or high cost and high complexity of the instrument.
Modified copper silicate hollow microsphere material is modified by hydrothermal reaction and inert atmosphere, combined with colorimetric method to detect volatile sulfides, and high sensitivity detection is achieved using peroxidase-like activity.
High sensitivity detection of volatile sulfides is achieved, with a detection limit of 0.15μmol/L. The method is simple, low cost, easy to promote, and is suitable for periodontal disease monitoring.
Smart Images

Figure CN118908233A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of detection technology, in particular to a modified copper silicate hollow microsphere material and preparation and application thereof, and a method for detecting volatile sulfide by colorimetry. Background Art
[0002] Periodontal disease seriously endangers the health of patients and brings a huge economic burden to society. It is of great significance to develop a convenient and fast detection method to screen and monitor periodontal disease. Volatile sulfides (VSCs), such as hydrogen sulfide, produced by the metabolism of periodontal pathogens are the main gases of bad breath and are also typical biomarkers of periodontitis. By monitoring the concentration of volatile sulfides in breath, periodontal pathogens can be monitored.
[0003] At present, the detection methods of volatile sulfides include subjective odor judgment method and objective instrument test method. Among them, the odor judgment method is highly subjective and not accurate enough; although instrument test methods such as surface enhanced Raman scattering, electrochemical analysis, gas chromatography and mass spectrometry have high sensitivity, they are difficult to promote widely due to the large size of the instruments, high detection costs and the need for special training. Colorimetry is a method based on a color reaction that generates a colored product. It determines the content of the component to be tested by comparing or measuring the color depth of the colored product solution. This method is simple, convenient, and the color is visible. It is often used as a quantitative analysis method in the fields of environment, food, and biomedicine. However, achieving ultra-high sensitivity colorimetric detection is still a challenge. Summary of the invention
[0004] In view of this, the purpose of the present invention is to provide a modified copper silicate hollow microsphere material and its preparation and application, and a method for detecting volatile sulfides by colorimetry. The modified copper silicate hollow microsphere material prepared by the present invention is used for the detection of volatile sulfides, which can achieve high-sensitivity detection of volatile sulfides.
[0005] In order to achieve the above-mentioned object of the invention, the present invention provides the following technical solutions:
[0006] The present invention provides a method for preparing a modified copper silicate hollow microsphere material, comprising the following steps:
[0007] The silica microspheres, copper nitrate, ammonia water and water are mixed for hydrothermal reaction to obtain copper silicate hollow spheres;
[0008] The copper silicate hollow spheres are subjected to modification treatment in an inert atmosphere to obtain the modified copper silicate hollow microsphere material.
[0009] Preferably, the mass fraction of the ammonia water is 25-28%, and the dosage ratio of the silica microspheres, copper nitrate, ammonia water and water is 80-120 mg: 0.6-0.8 mmol: 0.8-1.2 mL: 40-60 mL.
[0010] Preferably, the temperature of the hydrothermal reaction is 130-160° C., and the time is 12-16 hours.
[0011] Preferably, the inert atmosphere is nitrogen, argon or helium; the temperature of the modification treatment is 600-800° C., and the time is 12-24 hours.
[0012] The present invention provides a modified copper silicate hollow microsphere material prepared by the preparation method described in the above technical scheme.
[0013] The present invention provides application of the modified copper silicate hollow microsphere material described in the above technical solution in the detection of volatile sulfides, wherein the volatile sulfides are hydrogen sulfide or mercaptan.
[0014] Preferably, the thiol includes one or more of methyl mercaptan, propyl mercaptan and pentyl mercaptan.
[0015] Preferably, the volatile sulphur compounds originate from breath.
[0016] The present invention provides a method for detecting volatile sulfide by colorimetry, comprising the following steps:
[0017] The modified copper silicate hollow microsphere material, acidic phosphate buffer, 3,3',5,5'-tetramethylbenzidine solution, H 2 O 2 and mixing with a test liquid containing volatile sulfide, performing a color reaction, measuring the absorbance value of the reaction system at 652 nm, substituting the absorbance value into a predetermined standard curve to obtain the concentration of the volatile sulfide in the test liquid; the modified copper silicate hollow microsphere material is the modified copper silicate hollow microsphere material described in the above technical solution.
[0018] Preferably, the concentration of the modified copper silicate hollow microsphere material in the mixed solution is 10-15 μg / mL, the concentration of 3,3',5,5'-tetramethylbenzidine is 1 mmol / L, and the concentration of H 2 O 2 The concentration of is 6.25 μmol / L, and the pH value of the mixed solution is 4.
[0019] The present invention provides a method for preparing a modified copper silicate hollow microsphere material, comprising the following steps: mixing silica microspheres, copper nitrate, ammonia water and water for hydrothermal reaction to obtain copper silicate hollow spheres; modifying the copper silicate hollow spheres in an inert atmosphere to obtain the modified copper silicate hollow microsphere material. The present invention first prepares copper silicate hollow spheres, and the copper element has Fenton-like reaction catalytic activity; then the copper silicate hollow spheres are modified in an inert atmosphere, so that the copper silicate hollow spheres significantly increase the monovalent copper content while retaining the original structure, which not only has a better catalytic rate than divalent copper, but also has an advantage in promoting the activation of monovalent copper / divalent copper redox cycle, so that the copper silicate hollow spheres have better enzyme activity. The modified copper silicate hollow microsphere material prepared by the present invention has peroxidase-like activity, and as a peroxidase mimetic, can convert hydrogen peroxide into water, and generate hydroxyl radicals (·OH) at the same time, and the generated hydroxyl radicals can cause 3,3',5,5'-tetramethylbenzidine (TMB) to undergo an oxidation reaction to generate ox-TMB, which turns the solution blue; and volatile sulfide contains thiol, which can reduce this reaction, causing the blue solution to become colorless again. Therefore, the colorimetric method based on the peroxidase-like activity of the copper silicate hollow microsphere material can achieve high-sensitivity detection of volatile sulfide.
[0020] The present invention provides a method for detecting volatile sulfides by colorimetry. The detection method provided by the present invention is sensitive, convenient, fast and low-cost. It is an easily popularizable colorimetric detection system based on peroxidase-like active micro-nano preparations, which can realize high-sensitivity instant detection of volatile sulfides and provide a breakthrough new method for monitoring volatile sulfides.
[0021] The results of the examples show that the detection method provided by the present invention has a good linear relationship in the range of 0.125 to 4 μmol / L for the detection of hydrogen sulfide, a typical volatile sulfide, and a detection limit of 0.15 μmol / L. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 A schematic diagram of the principle of detecting volatile sulfides based on the peroxidase-like active copper silicate hollow sphere colorimetric method provided by the present invention;
[0023] Figure 2Schematic diagram of the process of preparing copper silicate hollow microsphere material in Example 1 (A), SEM image of CSHSs prepared in Example 1 (B), TEM image of CSHSs prepared in Example 1 (C), elemental composition diagram of CSHSs prepared in Example 1 (D), SEM image of CSHSs-Ar prepared in Example 1 (E), TEM image of CSHSs-Ar prepared in Example 1 (F), elemental composition diagram of CSHSs-Ar prepared in Example 1 (G), Cu 2p XPS spectra of CSHSs and CSHSs-Ar prepared in Example 1 (H), FT-IR image of CSHSs and CSHSs-Ar prepared in Example 1 (I), and XRD image of CSHSs and CSHSs-Ar prepared in Example 1 (J);
[0024] Figure 3 The UV-vis spectra after mixing different concentrations of hydrogen sulfide and the detection system (A, the inset in A is the color change of the test tube solution), the relationship between the change in absorption value and the concentration of hydrogen sulfide (B), and the linear relationship between the change in absorption value and the lg value of the concentration of hydrogen sulfide (C);
[0025] Figure 4 This is a schematic diagram of the process of testing the gingival crevicular fluid sample of the oral cavity of the patient with halitosis in the embodiment;
[0026] Figure 5 The UV-vis spectra of the oral gingival crevicular fluid samples of halitosis patients and healthy persons after mixing with the test solution in the embodiment (the inset shows the color change of the test tube solution), Figure 5 The blue curve and blue-marked test tube, as well as the red curve and red-marked test tube are test samples of two patients with halitosis, and the green curve and green-marked test tube represent test samples of healthy people. DETAILED DESCRIPTION
[0027] The present invention provides a method for preparing a modified copper silicate hollow microsphere material, comprising the following steps:
[0028] The silica microspheres, copper nitrate, ammonia water and water are mixed for hydrothermal reaction to obtain copper silicate hollow spheres;
[0029] The copper silicate hollow spheres are subjected to modification treatment in an inert atmosphere to obtain the modified copper silicate hollow microsphere material.
[0030] The present invention mixes silica microspheres, copper nitrate, ammonia water and water for hydrothermal reaction to obtain hollow copper silicate spheres. The present invention has no special requirements on the source of the silica microspheres, and the silica microspheres can be prepared by commercial products or by methods well known to those skilled in the art; in the embodiment of the present invention, the silica microspheres are prepared according to the classical method. The method is to prepare silica microspheres. In the present invention, the particle size of the silica microspheres is preferably 350-450 nm.
[0031] In the present invention, the copper nitrate is preferably in the form of Cu(NO 3 ) 2 ·3H 2 O; the mass fraction of the ammonia water is preferably 25-28%. In the present invention, the amount ratio of the silica microspheres, copper nitrate, ammonia water and water is preferably 80-120 mg: 0.6-0.8 mmol: 0.8-1.2 mL: 40-60 mL, more preferably 100 mg: 0.75 mmol: 1 mL: 50 mL.
[0032] The present invention preferably disperses silicon dioxide microspheres, copper nitrate and ammonia water uniformly in water, and transfers the obtained dispersion to a stainless steel pressure cooker lined with Teflon for hydrothermal reaction.
[0033] In the present invention, the temperature of the hydrothermal reaction is preferably 130-160° C., more preferably 140-150° C., and the time is preferably 12-16 h, more preferably 12-13 h.
[0034] After the hydrothermal reaction is completed, the present invention preferably washes and dries the obtained product in sequence to obtain the copper silicate hollow spheres. In the present invention, the washing is preferably performed by rinsing with water and ethanol in sequence; and the drying is preferably vacuum freeze drying.
[0035] The present invention adopts the silicon dioxide microspheres as self-sacrificing templates and prepares copper silicate hollow spheres (CSHSs) by a hydrothermal method, and the preparation is simple.
[0036] After obtaining the hollow copper silicate spheres, the present invention modifies the hollow copper silicate spheres in an inert atmosphere to obtain the modified hollow copper silicate microsphere material. In the present invention, the inert atmosphere is preferably nitrogen, argon or helium, more preferably argon; the temperature of the modification treatment is preferably 600-800°C, more preferably 600-700°C, and the time is preferably 12-24h. The present invention preferably places the hollow copper silicate spheres in a porcelain boat and performs the modification treatment in a tube furnace. Through the modification treatment, the hollow copper silicate spheres retain the original structure while significantly increasing the monovalent copper content. The modified hollow copper silicate spheres have stronger catalytic activity, which may be because they contain abundant monovalent copper, which not only has a better catalytic rate than divalent copper, but also has an advantage in promoting the activation of the monovalent copper / divalent copper redox cycle (the reaction formula involved is Cu(II)+H 2 O 2 →Cu(I)+H + +·OOH,Cu(I)+H2 O 2 +H + →Cu(II)+H 2 O+·OH), thus making the copper silicate hollow spheres have better enzyme activity.
[0037] The present invention provides a modified copper silicate hollow microsphere material prepared by the preparation method described in the above technical solution. In the present invention, the modified copper silicate hollow microsphere material has peroxidase-like activity.
[0038] The present invention provides application of the modified copper silicate hollow microsphere material described in the above technical solution in the detection of volatile sulfides, wherein the volatile sulfides are hydrogen sulfide or mercaptan.
[0039] In the present invention, the thiol preferably includes one or more of methyl mercaptan, propyl mercaptan and pentyl mercaptan; the volatile sulfide preferably comes from breath.
[0040] The present invention provides a method for detecting volatile sulfide by colorimetry, comprising the following steps:
[0041] The modified copper silicate hollow microsphere material, acidic phosphate buffer, 3,3',5,5'-tetramethylbenzidine solution, H 2 O 2 and mixing with a test liquid containing volatile sulfide, performing a color reaction, measuring the absorbance value of the reaction system at 652 nm, substituting the absorbance value into a predetermined standard curve to obtain the concentration of the volatile sulfide in the test liquid; the modified copper silicate hollow microsphere material is the modified copper silicate hollow microsphere material described in the above technical solution.
[0042] In the present invention, the volatile sulfide in the test liquid containing volatile sulfide is the same as that in the above technical solution, which will not be repeated here; the solvent of the test liquid containing volatile sulfide is preferably water or a mixed solvent of water and an organic solvent (such as DMSO).
[0043] In the present invention, the solvent of the 3,3',5,5'-tetramethylbenzidine solution is preferably DMSO.
[0044] In the present invention, the concentration of the modified copper silicate hollow microsphere material in the mixed solution is preferably 10-15 μg / mL, the concentration of 3,3',5,5'-tetramethylbenzidine (TMB) is preferably 1 mmol / L, and the concentration of H 2 O 2 The concentration of the solution is preferably 6.25 μmol / L, the concentration of the acidic phosphate buffer is preferably 20 mmol / L, and the pH value of the mixed solution is preferably 4. In the present invention, the color development reaction is preferably performed by incubating the obtained mixed solution at room temperature for 30 minutes.
[0045] In the present invention, the predetermined standard curve uses the lg value of the sulfide concentration as the horizontal coordinate and the absorbance value as the vertical coordinate. In the present invention, the method for obtaining the predetermined standard curve is: replacing the test solution containing volatile sulfide with a sulfide solution of gradient concentration, performing a color reaction in the same manner as above, measuring the absorbance value of each reaction system at 652nm, using the concentration of sulfide as the horizontal coordinate and the absorbance value as the vertical coordinate, and obtaining the standard curve by fitting. In an embodiment of the present invention, the sulfide solution of gradient concentration makes the final concentration of sulfide in the mixed solution 0.125-20 μmol / L, the sulfide in the sulfide solution is consistent with the volatile sulfide in the test solution, and when the volatile sulfide in the test solution is hydrogen sulfide, the sulfide in the sulfide solution is preferably sodium sulfide.
[0046] In the present invention, the absorbance values are all relative absorbance values, and the calculation formula is: relative absorbance value = (A 0 -A) / A 0 , where A represents the absorbance value in response to sulfide, A 0 Indicates the absorbance value without adding sulfide.
[0047] Figure 1 The present invention is a schematic diagram of the principle of colorimetric detection of volatile sulfides. The present invention is a method for detecting volatile sulfides based on a peroxidase-like active micro-nano preparation, wherein the modified copper silicate hollow microsphere material is used as a peroxidase mimetic in H 2 O 2 Under the presence of , colorless TMB can be oxidized to form blue ox-TMB. This process can be reduced by volatile sulfides containing thiol groups, causing the blue ox-TMB to fade.
[0048] The volatile sulfide detection method based on the hollow copper silicate spheres with peroxidase-like activity of the present invention has high sensitivity, low cost, convenience, and is easy to promote. It can realize high-sensitivity instant detection of volatile sulfides, such as the detection of hydrogen sulfide in breath, and can reduce the burden of complex oral examinations, reduce analysis time and cost, and can meet the detection needs of areas with poor medical standards, underdeveloped economies, and limited resources.
[0049] In order to further illustrate the present invention, the modified copper silicate hollow microspheres provided by the present invention, the preparation method and application thereof, and the method for detecting volatile sulfides by colorimetry are described in detail below with reference to examples, but they should not be construed as limiting the scope of protection of the present invention.
[0050] Example 1
[0051] Preparation of modified copper silicate hollow microsphere material (argon-modified copper silicate hollow sphere, denoted as CSHSs-Ar):
[0052] (1) According to the classic Methods Preparation of silica spheres: Tetraethyl orthosilicate (TEOS, 5 mL), ammonia (10 mL, 25 wt%), ethanol (65 mL) and water (25 mL) were mixed under stirring and dried to prepare silica microspheres with a particle size of 350-450 nm.
[0053] (2) The silica microspheres (100 mg) prepared in step (1), Cu(NO 3 ) 2 ·3H 2 O (0.75 mmol) and ammonia (1 mL, 25 wt%) were uniformly dispersed in 50 mL of water, transferred to a Teflon-lined stainless steel autoclave, and heated at 140 °C overnight; after the obtained product was cooled to room temperature, it was washed with water and ethanol in turn, and vacuum freeze-dried to obtain copper silicate hollow spheres (CSHSs);
[0054] (3) The copper silicate hollow spheres (CSHSs) prepared in step (2) were treated with argon at 600° C. in a pure argon atmosphere overnight to obtain argon-modified copper silicate hollow spheres (CSHSs-Ar), which were stored in a vacuum for further use.
[0055] Figure 2 A is a schematic diagram of the process of preparing copper silicate hollow microsphere material in Example 1.
[0056] Figure 2 B and C are SEM and TEM of CSHSs prepared in Example 1. It can be seen that CSHSs have a hollow sea urchin-like morphology.
[0057] Figure 2 D is the elemental composition of CSHSs prepared in Example 1. It can be seen that CSHSs contains Cu, Si, and O elements, which are evenly distributed.
[0058] Figure 2 E and F are SEM and TEM of CSHSs-Ar prepared in Example 1. It can be seen that CSHSs-Ar has a hollow sea urchin-like morphology.
[0059] Figure 2 G is the elemental composition of CSHSs-Ar prepared in Example 1. It can be seen that CSHSs-Ar contains Cu, Si, and O elements, which are evenly distributed.
[0060] Figure 2H is the Cu 2p XPS spectra of CSHSs and CSHSs-Ar prepared in Example 1. There are 4 fitting peaks at 932.9, 935.8, 952.7 and 955.6eV, which belong to Cu(I)2p3 / 2, Cu(II)2p3 / 2, Cu(I)2p1 / 2 and Cu(II)2p1 / 2, respectively, and the remaining peaks are satellite peaks (Sat.) of Cu(II). It is suggested that Cu(I) exists in CSHSs-Ar, but Cu(I) does not exist in CSHSs. The above results show that in the typical CSHSs-Ar synthesis process, electrons are transferred from Si atoms to Cu atoms, and a reduction reaction from Cu(II) to Cu(I) occurs.
[0061] Figure 2 I is the FT-IR of CSHSs and CSHSs-Ar prepared in Example 1. It can be seen that the two samples have similar functional groups. -1 The nearby peaks can be caused by the symmetric stretching vibration and asymmetric stretching vibration of Si-O.
[0062] Figure 2 J in Figure 1 is the XRD of CSHSs and CSHSs-Ar prepared in Example 1. The XRD pattern of CSHSs matches well with the standard peak of copper silicate (JCPDS No.03-0219), indicating the successful synthesis of copper silicate materials. Unlike CSHSs, CSHSs-Ar has other diffraction peaks at 29.58°, 36.44°, 42.33° and 61.41°, which can be attributed to Cu 2 The (110), (111), (200) and (220) crystal planes of O (JCPDS No. 78-2076).
[0063] Application Examples
[0064] Experiments have demonstrated the effectiveness of the peroxidase-like active copper silicate hollow sphere detection system in detecting hydrogen sulfide, a typical volatile sulfide.
[0065] Preparation of detection solution: The detection solution is a 3 mL system, including TMB (final concentration of 1 mmol / L, TMB is added in the form of TMB DMSO solution), CSHSs-Ar (final concentration of 15 μg / mL), H 2 O 2 (final concentration: 6.25 μmol / L), PBS with a pH value of 4 (final concentration: 20 mmol / L).
[0066] Standard curve drawing: the above detection solution was mixed with different final concentrations (0.125-20 μmol / L) of Na 2 S solution (providing H 2S) and placed at room temperature for 30 min, and the absorbance at 500-800 nm was measured using a UV-Vis spectrometer. Figure 3 As shown in A, with H 2 With the addition of S, the absorbance of oxTMB at 652 nm gradually decreased, and the color changed from blue to colorless, indicating that oxTMB was reduced to colorless TMB. 2 S concentration and relative absorbance value ((A 0 -A) / A 0 ), where A represents the linear relationship between 2 The absorbance value when S responds, A 0 Indicates no H 2 The absorbance value of S. The results are as follows Figure 3 As shown in B and C (the base of Log in C is 10). Analysis shows that H 2 The linear relationship of S concentration response in the range of 0.125 to 4 μmol / L is y=0.18839+0.09152x (x is H 2 The lg value of S concentration, y is the relative absorbance value, R 2 =0.979), good linear relationship, detection limit (LOD) was 0.15 μmol / L (3σ / slope, where σ is the linear slope and Slope is the standard deviation).
[0067] Detection of hydrogen sulfide to be tested: Mix the solution to be tested with the above-mentioned detection solution, place at room temperature for 30 minutes, measure the absorbance at 652nm with a UV-Vis spectrometer, and substitute the corresponding value into the above-mentioned concentration response linear equation to obtain the concentration of hydrogen sulfide to be tested.
[0068] Gingival crevicular fluid samples from two patients with halitosis were taken (representing breath samples containing hydrogen sulfide) and tested according to the above test method, and gingival crevicular fluid samples from healthy people without halitosis were used as comparison. Figure 4 Schematic diagram of the detection process. Figure 5 The UV-vis spectra of the gingival crevicular fluid samples of halitosis patients and healthy people after mixing with the above test solution (the inset shows the color change of the test tube solution). Figure 5 The blue curve and blue-marked test tube, as well as the red curve and red-marked test tube are test samples of two patients with halitosis, and the green curve and green-marked test tube represent test samples of healthy people. Figure 5 It can be seen that the detection system solution of patients with halitosis faded significantly, while the detection system solution of healthy people without halitosis still maintained blue.
[0069] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention, and these improvements and modifications should also be regarded as the protection scope of the present invention.
Claims
1. A method for preparing a modified copper silicate hollow microsphere material, characterized in that: The following steps are involved: The silica microspheres, copper nitrate, ammonia water and water are mixed for hydrothermal reaction to obtain copper silicate hollow spheres; The copper silicate hollow spheres are subjected to modification treatment in an inert atmosphere to obtain the modified copper silicate hollow microsphere material.
2. The preparation method according to claim 1, characterized in that: The mass fraction of the ammonia water is 25-28%, and the dosage ratio of the silica microspheres, copper nitrate, ammonia water and water is 80-120 mg: 0.6-0.8 mmol: 0.8-1.2 mL: 40-60 mL.
3. The preparation method according to claim 1 or 2, characterized in that: The temperature of the hydrothermal reaction is 130-160° C. and the time is 12-16 hours.
4. The preparation method according to claim 1, characterized in that: The inert atmosphere is nitrogen, argon or helium; the temperature of the modification treatment is 600-800° C., and the time is 12-24 hours.
5. The modified copper silicate hollow microsphere material prepared by the preparation method according to any one of claims 1 to 4.
6. Use of the modified copper silicate hollow microsphere material according to claim 5 in the detection of volatile sulfides, wherein the volatile sulfide is hydrogen sulfide or mercaptan.
7. The use according to claim 6, characterized in that: The mercaptan includes one or more of methyl mercaptan, propyl mercaptan and pentyl mercaptan.
8. The use according to claim 6 or 7, characterized in that: The volatile sulfur compounds come from breath.
9. A method for detecting volatile sulfides by colorimetry, characterized in that: The following steps are involved: The modified copper silicate hollow microsphere material, acidic phosphate buffer, 3,3',5,5'-tetramethylbenzidine solution, H2O2 and a test solution containing volatile sulfide are mixed to carry out a color reaction, the absorbance value of the reaction system at 652nm is measured, and the absorbance value is substituted into a predetermined standard curve to obtain the concentration of volatile sulfide in the test solution; the modified copper silicate hollow microsphere material is the modified copper silicate hollow microsphere material described in claim 5.
10. The method according to claim 9, characterized in that The concentration of the modified copper silicate hollow microsphere material in the mixed solution is 10-15 μg / mL, the concentration of 3,3',5,5'-tetramethylbenzidine is 1 mmol / L, the concentration of H2O2 is 6.25 μmol / L, and the pH value of the mixed solution is 4.
Citation Information
Patent Citations
Method for preparing mesoporous basic copper silicate hollow spheres
CN103263878A
Preparation method of copper-containing mesoporous adsorbent for gasoline desulfurization
CN105126747A
Magnetic copper-doped carbon nitride composite Fenton-like catalyst as well as preparation method and application thereof
CN116532145A
Visual optical device for the control of halitosis