Wastewater composite treatment agent and preparation method thereof
By using metal ions in the dye to form complex catalytic polymerization and photocatalytic flocculation technology to treat printing and dyeing wastewater, the problems of high-salt wastewater and environmental pollution in traditional salting out methods are solved, and efficient salinity reduction and metal ion recovery are achieved.
Patent Information
- Application Number
- CN202411081032.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-08
- Publication Date
- 2024-11-08
AI Technical Summary
The salting purification method in traditional dye production produces a large number of inorganic salt by-products and high-salt dye wastewater, which affects the environment, and the dye wastewater hinders photosynthesis and reduces dissolved oxygen levels.
The metal ions in the dye are used to form complex catalytic monomer polymerization, and the printing and dyeing wastewater is treated by flocculation treatment agent, and the precipitation is separated and precipitated by photocatalysis and ammonia bubbles to reduce salinity and recover metal ions.
It achieves efficient flocculation and salinity reduction of debris in wastewater, avoids secondary pollution, improves treatment efficiency, and saves costs.
Smart Images

Figure BDA0004983737520000071
Abstract
Description
Technical Field
[0001] The invention belongs to the field of water treatment, and in particular relates to a composite wastewater treatment agent and a preparation method thereof. Background Art
[0002] In order to improve the product quality and stability of traditional dyes in production engineering, salting-out purification is usually used. However, a large amount of inorganic salt byproducts such as sodium chloride, magnesium chloride, sodium sulfate, and magnesium sulfate will be produced during the salting-out process. The salt content in the finished dye can be as high as 30-40%, and a large amount of high-salt dye wastewater will be discharged, affecting the environment. Due to the presence of dyes in dye wastewater, the wastewater has color, which will prevent light from penetrating. If it is discharged directly, it will affect the photosynthesis rate in the aquatic system and lead to a decrease in dissolved oxygen levels. Summary of the invention
[0003] The present invention mainly provides a composite treatment agent and treatment method for treating printing and dyeing wastewater by using metal ions in dyes to form complexes to catalyze monomer polymerization, thereby forming flocculation. The technical scheme is as follows:
[0004] A composite wastewater treatment agent comprises a ligand, a polymerized monomer and a coating which wraps the ligand and the polymerized monomer which are placed separately.
[0005] Furthermore, the mass ratio of the ligand to the polymerization monomer is 1:(800-1000).
[0006] Furthermore, the coating is a water-soluble film, and the content begins to dissolve in 20 to 60 minutes; the polymer corresponding to the polymerization monomer is one of polyacrylic acid and polyacrylamide.
[0007] Furthermore, the ligand is wrapped around the polymerized monomer, and an inner coating is between the polymerized monomer and the ligand; the ligand is wrapped around an outer coating; the polymerized monomer and the ligand occupy no more than half of the volume of the inner cavity of the inner coating and the outer coating.
[0008] A method for preparing the above-mentioned composite wastewater treatment agent comprises the following steps:
[0009] a. In a flowing nitrogen atmosphere, o-phthalaldehyde and phenylethylamine were dissolved in dimethyl sulfoxide, and the temperature was raised and stirred for reaction for 12 to 24 hours. An aqueous solution of n-hexane was added to the system, and the stirring reaction was continued for 4 to 6 hours. After cooling to room temperature, acetone was added, and the mixture was fully mixed and allowed to stand for 2 to 3 hours. The precipitate was separated and washed with acetone, and the ligand was obtained after drying.
[0010] b. Place the polymerizable monomer in an inner coating, inflate and seal the inner coating, and then place it in an outer coating. Place the ligand between the outer coating and the inner coating, and then inflate and seal the outer coating.
[0011] Furthermore, the molar ratio of o-phthalaldehyde and phenylethylamine in step a is 1:(2-2.5).
[0012] Furthermore, in the n-hexane aqueous solution in step a, the concentration of n-hexane is 50-60% v / v, and the volume ratio of the added n-hexane aqueous solution to dimethyl sulfoxide is 1:(2-3); the volume ratio of acetone added in step a to dimethyl sulfoxide is 1:(0.5-1).
[0013] Furthermore, the temperature of the temperature-raising reaction in step a is 40-55°C.
[0014] A method for treating wastewater using the composite treatment agent comprises the following steps:
[0015] (1) placing the composite treatment agent in the wastewater to be treated, and irradiating it with light having a main wavelength of 320 to 400 nm for 2 to 4 hours. During the irradiation period, the composite treatment agent is moved to move on the surface of the wastewater. After the irradiation is completed, the composite treatment agent is allowed to stand until the precipitation no longer increases;
[0016] (2) Ammonia gas is bubbled into the wastewater until the precipitate stops increasing and the treatment is completed by separating the precipitate.
[0017] Furthermore, the concentration of the polymer precursor in the composite treatment agent in step (1) in the wastewater to be treated is 5 to 10 mg / L.
[0018] By adopting the above scheme, the method of the present invention has the following advantages:
[0019] 1. After the ligand of the present invention enters the wastewater, it forms a complex with metal ions such as magnesium in the water, and promotes the polymerization of polymer monomers under the action of photocatalysis, thereby achieving flocculation of impurities in the wastewater.
[0020] 2. The present invention utilizes the original metal ions in the wastewater to participate in the wastewater treatment process, does not need to introduce new impurities, avoids secondary pollution, and first complexation will make it easier to produce alkaline precipitation.
[0021] 3. The ligand and the polymerized monomer of the present invention are both wrapped by a soluble coating and can be suspended on the surface of wastewater to absorb light energy, thereby reducing the impact of the poor light transmittance of wastewater on the performance of the treatment agent.
[0022] 4. The ligand of the present invention is wrapped around the polymerizing monomer and reacts with the metal ions in water under light before the polymerizing monomer is exposed, so as to prepare for the subsequent catalytic polymerization. Different wrapping sequences make the exposure time and light exposure time different, and also make the reaction process more compact.
[0023] 5. The treatment method of the present invention bubbles the system after the polymerization and flocculation is completed, so that metal ions such as magnesium are forced to generate insoluble alkaline precipitates, thereby separating and greatly reducing the salinity of the wastewater. At the same time, the metal ions are recovered and the cost is saved.
[0024] 6. The treatment agent of the present invention has a wide range of applications and a simple treatment method, and can be applied to the treatment of a variety of wastewaters of the same nature. DETAILED DESCRIPTION
[0025] The technical solutions in the embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0026] Embodiment 1:
[0027] (1) In a flowing nitrogen atmosphere, o-phthalaldehyde and phenylethylamine are dissolved in dimethyl sulfoxide in a mass ratio of 1:2.2, and the temperature is raised to 40°C and stirred for reaction for 20 hours. A 50% v / v n-hexane aqueous solution 0.5 times the volume of dimethyl sulfoxide is added to the system, and the stirring reaction is continued for 5 hours. After cooling to room temperature, acetone 1 times the volume of dimethyl sulfoxide is added, and the mixture is fully mixed and allowed to stand for 2 to 3 hours. The precipitate is separated and washed with acetone, and the ligand is obtained after drying;
[0028] (2) 800 parts by weight of acrylamide and acryloyloxyethyltrimethylammonium chloride polymerization monomers are placed in an inner coating, the inner coating is inflated and sealed, and then placed in an outer coating, 1 part by weight of a ligand is placed between the outer coating and the inner coating, and then the outer coating is inflated and sealed to obtain a composite treatment agent.
[0029] Embodiment 2:
[0030] (1) In a flowing nitrogen atmosphere, o-phthalaldehyde and phenylethylamine were dissolved in dimethyl sulfoxide in a mass ratio of 1:2.2, heated to 55°C and stirred for reaction for 20 hours, 0.5 times the volume of dimethyl sulfoxide was added to the system with a 50% v / v n-hexane aqueous solution, and the reaction was continued with stirring for 5 hours. After cooling to room temperature, 1 times the volume of dimethyl sulfoxide was added with acetone, and the mixture was fully mixed and allowed to stand for 2 to 3 hours. The precipitate was separated and washed with acetone, and the ligand was obtained after drying;
[0031] (2) 800 parts by weight of acrylamide and acryloyloxyethyltrimethylammonium chloride polymerization monomers are placed in an inner coating, the inner coating is inflated and sealed, and then placed in an outer coating, 1 part by weight of a ligand is placed between the outer coating and the inner coating, and then the outer coating is inflated and sealed to obtain a composite treatment agent.
[0032] Embodiment 3:
[0033] (1) In a flowing nitrogen atmosphere, o-phthalaldehyde and phenylethylamine are dissolved in dimethyl sulfoxide in a mass ratio of 1:2.2, and the temperature is raised to 40°C and stirred for reaction for 20 hours. A 70% v / v n-hexane aqueous solution 0.5 times the volume of dimethyl sulfoxide is added to the system, and the stirring reaction is continued for 5 hours. After cooling to room temperature, acetone 1 times the volume of dimethyl sulfoxide is added, and the mixture is fully mixed and allowed to stand for 2 to 3 hours. The precipitate is separated and washed with acetone, and the ligand is obtained after drying;
[0034] (2) 800 parts by weight of acrylamide and acryloyloxyethyltrimethylammonium chloride polymerization monomers are placed in an inner coating, the inner coating is inflated and sealed, and then placed in an outer coating, 1 part by weight of a ligand is placed between the outer coating and the inner coating, and then the outer coating is inflated and sealed to obtain a composite treatment agent.
[0035] Embodiment 4:
[0036] (1) In a flowing nitrogen atmosphere, o-phthalaldehyde and phenylethylamine are dissolved in dimethyl sulfoxide in a mass ratio of 1:2.2, and the temperature is raised to 40°C and stirred for reaction for 20 hours. A 50% v / v n-hexane aqueous solution 0.5 times the volume of dimethyl sulfoxide is added to the system, and the stirring reaction is continued for 5 hours. After cooling to room temperature, acetone 2 times the volume of dimethyl sulfoxide is added, and the mixture is fully mixed and allowed to stand for 2 to 3 hours. The precipitate is separated and washed with acetone, and the ligand is obtained after drying.
[0037] (2) 800 parts by weight of acrylamide and acryloyloxyethyltrimethylammonium chloride polymerization monomers are placed in an inner coating, the inner coating is inflated and sealed, and then placed in an outer coating, 1 part by weight of a ligand is placed between the outer coating and the inner coating, and then the outer coating is inflated and sealed to obtain a composite treatment agent.
[0038] Embodiment 5:
[0039] (1) In a flowing nitrogen atmosphere, o-phthalaldehyde and phenylethylamine are dissolved in dimethyl sulfoxide in a mass ratio of 1:2.2, and the temperature is raised to 40°C and stirred for reaction for 20 hours. A 50% v / v n-hexane aqueous solution 0.5 times the volume of dimethyl sulfoxide is added to the system, and the stirring reaction is continued for 5 hours. After cooling to room temperature, acetone 1 times the volume of dimethyl sulfoxide is added, and the mixture is fully mixed and allowed to stand for 2 to 3 hours. The precipitate is separated and washed with acetone, and the ligand is obtained after drying;
[0040] (2) 1000 parts by weight of acrylamide and acryloyloxyethyltrimethylammonium chloride polymerization monomers are placed in an inner coating, the inner coating is inflated and sealed, and then placed in an outer coating, 1 part by weight of a ligand is placed between the outer coating and the inner coating, and then the outer coating is inflated and sealed to obtain a composite treatment agent.
[0041] Comparative Example 1:
[0042] (1) In a flowing nitrogen atmosphere, o-phthalaldehyde and phenylethylamine are dissolved in dimethyl sulfoxide in a mass ratio of 1:2.2, and the temperature is raised to 40°C and stirred for reaction for 20 hours. A 50% v / v n-hexane aqueous solution 0.5 times the volume of dimethyl sulfoxide is added to the system, and the stirring reaction is continued for 5 hours. After cooling to room temperature, acetone 1 times the volume of dimethyl sulfoxide is added, and the mixture is fully mixed and allowed to stand for 2 to 3 hours. The precipitate is separated and washed with acetone, and the ligand is obtained after drying;
[0043] (2) 800 parts by weight of the polymerizable monomer and 1 part by weight of the ligand are placed in the coating, and the coating is inflated and sealed to obtain a composite treatment agent.
[0044] Processing Example:
[0045] (1) placing the composite treatment agent in the wastewater to be treated, and irradiating it with light having a main wavelength of 320 to 400 nm for 2 to 4 hours. During the irradiation period, the composite treatment agent is moved to move on the surface of the wastewater. After the irradiation is completed, the composite treatment agent is allowed to stand until the precipitation no longer increases;
[0046] (2) Ammonia gas is bubbled into the wastewater until the precipitate stops increasing and the treatment is completed by separating the precipitate.
[0047] Treatment comparison example:
[0048] The composite treatment agent is placed in the wastewater to be treated and irradiated with light with a main wavelength of 320 to 400 nm for 2 to 4 hours. During the irradiation period, the composite treatment agent is moved to move on the surface of the wastewater. After the irradiation is completed, it is allowed to stand until the precipitation no longer increases.
[0049] Preparation and testing of samples of the embodiments:
[0050] MgSO4 and MgCl2 salt solution were added to a 50 mg / L Coomassie Brilliant Blue G-250 dye solution, so that the concentration of each salt solution in the dye solution was 0.5 g / L, and simulated wastewater was prepared. Each embodiment was treated with the simulated wastewater according to the method for treating the embodiment, and embodiment 1 was treated with the simulated wastewater according to the method for treating the comparative example. Each experiment was repeated 5 times and averaged. The concentrations of the dye and magnesium ion in the simulated wastewater before and after the treatment were measured respectively, and the ratio of the difference to the initial concentration was calculated to obtain a removal rate.
[0051] The results are as follows:
[0052]
[0053] In the process of preparing the ligand in Example 2, the reaction temperature is higher than that in Example 1, and the yield of the ligand is increased. The increase in reaction temperature is conducive to the generation of the ligand. The concentration of the n-hexane aqueous solution added in Example 3 is higher than that in Example 1, and the ligand yield is better. It may be that the n-hexane concentration is higher and the polarity difference of the solvent is greater, which is more conducive to the continuation of the reaction. More acetone is added in Example 4, which is more conducive to the generation and precipitation of precipitation, and the yield of the complex is increased. The amount of polymerization monomer in Example 5 is more, and the amount of ligand is relatively reduced. The removal rate of its dye and salt is not as good as that in Example 1, indicating that the presence of the ligand can help remove the dye and is also conducive to the generation of alkali precipitation of metal ions in the later stage.
[0054] Comparative Example 1 did not separate the ligand from the polymerized monomer, and the treatment agent's ability to remove dyes and salts was significantly reduced. It may be that if they were not separated, the material in the coating entered the wastewater too quickly, resulting in less light, less catalytic energy obtained by the ligand to produce complexes and monomer polymerization, less energy to form products in the wastewater, and the treatment agent could not fully play its role. In the experiment of the treatment comparative example, no ammonia bubbling was performed, and the salt removal rate dropped sharply, but it had a removal rate of 18.31%, indicating that the ligand of the present invention complexed with metal ions, and the polymer or light produced, can produce a certain removal effect on salt.
[0055] For those skilled in the art, various other corresponding changes and deformations can be made according to the technical solutions and concepts described above, and all of these changes and deformations should fall within the protection scope of the claims of the present invention.
Claims
1. A composite wastewater treatment agent, characterized in that: It comprises a ligand, a polymerized monomer placed separately and a coating which wraps the ligand and the polymerized monomer.
2. The composite wastewater treatment agent according to claim 1, characterized in that: The mass ratio of the ligand to the polymerization monomer is 1:(800-1000).
3. The composite wastewater treatment agent according to claim 1, characterized in that: The coating is a water-soluble film, and the content begins to dissolve in 20 to 60 minutes; the polymer corresponding to the polymerization monomer is one of polyacrylic acid and polyacrylamide.
4. The composite wastewater treatment agent according to claim 1, characterized in that: The ligand is wrapped around the polymerized monomer, and an inner coating is provided between the polymerized monomer and the ligand; the ligand is wrapped around the outer coating; the polymerized monomer and the ligand occupy no more than half of the volume of the inner cavity of the inner coating and the outer coating.
5. A method for preparing the composite wastewater treatment agent according to any one of claims 1 to 4, characterized in that: The following steps are involved: a. In a flowing nitrogen atmosphere, o-phthalaldehyde and phenylethylamine were dissolved in dimethyl sulfoxide, and the temperature was raised and stirred for reaction for 12 to 24 hours. An aqueous solution of n-hexane was added to the system, and the stirring reaction was continued for 4 to 6 hours. After cooling to room temperature, acetone was added, and the mixture was fully mixed and allowed to stand for 2 to 3 hours. The precipitate was separated and washed with acetone, and the ligand was obtained after drying. b. Place the polymerizable monomer in an inner coating, inflate and seal the inner coating, and then place it in an outer coating. Place the ligand between the outer coating and the inner coating, and then inflate and seal the outer coating.
6. The method for preparing the composite wastewater treatment agent according to claim 5, characterized in that: The molar ratio of o-phthalaldehyde and phenylethylamine in step a is 1:(2-2.5).
7. The method for preparing the composite wastewater treatment agent according to claim 5, characterized in that: In the n-hexane aqueous solution of step a, the concentration of n-hexane is 50-60% v / v, and the volume ratio of the added n-hexane aqueous solution to dimethyl sulfoxide is 1:(2-3); the volume ratio of acetone to dimethyl sulfoxide added in step a is 1:(0.5-1).
8. The method for preparing the composite wastewater treatment agent according to claim 5, characterized in that: The temperature of the temperature-raising reaction in step a is 40-55°C.
9. A method for treating wastewater using the composite treatment agent according to any one of claims 1 to 4, characterized in that: The following steps are involved: (1) placing the composite treatment agent in the wastewater to be treated, and irradiating it with light having a main wavelength of 320 to 400 nm for 2 to 4 hours. During the irradiation period, the composite treatment agent is moved to move on the surface of the wastewater. After the irradiation is completed, the composite treatment agent is allowed to stand until the precipitation no longer increases; (2) Ammonia gas is bubbled into the wastewater until the precipitate stops increasing and the treatment is completed by separating the precipitate.
10. The method for preparing the composite wastewater treatment agent according to claim 9, characterized in that: The concentration of the polymer precursor in the composite treatment agent in step (1) in the wastewater to be treated is 5 to 10 mg / L.
Citation Information
Patent Citations
Dyeing waste water treating agent and preparation method thereof
CN105600852A
Degradable magnetic organic-inorganic composite material and preparation method thereof
CN109250798A
Composite flocculant for treating printing and dyeing wastewater
CN109734145A
Separation method of metal ion
JP2013017994A