Preparation method of high-flame-retardant passenger plane interior material

By preparing PVC resin and other materials through high-speed stirring and multi-process processing, the problem of insufficient fire resistance of passenger aircraft interior materials is solved, and the passenger aircraft interior materials with high flame retardant performance and anti-mildew and antibacterial effects are achieved, which improves the safety of the aircraft and visual effects.

CN118909360APending Publication Date: 2024-11-08浙江明士达股份有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410968845.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-18
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The existing airliner interior materials have shortcomings in fire resistance and cannot meet the needs of lighter, more economical and flame retardant, especially the application of PVC materials.

Method used

Use PVC resin powder, plasticizer, stabilizer, elastoster, aviation flame retardant, toughener, internal slip agent, processing aid, external slip agent, anti-mildew antibacterial agent, titanium dioxide, yellow color material and black color Materials and other materials are prepared through high-speed stirring, extrusion, refining, filtration, calendering, cooling, edge cutting, curling, printing and drying and other processes.

Benefits of technology

The prepared materials have excellent flame retardant properties, can meet the B1 standard, improve the safety of the aircraft, and have anti-mildew and antibacterial effects, with good visual effects, suitable for the formation of a variety of textures and colors.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118909360A_ABST
    Figure CN118909360A_ABST
Patent Text Reader

Abstract

The invention provides a preparation method of a high-flame-retardant passenger plane interior material. The preparation method comprises the following steps: S1, mixing 90-110 parts by mass of PVC resin powder, 2-4 parts by mass of a plasticizer, 3-6 parts by mass of a stabilizer, 3.5-5.5 parts by mass of an elastic agent, 20-30 parts by mass of an aviation flame retardant, 6-10 parts by mass of a flexibilizer, 3-6 parts by mass of an internal lubricant, 4-5 parts by mass of a processing aid, 1-3 parts by mass of an external lubricant, 0.1-0.7 part by mass of an anti-mildew antibacterial agent, 10-18 parts by mass of titanium dioxide, 0.02-0.04 part by mass of a yellow pigment and 0.01-0.03 part by mass of a black pigment; uniformly mixing by a high-speed stirrer; s2, performing extrusion, open milling, filtration, calendering, cooling, trimming and curling on the mixture in the step S1 to obtain a PVC film; s3, the PVC film prepared in the step S2 is printed, dried, embossed and rolled, and the finished product of the high-flame-retardant passenger plane interior material can be obtained.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of interior material preparation, and in particular to a method for preparing a highly flame-retardant passenger aircraft interior material. Background Art

[0002] Fire is one of the important reasons that affect the safe flight of aircraft. Preventing aircraft fires and actively conducting fire prevention research are very important for aircraft safety. Whether it is a passenger aircraft, cargo aircraft, defense aircraft or business aircraft, there are strict fire prevention design requirements. In order to ensure the safety of the aircraft during use, the interior materials are required to be flame retardant. In other words, the aircraft interior materials must either have non-combustible properties. If a part of the interior material is combustible, it must also meet specific flame retardant performance requirements.

[0003] The materials used in the aircraft manufacturing process are usually based on traditional metal materials such as aluminum and steel, but the demand for lighter and more economical aircraft interior materials is increasing. PVC materials with good plasticity, light weight, strong functionality and affordable price have become the research focus of aircraft interior materials. Therefore, it is necessary to design a preparation method for highly flame-retardant passenger aircraft interior materials. Summary of the invention

[0004] The purpose of the present invention is to solve the above problems in the prior art and to propose a method for preparing a highly flame-retardant passenger aircraft interior material.

[0005] The object of the present invention can be achieved by the following technical scheme: A method for preparing a highly flame-retardant passenger aircraft interior material, the preparation method comprising the following steps:

[0006] S1. By mass: 90-110 parts of PVC resin powder, 2-4 parts of plasticizer, 3-6 parts of stabilizer, 3.5-5.5 parts of elastic agent, 20-30 parts of aviation flame retardant, 6-10 parts of toughening agent, 3-6 parts of internal lubricant, 4-5 parts of processing aid, 1-3 parts of external lubricant, 0.1-0.7 parts of mildew and antibacterial agent, 10-18 parts of titanium dioxide, 0.02-0.04 parts of yellow colorant, 0.01-0.03 parts of black colorant, and mix them evenly in a high-speed mixer;

[0007] S2, the mixture in step S1 is further extruded, refined, filtered, calendered, cooled, trimmed, and curled to obtain a PVC film;

[0008] S3. The PVC film obtained in step S2 is printed, dried, embossed, and rolled to obtain a finished product of a highly flame-retardant passenger aircraft interior material.

[0009] The elastic agent in step S1 is nitrile rubber.

[0010] The toughening agent in step S1 is methyl methacrylate-butadiene-styrene.

[0011] The stabilizer in step S3 is a liquid barium zinc stabilizer.

[0012] The high-speed mixer comprises a base, a stirring and mixing box is arranged on the top of the base, a mounting plate is fixedly installed on the top of the stirring and mixing box, a high-speed motor is fixedly installed on the top of the mounting plate, a transmission rod is fixedly installed on the output shaft of the high-speed motor, a stirring rod is fixedly installed on the bottom of the transmission rod, and a sealing device is arranged on the top of the base and located on the outside of the stirring and mixing box;

[0013] The sealing device includes a first arched mounting frame, which is arranged at the top of the base and located on the outside of the stirring and mixing box. Two second arched mounting frames are arranged at the bottom of the first arched mounting frame. Two sealing plates are fixedly installed at the bottom of the second arched mounting frame. The bottom of the sealing plate is located at the top of the stirring and mixing box and on both sides of the mounting plate.

[0014] Two electric push rods are fixedly mounted on the top of the first arched mounting frame, and the output ends of the electric push rods pass through the first arched mounting frame and are fixedly connected to the top of the second arched mounting frame.

[0015] Two slide grooves are arranged on the top of the base, and a sliding block is slidably connected inside the slide groove, and the top of the sliding block is fixedly connected to the bottom of the first arched mounting frame.

[0016] Two servo motors are fixedly installed on the left side of the base, and a threaded rod is fixedly installed on the output shaft of the servo motor. The right side of the threaded rod penetrates into the interior of the slide groove and is rotatably connected with the slider through a thread.

[0017] A rubber support block is fixedly installed at the bottom of the base, and evenly distributed support rods are fixedly installed at the bottom of the stirring and mixing box. The bottom of the support rod is fixedly connected to the top of the base.

[0018] The bottom of the stirring and mixing box is connected with a discharge pipe, and the right side of the discharge pipe extends rightward and extends to the right side of the base.

[0019] Two mounting rods are fixedly mounted on both sides of the top of the stirring rod, and the mounting rods are arranged in an eight-shaped shape.

[0020] The present invention is beneficial in that:

[0021] 1. After ink printing and embossing treatment, it can form a variety of textures and colors, which is good in appreciation and visual effect.

[0022] 2. Aviation-specific flame retardants are added to the PVC film formula. The finished product has excellent flame retardant properties. The finished product oxygen index test can reach the B1 standard, which greatly improves the safety of the aircraft.

[0023] 3. The product has anti-mildew and antibacterial effects, and will not turn black or moldy.

[0024] 4. The high-speed motor is used to accommodate the raw materials. The high-speed motor, the transmission rod and the stirring rod are used to stir the raw materials stored in the high-speed motor at high speed, so as to facilitate the subsequent fusion of the raw materials. The second arch mounting frame and the sealing plate are used to seal the top of the mixing box and the filling area on both sides of the mounting plate to avoid leakage of raw materials and waste when the raw materials are stirred at high speed. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0026] Figure 1 It is a structural schematic diagram of the present invention;

[0027] Figure 2 It is a schematic diagram of the structure of the stirring and mixing box of the present invention;

[0028] Figure 3 It is a schematic diagram of the structure of the sealing device of the present invention;

[0029] Figure 4 It is a schematic diagram of the structure of the stirring device of the present invention.

[0030] In the figure: 1. base; 2. rubber support block; 3. support rod; 4. discharge pipe; 5. stirring mixing box; 6. sealing device; 601. first arch mounting frame; 602. electric push rod; 603. second arch mounting frame; 604. sealing plate; 605. slider; 606. threaded rod; 607. servo motor; 608. slide; 7. mounting plate; 8. high-speed motor; 9. transmission rod; 10. mounting rod; 11. stirring rod. DETAILED DESCRIPTION

[0031] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0032] The following is combined with Figure 1-4 To further explain this application in detail,

[0033] The preparation method of the highly flame-retardant passenger aircraft interior material comprises the following steps:

[0034] S1. By mass: 90-110 parts of PVC resin powder, 2-4 parts of plasticizer, 3-6 parts of stabilizer, 3.5-5.5 parts of elastic agent, 20-30 parts of aviation flame retardant, 6-10 parts of toughening agent, 3-6 parts of internal lubricant, 4-5 parts of processing aid, 1-3 parts of external lubricant, 0.1-0.7 parts of mildew and antibacterial agent, 10-18 parts of titanium dioxide, 0.02-0.04 parts of yellow pigment, 0.01-0.03 parts of black pigment. , and mix them evenly with a high-speed mixer; specifically: by mass: 100 parts of PVC resin powder, 3 parts of plasticizer, 4 parts of stabilizer, 4.5 parts of elastic agent, 24 parts of aviation flame retardant, 8 parts of toughening agent, 4.8 parts of internal lubricant, 3.5 parts of processing aid, 1.6 parts of external lubricant, 0.3 parts of mildew and antibacterial agent, 16.2 parts of titanium dioxide, 0.0225 parts of yellow colorant, 0.0138 parts of black colorant, and mix them evenly with a high-speed mixer;

[0035] S2, the mixture in step S1 is further extruded, refined, filtered, calendered, cooled, trimmed, and curled to obtain a PVC film;

[0036] S3. The PVC film obtained in step S2 is printed, dried, embossed, and rolled to obtain a finished product of a highly flame-retardant passenger aircraft interior material.

[0037] The elastic agent in step S1 is nitrile rubber.

[0038] The toughening agent in step S1 is methyl methacrylate-butadiene-styrene.

[0039] The stabilizer in step S3 is a liquid barium zinc stabilizer.

[0040] Reference Figure 1 and Figure 3The high-speed mixer comprises a base 1, a stirring and mixing box 5 is arranged on the top of the base 1, a mounting plate 7 is fixedly installed on the top of the stirring and mixing box 5, a high-speed motor 8 is fixedly installed on the top of the mounting plate 7, a transmission rod 9 is fixedly installed on the output shaft of the high-speed motor 8, a stirring rod 11 is fixedly installed on the bottom of the transmission rod 9, and a sealing device 6 is arranged on the top of the base 1 and on the outside of the stirring and mixing box 5:

[0041] The sealing device 6 includes a first arched mounting frame 601, which is arranged at the top of the base 1 and located on the outside of the stirring and mixing box 5. Two second arched mounting frames 603 are arranged at the bottom of the first arched mounting frame 601. Two sealing plates 604 are fixedly installed at the bottom of the second arched mounting frame 603. The bottom of the sealing plate 604 is located at the top of the stirring and mixing box 5 and on both sides of the mounting plate 7.

[0042] Reference Figure 1 and Figure 3 Two electric push rods 602 are fixedly installed on the top of the first arch mounting frame 601. The output end of the electric push rod 602 passes through the first arch mounting frame 601 and is fixedly connected to the top of the second arch mounting frame 603. The setting of the electric push rod 602 is used to realize the lifting and lowering adjustment of the second arch mounting frame 603 and the sealing plate 604, so that the sealing plate 604 is separated from the mixing box 5 to facilitate the addition of raw materials into the mixing box 5.

[0043] Reference Figure 1 , Figure 2 and Figure 3 Two slide grooves 608 are provided on the top of the base 1, and a slider 605 is slidably connected inside the slide groove 608. The top of the slider 605 is fixedly connected to the bottom of the first arch mounting frame 601. The setting of the slider 605 and the slide groove 608 is used to realize the installation of the first arch mounting frame 601.

[0044] Reference Figure 1 and Figure 3 Two servo motors 607 are fixedly installed on the left side of the base 1, and a threaded rod 606 is fixedly installed on the output shaft of the servo motor 607. The right side of the threaded rod 606 penetrates into the interior of the slide groove 608 and is rotatably connected to the slider 605 through a thread. The setting of the slider 605, the threaded rod 606 and the servo motor 607 is used to realize the movement of the first arch mounting frame 601, thereby driving the sealing plate 604 to move out from the top of the mixing box 5 to facilitate the filling of the raw materials.

[0045] Reference Figure 1 and Figure 2A rubber support block 2 is fixedly installed at the bottom of the base 1, and evenly distributed support rods 3 are fixedly installed at the bottom of the mixing box 5. The bottom of the support rod 3 is fixedly connected to the top of the base 1. The rubber support block 2 is used to support the base 1, and the support rod 3 is used to install the mixing box 5 and lift the mixing box 5 at the same time.

[0046] Reference Figure 1 and Figure 2 The bottom of the stirring and mixing box 5 is connected to a discharge pipe 4, and the right side of the discharge pipe 4 extends to the right and extends to the right side of the base 1. The discharge pipe 4 is provided to discharge the mixed raw materials. By extending the discharge pipe 4 to the right side of the base 1, it is convenient to discharge the raw materials into the interior of the storage container.

[0047] Reference Figure 4 Two mounting rods 10 are fixedly installed on both sides of the top of the stirring rod 11. The mounting rods 10 are arranged in an eight-shaped shape. The mounting rods 10 are used to stir the raw materials. By arranging the mounting rods 10 in an eight-shaped shape, it is easy to stir the movement of the internal raw materials, thereby accelerating the mutual fusion between the raw materials.

[0048] The threaded rod 606 is driven to rotate by the servo motor 607, and the slider 605 is driven to move to the right under the action of the thread, and the first arched mounting frame 601 is driven to move to the right at the same time, so that the sealing plate 604 is removed from the top of the stirring and mixing box 5, and the raw materials to be mixed are sequentially added into the stirring and mixing box 5. The threaded rod 606 is driven to rotate by the servo motor 607, and the slider 605 is driven to move to the left under the action of the thread, so that the sealing plate 604 is located at the top of the stirring and mixing box 5. The second arched mounting frame 603 is pushed by the electric push rod 602 to drive the sealing plate 604 to descend, and then the filling area on the top of the stirring and mixing box 5 and on both sides of the mounting plate 7 is sealed. After sealing, the transmission rod 9 is driven by the high-speed motor 8 to drive the mounting rod 10 and the stirring rod 11 to rotate, thereby driving the internal raw materials to move and mix them. After mixing, the high-speed motor 8 is turned off to discharge the raw materials through the discharge pipe 4, and a mixture for making PVC film can be obtained.

[0049] The above shows and describes the basic principles, main features and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited to the above embodiments, and the above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, and these changes and improvements all fall within the scope of the present invention to be protected.

Claims

1. A method for preparing a highly flame-retardant passenger aircraft interior material, characterized in that: The preparation method comprises the following steps: S1. By mass: 90-110 parts of PVC resin powder, 2-4 parts of plasticizer, 3-6 parts of stabilizer, 3.5-5.5 parts of elastic agent, 20-30 parts of aviation flame retardant, 6-10 parts of toughening agent, 3-6 parts of internal lubricant, 4-5 parts of processing aid, 1-3 parts of external lubricant, 0.1-0.7 parts of mildew and antibacterial agent, 10-18 parts of titanium dioxide, 0.02-0.04 parts of yellow colorant, 0.01-0.03 parts of black colorant, and mix them evenly in a high-speed mixer; S2, the mixture in step S1 is further extruded, refined, filtered, calendered, cooled, trimmed, and curled to obtain a PVC film; S3. The PVC film obtained in step S2 is printed, dried, embossed, and rolled to obtain a finished product of a highly flame-retardant passenger aircraft interior material.

2. The method for preparing a highly flame-retardant passenger aircraft interior material according to claim 1, characterized in that: The elastic agent in step S1 is nitrile rubber.

3. The method for preparing a highly flame-retardant passenger aircraft interior material according to claim 1, characterized in that: The toughening agent in step S1 is methyl methacrylate-butadiene-styrene.

4. The method for preparing a highly flame-retardant passenger aircraft interior material according to claim 1, characterized in that: The stabilizer in step S3 is a liquid barium zinc stabilizer.

5. The method for preparing a highly flame-retardant passenger aircraft interior material according to claim 1, characterized in that: The high-speed mixer comprises a base (1), a stirring and mixing box (5) is arranged on the top of the base (1), a mounting plate (7) is fixedly mounted on the top of the stirring and mixing box (5), a high-speed motor (8) is fixedly mounted on the top of the mounting plate (7), a transmission rod (9) is fixedly mounted on the output shaft of the high-speed motor (8), a stirring rod (11) is fixedly mounted on the bottom of the transmission rod (9), and a sealing device (6) is arranged on the top of the base (1) and located on the outside of the stirring and mixing box (5); The sealing device (6) comprises a first arched mounting frame (601), the first arched mounting frame (601) being arranged on the top of the base (1) and located outside the stirring and mixing box (5), two second arched mounting frames (603) being arranged at the bottom of the first arched mounting frame (601), two sealing plates (604) being fixedly mounted at the bottom of the second arched mounting frame (603), the bottom of the sealing plates (604) being located at the top of the stirring and mixing box (5) and at both sides of the mounting plate (7); Two electric push rods (602) are fixedly mounted on the top of the first arched mounting frame (601), and the output ends of the electric push rods (602) pass through the first arched mounting frame (601) and are fixedly connected to the top of the second arched mounting frame (603).

6. The method for preparing a highly flame-retardant passenger aircraft interior material according to claim 5, characterized in that: Two slide grooves (608) are provided on the top of the base (1), and a slider (605) is slidably connected inside the slide groove (608), and the top of the slider (605) is fixedly connected to the bottom of the first arched mounting frame (601).

7. The method for preparing a highly flame-retardant passenger aircraft interior material according to claim 6, characterized in that: Two servo motors (607) are fixedly mounted on the left side of the base (1), and a threaded rod (606) is fixedly mounted on the output shaft of the servo motor (607). The right side of the threaded rod (606) passes through the interior of the slide groove (608) and is rotatably connected to the slider (605) via a thread.

8. The method for preparing a highly flame-retardant passenger aircraft interior material according to claim 5, characterized in that: A rubber support block (2) is fixedly mounted on the bottom of the base (1), and evenly distributed support rods (3) are fixedly mounted on the bottom of the stirring and mixing box (5), wherein the bottom of the support rod (3) is fixedly connected to the top of the base (1).

9. The method for preparing a highly flame-retardant passenger aircraft interior material according to claim 5, characterized in that: The bottom of the stirring and mixing box (5) is connected to a discharge pipe (4), and the right side of the discharge pipe (4) extends to the right and extends to the right side of the base (1).

10. The method for preparing a highly flame-retardant passenger aircraft interior material according to claim 5, characterized in that: Two mounting rods (10) are fixedly mounted on both sides of the top of the stirring rod (11), and the mounting rods (10) are arranged in an eight-shaped shape.