Method for adaptively adjusting technological parameters of fused yarn

By analyzing history records and introducing process evaluation functions for dynamic monitoring, the melting process parameters are automatically adjusted, which solves the problems of traditional adjustment efficiency and unstable quality, and achieves more efficient process adjustment and product quality improvement.

CN118910775AInactive Publication Date: 2024-11-08NANTONG SANRUN TECH DEV CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411406714.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-10
Publication Date
2024-11-08
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The traditional yarn-melting process parameter adjustment relies on manual experience, resulting in low regulation efficiency and unstable product quality, and the inability to adapt to production environment and raw material changes.

Method used

By obtaining and analyzing historical yarn process adjustment records, introducing yarn process evaluation functions, generating historical process indexes, dynamic process monitoring and adaptive adjustments, and automatically adjusting process parameters.

Benefits of technology

It improves the efficiency and accuracy of process adjustment, reduces manual intervention, and ensures the stability and production efficiency of product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118910775A_ABST
    Figure CN118910775A_ABST
Patent Text Reader

Abstract

The invention discloses an adaptive adjustment method for technological parameters of fused yarns, and relates to the technical field of blending, and the method comprises the following steps: obtaining a historical fused yarn technological adjustment record; extracting a first historical adjustment record, wherein the first historical adjustment record comprises a historical adjustment process scheme, a historical fused yarn manufacturing record and historical fused yarn quality inspection information; analyzing the historical fused yarn manufacturing record and quality inspection information by using a fused yarn process evaluation function to obtain a first historical process index; when the first historical process index accords with a preset process index limit value, taking the first historical process index parameter as a target process adjustment reference; performing dynamic process monitoring on the target fused yarn to obtain a target real-time process index parameter; and comparing the target real-time process index parameter with the first historical process index parameter, and when a comparison result reaches a preset comparison deviation, sending a self-adaptive adjustment instruction to perform process parameter adjustment on the target fused yarn. Therefore, the technical effects of improving the adjusting efficiency and improving the product quality are achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of blended spinning, and in particular to a method for adaptively adjusting process parameters of melt-bonded yarns. Background Art

[0002] Melt-bonded yarn is a type of yarn that is made by melting rather than spinning during the spinning process. It is widely used in textile, decoration and industrial fields.

[0003] The traditional adjustment of melt-bonding yarn process parameters mainly relies on manual experience or trial production to determine fixed set values. Operators will adjust process parameters such as temperature, pressure, speed, etc. based on experience or preset parameters. Manual adjustment is labor-intensive and inefficient, and may lead to unstable product quality due to differences in operator experience; fixed set values ​​cannot adapt to changes in production environment and raw materials, which may lead to a decline in product quality. There are technical problems such as low adjustment efficiency and unstable product quality. Summary of the invention

[0004] The present invention provides a method for adaptively adjusting process parameters of fusion-bonded yarns, so as to solve the technical problems of low adjustment efficiency and unstable product quality in the prior art, and achieve the technical effects of improving adjustment efficiency and improving product quality.

[0005] In a first aspect, the present invention provides a method for adaptively adjusting process parameters of a fusion-bonded yarn, wherein the method comprises: Acquire historical fusion yarn process adjustment records, wherein the historical fusion yarn process adjustment records include multiple historical adjustment records; Extracting a first historical adjustment record from the multiple historical adjustment records, wherein the first historical adjustment record includes a first historical adjustment process scheme, a first historical fused yarn manufacturing record, and first historical fused yarn quality inspection information; Introducing a fusion yarn process evaluation function to analyze the first historical fusion yarn manufacturing record and the first historical fusion yarn quality inspection information to obtain a first historical process index, wherein the first historical process index is used to quantitatively evaluate the first historical process indicator parameter in the first historical adjustment process scheme extracted based on the predetermined process indicator traversal; When the first historical process index meets the predetermined process index limit, the first historical process index parameter is used as a target process adjustment benchmark; Based on the predetermined process index, dynamic process monitoring is performed on the target fused yarn to obtain target real-time process index parameters; Comparing the target real-time process indicator parameter with the first historical process indicator parameter to obtain a first comparison result; When the first comparison result reaches a predetermined comparison deviation, an adaptive adjustment instruction is issued, and process parameters of the target fused yarn are adjusted based on the adaptive adjustment instruction.

[0006] In this method, by acquiring and extracting multiple historical fusion yarn process adjustment records, the historical adjustment process plans, manufacturing records and quality inspection information were comprehensively analyzed and evaluated, and a historical process index was established to quantify and evaluate the process indicator parameters in the historical adjustment process plans, thereby providing a reference benchmark for current process adjustments.

[0007] In this method, a fusion yarn process evaluation function is introduced to conduct quantitative evaluation of historical manufacturing records and quality inspection information to generate a process index, which can more objectively judge its compliance and effectiveness, provide a scientific basis for target process adjustment, and avoid the subjectivity and uncertainty of traditional manual experience judgment.

[0008] In this method, through real-time monitoring and dynamic comparison, process deviations can be discovered in a timely manner. When the deviation reaches a predetermined value, an adaptive adjustment instruction is automatically issued to perform real-time process parameter adjustments, thereby improving the response speed and accuracy of process adjustments.

[0009] In this method, the timeliness and effectiveness of process adjustment are ensured through the automatic execution of adaptive adjustment instructions, human intervention is reduced, and the automation degree and production efficiency of process adjustment are improved.

[0010] The method for self-adapting process parameters for fusion-bonding yarn disclosed in the present invention solves the technical problems of low adjustment efficiency and unstable product quality, and achieves the technical effects of improving adjustment efficiency and improving product quality. BRIEF DESCRIPTION OF THE DRAWINGS

[0011] Figure 1 It is a schematic flow chart of the process parameter adaptive adjustment method for melt-bonding yarn of the present invention; Figure 2 The present invention is a schematic diagram of a process flow for obtaining a first historical process index in the process parameter adaptive adjustment method for melt-bonding yarn. DETAILED DESCRIPTION

[0012] The technical solution provided in the embodiments of the present invention is to solve the technical problems of low regulation efficiency and unstable product quality in the prior art. The overall idea adopted is as follows: First, obtain the historical fusion yarn process adjustment record, which includes multiple historical adjustment records. Then, extract the first historical adjustment record from the multiple historical adjustment records, which includes the first historical adjustment process scheme, the first historical fusion yarn manufacturing record and the first historical fusion yarn quality inspection information. Then, introduce the fusion yarn process evaluation function to analyze the first historical fusion yarn manufacturing record and the first historical fusion yarn quality inspection information to obtain the first historical process index. The first historical process index is used to quantitatively evaluate the first historical process indicator parameters in the first historical adjustment process scheme extracted based on the predetermined process indicator traversal. When the first historical process index meets the predetermined process index limit, the first historical process indicator parameters are used as the target process adjustment benchmark. Dynamic process monitoring of the target fusion yarn is performed based on the predetermined process indicators to obtain the target real-time process indicator parameters.

[0013] The target real-time process index parameter is compared with the first historical process index parameter to obtain a first comparison result. When the first comparison result reaches a predetermined comparison deviation, an adaptive adjustment instruction is issued, and the process parameter of the target fused yarn is adjusted based on the adaptive adjustment instruction.

[0014] The above technical solution will be described in detail below in conjunction with the accompanying drawings and specific implementation methods of the specification to better understand the above technical solution. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments of the present invention. It should be understood that the present invention is not limited to the example embodiments used only to explain the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention. In addition, it should be noted that, for the convenience of description, only the parts related to the present invention are shown in the drawings, rather than all of them.

[0015] Figure 1 The present invention is a flow chart of a method for adaptively adjusting process parameters of a melt-bonded yarn; the method includes: A historical fusion yarn process adjustment record is obtained, wherein the historical fusion yarn process adjustment record includes multiple historical adjustment records.

[0016] Specifically, the fusible yarn is a sheath-core synthetic fiber, whose structure consists of an outer sheath and an inner core, and the sheath is partially fused with the core. The sheath is a low-melting-point material that usually melts when heated to 110°C to 150°C. The core is a high-melting-point material that retains its original shape when the sheath melts. When the fusible yarn is heated to a certain temperature, the fibers inside or between the yarns melt and stick together to form a more stable and durable structure.

[0017] Optionally, by interacting with the production management equipment in the target scene or the target production line, a historical adjustment log is obtained, and the historical adjustment log is analyzed to obtain a historical fusion yarn process adjustment record. The historical fusion yarn process adjustment record contains detailed information collected during the fusion yarn process adjustment process, including parameter settings, adjustment results, etc.

[0018] Optionally, the multiple historical adjustment records included in the historical fusion yarn process adjustment record correspond to multiple adjustment processes recorded when the fusion yarn process adjustment is performed at different time points. Exemplarily, the acquisition of the historical fusion yarn process adjustment record is based on a preset call constraint, and the call constraint is used to screen and filter the historical records to ensure that the acquired records meet specific requirements. Specifically, the call constraint includes an adjustment result constraint, a time window constraint, a target product performance constraint, etc.

[0019] Among them, the adjustment result constraint stipulates that only the adjustment records of certain specific results are of interest, such as only focusing on those records that improve product quality or production efficiency, which helps to quickly find effective adjustment strategies. The time window constraint means that only the records within a certain time period are of interest, such as only focusing on the records of the most recent year, thereby improving the timeliness of the obtained production situation and process improvement. The target product performance constraint is used to filter the records that meet the performance requirements of specific products, such as only focusing on the records that generate fusible yarns with specific strength or elasticity, thereby narrowing the confidence region of parameter adjustment and facilitating the efficient determination of process parameters that meet the performance requirements of specific products.

[0020] Through the above method, the historical records of the fusion yarn process adjustment are obtained, which provides basic data for subsequent data analysis and process optimization.

[0021] A first historical adjustment record among the multiple historical adjustment records is extracted, wherein the first historical adjustment record includes a first historical adjustment process scheme, a first historical fused yarn manufacturing record, and first historical fused yarn quality inspection information.

[0022] Optionally, a first historical adjustment record is obtained by randomly extracting multiple historical adjustment records included in the historical fusion yarn process adjustment record. The first historical adjustment record includes a first historical adjustment process scheme, a first historical fusion yarn manufacturing record and a first historical fusion yarn quality inspection information.

[0023] Among them, the first historical adjustment process plan includes various process parameters used in the manufacture of fusible yarn, such as heating temperature, heating time, the ratio of main fiber and cortical fiber, etc.; the first historical fusible yarn manufacturing record includes the actual operation record in the manufacturing process, reflecting the actual application of the aforementioned first historical adjustment process plan, such as the actual heating temperature, heating time, fiber ratio, production line operation status, possible abnormal conditions, etc.; the first historical fusible yarn quality inspection information includes the quality inspection results of the manufactured fusible yarn, such as the breaking strength, reinforcement rate, breaking elongation, elongation reduction, abrasion resistance, hairiness number, color difference, etc. of the yarn.

[0024] A fused yarn process evaluation function is introduced to analyze the first historical fused yarn manufacturing record and the first historical fused yarn quality inspection information to obtain a first historical process index, wherein the first historical process index is used to quantitatively evaluate the first historical process indicator parameters in the first historical adjustment process plan extracted based on the predetermined process indicator traversal.

[0025] Among them, the fusion yarn process evaluation function is an evaluation function determined based on the production requirements of the target scenario or target production line. It is used to quantitatively evaluate the historical adjustment process plan based on historical manufacturing records and quality inspection information to generate a process index.

[0026] Optionally, a fusion yarn process evaluation function is configured, and the configuration method may include: obtaining the production requirements of the target scenario or target production line, and configuring by an expert system or professionals; based on big data, obtaining the homologous sample process index and the corresponding process indicator parameters, and then, based on a machine learning model or a regression model, constructing a fusion yarn process evaluation function.

[0027] Optionally, based on the preset process indicators, the first historical adjustment process scheme is traversed to obtain the first historical process indicator parameters, wherein the preset process indicators are the core process indicators that the target scene or target production line needs to focus on, and the preset process indicators have a significant impact on the production control adjustment of the target scene or target production line. The first historical process indicator parameters are specific values ​​of the process indicators preset in the first historical adjustment process scheme, preferably, for the production of fusion yarn, they include heating temperature, heating time, and curing time.

[0028] Exemplarily, the preset process index can be determined by professional technicians or an expert system. In addition, the principal components of multiple process indexes in the first historical adjustment process scheme can be obtained based on the principal component analysis method and configured as the preset process index.

[0029] The introduction of the fusion yarn process evaluation function helps to more objectively judge the performance of process index parameters, provide a scientific basis for target process adjustment, and avoid the subjectivity and uncertainty of traditional manual experience judgment.

[0030] In some embodiments, a fusion yarn process evaluation function is introduced to analyze the first historical fusion yarn manufacturing record and the first historical fusion yarn quality inspection information to obtain a first historical process index, including: Read a predetermined manufacturing indicator, and traverse and extract the first historical fused yarn manufacturing record based on the predetermined manufacturing indicator to obtain a first historical manufacturing indicator parameter; read a predetermined quality inspection indicator, and traverse and extract the first historical fused yarn quality inspection information based on the predetermined quality inspection indicator to obtain a first historical quality inspection indicator parameter; analyze the first historical manufacturing indicator parameter and the first historical quality inspection indicator parameter according to the fused yarn process evaluation function to obtain the first historical process index.

[0031] Optionally, the fusion yarn process evaluation function uses the first historical manufacturing index parameter and the first historical quality inspection index parameter as independent variables to calculate and obtain the first historical process index, which represents the process quality level. The first historical manufacturing index parameter is the index parameter value of the predetermined manufacturing index in the first historical fusion yarn manufacturing record. The first historical quality inspection index parameter is the index parameter value of the predetermined quality inspection index in the first historical fusion yarn manufacturing record. Specifically, a data processing algorithm is used to extract the corresponding manufacturing parameters from the historical manufacturing records. In some implementations, the predetermined manufacturing indicators include at least a heating temperature, a heating time, and a curing time.

[0032] Specifically, by utilizing the difference in melting points between the low-melting-point skin material and the high-melting-point core material, and by controlling the appropriate heating temperature and heating time during the heating process, the skin layer is melted while the core layer maintains its physical structure unchanged. The melted skin layer has a good adhesion effect, which allows the surrounding fibers to be bonded and embraced, and has good peel strength. At the same time, the low-melting-point skin material is blended with the fibers in the yarn body (high-melting-point core material), making it difficult for the fibers in the yarn body to be pulled out and cause yarn breakage, thereby increasing the strength of the yarn.

[0033] Optionally, the curing time is the length of time it takes to cool the yarn to solidify after heating it to melt it during the production process of the hot melt yarn. During a longer curing time, the molten state of the yarn can better penetrate into other materials and form a stronger bond during the cooling process. It helps the yarn to bond better with other materials and improve the strength and durability of the hot melt yarn. As a result, a longer curing time will increase the time cost of yarn production and reduce production efficiency. In addition, the ambient humidity, ambient temperature and curing conditions (natural ventilation, forced ventilation, etc.) of the target scene will also affect the selection of curing time.

[0034] In some implementations, the predetermined quality inspection indicators include at least the glue content of the prepreg yarn, the uniformity of the yarn, the elongation of the yarn, the strength of the yarn, and the abrasion resistance of the yarn.

[0035] Optionally, the predetermined quality inspection index is a multi-dimensional index for evaluating the quality of the fusion-bonded yarn product, specifically, including the glue content of the prepreg yarn, the yarn uniformity, the yarn elongation, the yarn strength and the yarn wear resistance.

[0036] Among them, the glue content of the prepreg yarn refers to the content of the low-melting-point cortical material (resin or other adhesive) in the prepreg yarn. The glue content of the prepreg yarn is indicated as a percentage value, which directly affects the performance and quality of the fusible yarn. Yarn uniformity refers to the uniformity of the density and structural distribution of the yarn on the cross section. Uniform yarn can improve the isotropy and durability of the quality of the fusible yarn product. Yarn elongation refers to the ratio of the length of the yarn extended under force to the original length, reflecting the elastic properties of the yarn. Yarn strength refers to the ability of the yarn to resist breaking when subjected to external force, that is, the breaking strength. Yarn wear resistance refers to the ability of the yarn to maintain its original performance and structure under friction or wear. Yarn with good wear resistance is suitable for occasions with higher requirements. Specifically, the wear resistance of the yarn is characterized by the number of wear resistances. Yarn fuzzing is prone to occur during friction. The number of frictions when adhesion occurs for the second time is selected as the said number of wear resistances.

[0037] Optionally, the breaking strength and elongation of the yarn change with the extension of heating time and the increase of heating temperature. When the heating temperature increases, the reinforcement of the hot-melt yarn first shows an upward trend. When the temperature rises to an optimal temperature, if the temperature continues to rise, the yarn reinforcement rate decreases. If the heating temperature is further increased, the reinforcement rate will become negative, that is, the yarn breaking strength decreases. At the same time, the yarn elongation at break tends to decrease with the increase of temperature. Preferably, when hot-melt blending is performed with polyester-cotton blended yarn as the core material and 30% low-melting-point polyester as the skin material, the optimal hot-melt temperature is 150°C.

[0038] Specifically, when the heating temperature is too high and gradually approaches the melting point of the core layer material, the structure of the fibers of the core layer material may change, causing fiber damage, increasing the number of damaged fibers, and causing the strength of the yarn to decrease. For example, after long-term high-temperature heating, cotton fibers will show signs of carbonization.

[0039] In addition, when the high temperature is used for a long time, the low melting point cortical material is fully melted, the fiber bonding area is increased, and the molten cortical material becomes brittle and hard after cooling, which reduces the elongation of the yarn.

[0040] In some implementations, the expression of the fusion yarn process evaluation function is as follows: ; in, Characterizing the first historical process indicator parameters The first historical process index, and and Respectively characterize the first historical process index parameters The energy consumption, efficiency and quality of fused yarn production. and and Respectively represent and and The weight coefficient of , and and and Respectively characterize the first historical process index parameters Heating temperature, heating time, curing time and yarn waste rate, and and and are the first coefficient, the second coefficient, the third coefficient and the fourth coefficient respectively, and , .

[0041] Optionally, the independent variables of the fusion yarn process evaluation function also include the fusion yarn manufacturing energy consumption, fusion yarn manufacturing efficiency and fusion yarn quality corresponding to the historical process index parameters, wherein the fusion yarn manufacturing energy consumption Heating temperature , Heating time Influence, heating temperature Heating time The influence on the energy consumption of fusion yarn manufacturing is characterized by the first coefficient a and the second coefficient b. Heating time And curing time The third and fourth coefficients reflect the heating time. And curing time Efficiency of melt-bonded yarn production The mapping relationship.

[0042] Optionally, the manufacturing waste yarn rate is obtained by comparing the predetermined quality inspection index with the output quality inspection index value corresponding to the historical process index parameter, and performing statistical calculation.

[0043] Further, in some embodiments, the first historical manufacturing index parameter and the first historical quality inspection index parameter are analyzed according to the fusion yarn process evaluation function to obtain the first historical process index, which also includes: Obtain a second historical weaving record, wherein the second historical weaving record refers to a record of weaving a second historical fused yarn obtained from a second historical adjustment record, and the second historical adjustment record is any sequential adjustment record in the multiple historical adjustment records that is different from the first historical adjustment record; extract the second historical weaving waste yarn rate in the second historical weaving record, and combine it with the second historical quality inspection index parameter in the second historical adjustment record to form an intelligent training data group; based on the principle of neural network, supervised learning and verification are performed on the intelligent training data group to obtain an intelligent prediction model; the first historical quality inspection index parameter is used as input information of the intelligent prediction model to obtain an output result, and the output result includes a first historical weaving waste yarn rate, wherein the first historical weaving waste yarn rate refers to a waste yarn rate record when weaving the first historical fused yarn obtained from the first historical adjustment record, and the first historical weaving waste yarn rate is used to characterize the quality of the first historical fused yarn.

[0044] Specifically, based on the same method principle as that of obtaining the first historical adjustment record, random extraction is performed among multiple historical adjustment records except the first historical adjustment record to obtain the second historical adjustment record, and the second historical adjustment record is a differentiated record of the first historical adjustment record.

[0045] Optionally, the waste yarn rate in the second historical weaving record is combined with the quality inspection parameter in the second historical adjustment record to form an intelligent training data set. The intelligent training data set is used to train the neural network model. Then, the neural network model is supervised and tested using the intelligent training data set to obtain an intelligent prediction model, which is used to predict the waste yarn rate of given quality inspection parameters.

[0046] Furthermore, the first historical quality inspection index parameter is used as input information and input into the intelligent prediction model for analysis and prediction to obtain the first historical weaving waste yarn rate. The historical weaving waste yarn rate quantitatively represents the quality of the fused yarn produced corresponding to the historical adjustment record.

[0047] Through the above process, historical data is used to predict the possible results of new production parameters, which helps to optimize the production process, improve product quality and reduce waste yarn rate.

[0048] When the first historical process index meets the predetermined process index limit, the first historical process indicator parameter is used as a target process adjustment benchmark.

[0049] Optionally, if the first historical process index meets the predetermined process index limit, it means that the first historical adjustment process scheme of the first historical fusion yarn manufacturing record has a better adjustment effect. In other words, adaptive control based on the first historical adjustment process scheme can meet the fusion yarn processing requirements under the target scenario.

[0050] Optionally, the historical adjustment records are traversed and evaluated through the fusion yarn process evaluation function to obtain multiple historical process indexes, and then based on statistical methods such as regression analysis and covariance analysis, a model or functional relationship is found according to the historical process index and the corresponding waste yarn rate, so as to predict the process index corresponding to the target waste yarn rate, obtain the process index corresponding to the target waste yarn rate, and set it as the predetermined process index limit.

[0051] Based on the predetermined process index, dynamic process monitoring is performed on the target fusion-bonded yarn to obtain target real-time process index parameters.

[0052] In some implementations, the predetermined process parameters include heating temperature, heating time, extrusion speed, and extrusion pressure.

[0053] Specifically, according to the predetermined process indicators, the production process of the target fused yarn is monitored in real time through various sensors and data acquisition equipment. For example, temperature sensors, speed sensors, pressure sensors and other feasible acquisition equipment are obtained. Through monitoring, process indicator parameters such as heating temperature, heating time, extrusion speed and extrusion pressure can be obtained in real time. In this way, the state of the production process is evaluated, which is convenient for subsequent adaptive control.

[0054] The target real-time process indicator parameter is compared with the first historical process indicator parameter to obtain a first comparison result.

[0055] Specifically, if the real-time process index parameters deviate from the predetermined process index limit, the production parameters can be adjusted immediately to ensure product quality and production efficiency. The flexibility and efficiency of the production process can be greatly improved through dynamic monitoring and real-time adjustment.

[0056] In some embodiments, comparing the target real-time process indicator parameter with the first historical process indicator parameter to obtain a first comparison result includes: Extract the first predetermined process indicator from the predetermined process indicators; traverse the first predetermined process indicator in the target real-time process indicator parameters and the first historical process indicator parameters in turn to obtain the first target real-time parameter and the first historical parameter respectively; and form the first comparison result according to the first comparison deviation between the first target real-time parameter and the first historical parameter.

[0057] Specifically, compare the target real-time process indicator parameters with the historical process indicator parameters to help understand whether the production process is proceeding as expected and whether adjustments are needed. First, extract the first predetermined process indicator from the predetermined process indicators. The first predetermined process indicator can be any one of the heating temperature, heating time, extrusion speed or extrusion pressure. Then, in the target real-time process indicator parameters and the first historical process indicator parameters, traverse the first predetermined process indicator in turn to obtain the first target real-time parameters and the first historical parameters. Then, based on the values ​​of the first target real-time parameters and the first historical parameters, calculate the first comparison deviation, wherein the first comparison deviation includes the absolute value or relative value of the deviation. Finally, based on the first comparison deviation, form a first comparison result for further analysis and decision-making, wherein the first comparison result includes multiple comparison deviations corresponding to the predetermined process indicators.

[0058] When the first comparison result reaches a predetermined comparison deviation, an adaptive adjustment instruction is issued, and process parameters of the target fused yarn are adjusted based on the adaptive adjustment instruction.

[0059] Optionally, when there is a comparison deviation in the first comparison result that is greater than a preset deviation constraint, i.e., a predetermined comparison deviation, an adaptive adjustment instruction is generated based on the direction and size of the comparison deviation, and then the adaptive adjustment instruction is transmitted to the control program and components of the target scene or target production line to perform feedback adjustment of the process parameters.

[0060] For example, the PLC controls the frequency converter through a program to adjust the speed and torque of the motor, thereby adjusting the extrusion speed and extrusion pressure; a temperature closed-loop control system is used for feedback adjustment to change the heating power of the heater to ensure precise control of the heating temperature; the heating time is adjusted by adjusting the extrusion speed or changing the length of the heating area.

[0061] In summary, the method for adaptively adjusting process parameters of fusion-bonding yarn provided by the present invention has the following technical effects: By obtaining the historical melting yarn process adjustment records, including multiple historical adjustment records; extracting the first historical adjustment record from the multiple historical adjustment records, including the first historical adjustment process scheme, the first historical melting yarn manufacturing record and the first historical melting yarn quality inspection information; introducing the melting yarn process evaluation function, analyzing the first historical melting yarn manufacturing record and the first historical melting yarn quality inspection information, and obtaining the first historical process index, the index is used to quantitatively evaluate the first historical process index parameter in the first historical adjustment process scheme extracted based on the predetermined process index traversal; when the first historical process index meets the predetermined process index limit, the first historical process index parameter is used as the target process adjustment benchmark; based on the predetermined process index, the target melting yarn is dynamically monitored to obtain the target real-time process index parameter; the target real-time process index parameter is compared with the first historical process index parameter to obtain the first comparison result; when the first comparison result reaches the predetermined comparison deviation, an adaptive adjustment instruction is issued, and the process parameters of the target melting yarn are adjusted based on the instruction. Thus, the technical effect of improving the adjustment efficiency and improving the product quality is achieved.

[0062] It should be understood that the embodiments disclosed in the present invention and the above description can enable those skilled in the art to use the present invention to implement the present invention. At the same time, the present invention is not limited to the above-mentioned embodiments. It should be understood that those skilled in the art can still modify the technical solutions recorded in the above-mentioned embodiments, or replace some of the technical features therein by equivalents; and these modifications or replacements do not make the essence of the corresponding technical solutions deviate from the spirit and scope of the technical solutions of the embodiments of the present invention, and should be included in the protection scope of the present invention.

Claims

1. A method for adaptively adjusting process parameters of melt-bonded yarn, characterized in that: include: Acquire historical fusion yarn process adjustment records, wherein the historical fusion yarn process adjustment records include multiple historical adjustment records; Extracting a first historical adjustment record from the multiple historical adjustment records, wherein the first historical adjustment record includes a first historical adjustment process scheme, a first historical fused yarn manufacturing record, and first historical fused yarn quality inspection information; Introducing a fusion yarn process evaluation function to analyze the first historical fusion yarn manufacturing record and the first historical fusion yarn quality inspection information to obtain a first historical process index, wherein the first historical process index is used to quantitatively evaluate the first historical process indicator parameter in the first historical adjustment process scheme extracted based on the predetermined process indicator traversal; When the first historical process index meets the predetermined process index limit, the first historical process index parameter is used as a target process adjustment benchmark; Based on the predetermined process index, dynamic process monitoring is performed on the target fused yarn to obtain target real-time process index parameters; Comparing the target real-time process indicator parameter with the first historical process indicator parameter to obtain a first comparison result; When the first comparison result reaches a predetermined comparison deviation, an adaptive adjustment instruction is issued, and process parameters of the target fused yarn are adjusted based on the adaptive adjustment instruction.

2. The method for adaptively adjusting process parameters of melt-bonded yarn according to claim 1, characterized in that: The fusion yarn process evaluation function is introduced to analyze the first historical fusion yarn manufacturing record and the first historical fusion yarn quality inspection information to obtain the first historical process index, including: Reading a predetermined manufacturing index, and traversing and extracting the first historical fusion yarn manufacturing record based on the predetermined manufacturing index to obtain a first historical manufacturing index parameter; Reading a predetermined quality inspection index, and traversing and extracting the first historical fused yarn quality inspection information based on the predetermined quality inspection index to obtain a first historical quality inspection index parameter; The first historical process index is obtained by analyzing the first historical manufacturing index parameter and the first historical quality inspection index parameter according to the fusion yarn process evaluation function.

3. The method for adaptively adjusting process parameters of melt-bonded yarn according to claim 2, characterized in that: The predetermined manufacturing indexes at least include heating temperature, heating time and curing time.

4. The method for adaptively adjusting process parameters of melt-bonded yarn according to claim 2, characterized in that: The predetermined quality inspection indexes at least include the prepreg yarn glue content, yarn uniformity, yarn elongation, yarn strength and yarn wear resistance.

5. The method for adaptively adjusting process parameters of melt-bonded yarn according to claim 2, characterized in that: The first historical process index is obtained by analyzing the first historical manufacturing index parameter and the first historical quality inspection index parameter according to the fusion yarn process evaluation function, and the ... and the first historical quality inspection index is obtained by analyzing the first historical quality inspection index and the first historical process index is obtained by analyzing the first historical quality inspection index and the first historical process index is obtained by analyzing the first Obtaining a second historical weaving record, wherein the second historical weaving record refers to a record of weaving a second historical fused yarn obtained from a second historical adjustment record, and the second historical adjustment record is any sequential adjustment record among the multiple historical adjustment records that is different from the first historical adjustment record; Extracting the second historical weaving waste yarn rate in the second historical weaving record, and combining it with the second historical quality inspection index parameter in the second historical adjustment record to form an intelligent training data group; Based on the principle of neural network, supervised learning and testing are performed on the intelligent training data group to obtain an intelligent prediction model; The first historical quality inspection index parameter is used as input information of the intelligent prediction model to obtain an output result, wherein the output result includes a first historical weaving waste yarn rate, wherein the first historical weaving waste yarn rate refers to a waste yarn rate record when weaving the first historical fused yarn obtained by the first historical adjustment record, and the first historical weaving waste yarn rate is used to characterize the quality of the first historical fused yarn.

6. The method for adaptively adjusting process parameters of melt-bonded yarn according to claim 5, characterized in that: The expression of the fusion yarn process evaluation function is as follows: ; in, Characterizing the first historical process indicator parameters The first historical process index, and and Respectively characterize the first historical process index parameters The energy consumption, efficiency and quality of fused yarn production. and and Respectively represent and and The weight coefficient of , and and and Respectively characterize the first historical process index parameters Heating temperature, heating time, curing time and yarn waste rate, and and and are the first coefficient, the second coefficient, the third coefficient and the fourth coefficient respectively, and , .

7. The method for adaptively adjusting process parameters of melt-bonded yarn according to claim 1, characterized in that: The predetermined process parameters include heating temperature, heating time, extrusion speed and extrusion pressure.

8. The method for adaptively adjusting process parameters of melt-bonded yarn according to claim 1, characterized in that: Comparing the target real-time process indicator parameter with the first historical process indicator parameter to obtain a first comparison result, including: Extracting a first predetermined process indicator from the predetermined process indicators; The first predetermined process indicator is traversed in the target real-time process indicator parameter and the first historical process indicator parameter in turn to obtain a first target real-time parameter and a first historical parameter respectively; The first comparison result is established according to a first comparison deviation between the first target real-time parameter and the first historical parameter.