Piston ring coating

By applying chromium coating, DLC layer and phosphate layer on the piston ring, the challenges brought about by DLC coating run-in are solved, and the wear and heat resistance of the piston ring is improved and its service life is extended.

CN118911864APending Publication Date: 2024-11-08MAHLE INT GMBH
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202410560507.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2024-04-10
Filing Date
2024-05-08
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

Existing piston rings are challenged during initial operation due to run-in of DLC coatings and the DLC can be overheated and damaged, resulting in wear and chipping in the power cylinder assembly.

Method used

Using a piston ring made of metal material, the thickness of the cladding is optimized by applying a chromium coating on the outer and inner contact surfaces and depositing a diamond-like carbon (DLC) layer on it, combining a phosphate layer and a chromium intermediate layer. and flatness to improve wear and heat resistance.

Benefits of technology

It effectively improves the wear resistance and heat resistance of the piston ring, reduces the running-in problem during the initial operation, and extends the service life of the piston ring.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118911864A_ABST
    Figure CN118911864A_ABST
Patent Text Reader

Abstract

A piston ring and a method of forming the same, the piston ring including: a base portion formed of a metal material; outer and inner contact surfaces extending between a first face of the piston ring and a second face opposite the first face; a chromium coating on the second face, the outer contact surface, and the inner contact surface; a diamond-like carbon (DLC) layer disposed over the chromium coating layer on the outer contact surface; and a phosphate layer on the first side.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] CROSS-REFERENCE TO RELATED APPLICATIONS

[0002] This application claims priority to and the benefit of U.S. Provisional Application No. 63 / 464,675, filed on May 8, 2023, the contents of which are hereby incorporated by reference in their entirety. Technical Field

[0003] An exemplary technical field of the present disclosure may relate to, for example, a piston and a piston ring, and in particular, to a coating of a piston ring. Background Art

[0004] The power cylinder assembly of an internal combustion engine typically includes a reciprocating piston disposed within a cylindrical cavity of the engine block. One end of the cylindrical cavity is closed, while the other end of the cylindrical cavity is open. The closed end of the cylindrical cavity and the upper portion or top of the piston define a combustion chamber. The open end of the cylindrical cavity allows for oscillating motion of a connecting rod, which connects the lower portion of the piston to a crankshaft, which is partially submerged in an oil sump. The crankshaft converts the linear motion of the piston (caused by the combustion of fuel in the combustion chamber) into rotational motion.

[0005] The power cylinder assembly typically includes one or more piston rings and a cylindrical sleeve or cylinder liner that is disposed within the engine block and forms the side walls of the cylindrical cavity. The piston rings are disposed in grooves formed in the lateral walls of the piston and extend outwardly from the piston into the annular space defined by the piston wall and the cylinder liner. The piston rings bear on the cylinder liner during movement of the piston within the cylindrical cavity. The piston rings have at least two functions. First, they prevent gases from flowing from the combustion chamber through the annular space between the piston and the cylinder liner into the oil pan. Second, they minimize the flow of oil from the oil pan into the combustion chamber.

[0006] Piston rings typically must withstand the extreme temperatures and pressures generated by the combustion cycle. The outer surface of the piston ring that bears against the cylinder liner or bore surface typically includes a hardfacing coating or is otherwise treated to produce a hardened outer surface that is more durable than an untreated surface.

[0007] Thus, some known power cylinder assemblies include a piston ring having a chrome-plated lateral side, i.e., the side of the ring positioned to abut the piston ring groove surface, with diamond-like carbon (DLC) coated on the chrome. The chrome is positioned on the lower surface of the piston ring, while the DLC is positioned on the outer radial surface of the piston ring.

[0008] However, DLC has the ability to bond to faces above chrome, and often does so, particularly at the corner areas of the piston ring and where the underside meets the outer radius. Therefore, running-in of the piston ring (during early operation of a newly built engine) can be challenging, and the DLC can overheat and become damaged, with the DLC running face chipping during this initial operation.

[0009] Therefore, there is a need for improved piston ring design. Summary of the invention

[0010] The present disclosure relates to a piston ring and a method of forming a piston ring.

[0011] According to a first aspect, a piston ring comprises: a base portion formed of a metallic material; an outer contact surface and an inner contact surface extending between a first face of the piston ring and a second face opposite to the first face; a chrome coating on the inner contact surface, the outer contact surface and the second face; and a diamond-like carbon (DLC) layer positioned on the chrome coating on the outer contact surface.

[0012] According to one embodiment, a phosphate layer is provided on the first face of the piston ring. The phosphate layer may be applied directly to the metal material of the base portion. The phosphate layer may have a thickness of ≤3 μm. The phosphate layer may overlap with the DLC portion at an upper outer corner region of the base portion, and may overlap with the chrome coating portion at an upper inner corner region of the base portion. The phosphate layer may have a gradually decreasing thickness along the upper outer corner region and the upper inner corner region.

[0013] Additionally or alternatively, the DLC may have an approximately constant thickness along the outer contact surface and a gradually decreasing thickness at the lower outer corner region of the base portion and the upper outer corner region of the base portion. At least in the portion of approximately constant thickness, the DLC may have a thickness of 2 μm to 25 μm.

[0014] Additionally or alternatively, the chrome coating may have an approximately constant thickness along the outer contact surface, the lower outer corner region, the second face, the lower inner corner region of the base portion, and the inner contact surface. In addition, the chrome coating may have a gradually decreasing thickness at the upper outer corner region and the upper inner corner region.

[0015] The chromium coating may have a thickness between 10 μm and 20 μm, with a thickness variation of 5 μm or less. The chromium coating may have a flatness of 2 μm or less along at least the second face and the inner contact surface.

[0016] Additionally or alternatively, a Physical Vapor Deposition (PVD) chromium intermediate layer may be interposed between the DLC and the chromium coating along the outer contact surface. The chromium intermediate layer may have a thickness less than or equal to 1 μm.

[0017] Additionally or alternatively, a polymer layer may be provided covering the DLC.

[0018] According to a second aspect, a method for forming a piston ring includes providing a base portion formed of a metal material, the base portion having a first surface and a second surface opposite to the first surface; applying a chromium coating on the first surface, the second surface, the outer contact surface and the inner contact surface; and depositing a diamond-like carbon (DLC) layer on the chromium coating on the outer contact surface.

[0019] According to one embodiment, the method includes trapezoidally grinding the second face to planarize the outer surface of the chrome coating to a straightness variation of 2 μm or less.

[0020] The method may include brushing the second surface after the trapezoidal grinding to remove nodules from the chrome coating.

[0021] Additionally or alternatively, the method may include trapezoidal grinding the first face to remove substantially all of the chrome coating from the first face to expose the base portion and roughen the outer surface of the base portion; and depositing a phosphate layer on the first face. The phosphate layer may be applied directly to the metallic material of the base portion by phosphating. Furthermore, the phosphate layer may at least partially cover the DLC at the upper corner region of the base portion and partially overlap the chrome coating at the upper inner corner region of the base portion.

[0022] According to one embodiment, the method comprises trapezoidal grinding of the second face before applying the chrome coating.

[0023] Additionally or alternatively, the method may include outer diameter (OD) grinding the chrome coating along the outer contact surface prior to depositing the DLC; gap grinding the chrome coating at the piston ring gap prior to depositing the DLC; inner diameter (ID) brush grinding the chrome coating along the inner contact surface after gap grinding and prior to depositing the DLC; and gap finish grinding the chrome coating at the piston ring gap after depositing the DLC and prior to trapezoidal grinding the first face. A first or initial gap grinding may be performed prior to applying the chrome coating.

[0024] According to one embodiment, the trapezoidal grinding is performed after the OD grinding and before the gap grinding. Alternatively, the trapezoidal grinding may be performed after the gap finishing grinding.

[0025] According to one embodiment, the method comprises depositing a chromium intermediate layer on the chromium coating along the outer contact surface, such that the chromium intermediate layer is between the chromium coating and the DLC. The chromium intermediate layer may be deposited via physical vapor deposition, while the chromium coating may be electrochemically applied. The chromium intermediate layer may be deposited in the same step as the DLC. Additionally or alternatively, the chromium intermediate layer may be deposited at low temperature, for example, at a temperature of about 200° C. or less.

[0026] According to another embodiment, the polymer layer is deposited on the outer surface of the DLC layer.

[0027] Various other features and advantages will become apparent from the following detailed description and accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Referring now to the drawings, illustrative examples are shown in detail. Although the drawings represent exemplary illustrations described herein, the drawings are not necessarily drawn to scale, and certain features may be exaggerated to better illustrate and explain the innovative aspects of the exemplary illustrations. In addition, the exemplary illustrations described herein are not intended to be exhaustive or otherwise limited or restricted to the precise forms and configurations shown in the drawings and disclosed in the following detailed description. Exemplary illustrations of the present invention are described in detail with reference to the drawings as follows:

[0029] Figure 1 is a view of an exemplary piston assembly;

[0030] Figure 2A yes Figure 1 a view of a ring of a piston assembly;

[0031] Figure 2B is a cross-sectional view of a piston ring in a groove of a piston;

[0032] Figure 3A is a cross-sectional view of a piston ring according to an example;

[0033] Figure 3B yes Figure 3A A close-up view of the piston ring;

[0034] Figure 4 Shows the production according to Figure 3A The method steps of:

[0035] Figure 5 is a cross-sectional view of a piston ring according to another example;

[0036] Fig. 6A yes Figure 5 A close-up view of the piston ring;

[0037] Figure 6B yes Figure 5 A close-up view of the piston ring;

[0038] Figure 6C yes Figure 5 A close-up view of the piston ring;

[0039] Figure 7 Shown for production according to Figure 5 A flowchart of an exemplary method of a piston ring;

[0040] Figure 8 The steps of a method according to the present disclosure are shown;

[0041] Fig. 9 The steps of a method according to the present disclosure are shown;

[0042] Fig.10 The steps of a method according to the present disclosure are shown;

[0043] Fig.11 The steps of a method according to the present disclosure are shown; and

[0044] Fig.12 A cross-sectional view of a piston ring according to another example is shown. DETAILED DESCRIPTION

[0045] References in the specification to "exemplary illustrations," "examples," or similar language mean that a particular feature, structure, or characteristic described in conjunction with the exemplary method is included in at least one illustration. The phrase "in the illustrations" or similar types of language that appear in various places in the specification do not necessarily all refer to the same illustration or example.

[0046] Various exemplary illustrations are provided herein, which include a piston assembly having two or more rings that, when positioned in a groove of the piston assembly, provide various functions during piston operation. In one example, the piston assembly can have two rings, including a combustion ring and a scraper ring. The combustion ring typically blocks most of the combustion gases from passing through the piston assembly of an internal combustion engine, so that little or no gas is passed to the crank. The scraper ring provides a scraping motion during the downward movement of the piston assembly and provides a sliding motion during the upward movement of the piston assembly.

[0047] In another example, a three-ring piston assembly includes a combustion ring, an oil control ring, and a scraper ring positioned between the combustion ring and the oil control ring. The third or lower oil control ring controls the supply of oil to the bushing while lubricating the piston skirt and other rings. In some exemplary methods, the piston assembly may include a piston head having a first compression ring groove and a second compression ring groove, a compression ring in the groove, an oil control ring groove, and an oil control ring assembly.

[0048] According to various exemplary illustrations, the piston ring may include a base portion formed of a metallic material, an outer (radial) contact surface and an inner (radial) contact surface extending between a first face or surface of the piston ring and a second face or surface opposite the first face. A chromium coating is disposed on the inner contact surface, the outer contact surface, and the second face. A phosphate layer may be disposed on the first face. A diamond-like carbon coating (DLC) is deposited on the radially outermost surface above the chromium coating. A chromium intermediate layer may be inserted between the DLC and the chromium coating.

[0049] DLC is a class of amorphous carbon materials that exhibit properties such as very low coefficient of friction, high hardness, excellent wear resistance and very low wear. DLC coatings can be deposited using a cathodic arc physical vapor deposition (PVD) process. The cathodic arc PVD coating process involves using a cathodic arc source or a cathodic arc target (negatively charged), such as graphite or other suitable carbon materials, and depositing a thin film on a substrate or an anode (positively charged). The target material can be placed in a vacuum chamber together with the substrate to be coated or filled with an inert gas such as argon. Once the chamber is evacuated, a high voltage pulse is applied to the target material. The voltage pulse causes an arc discharge, which evaporates the target material. The evaporated material then condenses onto the substrate to form a thin film of the DLC coating. The DLC coating formed is amorphous and can include a combination of sp3 hybridized carbon atoms and fillers (e.g., sp2 carbon atoms), up to 3% hydrogen, and trace amounts of other metals to give the material desired properties. According to one embodiment, the DLC coating used herein may exhibit an sp ranging from 0.42 to 2.33. 3 With sp 2and a Rmr (0.2-0.5) distribution of greater than at least 25% and / or a Rmr (0.3-0.5) distribution of greater than at least 50%, as described in commonly owned patent application No. 15 / 289,097 filed on October 7, 2016, now U.S. Patent Application No. 10400895B2, the contents of which are hereby incorporated by reference in their entirety. According to one embodiment, the DLC coating used herein may also exhibit the following characteristics, wherein the DLC coating is on top of the intermediate coating, wherein the DLC coating includes a first DLC layer having a first hardness and a first porosity, and a second DLC layer having a second hardness lower than the first hardness and a second porosity greater than the first porosity, as described in commonly owned patent application No. 17 / 488,942 filed on September 29, 2021, now U.S. Publication 2022 / 0090680A1, claiming priority, the contents of which are hereby incorporated by reference in their entirety.

[0050] Typically, the wear environment between the lateral surface of a piston ring, such as the lower radially extending surface, and the receiving ring groove is different than the typical wear environment of the generally vertical radial outermost surface of the ring and the mating cast iron surface of the cylinder liner. For example, the material properties of the machined steel piston ring groove that engages the machined piston ring provide one difference. A second difference relates to the reciprocating vertical movement of the piston ring relative to the groove surface as the piston moves up and down. In addition, the ring flexes radially inwardly and radially outwardly, rubbing the piston ring groove surface during piston operation. Therefore, a method of forming a piston ring is disclosed, the method comprising providing a base portion formed of a metallic material, applying DLC ​​onto a radially outward surface, and applying a chromium layer to a lateral surface and / or an inner diameter (ID) surface of the base portion, the lateral surface and the ID surface being configured to enable surface docking with the piston ring groove.

[0051] refer to Figure 1 , an exemplary piston assembly 100 is shown. The piston assembly 100 includes a piston head 102, which includes an upper compression ring 104 positioned in an upper compression ring groove 106 and an oil control ring 108 positioned in a lower compression ring groove 110. The piston head 102 also includes a scraper ring or oil scraper ring 112 positioned in an intermediate groove 114. The rings 104, 108 and 112 seal against the cylinder bore surface during the reciprocating motion of the piston assembly 100 in the cylinder bore. The piston head 102 moves in a first or upward direction 116 during the upstroke phase of the piston assembly 100, and moves in a second or downward direction 118 during the downstroke phase of the piston assembly 100.

[0052] Reference now Figure 2A, a piston assembly 200 for an internal combustion engine includes a cylinder bore 202 having a central axis 204 (e.g., a reciprocating axis) and a cylinder wall 206 equidistant from the central axis 204. The piston assembly 200 includes a radial axis 208 orthogonal to the central axis 204. The piston assembly 200 includes a piston 210 having two or more ring grooves, the piston 210 including a combustion ring and groove 212, an oil control ring and groove 214, and an oil scraper ring 216 positioned in an oil scraper ring groove 218.

[0053] The cross-sectional details of the oil scraper ring 216 are shown in Figure 2B Reference Figure 2B The groove 218 is formed between the upper groove surface 220 and the lower groove surface 222. The oil scraper ring 216 is positioned in the groove 218 so that when the piston 210 moves in the downward direction 118 (corresponding to Figure 1 When the piston 210 moves in the upward direction 116, the scraper ring 216 is constrained against the upper groove surface 220, and when the piston 210 moves in the upward direction 116, the scraper ring 216 is constrained against the lower groove surface 222. In an exemplary method as shown herein, the scraper ring 216 is positioned in the groove 218 between the groove 212 and the groove 214.

[0054] Typically, when there are three ring grooves, the ring in groove 212 is typically a combustion ring that is primarily used to prevent combustion gases from passing over the piston 210. The ring in groove 214 is typically used primarily as an oil control ring that controls the distribution of oil for lubrication purposes. Therefore, if common convention is followed, the ring 216 can be placed in the middle groove 218. In addition, although the scraper ring 216 is shown in a three-ring design, it is contemplated that the scraper ring 216 can also be implemented in other multi-groove designs, such as a two-ring groove arrangement with only a combustion ring and a scraper ring 216, in which case the scraper ring 216 also serves as an oil control ring. In addition, the scraper ring is shown in a slightly non-rectangular arrangement, in which the surface 224 is non-orthogonally positioned relative to the lower surface 226 and the upper surface 232. A corner 242 is formed between the surface 224 and the surface 226.

[0055] Any one or all three of the grooves 212, 214, and 218 may benefit from rings made in accordance with the present disclosure. Figure 2A Any or all of the piston rings of may include the features of the piston rings and their coverings described herein.

[0056] Figure 3A is a cross-sectional view of a piston ring 300 according to the present invention, Figure 3B yes Figure 3AA close-up view of a corner of a piston ring 300. The piston ring 300 includes a base portion 302 formed of a metal material. The metal material may be composed of steel, for example, carbon steel and / or non-nitrided steel and / or chrome silicon steel wire. The base portion 302 includes an outer contact surface or outer contact surface (hereinafter referred to as outer contact surface) 304 extending between a first face or first side or upper side or upper surface (hereinafter referred to as the first face) 306 and a second face or second side or bottom side or bottom surface (hereinafter referred to as the second face) 308 opposite to the first face 306 of the piston ring 300 with respect to the central axis of the piston ring and / or piston and / or cylinder bore. According to the example shown, the first face 306 is a top surface and the second face 308 is a bottom surface. A corner region 310 is disposed at the intersection of the outer contact surface 304 and the second face 308. The corner region 310 may be a relatively sharp corner having a radius of several hundred μm (or micrometers) to one millimeter or more. A diamond-like carbon (DLC) layer 312 is positioned on the outer contact surface 304. The DLC 312 has an approximately constant thickness on the outer contact surface 304 and has a tapered thickness 318 in the corner region 310, tapering to zero thickness 320 at or beyond the corner region 310 (because the DLC 312 wraps around the corner region 310 and extends to zero thickness 320 with the tapered thickness 318). A chrome coating 314 is formed or positioned on the second face 308, the chrome coating 314 being formed over the tapered thickness 318 of the DLC layer 312, and the chrome coating 314 itself having a tapered thickness 316 in the corner region 310. A phosphate layer 322 may be disposed along the first face 306. The phosphate layer 322 may at least partially overlap or cover the DLC layer 312 in the (upper) corner region in a similar manner as the chrome coating 314 at the (lower) corner region 310 .

[0057] According to the present disclosure, the gradually decreasing thickness 316 layer of the chromium coating 314 is affected by the formation process and electrical and mechanical properties of the DLC and chromium. For example, as an example, the DLC layer 312 is formed by a known process such as ion beam deposition, sputtering, cathode arc, electron beam, laser or RF plasma deposition, and the DLC 312 can be formed according to any known process of the present disclosure. Due to the nature of the formation of the DLC 312, the DLC 312 (as described above) has a generally constant thickness on the outer contact surface 304, but in the corner area, the thickness gradually decreases as shown by the gradually decreasing thickness 318. Therefore, the gradually decreasing thickness 318 of the DLC 312 in the corner area 310 can be due to the nature of the formation method of the DLC, and may not be due to any post-processing (e.g., forming the gradually decreasing thickness). However, the tapered thickness 318 may also be formed by further post-processing, such as grinding or other techniques for removing material in the corner region 310 and around the circumference of the base portion 302 (the base portion 302 represents a circular piston ring as described).

[0058] Once the DLC 312 is formed and has a gradually decreasing thickness 318, a chrome layer is applied to the surface of the piston ring. Figure 3A and Figure 3B , the chromium coating 314 is deposited using an electrochemical process. Typically, such processes depend on the conductive properties of the base material on which the chrome is plated, in this case, base portion 302 represents the base material for the piston ring. However, while DLC is typically considered an electrical insulator, it should be understood that, despite being an insulator, there is some electrical conduction occurring through the DLC, in this case DLC 312. The conductivity of an object like an insulator also depends on the thickness of any layer through which the current is passed.

[0059] Thus, electrical conduction through the DLC, although very limited, is more pronounced in the regions of the tapered thickness 318 of the DLC 312 and around the corner regions 310. During deposition of the chromium coating 314 on the second side 308 of the base portion 302, electrical conduction through the DLC occurs to varying degrees through the tapered thickness 318 of the DLC 312, thereby forming a tapered thickness 316 of the chromium coating 314 above the DLC 312.

[0060] Thus, the piston ring may include: a base portion formed of a metal material; an outer contact surface extending between a first face of the piston ring and a second face opposite to the first face, forming a corner region at the intersection of the outer contact surface and the second face; a diamond-like carbon (DLC) layer positioned on the outer contact surface; and a chrome coating on the second face, the chrome coating being positioned above the DLC layer in the corner region. According to one embodiment, the phosphate layer may be disposed on the first face.

[0061] The DLC has an approximately constant thickness of the DLC on the outer contact surface. The DLC has a gradually decreasing thickness of the DLC in the corner area, which gradually decreases from the approximately constant thickness of the DLC to zero thickness of the DLC at or beyond the corner area. The chromium coating is an approximately constant thickness of the chromium coating on the second side. The chromium coating is an approximately constant thickness of the chromium coating on the second side. The chromium coating has a hardness of at least 8.5 Mohs hardness. DLC is an amorphous carbon material.

[0062] According to one aspect, a method of forming a piston ring includes providing a base portion formed of a metallic material, the base portion having a first side and a second side opposite the first side, an outer contact surface of the base portion extending between the first side and the second side; depositing a diamond-like carbon (DLC) layer on the outer contact surface; and depositing a chromium coating on the second (bottom) side and on the DLC layer in a corner region at the intersection of the outer contact surface and the second side. According to one embodiment, the method may also include applying a phosphate layer on the first (top) side of the base portion.

[0063] In one example, the chromium coating has a hardness of at least 8.5 on the Mohs scale. In one example, the DLC is an amorphous carbon material.

[0064] At a high level, and with reference to Figure 4 , a method of forming a piston ring 400 begins 402 and includes applying DLC ​​to an outer radial surface 404 of the piston ring and applying a chromium layer or a chromium-based layer to a bottom surface 406 of the piston ring such that the chromium coating is positioned over the DLC layer in a corner region between the outer radial surface and the bottom surface.

[0065] Furthermore, although the disclosed method is about Figure 1 and Figure 2A Although described with reference to a ring in the middle groove of the three grooves shown in FIG, it is contemplated that the disclosed method and apparatus may be used with any ring groove where wear occurs due to frictional wear of the ring in the groove, or where improved flatness is desired to better seal the ring with the piston to control blowby of oil and / or combustion gases.

[0066] The method includes depositing DLC ​​with an approximately constant thickness on the outer contact surface. The method includes depositing DLC ​​with a gradually decreasing thickness of the DLC in the corner area, starting from an approximately constant thickness of the DLC, gradually decreasing to zero thickness of the DLC at or beyond the corner area. The method includes depositing a chromium coating with an approximately constant thickness of the chromium coating on the bottom surface. The method includes depositing the chromium coating with a gradually decreasing thickness in the corner area, starting from an approximately constant thickness of the chromium coating, gradually decreasing to zero thickness of the chromium coating at or beyond the corner area. The method includes depositing the DLC layer using a physical vapor deposition (PVD) process.

[0067] Figure 5 is a cross-sectional view of a piston ring 100 according to the present disclosure, and Fig. 6A , Figure 6B and Figure 6C yes Figure 5 A close-up view of the corner of a piston ring 500. The piston ring 500 includes a base portion 502 formed of a metal material, such as steel, such as carbon steel and / or non-nitrided steel and / or chrome silicon steel wire. The base portion 502 includes an outer contact surface 504 extending between a first face 506 (e.g., an upper surface or upper side) of the piston ring 500 and a second face 508 (e.g., a lower surface or lower side) opposite to the first face 506, an upper outer corner region 518 is formed at the intersection of the outer contact surface 504 and the first face 506, and a lower outer corner region 520 is formed at the intersection of the outer contact surface 504 and the second face 508. The base portion 502 includes an inner contact surface 510 extending between a first face 506 and a second face 508 of the piston ring 500, forming a first (upper) inner corner area 522 at the intersection of the inner contact surface 510 and the first face 506, and forming a second (lower) inner corner area 524 at the intersection of the inner contact surface 510 and the second face 508.

[0068] The piston ring 500 includes a chrome coating 514 disposed on one or more of the outer contact surface 504, the second (lower) face 508, and the inner contact surface 510. In the example shown, the chrome coating 514 is disposed on each of the outer contact surface 504, the second (lower) face 508, and the inner contact surface 510. The chrome coating 514 may have a thickness of 10 μm to 20 μm, wherein the thickness variation is ≤ 5 μm. The flatness of the chrome coating at least along the second face 508 and the inner contact surface 510 may be ≤ 2 μm. The DLC 512 is disposed on the chrome coating 514 along the outer contact surface 504, for example, the DLC 512 covers the chrome coating 514 to form an outer sliding layer. The DLC may have a thickness of 2 μm to 25 μm. A chrome intermediate layer 532 may be disposed between the chrome coating 514 and the DLC 512 along the outer contact surface 504 to improve the adhesion between the DLC 512 and the chrome coating 514. The chromium intermediate layer 532 may have a thickness of less than or equal to (≤) 1 μm. The phosphate layer 516 is disposed on the first (upper) face 506 and may be applied directly to the base portion 502 at least in some areas along the first face 506 and may also partially overlap with the DLC 512 in the upper outer corner region 518. The phosphate layer 516 may have a thickness of ≤ 3 μm. The phosphate layer 516 may promote improved wear and lubrication properties and help prevent rust and / or oxidation.

[0069] Fig. 6A , Figure 6B and Figure 6C 5. A close-up view of the lower outer corner region 520, the upper outer corner region 518, and the upper inner corner region 522, respectively. Corner regions 518, 520, 522, 524 can be relatively sharp corners with a radius of several hundred μm to one millimeter or more. The chromium coating 514 can be formed or positioned on the second face 508, the inner contact surface 510, and the outer contact surface 504, and has a substantially constant thickness (e.g., greater than 5 μm, particularly 10-20 μm) on the second face 508, the inner contact surface 510, and the outer contact surface 504. As used herein, the approximately constant thickness of the chromium coating 512 means a thickness variation of less than 5 μm.

[0070] refer to Fig. 6A, the chromium coating 514 may have a substantially constant thickness on the second face 508, and maintain a substantially constant thickness when the chromium coating 514 wraps around the lower outer corner region 520 to the outer contact surface 504. The DLC 512 is disposed on the chromium coating 514 along the outer contact surface 504 and may form an outermost sliding layer. The DLC 512 may have an approximately constant thickness on the outer contact surface 504, and may have a gradually decreasing thickness 602 in the lower outer corner region 520, which gradually decreases to zero thickness 604 at or beyond the lower outer corner region 520 (as the DLC 512 wraps around the lower outer corner region 520 and extends to zero thickness 604 with a gradually decreasing thickness 602). According to one embodiment, a chromium intermediate layer 532 is interposed between the DLC 512 and the chromium coating 514. The chromium intermediate layer 532 may have a thickness of 1 μm or less. The chromium intermediate layer 532 may be formed in a manner similar to the DLC 512 , such as, for example, an approximately constant thickness along the outer contact surface 504 , and a gradually decreasing thickness at the top and bottom outer corner regions 518 , 520 .

[0071] Reference now Figure 6B , the chrome coating 514 may have an approximately constant thickness on the outer contact surface 504, and may have a tapered thickness 606 in the upper outer corner region 518, which tapers to a zero thickness 614 at or beyond the upper outer corner region 518 (as the chrome coating 514 wraps around the upper outer corner region 518 and extends to the zero thickness 614 with the tapered thickness 606). The DLC 512 wraps around the chrome coating 514 on the outer contact surface 504 with an approximately constant thickness. The DLC 512 may then have a tapered thickness 608 in the upper outer corner region 518, which tapers to a zero thickness 616 at or beyond the upper outer corner region 518 (as the DLC 512 wraps around the upper outer corner region 518 and extends to the zero thickness 616 with the tapered thickness 608). The phosphate layer 516 is disposed along the first (upper) face 506 and may have an approximately constant thickness along the first face 506 and a tapered thickness 610 in the upper outer corner region 518, tapering to zero thickness 612 at or beyond the upper outer corner region 518 (as the phosphate layer 516 wraps around the upper outer corner region 518 and extends to zero thickness 612 with the tapered thickness 610). Thus, the phosphate layer 516 may partially overlap or cover the DLC 512 in the upper outer corner region 518. According to one embodiment, the phosphate layer 516 has a thickness of 3 μm or less.

[0072] Reference now Figure 6C, the chromium coating 514 may have an approximately constant thickness on the inner contact surface 510 and have a gradually decreasing thickness 620 in the upper inner corner region 522, gradually decreasing to a zero thickness 624 at or beyond the upper inner corner region 522 (as the chromium coating 514 wraps around the upper inner corner region 522 and extends to the zero thickness 624 with the gradually decreasing thickness 620). The phosphate layer 516 may have an approximately constant thickness on the first face 506 and have a gradually decreasing thickness 618 in the upper inner corner region 522, gradually decreasing to a zero thickness 622 at or beyond the upper inner corner region 522 (as the phosphate layer 516 wraps around the upper inner corner region 522 and extends to the zero thickness 624 with the gradually decreasing thickness 618). Therefore, the phosphate layer 516 may overlap the chromium coating 514 at least partially in the upper inner corner region 522.

[0073] like Figure 5 As shown, the chrome coating 512 may have an approximately constant thickness along the second (lower) face 508 , the lower inner corner region 524 , and the inner contact surface 510 , and then gradually decrease in thickness 620 to zero thickness 624 in the upper inner corner region 522 .

[0074] Without wishing to be bound by theory, the chromium coating 514 having a tapered thickness 606 in the upper outer corner region 518 may be affected by the formation process and electrical and mechanical properties of the DLC and chromium. For example, the DLC 512 may be formed by known processes such as physical vapor deposition (PVD) including ion beam deposition, sputtering, cathodic arc, electron beam, laser, or RF plasma deposition. Due to the nature of the formation of the DLC 512, the DLC 512 (as described above) generally has a constant thickness on the outer contact surface 504, but the thickness gradually decreases in the upper outer corner region 518 and the lower outer corner region 520 as shown by the tapered thickness 608 and the tapered thickness 602, respectively. Thus, according to the present disclosure, the gradually decreasing thickness 608 of the DLC 512 in the upper outer corner region 518 and the gradually decreasing thickness 602 of the DLC 512 in the lower outer corner region 520 are due to the nature of the manner in which the DLC 512 is formed, and may not be due to any post-processing (e.g., forming the gradually decreasing thickness). However, according to the present disclosure, the gradually decreasing thicknesses 608 and 602 may also be formed by further post-processing, such as grinding or other techniques for removing material in the upper outer corner region 518 and the lower outer corner region 520 and around the circumference of the base portion 502 (the base portion 502 represents the described circular piston ring).

[0075] An electrochemical process (eg, electroplating) may be used to deposit the chrome coating 514. Typically, such a process relies on the conductive properties of the base material upon which the chrome is plated, in this case, base portion 502 representing the base material for the piston ring.

[0076] refer to Figure 7 , a method of forming a piston ring 700 according to an example is shown. At block 702, a metal base portion is provided. At block 704, the outer diameter is formed to a preferred profile of the piston ring. A chromium coating is electrochemically applied 706 to the periphery of the base portion, including a first face, a second face, an outer contact surface, and an inner contact surface. A chromium intermediate layer is applied 708 to the outer contact surface above the chromium coating. The chromium intermediate layer (also referred to as a chromium punch layer) can be applied at low temperatures (e.g., about 200° C.) by a PVD process to prevent the hardness of the chromium coating from decreasing. The chromium intermediate layer can have a thickness of about 1 μm or less and can generally be softer than the chromium coating to help provide adhesion and running-in characteristics. At block 710, DLC is then applied (e.g., via PVD) to the outer contact surface so that the DLC layer is positioned above the chromium intermediate layer and the chromium coating. Before the phosphate layer is applied 712 to the first face, the first face is treated by grinding or another technique to remove the chromium coating.

[0077] Applying a chrome coating on the second face protects the ring and the bottom groove. The process for manufacturing the piston ring is modified so that the first face is ground after the chrome coating is applied so that the first face can be layered with phosphate. Chromium thickness, which is typically greater than 5 μm, at least in areas of constant thickness (e.g., along the outer contact surface, the second (bottom) face, and the inner contact surface) is notoriously difficult to control in a production environment. Applying a chrome coating on the second face and applying a phosphate on the first face allows the ring to maintain an ideal piston ring clearance in a production setting.

[0078] Figures 8 to 11 Shows Figure 7A further development of method 700 in . In an exemplary method for forming a piston ring, it should be understood that the second face (bottom side) is "keystoned" before being fully chrome plated (e.g., applying a chrome coating). The trapezoid may refer to the shape of a ring in which the first (top) face and the second (bottom) face are wedge-shaped. Keystone grinding or keystoned may refer to the process of grinding a face into a trapezoidal shape, and may also be referred to as side grinding. After the second face is keystoned, chromium is applied to the periphery of a base portion including the first face, the second face, the outer contact surface, and the inner contact surface. A chromium intermediate layer may be applied to the chromium coating along the outer contact surface. DLC is then applied to the outer contact surface above the chromium intermediate layer and / or the chromium coating. Because the thickness of chromium is difficult to control, the first face (top surface) is keystoned after the DLC is applied. The bottom keystone is used to determine how much keystone treatment is required on the top surface to maintain an ideal gap. Once the top surface is keystoned, a phosphate layer is deposited on the top surface. This process ensures the ideal thickness and size of the piston ring. Intermediate gap grinding can take place before or after full chrome plating.

[0079] refer to Figure 8 , shows an exemplary method 800 for producing a piston ring according to an embodiment. The method 800 includes providing a base portion, which may include coiling 802 a base material (e.g., steel), stress relief 804 (e.g., annealing and / or tempering), first gap grinding 806 of the piston ring gap, PIP marking 808 (e.g., marking the top side of the piston ring), first side grinding 810, light grinding 812, forming the base portion 814 by outer diameter (OD) profile grinding and optional chamfering, and OD brush grinding 816.

[0080] After the base portion has been provided by one or more of steps 802-816, a first trapezoidal grinding 818 is performed on the second (bottom) surface of the base portion to shape and / or roughen the second surface. In step 820, chrome is plated at least on the second (bottom) surface and the inner contact surface to form a chrome coating. According to one embodiment, the base portion including the outer contact surface, the inner contact surface, the first (top) surface and the second (bottom) surface is completely chrome plated. The chrome plating is electrochemical and may include at least 3 rotations of the base portion (cathode) during electroplating to ensure appropriate thickness and quality. Next, OD grinding 822 is performed to flatten the chrome coating along the outer contact surface, followed by a second or intermediate gap grinding 824, an inner diameter (ID) brushing 826 and dry sandblasting 828.

[0081] At step 830, DLC is applied via PVD to the outer contact surface over the chrome (plated) coating. Optionally, a chrome interlayer is applied via PVD to the chrome coating in step 830, and then DLC is applied to the chrome interlayer. It should be understood that the chrome interlayer can be applied in a separate step from the DLC, such as after dry blasting 1028 and before applying the DLC coating 1030. After applying the DLC, OD polishing 832 (e.g., diamond paper) is performed on the DLC, followed by a third or gap finish grind 834, and side brushing or trapezoidal brushing is performed on the second (bottom) surface.

[0082] At step 838, a second trapezoidal grind is performed on the first (top) face / side to remove the chrome plating along the first side, exposing the base portion material, and then a phosphate coating is applied via phosphating along the first side at step 840. The piston ring is inspected 842 and the process ends.

[0083] Fig. 9 An exemplary method 900 for producing a piston ring according to another embodiment is shown. Fig. 9 and Figure 8 The difference between the above process is only in the order of the intermediate gap grinding 924 and the OD grinding 922, wherein the intermediate gap grinding 924 occurs before the OD grinding 922, for example, between the OD profile grinding 914 and the OD brush grinding 916, and the OD grinding 922 is performed after the OD brush grinding 916 and before the first side (trapezoidal) grinding of the second (bottom) surface. In other respects, the process is the same as Figure 8 The processes in are the same as indicated by the same figure numerals.

[0084] refer to Fig.10 , shows an exemplary method 1000 for producing a piston ring according to another embodiment. The exemplary method 1000 includes providing a base portion of a piston ring, which may include forming the base portion from a base material (e.g., steel) or coiling 1002 the base material, stress relieving 1004 (e.g., tempering / annealing or other heat treatment at a temperature below its critical temperature for a sufficient time so that the base metal can recrystallize to relieve internal stresses), first gap grinding 1006 (e.g., circumferentially grinding the gap between the first end and the second end of the disc / base portion), PIP marking 1008 (e.g., to mark the top side of the piston ring), first side grinding 1010 grinding the first face and / or the second face (e.g., rough grinding), light grinding 1012, shaping the base portion 1014 by grinding the outer diameter (OD) profile (e.g., outer contact surface) to a desired profile and optional chamfers, and OD brushing 1016.

[0085] At step 1018, the base portion undergoes further shaping via a first trapezoidal grind on the second face or side grinding (if not already formed as a trapezoid) so that the second (bottom) face is ground to form a trapezoidal surface. Trapezoidal grinding 1018 prior to chrome plating improves the precision and tolerance control of the piston ring. After the first trapezoidal grind on the second face and / or first face and prior to applying chrome plating, an optional side brush grinding 1044 may be performed to break up any nodules on the ring surface.

[0086] At step 1020, the base portion is electrochemically plated with chromium by fully immersing the base portion (cathode) in a chromium-containing electrolyte to provide a full electroplated chromium coating on the base portion, thereby providing a chromium coating on the inner and outer contact surfaces, the first and second faces, and the corner areas. For example, the anode can be chromium metal. The base portion is rotated one or more times, and in one embodiment at least three (3) times, to ensure a complete, solid coating with a satisfactory thickness (e.g., between 10 and 20 μm, as measured by X-ray fluorescence) and to help promote a reduction in thickness variation. It should be understood that after the electrodeposition process, the thickness of the chromium coating can be slightly greater than the desired or predetermined thickness (e.g., 20 μm), which is subsequently reduced to a predetermined thickness between 10 and 20 μm by a grinding and / or grinding step, wherein the thickness variation on the inner, outer and second / bottom surfaces is ≤ 5 μm and the straightness is ≤ 2 μm.

[0087] At step 1022, an outer diameter (OD) grind is then performed along the outer contact surface of the base portion to remove excess chrome material and flatten the surface to achieve a predefined chrome coating thickness variation, which according to one embodiment may be ≤ 5 μm. An optional side brush grind 1044 may be performed after the OD grind to break up nodules on the chrome surface, but without removing material.

[0088] After flattening the chrome coating to a predetermined thickness and thickness variation along the outer diameter of the piston ring, the method 1000 may include a second or mid-gap grinding performed on the piston ring gap 1024 to further flatten any chrome buildup at the ends of the ring / disk. At step 1026, an ID brushing is performed, e.g., an ID brushing of the inner contact surface, to remove nodules on the chrome surface, followed by dry blasting 1028 of the disk (e.g., outer contact surface).

[0089] In step 1030, a running surface or sliding surface can be formed on the outer contact surface above the chromium coating. Step 1030 includes, for example, forming a chromium intermediate layer covering the chromium coating along the outer contact surface by PVD. The PVD chromium intermediate layer is softer than the electrochemical chromium plating layer and improves the adhesion between the chromium plating layer and the DLC coating. The PVD chromium intermediate layer can form a thin film (e.g., ≤1 μm) on the electrochemical chromium plating layer along the outer contact surface and some or all of the upper outer corner area and the lower outer corner area of ​​the base portion. Then a DLC coating is formed via PVD applied to the outer contact surface, for example, on the chromium intermediate layer to form the outer sliding surface of the piston ring. The DLC coating can have a thickness of 2 μm to 25 μm. The chromium intermediate layer and the DLC coating can be applied at low temperatures, for example, about 200 ° C or lower, to help reduce the hardness reduction that may be associated with higher application temperatures. The chromium intermediate layer can be formed in a single step during the PVD process for DLC. Alternatively, the chromium intermediate layer can be applied in a separate step before DLC.

[0090] After step 1030, including applying a chrome interlayer and / or applying a DLC coating in embodiments where a chrome interlayer is not used, an outer diameter (OD) polish is performed on the DLC coating using diamond sandpaper 1032. At step 1034, a third gap grind or gap finish grind is performed on the piston ring gap so that the first and second ends of the ring / disc stock are finished to a desired roughness.

[0091] At step 1046, a trapezoidal (or side) grind is performed on one or both of the sides of the base portion to remove portions of the chromium material and planarize the surface of the coating. The trapezoidal grind 1046 can planarize the chromium coating along the second (bottom) surface by removing outer portions of the chromium material to form a chromium coating having a desired thickness (10 μm to 20 μm), thickness variation (≤ 5 μm), and straightness (≤ 2 μm). Additionally or alternatively, the trapezoidal grind 1046 can remove portions of the chromium material along the first (top) surface, such as at the upper inner corner region, to facilitate planarizing and shaping the chromium coating. At step 1036, a trapezoidal brush grind is then performed on the second surface to reduce or remove nodules on the chromium surface.

[0092] At step 1038, a second trapezoidal grinding 1038 is performed on the first (top) surface to remove all or substantially all of the chromium material along the first surface from the upper inner corner region to the upper outer corner region, exposing the material of the base portion, and roughening the exposed surface of the base material. The second trapezoidal grinding 1038 can also help shape the upper outer corner region to provide a gradually decreasing thickness of the DLC and / or shape the upper inner corner region to provide a gradually decreasing thickness of the chromium coating. At step 1040, a phosphate coating is applied to the first (top) surface by phosphatization to form a phosphate coating having a thickness of approximately ≤3 μm (e.g., between 2 μm and 3 μm), which can be directly applied to the base portion along the first surface (via the second trapezoidal grinding 1038) and at least partially overlaps the DLC on the upper outer corner region and at least partially on the chromium coating on the upper outer corner region. The phosphate coating helps to improve corrosion resistance and promote lubrication and wear resistance. The phosphate coating can include, for example, magnesium phosphate. A final check 1042 may be performed and the process ends.

[0093] Fig.11 An exemplary method 1100 for producing a piston ring according to another embodiment is shown. Fig.11 and Fig.10 The difference is the order of the trapezoidal grind 1146, wherein, according to method 1100, the trapezoidal grind 1146 is performed before the second / mid-gap grind 1124 (e.g., after the OD grind 1122) and can help form a gradually decreasing thickness of the chrome coating at the upper outer corner area. The trapezoidal grind 1146 flattens the outer surface of the chrome coating along the second (bottom) surface by passing some of the chrome material through to form a chrome coating having a desired thickness (10μm to 20μm), thickness variation (≤5μm), and straightness (≤2μm). The OD grind 1122 and the trapezoidal grind 1144 together form and flatten the outer profile of the chrome-coated ring (e.g., the outer contact surface, the first / top surface, and the second / bottom surface). The method 1100 may also include an optional side brush grind 1144 on the first and / or second surface after the trapezoidal grind 1146 to break up nodules on the chrome surface. In other respects, the process remains the same as Fig.10 The same as in the above are represented by the same reference numerals.

[0094] It should be understood that grinding is different from lapping in that lapping helps increase smoothness and straightness (flatness), whereas grinding removes more material and produces a rougher surface than lapping.

[0095] Therefore, according to the present disclosure and Figure 5 and FIG. 6A to FIG. 6C , and according to Figures 7 to 11In the method of the present invention, at steps 706, 820, 920, 1020, 1120, a chromium coating 514 is deposited on an outer surface 530 of the base portion 502. The outer surface 530 surrounds the periphery of the base portion 502, including on the first face 506, the second face 508, the outer contact surface 504 facing the side of the ring 500, and the inner contact surface 510. After shaping at least the outer diameter of the base portion 502 along the outer contact surface 504 (e.g., by OD grinding 822, 922, 1022, 1122 and / or grinding) to remove excess chromium material, at steps 710, 830, 930, 1030, 1130, DLC 512 is deposited (e.g., via PVD) on the outer surface of the chromium coating 514 on the outer contact surface 504 facing the side of the ring 500. According to one embodiment, a chromium intermediate layer 532 may also be deposited (e.g., via PVD) on the outer surface of the chromium coating 514 along the outer contact surface 504 to improve adhesion between the chromium coating 514 and the DLC 512. Thereafter, the first face 506 is ground 838, 938, 1038, 1138 such that the chromium coating 514 is removed from the first face 506 and the outer surface 530 is exposed on the first face 506 facing the side of the ring 500. The chromium coating 514 remains on the outer surface 530 on the second face 508, the outer contact surface 504 facing the side of the ring 500, and the inner contact surface 510. At steps 712, 840, 940, 1040, 1140, a phosphate layer 516 is deposited on the first face 506 by phosphating such that the phosphate layer 516 is deposited on the outer surface 530 from which the chromium coating 514 was removed. The phosphate layer 516 may additionally be deposited on the outer corner surface 536 in the upper outer corner region 518. The outer corner surface 536 is the outer surface of the DLC layer 512 as the DLC layer 512 extends from the tapered thickness 608 to the zero thickness 610. Thus, the phosphate layer 516 may partially cover / overlap the DLC 512 on the outer corner surface 536 so as to wrap around the upper outer corner region 518 and be located on the outer surface 536 of the DLC layer 512. The phosphate layer 516 is also deposited on the inner corner surface 534 in the upper inner corner region 522. The inner corner surface 534 is the outer surface of the chrome coating 514 as the chrome coating 514 extends from the tapered thickness 620 to the zero thickness 624. The phosphate layer 516 may partially cover / overlap the chrome coating 514 on the inner corner surface 534 so as to wrap around the upper inner corner region 522 and be located on the outer surface 534 of the chrome coating 514 .

[0096] In another example, Fig.12As shown, a polymer layer 1218 is provided. The piston ring 1200 includes a base portion 1202 formed of a metal material such as steel. The base portion includes an outer contact surface 1204 extending between a first face 1206 (e.g., an upper surface) of the piston ring 1200 and a second face 1208 (e.g., a lower surface) opposite to the first face 1206. The base portion includes an inner contact surface 1210 extending between the first face 1206 and the second face 1208 of the piston ring 1200. A chrome coating 1214 is formed or positioned on the second face 1208, the outer contact surface 1204, and the inner contact surface 1210. A DLC layer 1212 is formed on the outer contact surface 504 above the chrome layer 1014, and a chrome intermediate layer (not shown) may be interposed between the DLC layer 1212 and the chrome coating 1214. A phosphate layer 1216 is formed on the first face 1206. The polymer layer 1218 is formed on the DLC layer 1212 so that the polymer layer 1218 covers the outer surface of the DLC layer 1212. The high hardness of the DLC layer 1212 makes it difficult for the piston ring 1200 to break in during the early period of the engine life. The polymer layer 1218 provides a solid lubricant to the outer contact surface 1204 of the piston ring 1200 to allow faster running-in of the engine components and improve the durability of the piston ring 1200. The polymer layer 1218 is a resin-bonded coating, and in particular, may include a resin-bonded polyamideimide (PAI) or a resin-bonded polytetrafluoroethylene (PTFE) added with molybdenum disulfide. For example, the polymer layer 1218 may be formed according to the present invention. Figures 7 to 11 The method shown forms the piston ring 1200 with the addition of applying a polymer layer 1218 to the outer contact surface 1204 above the DLC layer 1212. Thus, it should be understood that the polymer layer 1218 may be applied to Figures 5 to 6C DLC 512 is shown, for example, without departing from the scope of the present disclosure.

[0097] In one example, the phosphate layer 1016 is approximately ≤3 μm, for example, approximately 2-3 μm, and the polymer layer 1018 is approximately 5-15 μm, for example, approximately 10 μm. The chrome coating 1014 is approximately 10-20 μm, with a thickness variation of ≤5 μm and a flatness of ≤2 μm (at least on the second face 508 including the corner regions 520, 524 and the inner contact surface 510). The chrome intermediate layer can be approximately ≤1 μm. The DLC layer can be approximately 2-25 μm.

[0098] It should be understood that the above description is intended to be illustrative and not restrictive. Many applications other than the examples provided will be derived after reading the above description. The scope of the present disclosure should not be determined with reference to the above description, but should be determined with reference to the full scope of equivalents given by the attached claims and these claims. It is foreseeable and expected that future developments will occur in the fields discussed herein, and the disclosed systems and methods will be incorporated into such future embodiments. In short, it should be understood that the present disclosure is capable of modification and variation and is limited only by the attached claims.

[0099] All terms used in the claims are intended to be given their broadest reasonable interpretations and their ordinary meanings as understood by those skilled in the art unless an explicit indication to the contrary is made herein. In particular, the use of singular articles such as "a", "an", "the", "said", etc. should be understood to recite one or more of the indicated elements unless a claim recites an explicit limitation to the contrary.

[0100] It should be understood that references to individual elements are not necessarily limited thereto and may include one or more of such elements. Any directional references (e.g., positive, negative, up, down, upward, downward, left, right, leftward, rightward, top, bottom, above, below, vertical, horizontal, clockwise, and counterclockwise) are used only for identification purposes to help the reader understand the present disclosure and do not create limitations, especially with respect to the use of positions, orientations, or examples / embodiments.

[0101] “One or more” includes functions performed by one element, functions performed by more than one element, e.g., in a distributed fashion, multiple functions performed by one element, multiple functions performed by multiple elements, or any combination of the foregoing.

[0102] It should also be understood that, although in some cases, the terms first, second, etc. are used to describe various elements in this article, these elements should not be limited by these terms. These terms are only used to distinguish one element from another element. For example, without departing from the scope of the various described embodiments, the first element can be referred to as the second element, and similarly, the second element can be referred to as the first element. The first element and the second element are both elements, but they are not the same element.

[0103] The terms used in the description of the various described embodiments herein are only used for the purpose of describing specific embodiments, and are not intended to be limited. As used in the description of the various described embodiments and the appended claims, the singular forms "one", "an" and "the" are intended to also include plural forms, unless the context clearly indicates otherwise. It will also be understood that the term "and / or" as used herein refers to and encompasses any and all possible combinations of one or more of the associated listed items. It will be further understood that when used in this specification, the terms "include", "comprise", "include" and / or "comprises" specify the existence of stated features, integers, steps, operations, elements and / or components, but do not exclude the existence or addition of one or more other features, integers, steps, operations, elements, components and / or their groups.

Claims

1. A piston ring, comprising: a base portion formed of a metal material; an outer contact surface and an inner contact surface extending between a first face of the piston ring and a second face opposite the first face; a chrome coating on said inner contact surface, said outer contact surface and said second face; A diamond-like carbon (DLC) layer is disposed over the chromium coating on the outer contact surface.

2. The piston ring according to claim 1, wherein: The piston ring further includes a phosphate layer on the first face of the piston ring.

3. The piston ring according to claim 2, wherein: The phosphate layer overlaps the DLC portion at an upper outer corner region of the base portion, and overlaps the chrome coating portion at an upper inner corner region of the base portion.

4. The piston ring according to claim 3, wherein: The phosphate layer has a gradually decreasing thickness along the upper outer corner region and the upper inner corner region.

5. The piston ring according to claim 1, wherein: The piston ring further includes a physical vapor deposition (PVD) chromium intermediate layer between the DLC and the chromium coating along the outer contact surface.

6. The piston ring according to claim 1, wherein: The piston ring further includes a polymer layer covering the DLC.

7. The piston ring according to claim 1, wherein: The DLC has a substantially constant thickness along the outer contact surface and has a gradually decreasing thickness at a lower outer corner region of the base portion and an upper outer corner region of the base portion.

8. The piston ring according to claim 7, wherein: the chrome coating having a substantially constant thickness along the outer contact surface, the lower outer corner region, the second face, the lower inner corner region of the base portion, and the inner contact surface; and The chrome coating has a gradually decreasing thickness at an upper outer corner region and an upper inner corner region of the base portion.

9. The piston ring according to claim 1, wherein: The chromium coating has a thickness between 10 μm and 20 μm with a thickness variation equal to or less than 5 μm, and wherein the chromium coating has a flatness equal to or less than 2 μm along the second face and the inner contact surface.

10. A method of forming a piston ring, comprising: providing a base portion formed of a metal material, the base portion having a first surface, a second surface opposite the first surface, an outer contact surface, and an inner contact surface; applying a chrome coating on the first face, the second face, the outer contact surface, and the inner contact surface; A diamond-like carbon (DLC) layer is deposited over the chromium coating on the outer contact surface.

11. The method according to claim 10, wherein: The method further includes trapezoidally grinding the second surface to planarize the outer surface of the chrome coating to a straightness variation of 2 μm or less.

12. The method according to claim 11, wherein: The method further includes brushing the second surface after the trapezoidal grinding to remove nodules from the chrome coating.

13. The method according to claim 11, wherein: The method further comprises: trapezoidally grinding the first face to remove substantially all of the chrome coating from the first face, thereby exposing the base portion and roughening an outer surface of the base portion; and A phosphate layer is deposited on the first side.

14. The method according to claim 13, wherein: The method further includes trapezoidally grinding the second face prior to applying the chrome coating.

15. The method according to claim 13, wherein: The method further comprises: grinding the chromium coating along the outer contact surface prior to depositing the DLC; Prior to depositing the DLC, the chromium coating is gap-grinded at the piston ring gap; brush grinding the chrome coating along the inner contact surface after the gap grinding and before depositing the DLC; and After depositing the DLC and before trapezoidal grinding of the first surface, the chrome coating is gap-finish ground at the piston ring gap.

16. The method according to claim 16, wherein: The trapezoidal grinding is performed after the OD grinding and before the gap grinding.

17. The method according to claim 10, wherein: The method further includes depositing a chromium intermediate layer over the chromium overlay along the outer contact surface, the chromium intermediate layer being interposed between the chromium overlay and the DLC.

18. The method according to claim 17, wherein: The chromium coating is applied electrochemically and the chromium intermediate layer is deposited via physical vapor deposition.

19. The method according to claim 17, wherein: The method has at least one of the following features: The chromium intermediate layer is deposited in the same step as the DLC; and The chromium intermediate layer is deposited at a temperature of about 200° C. or less.

20. The method according to claim 11, wherein: The method further includes depositing a polymer layer on an outer surface of the DLC layer.

Citation Information

Patent Citations

  • Sliding element

    US10400895B2

  • Piston ring and method of manufacture

    US12123500B2