Pretreatment method for spectral analysis of high-temperature alloy material
By using mechanical processing and chemical reaction methods in the spectral analysis pretreatment of GH3044 high-temperature alloy materials, the problems of incomplete decomposition and impurities were solved, and efficient and accurate spectral analysis results were achieved. It is suitable for spectral analysis of GH3044 materials before spectral analysis deal with.
Patent Information
- Application Number
- CN202410856041.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-28
- Publication Date
- 2024-11-08
AI Technical Summary
In the pre-spectroscopic analysis, GH3044 high-temperature alloy material has problems such as incomplete decomposition and insoluble particles in the sample solution, which leads to a large deviation in the results of the spectral quantitative analysis, which is difficult to effectively solve the existing methods.
After the sample is prepared by mechanical processing, it is washed with high-purity acetone in an ultrasonic cleaning machine and dried. Then, a mixed solution of hydrochloric acid, nitric acid and hydrofluoric acid is used to perform chemical reactions in a water bath until the residue is completely reacted. Transfer to the volumetric flask to be tested and tested using an inductively coupled plasma emission spectrometer.
This method achieves complete decomposition and removal of impurities of GH3044 material, improves the accuracy and reliability of the spectral analysis results, is simple and efficient in operation, and is suitable for spectral analysis pretreatment of high-temperature alloy materials.
Smart Images

Figure SMS_1
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of spectral analysis, and in particular relates to a pre-processing method for spectral analysis of high-temperature alloy materials. Background Art
[0002] Spectral analysis is an analytical technique that uses the characteristic spectrum generated when matter interacts with electromagnetic radiation to identify the composition, structure and content of a substance. That is, each element or compound has a unique spectrum and absorbs and emits electromagnetic radiation of a specific wavelength under specific conditions. This technology is widely used in chemistry, material science, environmental monitoring, geological exploration, medicine, food safety and other fields. When using spectral analysis to quantitatively analyze the element content of a material, it is often necessary to completely decompose the material in a solution for measurement. Therefore, it is particularly important to consider how to completely decompose the material in a solution through pretreatment methods.
[0003] GH3044 is a nickel-based high-temperature alloy material, mainly used in high-performance fields such as aircraft engines and gas turbines. It has excellent high-temperature strength, good oxidation resistance and corrosion resistance, and can maintain stable mechanical properties under extreme environments. The main elements in GH3044 material are nickel, chromium, tungsten, etc., and the tungsten content is 13.00%-16.00%. Tungsten has stable chemical properties and does not react with any concentration of hydrochloric acid, nitric acid, sulfuric acid, hydrofluoric acid and aqua regia at room temperature, which makes the pretreatment of GH3044 material very difficult. When the pretreatment methods recommended by national standards GB222 and industry standards HB20241 are used to pretreat GH3044 materials, the pretreatment effect is not good, and there are problems such as incomplete decomposition and a small amount of insoluble particles in the sample solution, which leads to large deviations in the quantitative analysis results of GH3044 spectra. Summary of the invention
[0004] The purpose of the present invention is to overcome the above-mentioned shortcomings and provide a high-temperature alloy material spectral analysis pretreatment method which is simple to operate, efficient, feasible, accurate and reliable.
[0005] The purpose of the present invention and the solution of its main technical problems are achieved by adopting the following technical solutions: The high-temperature alloy material spectral analysis pre-treatment method of the present invention comprises the following steps: (1) Sample preparation: Obtain the GH3044 high-temperature alloy sample to be tested by mechanical processing, clean it in an ultrasonic cleaner with 50-100 mL of acetone with a concentration greater than 99.5% for 10-15 minutes, and then place it on filter paper to dry in order to remove impurities such as grease and water during the sampling process; (2) Sample weighing: Weigh 0.1000-0.1050g of GH3044 sample and place it in a clean polytetrafluoroethylene beaker; (3) Reagent preparation and use: Add 19-21 mL of hydrochloric acid and nitric acid in a volume ratio of 10:0.8-10:1.2 to a beaker to form a mixed solution. Heat in a water bath for 60-90 minutes at a temperature of 50-55°C. Slowly add 1.5-2 mL of hydrofluoric acid and continue heating until the residue reacts completely. Transfer to a volumetric flask, dilute to volume and shake well for testing. (4) Spectrometer determination: Start the inductively coupled plasma emission spectrometer, preheat for 6-24 hours, and then place the GH3044 sample solution obtained in step (3) into the spectrometer for detection.
[0006] In the above-mentioned method for pre-processing high-temperature alloy materials for spectral analysis, the mechanical processing method described in step (1) is milling or drilling.
[0007] The above-mentioned high-temperature alloy material spectral analysis pretreatment method, wherein: the concentration of the hydrochloric acid in step (3) is 36%-38%.
[0008] The above-mentioned high-temperature alloy material spectral analysis pretreatment method, wherein: the concentration of nitric acid in step (3) is 65%-68%.
[0009] The above-mentioned high-temperature alloy material spectral analysis pretreatment method, wherein: the concentration of the hydrofluoric acid in step (3) is 40%-50%.
[0010] Compared with the prior art, the present invention has obvious advantages and beneficial effects. It can be seen from the above technical scheme that in the method for pre-treatment of spectral analysis of high-temperature alloy materials of the present invention, the steps of preparing samples, weighing samples, configuring and using reagents, and measuring with a spectrometer are adopted to solve the problem of incomplete decomposition of the pre-treatment samples of the high-temperature alloy GH3044 spectral analysis. The chemical reaction is mild during the pre-treatment process, and the entire pre-treatment process is easy to control, which improves the accuracy of the test results, and provides support for the spectral quantitative analysis of GH3044 materials. In short, the present invention is simple to operate, efficient, feasible, accurate and reliable, and is suitable for the promotion and use of pre-treatment of spectral analysis of high-temperature alloy materials. DETAILED DESCRIPTION
[0011] In combination with the preferred embodiments, the specific implementation manner, structure, characteristics and efficacy of the high-temperature alloy material spectral analysis pretreatment method proposed in the present invention are described in detail as follows.
[0012] Embodiment 1: A method for pre-processing a high-temperature alloy material for spectral analysis comprises the following steps: (1) Sample preparation: The GH3044 high-temperature alloy sample to be tested was obtained by milling, and was cleaned in an ultrasonic cleaner with 50 mL of acetone with a concentration greater than 99.5% for 10 minutes, and then placed on filter paper to dry in order to remove impurities such as grease and water during the sampling process; (2) Sample weighing: Weigh 0.1000 g of GH3044 sample and place it in a clean polytetrafluoroethylene beaker; (3) Reagent preparation and use: Add 19 mL of 36% hydrochloric acid and 65% nitric acid in a volume ratio of 10:0.8 to a beaker to form a mixed solution. Heat in a water bath for 60 minutes at 50°C. Slowly add 1.5 mL of 40% hydrofluoric acid. Continue heating until the residue reacts completely. Transfer to a volumetric flask, dilute to volume and shake well for testing. (4) Spectrometer determination: Start the inductively coupled plasma emission spectrometer and, after preheating for 6 hours, place the GH3044 sample solution obtained in step (3) into the spectrometer for detection.
[0013] Embodiment 2: A method for pre-processing a high-temperature alloy material for spectral analysis comprises the following steps: (1) Sample preparation: The GH3044 high-temperature alloy sample to be tested was obtained by drilling, and was cleaned in an ultrasonic cleaner for 12.5 minutes using 75 mL of acetone with a concentration greater than 99.65%, and then placed on filter paper to dry in order to remove impurities such as grease and water during the sampling process; (2) Sample weighing: Weigh 0.1025 of GH3044 sample and place it in a clean polytetrafluoroethylene beaker; (3) Reagent preparation and use: Add 20 mL of 37% hydrochloric acid and 66.5% nitric acid in a volume ratio of 10:1.0 to a beaker to form a mixed solution. Heat in a water bath for 75 minutes with the temperature controlled at 52.5°C. Slowly add 1.75 mL of 45% hydrofluoric acid and continue heating until the residue reacts completely. Transfer to a volumetric flask, dilute to volume and shake well for testing. (4) Spectrometer determination: Start the inductively coupled plasma emission spectrometer and, after preheating for 15 hours, place the GH3044 sample solution obtained in step (3) into the spectrometer for detection.
[0014] Embodiment 3: A method for pre-processing a high-temperature alloy material for spectral analysis comprises the following steps: (1) Sample preparation: The GH3044 high-temperature alloy sample to be tested was obtained by milling, and was cleaned in an ultrasonic cleaner with 100 mL of acetone with a concentration greater than 99.8% for 15 minutes, and then placed on filter paper to dry in order to remove impurities such as grease and water during the sampling process; (2) Sample weighing: Weigh 0.1050 g of GH3044 sample and place it in a clean polytetrafluoroethylene beaker; (3) Reagent preparation and use: Add 21 mL of 38% hydrochloric acid and 68% nitric acid in a volume ratio of 10:1.2 to a beaker to form a mixed solution. Heat in a water bath for 90 minutes at 55°C. Slowly add 2 mL of 50% hydrofluoric acid and continue heating until the residue reacts completely. Transfer to a volumetric flask, dilute to volume and shake well for testing. (4) Spectrometer determination: Start the inductively coupled plasma emission spectrometer and, after preheating for 24 hours, place the GH3044 sample solution obtained in step (3) into the spectrometer for detection.
[0015] After the spectrometer measurement is completed, the element content spectrum line selection of the high-temperature alloy GH3044 refers to Table 1.
[0016] In addition, the spectrometer should be equipped with a hydrofluoric acid injection system. The spectrometer can be a simultaneous type or a sequential type. If the sequential type spectrometer is equipped with a device for simultaneously measuring the internal standard line, the internal standard method can be used.
[0017] Table 1 Spectral lines of element content of GH3044 determined by ICP spectrometer The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. Any simple modification, equivalent change and modification made to the above embodiment according to the technical essence of the present invention without departing from the technical solution of the present invention still falls within the scope of the technical solution of the present invention.
Claims
1. A method for pre-processing high-temperature alloy material spectral analysis, comprising the following steps: (1) Sample preparation: Obtain the GH3044 high-temperature alloy sample to be tested by mechanical processing, clean it in an ultrasonic cleaner with 50-100 mL of acetone with a concentration greater than 99.5% for 10-15 minutes, and then place it on filter paper to dry in order to remove impurities such as grease and water during the sampling process; (2) Sample weighing: Weigh 0.1000-0.1050g of GH3044 sample and place it in a clean polytetrafluoroethylene beaker; (3) Reagent preparation and use: Add 19-21 mL of hydrochloric acid and nitric acid in a volume ratio of 10:0.8-10:1.2 to a beaker to form a mixed solution. Heat in a water bath for 60-90 minutes at a temperature of 50-55°C. Slowly add 1.5-2 mL of hydrofluoric acid and continue heating until the residue reacts completely. Transfer to a volumetric flask, dilute to volume and shake well for testing. (4) Spectrometer determination: Start the inductively coupled plasma emission spectrometer, preheat for 6-24 hours, and then place the GH3044 sample solution obtained in step (3) into the spectrometer for detection.
2. The method for pre-processing high-temperature alloy material spectral analysis according to claim 1, characterized in that: The machining method described in step (1) is milling or drilling.
3. The method for pre-processing high-temperature alloy material spectral analysis according to claim 1, characterized in that: The concentration of the hydrochloric acid in step (3) is 36%-38%.
4. The method for pre-processing high-temperature alloy material for spectral analysis according to claim 1, characterized in that: The concentration of nitric acid in step (3) is 65%-68%.
5. The method for pre-processing high-temperature alloy material for spectral analysis according to claim 1, characterized in that: The concentration of the hydrofluoric acid in step (3) is 40%-50%.