Method for detecting welding strength of internal brazing workpiece

Through the welding strength detection method of internal brazing workpieces, resistance detection and mechanical impact technology are used to solve the destructive problem of existing brazing strength detection, realizing lossless, efficient and accurate judgment of batch product welding, and is suitable for assembly line applications.

CN118913962APending Publication Date: 2024-11-08HANGZHOU SUNRISE TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410947492.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-16
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

In the prior art, the strength detection of brazing is usually destructive detection, and it is impossible to effectively determine whether the welding of each solder joint of batch products is firm and is not suitable for assembly line detection.

Method used

The welding strength detection method of internal brazed workpiece is used to detect the initial resistance value through a resistance detector, and after fixing the workpiece, the pneumatic impact machine and vibrator are used to perform mechanical impact on the welding point, and the resistance value after impact is read to the initial value. Yes, determine whether the brazing strength is reliable for connection.

Benefits of technology

It realizes non-destructive testing of batch products welding, can efficiently and accurately judge the welding strength, is suitable for assembly line use, eliminates defective products, and has the characteristics of high efficiency, accuracy and ease of use.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118913962A_ABST
    Figure CN118913962A_ABST
Patent Text Reader

Abstract

The method comprises the steps that one end of a resistance detector is connected to a second metal piece, the other end of the resistance detector is connected to a first metal piece, the initial resistance between the first metal piece and the second metal piece is detected through the resistance detector, and the inner brazing workpiece is fixed to a base; a pneumatic impact machine is used for driving an impact head to impact the second metal piece at the brazing joint for the first time of more than 2J, and the impact head keeps in contact with the second metal piece; the pneumatic vibrator drives the impact head to continuously impact the second metal piece with 1J pulses of about 16-20 times per second for 0.5-1 second, and the impact head retracts after transmitting vibration force; the current resistance value detected by the resistance detector is read, the current resistance value is compared with the initial resistance value, and whether the brazing strength is reliably connected or not is judged according to the comparison result; the non-destructive testing method for good products can be embedded into an assembly line to be carried out, and has the advantages of being efficient, accurate and easy to use.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of welding strength detection, in particular to a welding strength detection method for an internal brazing workpiece. Background Art

[0002] Brazing refers to a welding method in which the solder and the workpiece are heated to the melting temperature of the solder at the same time, and the gap of the solid workpiece is filled with liquid solder to connect the metals. When brazing, the oxide film and oil stains on the contact surface of the parent material must be removed first, so as to facilitate the capillary to play a role after the solder melts, increase the wettability and capillary fluidity of the solder. According to the melting point of the solder, brazing is divided into hard soldering and soft soldering. Brazing has small deformation and smooth and beautiful joints. It is suitable for welding precise, complex components made of different materials, such as honeycomb structure plates, turbine blades, carbide tools and printed circuit boards.

[0003] Brazing with a melting point of brazing material higher than 450°C is called hard brazing, and the hard brazing material includes copper-based, silver-based, aluminum-based and other alloys. In the related art, the strength test of brazing is usually a destructive test of the workpiece, that is, the welding state of the workpiece will be destroyed after the test, which is not conducive to judging whether the welding of each welding point of batch products is firm, and is not suitable for assembly line testing. Summary of the invention

[0004] The purpose of the present invention is to overcome the above technical deficiencies, propose a method for detecting the welding strength of an internally brazed workpiece, and solve the technical problem that the strength detection of brazing in the prior art is usually a destructive detection of the workpiece, which is not conducive to judging whether the welding of each welding point of a batch product is firm.

[0005] In order to achieve the above technical objectives, in a first aspect, the technical solution of the present invention provides a method for detecting the welding strength of an internally brazed workpiece, comprising the following steps:

[0006] The first metal member and the second metal member are connected by soldering to obtain an inner brazing workpiece;

[0007] Use a resistance detector to connect one end to the second metal piece and the other end to the first metal piece, and use the resistance detector to detect the initial resistance between the first metal piece and the second metal piece;

[0008] Fixing the inner brazing workpiece on a base, with the first metal piece at the bottom and the second metal piece at the top;

[0009] Using a pneumatic impact machine to drive an impact head to perform a first impact of more than 2J on the second metal member at the brazed connection, wherein the impact head maintains contact with the second metal member;

[0010] The pneumatic vibrator drives the impact head to continuously impact the second metal part with a 1J pulse of about 16-20 times / s for a duration of 0.5-1s, and the impact head retracts after transmitting the vibration force;

[0011] The current resistance value detected by the resistance detector is read, the current resistance value is compared with the initial resistance value, and whether the brazing strength is reliably connected is determined according to the comparison result.

[0012] Compared with the prior art, the welding strength detection method of the internal brazing workpiece provided by the present invention has the following beneficial effects:

[0013] When two metal parts of different materials are welded by brazing, if the brazing filler is filled and melted evenly, the contact surface has strong resistance to mechanical impact, otherwise it is easy to come apart. In the related art, the strength detection of brazing is usually a destructive detection of the workpiece, that is, the welding state of the workpiece will be destroyed after the detection. The welding strength detection method of the internal brazing workpiece of the present application impacts each welding point of the batch product, and measures the resistance value of the internal brazing workpiece after the impact, compares the current resistance value with the initial resistance value, and judges whether the brazing strength is reliably connected according to the comparison result to judge whether the welding is firm. This non-destructive detection method for good products can be embedded in the assembly line and defective products can be eliminated. It is efficient, accurate and easy to use.

[0014] According to some embodiments of the present invention, the first metal piece is a brass piece, and the second metal piece is a copper piece.

[0015] According to some embodiments of the present invention, a pneumatic vibrator drives an impact head to continuously impact the second metal part with a 1J pulse of about 16-20 times / s for a duration of 0.5-1s, and the impact head retracts after transmitting the vibration force, including the steps of:

[0016] The impact head is driven by a pneumatic vibrator to perform 1J pulse impact on the second metal part continuously for about 16 times / s for a duration of 0.5s. The impact head retracts after transmitting the vibration force.

[0017] According to some embodiments of the present invention, judging whether the brazing strength is reliably connected according to the comparison result includes the following steps:

[0018] When the current resistance value is higher than 150% of the initial resistance value, the soldering strength is determined to be an unreliable connection.

[0019] According to some embodiments of the present invention, judging whether the brazing strength is reliably connected according to the comparison result includes the following steps:

[0020] When the current resistance value is between 100% and 120% of the initial resistance value, the soldering strength is determined to be a reliable connection.

[0021] Additional aspects and advantages of the present invention will be given in part in the following description and in part will be obvious from the following description, or will be learned through practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] The above and / or additional aspects and advantages of the present invention will become apparent and easily understood from the description of the embodiments in conjunction with the following drawings, wherein the abstract drawings are identical to one of the drawings in the specification:

[0023] Figure 1 A flow chart of a method for detecting welding strength of an internally brazed workpiece provided by one embodiment of the present invention;

[0024] Figure 2 A schematic diagram of a welding strength testing device for internally brazed workpieces provided by one embodiment of the present invention. DETAILED DESCRIPTION

[0025] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.

[0026] It should be noted that, although the functional modules are divided in the system schematic diagram and the logical order is shown in the flowchart, in some cases, the steps shown or described may be performed in a different order than the module division in the system or the order in the flowchart. The terms "first", "second", etc. in the specification, claims and the above drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence.

[0027] The embodiments of the present invention are further described below in conjunction with the accompanying drawings.

[0028] Reference Figure 1 , Figure 2 , Figure 1 A flow chart of a method for detecting welding strength of an internally brazed workpiece provided by one embodiment of the present invention; Figure 2 A schematic diagram of a welding strength detection device for internally brazed workpieces provided by an embodiment of the present invention. The welding strength detection method for internally brazed workpieces includes but is not limited to steps S110 to S160.

[0029] Step S110, welding the first metal part and the second metal part to obtain an inner brazing workpiece by means of brazing filler metal;

[0030] Step S120, using a resistance detector, one end of which is connected to the second metal member, and the other end of which is connected to the first metal member, to detect the initial resistance between the first metal member and the second metal member by the resistance detector;

[0031] Step S130, fixing the inner brazing workpiece on the base, with the first metal piece at the bottom and the second metal piece at the top;

[0032] Step S140, using a pneumatic impact machine to drive the impact head to perform a first impact of more than 2J on the second metal member at the brazed connection, and the impact head maintains contact with the second metal member;

[0033] Step S150, driving the impact head with a pneumatic vibrator to continuously impact the second metal part with a 1J pulse of about 16-20 times / s for a duration of 0.5-1s, and the impact head retracts after transmitting the vibration force;

[0034] Step S160, reading the current resistance value detected by the resistance detector, comparing the current resistance value with the initial resistance value, and judging whether the brazing strength is reliably connected according to the comparison result.

[0035] In one embodiment, a method for detecting the welding strength of an internally brazed workpiece includes the steps of: connecting a first metal part and a second metal part by soldering to obtain an internally brazed workpiece; using a resistance detector to connect one end to the second metal part and the other end to the first metal part, detecting the initial resistance between the first metal part and the second metal part by the resistance detector, fixing the internally brazed workpiece on a base with the first metal part at the bottom and the second metal part at the top; using a pneumatic impact machine to drive the impact head to perform an initial impact of more than 2J on the second metal part at the brazed connection, with the impact head maintaining contact with the second metal part; using a pneumatic vibrator to drive the impact head to perform a continuous 1J pulse impact of about 16-20 times / s on the second metal part for a duration of 0.5-1s, and the impact head retracts after transmitting the vibration force; reading the resistance detector to detect the current resistance value between the first metal part and the second metal part, comparing the current resistance value with the initial resistance value, and judging whether the brazing strength is reliably connected based on the comparison result.

[0036] When two metal parts of different materials are welded by brazing, if the brazing filler is filled and melted evenly, the contact surface has strong resistance to mechanical impact, otherwise it is easy to come apart. In the related technology, the strength detection of brazing is usually a destructive detection of the workpiece, that is, the welding state of the workpiece will be destroyed after the detection. The welding strength detection method of the internal brazing workpiece of the present application impacts each welding point of the batch product, and measures the resistance value of the internal brazing workpiece after the impact, compares the current resistance value with the initial resistance value, and judges whether the brazing strength is reliably connected according to the comparison result to judge whether the welding is firm. This non-destructive detection method for good products can be embedded in the assembly line and defective products can be eliminated. It is efficient, accurate and easy to use.

[0037] The welding strength detection method of the internal brazing workpiece of the present application can be applied to the workpiece welded by the copper plate and the brass column through the brazing filler metal. The impact and vibration device is encapsulated in the upper mechanism that can be raised and lowered. The lower mechanism is the machine table to fix the workpiece to be tested. The micro-pneumatic impact machine completes the first impact task (more than 2J). The impact point is the copper plate surface of the workpiece. The impact head does not retract. The micro-pneumatic vibration machine starts the upper structure to perform subsequent 1J pulse impacts of about 16 times / s, with a duration of 0.5s. The impact head retracts after transmitting the vibration force. The additional contact resistance detector is used for detection after the upper impact and vibration. If the resistance is too large, the welding surface is detached and it is judged as a defective product.

[0038] According to the welding strength detection method for internally brazed workpieces of the present invention, the welding point position of the internally brazed workpiece, after being subjected to the initial impact task, is subjected to a 1J pulse impact of about 16 times / s for 0.5s. If the welding point is broken, it is considered that the current welding surface is an unreliable connection. If the welding surface remains unchanged, it is considered that it is a reliable connection. Then, when applied to the assembly line, how to determine whether the welding surface is broken is the key point of the problem. The present application measures the current resistance value between the first metal part and the second metal part by setting a contact resistance detector, compares the initial resistance value with the current resistance value, and judges whether the brazing strength is reliably connected according to the comparison result. When cracks appear on the welding surface, the current resistance value increases significantly relative to the initial resistance value; when the welding surface remains unchanged, the current resistance value will be close to the initial resistance value.

[0039] In one embodiment, a method for detecting the welding strength of an internally brazed workpiece includes the steps of: connecting a first metal part and a second metal part by soldering to obtain an internally brazed workpiece; using a resistance detector to connect one end to the second metal part and the other end to the first metal part, detecting the initial resistance between the first metal part and the second metal part by the resistance detector, fixing the internally brazed workpiece on a base with the first metal part at the bottom and the second metal part at the top; using a pneumatic impact machine to drive the impact head to perform an initial impact of more than 2J on the second metal part at the brazed connection, with the impact head maintaining contact with the second metal part; using a pneumatic vibrator to drive the impact head to perform a continuous 1J pulse impact of about 16-20 times / s on the second metal part for a duration of 0.5-1s, and the impact head retracts after transmitting the vibration force; reading the resistance detector to detect the current resistance value between the first metal part and the second metal part, comparing the current resistance value with the initial resistance value, and judging whether the brazing strength is reliably connected based on the comparison result. When the current resistance value is higher than 150% of the initial resistance value, the brazing strength is judged to be an unreliable connection; when the current resistance value is between 100% and 120% of the initial resistance value, the brazing strength is judged to be a reliable connection.

[0040] The above is a specific description of the preferred implementation of the present invention, but the present invention is not limited to the above-mentioned implementation mode. Technical personnel familiar with the field can also make various equivalent deformations or substitutions without violating the spirit of the present invention. These equivalent deformations or substitutions are all included in the scope defined by the claims of the present invention.

[0041] The specific implementation of the present invention described above does not constitute a limitation on the protection scope of the present invention. Any other corresponding changes and modifications made based on the technical concept of the present invention should be included in the protection scope of the claims of the present invention.

Claims

1. A method for detecting the welding strength of an internal brazing workpiece, characterized in that: The following steps are involved: The first metal member and the second metal member are connected by soldering to obtain an inner brazing workpiece; Use a resistance detector to connect one end to the second metal piece and the other end to the first metal piece, and use the resistance detector to detect the initial resistance between the first metal piece and the second metal piece; Fixing the inner brazing workpiece on a base, with the first metal piece at the bottom and the second metal piece at the top; Using a pneumatic impact machine to drive an impact head to perform a first impact of more than 2J on the second metal member at the brazed connection, wherein the impact head maintains contact with the second metal member; The pneumatic vibrator drives the impact head to continuously impact the second metal part with a 1J pulse of about 16-20 times / s for a duration of 0.5-1s, and the impact head retracts after transmitting the vibration force; The resistance detector reads the current resistance value between the first metal member and the second metal member, compares the current resistance value with the initial resistance value, and determines whether the brazing strength is reliably connected based on the comparison result.

2. The welding strength detection method of the internal brazing workpiece according to claim 1, characterized in that: The first metal piece is a brass piece, and the second metal piece is a copper piece.

3. The welding strength detection method of the internal brazing workpiece according to claim 1, characterized in that: The pneumatic vibrator drives the impact head to continuously impact the second metal part with a 1J pulse of about 16-20 times / s for a duration of 0.5-1s, and the impact head retracts after transmitting the vibration force, including the steps of: The impact head is driven by a pneumatic vibrator to perform 1J pulse impact on the second metal part continuously for about 16 times / s for a duration of 0.5s. The impact head retracts after transmitting the vibration force.

4. The welding strength detection method of the internal brazing workpiece according to claim 1, characterized in that: Judging whether the brazing strength is reliable or not based on the comparison results includes the following steps: When the current resistance value is higher than 150% of the initial resistance value, the soldering strength is determined to be an unreliable connection.

5. The welding strength detection method of the internal brazing workpiece according to claim 1, characterized in that: Judging whether the brazing strength is reliable or not based on the comparison results includes the following steps: When the current resistance value is between 100% and 120% of the initial resistance value, the soldering strength is determined to be a reliable connection.