Heavy metal risk assessment method in coal-based solid waste comprehensive utilization process
Through the combination of step-by-step chemical extraction of coal-based solid waste and the toxic response coefficient, the problem of insufficient environmental risk assessment of heavy metals during coal-based solid waste utilization is solved, and more accurate risk assessment is achieved, sustainable management and resource utilization are supported, and the use of resources is reduced. Environmental impact.
Patent Information
- Application Number
- CN202410846439.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-27
- Publication Date
- 2024-11-08
AI Technical Summary
The existing technology has insufficient environmental risk assessment of heavy metals in the coal-based solid waste utilization process. This is mainly due to the different focus of soil pollution assessment methods, which leads to biased calculation results and cannot fully reflect the heavy metal risks in the coal-based solid waste utilization process.
The combination of heavy metal content in the solution at different utilization stages is adopted by the step-by-step chemical extraction of coal-based solid waste and the combination of heavy metal content in the solution, and the toxic response coefficient is added, and the single element and comprehensive environmental risks are calculated through specific chemical treatment and extraction methods, including roasting, microwave heating, and magnetic stirring. , digestion and Tessier five-state step-by-step extraction method, obtain the full quantitative and active state content of heavy metals, and use specific formulas for risk assessment.
It improves the accuracy and effectiveness of the assessment of environmental risk of heavy metals, provides a scientific basis for the sustainable management and resource utilization of coal-based solid waste, minimizes the impact on the environment, and promotes the harmonious unity of environmental protection and resource utilization.
Smart Images

Figure CN118914453A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of heavy metal pollution risk control and ecological risk assessment, and in particular to a heavy metal risk assessment method in the comprehensive utilization of coal-based solid waste, which is suitable for risk assessment of heavy metals such as cadmium, copper, lead, chromium, zinc, and nickel. Background Art
[0002] At present, for the environmental risk assessment method of coal-based solid waste utilization process, technical personnel in this field often use the soil heavy metal pollution assessment method. The methods used include geoaccumulation index, Nemerow comprehensive pollution index, potential ecological risk index, etc., but the calculation results are biased due to different emphases of the methods. Therefore, many scholars have modified and optimized the soil heavy metal assessment method to make the obtained results more in line with the current soil pollution environment.
[0003] In the existing technology, some methods change the average value of the single factor pollution index in the Nemerow comprehensive risk assessment method formula to the average value of the single factor pollution index after weighting, so as to make the obtained result more reasonable; some methods optimize the formula based on the geoaccumulation index and the Nemerow comprehensive pollution index to obtain a new potential ecological risk index calculation formula; and some methods use the single factor pollution index as the basis, fit the solution pH, heavy metal leaching concentration, and soil heavy metal residual concentration by calculating the solution pH, heavy metal leaching concentration, and soil heavy metal residual concentration, and then add the two fitting formulas, multiply by 0.5, and divide by the total concentration of heavy metals in the soil to obtain the environmental risk of a single heavy metal.
[0004] However, the above methods all take soil pollution as the main assessment object, and there are certain deficiencies in the environmental risk assessment of coal-based solid waste utilization processes. Summary of the invention
[0005] The technical problem to be solved by the present invention is to provide a heavy metal risk assessment method in the comprehensive utilization of coal-based solid waste. By combining the step-by-step chemical extraction of coal-based solid waste and the heavy metal content in the solution at different utilization stages, and adding a toxicity response coefficient, the heavy metal environmental risk in the utilization process of coal-based solid waste can be better assessed.
[0006] In order to solve the above technical problems, the technical solution adopted by the present invention is:
[0007] A heavy metal risk assessment method in the comprehensive utilization of coal-based solid waste comprises the following steps:
[0008] Step 1, collect coal-based solid waste samples, crush and fully grind them, place the ground samples in an oven, spread them out evenly and dry them;
[0009] Step 2, mixing the dried sample with sodium carbonate in a uniform proportion, and placing the mixture in a muffle furnace for calcination;
[0010] Step 3, dissolving the roasted sample and hydrochloric acid according to the solid-liquid ratio, heating with microwave, and stirring with magnetic force at the same time, and after cooling, processing the dissolved solution through a centrifuge to obtain a leachate and leach residue;
[0011] Step 4, using a mixture of nitric acid and hydrofluoric acid to perform a digestion experiment on the sample dried in step 1 under high temperature and high pressure conditions to obtain the total amount of heavy metal elements in the coal-based solid waste;
[0012] Step 5, using the Tessier five-state stepwise extraction method to perform a stepwise chemical extraction experiment on the sample dried in step 1 to obtain the contents of the five occurrence states of heavy metals, and then obtain the active state content of the coal-based solid waste;
[0013] Step 6: Detect the element concentration in the leaching solution and leaching residue obtained in step 3, and perform heavy metal environmental risk assessment according to formula (1) and formula (2). The formula is as follows:
[0014]
[0015] Where P sgei is a single element environmental risk; P sge is the comprehensive environmental risk; i Q is the active state content of coal-based solid waste, in mg / L; i is the total amount of heavy metals in coal-based solid waste, in mg / L; C i It is the detection value of heavy metal content in the process of coal-based solid waste utilization, in mg / L; S i is the soil background value in natural state; T i is the toxicity response coefficient;
[0016] Step 7, using any one of precipitation, extraction and adsorption methods to treat the leaching solution obtained in step 3 to enrich and purify the valuable elements, and using formula (1) and formula (2) to evaluate the single element risk and comprehensive risk of the process of enriching and purifying the valuable elements.
[0017] A further improvement of the technical solution of the present invention is that in step 1, the types of coal-based solid waste include fly ash, coal gangue, gasification slag and coal liquefaction slag; the drying temperature of the sample is 100-200°C, and the drying time is 18-30h.
[0018] A further improvement of the technical solution of the present invention is that in step 1, the drying temperature of the sample is 180° C. and the drying time is 24 hours.
[0019] The further improvement of the technical solution of the present invention is that in step 2, sodium carbonate and the sample are uniformly mixed in a ratio of 1-1.4:1, the roasting temperature is 700-1500° C., and the roasting time is 80-120 min.
[0020] A further improvement of the technical solution of the present invention is that in step 2, sodium carbonate and the sample are uniformly mixed in a ratio of 1.2:1, the roasting temperature is 900° C., and the roasting time is 90 min.
[0021] A further improvement of the technical solution of the present invention is that in step 3, the solid-liquid ratio of the roasted sample to hydrochloric acid is 1:10-1:40, the concentration of hydrochloric acid is 2mol / L-6mol / L, the microwave heating temperature is 50-90°C, and the magnetic stirring leaching time is 20-50min.
[0022] A further improvement of the technical solution of the present invention is that in step 3, the solid-liquid ratio of the roasted sample to hydrochloric acid is 1:20, the concentration of hydrochloric acid is 3 mol / L, the microwave heating temperature is 80° C., and the magnetic stirring leaching time is 30 min.
[0023] A further improvement of the technical solution of the present invention is that in step 4, the concentration of the nitric acid is 20%-80%, and the amount is 4-20 ml; the concentration of the hydrofluoric acid is 20-80%, and the amount is 2-10 ml; the temperature is 150-300°C.
[0024] A further improvement of the technical solution of the present invention is that in step 4, the concentration of the nitric acid is 66%, and the amount used is 8 ml; the concentration of the hydrofluoric acid is 40%, and the amount used is 4 ml; and the temperature is 180°C.
[0025] A further improvement of the technical solution of the present invention is that in step 5, the five occurrence states of the heavy metals include: metal exchangeable state, carbonate bound state, iron / manganese oxide bound state, organic matter and sulfide bound state, and residue lattice bound state.
[0026] Due to the adoption of the above technical solution, the technical progress achieved by the present invention is:
[0027] The present invention aims at the heavy metal environmental risks that may be generated during the utilization of coal-based solid waste. By obtaining the total content of heavy metal elements in coal-based solid waste and the active content of coal-based solid waste and adding a toxicity response coefficient, a detailed assessment of the environmental risks of heavy metals in the leaching solution and leaching residue, as well as the element enrichment and purification process is carried out. This not only improves the accuracy and effectiveness of risk assessment, but also provides important scientific basis and technical support for the formulation of sustainable coal-based solid waste management strategies and resource utilization plans.
[0028] The present invention can more scientifically guide the treatment and utilization of coal-based solid waste, minimize the impact on the environment, and promote the harmonious unity of environmental protection and resource utilization. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art are briefly introduced below. Obviously, the drawings described below are some embodiments of the present invention. For those of ordinary skill in the art, other drawings can be obtained based on these drawings without creative work.
[0030] Figure 1 It is a flow chart of a heavy metal risk assessment method in the comprehensive utilization of coal-based solid waste provided in an embodiment of the present invention. DETAILED DESCRIPTION
[0031] It should be noted that the terms "including" and "having" and any variations thereof in the specification and claims of the present invention and the above-mentioned drawings are intended to cover non-exclusive inclusions. For example, a process, method, system, product or apparatus comprising a series of steps or units is not necessarily limited to those steps or units clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or apparatus.
[0032] The present invention is further described in detail below with reference to the accompanying drawings and embodiments:
[0033] like Figure 1 As shown, a heavy metal risk assessment method in the comprehensive utilization of coal-based solid waste includes the following steps:
[0034] Step 1, collect coal-based solid waste samples, crush and fully grind them, place the ground samples in an oven, spread them out evenly and dry them;
[0035] Coal-based solid waste types include fly ash, coal gangue, gasification slag and coal liquefaction slag, etc.; the coal-based solid waste sample here is one of fly ash, coal gangue, gasification slag and coal liquefaction slag;
[0036] The drying temperature of the sample is 100-200°C, preferably 180°C; the drying time is 18-30h, preferably 24h.
[0037] Step 2, mixing the dried sample with sodium carbonate in a uniform proportion, and placing the mixture in a muffle furnace for calcination;
[0038] Sodium carbonate and the sample are uniformly mixed in a ratio of 1-1.4:1, preferably 1.2:1; the roasting temperature is 700-1500° C., preferably 900° C.; the roasting time is 80-120 min, preferably 90 min.
[0039] Step 3, dissolving the roasted sample and hydrochloric acid according to the solid-liquid ratio, heating with microwave, and magnetically stirring, cooling to room temperature, and then treating the dissolved solution with a centrifuge to obtain a leachate and leach residue;
[0040] The solid-liquid ratio of the calcined sample to hydrochloric acid is 1:10-1:40, preferably 1:20; the concentration of hydrochloric acid is 2mol / L-6mol / L, preferably 3mol / L; the microwave heating temperature is 50-90°C, preferably 80°C; the microwave heating and magnetic stirring time is 20-50min, preferably 30min.
[0041] In this step, microwave heating and magnetic stirring are performed simultaneously.
[0042] Step 4, using a mixture of nitric acid and hydrofluoric acid to perform a digestion experiment on the sample dried in step 1 under high temperature and high pressure conditions to obtain the total amount of heavy metal elements in the coal-based solid waste;
[0043] The concentration of nitric acid is 20%-80%, preferably 66%; the dosage is 4-20 ml, preferably 8 ml.
[0044] The concentration of hydrofluoric acid is 20-80%, preferably 40%; the dosage is 2-10 ml, preferably 4 ml; the temperature is 150-300°C, preferably 180°C.
[0045] The digestion process takes place in a closed container, and the internal pressure increases as the temperature increases.
[0046] Step 5, using the Tessier five-state stepwise extraction method to perform a stepwise chemical extraction experiment on the sample dried in step 1 to obtain the contents of the five occurrence states of heavy metals, and then obtain the active state content of the coal-based solid waste;
[0047] The five occurrence states of heavy metals are: metal exchangeable state (exchangeable state), carbonate bound state (carbonate state), iron / manganese oxide bound state (iron / manganese state), organic matter and sulfide bound state (organic state), and residual lattice bound state (residual state).
[0048] Step 6: Detect the element concentration in the leaching solution and leaching residue obtained in step 3, and perform heavy metal environmental risk assessment according to formula (1) and formula (2). The formula is as follows:
[0049]
[0050] Where P sgei is a single element environmental risk; P sge is the comprehensive environmental risk; i Q is the active state content of coal-based solid waste, in mg / L; i is the total amount of heavy metals in coal-based solid waste, in mg / L; C i It is the detection value of heavy metal content in the process of coal-based solid waste utilization, in mg / L; S i is the soil background value in natural state; T i is the toxicity response coefficient;
[0051] Step 7, using any one of precipitation, extraction and adsorption methods to treat the leaching solution obtained in step 3 to enrich and purify the valuable elements, and using formula (1) and formula (2) to evaluate the single element risk and comprehensive risk of the process of enriching and purifying the valuable elements.
[0052] The results obtained from formulas (1) and (2) are graded according to the evaluation criteria of Nemerow comprehensive pollution assessment method and potential ecological risk index method, as shown in Table 1:
[0053] Table 1 Risk level classification
[0054] Ecological risk level <![CDATA[P sgei ]]> <![CDATA[P sge ]]> clean P<1 Ec<1 Low risk 1≤P<4 1≤Ec<10 Medium risk 4≤P<6 10≤Ec<30 High risk P≥6 Ec≥30
[0055] Example 1
[0056] A heavy metal risk assessment method in the comprehensive utilization of coal-based solid waste comprises the following steps:
[0057] Step 1, collect coal-based solid waste samples, crush and fully grind them, place the ground samples in an oven, spread them out evenly and dry them;
[0058] The type of coal-based solid waste in this embodiment is fly ash; the drying temperature of the sample is 180° C.; and the drying time is 24 hours.
[0059] Step 2, mixing the dried sample with sodium carbonate in a uniform proportion, and placing the mixture in a muffle furnace for calcination;
[0060] Sodium carbonate and the sample are uniformly mixed in a ratio of 1.2:1; the roasting temperature is 900°C; and the roasting time is 90 min.
[0061] Step 3, dissolving the roasted sample and hydrochloric acid according to the solid-liquid ratio, heating with microwave, and stirring with magnetic force, cooling to room temperature, and then treating the dissolved solution with centrifuge to obtain leaching solution and leaching residue;
[0062] The solid-liquid ratio of the roasted sample to hydrochloric acid is 1:20; the concentration of hydrochloric acid is 3 mol / L; the microwave heating temperature is 80°C; and the magnetic stirring leaching time is 30 min.
[0063] Step 4, using a mixture of nitric acid and hydrofluoric acid to perform a digestion experiment on the sample dried in step 1 under high temperature and high pressure conditions to obtain the total amount of heavy metal elements in the coal-based solid waste;
[0064] The concentration of nitric acid is 66%; the dosage is 8 ml.
[0065] The concentration of hydrofluoric acid is 40%; the dosage is 4 ml; the temperature is 180°C.
[0066] Step 5: Perform a step-by-step chemical extraction experiment on the sample dried in step 1 using the Tessier five-state step-by-step extraction method to obtain the contents of the five occurrence states of heavy metals, and then obtain the active state content of the coal-based solid waste;
[0067] Step 6: Detect the element concentration in the leaching solution and leaching residue obtained in step 3, and perform heavy metal environmental risk assessment according to formula (1) and formula (2). The formula is as follows:
[0068]
[0069] Where P sgei is a single element environmental risk; P sge is the comprehensive environmental risk; i Q is the active content of coal-based solid waste (exchangeable state, acid-soluble state), in mg / L; i is the total amount of heavy metals in coal-based solid waste, in mg / L; C i It is the detection value of heavy metal content in the process of coal-based solid waste utilization, in mg / L; S i is the soil background value in natural state; T i is the toxicity response coefficient.
[0070] The active state proportion and toxicity response coefficient of each metal element in the fly ash in this embodiment, and the natural background value of the soil are shown in Table 2:
[0071] Table 2 Active state percentage and toxicity response coefficient of each metal element in fly ash, and natural background value of soil
[0072]
[0073]
[0074] The environmental risks of the leachate in this embodiment are shown in Table 3:
[0075] Table 3 Environmental risks of leachate
[0076]
[0077] According to the soil environmental quality standard (GB 15618-1995), the soil background value is obtained. The heavy metal environmental risk of the coal-based solid waste-fly ash utilization process-valuable element leaching stage is compared with Table 1 and Table 3. It can be seen that the heavy metal risk values in the leachate are all less than 1, which belongs to the clean level; while the Cd environmental risk in the leaching residue is greater than 6, which belongs to high risk. The comprehensive risk of the leachate is less than 1, which belongs to the clean level, while the comprehensive risk of the leaching residue is greater than 10, which belongs to the medium risk.
[0078] Example 2
[0079] A heavy metal risk assessment method in the comprehensive utilization of coal-based solid waste comprises the following steps:
[0080] Steps 1-6 are the same as in Example 1.
[0081] Step 7, using the step-by-step precipitation method to treat the leaching solution obtained in step 3, to enrich and purify the valuable elements, and using formula (1) and formula (2) to evaluate the single element risk and comprehensive risk of the process of enriching and purifying the valuable elements.
[0082] Specifically, sodium bicarbonate and hydrochloric acid are used to adjust the pH of the leaching solution to precipitate rare earth elements in steps, with the goal of precipitating a large amount of heavy metals in the pH 0-4.5 process, mainly precipitating relatively pure rare earth elements in the pH 4.5-6 stage, and precipitating the remaining unprecipitated rare earths in the pH 6-7.5 stage. Therefore, the comprehensive risk of harmful elements in the precipitation is higher at pH = 4.5, while it is less in the other two stages, as shown in Table 4:
[0083] Table 4 Environmental risk assessment of heavy metals during the implementation of the step-by-step precipitation method
[0084]
[0085] As shown in Table 4, when pH = 4.5, the comprehensive risk is greater than 1 and less than 4, which is a light risk, while the risk of Cd single element is 2.934532, which is a light risk range, and the other elements are in the clean range. Except for the first stage where the environmental risk is relatively high, the environmental risks at pH = 6 and 7.5 are relatively low. The environmental risk and comprehensive risk of single elements in the waste liquid are also clean.
[0086] Example 3
[0087] A heavy metal risk assessment method in the comprehensive utilization of coal-based solid waste comprises the following steps:
[0088] Steps 1-6 are the same as in Example 1.
[0089] The type of coal-based solid waste in this embodiment is coal gangue, and the valuable element Ga is leached from the coal gangue;
[0090] The active state proportions and toxicity response coefficients of various metal elements in the coal gangue in this embodiment, as well as the natural background values of the soil, are shown in Table 5:
[0091] Table 5 Active state percentage and toxicity response coefficient of each metal element in coal gangue, and natural background value of soil
[0092] element Active state ratio Toxicity response factor Soil natural background value Cr 13.11% 2 90 Pb 23.8% 5 35 Cd 30.3% 30 0.2 Ni 25.9% 5 40 Cu 11.1% 5 35 Zn 20.9% 1 100
[0093] The environmental risks of the leachate in this example are shown in Table 6:
[0094] Table 6 Environmental risks of leachate
[0095]
[0096] The heavy metal environmental risk of coal-based solid waste-coal gangue utilization process-valuable element Ga leaching stage is compared with Table 1 and Table 6. It can be seen that the heavy metal risk value Cd in the leachate is greater than 6, which is a high risk, and the others are less than 1, which is a clean level; while the Cd environmental risk in the leaching residue is greater than 6, which is a high risk, Ni and Cu are greater than 1 and less than 4, which are light risks, and the other elements are clean levels. The comprehensive risk of the leachate is greater than 10, which is a medium risk, and the comprehensive risk of the leaching residue is greater than 30, which is a high risk.
[0097] Example 4
[0098] A heavy metal risk assessment method in the comprehensive utilization of coal-based solid waste comprises the following steps:
[0099] Steps 1-6 are the same as in Example 3.
[0100] The sample is coal-based solid waste - coal gangue, and the valuable element Ga is enriched and purified from the coal gangue leaching solution;
[0101] Step 7: Use the extraction method to treat the leaching solution obtained in step 3 to enrich and purify the valuable element Ga, and use formulas (1) and (2) to evaluate the single element risk and comprehensive risk of the process.
[0102] Specifically, the extractant P507 and the diluent n-heptane were mixed, mixed with the leaching solution in a ratio of 1:1 and shaken to extract the valuable elements to obtain an extract and a raffinate, and then the raffinate was eluted with hydrochloric acid to obtain an eluate and a waste liquid, as shown in Table 7:
[0103] Table 7 Environmental risk assessment of the extraction process
[0104] element Extract Raffinate Eluent Wastewater Cr 0.0212 0.0848 0.0085 0.0127 Pb 0.0749 0.2996 0.0300 0.0449 Cd 4.2723 17.0892 1.7089 2.5634 Ni 0.0772 0.3089 0.0309 0.0463 Cu 0.1201 0.4804 0.0480 0.0721 Zn 0.0222 0.0888 0.0089 0.0133 Comprehensive Risk 4.5879 18.3516 1.8352 2.7527
[0105] By comparing Table 1 and Table 7, it can be seen that the heavy metal environmental risk value Cd in the extract is greater than 4, which is a medium risk, and the rest are less than 1, which is a clean level; the Cd environmental risk in the raffinate is greater than 6, which is a high risk; Cd in the eluate and waste liquid is greater than 1 and less than 4, which is a light risk; except Cd, the other elements are less than 1, which is a clean level; the comprehensive risks of the extract, eluate and waste liquid are all less than 10, which is a light risk, and the comprehensive risk in the raffinate is greater than 10, which is a medium risk.
[0106] In addition, the upper and lower limits and interval values of the process parameters (such as temperature, time, concentration, ratio, dosage, etc.) of the present invention can all achieve the present invention, and the embodiments are not listed one by one here.
[0107] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A heavy metal risk assessment method in the comprehensive utilization of coal-based solid waste, characterized by: The following steps are involved: Step 1, collect coal-based solid waste samples, crush and fully grind them, place the ground samples in an oven, spread them out evenly and dry them; Step 2, mixing the dried sample with sodium carbonate in a uniform proportion, and placing the mixture in a muffle furnace for calcination; Step 3, dissolving the roasted sample and hydrochloric acid according to the solid-liquid ratio, heating with microwave, and stirring with magnetic force at the same time, and after cooling, processing the dissolved solution through a centrifuge to obtain a leachate and leach residue; Step 4, using a mixture of nitric acid and hydrofluoric acid to perform a digestion experiment on the sample dried in step 1 under high temperature and high pressure conditions to obtain the total amount of heavy metal elements in the coal-based solid waste; Step 5, using the Tessier five-state stepwise extraction method to perform a stepwise chemical extraction experiment on the sample dried in step 1 to obtain the contents of the five occurrence states of heavy metals, and then obtain the active state content of the coal-based solid waste; Step 6: Detect the element concentration in the leaching solution and leaching residue obtained in step 3, and perform heavy metal environmental risk assessment according to formula (1) and formula (2). The formula is as follows: Where P sgei is a single element environmental risk; P sge is the comprehensive environmental risk; i Q is the active state content of coal-based solid waste, in mg / L; i is the total amount of heavy metals in coal-based solid waste, in mg / L; C i It is the detection value of heavy metal content in the process of coal-based solid waste utilization, in mg / L; S i is the soil background value in natural state; T i is the toxicity response coefficient; Step 7, using any one of precipitation, extraction and adsorption methods to treat the leaching solution obtained in step 3 to enrich and purify the valuable elements, and using formula (1) and formula (2) to evaluate the single element risk and comprehensive risk of the process of enriching and purifying the valuable elements.
2. The method for heavy metal risk assessment in the comprehensive utilization of coal-based solid waste according to claim 1, characterized in that: In step 1, the types of coal-based solid waste include fly ash, coal gangue, gasification slag and coal liquefaction slag; the drying temperature of the sample is 100-200°C, and the drying time is 18-30h.
3. The method for heavy metal risk assessment in the comprehensive utilization of coal-based solid waste according to claim 1, characterized in that: In step 1, the drying temperature of the sample is 180°C and the drying time is 24h.
4. The method for heavy metal risk assessment in the comprehensive utilization of coal-based solid waste according to claim 1, characterized in that: In step 2, sodium carbonate and the sample are uniformly mixed in a ratio of 1-1.4:1, the roasting temperature is 700-1500° C., and the roasting time is 80-120 min.
5. The method for heavy metal risk assessment in the comprehensive utilization of coal-based solid waste according to claim 1, characterized in that: In step 2, sodium carbonate and the sample are uniformly mixed in a ratio of 1.2:1, and the roasting temperature is 900° C. and the roasting time is 90 min.
6. The method for heavy metal risk assessment in the comprehensive utilization of coal-based solid waste according to claim 1, characterized in that: In step 3, the solid-liquid ratio of the roasted sample to hydrochloric acid is 1:10-1:40, the concentration of hydrochloric acid is 2 mol / L-6 mol / L, the microwave heating temperature is 50-90° C., and the magnetic stirring leaching time is 20-50 min.
7. The method for heavy metal risk assessment in the comprehensive utilization of coal-based solid waste according to claim 1, characterized in that: In step 3, the solid-liquid ratio of the roasted sample to hydrochloric acid is 1:20, the concentration of hydrochloric acid is 3 mol / L, the microwave heating temperature is 80° C., and the magnetic stirring leaching time is 30 min.
8. The method for heavy metal risk assessment in the comprehensive utilization of coal-based solid waste according to claim 1, characterized in that: In step 4, the concentration of nitric acid is 20%-80%, and the amount is 4- 20ml; the concentration of the hydrofluoric acid is 20-80%, the dosage is 2-10ml; the temperature is 150-300°C.
9. The method for heavy metal risk assessment in the comprehensive utilization of coal-based solid waste according to claim 1, characterized in that: In step 4, the concentration of the nitric acid is 66%, and the amount used is 8 ml; the concentration of the hydrofluoric acid is 40%, and the amount used is 4 ml; the temperature is 180°C.
10. The method for heavy metal risk assessment in the comprehensive utilization of coal-based solid waste according to claim 1, characterized in that: In step 5, the five occurrence states of the heavy metals include: metal exchangeable state, carbonate bound state, iron / manganese oxide bound state, organic matter and sulfide bound state, and residue lattice bound state.