Test method and device, electronic equipment and storage medium
By performing multiple heating and cooling tests on tempered glass, the aging level is determined by using the stress value difference, the problem of inaccurate data and high cost of aging test in the prior art is solved, and more accurate and economical Test method.
Patent Information
- Application Number
- CN202410860121.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-28
- Publication Date
- 2024-11-08
AI Technical Summary
In the prior art, testing the aging degree of tempered glass requires destructive shattering, resulting in the inability to use the same piece of glass for front and back testing, resulting in inaccurate data and high cost.
By measuring the initial stress value of the glass to be tested, and performing multiple heating and cooling tests in the preset environment, the aging level is determined using the stress value difference, and the same piece of glass is used for testing, simulating the actual use environment and improving the test accuracy.
Improve the accuracy and efficiency of tests, reduce costs, and solve the problems of inaccurate data and destructive testing.
Smart Images

Figure CN118914526A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to the technical field of glass testing, and in particular to a testing method, device, electronic equipment and storage medium. Background Art
[0002] As the gas stove is used, the tempered glass of the gas stove gradually ages and its explosion resistance will be weakened. Therefore, the degree of aging of the tempered glass is usually determined by testing its explosion resistance. Generally, the explosion resistance of tempered glass is determined by the density of fragments inside the tempered glass. The higher the density of fragments, the less likely it is to automatically burst during use in a high-temperature combustion environment.
[0003] In order to test whether there is a difference in the density of fragments of tempered glass after it has been used for a period of time and before it has been used, the tempered glass needs to be broken into pieces to determine the number of fragments produced within a certain area, so as to obtain the degree of aging of the tempered glass after it has been used for a period of time. This destructive breaking method makes it impossible to determine the density of fragments after it has been used for a period of time and before it has been used using the same tempered glass, resulting in errors in the measurement results and high costs. Summary of the invention
[0004] In order to solve at least one of the above-mentioned technical problems, the present disclosure proposes a testing method, a device, an electronic device and a storage medium.
[0005] According to some embodiments of the present disclosure, a testing method is provided, the testing method comprising:
[0006] Measuring the initial stress value of at least one point to be tested in the glass to be tested;
[0007] Placing the glass to be tested in a preset environment and performing K tests to obtain a target stress value of at least one of the test points in the glass to be tested after the Kth test, where K is a positive integer greater than or equal to 1;
[0008] The aging grade of the glass to be tested is determined based on the difference between the initial stress value and the target stress value of at least one of the points to be tested.
[0009] Based on the above scheme, the glass to be tested is placed in a preset environment for multiple tests, and the aging degree of the glass to be tested is determined according to the change in stress values of multiple test points in the glass to be tested before and after the test. The same glass to be tested is used for testing to determine the aging degree of the glass to be tested, which solves the problem that the aging degree can only be determined by breaking the glass, the same test sample cannot be used before and after the test, the data is inaccurate and the cost is high.
[0010] In some possible implementations, placing the glass to be tested in a preset environment and performing K tests to obtain a target stress value of at least one of the test points in the glass to be tested after the Kth test includes: heating the glass to be tested K times based on a preset temperature, with a heating time being a first preset time; cooling the glass to be tested after each heating by a cooling medium, with a cooling time being a second preset time; and measuring the stress value of at least one of the test points in the glass to be tested after the Kth cooling to obtain the target stress value.
[0011] Based on the above scheme, by repeatedly heating and then cooling the glass to be tested, it is more in line with the actual use environment of tempered glass during application, which helps to improve the accuracy of the target stress value obtained, and then better determine the degree of aging, thereby improving the accuracy of the test.
[0012] In some possible implementations, determining the aging grade of the glass to be tested based on the difference between the initial stress value and the target stress value of at least one of the points to be tested includes:
[0013] Acquire a preset relationship; wherein the preset relationship indicates a corresponding relationship between the difference and the aging level, and the difference is positively correlated with the aging level;
[0014] Based on the difference and the preset relationship, the aging grade of the glass to be tested is determined.
[0015] Based on the above scheme, the preset relationship is obtained based on experimental testing. Therefore, when the stress value difference before and after the test of the glass to be tested obtained by the current test is obtained, combined with the preset relationship, the aging level of the glass to be tested can be determined more accurately, and then the quality of the glass to be tested can be determined.
[0016] In some possible implementations, measuring the initial stress value of at least one point to be tested in the glass to be tested includes: performing an i-th stress value measurement on at least one of the points to be tested to generate an i-th stress value; when a difference between the i-th stress value and the i-1-th stress value meets a preset condition, determining the i-th stress value as the initial stress value of the point to be tested, where i is a positive integer greater than 1.
[0017] Based on the above scheme, multiple stress value measurements are performed on multiple test points of the glass to be tested. When it is determined that the stress value difference between two adjacent measurements of the test point meets the preset conditions, it is determined as the initial stress value corresponding to the test point. The measurement is repeated multiple times to improve the accuracy of the initial stress value of the glass to be tested.
[0018] In some possible embodiments, a cooking mold is placed on the glass to be tested; and heating the glass to be tested K times based on a preset temperature, and the heating time is a first preset time, includes: heating the cooking mold placed on the glass to be tested K times based on a preset temperature, and the heating time is a first preset time.
[0019] Based on the above scheme, a cooking mold is placed on the glass to be tested to simulate the gravity that the tempered glass bears when installed on a gas stove. This can more accurately determine the actual use environment of the glass to be tested and improve the accuracy of the test results.
[0020] In some possible implementations, the cooling medium is gas.
[0021] Based on the above scheme, the glass to be tested is cooled by a gas cooling medium, which not only controls the cost but also expands the contact surface between the cooling medium and the glass to be tested, thereby improving the cooling efficiency.
[0022] In some possible implementations, the cooling medium is generated by a cooling device, and the cooling device is disposed above the glass to be tested.
[0023] Based on the above scheme, the cooling device is arranged above the glass to be tested, and the cooling medium can be sprayed on the glass to be tested in all directions, so that the glass to be tested can be evenly cooled under the action of the cooling medium. While increasing the cooling rate, it also prevents the glass to be tested from self-exploding due to large temperature differences and causing losses.
[0024] According to some other embodiments of the present disclosure, a testing device is provided, comprising: a measuring module, used to measure an initial stress value of at least one point to be tested in a glass to be tested; a testing module, used to place the glass to be tested in a preset environment and perform K tests to obtain a target stress value of at least one point to be tested in the glass to be tested after the Kth test, where K is a positive integer greater than or equal to 1; and a determining module, used to determine an aging grade of the glass to be tested based on a difference between the initial stress value and the target stress value of at least one point to be tested.
[0025] According to some other embodiments of the present disclosure, an electronic device is provided, which includes a processing device and a memory, wherein the memory stores at least one instruction or at least one program, and the at least one instruction or the at least one program is loaded and executed by the processing device to implement the test method described in any one of the above embodiments.
[0026] According to some other embodiments of the present disclosure, a computer-readable storage medium is provided, in which at least one instruction or at least one program is stored. The at least one instruction or the at least one program is loaded by a processing device and executes the test method described in any one of the above embodiments.
[0027] It is to be understood that both the foregoing general description and the following detailed description are exemplary and explanatory only and are not restrictive of the disclosure.
[0028] Further features and aspects of the present disclosure will become apparent from the following detailed description of exemplary embodiments with reference to the attached drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] In order to more clearly illustrate the technical solutions and advantages in the embodiments of this specification or the prior art, the drawings required for use in the embodiments or the prior art descriptions are briefly introduced below. Obviously, the drawings described below are only some embodiments of this specification. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0030] Figure 1 A schematic diagram showing a flow chart of a testing method according to an embodiment of the present disclosure;
[0031] Figure 2 A schematic diagram of a process for obtaining an initial stress value according to an embodiment of the present disclosure is shown;
[0032] Figure 3 A schematic diagram of a process for obtaining a target stress value according to an embodiment of the present disclosure is shown;
[0033] Figure 4 A block diagram of a testing device according to an embodiment of the present disclosure is shown. DETAILED DESCRIPTION
[0034] The following will be combined with the drawings in the embodiments of this specification to clearly and completely describe the technical solutions in the embodiments of this specification. Obviously, the described embodiments are only part of the embodiments of this specification, not all of the embodiments. Based on the embodiments in this specification, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0035] It should be noted that the terms "first", "second", etc. in the specification and claims of the present invention and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the data used in this way can be interchangeable where appropriate, so that the embodiments of the present invention described herein can be implemented in an order other than those illustrated or described herein. In addition, the terms "including" and "having" and any variations thereof are intended to cover non-exclusive inclusions, for example, a process, method, system, product, or server that includes a series of steps or units is not necessarily limited to those steps or units clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products, or devices.
[0036] Various exemplary embodiments, features and aspects of the present disclosure will be described in detail below with reference to the accompanying drawings. The same reference numerals in the accompanying drawings represent elements with the same or similar functions. Although various aspects of the embodiments are shown in the accompanying drawings, the drawings are not necessarily drawn to scale unless otherwise specified.
[0037] The word “exemplary” is used exclusively herein to mean “serving as an example, example, or illustration.” Any embodiment described herein as “exemplary” is not necessarily to be construed as preferred or advantageous over other embodiments.
[0038] The term "and / or" herein is only a description of the association relationship of the associated objects, indicating that there may be three relationships. For example, A and / or B can represent: A exists alone, A and B exist at the same time, and B exists alone. In addition, the term "at least one" herein represents any combination of at least two of any one or more of a plurality of. For example, including at least one of A, B, and C can represent including any one or more elements selected from the set consisting of A, B, and C.
[0039] In addition, in order to better illustrate the present disclosure, numerous specific details are given in the following specific embodiments. It should be understood by those skilled in the art that the present disclosure can also be implemented without certain specific details. In some examples, methods, means, components and circuits well known to those skilled in the art are not described in detail in order to highlight the subject matter of the present disclosure.
[0040] At present, the aging degree of tempered glass is determined by its explosion resistance. The tempered glass is broken into pieces at a position about 20 mm away from the periphery on the center line of the longest side of the sample using a small hammer or punch with a tip curvature radius of 0.2 mm and an error of 0.05 mm. A square counting frame with a side length of 50 mm is used to count the number of fragments in the frame. No through cracks can exist in each fragment. Fragments crossing the edge of the counting frame are counted as 0.5 fragments. The density of the fragments is then calculated to determine the aging degree of the tempered glass after a period of use.
[0041] In this way, each time the density of tempered glass fragments is calculated, the tempered glass must be broken destructively first, which results in the tempered glass tested before use and the tempered glass tested after use being different, and only different samples from the same batch can be used to test the density of fragments before and after use. Even samples from the same batch will have slight differences, which will also cause the test results to be inaccurate, and this test method will destroy at least two pieces of tempered glass for each test, which is costly.
[0042] In order to solve the above technical problems, the embodiment of the present disclosure provides a testing method, which includes measuring the initial stress value of at least one test point in the glass to be tested, placing the glass to be tested in a preset environment for K tests, and determining the aging level of the glass to be tested based on the difference between the target stress value of at least one test point obtained after the Kth test and the initial stress value. The testing method of the embodiment of the present disclosure uses the same glass to be tested to determine the aging degree of the glass to be tested, and the test results are more accurate, which solves the problem that the same test sample cannot be used before and after the test because the aging degree can only be determined by breaking the glass, which results in inaccurate data and high costs.
[0043] Please refer to Figure 1 , Figure 1 A flow chart of a testing method according to an embodiment of the present disclosure is shown, and the testing method comprises:
[0044] S101: measuring the initial stress value of at least one point to be tested in the glass to be tested.
[0045] Specifically, the glass to be tested may be tempered glass used on equipment that needs to be resistant to high temperatures, such as tempered glass on a kitchen stove, which may be an oven, a gas stove, etc.; or tempered glass on furniture, which may be a coffee table, a dining table, etc.; in this embodiment, the glass to be tested is tempered glass used on a gas stove.
[0046] Specifically, the number of the points to be tested is a preset value, and the number of the points to be tested is represented by M; optionally, the number of the points to be tested may be 10, 15 or 20; preferably, the number of the points to be tested is 15.
[0047] Specifically, the initial stress value can be obtained by any measurement method that will not cause damage to the tempered glass. Optionally, in this embodiment, the initial stress value can be measured by a laser stress tester; by using a laser stress tester to measure the stress value, the operator does not need to directly contact a high temperature or dangerous test environment, which improves the safety of the measurement. At the same time, it will not cause physical damage to the glass to be tested, ensuring the integrity of the product and not affecting subsequent tests.
[0048] Optionally, the initial stress value may also be measured by X-ray diffraction, refractive index, scanning electron microscopy combined with microcrack detection, Raman spectroscopy, and the like.
[0049] Optionally, the initial stress value may also be determined by measuring the speed at which sound waves propagate in the tempered glass. Stress may affect the speed at which sound waves propagate, thereby indirectly measuring the stress value of the tempered glass.
[0050] S102: placing the glass to be tested in a preset environment and performing K tests to obtain a target stress value of at least one of the test points in the glass to be tested after the Kth test, where K is a positive integer greater than or equal to 1.
[0051] Specifically, K is a preset value; optionally, K may be 5, or any other value such as 10 or 20; preferably, K is 5.
[0052] Specifically, the preset environment is set based on the actual application scenario of the gas stove, including a heating environment and a cooling environment. By repeatedly performing a cycle of heating and cooling the glass to be tested, the actual gas stove usage environment is simulated so that the stress value change of the tempered glass of the gas stove after a period of actual use can be obtained.
[0053] S103: Determine the aging grade of the glass to be tested based on the difference between the initial stress value and the target stress value of at least one of the points to be tested.
[0054] Specifically, the number of the points to be tested is represented by M; the value of M may be 10, 15 or 20; preferably, the number of the points to be tested is 15.
[0055] In a possible implementation manner, the initial stress value corresponding to the point to be measured can be expressed as Q n The target stress value can be expressed as P n Indicates that the difference between the initial stress value and the target stress value is Q, n is an integer greater than or equal to 1 and less than or equal to M.
[0056] In a possible implementation, determining the aging grade of the glass to be tested based on the difference between the initial stress value and the target stress value of at least one of the test points includes: acquiring a preset relationship; wherein the preset relationship indicates a corresponding relationship between the difference and the aging grade, and the difference is positively correlated with the aging grade; and determining the aging grade of the glass to be tested based on the difference and the preset relationship.
[0057] Specifically, the preset relationship can be obtained through experimental measurement; specifically, the preset relationship can be obtained by conducting a breakage experiment after obtaining the stress value difference based on the test method in advance, and statistically generating the difficulty of breaking the glass to be tested corresponding to different differences, or it can be obtained through theoretical calculation simulation experiments.
[0058] Specifically, the larger the difference is, the higher the aging grade of the glass to be tested is, which indicates that the aging degree of the glass to be tested is more serious and the quality is worse; the smaller the difference is, the lower the aging grade of the glass to be tested is, which indicates that the aging degree of the glass to be tested is lighter and the quality is better.
[0059] In an embodiment of the present invention, the glass to be tested is placed in a preset environment for multiple tests, and an aging grade indicating the aging degree of the glass to be tested is determined according to the stress value changes at multiple test points in the glass to be tested before and after the test. The same glass to be tested is used for testing to determine the aging degree of the glass to be tested, and the test result is more accurate, which solves the problem that the aging degree can only be determined by breaking the glass, the same test sample cannot be used before and after the test, the data is inaccurate, and the cost is high.
[0060] Figure 2 A schematic diagram of a process for obtaining an initial stress value according to an embodiment of the present disclosure is shown. Figure 2 As shown, the measuring of the initial stress value of at least one point to be tested in the tested glass includes:
[0061] S201: performing an i-th stress value measurement on at least one of the points to be measured to generate an i-th stress value;
[0062] S202: When the difference between the i-th stress value and the i-1-th stress value meets a preset condition, the i-th stress value is determined as the initial stress value of the point to be measured, where i is a positive integer greater than 1.
[0063] Specifically, the preset condition is that the difference is not greater than 2 percent of the (i-1)th stress value; and the point to be measured may be preset.
[0064] Specifically, the stress value of the nth point to be measured is measured i times until the i-th stress value P' obtained by the i-th measurement is i The stress value P' obtained from the last measurement is i-1 The difference between In the case of i As the initial stress value P of the nth test point n Here, n is an integer greater than or equal to 1 and less than or equal to M, and i is a positive integer greater than or equal to 1.
[0065] In this way, the initial stress value can be determined more accurately by continuously measuring and comparing the stress values obtained from two measurements. This process can be performed manually or with the help of automated equipment and computer programs to simplify the operation, thereby reducing human operation errors and testing time.
[0066] Figure 3 A schematic diagram of a process for obtaining a target stress value according to an embodiment of the present disclosure is shown as follows: Figure 3 As shown, the glass to be tested is placed in a preset environment for K tests to obtain a target stress value of at least one of the test points in the glass to be tested after the Kth test, including:
[0067] S301: heating the glass to be tested K times based on a preset temperature, and the heating time is a first preset time;
[0068] Specifically, the first preset time length is a preset value; illustratively, the first preset time length may be 30 minutes, or 45 minutes or 60 minutes; preferably, the first preset time length is 30 minutes.
[0069] Specifically, the preset temperature is a preset temperature, and the preset temperature can be any temperature value between 800 degrees Celsius and 1800 degrees Celsius; exemplarily, the preset temperature can be 900 degrees Celsius or 1400 degrees Celsius; preferably, the preset temperature is 1300 degrees Celsius.
[0070] Optionally, the preset temperature can be achieved by burning a combustion medium, wherein the combustion medium is generated by a heating device installed on the glass to be tested.
[0071] Optionally, the combustion medium may be natural gas, propane or butane, etc.; preferably, the combustion medium is natural gas, which can be closer to the actual use environment of the gas stove in life, making the test result more accurate and the cost lower.
[0072] In an optional embodiment, the glass to be tested is directly heated for a first preset time period based on burning the combustion medium to reach a preset temperature.
[0073] In an alternative embodiment, a cooking mold is placed on the glass to be tested; the above step S301 also includes: heating the cooking mold placed on the glass to be tested K times based on a preset temperature, and the heating time is a first preset time.
[0074] Specifically, the cooking mold has a preset weight, and the diameter of the contact surface between the cooking mold and the combustion medium is a preset length.
[0075] Optionally, the preset weight can be a preset value, or it can be dynamically adjusted based on different test requirements. The preset weight is achieved by placing a heat-resistant object in the cooking mold, and the heat-resistant object includes but is not limited to sand, salt rock blocks, cast iron blocks, fire bricks, etc., which are not specifically limited here. In this way, by setting a certain weight on the cooking mold to increase the pressure on the glass to be tested, on the basis of making the test environment closer to the actual use scenario of the gas stove, by adding a heat-resistant object in the cooking mold, it is possible to ensure that the cooking mold maintains a relatively stable temperature during the heating process, thereby extending the service life of the cooking mold.
[0076] Optionally, the preset weight may be 6 kg, 8 kg or 12 kg; preferably, the preset weight is 8 kg.
[0077] In an optional embodiment, 8 kg of fine sand may be placed in the cooking mold, and the cooking mold with the fine sand may be placed on the glass to be tested, and the cooking mold may be heated for a first preset time by burning a combustion medium to reach a preset temperature.
[0078] It should be noted that sand is a material with good thermal conductivity, which can effectively absorb and transfer heat to achieve more uniform heating. It also has a certain heat capacity and thermal inertia, which can maintain a relatively stable temperature during the heating process, reduce the direct contact of the combustion medium with the cooking mold, and extend the service life of the cooking mold.
[0079] Optionally, the preset length may be a preset value, or may be dynamically adjusted based on different test requirements, and the preset length is proportional to the heating area of the cooking mold.
[0080] Optionally, the preset length may be 22 cm, 30 cm or 35 cm; preferably, the preset length is 30 cm.
[0081] Specifically, the preset length determines the size of the contact surface. If the preset length of the diameter is larger, the contact surface between the cooking mold and the combustion medium is larger, and during the heating process, the heated area of the glass to be tested is larger. If the preset length of the diameter is smaller, the contact surface between the cooking mold and the combustion medium is smaller, and during the heating process, the heated area of the glass to be tested is smaller. In this way, the heated area of the glass to be tested can be adjusted by adjusting the preset length, which is more in line with the heating conditions of tempered glass in the actual application process of gas stoves.
[0082] It should be noted that by setting a cooking mold on the glass to be tested and heating the cooking mold multiple times, on the basis of making the preset environment more in line with the actual use environment of the gas stove, local testing of the glass to be tested can also be achieved. Compared with the overall test, the cost is lower and the test efficiency is higher.
[0083] S302: Cooling the glass to be tested after each heating by a cooling medium, wherein the cooling time is a second preset time;
[0084] Specifically, the second preset time length is an arbitrary pre-set value. For example, the second preset time length may be 15 minutes, 20 minutes or 40 minutes; preferably, the second preset time length is 20 minutes.
[0085] In an optional embodiment, the cooling medium is gas.
[0086] Optionally, the cooling medium can be air, nitrogen, argon, etc. Cooling the glass to be tested by means of a gas cooling medium can provide efficient heat exchange, so that the medium reaches the required temperature in a shorter time, and has strong controllability, and is easy to adjust and control to meet different process requirements and temperature requirements; at the same time, the gas cooling medium can complete the cooling process more efficiently, thereby reducing energy consumption, and is safer and does not generate pollution. Preferably, in this embodiment, the cooling medium is air.
[0087] In an optional embodiment, the cooling medium is generated by a cooling device, and the cooling device is arranged above the glass to be tested.
[0088] Specifically, the cooling device can be a nozzle, or a cooling tower, a cooling fan, etc.; the cooling device is arranged above the glass to be tested, and the cooling device is installed at a preset distance from the upper surface of the glass to be tested, and the preset distance can be dynamically adjusted. In this embodiment, the cooling device is a nozzle, and the length of the preset distance is proportional to the spraying range. The cooling medium is installed 10 cm above the glass to be tested, so that the cooling medium can be sprayed to a larger area to improve the cooling efficiency.
[0089] It should be noted that, by using the nozzle as a spraying device for the gas cooling medium, the cooling medium can be evenly sprayed on the surface of the heated glass to be tested, ensuring that the entire surface can be evenly cooled to avoid excessive local temperature differences. At the same time, the nozzle has a wide spray range and can complete the cooling of the object in a shorter time, with high cooling efficiency. By controlling the spray range, the cooling medium can be accurately sprayed on the area that needs cooling, saving resources.
[0090] In an alternative embodiment, the cooling rate can be changed by adjusting the pressure of the cooling medium generated by the cooling device; the cooling rate is positively correlated with the pressure of the cooling medium.
[0091] In this embodiment, the cooling medium is gas. When the pressure of the cooling medium increases, the average kinetic energy of the gas cooling medium output by the cooling device also increases, and the collisions between molecules become more frequent and intense, thereby accelerating the heat transfer speed and improving the cooling rate.
[0092] Optionally, the cooling medium pressure is 0.2 MPa, the cooling medium pressure may also be 0.3 MPa or 0.1 MPa, etc., which may be dynamically adjusted based on different requirements.
[0093] In an alternative embodiment, the glass to be tested may be cooled naturally after each heating.
[0094] S303: measuring the stress value of at least one of the test points in the test glass after the K-th cooling to obtain the target stress value.
[0095] Specifically, the method for measuring the target stress value of the test point is the same as the method for measuring the initial stress value, which will not be described in detail here.
[0096] In this embodiment, by measuring the initial stress value of at least one test point in the glass to be tested, and placing the glass to be tested in a preset environment for K tests, the aging level of the glass to be tested is determined based on the difference between the target stress value of at least one test point obtained after the Kth test and the initial stress value. The test method of the disclosed embodiment uses the same glass to be tested to determine the aging degree of the glass to be tested, and the test result is more accurate, which solves the problem that the aging degree can only be determined by breaking the glass, the same test sample cannot be used before and after the test, the data is inaccurate, and the cost is high.
[0097] The following is a specific example to illustrate the test method described in the embodiment of the present invention:
[0098] Step 1: Measure the initial stress value of at least one test point in the glass to be tested.
[0099] Specifically, the glass to be tested is tempered glass installed on a gas stove. 15 test points are determined by a preset positioning mold, and stress values of the 15 test points on the surface of the glass to be tested are measured by a portable intelligent laser glass stress analyzer.
[0100] Specifically, the number of points to be measured is represented by M, and n is an integer greater than or equal to 1 and less than or equal to M; here, M is 15, and n is an integer greater than or equal to 1 and less than or equal to 15. During the measurement process, the value of n is increased by 1 from 1 to 15 in sequence, and the stress values of the 15 points to be measured are measured in sequence.
[0101] The stress value of the nth point to be measured is measured i times until the i-th stress value P' obtained by the i-th measurement is i The stress value P' obtained from the last measurement is i-1 The difference between In the case of i As the initial stress value P of the nth test point n Here, i is a positive integer greater than or equal to 1.
[0102] In this way, the initial stress value can be determined more accurately by continuously measuring and comparing the stress values obtained from two measurements. This process can be performed manually or with the help of automated equipment and computer programs to simplify the operation, thereby reducing human operation errors and testing time.
[0103] Step 2: placing the glass to be tested in a preset environment and performing K tests to obtain a target stress value of at least one of the test points in the glass to be tested after the Kth test, where K is a positive integer greater than or equal to 1.
[0104] Specifically, in this embodiment, K is 5, and the ambient temperature of the preset environment is 20 degrees Celsius; it should be noted that the ambient temperature is controlled between 15 degrees Celsius and 25 degrees Celsius. In this way, the influence of the ambient temperature on the test results can be avoided, and it is more in line with the ambient temperature of the actual use environment of the gas stove, thereby improving the test accuracy.
[0105] Step 2.1: A cooking mold is placed on the glass to be tested, and the cooking mold is heated based on a preset temperature, and the heating time is a first preset time.
[0106] Specifically, the cooking mold has a preset weight, and the diameter of the contact surface between the cooking mold and the combustion medium is a preset length; the first preset time is pre-set, and the preset temperature is a preset temperature, and the preset temperature is proportional to the pressure of the burning combustion medium.
[0107] In this embodiment, the cooking mold is a 33 cm flat-bottomed cast iron pot containing 8 kg of fine sand; the diameter of the contact surface between the cast iron pot and the combustion medium is 29.5 cm, the first preset time is 30 minutes, the preset temperature is 1300 degrees Celsius, and the preset temperature is reached by burning natural gas. The natural gas pressure is 3000 Pa, which is generated by a heating device installed on the glass to be tested.
[0108] Specifically, 3000Pa of natural gas is output through the heating device and fully burned to heat 8 kg of fine sand in the flat-bottomed cast iron pot for 30 minutes. The heated area of the glass to be tested is the area radiated by the flame when the flat-bottomed cast iron pot is heated. After completing the 30-minute heating operation, step 2.2 is performed.
[0109] It should be noted that sand is a material with good thermal conductivity, which can effectively absorb and transfer heat to achieve more uniform heating; and it has a certain heat capacity and thermal inertia, which can maintain a relatively stable temperature during the heating process, reduce the direct contact of the combustion medium with the cooking mold, and extend the service life of the cooking mold; by setting the cooking mold on the glass to be tested and heating the cooking mold multiple times, while making the preset environment more in line with the actual use environment of the gas stove, it is also possible to perform local testing on the glass to be tested. Compared with the overall test, the cost is lower and the test efficiency is higher.
[0110] Step 2.2: Cooling the heated glass to be tested by a cooling medium, wherein the cooling time is a second preset time.
[0111] Specifically, the cooling medium is gas, and the pressure of the cooling medium is 0.2 MPa; the cooling medium is generated by a cooling device, and the cooling device is installed at a preset distance from the upper surface of the glass to be tested.
[0112] Optionally, the cooling medium can be air, nitrogen, argon, etc.; the cooling medium pressure can be a preset value or can be dynamically adjusted; the cooling device can be a nozzle, or a cooling tower, a cooling fan, etc.; the second preset time length is an arbitrary pre-set value.
[0113] In this embodiment, the cooling medium is air, the cooling device is a nozzle, and the second preset time is 20 minutes. Specifically, a copper spray nozzle is installed 10 cm above the center of the cooking mold, and the compressed air pressure output by the nozzle is 0.2 MPa. After the gas stove is ignited and burned for 30 minutes, the fire is turned off, and the compressed air valve is opened to cool the cooking mold for 20 minutes.
[0114] Determine the number of cooling times. When the number of cooling times reaches K times, execute step 2.3; when the number of cooling times does not reach K times, execute step 2.1.
[0115] Step 2.3: Measure the stress value of at least one of the points to be measured in the glass to be measured after the Kth cooling to obtain the target stress value.
[0116] The initial stress value corresponding to the point to be measured can be represented by Q n and the target stress value can be represented by P n The difference between the initial stress value and the target stress value is Q.
[0117] Step 3: Based on the difference between the initial stress value and the target stress value of at least one of the points to be measured, determine the aging grade of the glass to be measured.
[0118] Specifically, based on the preset relationship and the difference, determine the aging grade; the preset relationship indicates the corresponding relationship between the difference and the aging grade; the aging grade is positively correlated with the difference. The preset relationship is as follows:
[0119] When it is determined that the difference Q ≤ 1, determine that the aging grade of the glass to be measured is grade 1;
[0120] When it is determined that the difference 1 < Q ≤ 2, determine that the aging grade of the glass to be measured is grade 2;
[0121] When it is determined that the difference 2 < Q ≤ 3, determine that the aging grade of the glass to be measured is grade 3;
[0122] When it is determined that the difference Q > 3, determine that the aging grade of the glass to be measured is grade 4.
[0123] Specifically, the aging grade is proportional to the difference. The larger the difference, the higher the aging grade of the glass to be measured, indicating that the aging degree of the glass to be measured is more serious and the quality is worse; the smaller the difference, the lower the aging grade of the glass to be measured, indicating that the aging degree of the glass to be measured is lighter and the quality is better. In this way, it is realized to determine the aging grade indicating the aging degree of the glass to be measured through the change amount of the stress values of multiple measurement points in the glass to be measured before and after the test, and then determine the quality of the glass to be measured based on the aging degree.
[0124] In an embodiment of the present invention, the glass to be tested is placed in a preset environment for multiple tests, and an aging grade indicating the aging degree of the glass to be tested is determined according to the stress value changes at multiple test points in the glass to be tested before and after the test. The same glass to be tested is used for testing to determine the aging degree of the glass to be tested, and the test result is more accurate, which solves the problem that the aging degree can only be determined by breaking the glass, the same test sample cannot be used before and after the test, the data is inaccurate, and the cost is high.
[0125] Please refer to Figure 4 , which shows a block diagram of a test device provided by an embodiment of the present application. The test device has the function of implementing the above method example, and the function can be implemented by hardware or by hardware executing corresponding software. The test device may include:
[0126] The measuring module 410 is used to measure the initial stress value of at least one point to be measured in the glass to be measured;
[0127] A testing module 420 is used to place the glass to be tested in a preset environment and perform K tests to obtain a target stress value of at least one of the test points in the glass to be tested after the Kth test, where K is a positive integer greater than or equal to 1;
[0128] The determination module 430 is used to determine the aging grade of the glass to be tested based on the difference between the initial stress value and the target stress value of at least one of the points to be tested.
[0129] In an optional implementation, the testing module 420 is further configured to:
[0130] Heating the glass to be tested K times based on a preset temperature, and the heating time is a first preset time;
[0131] Cooling the glass to be tested after each heating by a cooling medium, wherein the cooling time is a second preset time;
[0132] The stress value of at least one of the test points in the test glass after the K-th cooling is measured to obtain the target stress value.
[0133] In an optional implementation manner, the determining module 430 is further configured to:
[0134] Acquire a preset relationship; wherein the preset relationship indicates a corresponding relationship between the difference and the aging level, and the difference is positively correlated with the aging level;
[0135] Based on the difference and the preset relationship, the aging grade of the glass to be tested is determined.
[0136] In an optional implementation, the measurement module 410 is further configured to:
[0137] Performing an i-th stress value measurement on at least one of the points to be measured to generate an i-th stress value;
[0138] When the difference between the i-th stress value and the i-1-th stress value meets a preset condition, the i-th stress value is determined as the initial stress value of the point to be measured, where i is a positive integer greater than 1.
[0139] In an optional embodiment, a cooking mold is placed on the glass to be tested;
[0140] The testing module 420 is also used for:
[0141] The cooking mold placed on the glass to be tested is heated K times based on a preset temperature, and the heating time is a first preset time.
[0142] In an optional embodiment, the cooling medium is gas.
[0143] In an optional implementation, the cooling medium is generated by a cooling device, and the cooling device is disposed above the glass to be tested.
[0144] The present application also provides another testing device, which includes a processor and a memory, wherein the memory stores at least one instruction or at least one program, and the at least one instruction or at least one program is loaded and executed by the processor to implement any of the testing methods described above.
[0145] The present application also provides a computer-readable storage medium, in which at least one instruction or at least one program is stored, and the at least one instruction or at least one program is loaded and executed by a processor to implement any of the test methods described above.
[0146] In some embodiments, the computer device (not shown) may include a processor, a memory, and a network interface connected via a system bus. The processor of the computer device is used to provide computing and control capabilities. The memory of the computer device includes a non-volatile storage medium and an internal memory. The non-volatile storage medium stores an operating system, a computer program, and a database. The internal memory provides an environment for the operation of the operating system and the computer program in the non-volatile storage medium. The network interface of the computer device is used to communicate with an external terminal via a network connection. When the computer program is executed by the processor, a test method is implemented.
[0147] It should be noted that the above-mentioned sequence of the embodiments of the present application is for description only and does not represent the advantages and disadvantages of the embodiments. The above-mentioned specific embodiments of this specification are described. Other embodiments are within the scope of the attached claims. In some cases, the actions or steps recorded in the claims can be performed in an order different from that in the embodiments and still achieve the desired results. In addition, the processes depicted in the drawings do not necessarily require the specific order or continuous order shown to achieve the desired results. In some embodiments, multitasking and parallel processing are also possible or may be advantageous.
[0148] Each embodiment in this specification is described in a progressive manner, and the same or similar parts between the embodiments can be referred to each other, and each embodiment focuses on the differences from other embodiments. In particular, for the device and server embodiments, since they are basically similar to the method embodiments, the description is relatively simple, and the relevant parts can be referred to the partial description of the method embodiments.
[0149] A person skilled in the art will understand that all or part of the steps to implement the above embodiments may be accomplished by hardware or by instructing related hardware through a program, and the program may be stored in a computer-readable storage medium, and the above-mentioned storage medium may be a read-only memory, a disk or an optical disk, etc.
[0150] The embodiments of the present disclosure have been described above, and the above description is exemplary, not exhaustive, and is not limited to the disclosed embodiments. Many modifications and changes will be apparent to those of ordinary skill in the art without departing from the scope and spirit of the described embodiments. The selection of terms used herein is intended to best explain the principles of the embodiments, practical applications, or technical improvements in the market, or to enable other persons of ordinary skill in the art to understand the embodiments disclosed herein.
Claims
1. A testing method, characterized in that: The test method includes: Measuring the initial stress value of at least one point to be tested in the glass to be tested; Placing the glass to be tested in a preset environment and performing K tests to obtain a target stress value of at least one of the test points in the glass to be tested after the Kth test, where K is a positive integer greater than or equal to 1; The aging grade of the glass to be tested is determined based on the difference between the initial stress value and the target stress value of at least one of the points to be tested.
2. The method according to claim 1, characterized in that Placing the glass to be tested in a preset environment and performing K tests to obtain a target stress value of at least one of the test points in the glass to be tested after the Kth test includes: Heating the glass to be tested K times based on a preset temperature, and the heating time is a first preset time; Cooling the glass to be tested after each heating by a cooling medium, wherein the cooling time is a second preset time; The stress value of at least one of the test points in the test glass after the K-th cooling is measured to obtain the target stress value.
3. The method according to claim 1 or 2, wherein determining the aging grade of the glass to be tested based on the difference between the initial stress value and the target stress value of at least one of the test points comprises: Acquire a preset relationship; wherein the preset relationship indicates a corresponding relationship between the difference and the aging level, and the difference is positively correlated with the aging level; Based on the difference and the preset relationship, the aging grade of the glass to be tested is determined.
4. The method according to claim 1, characterized in that: The step of measuring the initial stress value of at least one point to be tested in the glass to be tested comprises: Performing an i-th stress value measurement on at least one of the points to be measured to generate an i-th stress value; When the difference between the i-th stress value and the i-1-th stress value meets a preset condition, the i-th stress value is determined as the initial stress value of the point to be measured, where i is a positive integer greater than 1.
5. The method according to claim 2, characterized in that: A cooking mold is placed on the glass to be tested; The step of heating the glass to be tested K times based on a preset temperature, wherein the heating time is a first preset time, comprises: The cooking mold placed on the glass to be tested is heated K times based on a preset temperature, and the heating time is a first preset time.
6. The method according to claim 2, characterized in that The cooling medium is gas.
7. The method according to claim 2 or 3, characterized in that: The cooling medium is generated by a cooling device, and the cooling device is arranged above the glass to be tested.
8. A testing device, characterized in that: The testing device comprises: A measuring module, used for measuring the initial stress value of at least one point to be tested in the glass to be tested; A testing module, used for placing the glass to be tested in a preset environment and performing K tests to obtain a target stress value of at least one of the test points in the glass to be tested after the Kth test, where K is a positive integer greater than or equal to 1; The determination module is used to determine the aging grade of the glass to be tested based on the difference between the initial stress value and the target stress value of at least one of the points to be tested.
9. An electronic device, characterized in that: The device includes a processing device and a memory, wherein the memory stores at least one instruction or at least one program, and the at least one instruction or the at least one program is loaded and executed by the processing device to implement the testing method according to any one of claims 1 to 7.
10. A computer-readable storage medium, characterized in that: The storage medium stores at least one instruction or at least one program, and the at least one instruction or the at least one program is loaded by a processing device and executes the testing method according to any one of claims 1 to 7.