Establishment method and device of OPC (Optical Proximity Correction) model, optical proximity correction method and equipment, and storage medium

By converting post-etching measurements to post-development measurements during the OPC model establishment process, the problem of large OPC model errors was solved, and higher precision optical proximity correction was achieved.

CN118915374APending Publication Date: 2024-11-08ZHEJIANG ICSPROUT SEMICONDUCTOR CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411231854.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-03
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The existing OPC model has large errors, which affects the accuracy and efficiency of optical proximity correction.

Method used

The etched layer is measured using a measurement instrument to obtain the post-etching measurement values, which are then converted into post-development measurement values. An OPC model is then established based on the post-development measurement values.

Benefits of technology

It improves the accuracy and precision of the OPC model, reduces the error of optical proximity correction, and improves the quality of lithographic pattern transfer.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118915374A_ABST
    Figure CN118915374A_ABST
Patent Text Reader

Abstract

The invention discloses an OPC model establishing method and device, an optical proximity correction method and equipment and a storage medium, and the method comprises the steps: forming a semiconductor structure which is provided with an etched layer; measuring the etched layer through a measuring machine to obtain a measured value after etching; the measurement value after etching is converted into a corresponding measurement value after developing; and establishing an OPC model according to the measured value after development. The contour definition of the pattern in the etched layer is higher, the measured value after etching obtained by a measuring machine is higher in accuracy and precision, the error of the OPC model established on the basis of the measured value after developing obtained by converting the measured value after etching is smaller, the precision is higher, the error of the optical proximity correction method is reduced, and the correction precision is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of photolithography, and in particular to an OPC model establishment method and device, an optical proximity correction method and equipment, and a storage medium. Background Art

[0002] In the semiconductor manufacturing process, in order to transfer the circuit pattern of an integrated circuit (IC) to a semiconductor chip, the circuit pattern of the integrated circuit needs to be designed as a mask pattern, and then the mask pattern is transferred from the mask surface to the semiconductor chip.

[0003] As the critical dimension (CD) of integrated circuits shrinks and is affected by the resolution limit of the optical exposure tool (OET), the optical proximity effect (OPE) is easily generated when the high-density mask pattern is exposed for pattern transfer, causing defects in the mask pattern transfer. To address the problem of optical proximity effect, a method currently commonly used in the industry is optical proximity correction (OPC), which reduces the deviation of the lithography pattern obtained by exposure by changing the shape of the original layout pattern.

[0004] One optical proximity correction method is to perform correction based on a model, and the key to this correction method is to establish an accurate OPC model. However, the OPC model established by the existing method often has a large error problem. Summary of the invention

[0005] The problem solved by the present invention is how to reduce the error of the OPC model.

[0006] To solve the above problems, the present invention provides a method for establishing an OPC model, comprising:

[0007] A semiconductor structure is formed, wherein the semiconductor structure has an etched layer; the etched layer is measured by a measuring machine to obtain a post-etching measurement value; the post-etching measurement value is converted into a corresponding post-development measurement value; and an OPC model is established according to the post-development measurement value.

[0008] Optionally, in the step of measuring the etched layer by a measuring machine to obtain a post-etching measurement value, the measuring machine is a feature dimension scanning electron microscope.

[0009] Optionally, in the step of converting the post-etching measurement value into the corresponding post-developing measurement value, the post-etching measurement value is converted into the corresponding post-developing measurement value according to a global deviation, wherein the global deviation is the difference between the post-etching measurement value and the post-developing measurement value.

[0010] Optionally, the method further includes: measuring the etched layer by a measuring machine, and after obtaining a post-etching measurement value, before converting the post-etching measurement value into a corresponding post-development measurement value, clearing invalid data in the obtained post-etching measurement value.

[0011] Optionally, the method further includes: after establishing an OPC model according to the post-development measurement value, verifying the OPC model.

[0012] Optionally, the steps of forming a semiconductor structure include: providing a layer to be etched; forming a photoresist on the layer to be etched; patterning the photoresist to form a patterned photoresist; and etching the layer to be etched using the patterned photoresist as a mask to form the etched layer.

[0013] Accordingly, the present invention also provides an optical proximity correction method, comprising:

[0014] Obtain a design layout; establish an OPC model, wherein the OPC model is established by the establishment method of the present invention; and use the OPC model to modify the design layout to obtain a tape-out layout.

[0015] Optionally, in the step of obtaining a design layout, the design layout is a design layout of a contact hole layer.

[0016] In addition, the present invention also provides an OPC model establishment device, comprising:

[0017] A process unit, wherein the process unit is suitable for forming a semiconductor structure, wherein the semiconductor structure has an etched layer; a measurement unit, wherein the measurement unit is suitable for measuring the etched layer to obtain a post-etching measurement value; a conversion unit, wherein the conversion unit is suitable for converting the post-etching measurement value into a corresponding post-development measurement value; and a modeling unit, wherein the modeling unit is suitable for establishing an OPC model according to the post-development measurement value.

[0018] Optionally, the measurement unit includes: a characteristic dimension scanning electron microscope.

[0019] Optionally, the conversion unit converts the post-etching measurement value into a corresponding post-developing measurement value according to a global deviation, wherein the global deviation is a difference between the post-etching measurement value and the post-developing measurement value.

[0020] Optionally, it also includes: a clearing unit, which is suitable for clearing invalid data in the obtained post-etching measurement values.

[0021] Optionally, it further includes: a verification unit, wherein the verification unit is suitable for verifying the OPC model.

[0022] Accordingly, the present invention also provides an optical proximity correction device, comprising:

[0023] An establishing device, wherein the establishing device is suitable for establishing an OPC model, and the establishing device is the establishing device of the present invention; an acquiring device, wherein the acquiring device is suitable for acquiring a design layout; and a correcting device, wherein the correcting device is suitable for using the OPC model to correct the design layout to obtain a tape-out layout.

[0024] Optionally, the design layout acquired by the acquisition device is a design layout of a contact hole layer.

[0025] In addition, the present invention also provides a storage medium on which a computer program is stored. The computer program is executed by a processor to implement the steps of the establishment method of the present invention.

[0026] Compared with the prior art, the technical solution of the present invention has the following advantages:

[0027] In the technical solution of the present invention, the etched layer is measured by a measuring machine to obtain post-etching measurement values; after the post-etching measurement values ​​are converted into corresponding post-development measurement values, an OPC model is established based on the post-development measurement values. The contour clarity of the pattern in the etched layer is higher, the post-etching measurement values ​​obtained by the measuring machine are more accurate and precise, and the OPC model established based on the post-development measurement values ​​converted from the post-etching measurement values ​​has smaller errors and higher precision, which is conducive to reducing the error of the optical proximity correction method and improving the correction accuracy. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 It is a flow chart of an embodiment of an OPC model establishment method of the present invention;

[0029] Figures 2 to 4 Shows Figure 1 A schematic diagram of the structure of each step in the process of forming a semiconductor structure in an embodiment of the OPC model establishment method shown;

[0030] Figure 5 It is a schematic diagram of a top view of a patterned photoresist formed in a process of forming a semiconductor structure in an embodiment of an OPC model establishment method of the present invention;

[0031] Figure 6 yes Figure 5A schematic diagram of a top view structure of an etched layer obtained in a process of forming a semiconductor structure in an embodiment of the OPC model building method;

[0032] Figure 7 It is a functional block diagram of an embodiment of an optical proximity correction device of the present invention. DETAILED DESCRIPTION

[0033] As can be seen from the background technology, the OPC model in the prior art has a large error problem. Now, the reasons for the large error problem are analyzed in combination with the establishment process of an OPC model:

[0034] An OPC model is established based on after-development inspection (ADI) measurement data. The specific process is: after the photoresist is exposed and developed for patterning, the patterned photoresist is measured by a critical dimension scanning electron microscope (CD-SEM) to obtain after-development measurement data; and the OPC model is established based on the after-development measurement data.

[0035] However, in patterned photoresist, burrs often appear on the edges of the patterns, which can easily affect the measurement accuracy, resulting in reduced accuracy of the post-development measurement data. Moreover, the shrinkage of the photoresist under electron beam bombardment will also affect the accuracy of the post-development measurement data. The reduced accuracy of the post-development measurement data will deteriorate the accuracy of the OPC model established based on the data, resulting in larger errors in the OPC model. The larger errors in the OPC model will not only affect the modeling speed of the OPC model, but will also deteriorate the accuracy of subsequent optical proximity correction using the model.

[0036] In order to solve the technical problem, the present invention provides a method for establishing an OPC model, comprising:

[0037] A semiconductor structure is formed, wherein the semiconductor structure has an etched layer; the etched layer is measured by a measuring machine to obtain a post-etching measurement value; the post-etching measurement value is converted into a corresponding post-development measurement value; and an OPC model is established according to the post-development measurement value.

[0038] The technical solution of the present invention measures the etched layer by a measuring machine to obtain post-etching measurement values; after converting the post-etching measurement values ​​into corresponding post-development measurement values, an OPC model is established based on the post-development measurement values. The contour clarity of the pattern in the etched layer is higher, the post-etching measurement values ​​obtained by the measuring machine are more accurate and precise, and the OPC model established based on the post-development measurement values ​​converted from the post-etching measurement values ​​has smaller errors and higher precision, which is conducive to reducing the error of the optical proximity correction method and improving the correction accuracy.

[0039] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.

[0040] refer to Figure 1 , showing a flow chart of an embodiment of an OPC model building method of the present invention.

[0041] The method for establishing the OPC model includes:

[0042] Step S110, forming a semiconductor structure, wherein the semiconductor structure has an etched layer;

[0043] Step S120, measuring the etched layer by a measuring machine to obtain a post-etching measurement value;

[0044] Step S130, converting the post-etching measurement value into a corresponding post-development measurement value;

[0045] Step S140 , establishing an OPC model according to the post-development measurement values.

[0046] The technical solution of the OPC model building method embodiment of the present invention is described in detail below with reference to the accompanying drawings.

[0047] like Figure 1 As shown, step S110 is first performed to form a semiconductor structure having an etched layer.

[0048] The OPC model can describe the entire photolithography process including the optical system, mask, photoresist, and etching process. Some parameters in the OPC model are calibrated by fitting experimental data, so that the calculated structure of the OPC model is consistent with the experimental results. Step S110, forming a semiconductor structure, wherein the semiconductor has an etched layer, and the etched layer of the formed semiconductor structure is used to extract the experimental data required to establish the OPC model.

[0049] In some embodiments of the present invention, step S110, the step of forming a semiconductor structure includes: Figure 2 As shown, a layer to be etched is provided; a photoresist is formed on the layer to be etched; as shown Figure 3 As shown, the photoresist is patterned to form a patterned photoresist; as shown Figure 4 As shown, the patterned photoresist is used as a mask to etch the layer to be etched to form the etched layer.

[0050] like Figure 2 As shown, in some embodiments, in the step of providing a layer to be etched, a substrate 210 is provided, and the substrate 210 has a layer to be etched 221. Specifically, the substrate 210 is used to provide mechanical support, and the layer to be etched 221 is used to provide a process basis.

[0051] In some specific embodiments, the substrate 210 may be a silicon substrate. In other embodiments of the present invention, the substrate may also be other substrates suitable for conducting OPC model building experiments.

[0052] The layer to be etched 221 is a patterned object for etching to form an etched layer. In some embodiments of the present invention, the OPC model established by the establishment method is applied to the correction of the contact hole layer pattern, and the layer to be etched 221 is a dielectric layer. Specifically, the layer to be etched 221 can be formed on the surface of the substrate 210 by deposition.

[0053] In other embodiments of the present invention, the layer to be etched may also be other material layers suitable for conducting an OPC model building experiment. The layer to be etched may also be formed by other processes suitable for conducting an OPC model building experiment.

[0054] Continue to refer Figure 2 After providing the layer to be etched 221 , a photoresist 231 is formed on the layer to be etched 221 .

[0055] The photoresist 231 is suitable for transferring patterns. The photoresist 231 can be a photoresist suitable for conducting an OPC model building experiment. Specifically, the photoresist 231 can be formed on the surface of the to-be-etched layer 231 by spin coating.

[0056] After forming the photoresist 231, Figure 3 As shown, the photoresist 231 (such as Figure 2 As shown) is patterned to form a patterned photoresist 230.

[0057] Step S110, the step of forming a semiconductor structure also includes: forming a modeling layout, the modeling layout having multiple modeling graphics; manufacturing a mask template based on the modeling graphics; in the process of patterning the photoresist 231, using the mask template to expose and develop the photoresist 231, and transferring the modeling layout on the mask template to the photoresist 231 to form a patterned photoresist 230.

[0058] Specifically, the process of patterning the photoresist 231 can be carried out by a method suitable for conducting an OPC model building experiment. The patterned photoresist 230 has a plurality of experimental patterns. The experimental pattern in the patterned photoresist 230 is consistent with the modeling pattern in the modeling layout. The consistency of the experimental pattern with the modeling pattern means that a plurality of experimental patterns correspond to a plurality of modeling patterns one by one.

[0059] It should be noted that the modeling layout is the graphics designed in the design of experiment (DOE). In order to ensure the accuracy of the established OPC model, it is necessary to improve the coverage of the modeling graphics in the modeling layout to the designed layout as much as possible; for complex design layouts, the more diverse the modeling graphics, the more accurate the established OPC model; but the more diverse the modeling graphics, the corresponding increase in measurement and modeling time. In order to ensure the coverage of the modeling graphics, during the design experiment, graphics can be directly extracted from the design layout as the modeling graphics. Specifically, graphics that are difficult and complex to lithography are extracted from the design layout as key graphics; similar key graphics are classified into one category; representative graphics are extracted from the key graphics of the same category as modeling graphics to construct the modeling layout, and then the mask is made.

[0060] like Figure 4 As shown, after forming the patterned photoresist 230, as shown in Figure 4 As shown, with the patterned photoresist (such as Figure 3 As shown) is a mask, the layer to be etched 221 (as shown Figure 3 As shown in the figure, etching is performed to form an etched layer 220.

[0061] During the etching of the to-be-etched layer 221, the plurality of experimental patterns of the patterned photoresist 230 are transferred to the to-be-etched layer 221 to form the etched layer 220, and the etched layer 220 also has a pattern consistent with the experimental pattern in the patterned photoresist 230. The etched layer 220 has a plurality of to-be-measured patterns, and the plurality of to-be-measured patterns correspond one-to-one to the plurality of experimental patterns in the patterned photoresist 230.

[0062] The etched layer 220 is formed by etching, and the etched layer 220 has fewer burrs on the edges of the graphics and higher definition of the graphics contours, which can provide a good basis for subsequent data measurement. The data obtained by the measurement has higher accuracy and precision, thereby providing a better data basis for establishing an OPC model with smaller errors and higher precision.

[0063] In some embodiments, in the step of etching the layer to be etched 221, the layer to be etched 221 may be etched by anisotropic etching. In other embodiments, in the process of etching the layer to be etched 221, other methods suitable for conducting OPC model building experiments may also be used.

[0064] It should be noted that, in some embodiments of the present invention, after etching the to-be-etched layer 221 to form the etched layer 220, step S110, the step of forming the semiconductor structure further includes: removing the patterned photoresist 230. After forming the etched layer 220, removing the patterned photoresist 230 can effectively avoid the interference of the patterned photoresist 230 on subsequent data measurement, and can effectively improve the precision and accuracy of the measurement data.

[0065] Continue to refer Figure 1 The method for establishing the OPC model further includes: step S120, measuring the etched layer by a measuring machine to obtain a post-etching (after develop insection, AEI) measurement value.

[0066] Specifically, the etched layer 220 has a plurality of patterns to be measured corresponding one to one to the experimental patterns. The etched layer is measured by a measuring machine. In the step of obtaining the post-etching measurement value, the plurality of patterns to be measured in the etched layer 220 are measured one by one by the measuring machine to obtain the plurality of post-etching measurement values.

[0067] The post-etching measurement value may be at least one of the critical dimension (CD), spacing, pitch, length, and extension of the pattern to be measured. Figure 4 As shown, the line width, line spacing and pitch of the pattern to be measured in the etched layer 220 are shown.

[0068] Specifically, the method for establishing the OPC model further includes: setting a measurement position; in step S120, measuring the etched layer by a measuring machine to obtain a post-etching measurement value, the measuring machine measures the etched layer at the set measurement position to obtain a corresponding post-etching measurement value. The setting of the measurement position is related to the requirements of the post-etching measurement value to be obtained and to the data requirements for establishing the OPC model.

[0069] For example, in the step of setting the measurement positions, the specific number and specific positions of the measurement positions set may refer to the method for establishing the existing OPC model, and the present invention will not elaborate on them here.

[0070] In some embodiments of the present invention, in step 120, in the step of measuring the etched layer by a measuring machine to obtain the post-etching measurement value, the measuring machine is a critical dimensions scanning electron microscope (CD-SEM). The critical dimensions scanning electron microscope has a high resolution, and its use can effectively ensure the acquisition of high-precision measurement data. Since the material of the etched layer 220 is a non-photoresist material, the etched layer 220 can be measured by a critical dimensions scanning electron microscope while improving the measurement accuracy, avoiding the shrinkage of the photoresist under the bombardment of the electron beam, and can effectively ensure the accuracy and precision of the measurement data.

[0071] It should be noted that if Figure 1 In some embodiments shown, the method for establishing the OPC model further includes: step S120, measuring the etched layer by a measuring machine, and after obtaining the post-etching measurement value, executing step S150 to clear invalid data in the obtained post-etching measurement value.

[0072] Incorrect data used to establish the OPC model will seriously affect the accuracy of the established model; executing step S150 to clear invalid data in the obtained post-etching measurement values, that is, cleaning the data, can remove incorrect data to ensure the accuracy of the established OPC model. Specifically, in step S150, in the step of clearing invalid data in the obtained post-etching measurement values, by comparing repeated and similar experimental patterns, post-etching measurement values ​​that are significantly deviated from the average value are found and cleared.

[0073] like Figure 1 As shown, after obtaining the post-etching measurement value, the OPC model establishment method further includes: step S130, converting the post-etching measurement value into a corresponding post-development (after etch inspection, AEI) measurement value.

[0074] Combined with reference Figure 5 and Figure 6 ,in Figure 5 A schematic diagram of a top view of a patterned photoresist formed in a process of forming a semiconductor structure in an embodiment of an OPC model establishment method of the present invention is shown;

[0075] Figure 6 yes Figure 5 The schematic diagram of the top view structure of the etched layer obtained in the process of forming the semiconductor structure in the embodiment of the OPC model building method is shown.

[0076] The pattern of the etched layer is consistent with the pattern of the patterned photoresist. The multiple patterns to be measured of the etched layer and the multiple experimental patterns of the patterned photoresist correspond one to one, and the corresponding patterns to be measured and the experimental patterns are close in position, similar in shape, and have fixed size and position relationship.

[0077] Specifically, in step S130, in the step of converting the post-etching measurement value into the corresponding post-development measurement value, the post-etching measurement value is converted into the corresponding post-development measurement value based on the size and position relationship between the pattern to be measured and the experimental pattern.

[0078] In some embodiments of the present invention, the size difference and position difference between the measured pattern and the experimental pattern are fixed values, and the resulting difference between the post-etching measurement value and the post-development measurement value is a fixed value, and the difference between the post-etching measurement value and the post-development measurement value is a global bias; therefore, in the step of converting the post-etching measurement value into the corresponding post-development measurement value, the post-etching measurement value is converted into the corresponding post-development measurement value according to the global bias: ADI=AEI+global_bias; wherein AEI is a post-etching measurement value, global_bias is the global bias, and ADI is the post-development measurement value corresponding to the post-etching measurement value.

[0079] Continue to refer Figure 1 After obtaining the post-development measurement value, the OPC model establishment method further includes: step S140, establishing the OPC model according to the post-development measurement value.

[0080] Although the strict OPC model has high accuracy, the computing power required to establish the OPC model is also very high. It is very difficult to complete the establishment of the chip-level OPC model within the time required by the market, and the computing power requirements are very high. Therefore, in order to balance the conflict between the computing power requirements and the OPC model accuracy requirements, a semi-empirical simplified OPC model is established in the steps of establishing the OPC model. The simplified OPC model is a model that replaces the complex processes in the precise model with some simplified empirical formulas, where the empirical formula includes multiple parameters. The parameters in the empirical formula can be obtained based on the measurement values ​​after development, and finally the calculation structure of the simplified lithography model is consistent with the experimental results.

[0081] Specifically, step S140, the step of establishing an OPC model according to the post-development measurement values ​​includes: obtaining an initial OPC model, the initial OPC model having a plurality of parameters to be fitted; performing fitting calculations according to the post-development measurement values ​​to obtain values ​​of the parameters to be fitted; and establishing the OPC model according to the values ​​of the parameters to be fitted in combination with the initial OPC model.

[0082] It should be noted that if Figure 1 As shown, in some embodiments of the present invention, the method for establishing the OPC model further includes: after establishing the OPC model according to the post-development measurement value, executing step S160 to verify the OPC model.

[0083] Step S160 , the step of verifying the OPC model, can discover software bugs, design errors, and possible hot spots.

[0084] In some embodiments of the present invention, step S160, the step of verifying the OPC model includes: obtaining a verification layout; performing optical proximity correction on the verification layout based on the established OPC model to obtain a corrected layout; forming a semiconductor structure based on the verification layout, the semiconductor structure including a graphic layer, the graphic layer being formed by patterning based on the verification layout, wherein the graphic layer is at least one of the patterned photoresist and the etched layer; obtaining an image of the graphic layer; and comparing the image of the graphic layer with the corrected layout to verify the OPC model.

[0085] In other embodiments, in the step of establishing the OPC model according to the post-development measurement values, the OPC model is established according to a partial number of post-development measurement values; step S160, the step of verifying the OPC model includes: based on the established OPC model, performing optical proximity correction on the modeling layout to obtain a corrected layout; according to the remaining post-development measurement values, measuring the corrected layout to obtain corrected measurement values, the corrected measurement values ​​corresponding to the remaining post-development measurement values ​​one by one, wherein the remaining post-development measurement values ​​are post-development measurement values ​​that are not used in the process of establishing the OPC model; comparing the corrected measurement values ​​with the corresponding post-development measurement values ​​to verify the OPC model.

[0086] Correspondingly, the present invention also provides an optical proximity correction method.

[0087] The optical proximity correction method comprises: obtaining a design layout; establishing an OPC model, wherein the OPC model is established by the establishment method of the present invention; and using the OPC model to correct the design layout to obtain a tape-out layout.

[0088] Specifically, the step of obtaining the design layout includes: obtaining a GDS (Geometry Summary Data) file of the design layout. The GDS file is used to define the three-dimensional structure and electrical characteristics of the chip, and the GDS file contains geometric data about the chip structure, shape and hierarchy. For example, in the step of obtaining the design layout, the design layout is the design layout of the contact hole layer, that is, obtaining the GDS file of the design layout of the contact hole layer.

[0089] In the step of establishing the OPC model, the OPC model is established by the establishment method of the present invention. The specific technical scheme of the step of establishing the OPC model can refer to the embodiment of the above-mentioned method for establishing the OPC model, and the present invention will not repeat it here.

[0090] Afterwards, the design layout is modified based on the OPC model to obtain a tape-out layout.

[0091] The establishment method of the present invention is to establish the OPC model based on the post-development measurement values ​​converted from the post-etching measurement values, so the error of the established OPC model is smaller and the precision is higher; the correction with the OPC model with smaller error and higher precision can effectively improve the accuracy and precision of the obtained wafer layout; especially in the design layout of the contact hole layer, the density of the contact hole pattern is relatively large, and the OPC model of the present invention is used to correct the design layout of the contact hole layer, which effectively improves the accuracy and precision of the correction, which is conducive to the formation of a high-quality contact hole layer and a high-quality contact hole structure.

[0092] Correspondingly, the present invention also provides a device for establishing an OPC model.

[0093] refer to Figure 7 , showing a functional block diagram of an embodiment of an OPC establishment device of the present invention.

[0094] A process unit 310, wherein the process unit 310 is suitable for forming a semiconductor structure, wherein the semiconductor structure has an etched layer; a measurement unit 320, wherein the measurement unit 320 is suitable for measuring the etched layer to obtain a post-etching measurement value; a conversion unit 330, wherein the conversion unit 330 is suitable for converting the post-etching measurement value into a post-development measurement value; and a modeling unit 340, wherein the modeling unit 340 is suitable for establishing an OPC model according to the post-development measurement value.

[0095] The technical solution of the OPC establishing device embodiment of the present invention will be described in detail below with reference to the accompanying drawings.

[0096] The process unit 310 is used to form a semiconductor structure having an etched layer.

[0097] The OPC model can describe the entire photolithography process including the optical system, mask, photoresist, and etching process. Some parameters in the OPC model are calibrated by fitting experimental data, so that the calculated structure of the OPC model is consistent with the experimental results; the etched layer of the semiconductor structure formed by the process unit 310 is used to extract the experimental data required to establish the OPC model.

[0098] In some embodiments of the present invention, the process unit 310 may be a semiconductor manufacturing system for the entire photolithography process including an optical system, a mask, a photoresist, and an etching process. In other embodiments of the present invention, the process unit may also be a control device connected to the semiconductor manufacturing system.

[0099] like Figure 4 As shown, in the semiconductor structure, the etched layer 220 is a material layer formed by etching and having a pattern. The etched layer 220 has a plurality of patterns to be measured, and the plurality of patterns to be measured correspond to a plurality of experimental patterns in the patterned photoresist.

[0100] The measuring unit 320 is used to measure the etched layer to obtain the post-etching measurement value.

[0101] Specifically, the etched layer 220 has a plurality of patterns to be measured corresponding to the experimental patterns one by one, and the measurement unit 320 measures the plurality of patterns to be measured in the etched layer 220 one by one to obtain a plurality of post-etching measurement values.

[0102] The post-etching measurement value may be at least one of a critical dimension (CD), spacing, pitch, length, and extension of the pattern to be measured.

[0103] Specifically, the measurement unit 320 measures the etched layer at a set measurement position to obtain a post-etch measurement value. The setting of the measurement position is related to the requirement of the post-etch measurement value to be obtained and the data requirement for establishing the OPC model.

[0104] It should be noted that the measurement position measured by the measurement unit 320 can refer to the process setting of establishing the existing OPC model, and the present invention will not be repeated here.

[0105] In some embodiments of the present invention, the measurement unit 320 includes: a critical dimension scanning electron microscope (CD-SEM). The critical dimension scanning electron microscope has a high resolution, and its use can effectively ensure the acquisition of high-precision measurement data. Since the material of the etched layer is a non-photoresist material, the etched layer can be measured by the critical dimension scanning electron microscope, while improving the measurement accuracy, avoiding the shrinkage of the photoresist under the bombardment of the electron beam, and can effectively ensure the accuracy and precision of the measurement data.

[0106] It should be noted that if Figure 7 As shown, the establishment device further includes: a clearing unit 350, which is suitable for clearing invalid data in the obtained post-etching measurement values. Incorrect data is used to establish the OPC model, which will seriously affect the accuracy of the established model; the clearing unit 350 cleans the data and can remove incorrect data to ensure the accuracy of the established OPC model. Specifically, the clearing unit 350 finds the post-etching measurement values ​​that are significantly deviated from the average value by comparing repeated and similar experimental patterns, and then clears them.

[0107] Continue to refer Figure 7 The conversion unit 330 is used to convert the post-etching measurement value into a post-development measurement value.

[0108] Combined with reference Figure 5 and Figure 6 ,in Figure 5 A schematic diagram of the top view of the structure of the patterned photoresist formed in an embodiment of the OPC modeling device of the present invention is shown; Figure 6 yes Figure 5 The schematic diagram of the top view structure of the etched layer in the embodiment of the OPC establishment device is shown.

[0109] The pattern of the etched layer is consistent with the pattern of the patterned photoresist. The multiple patterns to be measured of the etched layer and the multiple experimental patterns of the patterned photoresist correspond one to one, and the corresponding patterns to be measured and the experimental patterns are close in position, similar in shape, and have fixed size and position relationship.

[0110] The conversion unit 330 converts the post-etching measurement value into a corresponding post-development measurement value based on the size and position relationship between the pattern to be measured and the experimental pattern.

[0111] In some embodiments of the present invention, the size difference and position difference between the measured pattern and the experimental pattern are fixed values, and the resulting difference between the post-etching measurement value and the post-development measurement value is a fixed value, and the difference between the post-etching measurement value and the post-development measurement value is a global bias; therefore, the conversion unit 330 converts the post-etching measurement value into a corresponding post-development measurement value according to the global bias: ADI=AEI+global_bias; wherein AEI is a post-etching measurement value, global_bias is the global bias, and ADI is the post-development measurement value corresponding to the post-etching measurement value.

[0112] like Figure 7 As shown, the modeling unit 340 is adapted to establish an OPC model according to the post-development measurement values.

[0113] Although the strict OPC model has high accuracy, the computing power required to establish the OPC model is also very high. It is very difficult to complete the establishment of the chip-level OPC model within the time required by the market, and the computing power requirements are very high. Therefore, in order to balance the conflict between the computing power requirements and the OPC model accuracy requirements, a semi-empirical simplified OPC model is established in the steps of establishing the OPC model. The simplified OPC model is a model that replaces the complex processes in the precise model with some simplified empirical formulas, where the empirical formula includes multiple parameters. The parameters in the empirical formula can be obtained based on the measurement values ​​after development, and finally the calculation structure of the simplified lithography model is consistent with the experimental results.

[0114] Specifically, the modeling unit 340 pre-stores an initial OPC model, and the initial OPC model has multiple parameters to be fitted; the modeling unit 340 performs fitting calculations based on the post-development measurement values ​​to obtain the values ​​of the parameters to be fitted; the modeling unit 340 establishes the OPC model based on the values ​​of the parameters to be fitted in combination with the initial OPC model.

[0115] It should be noted that if Figure 7 As shown, in some embodiments of the present invention, the OPC model establishment device further includes: a verification unit 360, and the verification unit 360 is suitable for verifying the OPC model.

[0116] The verification unit 360 can discover software bugs, design errors, and possible hot spots.

[0117] In some embodiments of the present invention, the verification unit 360 is preset with obtaining a verification layout; based on the established OPC model, the verification unit 360 performs optical proximity correction on the verification layout to obtain a corrected layout; the process unit 310 forms a semiconductor structure based on the verification layout, the semiconductor structure includes a graphic layer, the graphic layer is formed based on the patterning of the verification layout, wherein the graphic layer is at least one of the patterned photoresist and the etched layer; the measurement unit 320 obtains an image of the graphic layer; the verification unit 360 compares the image of the graphic layer with the corrected layout to verify the OPC model.

[0118] In other embodiments, the modeling unit establishes the OPC model according to a partial number of post-development measurement values; the verification unit performs optical proximity correction on the modeling layout based on the established OPC model to obtain a corrected layout; the verification unit has a measuring device, and the measuring device measures the corrected layout according to the remaining post-development measurement values ​​to obtain corrected measurement values, and the corrected measurement values ​​correspond to the remaining post-development measurement values ​​one by one, wherein the remaining post-development measurement values ​​are post-development measurement values ​​that are not used in the process of establishing the OPC model; the verification unit compares the corrected measurement values ​​with the corresponding post-development measurement values ​​to verify the OPC model.

[0119] Correspondingly, the present invention also provides an optical proximity correction device.

[0120] like Figure 7 As shown, the optical proximity correction device includes:

[0121] An establishing device 410, wherein the establishing device 410 is suitable for establishing an OPC model, and the establishing device is the establishing device of the present invention; an acquiring device 420, wherein the acquiring device 420 is suitable for acquiring a design layout; and a correcting device 430, wherein the correcting device 430 is suitable for using the OPC model to correct the design layout to obtain a tape-out layout.

[0122] Specifically, the acquisition device 420 obtains a GDS (Geometry Summary Data) file of the design layout. The GDS file is used to define the three-dimensional structure and electrical characteristics of the chip, and the GDS file contains geometric data about the chip structure, shape and hierarchy. For example, the design layout is the design layout of the contact hole layer, that is, the GDS file of the design layout of the contact hole layer is obtained.

[0123] The establishing device 410 is the establishing device of the present invention. The specific technical solution of the establishing device 410 can refer to the embodiment of the aforementioned OPC model establishing device, and the present invention will not repeat it here.

[0124] The correction device 430 corrects the design layout based on the OPC model to obtain a tape-out layout.

[0125] The establishing device 410 establishes the OPC model based on the post-development measurement values ​​converted from the post-etching measurement values, so the established OPC model has smaller errors and higher precision; the correcting device 430 corrects with the OPC model with smaller errors and higher precision, which can effectively improve the accuracy and precision of the obtained wafer layout; especially in the design layout of the contact hole layer, the density of the contact hole pattern is relatively large, and the correcting device 430 uses the OPC model established by the establishing device 410 of the present invention to correct the design layout of the contact hole layer, effectively improving the accuracy and precision of the correction, which is conducive to the formation of a high-quality contact hole layer and a high-quality contact hole structure.

[0126] In addition, the present invention also provides a readable storage medium on which a computer program is stored. The computer program is executed by a processor to implement the steps of the OPC model establishment method of the present invention.

[0127] The computer program stored in the readable storage medium is executed by the processor to implement the steps of the OPC model establishment method of the present invention. The specific technical solution of the readable storage medium can refer to the embodiment of the above-mentioned OPC model establishment method, and the present invention will not repeat it here.

[0128] In summary, the etched layer is measured by a measuring machine to obtain post-etching measurement values; after the post-etching measurement values ​​are converted into corresponding post-development measurement values, an OPC model is established based on the post-development measurement values. The contour clarity of the pattern in the etched layer is higher, the post-etching measurement values ​​obtained by the measuring machine are more accurate and precise, and the OPC model established based on the post-development measurement values ​​converted from the post-etching measurement values ​​has smaller errors and higher precision, which is conducive to reducing the error of the optical proximity correction method and improving the correction accuracy.

[0129] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.

Claims

1. A method for establishing an OPC model, characterized in that: include: forming a semiconductor structure having an etched layer; Measuring the etched layer by a measuring machine to obtain a post-etching measurement value; converting the post-etching measurement value into a corresponding post-developing measurement value; Based on the post-development measurements, an OPC model is established.

2. The method of establishing as claimed in claim 1, characterized in that: In the step of measuring the etched layer by a measuring machine to obtain a post-etching measurement value, the measuring machine is a feature size scanning electron microscope.

3. The establishment method according to claim 1, characterized in that: In the step of converting the post-etching measurement value into the corresponding post-developing measurement value, the post-etching measurement value is converted into the corresponding post-developing measurement value according to a global deviation, wherein the global deviation is the difference between the post-etching measurement value and the post-developing measurement value.

4. The establishment method according to claim 1, characterized in that: Also includes: The etched layer is measured by a measuring machine. After obtaining the post-etching measurement value, invalid data in the obtained post-etching measurement value is cleared before converting the post-etching measurement value into the corresponding post-development measurement value.

5. The establishment method according to claim 1, characterized in that: Also includes: After establishing the OPC model according to the post-development measurement values, the OPC model is verified.

6. The establishment method according to claim 1, characterized in that: The steps of forming a semiconductor structure include: providing a layer to be etched; forming a photoresist on the layer to be etched; Patterning the photoresist to form a patterned photoresist; The patterned photoresist is used as a mask to etch the layer to be etched to form the etched layer.

7. An optical proximity correction method, characterized in that: include: Get the design layout; Establishing an OPC model, wherein the OPC model is established by the establishment method described in any one of claims 1 to claim 6; The OPC model is used to modify the design layout to obtain a tape-out layout.

8. The optical proximity correction method according to claim 7, wherein: In the step of obtaining a design layout, the design layout is a design layout of a contact hole layer.

9. An OPC model establishment device, characterized in that: include: a process unit adapted to form a semiconductor structure having an etched layer; A measurement unit, wherein the measurement unit is suitable for measuring the etched layer to obtain a post-etching measurement value; a conversion unit adapted to convert the post-etching measurement value into a corresponding post-developing measurement value; A modeling unit is adapted to establish an OPC model according to the post-development measurement values.

10. The establishment device according to claim 9, characterized in that The measuring unit includes: a characteristic dimension scanning electron microscope.

11. The establishment device according to claim 9, characterized in that The conversion unit converts the post-etching measurement value into a corresponding post-developing measurement value according to a global deviation, wherein the global deviation is a difference between the post-etching measurement value and the post-developing measurement value.

12. The establishment device according to claim 9, characterized in that Also includes: A clearing unit is adapted to clear invalid data in the obtained post-etching measurement value.

13. The establishment device according to claim 9, characterized in that Also includes: A verification unit, wherein the verification unit is adapted to verify the OPC model.

14. An optical proximity correction device, characterized in that include: Establishment means, the establishment means being adapted to establish an OPC model, the establishment means being as claimed in any one of claims 9 to 13; An acquisition device, wherein the acquisition device is suitable for acquiring a design layout; The correction device is suitable for using the OPC model to correct the design layout to obtain a tape-out layout.

15. The optical proximity correction device according to claim 14, characterized in that The design layout acquired by the acquisition device is the design layout of the contact hole layer.

16. A storage medium having a computer program stored thereon, characterized in that: The computer program is executed by a processor to implement the steps of the method according to any one of claims 1 to 6.

Citation Information

Cited By

  • Critical dimension strip-shaped structure for process monitoring and critical dimension monitoring method

    CN122138671A