Through the secondary annealing and multi-layer insulating structure design of flexible fire-resistant cable conductors, the problems of high conductor hardness and easy oxidation of copper sheath are solved, and soft and easy to bend and high flame retardancy are achieved. It is suitable for installation in narrow areas and use in humid environments. .
Patent Information
- Application Number
- CN202410374411.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-29
- Publication Date
- 2024-11-08
AI Technical Summary
The existing flexible fire-proof cable conductors have high hardness and large bending radius due to the tightening conductor, making it difficult to install in narrow areas. In humid environments, the copper sheath is prone to oxidation and blackening, and the cost is high.
Secondary annealing is used for twisted conductors to reduce the degree of monofilament hardening, increase the core insulation layer, flame retardant filling layer and outer sheath. The copper sheath is equipped with copper-belt chain armor, and the outer sheath is B1 grade halogen-free and low smoke Polyolefin, combined with tension ring structure, improves the flexibility and flame retardancy of the cable.
The softness and flame retardancy of the conductor are improved, the oxidation risk of copper sheath is reduced, the bending capacity and service life of the cable in narrow areas is improved, and the cost is reduced.
Smart Images

Figure CN118919153A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of fireproof cables, in particular to a soft and flexible fireproof cable and a method for manufacturing a twisted conductor thereof. Background Art
[0002] With the development of science and technology and the improvement of people's daily living standards, more and more attention is paid to the fire resistance and installation bending performance of wires and cables in special occasions. As cable companies and research institutes continue to increase their efforts in the development of fire-resistant cables and market demand, more and more flexible fire-resistant cables are widely used in high-rise buildings, petrochemicals, airports, aerospace, parking lots, hospitals and other crowded places.
[0003] At present, most domestic flexible fire-proof cables use round compressed conductors made of annealed single-filament twisted wires. At the same time, since most of these cables have 3 or more cores, round compressed conductors are used. The conductors are wrapped with mica tape and then cabled. After the cable is formed, mica tape is wrapped around the outside, and a copper sheath is welded after the mica tape. For example, in the Chinese patent document, patent number CN2021220695916 disclosed on July 15, 2022, is a kind of metal copper sheathed flexible mineral insulated fire-proof cable, including a copper conductive core, a mineral insulation layer wrapped on the outside of the copper conductive core, a halogen-free flame-retardant filling rope wrapped on the outside of the mineral insulation layer, a halogen-free flame-retardant tape layer wrapped on the outside, a metal copper sheath protective layer wrapped on the outside of the halogen-free flame-retardant tape layer, and a halogen-free low-smoke flame-retardant outer sheath wrapped on the outside of the metal copper sheath protective layer. The shortcomings of the prior art are: since the wires are made of multi-core cables made of Class II compressed conductors and welded copper sheaths, the cable has a large bending radius, especially in areas with narrow spaces where the cable cannot be installed at all due to the large bending radius. This large-section conductor can only be installed with a single core, resulting in high cable costs for customers. At the same time, this cable has no plastic sheath but only a copper sheath, and the copper sheath is easily oxidized and blackened in a humid environment. Summary of the invention
[0004] In order to overcome the shortcomings of the fireproof cable in the prior art, that is, the cable is too hard to bend and the construction is difficult, the present invention provides a method for manufacturing a soft and flexible fireproof cable and a twisted conductor thereof.
[0005] In order to achieve the above object, the present invention adopts the following technical solutions: A soft and flexible fireproof cable comprises a twisted conductor, a core insulation layer, a flame retardant filling layer, a tape insulation layer, a copper sheath and an outer sheath. The twisted conductor is subjected to secondary annealing after twisting. A plurality of twisted conductors are provided, each of which is coated with an independent core insulation layer. The core insulation layer coats all the twisted conductors. The flame retardant filling layer is filled inside the tape insulation layer and coated outside the core insulation layer. The copper sheath and the outer sheath are arranged in sequence from the tape insulation layer to the outside.
[0006] In the present application, the stranded conductor is subjected to secondary annealing after stranding. After annealing, the lattice is reorganized, and the degree of hardening of the single wire during the conductor compression process is reduced. While making the conductor soft, the volume resistivity of the copper single wire is greatly reduced, so that the overall 20°C volume resistivity of the conductor can be controlled below 0.01745Ω.mm2 / m, and the 20°C DC resistance of the conductor is more superior. The cable has good flexibility and can be bent and installed in a small space. The outer sheath protects the outer surface of the copper sheath, prevents the copper sheath from oxidation and blackening, and extends the service life of the copper sheath.
[0007] As a preferred embodiment, the core insulation layer is a calcined mica tape, the flame retardant filling layer is a flame retardant high temperature filling rope, the tape insulation layer is a calcined mica tape, the copper sheath is formed by copper tape interlocking armoring, and the outer sheath is a B1 grade halogen-free low-smoke polyolefin sheath. The core insulation layer is the outer insulation layer of the twisted conductor. In the event of a fire, it maintains the normal power supply of the cable for no less than 180 minutes, providing time for personnel to escape and transfer items. The flame retardant filling layer not only increases the roundness of the cable, but also has a flame retardant effect. The tape insulation layer can not only be tied into a cable core, but also serve as a fire-blocking insulation layer. As a grounding wire, the copper sheath can well protect the internal wire core from damage. At the same time, after adopting the interlocking armoring process, the cable can be bent 360 degrees, and the bending radius is greatly improved. When the outer sheath is on fire in the outside world, it is not easy to burn due to its high flame retardancy, excellent crusting performance, no drop, and low environmental smoke emission, which can well protect the copper sheath from oxidation.
[0008] Preferably, the core insulation layer is a multi-layer 0.14 mm calcined mica tape with overlapping wrapping, and the wrapping coverage rate is 30%-40%. As the innermost insulation layer, this thickness and wrapping coverage rate can ensure the flame retardant and protective effect of the core insulation layer.
[0009] Preferably, the insulating layer is a multi-layer 0.14 mm calcined mica tape wrapped in overlapping layers, with a wrapping coverage of not less than 25%. The tape is tied tightly into a cable core, which can serve as a fire barrier in addition to being an insulating layer, thereby ensuring the effect of the insulating layer.
[0010] Preferably, the outer sheath is formed by extrusion, and the thinnest point of the extrusion thickness is not less than 1.43 mm, so as to ensure the flame retardant effect of the outer sheath and the protective effect on the copper sheath.
[0011] Preferably, when the outer sheath is extruded, the first outer sheath layer is first extruded on the outer side of the copper sheath, and then a plurality of tension rings are provided on the first outer sheath layer at intervals along the length direction of the cable, and the tension rings are made of metal or ceramic materials, and then the second outer sheath layer is extruded outside the first outer sheath layer and the tension rings. After the second outer sheath layer is extruded, the tension ring and the second outer sheath layer are an integral structure, the first outer sheath layer and the second outer sheath layer are an integral structure, and the tension ring and the first outer sheath layer are a separate structure. When the outer sheath is burned at high temperature, the outer side of the outer sheath will shrink and form a crust. Since the tension ring and the first outer sheath layer are a separate structure, the position of the first outer sheath layer corresponding to the tension ring is not easy to form a crust. The position of the outer sheath layer can be located by the position of the tension ring, so that the outer sheath shrinks to the position of the tension ring, so as to avoid the position displacement of the outer sheaths at both ends of the cable during the process of tightening the outer sheath due to the excessive length of the cable, which directly destroys the protection ability of the outer sheath.
[0012] Preferably, the inner circumference of the tension ring is a cylindrical surface that fits the first outer sheath layer, and a positioning ring with an outward protrusion is provided on the outer circumference of one end of the tension ring. The provision of the positioning ring can further improve the positioning effect of the tension ring.
[0013] Preferably, the axial length of the tension ring is 2 to 5 mm. Under the condition of ensuring the positioning function of the tension ring, the tension ring is prevented from being too long to affect the bending ability of the cable, thereby ensuring the convenient bending of the cable.
[0014] A method for manufacturing a twisted conductor for the above-mentioned soft and flexible fireproof cable, wherein the twisted conductor uses an oxygen-free copper rod with a copper content of 99.95%, comprising the following steps: Wire drawing, conductor is semi-annealed during wire drawing, and the elongation at break of copper wire after annealing is controlled between 20% and 25%. Conductor twisting: conductor twisting is completed by compacting; Secondary annealing: the twisted conductor is annealed through a solid-state induction device at a temperature of 310±10 degrees Celsius. When the annealing solid-state induction device is less than 3 meters, the wire speed is not more than 3m / min. When the length of the solid-state induction device increases, the wire speed increases accordingly. The maximum wire speed does not exceed 12m / min. Nitrogen protection is used during the secondary annealing to prevent conductor oxidation. After annealing, the single wire elongation is controlled between 22% and 26%.
[0015] The conductor is made of oxygen-free copper rod with a copper content of 99.95%, which is semi-annealed during wire drawing. After annealing, the elongation at break of the copper wire is controlled between 20% and 25%. In this way, the single wire is not easily stretched during stranded wire production, and the conductor cross-section changes little. The conductor is twisted in a compacting manner, and after twisting, it is annealed through a solid-state induction device at an annealing temperature of 310±10 degrees Celsius. When the annealed solid-state induction device is less than 3 meters, the line speed is not more than 3m / min; when the length of the solid-state induction device is doubled, the speed can also be doubled, but the maximum does not exceed 12m / min, because when the length of the solid-state induction device is doubled, the energy loss is also increased due to sealing. For economy, the length of the annealed fixed induction device does not exceed 12m; nitrogen protection is used during annealing to prevent conductor oxidation, and the elongation of the single wire after annealing is controlled between 22% and 26. After annealing, the lattice is reorganized, and the degree of hardening of the single wire during the conductor compression process is reduced. While making the conductor soft, the volume resistivity of the copper single wire is greatly reduced, so that the overall 20°C volume resistivity of the conductor can be controlled below 0.01745Ω.mm2 / m, and the 20°C DC resistance of the conductor is more superior. And the conductor structure meets the requirements of the second category twisted conductor in the GB / 3956 standard. The small number of single wires facilitates twisting production, but the softness is comparable to the softness of the Category 5 conductor in the GB / 3956 standard. Because when the single wire in the Category 5 conductor is ≥0.50, the single wire breaking elongation is less than or equal to 25%, and when the single wire in the Category 5 conductor is ≤0.50, the single wire breaking elongation is less than or equal to 20%. Therefore, the softness of the twisted conductor formed by the secondary annealing of the present application is comparable to that of the Category 5 conductor, and the cable using this conductor is easier to bend and easier to install and lay.
[0016] These features and advantages of the present invention will be disclosed in detail in the following specific embodiments and drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] The present invention is further described below in conjunction with the accompanying drawings and specific embodiments.
[0018] Figure 1 is a schematic structural diagram of a soft and flexible fireproof cable proposed in one embodiment of the present invention; Figure 2 It is a schematic axial cross-sectional view of a soft and flexible fireproof cable proposed in one embodiment of the present invention.
[0019] In the figure: a stranded conductor 1, a core insulation layer 2, a flame retardant filling layer 3, a tape insulation layer 4, a copper sheath 5, an outer sheath 6, a first outer sheath layer 61, a second outer sheath layer 62, a tensioning ring 63, and a positioning ring 64. DETAILED DESCRIPTION
[0020] The technical solutions of the embodiments of the present invention are explained and described below in conjunction with the drawings of the embodiments of the present invention, but the following embodiments are only preferred embodiments of the present invention, not all. Based on the embodiments in the implementation mode, other embodiments obtained by those skilled in the art without creative work are all within the protection scope of the present invention.
[0021] In the description of this embodiment, it should be noted that, if the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", "front", "back", etc. appear, the orientation or position relationship indicated is based on the orientation or position relationship shown in the accompanying drawings, which is only for the convenience of describing the present invention and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operate in a specific orientation, and therefore, cannot be understood as limiting the present invention. In addition, if the terms "first", "second", and "third" appear, they are only used for descriptive purposes and cannot be understood as indicating or implying relative importance.
[0022] Figure 1 and Figure 2 As shown, a soft and flexible fire-proof cable proposed in one embodiment of the present invention includes a twisted conductor 1, a core insulation layer 2, a flame retardant filling layer 3, a tape insulation layer 4, a copper sheath 5 and an outer sheath 6. The twisted conductor 1 is subjected to secondary annealing after twisting. Three twisted conductors 1 are provided, each of which is coated with an independent core insulation layer 2, and the core insulation layer 2 covers all the twisted conductors 1. The flame retardant filling layer 3 is filled in the tape insulation layer 4 and coated on the outside of the core insulation layer 2. The copper sheath 5 and the outer sheath 6 are arranged in sequence from the tape insulation layer 4 to the outside.
[0023] In this embodiment, the twisted conductor 1 is made by a secondary annealing process, which is highly flexible and convenient for bending and setting of the cable. Three twisted conductors 1 are arranged in a circular array, and the outer sides of the core insulation layers 2 of the adjacent twisted conductors 1 are abutted. The flame retardant filling layer 3 is filled between the three twisted conductors 1 to improve the roundness of the cable. The twisted conductor 1 adopts a circular compressed conductor with a small outer diameter, which saves installation space and material costs. After annealing with the second-class conductor in GB / T 3956, the single-filament elongation of the twisted conductor 1 after secondary annealing is controlled between 22% and 26. After annealing, the lattice is reorganized, and the degree of hardening of the single-filament during the conductor compression process is reduced. While making the conductor soft, the volume resistivity of the copper single filament is greatly reduced, so that the overall 20°C volume resistivity of the conductor can be controlled below 0.01745Ω.mm2 / m, and the 20°C DC resistance of the conductor is more superior. And the conductor structure meets the requirements of the second type of twisted conductor in the GB / 3956 standard. The small number of single wires facilitates twisting production, but the softness is comparable to the softness of Category 5 conductors in the GB / 3956 standard. Because when the single wire in Category 5 conductor is ≥0.50, the single wire breaking elongation is less than or equal to 25%, and when the single wire in Category 5 conductor is ≤0.50, the single wire breaking elongation is less than or equal to 20%. Therefore, the softness of this conductor is comparable to that of Category 5 conductor, and the cable using this conductor is easier to bend and easier to install and lay.
[0024] As a simple alternative to the above solution, the number of stranded conductors 1 may be replaced with four, five, etc.
[0025] As one of the embodiments of the present invention, a soft and flexible fireproof cable is proposed, wherein the core insulation layer 2 is a calcined mica tape, the flame retardant filling layer 3 is a flame retardant high temperature filling rope, the tape insulation layer 4 is a calcined mica tape, the copper sheath 5 is formed by copper tape interlocking armor, and the outer sheath 6 is a B1 grade halogen-free low-smoke polyolefin sheath. Specifically, the core insulation layer 2 is a multi-layer 0.14mm calcined mica tape overlapped and wrapped, with a wrapping coverage rate of 30%-40%. As the innermost insulation layer, in the event of a fire, the cable maintains normal power supply for no less than 180 minutes, providing time for personnel to escape and transfer items. The tape insulation layer 4 is a multi-layer 0.14mm calcined mica tape overlapped and wrapped, with a wrapping coverage rate of not less than 25%. The tape insulation layer 4 can be tied tightly into a cable core, and in addition to being an insulation layer, it can also be used as a fire barrier. The copper sheath 5 is in the form of interlocking armor, which is different from the welded copper sheath 5 in that the interlocking armored copper sheath can be bent 360 degrees, which is convenient for installation in a small space, while the welded copper sheath 5 cannot be bent or installed in a small space. The outer sheath 6 is formed by extrusion, and the thinnest point of the extrusion thickness is not less than 1.43mm. When it catches fire, it is not easy to burn due to its high flame retardancy, does not fall, and has low environmental smoke. At the same time, it serves as a protective layer for the copper sheath 5 to prevent the copper sheath 5 from oxidizing and blackening.
[0026] As one of the embodiments of the present invention, a soft and flexible fireproof cable is provided. Figure 2 As shown, when the outer sheath 6 is extruded, a first outer sheath layer 61 is first extruded on the outside of the copper sheath 5, and then a plurality of tensioning rings 63 are provided on the first outer sheath layer 61 at intervals along the length direction of the cable. The tensioning rings 63 are made of metal or ceramic materials, and then a second outer sheath layer 62 is extruded outside the first outer sheath layer 61 and the tensioning rings 63. After the second outer sheath layer 62 is extruded, the tension ring 63 and the second outer sheath layer 62 are in an integral structure, the first outer sheath layer 61 and the second outer sheath layer 62 are in an integral structure, and the tension ring 63 and the first outer sheath layer 61 are in a separate structure. When the external high temperature burns, the outer side of the outer sheath 6 will shrink and form a crust. Since the tension ring 63 and the first outer sheath layer 61 are in a separate structure, the position of the first outer sheath layer 61 corresponding to the tension ring 63 is not easy to form a crust. The position of the outer sheath 6 layer can be located by the position of the tension ring 63, so that the outer sheath 6 is tightened to the position of the tension ring 63, so as to avoid the outer sheath 6 at both ends of the cable from being offset in the process of tightening the outer sheath 6 due to the excessive length of the cable, thereby directly destroying the protection capability of the outer sheath 6. In this embodiment, the inner periphery of the tension ring 63 is a cylindrical surface that fits the first outer sheath layer 61, and a positioning ring 64 with an outward protrusion is provided on the outer periphery of one end of the tension ring 63. In order to ensure the bending ability of the soft and flexible fireproof cable and at the same time ensure the function of the tensioning ring 63, the axial length of the tensioning ring 63 is 5 mm, and the axial length of the positioning ring 64 is 1 mm.
[0027] As one of the embodiments of the present invention, a method for manufacturing a twisted conductor 1 for the above-mentioned soft and flexible fire-proof cable is proposed, wherein the twisted conductor 1 adopts an oxygen-free copper rod with a copper content of 99.95%, and comprises the following steps: Wire drawing, conductor is semi-annealed during wire drawing, and the elongation at break of copper wire after annealing is controlled between 20% and 25%. Conductor twisting: conductor twisting is completed by compacting; Secondary annealing: the twisted conductor is annealed through a solid-state induction device at a temperature of 310±10 degrees Celsius. When the annealing solid-state induction device is less than 3 meters, the wire speed is not more than 3m / min. When the length of the solid-state induction device increases, the wire speed increases accordingly. The maximum wire speed does not exceed 12m / min. Nitrogen protection is used during the secondary annealing to prevent conductor oxidation. After annealing, the single wire elongation is controlled between 22% and 26%.
[0028] The conductor is made of oxygen-free copper rod with a copper content of 99.95%, which is semi-annealed during wire drawing. After annealing, the elongation at break of the copper wire is controlled between 20% and 25%. In this way, the single wire is not easily stretched during stranded wire production, and the conductor cross-section changes little. The conductor is twisted by compaction, and then annealed by filling magnesium oxide solid-state induction device after twisting. The annealing temperature is 310±10. When the annealed solid-state induction device is less than 3 meters, the line speed is not more than 3m / min. When the length of the solid-state induction device doubles, the speed can also double, but it is not recommended to exceed 12m / min at most, because when the length of the solid-state induction device doubles, the energy loss is also increasing due to the sealing. For the sake of economy, it is recommended not to exceed 12m. Nitrogen protection is used during annealing to prevent conductor oxidation. After annealing, the elongation of the single wire is controlled between 22% and 26. After annealing, the lattice is reorganized, and the degree of hardening of the single wire during the conductor pressing process is reduced. While making the conductor soft, the volume resistivity of the copper single wire is greatly reduced, so that the overall volume resistivity of the conductor at 20℃ can be controlled below 0.01745Ω.mm2 / m, and the 20℃ DC resistance of the conductor is more superior. And the conductor structure meets the requirements of the second type of twisted conductor in the GB / 3956 standard. The small number of single wires facilitates twisting production, but the softness is comparable to the softness of Category 5 conductors in the GB / 3956 standard. Because when the single wire in Category 5 conductor is ≥0.50, the single wire breaking elongation is less than or equal to 25%, and when the single wire in Category 5 conductor is ≤0.50, the single wire breaking elongation is less than or equal to 20%. Therefore, the softness of this conductor is comparable to that of Category 5 conductor, and the cable using this conductor is easier to bend and easier to install and lay.
[0029] The above are only specific embodiments of the present invention, but the protection scope of the present invention is not limited thereto. Those skilled in the art should understand that the present invention includes but is not limited to the contents described in the drawings and the above specific embodiments. Any modification that does not deviate from the functional and structural principles of the present invention will be included in the scope of the claims.
Claims
1. A soft and flexible fireproof cable, characterized in that: It includes a twisted conductor, a core insulation layer, a flame retardant filling layer, a tape insulation layer, a copper sheath and an outer sheath. The twisted conductor is subjected to secondary annealing after twisting. There are several twisted conductors, each of which is covered with an independent core insulation layer. The core insulation layer covers all the twisted conductors. The flame retardant filling layer is filled inside the tape insulation layer and covered outside the core insulation layer. The copper sheath and the outer sheath are arranged in sequence from the tape insulation layer to the outside.
2. A soft and flexible fireproof cable according to claim 1, characterized in that: The core insulation layer is a calcined mica tape, the flame retardant filling layer is a flame retardant high temperature filling rope, the tape insulation layer is a calcined mica tape, the copper sheath is formed by copper tape interlocking armoring, and the outer sheath is a B1 grade halogen-free low-smoke polyolefin sheath.
3. A soft and flexible fireproof cable according to claim 2, characterized in that: The core insulation layer is composed of multiple layers of 0.14 mm calcined mica tapes wrapped in an overlapping manner, with an overlap rate of 30%-40%.
4. A soft and flexible fireproof cable according to claim 2, characterized in that: The tape insulation layer is a plurality of layers of 0.14 mm calcined mica tapes which are overlapped and wrapped, and the wrapping overlap rate is not less than 25%.
5. A soft and flexible fireproof cable according to claim 1, characterized in that: The outer sheath is formed by extrusion, and the thinnest point of the extrusion thickness is not less than 1.43 mm.
6. A soft and flexible fireproof cable according to claim 5, characterized in that: When the outer sheath is extruded, a first outer sheath layer is first extruded outside the copper sheath, and then a plurality of tensioning rings are provided on the first outer sheath layer at intervals along the length direction of the cable, wherein the tensioning rings are made of metal or ceramic materials, and then a second outer sheath layer is extruded outside the first outer sheath layer and the tensioning rings.
7. A soft and flexible fireproof cable according to claim 6, characterized in that: The inner circumference of the tension ring is a cylindrical surface that fits the first outer sheath layer, and a positioning ring that is convexly arranged is provided on the outer circumference of one end of the tension ring.
8. A soft and flexible fireproof cable according to claim 6, characterized in that: The axial length of the tension ring is 2 to 5 mm.
9. A method for manufacturing a stranded conductor for a soft, flexible, fire-resistant cable as claimed in claims 1 to 8, characterized in that: The stranded conductor uses an oxygen-free copper rod with a copper content of 99.95%, and includes the following steps: A. Wire drawing: semi-annealing is performed during wire drawing. The elongation at break of the copper wire after annealing is controlled between 20% and 25%. B. Conductor twisting: conductor twisting is completed by compacting; C. Secondary annealing: The twisted conductor is annealed through a solid-state induction device at a temperature of 310±10 degrees Celsius. When the annealing solid-state induction device is less than 3 meters, the wire speed is not more than 3m / min. When the length of the solid-state induction device increases, the wire speed increases accordingly. The maximum wire speed does not exceed 12m / min. Nitrogen protection is used during the secondary annealing to prevent conductor oxidation. After annealing, the single wire elongation is controlled between 22% and 26%.