Nitrogen polarity InGaN-based red light LED with component gradient barrier layer and preparation method of nitrogen polarity InGaN-based red light LED

By designing the component gradient barrier layer and the opposite polarization electric field direction in InGaN-based red LED, electron and hole potential wells are formed, the problem of low luminescence efficiency of InGaN-based red LED is solved, and the luminescence efficiency and power conversion are improved efficiency.

CN118919619APending Publication Date: 2024-11-08JILIN UNIVERSITY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410978156.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-22
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The luminescence efficiency of InGaN-based red LED is low and the power conversion efficiency is low. It is mainly due to the increase in compressive stress and polarization electric field caused by the high In components in the quantum well, which reduces the radiation recombination efficiency of carriers.

Method used

Design a nitrogen-polar InGaN-based red LED with a component gradient barrier layer. The internal polarization electric field direction is opposite to that of a traditional metal polar LED. The last barrier layer in the quantum well is an InGaN layer with component gradient, forming electrons. and hole potential wells to improve radiation recombination efficiency.

Benefits of technology

Through the opposite polarization electric field direction and component gradient barrier layer, the luminous efficiency and power conversion efficiency of the red LED are improved, the opening voltage is reduced, and the carrier confinement capacity and hole injection capacity are improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118919619A_ABST
    Figure CN118919619A_ABST
Patent Text Reader

Abstract

The invention discloses a nitrogen polarity InGaN-based red light LED with a component gradient barrier layer and a preparation method thereof, and belongs to the technical field of semiconductor light emitting devices. The light emitting diode is composed of a substrate, a nucleating layer, an n-type GaN layer quantum well active layer and a p-type GaN layer from bottom to top in sequence, and an upper electrode and a lower electrode are arranged on the p-type layer and the n-type layer respectively. Wherein the lattice polarity of each epitaxial nitride layer except the substrate is nitrogen polarity, and the last barrier layer of the quantum well active layer is an InGaN layer of which the In component is gradually increased. The component gradient barrier layer and the p-type GaN layer form an electron potential well and a hole potential well at the same time, electrons and holes accumulated in the two potential wells have high spatial wave function overlapping degree, efficient radiative recombination can be generated, and therefore the luminous efficiency of the InGaN-based red light LED is effectively improved. According to the invention, the high-performance InGaN-based red light LED can be obtained, so that the development of a Micro LED display technology is promoted.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of semiconductor light-emitting devices, and in particular relates to a nitrogen-polarity InGaN-based red light LED with a component gradient barrier layer and a preparation method thereof. Background Art

[0002] Micro LED display technology has the advantages of high resolution, high brightness, low energy consumption and long durability, and has broad application prospects in the fields of augmented reality / virtual reality, visible light communication, wearable devices, space imaging, etc. At present, one of the challenges facing Micro LED display technology is the lack of efficient and reliable red light microchips. InGaN is an ideal material for preparing red light microchips required for Micro LED display technology. It has a short carrier diffusion length (~100nm) and the device size has little effect on LED performance. At the same time, it has good mechanical stability and is easy to achieve process compatibility with InGaN-based blue and green LEDs, which can simplify the industrial production process of Micro LED display technology.

[0003] However, the current luminous efficiency of InGaN-based red LEDs is relatively low, and the power conversion efficiency is mostly below 5%. This is mainly related to the high In component in the InGaN quantum wells in the active region (usually the In component must be greater than 40% to enable the LED to reach the red light band). A high In component in the quantum well is a necessary condition for the realization of red light LEDs. In order to obtain a high In component, the quantum well needs to be grown at low temperature, but low temperature conditions often lead to poor crystal quality of the quantum well. In addition, the high In component causes the quantum well to be subjected to greater compressive stress, which reduces the incorporation of In atoms in the well layer and aggravates phase separation. Moreover, the large compressive stress increases the polarization electric field in the well layer, aggravates the quantum confined Stark effect, and reduces the radiative recombination efficiency of carriers. Summary of the invention

[0004] The present invention proposes a nitrogen-polarity InGaN-based red light LED with a composition gradient barrier layer and a preparation method thereof. Different from the traditional and widely studied metal-polarity InGaN-based LED, the nitrogen-polarity InGaN-based LED described in the present invention has an internal polarization electric field direction opposite to that of the metal-polarity LED. The opposite polarization electric field direction enables the quantum well active region in the nitrogen-polarity InGaN-based LED structure to have a stronger carrier confinement capability. At the same time, the nitrogen-polarity InGaN-based LED has a stronger hole injection capability and the ability to suppress electron overflow. Importantly, the last barrier layer in the quantum well of the nitrogen-polarity InGaN-based red light LED described in the present invention is designed to be an InGaN layer with a composition gradient increase, and the interface of the composition gradient InGaN barrier layer and the p-GaN hole supply layer will simultaneously form an electron potential well and a hole potential well, and the electrons and holes accumulated in the two potential wells have a high degree of spatial wave function overlap, which can produce efficient radiation recombination, thereby effectively improving the luminous efficiency of the red light LED.

[0005] The present invention discloses a nitrogen-polarity InGaN-based red light LED having a compositionally graded barrier layer (see attached Figure 1 and the accompanying drawings), it is composed of a substrate 1, a nucleation layer 2, an n-type GaN layer 3, a quantum well active layer 4 and a p-type GaN layer 5 from bottom to top, and an exposed n-type GaN layer 3 table is formed between the quantum well active layer 4 and the n-type GaN layer 3, and a lower electrode 7 and an upper electrode 6 are respectively prepared on the table and the p-type GaN layer 5.

[0006] Furthermore, the quantum well active layer 4 is composed of In x Ga 1-x N barrier layer and In y Ga 1-y N-well layers are stacked alternately, In x Ga 1- x N barrier layer and In y Ga 1-y The number of alternating stacking cycles of the N-well layer is 1 to 5 cycles, and the last barrier layer is an In layer with a gradient In composition. z Ga 1-z N layers, the component z of In increases gradually from m to n along the growth direction; where 0≤x<y=n<1, 0≤m<n, that is, in the same device, x and y are fixed values, while z is variable; In x Ga 1-x N barrier and compositional gradient In z Ga 1-z The thickness of the N barrier layer is 8-15nm. y Ga 1-y The thickness of the N-well layer is 1 to 5 nm.

[0007] Furthermore, the lattice polarity of the nucleation layer 2, the n-type GaN layer 3, the quantum well active layer 4 and the p-type GaN layer 5 are all nitrogen polar. The nitrogen polar nitride semiconductor has a hexagonal wurtzite structure, and its c-axis <0001> The direction is asymmetric, that is, the positive charge center of the metal atom and the negative charge center of the nitrogen atom along the c-axis do not coincide, and there is a spontaneous polarization effect. When the nitride material grows along the c-axis, when the bonding direction of the metal atoms and nitrogen atoms parallel to the c-axis along the growth direction is the metal atom pointing to the nitrogen atom, the lattice polarity of the material is metal polarity. Conversely, if the bonding direction of the metal atoms and nitrogen atoms parallel to the c-axis along the growth direction is the nitrogen atom pointing to the metal atom, the polarity of the material is nitrogen polarity. The polarization directions in nitrogen-polar nitride materials and metal-polar nitride materials are opposite, so the polarization electric fields along the growth direction in these two polar materials are opposite. The method for obtaining a nitrogen-polar nitride layer is related to the substrate and the surface treatment process of the substrate. For example, a nitrogen-polar nitride layer can be directly grown on a carbon-faced silicon carbide substrate and a nitrogen-faced GaN substrate, and a nitrogen-polar nitride layer can also be grown on a sapphire substrate treated with high-temperature ammonia (i.e., ammonia gas is introduced at a high temperature of 1000-1100°C for 5-10 minutes).

[0008] Furthermore, the substrate 1 can be any substrate that can grow a nitrogen-polar nitride layer, such as a carbon-surface silicon carbide substrate, a nitrogen-surface GaN substrate, a sapphire substrate treated with ammonia at high temperature (treated at 1000-1100°C for 5-10 minutes); the nucleation layer 2 is a low-temperature GaN or AlN layer with a thickness of 20-50 nm; the n-type GaN layer 3 is a Si-doped GaN layer with a doping concentration of 10 18 cm -3 The p-type GaN layer 5 is a Mg-doped GaN layer with a doping concentration of 10 19 cm -3 The thickness is of the order of magnitude and is 100 to 200 nm; the upper electrode 6 can be a single layer of a mono-alloy such as Au, Pt, a binary alloy composite layer such as Ni-Au, Ni-Pt, or a ternary alloy composite layer such as Ni-Pt-Au, with a thickness of 30 to 120 nm; the lower electrode 7 can be a binary alloy composite layer such as Ti-Au, a ternary alloy composite layer such as Ti-Al-Au, or a quaternary alloy composite layer such as Ti-Al-Ni-Au, Ti-Al-Ti-Au, with a thickness of 60 to 300 nm.

[0009] The method for preparing a nitrogen-polar InGaN-based red light LED having a composition-gradient barrier layer as described above comprises the following steps:

[0010] (1) A nucleation layer 2, an n-type GaN layer 3, a quantum well active layer 4 and a p-type GaN layer 5 are epitaxially grown on a substrate 1 in sequence by a metal organic chemical vapor deposition (MOCVD) method; nitrogen is used as a carrier gas when growing the quantum well active layer 4, and hydrogen is used as a carrier gas when growing the other layers; trimethylaluminum (TMAl), trimethylindium (TMIn) and trimethylgallium (TMGa) are used as Al source, In source and Ga source, respectively; high-purity ammonia is used as an N source; silane is used as an n-type doping source, and bis(cyclopentadienyl)magnesium is used as a p-type doping source; the growth temperature of the nucleation layer 2 is 530-550°C, the growth pressure is 100-400 mbar, and the growth thickness is 20-50 nm; the growth temperature of the n-type GaN layer 3 is 800-1100°C, the growth pressure is 100-400 mbar, the growth thickness is 1-3 μm, and the n-type doping concentration is 10 18 cm -3 Order of magnitude; in the quantum well active layer 4, In y Ga 1-y The growth temperature of the N-well layer is 700-850°C, the growth pressure is 200-800 mbar, and the growth thickness is 1-5 nm; x Ga 1-x The growth temperature of the N barrier layer is 700-950°C, the growth pressure is 100-400 mbar, and the growth thickness is 8-15 nm; x Ga 1-x N barrier layer and In y Ga 1-y The number of alternating stacking cycles of the N-well layer is 1 to 5 cycles; the last component gradually changes to In z Ga 1-z The growth temperature of the N barrier layer is 700-900°C. During the growth process, the temperature can be gradually reduced within the range of 700-900°C, or the Ga source flow rate can be gradually reduced while the In source flow rate is gradually increased to achieve a gradual increase in the In component of the film. The growth temperature of the p-type GaN layer 5 is 900-1000°C, the growth pressure is 100-400mbar, the growth thickness is 100-200nm, and the Mg doping concentration is 10 19 cm -3 Magnitude.

[0011] (2) etching the area on one side of the upper surface of the p-type GaN layer 5 to the n-type GaN layer 3 by inductively coupled plasma (ICP) etching or other methods to obtain an exposed n-type GaN layer 3 table; then preparing an upper electrode 6 and a lower electrode 7 on the p-type GaN layer 5 and the exposed n-type GaN layer 3 table by thermal evaporation or electron beam evaporation, respectively, to obtain the nitrogen-polar InGaN-based red light LED with a compositionally graded barrier layer.

[0012] Effects and benefits of the present invention: (1) The last barrier layer of the nitrogen-polarity InGaN-based red LED is designed to be a gradient InGaN layer. z Ga 1-z N layers, the result is a gradient component In z Ga 1-z An electron potential well and a hole potential well are formed at the interface between the N barrier layer and the p-type GaN layer 5, and the electrons and holes accumulated in these two potential wells have a high degree of spatial wave function overlap, which can produce efficient radiative recombination, thereby effectively improving the luminous efficiency of InGaN-based red light LEDs. It should be noted that if the polarity of the nitrogen-polar InGaN-based red light LED is transformed into the traditional widely studied metal polarity, the composition gradient InGaN z Ga 1-z Electron potential wells and hole potential wells are not formed at the interface between the N barrier layer and the p-type GaN layer at the same time, so the luminescence performance of the LED cannot be improved. (2) The direction of the polarization electric field in the nitrogen-polarity InGaN-based red light LED is opposite to the direction of the polarization electric field in the traditional metal-polarity InGaN-based red light LED that has been widely studied. The opposite polarization electric field makes the nitrogen-polarity InGaN-based LED quantum well active region have a stronger confinement effect on carriers. In addition, the direction of the polarization electric field is the same as the direction of the external forward bias of the LED, which can reduce the turn-on voltage of the LED and improve the power conversion efficiency of the LED. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] Figure 1 : A schematic diagram of the structure of a nitrogen-polar InGaN-based red light LED with a composition-gradient barrier layer according to the present invention;

[0014] Figure 2 :The nitrogen polar red LED simulated in Example 1 is 180A / cm 2 Energy band structure diagram under current density;

[0015] Figure 3 :The metal polarity red light LED simulated in Example 1 is 180A / cm 2 Energy band structure diagram under current density;

[0016] Figure 4 :The nitrogen polar red LED simulated in Example 1 is 180A / cm 2 Electron and hole concentration profiles at current density;

[0017] Figure 5 :The nitrogen red LED simulated in Example 1 is at 180A / cm 2 Radiative recombination rate curve under current density;

[0018] Figure 6:The metal polarity red light LED simulated in Example 1 is 180A / cm 2 Electron and hole concentration profiles at current density;

[0019] Figure 7 :The metal polarity red light LED simulated in Example 1 is 180A / cm 2 Radiative recombination rate curve under current density;

[0020] Figure 8 : Internal quantum efficiency curves of the nitrogen polarity red light LED and the metal polarity red light LED simulated in Example 1;

[0021] Fig. 9 : IV curves of the nitrogen polarity red LED and the metal polarity red LED simulated in Example 1;

[0022] Fig.10 : The nitrogen polarity red light LED and metal polarity red light LED simulated in Example 1 are at 180A / cm 2 Electroluminescence spectra at different current densities. DETAILED DESCRIPTION

[0023] Example 1

[0024] We used Crosslight's Advanced Physical Models of Semiconductor Devices (APSYS) software to perform two-dimensional device performance simulations on the nitrogen-polarity InGaN-based red LED with a gradient barrier layer and the metal-polarity InGaN-based red LED with a gradient barrier layer prepared by the present invention. These two LEDs are referred to as nitrogen-polarity red LED and metal-polarity red LED, respectively. Figure 1 As shown, the specific structures of the two LEDs include a sapphire substrate 1, a GaN nucleation layer 2, an n-type GaN layer 3, a quantum well active layer 4 and a p-type GaN layer 5, and an upper electrode 6 and a lower electrode 7 are prepared on the p-type GaN layer 5 and the n-type GaN layer 3, respectively. The last barrier layer of the quantum well active layer 4 of the two samples is an InGaN layer with an increased In composition gradient. The difference between the epitaxial structures of the two LEDs is that the lattice polarity of the GaN nucleation layer 2, the n-type GaN layer 3, the quantum well active layer 4 and the p-type GaN layer 5 in the nitrogen polarity red LED is nitrogen polarity, while the lattice polarity of the GaN nucleation layer 2, the n-type GaN layer 3, the quantum well active layer 4 and the p-type GaN layer 5 in the metal polarity red LED is metal polarity. In the simulation, we change the polarity of the red LED by changing the vector in the polarization effect model. For the nitrogen polarity red LED, vector = (0, -1, 0), and for the metal polarity red LED, vector = (0, 1, 0).

[0025] In the device simulation, the thickness of the nucleation layer 2 in the nitrogen-polarity red LED and the metal-polarity red LED is 40 nm; the n-type doping concentration of the n-type GaN layer 3 is 5×10 18 cm -3 , the thickness is 3μm; in the quantum well active layer 4, In y Ga 1-y The thickness of the N-well layer is 3nm, and the In composition y is 0.42; x Ga 1-x The thickness of the N barrier layer is 12nm, and the In composition x is 0.15; x Ga 1-x N barrier layer and In y Ga 1-y The alternating stacking period of the N-well layer is 5; the last barrier layer In z Ga 1-z The In component of the N layer changes gradually from 0.22 to 0.42 along the growth direction z, and the thickness is 12nm; the p-type doping concentration of the p-type GaN layer 5 is 5×10 19 cm -3 , the thickness is 150nm, and the upper electrode 6 and the lower electrode 7 are both set to ohmic contact.

[0026] In addition, in our simulation setup, the Shockley-Read-Hall (SRH) recombination lifetime in the active region is 10 ns and the Auger coefficient is 1×10 -31 cm 6 / s, the InGaN / GaN conduction band order and valence band order ratios are set to 0.7 / 0.3, and considering the screening effect of dislocations, defects and other interface charges on polarization charges, we set the polarization screening factor to 0.4.

[0027] Figure 2 and Figure 3 The nitrogen polarity red LED and metal polarity red LED simulated in Example 1 are respectively at 180A / cm 2Energy band structure diagram under current density. As can be seen from the figure, the quantum well barrier of nitrogen polar red LED restricts electron overflow is 561meV, which is 193meV higher than that of metal polar red LED. At the same time, nitrogen polar red LED has a higher electron blocking barrier (1.143eV), which can effectively suppress the electrons from overflowing from the quantum well active area to the p-type GaN layer. In addition, nitrogen polar red LED also has a lower hole injection barrier (236meV), which is nearly 2 / 3 of that of metal polar red LED, which helps to inject holes from the p-type GaN side into the quantum well active area. In addition, the component gradient barrier layer and the p-type GaN layer interface of nitrogen polar red LED will simultaneously form electron potential wells and hole potential wells. Since both the electron potential well and the hole potential well are approximately triangular potential wells and close to the p-type GaN interface, the wave function space overlap of the electrons and holes restricted by the potential well is large, which can form a high efficiency radiation recombination rate. However, only a deeper electron potential well can be formed at the interface between the component gradient barrier layer and the p-type GaN of the metallic polarity red light LED, but no hole potential well can be formed.

[0028] Figure 4 The electron and hole concentration distribution diagram of the nitrogen polar red light LED simulated in Example 1 can be seen from the figure that the electrons and holes will accumulate at the interface between the composition gradient barrier layer and the p-type GaN layer at the same time. Among them, the accumulated hole concentration at the interface is higher than the electron concentration. There are two reasons for this. One is that the hole potential well at the interface is narrower than the electron potential well (such as Figure 2 As shown in Figure 2, holes have a stronger limiting effect on the surface. Secondly, the migration ability of holes is weaker than that of electrons, so holes are easily accumulated in the interface potential well close to the p-type GaN side. The electrons and holes accumulated at the interface have a high degree of wave function overlap and can form efficient radiative recombination, such as Figure 5 shown.

[0029] Figure 6 This is the electron and hole concentration distribution diagram of the metal polarity red light LED simulated in Example 1. It can be seen from the figure that only electrons accumulate at the interface between the component gradient barrier layer and the p-type GaN layer, but no holes accumulate. This is because the component gradient In x Ga 1-x Only a deep electron potential well is formed at the interface between the N layer and p-GaN, but no hole potential well is formed (such as Figure 3 This is consistent with our previous analysis based on energy bands. Therefore, effective radiative recombination cannot be formed at the interface between the composition gradient barrier layer and the p-type GaN layer in the metallic polarity red LED, as shown in Figure 2. Figure 7 shown.

[0030] Figure 8This is the relationship between the internal quantum efficiency of the nitrogen polarity red light LED and the metal polarity red light LED and the current density obtained by simulation in Example 1. It can be seen from the figure that the nitrogen polarity red light LED has a higher luminous efficiency and a weaker efficiency drop phenomenon.

[0031] Fig. 9 It is the IV curve of the nitrogen polarity red light LED and the metal polarity red light LED simulated in Example 1. It can be seen from the figure that the turn-on voltage of the nitrogen polarity red light LED is 3.0V, which is 1.1V lower than the turn-on voltage of the metal polarity red light LED. This is mainly because the direction of the polarization electric field in the quantum well of the nitrogen polarity group red light LED is opposite to the direction of the external electric field, so it has a lower turn-on voltage.

[0032] Fig.10 The nitrogen polarity red light LED and the metal polarity red light LED simulated in Example 1 are 180A / cm 2 Electroluminescence spectra under current density. It can be seen from the figure that the emission wavelengths of the two samples are both 620nm, but the luminous intensity of the nitrogen polar red light LED is more than 40% higher than that of the metal polar red light LED.

Claims

1. A nitrogen-polar InGaN-based red light LED with a compositionally graded barrier layer, which is composed of a substrate (1), a nucleation layer (2), an n-type GaN layer (3), a quantum well active layer (4) and a p-type GaN layer (5) from bottom to top, wherein an exposed n-type GaN layer (3) table is formed between the quantum well active layer (4) and the n-type GaN layer (3), and a lower electrode (7) and an upper electrode (6) are respectively prepared on the table and the p-type GaN layer (5); characterized in that: The lattice polarities of the nucleation layer (2), the n-type GaN layer (3), the quantum well active layer (4) and the p-type GaN layer (5) are all nitrogen polarities, and the quantum well active layer (4) is composed of In x Ga 1-x N barrier layer and In y Ga 1-y The N well layers are stacked alternately, and the last barrier layer of the quantum well active layer (4) is an In with a gradient In composition. z Ga 1-z N layer, the In component z gradually increases from m to n along the growth direction; where 0≤x<y=n<1, 0≤m<n, In x Ga 1-x N barrier layer and In y Ga 1-y The number of alternating stacking cycles of the N-well layer is 1 to 5 cycles.

2. A nitrogen-polar InGaN-based red light LED with a composition-gradient barrier layer as claimed in claim 1, characterized in that: The substrate (1) is a carbon-surface silicon carbide substrate, a nitrogen-surface GaN substrate, or a sapphire substrate treated with ammonia at high temperature; the nucleation layer (2) is a low-temperature GaN or AlN layer with a thickness of 20 to 50 nm; the n-type GaN layer (3) is a Si-doped GaN layer with a doping concentration of 10 18 cm -3 In order of magnitude, thickness is 1 to 3 μm; x Ga 1-x N barrier and compositional gradient In z Ga 1-z The thickness of the N barrier layer is 8-15nm. y Ga 1-y The thickness of the N well layer is 1 to 5 nm; the p-type GaN layer (5) is a Mg-doped GaN layer with a doping concentration of 10 19 cm -3 The upper electrode (6) is a single alloy layer, a binary alloy composite layer or a ternary alloy composite layer of Au, Pt, Ni-Au, Ni-Pt or Ni-Pt-Au, and the thickness is 30 to 120 nm; the lower electrode (7) is a binary alloy composite layer, a ternary alloy composite layer or a quaternary alloy composite layer of Ti-Au, Ti-Al-Au, Ti-Al-Ni-Au or Ti-Al-Ti-Au, and the thickness is 60 to 300 nm.

3. A method for preparing a nitrogen-polar InGaN-based red light LED having a composition-gradient barrier layer according to claim 1 or 2, wherein the steps are as follows: (1) A nucleation layer (2), an n-type GaN layer (3), a quantum well active layer (4) and a p-type GaN layer (5) are epitaxially grown in sequence on a carbon-surface silicon carbide, a nitrogen-surface GaN or a sapphire substrate (1) treated with ammonia at high temperature by a metal organic chemical vapor deposition method; nitrogen is used as a carrier gas when growing the quantum well active layer (4), and hydrogen is used as a carrier gas when growing the other layers; TMAl, TMIn and TMGa are used as Al source, In source and Ga source respectively, high-purity ammonia is used as a nitrogen source, silane is used as an n-type doping source, and bis(cyclopentadienyl)magnesium is used as a p-type doping source; the growth temperature of the nucleation layer (2) is 530-550° C., and the growth pressure is 100-400 mbar; the growth temperature of the n-type GaN layer (3) is 1000-1100° C., the growth pressure is 100-400 mbar, and the n-type doping concentration is 10 18 cm -3 Order of magnitude; in the quantum well active layer (4), In y Ga 1-y The growth temperature of the N-well layer is 700-850°C and the growth pressure is 200-800 mbar; x Ga 1-x The growth temperature of the N barrier layer is 700-950°C and the growth pressure is 100-400 mbar; the last component gradually changes to In z Ga 1-z The growth temperature of the N barrier layer is 700-900°C, and during the growth process, the temperature is gradually reduced, or the Ga source flow rate is gradually reduced while the In source flow rate is gradually increased to achieve a gradual increase in the In component in the film; the growth temperature of the p-type GaN layer (5) is 900-1000°C, the growth pressure is 100-400mbar, and the p-type doping concentration is 10 19 cm -3 Magnitude; ① Etching a region on one side of the upper surface of a p-type GaN layer (5) to the n-type GaN layer (3) by an inductively coupled plasma etching method to obtain an exposed n-type GaN layer (3) table; then preparing an upper electrode (6) and a lower electrode (7) on the p-type layer (5) and the exposed n-type GaN layer (3) table by thermal evaporation or electron beam evaporation, respectively, thereby preparing a nitrogen-polar InGaN red light LED with a compositionally graded barrier layer.