Composite current collector and energy storage device

By introducing a combination of linear reinforcement layer and carbon-based conductive film materials into the composite liquid collector, the problem of poor strength of the non-metallic conductive layer is solved, the conductivity and strength of the current collector are improved, and the continuous processing performance of the secondary battery is improved. and the overall performance of energy storage products.

CN118919733APending Publication Date: 2024-11-08ZHEJIANG RUOZHEN TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411284763.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-13
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The strength of the non-metal conductive layer of the existing composite fluid collector limits its continuous processing performance in secondary batteries and the strength of energy storage products. The tensile strength of graphite paper as a support layer is insufficient, making it difficult to improve.

Method used

The combined structure of a non-metallic conductive support layer and a linear reinforcement layer is adopted. The linear reinforcement layer includes a plurality of linear reinforcement units arranged at intervals, which are arranged along the longitudinal direction of the film. The conductive support layer forms an interface at the intervals to enhance the conductivity and strength of the current collector. And a good interface between conduction and heat is formed by a combination of carbon-based conductive film material and linear polymer material.

Benefits of technology

It significantly improves the strength and processing performance of the current collector, improves the overall performance of energy storage products, ensures the conductivity of conductivity and heat, and adapts to single-sided or double-sided conductive layer structures, reducing the non-conductivity in traditional composite liquid collectors. , defects that are not thermally conductive.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118919733A_ABST
    Figure CN118919733A_ABST
Patent Text Reader

Abstract

The invention discloses a composite current collector and an energy storage device, and belongs to the technical field of current collectors, the composite current collector comprises a non-metal conductive supporting layer, and at least one surface layer of the conductive supporting layer forms a first conductive layer; the conductive support layer is connected with a linear enhancement layer, the linear enhancement layer comprises a plurality of linear enhancement units arranged at intervals, the linear enhancement units are longitudinally arranged along the thin film, transverse intervals are formed between adjacent linear enhancement units, the conductive support layer forms an interface at the interval, and the conductive support layer forms an electric and thermal good interface at the interface. The composite current collector is provided with the connection reinforcing material layer, so that the problem of poor strength of the non-metal conductive layer can be solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field The present invention relates to the technical field of current collectors, and in particular to a composite current collector and an energy storage device. Background Art In secondary batteries, a current collector is needed as the part for current convergence, and its material is generally aluminum foil or copper foil. In the prior art, for safety considerations, a composite current collector is proposed, which includes a polymer support layer and a metal layer arranged on both sides of the support layer. However, the current collector structure with a polymer support layer as a carrier needs to be deposited by evaporation or sputtering, which can easily form defects such as pinholes on the support layer. At the same time, the polymer material has poor conductivity, so transfer welding is required for subsequent welding of the pole ears. Prior art [1] , a current collector with a metal layer structure arranged on the surface of a non-metallic conductive film, such as graphite paper, is used as a supporting layer to improve the overall conductivity. However, when graphite paper is used as the support layer, its tensile strength is generally only 4-4.5 MPa, which is not conducive to continuous processing and is also not conducive to the battery manufacturing process. Therefore, further improvement is needed.

[0001] CN 218525607 U Summary of the invention The present invention aims to solve one of the technical problems in the related art at least to a certain extent. To this end, one object of the present invention is to provide a composite current collector having a connection reinforcement material layer, which can improve the problem of poor strength of the non-metallic conductive layer. Another object of the present invention is to provide an energy storage device based on the above current collector. The technical solution of the present invention is as follows: A composite current collector includes a non-metallic conductive support layer; The conductive support layer is connected to the linear enhancement layer, which includes a plurality of linear enhancement units arranged at intervals. The linear enhancement units are arranged along the longitudinal direction of the film, and there are lateral intervals between adjacent linear enhancement units. The conductive support layer forms an interface at the intervals, and the conductive support layer forms an electrical and thermal good interface at the interface. Based on the above technical solution, the linear reinforcement layer can greatly improve the strength of the current collector while ensuring the conductivity of the current collector, thereby improving the processing performance and the strength of subsequent energy storage products; the linear reinforcement units have lateral spacing, which can fully retain the performance of the non-metallic conductive support layer. Further, at least one surface layer of the conductive support layer forms a conductive layer. Based on the above technical solution, the conductive performance of the current collector can be further improved. Furthermore, the conductive supporting layer comprises a single layer or a composite structure of multiple supporting layer units, and the linear reinforcement layer is arranged on the side of the supporting layer or between the supporting layer units. Based on the above technical solution, a current collector with a single-sided or double-sided conductive layer structure can be adapted. Furthermore, the conductive support layer is a carbon-based conductive film material, including a graphite film and a graphene film. Based on the above technical solution, it has good thermal conductivity and electrical conductivity, and can improve the defects of non-conductivity and non-thermal conductivity in traditional composite current collectors. Furthermore, the thickness of the conductive support layer is set to 4-100 μm. Based on the above technical solution, a suitable thickness of the support layer can be selected to suit the convenience of processing and at the same time, to make it as thin as possible. Further, the linear reinforcing unit includes a linear polymer material. Based on the above technical solution, it is convenient to achieve the thinning of the linear reinforcement layer and the bonding of the composite structure to ensure electrical and thermal conductivity. Further, the linear enhancement unit is in the shape of a wire bundle; Based on the above technical solution, smaller bonding points can be formed, which is convenient for continuous processing. Furthermore, the linear enhancement unit is flat. Based on the above technical solution, the effective area during subsequent composite bonding can be greatly increased, and it is beneficial to the spreading and thinning of the material after rolling. Furthermore, the ratio of width to thickness of the flat linear reinforcing unit is preferably not less than 100:1. Furthermore, a groove is formed on the flat linear reinforcing unit. Based on the above technical solution, the grooves are opened to reduce the lateral interaction force of the flat linear reinforcement unit, so that it can be better composited with the conductive support layer during subsequent hot rolling, reduce the lateral shrinkage stress after hot pressing composite, and prevent delamination; in addition, after the grooves are opened, the reinforcement unit can form a partial overlap at the groove, and the overlapping part will produce crystal bonding after hot pressing, which increases the interlayer adhesion to a certain extent and is not easy to delaminate. Furthermore, the projections of the grooves in the same group in the horizontal or vertical direction substantially overlap. Based on the above technical solution, the corresponding groove structure distribution in the transverse and longitudinal directions can reduce the shrinkage deformation caused by the tensile tension during processing due to the groove misalignment. Furthermore, a plurality of linear extensions are formed outside the linear enhancement unit. Based on the above technical solution, the effective area of ​​the linear enhancement unit can be further increased. Furthermore, the conductive layer is a metal material; And / or, the conductive layer is a conductive paste. An energy storage device comprises the composite current collector. BRIEF DESCRIPTION OF THE DRAWINGS The accompanying drawings are used to provide a further understanding of the present invention and constitute a part of the specification. Together with the embodiments of the present invention, they are used to explain the present invention and do not constitute a limitation of the present invention. In the accompanying drawings: Figure 1 Schematic diagram of the structure of the first composite current collector; Figure 2 Schematic diagram of the structure of the second composite current collector; Figure 3 Schematic diagram of the structure of the third composite current collector; Figure 4 Schematic diagram of the structure of the fourth composite current collector; Figure 5 for Figure 4 Schematic diagram of the second linear enhancement unit in FIG. In the figure: 1-conductive support layer; 11-composite interface 2- first conductive layer; 3-first linear enhancement unit; 31-extension section; 4- second conductive layer; 5-second linear enhancement unit; 51-slot. DETAILED DESCRIPTION The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments. Examples of the embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are intended to be used to explain the present invention, and should not be construed as limiting the present invention. In the prior art, the composite current collector based on graphite paper has limited tensile strength and restricted continuous processing performance. In view of the above problems, in some embodiments of the present application, reference is made to Figure 1 A composite current collector is proposed, including a non-metallic conductive support layer 1, and a first conductive layer 2 can be further formed on a surface layer of the conductive support layer 1 to increase the conductivity; the other surface layer of the conductive support layer 1 is connected to a linear enhancement layer, and the linear enhancement layer includes a plurality of (spaced) first linear enhancement units 3, the first linear enhancement units 3 are arranged along the longitudinal direction of the film, and the non-metallic conductive support layer 1 has a lateral gap between adjacent first linear enhancement units 3. The conductive support layer 1 is a carbon-based conductive film material, such as a graphite film (graphite paper), a graphene film or other film material, which has good thermal conductivity and electrical conductivity, and its thickness is set to 4-100 μm. The first linear reinforcing unit 3 is a linear polymer bundle, which is hot-pressed and bonded to the surface of the conductive support layer 1. In some embodiments of the present application, the hot pressing treatment method is hot rolling, and other conventional heating and pressurizing methods are also acceptable. After hot pressing, the cross section thereof is a flat ellipse. The material of the first linear reinforcing unit includes a filament bundle formed by one or a combination of polyester, polyamide, polystyrene, nylon, etc., and its denier number is 50D-500D. It can also be selected in combination with the width and performance requirements of the collector. The number of the first linear reinforcing units can also be determined in combination with the width and thickness (denier number). The spacing between relatively thick first linear reinforcing units can be appropriately increased; for example, the spacing between the first linear reinforcing units can be set to 50-100mm. Since the conductive support layer 1 itself has relatively good hardness and temperature resistance, the temperature and pressure can be appropriately increased during hot pressing so that the linear reinforcement layer and the conductive support layer 1 have good adhesion after composite. The rolling pressure is 5-15MPa (multi-stage rolling can be performed; the temperature can also be gradually increased). The temperature can be near the glass transition temperature of the linear reinforcement layer. The pressure and holding time are adjusted in combination with the diameter or width of the first linear reinforcement unit 3 so that the surface of the linear reinforcement unit produces a molten self-adhesive effect. The hot pressing time is within 1s, preferably within 0.5s, to avoid excessively high temperature causing the structure of the linear material to be significantly deformed or melted, thereby affecting its strength. The first conductive layer 2 can be formed by plating, such as sputtering, evaporation, chemical plating, etc., or by directly coating a conductive paste. Based on the formation method of the conductive layer, its material can be selected from metal materials, such as one or a combination of silver, copper, gold, aluminum, tungsten, nickel, chromium, etc., or a conductive paste made from the above metal materials. The configuration method of the relevant plating or paste belongs to the existing conventional technical means and will not be repeated. Setting a conductive support layer based on the linear enhancement layer can greatly enhance the overall strength of the current collector and improve the processability of the non-metallic conductive support layer; at the same time, the first linear enhancement units 3 in the linear enhancement layer are arranged at intervals to reduce the impact of the conductive support layer's own performance. Figure 1 Schematic diagram shows a case where a conductive layer is disposed on one side of the conductive support layer 1 . In other embodiments, conductive layers are disposed on both sides of the conductive support layer 1 . At this time, if Figure 2As shown, the conductive support layer 1 includes two laminated support layer units, and the first linear enhancement unit 3 is arranged on the laminated surface of the support layer unit. The first linear enhancement unit 3 composites and bonds the two groups of support layer units under the action of hot rolling, and a composite interface 11 is formed at the laminated surface. Since the interface spacing formed after rolling is extremely small, the interface has good electrical and thermal conductivity. Of course, the use of more groups of conductive support layers and / or the use of linear reinforcement units in bonding and compounding adjacent support layer units should also be included in the protection scope of the present application. In order to ensure that the conductive support layer with a multi-layer structure can ensure sufficient adhesion and fit at the interface, in addition to reasonably setting the weight and spacing of the linear reinforcement unit, further reference is made to Figure 3 In some embodiments of the present application, a plurality of linear extensions 31 are formed on the periphery of the first linear enhancement unit 3 to further increase the coverage area (width direction) of the linear enhancement unit 3; the linear extensions 31 are randomly distributed, and their overlapping portions also have certain gaps. For the linear reinforcement unit with polymer tow, which is formed by twisting a number of polymer plastic fiber filaments (including filaments and / or staple fibers), the linear extension 31 can be formed by a raising process, and the length of the linear extension 31 is 2-20 mm. Since the linear extension 31 has a smaller diameter, it can maintain a certain porosity during compounding, and under the action of hot rolling during compounding, it is further thinned and embedded into the gap between layers at the interface, reducing the thickness of the composite, thereby reducing the impact on the performance at the interface between layers. Reference Figure 4 In some embodiments of the present application, the linear enhancement unit is configured as a second linear enhancement unit 5, and its main body is configured to be a flat structure to increase the bonding area with the conductive support layer 1; the width to thickness ratio of the second linear enhancement unit 5 is preferably not less than 100:1, and more preferably not less than 1000:1. The flat structure is conducive to further thinning and spreading of the limiting unit after rolling, and can form a thinner composite interface 11; the flat structure can be obtained by rolling the polymer bundle. Further references Figure 5 , and Figure 4 The main difference between the scheme and the middle scheme is that a plurality of (interval) grooves 51 are provided on the second linear reinforcing unit 5 along the longitudinal direction of the film (the length direction of the second linear reinforcing unit 5), and the projections of the grooves 51 in the same group in the transverse or longitudinal direction are basically overlapped, so as to avoid the formation of a staggered groove structure during the processing, and to avoid the deformation of the grooves 51 parts that are easily alternating in front and back during continuous processing under the action of tension, and being stretched and deformed into a mesh structure, which will greatly shorten the width of the second linear reinforcing unit 5, which is not conducive to the composite between layers; At the same time, after grooving, the lateral interaction force of the flat second linear reinforcing unit 5 can be reduced, so that it can be better composited with the conductive support layer 1 during subsequent hot rolling, reducing the lateral shrinkage stress after hot pressing composite, and preventing delamination; in addition, after grooving, the reinforcing unit can form a partial overlap at the groove 51, and the overlapping part will produce crystal bonding after hot pressing, which increases the interlayer adhesion to a certain extent and is not easy to delaminate. In addition, in some embodiments of the present application, an energy storage device based on the above-mentioned composite current collector, such as a secondary battery, is also disclosed. Embodiment 1 Conductive support layer tensile strength test, 50D PET yarn, 50mm interval, hot roll laminated between two sets of 15μm thick graphite paper, roll pressure of 5MPa, holding time of 0.3s, roll temperature set at about 170℃. The measured tensile strength is 182MPa. In comparative example 1, the tensile strength of conventional 30 μm graphite paper is 4.2 MPa. Interlayer adhesion test The bonding strength test was conducted using ethylene-acrylic acid copolymer (EAA) peel test technology. The test equipment was an electronic universal testing machine, which specifically included the following steps: A layer of Permacel P-94 double-sided tape was bonded to a 1 mm thick aluminum foil, a composite current collector to be tested was bonded to the double-sided tape, an ethylene acrylic acid copolymer film was covered on the composite current collector, and then a 1.3 × 10 5 N / m 2 , hot press at 120℃ for 10s, cool to room temperature, and cut into 150mm×15mm strips. Finally, fix the ethylene acrylic acid copolymer film of the sample strip to the upper fixture of the tensile machine, and the rest to the lower fixture. After fixation, the two are peeled at an angle of 180° and a speed of 100mm / min, and the maximum value is recorded. Embodiment 2 The 50D PET line was laminated between two sets of 15μm thick graphite paper with a spacing of 50mm by hot roller pressing. The rolling pressure was 5MPa, the holding time was 0.3s, and the hot roller pressing was performed twice. The rolling temperature was set at 170℃. The maximum adhesion value obtained by the test was 1.7N / 15mm. Embodiment 3 The difference from the second embodiment is that the length of the fluff formed by the linear extension 31 of the PET wire after the grinding treatment is about 4 mm, and the maximum adhesion value obtained by the test is 2.1 N / 15 mm. Embodiment 4 500D PET lines were selected and pre-rolled into flat strips with a width of 20mm and a thickness of 0.2mm. The strips were 70mm apart and hot rolled between two sets of 15μm thick graphite papers. The rolling pressure was 12MPa, the rolling temperature was set to 170℃, the pressure was maintained for 0.5s, and repeated three times. The maximum peeling force was measured to be 2.3N / 15mm. Embodiment 5 The difference from the fourth embodiment is that 1.5 cm long grooves are provided in the linear reinforcing unit at 3 cm intervals in the longitudinal direction, and two groups are provided in the transverse direction at 1 cm intervals in the transverse direction. The maximum peeling force measured is 2.7 N / 15 mm. This indicates that in the limited reinforcement unit after the grooves, overlapping and extrusion flow and recrystallization occur at the grooves, which is beneficial for combining and anchoring in the gaps of the graphite paper and increasing the adhesion. In the description of the present invention, it is to be understood that the terms “center”, “longitudinal”, “lateral”, “length”, “width”, “thickness”, “up”, “down”, “front”, “back”, “left”, “right”, “vertical”, “horizontal”, “top”, “bottom”, “inside”, “outside”, “clockwise”, “counterclockwise”, “axial”, “radial”, “circumferential”, etc., indicating orientations or positional relationships based on the orientations or positional relationships shown in the drawings or conventionally expressed in the prior art, are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention. In the description of the embodiments of the present application, the term "and / or" is only a description of the association relationship of associated objects, indicating that three relationships may exist. For example, A and / or B can represent: A exists, A and B exist at the same time, and B exists. In addition, the character " / " in this article generally indicates that the associated objects before and after are in an "or" relationship. The term "multiple" as used in this application refers to more than two (including two). Similarly, "multiple groups" refers to more than two groups (including two groups), and "multiple sheets" refers to more than two sheets (including two sheets). The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A composite current collector comprising a non-metallic conductive support layer; It is characterized in that The conductive support layer is connected to the linear enhancement layer, which includes a plurality of linear enhancement units arranged at intervals. The linear enhancement units are arranged along the longitudinal direction of the film, and there are lateral intervals between adjacent linear enhancement units. The conductive support layer forms an interface at the intervals, and the conductive support layer forms an electrical and thermal good interface at the interface.

2. The composite current collector according to claim 1, characterized in that: The conductive supporting layer comprises a single layer or a composite structure of multiple supporting layer units, and the linear reinforcing layer is arranged on the side of the supporting layer or between the supporting layer units.

3. The composite current collector according to claim 1, characterized in that: The conductive support layer is a carbon-based conductive film material, including a graphite film and a graphene film; The thickness of the conductive support layer is set to 4-100 μm; And / or, at least one surface layer of the conductive support layer forms a conductive layer.

4. The composite current collector according to claim 1, characterized in that: The linear reinforcing unit includes a linear polymer material.

5. The composite current collector according to claim 4, characterized in that: The linear enhancement unit is in the shape of a wire bundle; And / or, the linear enhancement unit is flat.

6. The composite current collector according to claim 5, characterized in that: The ratio of width to thickness of the flat linear reinforcing unit is preferably not less than 100:

1.

7. The composite current collector according to claim 6, characterized in that: A slot is provided on the flat linear reinforcing unit.

8. The composite current collector according to claim 7, characterized in that: The horizontal or vertical projections of the grooves in the same group basically overlap.

9. The composite current collector according to any one of claims 1 to 8, characterized in that: A plurality of linear extensions are formed outside the linear enhancement unit.

10. An energy storage device, characterized in that: Comprising the composite current collector as claimed in claim 9.