Cylindrical secondary battery

By incorporating insulators within the electrode body to optimize electrolyte distribution, the problem of uneven electrolyte distribution in large-scale cylindrical secondary batteries was solved, achieving high capacity and excellent charge-discharge cycle characteristics.

CN118922972APending Publication Date: 2024-11-08PANASONIC INTELLECTUAL PROPERTY MANAGEMENT CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202380027513.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-03-31
Filing Date
2023-03-06
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

Large cylindrical secondary batteries are prone to uneven electrolyte distribution within the electrode body, which leads to reduced charge-discharge cycle characteristics.

Method used

An insulator is disposed between at least one of the positive and negative electrodes and the separator, ensuring that the projected area of ​​the insulator on the separator is larger on the inner side of the winding than on the outer side of the winding, thereby optimizing the electrolyte distribution.

Benefits of technology

It improves battery capacity and charge/discharge cycle characteristics, balancing high battery capacity and charge/discharge performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118922972A_ABST
    Figure CN118922972A_ABST
Patent Text Reader

Abstract

A cylindrical secondary battery according to one embodiment of the present invention is provided with: an electrode body in which a positive electrode and a negative electrode are wound with a separator interposed therebetween; an electrolyte; and a cylindrical outer case that accommodates the electrode body and the electrolyte, in which an insulator is disposed between the separator and at least one of the positive electrode and the negative electrode, and in which the insulator is disposed in the center of the separator in the longitudinal direction into an inner winding region on the inner side of the winding and an outer winding region on the outer side of the winding. A projected area of the insulator in the winding inner region on the separator is larger than a projected area of the insulator in the winding outer region on the separator.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a cylindrical secondary battery. Background Art

[0002] A cylindrical secondary battery is a battery in which an electrode body formed by winding a positive electrode and a negative electrode with a separator interposed therebetween is housed in a cylindrical outer casing. Patent Documents 1 and 2 disclose separators having a surface with projections and depressions for the purpose of easily injecting an electrolyte into the outer casing when manufacturing a battery.

[0003] Prior art literature

[0004] Patent Literature

[0005] Patent Document 1: Japanese Patent No. 4529903

[0006] Patent Document 2: Japanese Patent Application Publication No. 2008-226696 Summary of the invention

[0007] In recent years, the enlargement of cylindrical secondary batteries has been studied for the purpose of increasing capacity. The inventors have conducted in-depth research and found that in a wound electrode body, the distribution of the electrolyte is sometimes uneven in the electrode body, and the battery capacity is reduced due to repeated charging and discharging. This tendency is significant in large cylindrical secondary batteries. The technology described in Patent Documents 1 and 2 does not study the enlargement of batteries, and there is still room for improvement.

[0008] An object of the present invention is to provide a cylindrical secondary battery having a high capacity and excellent charge and discharge cycle characteristics.

[0009] A cylindrical secondary battery as a technical solution of the present invention comprises: an electrode body, which is formed by winding a positive electrode and a negative electrode with a separator between them; an electrolyte; and a cylindrical outer shell, which accommodates the electrode body and the electrolyte, and is characterized in that an insulator is arranged between at least one of the positive electrode and the negative electrode and the separator, and when the separator is divided into a winding inner area on the inner side of the winding and a winding outer area on the outer side of the winding in the center of the long side direction of the separator, the projected area of ​​the insulator in the winding inner area on the separator is larger than the projected area of ​​the insulator in the winding outer area on the separator.

[0010] According to the cylindrical secondary battery of the present invention, the battery capacity and the charge-discharge cycle characteristics can be improved. BRIEF DESCRIPTION OF THE DRAWINGS

[0011] Figure 1 It is an axial cross-sectional view of a cylindrical secondary battery as an example of an embodiment.

[0012] Figure 2 yes Figure 1The illustrated secondary battery is a perspective view of a wound electrode assembly.

[0013] Figure 3 This is a front view showing a separator constituting an electrode body of an example of the embodiment in a developed state, and is a view in which an insulator is projected.

[0014] Figure 4 is included Figure 3 The top view of the upper surface of the electrode body of the separator shown is a diagram showing the position where the insulator is arranged. DETAILED DESCRIPTION

[0015] In recent years, the enlargement of cylindrical secondary batteries has been studied for the purpose of increasing battery capacity. However, compared with previous batteries, enlarged batteries are prone to electrolyte shortage on the winding center side of the electrode body, so the charge and discharge cycle characteristics are easily reduced. In order to solve this problem, the inventors conducted in-depth research and found that by configuring an insulator at a specified position between at least one of the positive and negative electrodes and the separator, the reduction of battery capacity can be suppressed and the charge and discharge cycle characteristics can be improved. That is, in the case where the center of the long side direction of the separator is divided into a winding inner area on the inner side of the winding and a winding outer area on the outer side of the winding, by configuring an insulator in the winding inner area where the electrolyte is easily insufficient, and making the insulator in the winding outer area rich in electrolyte compared to the winding inner area The projected area on the separator is reduced, it is possible to take into account both battery capacity and charge and discharge cycle characteristics.

[0016] Hereinafter, an example of an embodiment of a cylindrical secondary battery of the present invention will be described in detail with reference to the accompanying drawings. In the following description, specific shapes, materials, numerical values, directions, etc. are examples for easy understanding of the present invention and can be appropriately changed according to the specifications of the cylindrical secondary battery. In addition, in the following description, when multiple embodiments and variations are included, it is envisaged from the beginning that their characteristic parts are appropriately combined and used.

[0017] Figure 1 FIG. 1 is an axial cross-sectional view of a cylindrical secondary battery 10 as an example of an embodiment. Figure 1In the secondary battery 10 shown, the electrode body 14 and the electrolyte (not shown) are contained in a cylindrical outer shell 15. The electrode body 14 has a winding structure in which the positive electrode 11 and the negative electrode 12 are wound across the separator 13. As a non-aqueous solvent (organic solvent) of the electrolyte, carbonates, lactones, ethers, ketones, esters, etc. can be used, and these solvents can be mixed with two or more. In the case of mixing two or more solvents, a mixed solvent containing cyclic carbonates and chain carbonates is preferably used. For example, as cyclic carbonates, ethylene carbonate (EC), propylene carbonate (PC), butylene carbonate (BC), etc. can be used, and as chain carbonates, dimethyl carbonate (DMC), ethyl methyl carbonate (EMC) and diethyl carbonate (DEC), etc. can be used. As an electrolyte salt of the electrolyte, LiPF6, LiBF4, LiCF3SO3, etc. and mixtures thereof can be used. The amount of the electrolyte salt dissolved in the nonaqueous solvent can be, for example, 0.5 mol / L to 2.0 mol / L. In the following, for convenience of description, the sealing body 16 side is referred to as "upper" and the bottom side of the outer shell 15 is referred to as "lower".

[0018] The open end of the outer shell 15 is blocked by the sealing body 16, so that the interior of the secondary battery 10 is sealed. An insulating plate 17 and an insulating plate 18 are provided above and below the electrode body 14, respectively. The positive lead 19 extends upward through the through hole of the insulating plate 17 and is welded to the lower surface of the filter 22 which is the bottom plate of the sealing body 16. In the secondary battery 10, the cover 26 which is the top plate of the sealing body 16 and is electrically connected to the filter 22 becomes the positive terminal. On the other hand, the negative lead 20 extends to the bottom side of the outer shell 15 through the through hole of the insulating plate 18 and is welded to the bottom inner surface of the outer shell 15. In the secondary battery 10, the outer shell 15 becomes the negative terminal. In addition, when the negative lead 20 is provided at the outer end of the winding, the negative lead 20 extends to the bottom side of the outer shell 15 through the outside of the insulating plate 18 and is welded to the bottom inner surface of the outer shell 15.

[0019] The outer shell 15 is, for example, a metal outer shell can in a bottomed cylindrical shape. A gasket 27 is provided between the outer shell 15 and the sealing body 16 to ensure the airtightness of the interior of the secondary battery 10. The outer shell 15 has a groove portion 21 formed, for example, by pressurizing the side surface from the outside to support the sealing body 16. The groove portion 21 is preferably formed in an annular shape along the circumference of the outer shell 15, and the sealing body 16 is supported by the upper surface of the groove portion 21.

[0020] The sealing body 16 has a filter 22, a lower valve core 23, an insulating member 24, an upper valve core 25 and a cover 26 stacked in order from the electrode body 14 side. The components constituting the sealing body 16 have, for example, a disc shape or a ring shape, and the components except the insulating member 24 are electrically connected to each other. The lower valve core 23 and the upper valve core 25 are connected to each other at their respective central portions, and the insulating member 24 is interposed between the peripheral portion of the lower valve core 23 and the peripheral portion of the upper valve core 25. When the internal pressure of the battery rises due to abnormal heat, for example, the lower valve core 23 breaks, whereby the upper valve core 25 bulges toward the cover 26 side and leaves the lower valve core 23, thereby cutting off the electrical connection between the two. When the internal pressure rises further, the upper valve core 25 breaks, and the gas is discharged from the opening 26a of the cover 26.

[0021] Next, refer to Figure 2 to Figure 4 Next, the electrode body 14 will be described. The diameter of the electrode body 14 is preferably 20 mm or more. This can increase the battery capacity of the secondary battery 10.

[0022] Figure 2 It is a three-dimensional diagram of the electrode body 14. As described above, the electrode body 14 has a winding structure in which the positive electrode 11 and the negative electrode 12 are wound in a spiral shape with the separator 13 interposed therebetween. The positive electrode 11, the negative electrode 12 and the separator 13 are all formed in a strip shape, and are wound in a spiral shape around a winding core arranged along the winding axis 28, thereby being alternately stacked in the radial direction of the electrode body 14. In the electrode body 14, the long side direction of the positive electrode 11 and the negative electrode 12 becomes the winding direction, and the short side direction of the positive electrode 11 and the negative electrode 12 becomes the axial direction. The positive electrode lead 19 extends axially from the upper end of the electrode body 14, approximately in the center of the radius between the center and the outermost periphery. In addition, the negative electrode lead 20 extends axially from the vicinity of the winding axis 28 at the lower end of the electrode body 14.

[0023] The positive electrode 11 has a strip-shaped positive electrode current collector and a positive electrode mixture layer formed on the surface of the positive electrode current collector. The positive electrode mixture layer is preferably formed on both sides of the positive electrode current collector. For the positive electrode current collector, a foil of a metal such as aluminum or an aluminum alloy that is stable within the potential range of the positive electrode 11, a film that arranges the metal on the surface, etc. can be used.

[0024] The positive electrode mixture layer may include a positive electrode active material, a conductive agent, a binder, etc. The positive electrode mixture layer can be manufactured, for example, by applying a positive electrode mixture slurry including a positive electrode active material, a conductive agent, a binder, and a solvent such as N-methyl-2-pyrrolidone (NMP) to both surfaces of the positive electrode collector and drying the mixture, followed by rolling.

[0025] Examples of the positive electrode active material contained in the positive electrode mixture layer include lithium transition metal oxides containing transition metal elements such as Co, Mn, and Ni. For example, lithium transition metal oxides are Li x CoO2、Lix NiO2、Li x MnO2、Li x Co y Ni 1-y O2、Li x Co y M 1-y O z , Li x Ni 1-y M y O z , Li x Mn2O4、Li x Mn 2-y M y O4, LiMPO4, Li2MPO4F (M is at least one of Na, Mg, Sc, Y, Mn, Fe, Co, Ni, Cu, Zn, Al, Cr, Pb, Sb, B, 0<x≤1.2, 0<y≤0.9, 2.0≤z≤2.3). They can be used alone or in combination. From the perspective of achieving a high capacity of the secondary battery 10, the positive electrode active material preferably contains Li x NiO2、Li x Co y Ni 1-y O2、Li x Ni 1-y M y O z (M is at least one of Na, Mg, Sc, Y, Mn, Fe, Co, Ni, Cu, Zn, Al, Cr, Pb, Sb, B, 0<x≤1.2, 0<y≤0.9, 2.0≤z≤2.3) and the like lithium nickel composite oxides.

[0026] Examples of the conductive agent contained in the positive electrode mixture layer include carbon black (CB), acetylene black (AB), Ketjen black, carbon nanotubes (CNT), graphene, graphite and other carbonaceous particles, which may be used alone or in combination of two or more.

[0027] As the binder included in the positive electrode mixture layer, for example, fluorine resins such as polytetrafluoroethylene (PTFE) and polyvinylidene fluoride (PVDF), polyimide resins, acrylic resins, polyolefin resins, and polyacrylonitrile (PAN) can be cited. They can be used alone or in combination of two or more.

[0028] The negative electrode 12 has a strip-shaped negative electrode current collector and a negative electrode mixture layer formed on the surface of the negative electrode current collector. The negative electrode mixture layer is preferably formed on both sides of the negative electrode current collector. For the negative electrode current collector, a foil of a metal such as copper or a copper alloy that is stable within the potential range of the negative electrode 12, a film that arranges the metal on the surface, etc. can be used.

[0029] The negative electrode mixture layer may contain a negative electrode active material, a binder, etc. The negative electrode mixture layer is produced, for example, by applying a negative electrode mixture slurry containing a negative electrode active material, a binder, and a solvent such as water to both surfaces of a negative electrode current collector, drying the slurry, and then rolling the slurry.

[0030] The negative electrode active material contained in the negative electrode mixture layer is not particularly limited as long as it is a material that can reversibly absorb and release lithium ions, and carbon materials such as graphite are generally used. The graphite can be any of natural graphites such as flaky graphite, block graphite, and earthy graphite, block artificial graphite, and artificial graphites such as graphitized mesophase carbon microbeads.

[0031] As the negative electrode active material, it is preferred to include a silicon-containing material. This can improve the battery capacity of the secondary battery 10. For the negative electrode 12 including the silicon-containing material, although the volume change caused by the charge and discharge of the battery is large and it is easy to cause electrolyte shortage on the winding center side of the electrode body 14, the effect of the present invention can improve the charge and discharge cycle characteristics. As the silicon-containing material, for example, SiO x (0.5≤x≤1.6) represented by a silicon-containing compound, in which Li 2y SiO (2+y) A silicon-containing compound in which fine particles of Si are dispersed in a lithium silicate phase represented by (0<y<2), and a silicon-containing compound in which fine particles of Si are dispersed in a carbon phase.

[0032] As the binder contained in the negative electrode mixture layer, for example, styrene-butadiene rubber (SBR), nitrile rubber (NBR), carboxymethyl cellulose (CMC) or its salt, polyacrylic acid (PAA) or its salt, polyvinyl alcohol (PVA) can be cited. They can be used alone or in combination of two or more.

[0033] For the separator 13, for example, a porous sheet having ion permeability and insulation is used. Specific examples of the porous sheet include microporous films, woven fabrics, and nonwoven fabrics. As the material of the separator 13, olefin resins such as polyethylene and polypropylene, cellulose, etc. are preferred. The separator 13 may be a laminate having a cellulose fiber layer and a thermoplastic resin fiber layer such as an olefin resin, or may be a multilayer separator including a polyethylene layer and a polypropylene layer.

[0034] The separator 13 may have a heat-resistant layer on at least one surface. In other words, the separator 13 may have a heat-resistant layer on at least one of the surface opposite to the positive electrode 11 and the surface opposite to the negative electrode 12. The heat-resistant layer is preferably provided at least on the surface opposite to the positive electrode 11. The heat-resistant layer is provided on the entire surface of the separator 13, for example.

[0035] The heat-resistant layer, for example, includes a filler and a binder. As a filler, for example, metal oxide particles such as aluminum oxide, metal nitride particles, metal fluoride particles, metal carbide particles, and sulfide particles can be cited. They can be used alone or in combination of two or more. As a binder, for example, fluorine resins such as polyvinylidene fluoride (PVDF), polytetrafluoroethylene (PTFE), polyimide resins, polyamide resins, acrylic resins, polyolefin resins, styrene-butadiene rubber (SBR), nitrile rubber (NBR), carboxymethyl cellulose (CMC) or its salt, polyacrylic acid (PAA) or its salt, polyvinyl alcohol (PVA) can be cited. They can be used alone or in combination of two or more.

[0036] In the electrode body 14, the insulator 30 is disposed between the separator 13 and at least one of the positive electrode 11 and the negative electrode 12. This facilitates the penetration of the electrolyte solution into the separator 13, thereby improving the charge and discharge cycle characteristics. Figure 3 This is a front view showing the separator 13 of the electrode body 14 constituting an example of the embodiment in an unfolded state, and is a figure obtained by projecting the insulator. In this embodiment, the insulator 30 has a linear shape extending along the short side direction of the separator 13. In other words, the linear insulator 30 is arranged approximately parallel to the short side direction of the separator 13, and the length of the insulator 30 is approximately the same as the length of the short side direction of the separator 13.

[0037] When the center of the separator 13 in the long side direction is divided into the inner winding area 13a on the inner side of the winding and the outer winding area 13b on the outer side of the winding, the projected area of ​​the insulator 30 in the inner winding area 13a on the separator 13 is larger than the projected area of ​​the insulator 30 in the outer winding area 13b on the separator 13. As a result, the volume of the insulator 30 can be reduced as much as possible while suppressing the shortage of the electrolyte on the inner center side of the winding, so that the battery capacity and the charge and discharge cycle characteristics can be taken into account. Since the insulator 30 is configured, the volume of the positive electrode 11 and the negative electrode 12 that can be accommodated in the outer shell 15 is reduced, so the battery capacity becomes smaller, but by configuring more insulators 30 in the inner winding area 13a than in the outer winding area 13b, the battery capacity and the charge and discharge cycle characteristics can be taken into account. The projected area of ​​the insulator 30 in the winding inner region 13a on the separator 13 is preferably 0.1% to 50% of the area of ​​the winding inner region 13a, more preferably 0.1% to 20%, further preferably 0.1% to 10%, and particularly preferably 0.1% to 5%.

[0038] exist Figure 3 In the illustrated embodiment, five insulators 30 having the same width are arranged at equal intervals only in the winding inner region 13 a , and no insulator 30 is arranged in the winding outer region 13 b . Figure 4 is included Figure 3The top view of the upper surface of the electrode body 14 of the separator 13 shown in FIG. 1 is a diagram showing the position where the insulator 30 is arranged. Figure 4 As shown, the insulator 30 is arranged on the winding center side. In addition, the arrangement of the insulator 30 is not limited to this example. The number of insulators 30 is not particularly limited, the widths of the insulators 30 may be different from each other, and the intervals between the insulators 30 may be different from each other. In addition, the insulator 30 may also be arranged in the winding outer area 13b.

[0039] The width of the linear insulator 30 is, for example, 1 mm or less. The lower limit of the width of the linear insulator 30 is, for example, 0.01 mm. The height of the linear insulator 30 is, for example, 0.5 μm to 1 mm. The cross-sectional shape of the linear insulator 30 is not particularly limited, and is, for example, circular or rectangular.

[0040] The shape of the insulator 30 is not limited to Figure 3 For example, the insulator 30 may have a dot shape. The outer shape of the dot-shaped insulator 30 is, for example, φ1 mm or less. The lower limit of the outer shape of the dot-shaped insulator 30 is, for example, 0.01 mm. The height of the dot-shaped insulator 30 is, for example, 0.5 μm to 1 mm. The shape of the dot-shaped insulator 30 is not particularly limited, and when viewed from the front, it is, for example, a circular shape or a rectangular shape.

[0041] The material of the insulator 30 is not particularly limited as long as it is insulating, and may be, for example, ceramic or resin. The material of the insulator 30 is preferably a resin. As the resin used for the insulator 30, for example, PET (polyethylene terephthalate), PI (polyimide), PP (polypropylene), PBT (polybutylene terephthalate), polytetrafluoroethylene (PTFE) and other fluorine-based resins, polyacrylic acid, polymethacrylic acid, polyacrylate, polymethacrylate and other acrylic resins, etc., can be cited. They can be used alone or in combination of two or more. As a linear insulator 30, for example, PET fibers can be used. The point-shaped insulator 30 can be formed on the surface of the positive electrode 11, the negative electrode 12 or the separator 13 by, for example, dissolving the above-mentioned resin in a solvent and using an inkjet method or the like.

[0042] Example

[0043] Hereinafter, the present invention will be further described by way of examples, but the present invention is not limited to these examples.

[0044] [Production of positive electrode]

[0045] 95 parts by mass of LiNi 0.8 Co 0.15 Al 0.05O2, 2.5 parts by mass of acetylene black (AB), and 2.5 parts by mass of polyvinylidene fluoride (PVDF) with an average molecular weight of 1.1 million are mixed, and an appropriate amount of N-methyl-2-pyrrolidone (NMP) is added to prepare a positive electrode mixture slurry. Next, the positive electrode mixture slurry is applied to both surfaces of a strip-shaped positive electrode collector composed of aluminum foil and dried, then rolled, cut according to a specified plate size, and a positive electrode with a positive electrode mixture layer formed on both surfaces of the positive electrode collector is produced. In the approximate center of the long side direction of the positive electrode, a positive electrode exposure portion is provided where there is no mixture layer and the collector surface is exposed, and an aluminum positive electrode lead is welded to the positive electrode exposure portion.

[0046] [Production of negative electrode]

[0047] 94 parts by mass of graphite, 6 parts by mass of SiO, 1 part by mass of carboxymethyl cellulose (CMC) and 1 part by mass of styrene-butadiene rubber (SBR) were mixed and an appropriate amount of water was added to prepare a negative electrode mixture slurry. Next, the negative electrode mixture slurry was applied to both surfaces of a strip-shaped negative electrode collector composed of copper foil and dried, then rolled and cut according to a specified plate size to produce a negative electrode having a negative electrode mixture layer formed on both surfaces of the negative electrode collector. A negative electrode exposure portion in which the collector surface is exposed without a mixture layer is provided at the inner end of the winding, and a negative electrode lead made of nickel is welded to the negative electrode exposure portion.

[0048] [Preparation of electrolyte]

[0049] 5 parts by mass of vinylene carbonate (VC) was added to 100 parts by mass of a mixed solvent of ethylene carbonate (EC) and dimethyl carbonate (DMC) (EC:DMC=1:3 by volume ratio), and LiPF6 was dissolved in the mixed solvent to a concentration of 1 mol / L, thereby preparing an electrolyte solution.

[0050] [Manufacturing of Secondary Batteries]

[0051] Ten PET fibers of φ0.1 mm are evenly arranged on the entire portion of the positive electrode surface corresponding to the inner winding area of ​​the separator, and one PET fiber of φ0.1 mm is arranged in the center of the portion of the positive electrode surface corresponding to the outer winding area of ​​the separator. The projected area of ​​one PET fiber on the separator is 0.05% of the area of ​​the inner winding area (or the outer winding area). Afterwards, the positive electrode and the negative electrode are wound with a polyethylene separator to produce an electrode body. Insulating plates are arranged on the upper and lower parts of the electrode body, respectively, and the electrode body is housed in a cylindrical outer shell. Next, the negative electrode lead is welded to the bottom of the outer shell, and the positive electrode lead is welded to the sealing body. Afterwards, the electrolyte is injected into the interior of the outer shell by decompression, and then the open end of the outer shell is sealed by fastening it to the sealing body through a gasket, thereby producing a secondary battery.

[0052] <Example 2>

[0053] In the process of manufacturing a secondary battery, the arrangement of the PET fibers was changed in such a way that only two PET fibers from the winding center side of the 10 PET fibers arranged on the surface of the positive electrode in Example 1 were retained, and the positive electrode and the negative electrode were lengthened in such a way that the diameter of the electrode body became the same as the diameter of the electrode body in Example 1. Except for this, a secondary battery was manufactured in the same manner as Example 1.

[0054] <Example 3>

[0055] In the process of manufacturing a secondary battery, with respect to the PET fibers arranged in the portion corresponding to the winding inner area of ​​the separator on the surface of the positive electrode, the number of PET fibers was changed to 20 in such a manner that the interval between the PET fibers became half the interval between the PET fibers in Example 1, and the positive electrode and the negative electrode were shortened in such a manner that the diameter of the electrode body became the same as the diameter of the electrode body in Example 1. Except for this, a secondary battery was manufactured in the same manner as Example 1.

[0056] <Example 4>

[0057] In the process of manufacturing the secondary battery, PET fibers were not arranged in the area of ​​the positive electrode surface corresponding to the outer winding area of ​​the separator, and the positive electrode and the negative electrode were lengthened in a manner that made the diameter of the electrode body the same as the diameter of the electrode body in Example 1. Except for this, the secondary battery was manufactured in the same manner as Example 1.

[0058] <Comparative Example 1>

[0059] During the production of the secondary battery, the secondary battery was produced in the same manner as in Example 1 except that the positive electrode and the negative electrode were lengthened so that the diameter of the electrode body was the same as that of the electrode body in Example 1 without arranging PET fibers on the surface of the positive electrode.

[0060] <Comparative Example 2>

[0061] In the process of manufacturing a secondary battery, a secondary battery was manufactured in the same manner as in Example 1 except that 10 PET fibers were evenly arranged in the entire area of ​​the positive electrode surface corresponding to the outer winding area of ​​the separator, and the positive and negative electrodes were shortened so that the diameter of the electrode body was the same as that of the electrode body in Example 1.

[0062] [Evaluation of initial discharge capacity and capacity retention rate]

[0063] At an ambient temperature of 25°C, the secondary batteries of the embodiments and comparative examples were charged to 4.2V at a constant current of 1C, and then charged at a constant voltage of 4.2V until the current value reached 0.05C. After standing for 20 minutes, they were discharged to 2.5V at a constant current of 1C. The charge and discharge were regarded as one cycle, and 200 cycles were performed. The capacity retention rate of the secondary batteries of each embodiment and each comparative example in the charge and discharge cycle was calculated by the following formula. In addition, the discharge capacity of the first cycle was taken as the initial discharge capacity.

[0064] Capacity retention rate = (discharge capacity at the 200th cycle / discharge capacity at the 1st cycle) × 100

[0065] Table 1 shows the evaluation results of the initial discharge capacity and capacity retention rate of the secondary batteries of the examples and comparative examples. The initial discharge capacity of the secondary batteries of Examples 1 to 4 and Comparative Example 2 is a value relatively expressed when the initial discharge capacity of the secondary battery of Comparative Example 1 is set to 100. In addition, Table 1 also shows the ratio of the projected area of ​​the insulator to the area of ​​the inner winding area (or the outer winding area) in the inner winding area and the outer winding area.

[0066] [Table 1]

[0067]

[0068] In the secondary battery of the embodiment, both the initial discharge capacity and the charge-discharge cycle characteristics can be taken into account. On the other hand, the charge-discharge cycle characteristics of the secondary battery of Comparative Example 1 in which the insulator is not configured are poor, and the initial discharge capacity of the secondary battery of Comparative Example 2 in which the number of insulators in the outer winding area is configured with the same number as the number of insulators in the inner winding area is poor. Therefore, it can be seen that by configuring the insulator in the inner winding area so that the projected area of ​​the insulator on the separator is larger than the projected area of ​​the insulator in the outer winding area on the separator, both the battery capacity and the charge-discharge cycle characteristics are improved.

[0069] Description of Reference Numerals

[0070] 10. Secondary battery; 11. Positive electrode; Inner end of winding; 12. Negative electrode; 13. Separator; 13a. Inner region of winding; 13b. Outer region of winding; 14. Electrode body; 15. Outer shell; 16. Sealing body; 17, 18. Insulating plate; 19. Positive electrode lead; 20. Negative electrode lead; 21. Groove; 22. Filter; 23. Lower valve core; 24. Insulating member; 25. Upper valve core; 26. Cover; 26a. Opening; 27. Gasket; 28. Winding shaft; 30. Insulator.

Claims

1. A cylindrical secondary battery comprising: An electrode body, which is formed by winding a positive electrode and a negative electrode with a separator interposed therebetween; electrolyte; and A cylindrical outer shell contains the electrode body and the electrolyte, wherein: An insulator is disposed between at least one of the positive electrode and the negative electrode and the separator, When the separator is divided into an inner winding area on the inner side of the winding and an outer winding area on the outer side of the winding in the center of the long side direction, the projection area of ​​the insulator in the inner winding area on the separator is larger than the projection area of ​​the insulator in the outer winding area on the separator.

2. The cylindrical secondary battery according to claim 1, wherein The separator has a heat-resistant layer on at least one of a surface facing the positive electrode and a surface facing the negative electrode.

3. The cylindrical secondary battery according to claim 1 or 2, wherein: The insulator has a linear shape extending along a short side direction of the separator.

4. The cylindrical secondary battery according to claim 3, wherein: The insulator has a width of 1 mm or less.

5. The cylindrical secondary battery according to claim 1 or 2, wherein: The insulator has a dot-like shape.

6. The cylindrical secondary battery according to claim 5, wherein: The outer shape of the insulator is φ1 mm or less.

7. The cylindrical secondary battery according to any one of claims 1 to 6, wherein The projected area of ​​the insulator in the winding inner region on the separator is 0.1% to 50% of the area of ​​the winding inner region.

8. The cylindrical secondary battery according to any one of claims 1 to 7, wherein The insulator is not arranged in the outer winding region.

9. The cylindrical secondary battery according to any one of claims 1 to 8, wherein The insulator is made of resin.

10. The cylindrical secondary battery according to any one of claims 1 to 9, wherein The negative electrode includes a silicon-containing material as a negative electrode active material.

11. The cylindrical secondary battery according to any one of claims 1 to 10, wherein The electrode body has a diameter of 20 mm or more.

Citation Information

Patent Citations

  • Nonaqueous electrolyte secondary battery

    JP2008226696A