Flexible film, salt crystallization device and salt crystallization method

By using flexible film adhesion wires during salt crystallization, the surface free energy is reduced, and combined with a roll-type recovery device, the problems of low efficiency and large artificial investment in the existing salt crystallization technology are solved, and high-efficiency salt crystallization and collection are achieved.

CN118925265APending Publication Date: 2024-11-12SHANGHAI SHENGLONG ENVIRONMET REMEDIATION TECH CO LTD

Patent Information

Application Number
CN202411351234.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-26
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

The existing salt crystallization technology has the problem of low crystallization efficiency, impurities need to be added, and salt collection requires high working intensity and low efficiency.

Method used

Using a flexible film, wires are attached to the surface to reduce the surface free energy during crystal nucleation, improve crystallization efficiency, and efficient collection of salt crystals is achieved through a roll recovery device.

Benefits of technology

The efficiency of salt crystallization and salt formation efficiency are improved, manual investment is reduced, and the effect of rapid salt formation on a large area is achieved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118925265A_ABST
    Figure CN118925265A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of salt pan production, and discloses a device for promoting salt formation and mechanically collecting salt crystals through a flexible film and a salt crystallization method. The surface of the flexible film (1) is connected with attachment wires (2), the length of each attachment wire (2) is 0.5-1.5 cm, the diameter of the cross section of each attachment wire (2) is smaller than or equal to 0.3 mm, and the number of the attachment wires on the surface of each square centimeter of the flexible film is 10-50. The invention provides a flexible film (1) beneficial to salt crystallization, which provides attachment points for salt crystallization, can effectively reduce the surface free energy in the crystal nucleation process, improve the crystallization efficiency and promote large-area rapid salt formation, and also provides a salt collecting mechanism for improving the salt formation efficiency and reducing the labor investment to integrally optimize and improve the salt crystallization method.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of salt field production, and in particular to a flexible membrane, a salt crystallization device and a salt crystallization method. Background Art

[0002] After relevant experimental analysis, after the brine is exposed to the sun and concentrated by evaporation, the first salt to be saturated is NaCl. The longer the NaCl is exposed to the sun, the more crystals are obtained after evaporation. Before the brine formation rate becomes 3.1%, the NaCl content is the highest in the total amount of salts, and it can produce industrial salt. In the final stage of evaporation, the amount of NaCl precipitation will be greatly reduced, and the content will only account for 62.05%. This is due to the precipitation of other salts in the salt field. At the same time, in the final stage of potassium extraction, the concentration of some trace elements in the mother brine will gradually increase, and the corresponding content in the precipitated solid phase will also increase accordingly. From this analysis, salt lake brine will usually evaporate naturally in the sun, but a large amount of rock salt and water alkali will precipitate during the evaporation process. In the later stage of evaporation, high-quality potassium-rich, boron-rich mixed salts and various mother halides will be obtained. These substances are valuable resources for extracting inorganic salts such as potassium, lithium, and boron.

[0003] The solarization process is a relatively scientific, environmentally friendly and convenient way to extract salt resources. The production process saves energy and produces high-quality products. However, the solarization process mainly uses solar energy for processing and is greatly affected by natural weather. At the same time, through the discussion of the solarization process of salt lake brine to extract potassium from salt pans, its process flow still has some shortcomings. Only by finding the reasons can we better improve the process. In production practice, it is necessary to continuously introduce reasonable equipment and facilities, optimize the salt pan construction plan, and use the salt pan solarization process to extract potassium, which can minimize the water loss during the evaporation of brine, thereby reducing cost investment and maximizing salt production.

[0004] The key to salt production is crystallization, but the existing salt crystallization technology has low crystallization efficiency, and salt crystallization requires the addition of other substances to introduce impurities, and salt collection requires manual work, high labor intensity and low efficiency. Therefore, there is an urgent need for an efficient salt-forming and harvesting device and method. Summary of the invention

[0005] The purpose of the present invention is to overcome the problems of low crystallization efficiency in the prior art, the need to add other substances to introduce impurities, and the need for manual work, high labor intensity and low efficiency in collecting salt, and to provide a flexible membrane, a salt crystallization device and a salt crystallization method.

[0006] In order to achieve the above object, the first aspect of the present invention provides a flexible film, wherein the surface of the flexible film is connected with attachment threads, the length of the attachment threads is 0.5-1.5 cm, the cross-sectional diameter is ≤0.3 mm, and the number of attachment threads per square centimeter of the flexible film surface is 10-50.

[0007] A second aspect of the present invention provides a salt crystallization device, which comprises the flexible membrane and a membrane collection mechanism described in the first aspect.

[0008] A third aspect of the present invention provides a method for salt crystallization, comprising: performing salt crystallization in the presence of the flexible membrane described in the first aspect.

[0009] Through the above technical scheme, the present invention provides a flexible membrane that is conducive to salt crystallization, provides attachment points for salt crystals, can effectively reduce the surface free energy in the crystal nucleation process, improve crystallization efficiency, and promote large-area rapid salt formation. At the same time, it provides a membrane collection mechanism that improves salt formation efficiency and reduces labor input, thereby optimizing and improving the salt crystallization method as a whole. BRIEF DESCRIPTION OF THE DRAWINGS

[0010] Figure 1 is a schematic side view of a salt crystallization device;

[0011] Figure 2 It is a top view of the salt crystallization device;

[0012] Figure 3 It is a schematic diagram of the attachment thread positions and punching positions on the flexible membrane.

[0013] Description of Reference Numerals

[0014] 1-salt field dam; 2-salt collecting container; 3-reel base; 4-reel; 5-vibrating soft brush; 6-telescopic device; 7-flexible membrane; 8-flexible membrane traction rope. DETAILED DESCRIPTION

[0015] The endpoints and any values ​​of the ranges disclosed in this article are not limited to the precise ranges or values, and these ranges or values ​​should be understood to include values ​​close to these ranges or values. For numerical ranges, the endpoint values ​​of each range, the endpoint values ​​of each range and the individual point values, and the individual point values ​​can be combined with each other to obtain one or more new numerical ranges, which should be considered as specifically disclosed in this article.

[0016] The first aspect of the present invention provides a flexible film, wherein the surface of the flexible film is connected with attachment threads, the length of the attachment threads is 0.5-1.5 cm, the cross-sectional diameter is ≤0.3 mm, and the number of attachment threads per square centimeter of the flexible film surface is 10-50.

[0017] In the present invention, a flexible membrane and attached wires connected to the surface are used to accelerate salt crystallization and increase the size of salt particles during the salt drying process, thereby promoting rapid salt formation over a large area. The salt material is rolled up through a roll-type recovery device, and the salt particles are separated from the screen material using a vibrating soft brush, thereby achieving the effect of improving salt formation efficiency and reducing labor input.

[0018] In some specific embodiments of the present invention, the length of the attachment wire is 0.8-1.2 cm; the attachment wire in the above length range serves as an attachment point for crystallization nucleation, which can provide a greater contact opportunity for crystal attachment growth and improve crystallization efficiency. The attachment wire can be welded to the flexible film by extrusion hot melting, or it can be produced by one-time extrusion molding.

[0019] In some specific embodiments of the present invention, the cross-sectional diameter of the attachment wire is 100-300 μm, preferably 150-250 μm; the attachment wire in the above cross-sectional diameter range serves as an attachment point for crystallization nucleation, which can provide greater contact opportunities for crystal attachment and growth, and further improve crystallization efficiency.

[0020] In some specific embodiments of the present invention, the number of attached filaments per square centimeter of the flexible film surface is 20-40; within the above range of the number of attached filaments per square centimeter of the flexible film surface, better crystallization efficiency can be ensured.

[0021] In some specific embodiments of the present invention, the thickness of the flexible film is 0.3-0.5 mm.

[0022] In some specific embodiments of the present invention, the present invention has no special requirements on the material of the flexible film, as long as it meets the strength required for curling. Preferably, the transverse tensile strength of the flexible film is ≥3-20KN / m, the elongation at break is ≥600%, and the tensile strength at break is ≥15N / mm. The attachment wire and the flexible film are made of the same material. Specifically, the material of the flexible film can be selected from HDPE, LDPE or UPVC.

[0023] In some specific embodiments of the present invention, in order to prevent the flexible membrane from being unable to be laid flat on the bottom of the salt pan due to buoyancy, the surface of the flexible membrane is also distributed with holes ( Figure 3 ), preferably, the hole is selected from a round hole and / or a square hole.

[0024] In some specific embodiments of the present invention, preferably, the area of ​​the hole (i.e., the cross-sectional area) is 1-9 mm 2 .

[0025] In some specific embodiments of the present invention, more preferably, the side length of the square hole is 1-3 mm.

[0026] In some specific embodiments of the present invention, more preferably, the diameter of the circular hole is 1-3 mm;

[0027] In some specific embodiments of the present invention, preferably, the pore spacing on the surface of the flexible membrane is 1-3 mm. The "pore spacing" is represented by the shortest interval between the centers of two adjacent pores.

[0028] A second aspect of the present invention provides a salt crystallization device, such as Figure 1 and Figure 2 As shown, the device includes the flexible film and film collection mechanism described in the first aspect. The film collection mechanism is placed on the salt pan dam 1, and a salt collecting container 2 is placed on the salt pan dam 1 (that is, the device may also include a salt collecting container placed on the salt pan dam when in use, for collecting salt crystals). The film collection mechanism is mainly used to retract and release the flexible film, that is, to release (rewind and lay flat) the flexible film into the salt pan during crystallization, and to retract (roll up) the flexible film with the crystallized salt attached after the crystallization is completed in order to collect the salt.

[0029] In some specific embodiments of the present invention, the film collecting mechanism comprises:

[0030] A reel base 3 and a reel 4, wherein the reel 4 is mounted on the reel base 3;

[0031] The reel 4 comprises a vibrating soft brush 5 and a telescopic device 6. The flexible film 7 is connected to the reel 4. The vibrating soft brush 5 is installed on one side of the flexible film 7 of the reel 4 so that the vibrating soft brush 5 can scrape the crystallized salt on the flexible film.

[0032] In some specific embodiments of the present invention, the vibrating soft brush 5 starts vibrating during the rolling up of the flexible film, vibrates and scrapes the salt crystals on the attached wire and the surface of the flexible film, causing them to fall into the salt collecting container below for salt collection.

[0033] In some specific embodiments of the present invention, a traction rope 8 is fixedly connected to the reel 4, and the flexible film 7 is rolled onto the reel 4 through the traction rope 8. The traction rope 7 can reversely stretch the reel 4 with the flexible film 1, and gradually stretch it until the flexible film is flattened on the bottom of the salt pan for the next crystallization and salt collection.

[0034] In some specific embodiments of the present invention, the reel 4 can be controllably rotated counterclockwise or clockwise to roll up and lay the flexible film 7 flat. Preferably, the reel 4 can be electrically controlled to rotate counterclockwise and clockwise to roll up and lay the flexible film 7 flat. The speed of rolling up and laying the flexible film flat can be any conventional control speed in the art.

[0035] The third aspect of the present invention provides a method for salt crystallization, which comprises: performing salt crystallization in the presence of the flexible membrane 1 described in the first aspect.

[0036] In some specific embodiments of the present invention, the method further comprises: collecting the crystallized salt obtained after the salt crystallization by the film collecting mechanism described in the second aspect.

[0037] In some specific embodiments of the present invention, the following steps are included:

[0038] (1) During the salt drying process in the salt pan, a reel device is installed on both sides of the salt pan dam, and a flexible film 7 is laid flat on the bottom of the salt pan, and the attachment wire connected to the flexible film 7 in the device is used to promote salt crystallization;

[0039] (2) controlling the reel 4 to rotate counterclockwise to roll up the flexible film 7, keeping the attached wire on the outside of the reel 4, and in the process of rolling up the flexible film 7, interlockingly turning on the vibrating soft brush 5 to scrape the salt crystals on the attached wire and the surface of the flexible film 7, so that they fall into the salt collecting container;

[0040] (3) After the flexible film 7 is rolled up, the vibrating soft brush 5 stops vibrating, and the winding drum 4 is controlled to rotate clockwise to lay the flexible film 7 back flat;

[0041] (4) Repeat steps (1) to (3) at least once.

[0042] In some specific embodiments of the present invention, the specific process of rewinding and laying the flexible film 7 is: rotating the reel 4 clockwise, stretching the reel in the opposite direction through the traction rope 8, and gradually stretching the flexible film until it is laid flat on the bottom of the salt pan, and then stopping the rotation of the reel 4.

[0043] In some specific embodiments of the present invention, wherein the crystallization is evaporative crystallization, preferably, the crystallization temperature is greater than or equal to 18°C ​​(such as 18-25°C).

[0044] In some specific embodiments of the present invention, preferably, underground brine extracted from salt pans is subjected to salt crystallization, that is, the brine to be subjected to salt crystallization is underground brine extracted from salt pans, and its components mainly include sodium chloride, potassium chloride, magnesium chloride, calcium chloride, magnesium sulfate and magnesium bromide. According to one embodiment of the present invention, the brine to be subjected to salt crystallization contains 15-20wt% sodium chloride, 1-3wt% potassium chloride, 3-15wt% magnesium chloride and 4-7wt% magnesium sulfate. The inorganic salt (such as sodium chloride, salt content>5wt%) is crystallized by the device of the present invention, and the liquid after crystallization also contains other impurities, and the liquid is further subjected to subsequent treatment.

[0045] In some specific embodiments of the present invention, the salt crystallization device is operated for 1-10 days, preferably 2-8 days, and during the operation, the flexible membrane is retracted and released once a day.

[0046] In some specific embodiments of the present invention, as the flexible film 7 is rolled up, the thickness of the roll 4 increases, and the telescopic device of the vibrating soft brush 5 automatically follows the thickness of the flexible film roll to extend outward to ensure synchronous scraping and sweeping operations. When winding the film, the roll reverses to pull the rolled film back to the bottom of the salt pond. According to the length of the film, the film winding roll is provided with a winch limit to prevent excessive winding from causing the film material to be torn or damaged or the traction rope to break.

[0047] In some specific embodiments of the present invention, the width of the flexible membrane is determined according to the block width of the salt pan. Generally, the width of the salt pan does not exceed 30m. Preferably, the width of the salt pool is 10-20m and the length is 20-30m. It can be arranged in a way of setting a flexible membrane for every 6-14m salt pan, and multiple flexible membranes can be placed in parallel in the salt pan to meet the collection requirements. It can also be adopted that a flexible membrane is set for each salt pan, or multiple flexible membranes can be welded together. The length of the flexible membrane is 1-3m longer than the longitudinal length of the bottom of the salt pan, which is convenient for the retracting and releasing operation of the flexible membrane during the hoisting process.

[0048] In some specific embodiments of the present invention, according to the different crystallization conditions and stages of different salts, the flexible membrane and the membrane collection mechanism can operate repeatedly, and the crystals of different salts can be effectively collected.

[0049] According to a particularly preferred embodiment of the present invention, a flexible film is provided, wherein the surface of the flexible film is connected with attachment threads, the length of the attachment threads is 0.8-1.2 cm, the cross-sectional diameter is 150-250 μm, and the number of attachment threads per square centimeter of the flexible film surface is 20-40; the thickness of the flexible film is 0.3-0.5 mm; the material of the flexible film is one of HDPE, LDPE or UPVC; the surface of the flexible film is also distributed with holes, and the area of ​​the holes is 1-9 mm 2 ; The hole spacing on the surface of the flexible membrane is 1-3mm.

[0050] The present invention will be described in detail below through examples.

[0051] In the following examples and comparative examples, if no specific conditions are specified, the experiments were carried out under conventional conditions or conditions recommended by the manufacturer. The reagents or instruments used, if no manufacturer is specified, are all conventional products that can be obtained through commercial channels.

[0052] Example 1

[0053] The salt pond is 15m wide and 25m long. It is used to crystallize underground brine from the salt fields in the Qinghai Salt Mine Area. The main compound contents range from 16.3-19.5wt% sodium chloride, 1.4-2.1wt% potassium chloride, 3.7-14.6wt% magnesium chloride and 4-6.3wt% magnesium sulfate.

[0054] A 15m×28m porous flexible membrane was laid in the salt pond. The material was HDPE and the thickness was 0.5mm. The parameters of the flexible membrane were shown in Table 1. The holes on the surface of the flexible membrane were circular, with a diameter of 2mm and uniform distribution. The spacing between holes on the surface of the flexible membrane was 2mm. Salt crystallization was carried out at a temperature of 18-25℃ for 3 days. The flexible membrane was retracted and released once a day to measure the amount of crystallized salt (measured by weight of NaCl crystals).

[0055] Example 2

[0056] The salt pond is 15m wide and 25m long. It is used to crystallize underground brine from the salt fields in the Qinghai Salt Mine Area. The main compound contents range from 16.3-19.5wt% sodium chloride, 1.4-2.1wt% potassium chloride, 3.7-14.6wt% magnesium chloride and 4-6.3wt% magnesium sulfate.

[0057] A 15m×28m porous flexible membrane is laid in the salt pond. The material is HDPE and the thickness is 0.5mm. The parameters of the flexible membrane are shown in Table 1. The holes distributed on the surface of the flexible membrane are circular, the diameter of the circular holes is 2mm, and the holes are evenly distributed. The spacing between the holes on the surface of the flexible membrane is 2mm. The sodium chloride salt is crystallized using the flexible membrane and the membrane collection mechanism. The operation is carried out for 3 days at a temperature of 18-25°C. The flexible membrane is collected and released once a day, and the amount of crystallized salt (measured by the weight of NaCl crystals) is measured.

[0058] Example 3

[0059] The salt pond is 15m wide and 25m long. It is used to crystallize underground brine from the salt fields in the Qinghai Salt Mine Area. The main compound contents range from 16.3-19.5wt% sodium chloride, 1.4-2.1wt% potassium chloride, 3.7-14.6wt% magnesium chloride and 4-6.3wt% magnesium sulfate.

[0060] A 15m×28m porous flexible membrane is laid in the salt pond. The material is HDPE and the thickness is 0.5mm. The parameters of the flexible membrane are shown in Table 1. The holes distributed on the surface of the flexible membrane are circular, the diameter of the circular holes is 3mm, and the holes are evenly distributed. The spacing between the holes on the surface of the flexible membrane is 2mm. The sodium chloride salt is crystallized using the flexible membrane and the membrane collection mechanism. The operation is carried out for 3 days at a temperature of 18-25°C. The flexible membrane is collected and released once a day, and the amount of crystallized salt (measured by the weight of NaCl crystals) is measured.

[0061] Example 4

[0062] The salt pond is 15m wide and 25m long. It is used to crystallize underground brine from the salt fields in the Qinghai Salt Mine Area. The main compound contents range from 16.3-19.5wt% sodium chloride, 1.4-2.1wt% potassium chloride, 3.7-14.6wt% magnesium chloride and 4-6.3wt% magnesium sulfate.

[0063] The flexible membrane and membrane collection mechanism are the same as those in Example 1, except that the cross-sectional diameter of the attached wire is 100 μm. Salt crystallization is carried out using the flexible membrane and membrane collection mechanism at a temperature of 18-25° C. for 3 days. The flexible membrane is collected and released once a day, and the amount of crystallized salt (measured by weight of NaCl crystals) is measured.

[0064] Example 5

[0065] The salt pond is 15m wide and 25m long. It is used to crystallize underground brine from the salt fields in the Qinghai Salt Mine Area. The main compound contents range from 16.3-19.5wt% sodium chloride, 1.4-2.1wt% potassium chloride, 3.7-14.6wt% magnesium chloride and 4-6.3wt% magnesium sulfate.

[0066] The flexible membrane and membrane collection mechanism are the same as those in Example 1, except that the number of attached threads per square centimeter of the flexible membrane surface is 10. Salt crystallization is carried out using the flexible membrane and membrane collection mechanism at a temperature of 18-25°C for 3 days. The flexible membrane is collected and released once a day, and the amount of crystallized salt (measured by weight of NaCl crystals) is measured.

[0067] Example 6

[0068] The salt pond is 15m wide and 25m long. It is used to crystallize underground brine from the salt fields in the Qinghai Salt Mine Area. The main compound contents range from 16.3-19.5wt% sodium chloride, 1.4-2.1wt% potassium chloride, 3.7-14.6wt% magnesium chloride and 4-6.3wt% magnesium sulfate.

[0069] The flexible membrane and membrane collection mechanism are the same as those in Example 1, except that the length of the attachment wire is 0.5 cm. Salt crystallization is carried out using the flexible membrane and membrane collection mechanism at a temperature of 18-25°C for 3 days. The flexible membrane is collected and released once a day, and the amount of crystallized salt (measured by weight of NaCl crystals) is measured.

[0070] Example 7

[0071] The salt pond is 15m wide and 25m long. It is used to crystallize underground brine from the salt fields in the Qinghai Salt Mine Area. The main compound contents range from 16.3-19.5wt% sodium chloride, 1.4-2.1wt% potassium chloride, 3.7-14.6wt% magnesium chloride and 4-6.3wt% magnesium sulfate.

[0072] The flexible membrane and membrane collection mechanism are the same as those in Example 1, except that the holes distributed on the surface of the flexible membrane are circular, and the diameter of the circular holes is 4 mm. Salt crystallization is carried out using the flexible membrane and membrane collection mechanism at a temperature of 18-25°C for 3 days. The flexible membrane is collected and released once a day, and the amount of crystallized salt (measured by weight of NaCl crystals) is measured.

[0073] Example 8

[0074] The salt pond is 15m wide and 25m long. It is used to crystallize underground brine from the salt fields in the Qinghai Salt Mine Area. The main compound contents range from 16.3-19.5wt% sodium chloride, 1.4-2.1wt% potassium chloride, 3.7-14.6wt% magnesium chloride and 4-6.3wt% magnesium sulfate.

[0075] The flexible membrane and membrane collection mechanism are the same as those in Example 1, except that the cross-sectional diameter of the attachment wire is 50 μm. Salt crystallization is carried out using the flexible membrane and membrane collection mechanism at a temperature of 18-25° C. for 3 days. The flexible membrane is collected and released once a day, and the amount of crystallized salt (measured by weight of NaCl crystals) is measured.

[0076] Comparative Example 1

[0077] The salt pond is 15m wide and 25m long. It is used to crystallize underground brine from the salt fields in the Qinghai Salt Mine Area. The main compound contents range from 16.3-19.5wt% sodium chloride, 1.4-2.1wt% potassium chloride, 3.7-14.6wt% magnesium chloride and 4-6.3wt% magnesium sulfate.

[0078] The flexible membrane and membrane collection mechanism are the same as those in Example 1, except that the length of the attachment wire is 0.3 cm. Salt crystallization is carried out using the flexible membrane and membrane collection mechanism at a temperature of 18-25°C for 3 days. The flexible membrane is collected and released once a day, and the amount of crystallized salt (measured by weight of NaCl crystals) is measured.

[0079] Comparative Example 2

[0080] The salt pond is 15m wide and 25m long. It is used to crystallize underground brine from the salt fields in the Qinghai Salt Mine Area. The main compound contents range from 16.3-19.5wt% sodium chloride, 1.4-2.1wt% potassium chloride, 3.7-14.6wt% magnesium chloride and 4-6.3wt% magnesium sulfate.

[0081] The flexible membrane and membrane collection mechanism are the same as those in Example 1, except that the number of attached threads per square centimeter of the flexible membrane surface is 5. Salt crystallization is carried out using the flexible membrane and membrane collection mechanism at a temperature of 18-25°C for 3 days. The flexible membrane is collected and released once a day, and the amount of crystallized salt (measured by weight of NaCl crystals) is measured.

[0082] The crystallization efficiency was determined by calculating the amount of crystallized salt per square meter of the flexible film. The results are shown in Table 1.

[0083] Table 1

[0084]

[0085] It can be seen from the results in Table 1 that the flexible membrane of the present invention has a significantly better effect when the length of the attached wires is 0.5-1.5 cm, the cross-sectional diameter is ≤0.3 mm, and the number of attached wires per square centimeter of the flexible membrane surface is 10-50.

[0086] The preferred embodiments of the present invention are described in detail above, but the present invention is not limited thereto. Within the technical concept of the present invention, the technical solution of the present invention can be subjected to a variety of simple modifications, including the combination of various technical features in any other suitable manner, and these simple modifications and combinations should also be regarded as the contents disclosed by the present invention and belong to the protection scope of the present invention.

Claims

1. A flexible film, characterized in that The surface of the flexible film is connected with attachment threads, the length of the attachment threads is 0.5-1.5 cm, the cross-sectional diameter is ≤0.3 mm, and the number of the attachment threads per square centimeter of the flexible film surface is 10-50.

2. The flexible film according to claim 1, wherein The length of the attachment thread is 0.8-1.2 cm; and / or, the cross-sectional diameter of the attachment filament is 100-300 μm, preferably 150-250 μm; and / or, the number of attached threads per square centimeter of the flexible film surface is 20-40; And / or, the thickness of the flexible film is 0.3-0.5 mm.

3. The flexible film according to claim 1 or 2, wherein: The surface of the flexible membrane is also distributed with holes, preferably, the holes are selected from round holes and / or square holes; Preferably, the area of ​​the hole is 1-9 mm 2 ; More preferably, the side length of the square hole is 1-3 mm; More preferably, the diameter of the circular hole is 1-3 mm; Preferably, the pore spacing on the surface of the flexible membrane is 1-3 mm.

4. A salt crystallization device, comprising the flexible membrane according to any one of claims 1 to 3 and a membrane collection mechanism.

5. The device according to claim 4, wherein: The film collecting mechanism comprises: A reel base (3) and a reel (4), wherein the reel (4) is mounted on the reel base (3); The reel (4) comprises a vibrating soft brush (5) and a telescopic device (6), the flexible film (7) is connected to the reel (4), and the vibrating soft brush (5) is installed on one side of the flexible film (7) of the reel (4) so ​​that the vibrating soft brush (5) can scrape the crystallized salt on the flexible film.

6. The device according to claim 5, wherein: The reel (4) is fixedly connected to a traction rope (8), and the flexible film (7) is connected to the reel (4) via the traction rope (8).

7. The device according to claim 5 or 6, wherein: The reel (4) can be controllably rotated counterclockwise or clockwise to roll up the flexible film (7) and lay it flat.

8. A method for salt crystallization, characterized in that: The method comprises: carrying out salt crystallization in the presence of a flexible membrane (7) as claimed in any one of claims 1 to 3.

9. The method according to claim 8, wherein: The method further comprises: collecting the crystallized salt obtained after the salt is crystallized by using the film collecting mechanism described in any one of claims 4 to 7.

10. The method according to claim 8 or 9, wherein: The crystallization is evaporative crystallization, and preferably, the crystallization temperature is greater than or equal to 18°C.

Citation Information

Patent Citations

  • Salt crystal extraction device

    CN220213988U

  • No rinse liquid car cleaner with solid polymers

    US4481126A

Cited By

  • Evaporation equipment and process special for concentrating salt-containing water

    CN120698546A