Temperature control method and device for strip steel, rolling mill and storage medium

By setting up strip cooling pipelines and emulsion spray valves on the rolling mill, the flow rate of emulsion is adjusted according to the rolling speed, which solves the problem of large temperature fluctuations in silicon steel rolling, and improves the yield and production stability.

CN118926320AActive Publication Date: 2024-11-12SHOUGANG ZHIXIN QIAN AN ELECTROMAGNETIC MATERIALS CO LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
CN202411169718.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-25
Publication Date
2024-11-12
Estimated Expiration
2044-08-25

AI Technical Summary

Technical Problem

In the prior art, when rolling silicon steel, the temperature fluctuates greatly, resulting in frequent side cracks, brittle fractures and belt breakage accidents, affecting production efficiency and product quality.

Method used

A strip cooling pipeline is set up on the emulsion spray pipeline of the rolling mill, and an emulsion spray valve is installed on the cooling pipeline. The opening of the emulsion spray valve is adjusted according to the rolling speed, and the flow rate of the emulsion is controlled to reduce deformation. Heat and friction heat, keep the strip temperature within a reasonable range.

Benefits of technology

It effectively reduces the temperature fluctuations of strip steel, improves the product yield, reduces edge cracks and strip breakage accidents caused by temperature instability, and improves the controllability of the rolling process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118926320A_ABST
    Figure CN118926320A_ABST
Patent Text Reader

Abstract

The embodiment of the invention provides a strip steel temperature control method and device, electronic equipment and a computer readable storage medium, and relates to the technical field of rolling. The method comprises the steps of obtaining the rolling speed of a rolling mill; when the rolling speed is smaller than 500 m / min, the opening degree of an emulsification spraying valve is adjusted according to the rolling speed; wherein the opening degree of the emulsifying spray valve is in positive correlation with the rolling speed, and the increasing speed of the opening degree is increased along with the increasing of the rolling speed; and when the rolling speed is greater than or equal to 500m / min, setting the opening degree of the emulsifying spray valve to be 100%. According to the embodiment of the invention, the branch of the strip steel cooling pipeline is arranged on the emulsified liquid spraying pipeline of the rolling mill, and the emulsified liquid spraying valve is arranged on the strip steel cooling pipeline, so that the flow of the emulsified liquid is controlled, the increase and decrease amplitude of the corresponding emulsified liquid flow can be set according to different speed intervals, and the yield of products is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of rolling technology, and in particular to a temperature control method, device, rolling mill and storage medium for a steel strip. Background Art

[0002] The rolling mill is a device that realizes the metal rolling process. The rolling mill is mainly composed of rollers, frames, roller gap adjustment devices, roller temperature adjustment devices, transmission devices, lubrication systems, control systems and roll removal devices. When rolling metal, the rolling mill needs to ensure that the temperature of the strip is controlled within a reasonable range. Taking silicon steel as an example, when the temperature of silicon steel during the rolling process is low, edge cracks and brittle fractures are prone to occur; when the temperature of silicon steel is high, the plate shape will fluctuate violently and is difficult to control. It is easy to break the strip, damage the rollers, cause the loss of raw materials and long-term shutdown. Therefore, the temperature control of the strip is very important during the operation of the rolling mill.

[0003] In the prior art, when silicon steel materials are rolled, the temperature of the strip can be controlled by a cooling pipeline, but there is still a problem of large fluctuations in the rolling temperature of the strip. Summary of the invention

[0004] The present application provides a temperature control method, device, rolling mill and storage medium for strip steel, which are used to solve the problem of large temperature fluctuations in strip steel rolling in the prior art.

[0005] According to one aspect of an embodiment of the present application, a temperature control method for a steel strip is provided, which is applied to a rolling mill, wherein the rolling mill is provided with an emulsion spray pipeline and a steel strip cooling pipeline, wherein the steel strip cooling pipeline is connected to the emulsion spray pipeline as a branch of the emulsion spray pipeline, and an emulsion spray valve is provided on the steel strip cooling pipeline, and the method comprises:

[0006] Obtain the rolling speed of the rolling mill;

[0007] When the rolling speed is less than 500m / min, the opening of the emulsification spray valve is adjusted according to the rolling speed; the opening of the emulsification spray valve is positively correlated with the rolling speed, and the increasing speed of the opening increases with the increase of the rolling speed;

[0008] When the rolling speed is greater than or equal to 500 m / min, the opening of the emulsification spray valve is set to 100%.

[0009] In a possible implementation, adjusting the opening of the emulsification spray valve according to the rolling speed includes:

[0010] When the rolling mill is in the startup phase with a rolling speed of zero, the initial opening of the emulsification spray valve is set to 5%.

[0011] In a possible implementation, adjusting the opening of the emulsification spray valve according to the rolling speed includes:

[0012] When the rolling mill is in the speed-up stage after starting and the rolling speed is less than or equal to 200 m / min, the opening increment of the emulsification spray valve is set to the product of the set first opening adjustment coefficient and the rolling speed.

[0013] In another possible implementation, adjusting the opening of the emulsification spray valve according to the rolling speed includes:

[0014] When the rolling mill is in the speed-up stage after starting, and the rolling speed is greater than 200 m / min and less than or equal to 500 m / min, the opening increment of the emulsification spray valve is set to the product of a preset second opening adjustment coefficient and the speed increment of the rolling speed relative to 200 m / min; wherein the first opening adjustment coefficient is less than the second opening adjustment coefficient.

[0015] In another possible implementation, the rolling mill is further provided with an auxiliary cooling pipeline, the auxiliary cooling pipeline being connected to the emulsion spray pipeline as a branch of the emulsion spray pipeline, and a pipeline control valve is provided on the auxiliary cooling pipeline; after determining that the opening of the emulsion spray valve is 100%, the method further includes:

[0016] Get the strip temperature of the rolling mill;

[0017] When the strip temperature exceeds the preset temperature upper limit, the pipeline control valve is opened.

[0018] In another possible implementation, after obtaining the strip temperature of the rolling mill, the following steps are included:

[0019] When the strip temperature exceeds the preset upper temperature limit, the rolling speed is reduced.

[0020] In another possible implementation, the preset upper temperature limit is 130°C.

[0021] According to another aspect of the embodiment of the present application, a temperature control device for a steel strip is provided, which is applied to a rolling mill. The rolling mill is provided with an emulsion spray pipeline and a steel strip cooling pipeline. The steel strip cooling pipeline is connected to the emulsion spray pipeline as a branch of the emulsion spray pipeline. An emulsion spray valve is provided on the steel strip cooling pipeline. The device comprises:

[0022] An acquisition module, used for acquiring the rolling speed of the rolling mill;

[0023] An adjustment module is used to adjust the opening of the emulsification spray valve according to the rolling speed when the rolling speed is less than 500m / min; wherein the opening of the emulsification spray valve is positively correlated with the rolling speed, and the increasing speed of the opening increases with the increase of the rolling speed;

[0024] The determination module is used to set the opening of the emulsification spray valve to 100% when the rolling speed is greater than or equal to 500m / min.

[0025] According to another aspect of the embodiment of the present application, a rolling mill is provided, wherein the rolling mill is equipped with an emulsion spray pipeline and a strip cooling pipeline, wherein the strip cooling pipeline is connected to the emulsion spray pipeline as a branch of the emulsion spray pipeline, and an emulsion spray valve is arranged on the strip cooling pipeline, and the rolling mill comprises:

[0026] An acquisition module, used for acquiring the rolling speed of the rolling mill;

[0027] An adjustment module is used to adjust the opening of the emulsification spray valve according to the rolling speed when the rolling speed is less than 500m / min; wherein the opening of the emulsification spray valve is positively correlated with the rolling speed, and the increasing speed of the opening increases with the increase of the rolling speed;

[0028] The determination module is used to set the opening of the emulsification spray valve to 100% when the rolling speed is greater than or equal to 500m / min.

[0029] According to another aspect of the embodiments of the present application, a computer-readable storage medium is provided, on which a computer program is stored. When the computer program is executed by a processor, the steps of the method shown in the first aspect of the embodiments of the present application are implemented.

[0030] The beneficial effects of the technical solution provided by the embodiment of the present application are:

[0031] The embodiment of the present application sets a strip cooling pipeline branch on the emulsion spray pipeline of the rolling mill, and configures an emulsion spray valve on the strip cooling pipeline to control the flow of the emulsion; specifically, the rolling speed of the rolling mill is first obtained, and when the rolling speed is less than 500m / min, the opening of the emulsion spray valve is adjusted according to the rolling speed. Since the opening of the emulsion spray valve is positively correlated with the rolling speed, and the increasing rate of the opening increases with the increase of the rolling speed, it can effectively reduce the deformation heat and friction heat generated by the strip as the rolling speed increases, and control the temperature of the strip within a reasonable range; until the rolling speed is greater than or equal to 500m / min, the opening of the emulsion spray valve is set to 100%; the embodiment of the present application can effectively solve the problem of large temperature fluctuations in strip rolling in the prior art, and can set the corresponding increase or decrease range of the emulsion flow rate according to different speed ranges, thereby improving the yield rate of the product. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, a brief introduction will be given below to the drawings required for use in the embodiments or the description of the prior art. Obviously, the drawings described below are some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative labor.

[0033] Figure 1 A schematic flow chart of a temperature control method for a steel strip provided in an embodiment of the present application;

[0034] Figure 2 A schematic diagram of a flow chart of opening a pipeline control valve in a temperature control method for a steel strip provided in an embodiment of the present application;

[0035] Figure 3 A schematic flow chart of a temperature control method for a steel strip provided as an example in an embodiment of the present application;

[0036] Figure 4 A schematic diagram of a cooling pipeline of a rolling mill in a temperature control method for a steel strip provided in an embodiment of the present application;

[0037] Figure 5 A schematic structural diagram of a temperature control device for a steel strip provided in an embodiment of the present application;

[0038] Description of reference numerals:

[0039] 1-emulsion spray pipeline, 2-left strip steel cooling pipeline, 3-right strip steel cooling pipeline, 4-pipeline without flow control valve, 5-flow controllable pipeline, 6-left auxiliary cooling pipeline, 7-right auxiliary cooling pipeline. DETAILED DESCRIPTION

[0040] Hereinafter, embodiments of the present disclosure will be described with reference to the accompanying drawings. However, it should be understood that these descriptions are exemplary only and are not intended to limit the scope of the present disclosure. In addition, in the following description, descriptions of well-known structures and technologies are omitted to avoid unnecessary confusion of the concepts of the present disclosure.

[0041] Various structural schematic diagrams according to embodiments of the present disclosure are shown in the accompanying drawings. These figures are not drawn to scale, and some details are magnified and some details may be omitted for the purpose of clear expression. The shapes of various regions and layers shown in the figures and the relative sizes and positional relationships therebetween are only exemplary, and may deviate in practice due to manufacturing tolerances or technical limitations, and those skilled in the art may further design regions / layers with different shapes, sizes, and relative positions according to actual needs.

[0042] In the context of the present disclosure, when a layer / element is referred to as being "on" another layer / element, the layer / element may be directly on the other layer / element or an intervening layer / element may exist between them. In addition, if a layer / element is "on" another layer / element in one orientation, the layer / element may be "below" the other layer / element when the orientation is reversed.

[0043] Silicon steel is a silicon alloy steel with a silicon content of 1.0-4.5% and a carbon content of less than 0.08%. It has the characteristics of high magnetic permeability, low coercive force, and large resistivity, so the hysteresis loss and eddy current loss are small. It is mainly used as a magnetic material in motors, transformers, electrical appliances, and electrical instruments. In order to meet the needs of punching and shearing when manufacturing electrical appliances, a certain plasticity is also required. In order to improve the magnetic induction performance and reduce the hysteresis loss, the content of harmful impurities is required to be as low as possible, and the plate shape is required to be flat and the surface quality is good. The strip temperature control method in the embodiment of the present application can be applied to the rolling of silicon steel.

[0044] When the silicon content of silicon steel is high (>3%), its brittleness and hardness increase. When the rolled thickness is between 1.1 and 1.8 mm, the silicon steel temperature during the rolling process is low, and edge cracks and brittle fractures are prone to occur. When the silicon steel temperature is high, the plate shape will fluctuate violently within a certain temperature range, which is difficult to control and prone to strip breakage accidents, damage to the rolls, loss of raw materials and long-term shutdown. Therefore, when rolling this type of silicon steel, the temperature control mode of the strip is crucial. A reasonable emulsion cooling method can be used in the first three passes of rolling to control the strip temperature within a reasonable range to ensure that the strip shape is stable and does not fluctuate violently without edge cracks, which is conducive to the adjustment of the operator.

[0045] Based on the above technical problems, the inventive concept of this application is to set a strip cooling pipeline branch on the emulsion spray pipeline of the rolling mill, and configure an emulsion spray valve on the strip cooling pipeline to control the flow of the emulsion. When the rolling speed is less than 500m / min, the opening of the emulsion spray valve is adjusted according to the rolling speed. Since the opening of the emulsion spray valve is positively correlated with the rolling speed, and the increasing speed of the opening increases with the increase of the rolling speed, it can effectively reduce the deformation heat and friction heat generated by the strip as the rolling speed increases, and control the temperature of the strip within a reasonable range.

[0046] The temperature control method for steel strip provided in the present application can effectively solve the problem of large temperature fluctuations in steel strip rolling in the prior art, and can set the corresponding increase or decrease range of the emulsion flow rate according to different speed ranges, thereby improving the yield rate of the product.

[0047] The following is a detailed description of the technical solution of the present application and how the technical solution of the present application solves the above-mentioned technical problems with specific embodiments. The following specific embodiments can be combined with each other, and the same or similar concepts or processes may not be repeated in some embodiments. The embodiments of the present application will be described below in conjunction with the accompanying drawings.

[0048] The present application provides a method for controlling the temperature of a steel strip. Figure 1 As shown, it can be applied to a rolling mill, the rolling mill is equipped with an emulsion spray pipeline and a strip cooling pipeline, the strip cooling pipeline is connected to the emulsion spray pipeline as a branch of the emulsion spray pipeline, and an emulsion spray valve is arranged on the strip cooling pipeline;

[0049] The method includes:

[0050] S101, obtaining the rolling speed of the rolling mill.

[0051] S102: When the rolling speed is less than 500 m / min, the opening of the emulsification spray valve is adjusted according to the rolling speed.

[0052] Among them, the opening of the emulsification spray valve is positively correlated with the rolling speed, and the increasing rate of the opening increases with the increase of the rolling speed.

[0053] Specifically, during the start-up stage of the rolling mill, the rolling speed is low, and the deformation heat and friction heat generated by the strip are small. In order to ensure that the temperature of the strip is high, a lower emulsion flow rate is used to cool the strip; as the rolling speed increases, the deformation heat and friction heat generated by the strip increase, and the emulsion flow rate needs to be increased to cool the strip, so that the temperature of the strip is not too high, but is kept within a certain reasonable range.

[0054] In the embodiment of the present application, the flow rate of the pipeline is controlled by changing the opening degree of the emulsified spray valve. According to the increase in speed, the opening degree of the valve body increases, and the emulsion flow rate increases, thereby achieving the purpose of cooling the steel strip, and vice versa. In the present application, the flow rate increase or decrease range of the emulsion spray mode can be set according to the temperature characteristics of the steel strip during the rolling pass and the speed interval.

[0055] S103, when the rolling speed is greater than or equal to 500 m / min, the opening of the emulsification spray valve is set to 100%.

[0056] The embodiment of the present application sets a strip cooling pipeline branch on the emulsion spray pipeline of the rolling mill, and configures an emulsion spray valve on the strip cooling pipeline to control the flow of the emulsion; specifically, the rolling speed of the rolling mill is first obtained, and when the rolling speed is less than 500m / min, the opening of the emulsion spray valve is adjusted according to the rolling speed. Since the opening of the emulsion spray valve is positively correlated with the rolling speed, and the increasing rate of the opening increases with the increase of the rolling speed, it can effectively reduce the deformation heat and friction heat generated by the strip as the rolling speed increases, and control the temperature of the strip within a reasonable range; until the rolling speed is greater than or equal to 500m / min, the opening of the emulsion spray valve is set to 100%; the embodiment of the present application can effectively solve the problem of large temperature fluctuations in strip rolling in the prior art, and can set the corresponding increase or decrease range of the emulsion flow rate according to different speed ranges, thereby improving the yield rate of the product.

[0057] A possible implementation method is provided in an embodiment of the present application, wherein the above-mentioned adjustment of the opening of the emulsification spray valve according to the rolling speed includes:

[0058] When the rolling mill is in the startup phase with a rolling speed of zero, the initial opening of the emulsification spray valve is set to 5%.

[0059] In the embodiment of the present application, during the initial start-up stage of the silicon steel rolling mill, the rolling speed is low, and the friction heat and deformation heat generated are less. In order to make the temperature of the strip higher, a lower emulsion spray flow rate needs to be set, and the initial opening degree C of the emulsion spray valve can be set smaller, for example, C=5%, to ensure that the strip temperature is high and no edge cracks occur.

[0060] A possible implementation method is provided in an embodiment of the present application, wherein the above-mentioned adjustment of the opening of the emulsification spray valve according to the rolling speed includes:

[0061] When the rolling mill is in the speed-up stage after starting and the rolling speed is less than or equal to 200 m / min, the opening increment of the emulsification spray valve is set to the product of the set first opening adjustment coefficient and the rolling speed.

[0062] Specifically, after the rolling mill is started and the rolling speed is lower than 200 m / min, the friction heat and deformation heat generated by the strip gradually increase, but are relatively small. The opening K of the emulsion spray valve can be set by the following formula (1):

[0063] K=5%+V / 1000×S1×100%; (1)

[0064] Among them, K is the opening, V is the rolling speed, S1 is the opening adjustment coefficient. At this time, S1 can be set to 1. When the rolling speed reaches 200m / min, the opening of the emulsion spray pipe valve is K=25%.

[0065] In an embodiment of the present application, when the rolling mill is in the speed-up stage after starting and the rolling speed is low, the friction heat and deformation heat generated in this stage are smaller than those in the high-speed stage of the rolling speed. Therefore, a smaller opening increase rate can be set based on the first opening adjustment coefficient to ensure that the strip temperature is within an appropriate range.

[0066] A possible implementation method is provided in an embodiment of the present application, wherein the above-mentioned adjustment of the opening of the emulsification spray valve according to the rolling speed includes:

[0067] When the rolling mill is in the speed-up stage after starting, and the rolling speed is greater than 200 m / min and less than or equal to 500 m / min, the opening increment of the emulsification spray valve is set to the product of the preset second opening adjustment coefficient and the speed increment of the rolling speed relative to 200 m / min.

[0068] The first opening adjustment coefficient is smaller than the second opening adjustment coefficient.

[0069] Specifically, when the rolling speed of the rolling mill is 200-500 m / min, the friction heat and deformation heat generated by the strip steel increase faster, and the opening K of the emulsion spray valve can be set by the following formula (2):

[0070] K=25%+(V-200) / 1000×S2×100%, (2)

[0071] Wherein, S2 is the opening adjustment coefficient of this stage, and S2=2.5 can be set.

[0072] When the rolling speed reaches 500 m / min, the opening degree K of the emulsion spray valve is 100%, that is, the valve body is fully opened.

[0073] In an embodiment of the present application, when the rolling mill is in the speed-up stage after starting and the rolling speed is high, the friction heat and deformation heat generated in this stage are larger than those in the low-speed stage of the rolling speed. A larger opening increase speed can be set based on the second opening adjustment coefficient to ensure that the strip temperature is within an appropriate range.

[0074] In the embodiment of the present application, during the deceleration stage of the rolling mill, contrary to the speed increase stage, the degree of reduction in the opening of the emulsion spray valve decreases as the speed decreases. The opening of the emulsion spray valve can still be set according to the above formulas (1) and (2), thereby ensuring the stability of the strip temperature during the deceleration of the rolling mill.

[0075] A possible implementation method is provided in the embodiment of the present application, such as Figure 2 As shown, the rolling mill is also equipped with an auxiliary cooling pipeline, which is connected to the emulsion spray pipeline as a branch of the emulsion spray pipeline, and a pipeline control valve is arranged on the auxiliary cooling pipeline.

[0076] After determining that the opening degree of the emulsion spray valve is 100%, the method further includes:

[0077] S201, obtaining the strip temperature of the rolling mill.

[0078] S202, when the strip temperature exceeds the preset temperature upper limit, the pipeline control valve is opened.

[0079] In an embodiment of the present application, when the rolling speed is greater than 500 m / min and the opening of the emulsification spray valve has reached 100%, but the strip temperature is still higher than a reasonable control range, the auxiliary cooling pipe can be opened through the pipeline control valve to further increase the flow rate of the emulsion, thereby reducing the strip temperature and further improving the controllability of the strip temperature.

[0080] A possible implementation method is provided in an embodiment of the present application, which includes, after obtaining the strip temperature of the rolling mill:

[0081] When the strip temperature exceeds the preset upper temperature limit, the rolling speed is reduced.

[0082] In an embodiment of the present application, when the rolling speed is greater than 500m / min, the opening of the emulsification spray valve has reached 100%, and the pipeline control valve of the auxiliary cooling pipe has been opened, but the strip temperature is still higher than the reasonable control range, the deformation heat and friction heat generated by the strip during the rolling process can be reduced by reducing the rolling speed, thereby achieving effective control of the strip temperature.

[0083] A possible implementation method is provided in an embodiment of the present application, and the above-mentioned preset temperature upper limit is 130°C.

[0084] In the embodiment of the present application, taking the rolling of silicon steel as an example, the upper limit of the strip temperature can be 130°C, and the reasonable control range of the strip temperature can be 110°C-130°C, which can effectively improve the yield rate of the strip.

[0085] In order to better understand the temperature control method of the above strip steel, Figure 3 and Figure 4 An example of a temperature control method for a steel strip according to the present invention is described in detail, which method can be applied to a Sendkimier rolling mill, such as Figure 4As shown, the rolling mill is equipped with an emulsion spray pipeline 1, a left strip cooling pipeline 2, a right strip cooling pipeline 3, a left auxiliary cooling pipeline 6, and a right auxiliary cooling pipeline 7. The left and right strip cooling pipelines and the left and right auxiliary cooling pipelines are connected to the emulsion spray pipeline 1 as branches of the emulsion spray pipeline 1; wherein each strip cooling pipeline also includes a pipeline without a flow control valve 4 and a flow controllable pipeline 5. An emulsion spray valve, namely a CV valve (Circulation Valve), is arranged on each strip cooling pipeline. The emulsion spray valve is used to control the flow of the emulsion in the strip cooling pipeline. A pipeline control valve, namely a SV valve (Solenoid Valve), is arranged on the auxiliary cooling pipeline. The pipeline control valve is used to control the opening or closing of the auxiliary cooling pipeline.

[0086] The temperature control method of the strip steel comprises the following steps:

[0087] S301, the initial starting speed of silicon steel rolling is low, and the friction heat and deformation heat generated are less. In order to make the temperature of the strip higher, a lower emulsion spray flow rate needs to be set, and the initial opening degree K of the emulsion spray valve can be set smaller, for example, K = 5%, to ensure that the strip temperature is high and no edge cracks occur.

[0088] S302, after the rolling mill is started, when the rolling speed is less than or equal to 200m / min, the friction heat and deformation heat generated by the strip gradually increase, but are also relatively small. The opening degree of the emulsion spray pipeline valve body can be set:

[0089] K = 5% + V / 1000 × S1 × 100%, where S1 = 1;

[0090] In the formula, K is the opening degree, V is the rolling speed, S1 is the opening degree adjustment coefficient, and when the rolling speed reaches 200m / min, the opening degree K of the emulsion spray pipeline valve body is 25%.

[0091] S303, when the rolling speed is between 200m / min-500m / min, the friction heat and deformation heat generated by the strip increase faster, and the opening degree of the emulsion spray pipeline valve body can be set:

[0092] K = 25% + (V-200) / 1000 × S2 × 100%, where S2 = 2.5;

[0093] When the rolling speed reaches 500 m / min, the opening degree K of the emulsion spray pipeline valve body is 100%.

[0094] S304, when the rolling speed is greater than or equal to 500m / min, the opening degree K of the emulsion spray pipeline valve body is 100%, and when the rolling speed is greater than 500m / min, even when the opening adjustment coefficient changes and K does not reach 100%, K can be directly set to 100% to give full play to the cooling capacity of the emulsion.

[0095] After the rolling mill starts, if the strip temperature is not within a reasonable control range at a certain stage, the emulsion spray flow rate can be manually adjusted to control the strip temperature. For example, if the strip temperature is higher than the reasonable control range, the emulsion spray flow rate can be manually increased to increase the emulsion cooling capacity and reduce the strip temperature to a reasonable control range.

[0096] S305, when the rolling speed is greater than 500m / min or higher, the opening degree of the emulsion spray pipeline valve body has reached 100%, and the strip temperature is still higher than the reasonable control range, the auxiliary cooling pipeline can be opened to increase the emulsion flow rate to cool the strip.

[0097] The present application provides a temperature control device for a steel strip, which is applied to a rolling mill. The rolling mill is equipped with an emulsion spray pipeline and a steel strip cooling pipeline. The steel strip cooling pipeline is connected to the emulsion spray pipeline as a branch of the emulsion spray pipeline. An emulsion spray valve is arranged on the steel strip cooling pipeline. Figure 5 As shown, the temperature control device 50 of the strip steel may include: an acquisition module 501, an adjustment module 502 and a determination module 503;

[0098] Wherein, the acquisition module 501 is used to acquire the rolling speed of the rolling mill;

[0099] The adjustment module 502 is used to adjust the opening of the emulsification spray valve according to the rolling speed when the rolling speed is less than 500 m / min; wherein the opening of the emulsification spray valve is positively correlated with the rolling speed, and the increasing speed of the opening increases with the increase of the rolling speed;

[0100] The determination module 503 is used to set the opening of the emulsification spray valve to 100% when the rolling speed is greater than or equal to 500 m / min.

[0101] In an embodiment of the present application, a possible implementation is provided. When the adjustment module 502 adjusts the opening of the emulsification spray valve according to the rolling speed, it is used to:

[0102] When the rolling mill is in the startup phase with a rolling speed of zero, the initial opening of the emulsification spray valve is set to 5%.

[0103] In an embodiment of the present application, a possible implementation is provided. When the adjustment module 502 adjusts the opening of the emulsification spray valve according to the rolling speed, it is used to:

[0104] When the rolling mill is in the speed-up stage after starting and the rolling speed is less than or equal to 200 m / min, the opening increment of the emulsification spray valve is set to the product of the set first opening adjustment coefficient and the rolling speed.

[0105] In an embodiment of the present application, a possible implementation is provided. When the adjustment module 502 adjusts the opening of the emulsification spray valve according to the rolling speed, it is used to:

[0106] When the rolling mill is in the speed-up stage after starting, and the rolling speed is greater than 200 m / min and less than or equal to 500 m / min, the opening increment of the emulsification spray valve is set to the product of a preset second opening adjustment coefficient and the speed increment of the rolling speed relative to 200 m / min; wherein the first opening adjustment coefficient is less than the second opening adjustment coefficient.

[0107] The present application provides a possible implementation method, wherein the rolling mill is further provided with an auxiliary cooling pipeline, the auxiliary cooling pipeline is connected with the emulsion spray pipeline as a branch of the emulsion spray pipeline, and a pipeline control valve is provided on the auxiliary cooling pipeline; after determining that the opening of the emulsion spray valve is 100%, the device further includes an opening module for:

[0108] Get the strip temperature of the rolling mill;

[0109] When the strip temperature exceeds the preset temperature upper limit, the pipeline control valve is opened.

[0110] A possible implementation method is provided in an embodiment of the present application. After obtaining the strip temperature of the rolling mill, the above-mentioned opening module is used to:

[0111] When the strip temperature exceeds the preset upper temperature limit, the rolling speed is reduced.

[0112] A possible implementation method is provided in an embodiment of the present application, and the above-mentioned preset temperature upper limit is 130°C.

[0113] The device of the embodiments of the present application can execute the method provided by the embodiments of the present application, and the implementation principles are similar. The actions performed by each module in the device of each embodiment of the present application correspond to the steps in the method of each embodiment of the present application. For the detailed functional description of each module of the device, please refer to the description in the corresponding method shown in the previous text, which will not be repeated here.

[0114] The embodiment of the present application sets a strip cooling pipeline branch on the emulsion spray pipeline of the rolling mill, and configures an emulsion spray valve on the strip cooling pipeline to control the flow of the emulsion; specifically, the rolling speed of the rolling mill is first obtained, and when the rolling speed is less than 500m / min, the opening of the emulsion spray valve is adjusted according to the rolling speed. Since the opening of the emulsion spray valve is positively correlated with the rolling speed, and the increasing rate of the opening increases with the increase of the rolling speed, it can effectively reduce the deformation heat and friction heat generated by the strip as the rolling speed increases, and control the temperature of the strip within a reasonable range; until the rolling speed is greater than or equal to 500m / min, the opening of the emulsion spray valve is set to 100%; the embodiment of the present application can effectively solve the problem of large temperature fluctuations in strip rolling in the prior art, and can set the corresponding increase or decrease range of the emulsion flow rate according to different speed ranges, thereby improving the yield rate of the product.

[0115] In an embodiment of the present application, an electronic device is provided, including a memory, a processor, and a computer program stored in the memory. The processor executes the above-mentioned computer program to implement the steps of the temperature control method of the strip. Compared with the related art, the following can be achieved: In an embodiment of the present application, a strip cooling pipeline is set as a branch on the emulsion spray pipeline of the rolling mill, and an emulsion spray valve is configured on the strip cooling pipeline to control the flow rate of the emulsion; specifically, the rolling speed of the rolling mill is first obtained, and when the rolling speed is less than 500m / min, the opening of the emulsion spray valve is adjusted according to the rolling speed. Since the opening of the emulsification spray valve is positively correlated with the rolling speed, and the increasing speed of the opening increases with the increasing rolling speed, the deformation heat and friction heat generated by the strip as the rolling speed increases can be effectively reduced, and the temperature of the strip can be controlled within a reasonable range; until the rolling speed is greater than or equal to 500m / min, the opening of the emulsification spray valve is set to 100%; the embodiment of the present application can effectively solve the problem of large fluctuations in the rolling temperature of the strip in the prior art, and the corresponding increase or decrease range of the emulsion flow rate can be set according to different speed ranges, thereby improving the yield rate of the product.

[0116] In an optional embodiment, a rolling mill is provided, wherein the rolling mill is equipped with an emulsion spray pipeline and a strip cooling pipeline, the strip cooling pipeline is connected to the emulsion spray pipeline as a branch of the emulsion spray pipeline, and an emulsion spray valve is arranged on the strip cooling pipeline, and the rolling mill comprises:

[0117] An acquisition module, used for acquiring the rolling speed of the rolling mill;

[0118] An adjustment module is used to adjust the opening of the emulsification spray valve according to the rolling speed when the rolling speed is less than 500m / min; wherein the opening of the emulsification spray valve is positively correlated with the rolling speed, and the increasing speed of the opening increases with the increase of the rolling speed;

[0119] The determination module is used to set the opening of the emulsification spray valve to 100% when the rolling speed is greater than or equal to 500m / min.

[0120] In the above description, the technical details such as the patterning of each layer are not described in detail. However, those skilled in the art should understand that various technical means can be used to form layers, regions, etc. of desired shapes. In addition, in order to form the same structure, those skilled in the art can also design methods that are not completely the same as the methods described above. In addition, although the various embodiments are described above separately, this does not mean that the measures in the various embodiments cannot be used in combination to advantage.

[0121] Although the preferred embodiments of the present application have been described, those skilled in the art may make other changes and modifications to these embodiments once they have learned the basic creative concept. Therefore, the appended claims are intended to be interpreted as including the preferred embodiments and all changes and modifications falling within the scope of the present application.

[0122] Obviously, those skilled in the art can make various changes and modifications to the present application without departing from the spirit and scope of the present application. Thus, if these modifications and variations of the present application fall within the scope of the claims of the present application and their equivalents, the present application is also intended to include these modifications and variations.

Claims

1. A temperature control method for a strip steel, applied to a rolling mill, It is characterized in that The rolling mill is equipped with an emulsion spray pipeline and a strip cooling pipeline, the strip cooling pipeline is connected to the emulsion spray pipeline as a branch of the emulsion spray pipeline, and an emulsion spray valve is arranged on the strip cooling pipeline. The method comprises: Acquiring a rolling speed of the rolling mill; When the rolling speed is less than 500 m / min, the opening of the emulsification spray valve is adjusted according to the rolling speed; wherein the opening of the emulsification spray valve is positively correlated with the rolling speed, and the increasing speed of the opening increases with the increase of the rolling speed; When the rolling speed is greater than or equal to 500 m / min, the opening of the emulsification spray valve is set to 100%.

2. The method according to claim 1, It is characterized in that The adjusting the opening of the emulsification spray valve according to the rolling speed includes: When the rolling mill is in the starting stage with a rolling speed of zero, the initial opening of the emulsification spray valve is set to 5%.

3. The method according to claim 1, It is characterized in that The adjusting the opening of the emulsification spray valve according to the rolling speed includes: When the rolling mill is in the speed-up stage after starting, and the rolling speed is less than or equal to 200 m / min, the opening increment of the emulsification spray valve is set to be the product of the set first opening adjustment coefficient and the rolling speed.

4. The method according to claim 3, It is characterized in that The adjusting the opening of the emulsification spray valve according to the rolling speed includes: When the rolling mill is in the speed-up stage after starting, and the rolling speed is greater than 200 m / min and less than or equal to 500 m / min, the opening increment of the emulsification spray valve is set to the product of a preset second opening adjustment coefficient and the speed increment of the rolling speed relative to 200 m / min; wherein the first opening adjustment coefficient is less than the second opening adjustment coefficient.

5. The method according to claim 1, It is characterized in that The rolling mill is also equipped with an auxiliary cooling pipeline, the auxiliary cooling pipeline is connected to the emulsion spray pipeline as a branch of the emulsion spray pipeline, and a pipeline control valve is arranged on the auxiliary cooling pipeline; after determining that the opening of the emulsion spray valve is 100%, the method further includes: Obtaining the strip temperature of the rolling mill; When the temperature of the steel strip exceeds a preset upper temperature limit, the pipeline control valve is opened.

6. The method according to claim 5, It is characterized in that After obtaining the strip temperature of the rolling mill, the method further comprises: When the temperature of the steel strip exceeds a preset upper temperature limit, the rolling speed is reduced.

7. The method according to claim 5, It is characterized in that The preset upper temperature limit is 130°C.

8. A temperature control device for strip steel, used in rolling mills, It is characterized in that The rolling mill is equipped with an emulsion spray pipeline and a strip cooling pipeline. The strip cooling pipeline is connected to the emulsion spray pipeline as a branch of the emulsion spray pipeline. The strip cooling pipeline is equipped with an emulsion spray valve. The device comprises: An acquisition module, used for acquiring the rolling speed of the rolling mill; An adjustment module, used for adjusting the opening of the emulsification spray valve according to the rolling speed when the rolling speed is less than 500 m / min; wherein the opening of the emulsification spray valve is positively correlated with the rolling speed, and the increasing speed of the opening increases with the increase of the rolling speed; The determination module is used to set the opening of the emulsification spray valve to 100% when the rolling speed is greater than or equal to 500 m / min.

9. A rolling mill, the rolling mill being equipped with an emulsion spray pipeline and a strip cooling pipeline, the strip cooling pipeline being connected to the emulsion spray pipeline as a branch of the emulsion spray pipeline, the strip cooling pipeline being equipped with an emulsion spray valve, the rolling mill, include: An acquisition module, used for acquiring the rolling speed of the rolling mill; An adjustment module, used for adjusting the opening of the emulsification spray valve according to the rolling speed when the rolling speed is less than 500 m / min; wherein the opening of the emulsification spray valve is positively correlated with the rolling speed, and the increasing speed of the opening increases with the increase of the rolling speed; The determination module is used to set the opening of the emulsification spray valve to 100% when the rolling speed is greater than or equal to 500 m / min.

10. A storage medium having a computer program stored thereon, It is characterized in that When the program is executed by a processor, the steps of the method according to any one of claims 1 to 7 are implemented.

Citation Information

Patent Citations

  • Method and system for identifying continuous casting secondary cooling spraying state

    CN115026256A

  • Cold rolling method for strip

    JP1981111505A

  • Controller for rolling mill

    JP1994182420A

  • Method for cooling strip

    JP1994190419A

  • Method for cold rolling steel strip

    JP2002172412A