Palm stretching forming method of stainless steel metal hand mold
By performing the first stretching molding, shear joint setting and second stretching molding during the molding process of stainless steel metal hand molds, the problem of stretching and cracking of the palm is solved, the production efficiency and molding quality are improved, and the production quality is reduced. cost.
Patent Information
- Application Number
- CN202411169429.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-24
- Publication Date
- 2024-11-12
AI Technical Summary
Stainless steel metal hand molds are prone to stretching and cracking during the palm forming process, especially at the joints at the finger joints.
A method of stretching and forming a palm part of a stainless steel metal hand mold is adopted, including first stretching and forming on a metal sheet to a preset depth to obtain the first half palm, and then cutting the fingers of the half palm of the half palm Cut the seams, then perform a second stretching and forming, and finally cut the edges along the palm profile and weld them to form the palm part. This method reduces the tensile force between the finger joints by pre-cutting and setting of shear joints to avoid material pulling and cracking.
It effectively reduces the stretching and cracking situation, ensures that the material at the root of the finger joints does not crack, improves production efficiency, reduces costs, and avoids intermediate annealing processes, simplifies the process, and improves the forming quality of the palm.
Smart Images

Figure CN118926390A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of metal hand mold production, and in particular to a palm stretching forming method of a stainless steel metal hand mold. Background Art
[0002] Since stainless steel products have stable dimensional accuracy, good thermal conductivity, corrosion resistance, and the plates can be made in various thicknesses, these characteristics just meet the production requirements of latex, silicone, PVC, nitrile and other products. That is, large-scale production, low processing cost, high production efficiency, lightness, high rigidity and high thermal conductivity, corrosion resistance, high temperature resistance and oxidation resistance, so stainless steel metal hand molds are gradually used in glove production.
[0003] The stainless steel metal hand mold is divided into a palm portion, a wrist portion and a base portion. The wrist portion is the middle portion connecting the palm portion and the base portion. The wrist portion and the palm portion are connected by welding, and the base portion and the wrist portion are connected by welding.
[0004] With respect to the above-mentioned related technologies, the inventors found that when manufacturing the palm, due to the large deformation at the connection between the fingers and between the fingers and the palm, that is, the finger seams of the palm, it is easy for stretching and cracking to occur in this area during molding. Summary of the invention
[0005] In order to reduce the occurrence of tensile cracking, the present application provides a palm stretching forming method for a stainless steel metal hand mold.
[0006] The palm stretching forming method of a stainless steel metal hand mold provided in the present application adopts the following technical solution: A palm stretching forming method of a stainless steel metal hand mold comprises the following steps: Step S100, performing a first stretching process at a preformed palm portion of the metal sheet to a preset stretching depth to obtain a half palm of the blank, wherein the preset stretching depth of the first stretching process is less than the stretching depth of the preformed palm portion; Step S200, shearing each finger seam of the semi-palm of the blank to form a shear seam; Step S300, performing a second stretching forming on the semi-palm of the initial blank to obtain the semi-palm of the blank; Step S400, trimming the half palm of the blank along the contour of the palm to obtain a left half palm or a right half palm; Step S500: welding the left half palm and the right half palm together to form a palm.
[0007] Preferably, the metal sheet needs to be pre-cut before the first stretch forming, and the two corners of the metal sheet are cut during the pre-cutting process, and the two corners of the metal sheet are on the side of the fingers in the pre-formed palm.
[0008] Preferably, the stretching depth of the preformed palm portion is H, and the preset stretching depth of the first stretching forming is L, wherein the difference between H and L is 3mm-5mm.
[0009] Preferably, the distance between the end of the shear seam and the root of the finger seam is 8mm-15mm.
[0010] Preferably, the first stretching and the second stretching are both performed through a stretching die, and the stretching is performed in the stretching die in the order of forming the two middle finger gaps and the two side finger gaps in sequence.
[0011] Preferably, the stretching forming die comprises an upper die and a lower die cooperating with the upper die; The upper mold comprises an upper mold base, an upper mold pad and an upper mold plate which are arranged in sequence, an upper mold convex mold is arranged on the lower surface of the upper mold plate, and the upper mold convex mold comprises two first finger-heel forming blocks formed by two middle finger gaps and two second finger-heel forming blocks formed by two finger gaps on both sides, the two first finger-heel forming blocks are telescopically installed in the upper mold convex mold, and the lower ends of the two first finger-heel forming blocks protrude from the lower surface of the upper mold plate; The lower mold includes a lower mold base, a lower mold plate and a lower mold pressing plate which are arranged in sequence. The lower mold plate is provided with a lower mold concave mold for cooperating with the upper mold punch. The lower mold pressing plate is arranged around the outside of the lower mold plate. The lower mold pressing plate is used to abut and cooperate with the upper mold plate. The lower mold base is provided with a driving part for driving the lower mold pressing plate to rise and fall.
[0012] Preferably, an installation cavity is provided in the upper mold pad, a mounting block is slidably installed in the installation cavity, one end of two first finger-heel forming blocks passes through the upper mold plate and is connected to the mounting block, and a finger-heel nitrogen spring connected to the mounting block is provided in the installation cavity.
[0013] Preferably, the driving part includes a fixed plate arranged on the lower die base, and a push rod slidably mounted on the fixed plate, the push rod is connected to the lower die pressing plate, and a driving hydraulic cylinder connected to the push rod is arranged on the fixed plate.
[0014] In summary, the present application includes at least one of the following beneficial technical effects: The present application obtains a half-palm blank through the first stretching forming, which not only ensures the initial forming shape of the material, but also ensures that the material in the root area of the finger joints does not crack, and the material thickness in the root area of the finger joints does not become excessively thinner. Therefore, after the setting of the shear seam, the connection between the materials of the fingers is cut off, ensuring that the materials on both sides of each finger are isolated. When the second stretching forming is carried out, the tensile force between the fingers is greatly reduced. At the same time, the radial force becomes smaller when the material is stretched, and the entanglement of the adjacent materials is lost, thereby reducing the occurrence of tensile cracking. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 It is a schematic diagram of the process of stretching and forming the palm of a stainless steel metal hand mold.
[0016] Figure 2 This is a schematic diagram of the structure of metal sheet corner cutting.
[0017] Figure 3 It is a schematic diagram of the structure of the shear seam of the initial half palm.
[0018] Figure 4 It is a structural schematic diagram of a stretch forming die.
[0019] Explanation of the reference numerals: 1. upper mold; 11. upper mold base; 12. upper mold pad; 13. upper mold plate; 14. upper mold punch; 15. first finger-heel forming block; 16. second finger-heel forming block; 17. mounting cavity; 18. mounting block; 19. finger-heel nitrogen spring; 2. lower mold; 21. lower mold base; 22. lower mold plate; 23. lower mold pressing plate; 24. lower mold concave mold; 25. driving unit; 251. fixing plate; 252. ejector pin. DETAILED DESCRIPTION
[0020] The following is combined with Figure 1-4 This application is described in further detail.
[0021] A palm stretching forming method for a stainless steel metal hand mold is used to stretch and form a metal plate into a palm. The metal plate is made of stainless steel. The metal plate is cut into a square sheet shape. The specifications of the square sheet can be set according to actual processing requirements.
[0022] The position of the palm is planned in advance on the metal plate, that is, the position of the preformed palm of the metal plate. It is worth noting that the preformed palm can be the palm of the left hand or the palm of the right hand, and is set according to actual needs. This embodiment does not make any specific limitations.
[0023] The palm has four finger gaps, which are defined as the middle two finger gaps and the two finger gaps on the sides in this embodiment. Based on the material flow during the stretching of the metal sheet, the middle two finger gaps are constrained by the forming of the two finger gaps on the sides during the forming stretching. From the material flow texture, it can be seen that the material flow in the middle two finger gaps is significantly less than that in the two finger gaps on the sides. The forming of the middle two finger gaps is more about the extension of the material itself. Therefore, when the deformation exceeds the extension limit of the material, the occurrence of cracking will be aggravated. When the two finger gaps on the sides are formed, the material will compensate the material from the side to the finger gaps, and the cracking will be alleviated.
[0024] Therefore, in order to reduce the occurrence of tensile cracking, the present application proposes a palm stretching forming method for a stainless steel metal hand mold, referring to Figure 1 As shown, the following steps are included: Step S100, a preformed palm portion of the metal sheet is first stretched to a preset stretching depth to obtain a half palm of the blank, wherein the preset stretching depth of the first stretching is less than the stretching depth of the preformed palm portion.
[0025] According to the technical solution defined in step S100, specifically, the stretching depth of the preformed palm is H, and the preset stretching depth of the first stretching is L, wherein the difference between H and L is 3mm-5mm, and in this embodiment, the preferred difference between H and L is 3mm.
[0026] The initial half palm is an intermediate transition form. The key to the initial half palm lies in its stretching depth. Since the initial half palm does not reach the final stretching depth of the palm, the initial half palm not only ensures the initial forming shape of the material, but also ensures that the material in the root area of the finger joints in the initial half palm will not crack, and the material thickness in the root area of the finger joints will not become transitionally thinner.
[0027] It is worth noting that, referring to Figure 2 As shown, the metal sheet needs to be pre-cut before the first stretch forming. In the pre-cutting process, the two corners of the metal sheet are cut, and the two corners of the metal sheet are on the side of the finger direction of the pre-formed palm. In one embodiment, the cutting angle of the corner is 45°. By cutting the two corners of the metal sheet, the purpose is to reduce the tangential stress of the material extrusion forming in this area when the material is stretched, and prevent the material from wrinkling while reducing the radial tensile stress of the material during stretching.
[0028] Step S200, cutting each finger seam of the semi-palm blank to form a shear seam.
[0029] According to the technical solution defined in step S200, specifically, refer to Figure 3As shown, the shear seam extends from the finger tip to the side of the finger heel, and the distance between the end of the shear seam and the root of the finger seam is 8mm-15mm. Preferably, the distance between the end of the shear seam and the root of the finger seam is 8mm. By setting the shear seam, the connection between the material of the finger and the finger in the semi-palm of the initial blank is cut off, ensuring that the material on both sides of each finger is isolated. During further stretching and forming, the stretching force between the finger seams is greatly reduced. At the same time, when the material is stretched, the radial force becomes smaller, and the adjacent material is lost. The material of the cut part can be easily moved in the stretching direction, which also greatly improves the degree of thinning of the material due to the tension.
[0030] It is worth mentioning that a stress circular hole is opened at the end of the shear seam. The setting of the stress circular hole can further prevent the generation of stress points at the end of the shear seam during stretching, so that cracks occur at the end of the shear seam and extend to the area of the preformed palm, resulting in defective products.
[0031] Step S300, the semi-palm of the initial blank is subjected to a second stretch forming to obtain a semi-palm of the initial blank.
[0032] According to the technical solution defined in step S300, specifically, the second stretching forming of the semi-palm of the initial blank is carried out after step S100 and step S200, and the stretching depth of the second stretching forming is H. The second stretching forming is to further stretch the fingers, finger gaps, palms and wrists to the full depth on the basis of the first stretching forming.
[0033] It is worth noting that the first stretching and the second stretching are both performed through a stretching die, and the stretching is performed in the stretching die in the order of forming the two middle finger gaps and the two finger gaps on both sides.
[0034] The above arrangement is beneficial to the forming of the two middle finger gaps. When the finger gaps are formed, the stretching forming mold first forms the two middle finger gaps, and the two finger gaps on both sides are formed later due to the arrangement. Therefore, the forming order is that the two middle finger gaps are formed first, and the two finger gaps on both sides are formed later. Therefore, the initial resistance of the forming of the two middle finger gaps will be reduced, thereby ensuring that the materials on both sides of the metal sheet fully flow to the two middle finger gaps, thereby reducing the difficulty of forming the two middle finger gaps.
[0035] Specifically, refer to Figure 4 As shown, the stretching forming die includes an upper die 1 and a lower die 2 matched with the upper die 1 .
[0036] The upper mold 1 includes an upper mold base 11, an upper mold pad 12 and an upper mold plate 13 which are arranged in sequence. An upper mold punch 14 is arranged on the lower surface of the upper mold plate 13. The shape of the upper mold punch 14 is the contour shape of the palm for stretching molding. In order to form two middle finger gaps and two finger gaps on both sides, the upper mold punch 14 has two first finger heel molding blocks 15 for molding the two middle finger gaps and two second finger heel molding blocks 16 for molding the two finger gaps on both sides. The two first finger heel molding blocks 15 can be telescopically installed in the upper mold punch 14, and the two second finger heel molding blocks 16 are integrally molded in the upper mold punch 14.
[0037] In order to realize the sequential forming sequence of the two middle finger gaps and the two side finger gaps in this embodiment, the lower ends of the two first finger heel forming blocks 15 protrude from the lower surface of the upper template 13, and the telescopic structure of the two first finger heel forming blocks 15 is described as follows.
[0038] The upper mold pad 12 is provided with a mounting cavity 17, in which a mounting block 18 is slidably mounted, one end of the two first finger-heel forming blocks 15 passes through the upper mold plate 13 and is connected to the mounting block 18, and a finger-heel nitrogen spring 19 connected to the mounting block 18 is provided in the mounting cavity 17. It is worth noting that the spacing between the mounting block 18 and the mounting cavity 17 is the telescopic distance of the first finger-heel forming block 15, and the telescopic distance is the distance that the first finger-heel forming block 15 protrudes from the lower surface of the upper mold plate 13.
[0039] The lower mold 2 includes a lower mold base 21, a lower mold plate 22 and a lower mold pressing plate 23 which are arranged in sequence. The lower mold plate 22 is provided with a lower mold concave mold 24 for cooperating with the upper mold convex mold 14. The lower mold concave mold 24 cooperates with the upper mold convex mold 14 to stretch and form the palm portion. The lower mold pressing plate 23 is arranged around the lower mold plate 22. The upper surface of the lower mold pressing plate 23 is higher than the upper surface of the lower mold plate 22. The lower mold pressing plate 23 is used to abut and cooperate with the upper mold plate 13. The lower mold base 21 is provided with a driving part 25 for driving the lower mold pressing plate 23 to rise and fall.
[0040] The driving part 25 includes a fixed plate 251 disposed on the lower die base 21 and a push rod 252 slidably mounted on the fixed plate 251 . The push rod 252 is connected to the lower die pressing plate 23 . A driving hydraulic cylinder connected to the push rod 252 is disposed on the fixed plate 251 .
[0041] The first stretching and second stretching operations of the stretching die will be described below.
[0042] In the first stretching process, the metal sheet is placed on the lower die pressing plate 23, and the upper die 1 is closed toward the lower die 2 under the action of the hydraulic press. At this time, the first finger and heel forming block 15 contacts the metal sheet before the second finger and heel forming block 16, so that the first finger and heel forming block 15 first forms the middle two finger gaps of the palm. With the continuous mold closing action, the upper mold plate 13 is pressed against the lower mold pressing plate 23, the first finger heel forming block 15 is pressurized so that the finger heel nitrogen spring 19 is compressed, and the lower end of the first finger heel forming block 15 is flush with the lower end of the second finger heel forming block 16; with the further mold closing action of the upper mold 1 and the lower mold 2, the second finger heel forming block 16 will form the two finger gaps on both sides of the palm, and the first stretching forming of the upper mold 1 and the lower mold 2 stops after the stretching depth reaches the preset stretching depth L. At this time, the metal sheet is formed into the shape of a semi-palm of the initial blank after the first stretching.
[0043] Subsequently, after each finger seam of the initial half palm is sheared to form a shear seam, the initial half palm is placed on the lower mold pressing plate 23 for a second stretching forming operation. In the second stretching forming, the stretching depth of the upper mold 1 is set to the full stretching depth. At this time, the initial half palm will form a blank half palm, and the blank half palm has the shape of a complete palm.
[0044] Step S400, trimming the half palm of the blank along the contour of the palm to obtain a left half palm or a right half palm.
[0045] According to the technical solution defined in step S400, specifically, trimming the half-palm of the blank along the contour of the palm mainly involves cutting off excess edge material on the half-palm of the blank, so that only the left half-palm and the right half-palm that meet the design size specifications are left on the half-palm of the blank.
[0046] Step S500: welding the left half palm and the right half palm together to form a palm.
[0047] According to the technical solution defined in step S500, specifically, after the left half palm and the right half palm are butt-jointed, the left half palm and the right half palm are butt-jointed and placed into a welding mold, the left half palm and the right half palm are buckled and positioned through the welding mold, and then spot-welded and fixed, and then fully welded and fixed.
[0048] This completes the production from the metal sheet to the palm.
[0049] In summary, the present application has the following beneficial effects by adopting the palm stretching forming method of the above-mentioned stainless steel metal hand mold: 1. Solving the problem of cracking of the fingers during the stretching forming process; 2. The annealing process in the intermediate process is no longer required during the stretching forming process, so as to effectively improve the production efficiency; 3. Solving the problem of transitional thinning of the roots of the fingers during the stretching forming process; 4. Solving the problem of too long stretching process and too long cycle; 5. Reducing costs; 6. Reducing labor and reducing costs through automated line operations.
[0050] The above are all preferred embodiments of the present application, and the protection scope of the present application is not limited thereto. Therefore, any equivalent changes made according to the structure, shape, and principle of the present application should be included in the protection scope of the present application.
Claims
1. A palm stretching forming method for a stainless steel metal hand mold, characterized in that: The steps include: Step S100, performing a first stretching process at a preformed palm portion of the metal sheet to a preset stretching depth to obtain a half palm of the blank, wherein the preset stretching depth of the first stretching process is less than the stretching depth of the preformed palm portion; Step S200, shearing each finger seam of the semi-palm of the blank to form a shear seam; Step S300, performing a second stretching forming on the semi-palm of the initial blank to obtain the semi-palm of the blank; Step S400, trimming the half palm of the blank along the contour of the palm to obtain a left half palm or a right half palm; Step S500: welding the left half palm and the right half palm together to form a palm.
2. The palm stretching forming method of a stainless steel metal hand mold according to claim 1, characterized in that: Before the metal sheet is subjected to the first stretching forming, it is necessary to perform a pre-cutting process on the metal sheet. In the pre-cutting process, two corners of the metal sheet are cut. The two corners of the metal sheet are on the side of the fingers in the pre-formed palm.
3. The palm stretching forming method of a stainless steel metal hand mold according to claim 1, characterized in that: The stretching depth of the preformed palm portion is H, and the preset stretching depth of the first stretching forming is L, wherein the difference between H and L is 3mm-5mm.
4. The palm stretching forming method of a stainless steel metal hand mold according to claim 1, characterized in that: The distance between the end of the shearing seam and the root of the finger seam is 8mm-15mm.
5. The palm stretching forming method of a stainless steel metal hand mold according to claim 1, characterized in that: The first stretching and the second stretching are both stretched through a stretching die, and the stretching is performed in the stretching die in the order of forming the two middle finger gaps and the two finger gaps on both sides.
6. The palm stretching forming method of a stainless steel metal hand mold according to claim 5, characterized in that: The stretching forming die comprises an upper die (1) and a lower die (2) matched with the upper die (1); The upper mold (1) comprises an upper mold base (11), an upper mold pad (12) and an upper mold plate (13) which are arranged in sequence. An upper mold punch (14) is arranged on the lower surface of the upper mold plate (13). The upper mold punch (14) comprises two first finger-heel forming blocks (15) for forming two finger gaps in the middle and two second finger-heel forming blocks (16) for forming two finger gaps on both sides. The two first finger-heel forming blocks (15) are telescopically installed in the upper mold punch (14). The lower ends of the two first finger-heel forming blocks (15) protrude from the upper mold plate (13). 13); the lower mold (2) comprises a lower mold base (21), a lower mold plate (22) and a lower mold pressing plate (23) which are arranged in sequence; the lower mold plate (22) is provided with a lower mold concave mold (24) for cooperating with the upper mold convex mold (14); the lower mold pressing plate (23) is arranged around the outside of the lower mold plate (22); the lower mold pressing plate (23) is used to abut and cooperate with the upper mold plate (13); the lower mold base (21) is provided with a driving part (25) for driving the lower mold pressing plate (23) to rise and fall.
7. The palm stretching forming method of a stainless steel metal hand mold according to claim 6, characterized in that: An installation cavity (17) is provided in the upper mold pad (12), a installation block (18) is slidably installed in the installation cavity (17), one end of two first finger-heel forming blocks (15) passes through the upper mold plate (13) and is connected to the installation block (18), and a finger-heel nitrogen spring (19) connected to the installation block (18) is provided in the installation cavity (17).
8. The palm stretching forming method of a stainless steel metal hand mold according to claim 6, characterized in that: The driving part (25) comprises a fixed plate (251) arranged on the lower die base (21), and a push rod (252) slidably mounted on the fixed plate (251), the push rod (252) being connected to the lower die pressing plate (23), and a driving hydraulic cylinder connected to the push rod (252) being arranged on the fixed plate (251).
Citation Information
Patent Citations
Forming process of glove mold
CN116493889A
Edge cutting device for glove mold
CN215998270U
Manufacturing method for pressed component, pressed component, and manufacturing method for blank material