Container product manufacturing method
Through mold design and gas pressure control, micro foaming and honeycomb foaming areas are formed, which solves the problem of poor insulation of plastic cups, achieves better thermal insulation effect and appearance texture, and simplifies the manufacturing process.
Patent Information
- Application Number
- CN202310527869.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-11
- Publication Date
- 2024-11-12
AI Technical Summary
The existing plastic cup has poor thermal insulation, and the manufacturing method of forming foamed and unfoamed parts through local temperature control is complicated and difficult to control.
Using a mold design, including the first and second components, a molten plastic composition of polymer and foaming agent is injected, and a gas pressure is controlled during cooling to form micro-foaming in the first zone and a honeycomb-like hair. bubbles, combined with mold displacement to control container thickness and shape.
It reduces manufacturing complexity, improves the insulation effect and appearance texture of the container, and ensures the quality, yield and consistency of the product.
Smart Images

Figure CN118927504A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a method for manufacturing a container product, and mainly refers to a method for manufacturing a cup-shaped container product formed by melting a polymer and a foaming agent. Background Art
[0002] Currently, injection-molded plastic cups are often used as disposable cups. In order to reduce costs, the plastic cups only need to be thick enough to hold beverages. However, the thinner plastic cups have poor heat insulation. When hot beverages are placed in the cups, the temperature is transferred to the outside of the cups, causing discomfort to the hands.
[0003] In order to improve the disadvantage of poor thermal insulation of the plastic cup, the current plastic cup can be made by molding a molten plastic composition composed of a polymer and a foaming agent, and after molding, a plastic cup with thicker foam can be formed, which can provide better thermal insulation effect than a plastic cup without foam.
[0004] However, when the entire plastic cup is thickly foamed, the appearance will have a disadvantage of less varied texture. For example, in the plastic cup of US11446849, a local position of the mold is cooled by temperature control so that the cooled position does not foam, and other uncooled positions can foam to form a plastic cup with both foamed and unfoamed parts. However, this local cooling method will increase the manufacturing complexity and the disadvantage of being difficult to control. Summary of the invention
[0005] The object of the present invention is to provide a method for manufacturing a container product which reduces manufacturing complexity and enables the product to have better thermal insulation effect and appearance texture, comprising the following steps: S1: A mold is provided, wherein the mold includes a first component and a second component, wherein the first component has a first surface, the second component has a second surface, and the second component has a blowing port.
[0006] S2: The mold is closed, and a cavity is defined between the first surface and the second surface, the cavity has a conical annular cavity portion, the annular cavity portion has a first end corresponding to the axial direction, a second end corresponding to the axial direction with a smaller diameter than the first end, the second end has a bottom cavity portion corresponding to the axial direction vertical, and the cavity has two first areas and one second area, the distance between the first surface corresponding to the two first areas and the second surface is smaller than the distance between the first surface corresponding to the second area and the second surface; and the two ends of the second area corresponding to the axial direction are respectively connected to the two first areas; S3: injecting a molten plastic composition comprising a polymer and a physical foaming agent into the cavity under injection pressure.
[0007] S4: The molten plastic composition in the cavity is cooled so that the molten plastic composition in the first zone is completely cooled and solidified or only a small amount of uncooled plastic composition in the center is formed; after cooling, the molten plastic composition in the second zone forms a first solid skin layer and a second solid skin layer respectively contacting the first surface and the second surface, and the molten plastic composition in the cavity is exposed to a pressure greater than the gas pressure that maintains the physical foaming agent dissolved in the polymer, so that the molten plastic compositions in the first zone and the second zone do not foam.
[0008] S5: The blowing port blows air to make the plastic composition adhere to the first surface of the first component, and the blowing is stopped after the adhesion, and the first component of the mold is axially displaced, and the molten plastic composition in the cavity is exposed to a gas pressure less than that maintaining the physical foaming agent dissolved in the polymer, so that the distance between the first surface and the second surface of the mold corresponding to the second zone position is correspondingly increased, and the first solid skin layer is still in contact with the first surface at this time, and the central molten plastic composition of the second zone is expanded through foaming to form a honeycomb foam body, and the second solid skin layer is in contact with the second surface; the plastic composition of the first zone is in contact with the first surface, and the first zone has been solidified or can only form micro-bubbles, so the shape and thickness of the first zone remain unchanged or the thickness is only slightly increased, and the first zone restricts the second zone to expand only toward the first surface.
[0009] S6: Cooling step, cooling the foamed container product in the mold to fix the shape.
[0010] S7: a mold opening step, wherein the first component and the second component of the mold are separated and the container product is taken out.
[0011] In one embodiment of the present invention, the two first areas are the bottom cavity part and the front end of the annular cavity part from the first end toward the second end; and the second area is the position in the annular cavity part from the first area to the bottom cavity part.
[0012] In one embodiment of the present invention, the blowing direction of the blowing port corresponds to the bottom cavity portion.
[0013] In one embodiment of the present invention, the blowing port has a permeable block at a position corresponding to the second surface, and the permeable block prevents the molten plastic composition from flowing into the blowing port.
[0014] In one embodiment of the present invention the polymer is polypropylene.
[0015] In one embodiment of the present invention, the physical blowing agent is nitrogen.
[0016] In one embodiment of the present invention, the first zone and the second zone in the step S4 have the same cooling temperature.
[0017] In one embodiment of the present invention, in the step S6, the first zone and the second zone have the same cooling temperature or are naturally cooled under normal temperature.
[0018] The manufacturing method of the present invention does not require complex temperature control, and can control the thickness of the container in accordance with the displacement distance of the first component of the mold, so that the product has better quality, yield and consistency. The container manufactured by the present invention has a ring wall, a bottom wall below the ring wall, and an opening above the ring wall. The ring wall is a tapered surface with a gradually decreasing diameter from the upper opening to the lower bottom wall. The top of the ring wall and the bottom wall are micro-foaming areas corresponding to the first area of the mold. The area between the micro-foaming area corresponding to the top of the ring wall and the bottom wall is a foaming area corresponding to the second area of the mold. The thickness of the foaming area is greater than the thickness of the micro-foaming area, which improves the appearance and texture of the container product, and the thicker foaming area has a better heat insulation effect.
[0019] The present invention will be more clearly understood by describing illustrative embodiments of the present invention with reference to the drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 It is a cross-sectional schematic diagram of the mold closing and injection of molten plastic composition of the present invention.
[0021] Figure 2 It is a schematic cross-sectional view of the axial displacement of the first component of the mold of the present invention.
[0022] Figure 3 It is a schematic diagram of the first zone micro-foaming and the second zone foaming of the present invention.
[0023] Figure 4 It is a schematic diagram of a container product of the present invention.
[0024] Description of Figure Numbers: 1 mold 11 first component 111 first surface 12 second component 121 second surface 122 blowing port 123 air permeable block 13 cavity 14 annular cavity part 141 first end 142 second end 15 bottom cavity portion 16 District 1 17 District 2 2 plastic composition 21 gas 22 first solid skin layer 23 second solid skin layer 24 foam 3 container 31 ring wall 32 bottom wall 33 opening 34 micro-foaming area 35 foaming area. DETAILED DESCRIPTION
[0025] See also Figures 1 to 3 The container product manufacturing method of the present invention comprises the following steps: S1: A mold 1 is set, and the mold 1 includes a first component 11 and a second component 12. The first component 11 has a first surface 111, and the second component 12 has a second surface 121. The second component 12 has a blowing port 122, and the blowing port 122 has a breathable block 123 at a position corresponding to the second surface 121.
[0026] S2: The mold 1 is closed, and a cavity 13 is defined between the first surface 111 and the second surface 121. The cavity 13 has a conical annular cavity portion 14, wherein the Figure 1 , Figure 2 Only a partial cross-section of the mold 1 is shown. The annular cavity portion 14 has a first end 141 corresponding to the axial direction, a second end 142 corresponding to the axial diameter smaller than the first end 141, and the second end 142 has a bottom cavity portion 15 corresponding to the axial direction and vertical, and the blowing direction of the blowing port 122 corresponds to the bottom cavity portion 15. The cavity 13 has two first areas 16 and a second area 17, and the second area 17 is connected to the two first areas 16 at the corresponding axial ends. The bottom cavity portion 15 of this embodiment and the front end of the annular cavity portion 14 from the first end 141 to the second end 142 form the first area 16, and the second area 17 is formed between the first area 16 and the bottom cavity portion 15 in the annular cavity portion 14. The distance D1 between the first surface 111 and the second surface 121 corresponding to the first area 16 is smaller than the distance D2 between the first surface 111 and the second surface 121 corresponding to the second area 17. In this embodiment, D1 can be about 0.5 mm, and D2 can be about 1 mm.
[0027] S3: Inject a molten plastic composition 2 containing a polymer and a physical foaming agent into the cavity 13 under injection pressure, wherein the physical foaming agent is a gas 21 dissolved in the polymer, wherein the polymer may be polypropylene, and the physical foaming agent may be nitrogen, and the air permeable block 123 may prevent the molten plastic composition 2 from flowing into the blowing port 122.
[0028] S4: The molten plastic composition 2 in the cavity 13 of the mold 1 is cooled so that the molten plastic composition 2 in the first zone 16 can be completely cooled and solidified or only a small amount of the molten plastic composition 2 in the center is not cooled. Figure 2 , Figure 3 As shown, after cooling, the molten plastic composition 2 in the second zone 17 forms a first solid skin layer 22 and a second solid skin layer 23 respectively contacting the first surface 111 and the second surface 121, and there is a molten plastic composition 2 between the first solid skin layer 22 and the second solid skin layer 23.
[0029] The molten plastic composition 2 in the cavity 13 is exposed to a pressure of the gas 21 greater than the pressure that maintains the physical foaming agent dissolved in the polymer, so that the molten plastic composition 2 in the first zone 16 and the second zone 17 does not foam.
[0030] In step S4, the first zone 16 and the second zone 17 are cooled at the same cooling temperature, and the thickness D1 of the first zone 16 is smaller, so that the molten plastic composition 2 in the first zone 16 can be solidified or almost completely solidified by the cooling temperature with only a small amount of incomplete cooling in the center.
[0031] S5: The blowing port 122 blows air to make the plastic composition 2 adhere to the first surface 111 of the first component 11, and the blowing is stopped after the adhesion. The first component 11 of the mold 1 is axially displaced, and the molten plastic composition 2 in the cavity 13 is exposed to a pressure less than the gas 21 that maintains the physical foaming agent dissolved in the polymer, so that at this time, the distance D3 between the first surface 111 and the second surface 121 of the mold 1 corresponding to the position of the second zone 17 increases accordingly. At this time, the first solid skin layer 22 is still in contact with the first surface 111, and the central molten plastic composition 2 of the second zone 17 is expanded and foamed to form a honeycomb foam body 24, so that the second solid skin layer 23 can contact the second surface 121, and the displacement distance of the first component 11 can limit the shape and thickness of the plastic composition 2 in the second zone 17. In this embodiment, the thickness of the foamed plastic composition 2 in the second zone 17 is equal to the distance D3 between the first surface 211 and the second surface 221 of the mold 2 corresponding to the position of the second zone 27 at this time, and D3 can be approximately 2.3 mm.
[0032] The molten plastic composition 2 in the first zone 16 is solidified or only has a small amount of uncooled in the center, so it can only form micro-bubbles. The plastic composition 2 in the first zone 16 maintains contact with the first surface 111, but the plastic composition 2 in the first zone 16 cannot expand and contact with the second surface 121. Therefore, the shape and thickness of the plastic composition 2 in the first zone 16 are basically unchanged or the thickness is only slightly increased. In addition, because the plastic composition 2 in the first zone 16 is basically fixed before the first component 11 is displaced, the molten plastic composition 2 in the second zone 17 can only be expanded toward the second surface 121, and will not expand axially toward the mold 1, which can improve the shape stability of the container product.
[0033] S6: Cooling step, cooling the foamed container product in the mold 1 to shape it, wherein the cooling method is to cool the first area 16 and the second area 17 at the same cooling temperature or to cool them naturally at room temperature.
[0034] S7: a mold opening step, in which the first component 11 and the second component 12 of the mold 1 are separated and the container product is taken out.
[0035] Please also read Figures 1 to 4 The container 3 manufactured by the manufacturing method of the present invention has an annular wall 31, a bottom wall 32 is provided below the annular wall 31, and an opening 33 is provided above the annular wall 31. The annular wall 31 is a tapered surface with a gradually decreasing diameter from the upper opening 33 to the lower bottom wall 32. The top of the annular wall 31 and the bottom wall 32 are micro-foaming areas 34 corresponding to the first area 16 of the mold 1. The area between the micro-foaming area 34 at the top of the annular wall 31 and the bottom wall 32 is a foaming area 35 corresponding to the second area 17 of the mold 1. The thickness of the foaming area 35 is greater than that of the micro-foaming area 34, which can improve the appearance and texture of the container 3. The thicker foaming area 35 can make the container 3 have a better heat insulation effect.
[0036] In the present invention, the displacement distance of the first component 11 of the mold 1 can control the foaming thickness of the foaming area 35 of the container 3, which can easily control the shape and thickness of the container 3. In addition, the present invention does not need to perform different temperature controls in different areas, which can reduce manufacturing complexity and enable the product to have better quality, yield and consistency. In addition, the container 3 has foaming areas 35 and micro-foaming areas 34 at different positions, which can have a better product texture.
[0037] The above embodiments are illustrative of the present invention, not limiting of the present invention. Any equivalent changes made according to the spirit of the present invention should also fall within the scope of the present invention.
Claims
1. A method for manufacturing a container product, characterized in that: The following steps are involved: S1: a mold is provided, the mold comprising a first component and a second component, the first component has a first surface, the second component has a second surface, and the second component has a blowing port; S2: The mold is closed, and a cavity is defined between the first surface and the second surface, the cavity has a conical annular cavity portion, the annular cavity portion has a first end corresponding to the axial direction, a second end corresponding to the axial direction with a smaller diameter than the first end, the second end has a bottom cavity portion corresponding to the axial direction vertical, and the cavity has two first areas and one second area, the distance between the first surface corresponding to the two first areas and the second surface is smaller than the distance between the first surface corresponding to the second area and the second surface; and the two ends of the second area corresponding to the axial direction are respectively connected to the two first areas; S3: injecting a molten plastic composition comprising a polymer and a physical foaming agent into the cavity under injection pressure; S4: The molten plastic composition in the cavity is cooled so that the molten plastic composition in the first zone is completely cooled and solidified or only a small amount of the molten plastic composition in the center is not cooled; after cooling, the molten plastic composition in the second zone forms a first solid skin layer and a second solid skin layer respectively contacting the first surface and the second surface, and there is a molten plastic composition between the first solid skin layer and the second solid skin layer. The molten plastic composition in the cavity is exposed to a pressure greater than the gas pressure that maintains the physical foaming agent dissolved in the polymer, so that the molten plastic compositions in the first zone and the second zone do not foam; S5: The blowing port blows air to make the plastic composition adhere to the first surface of the first component, and the blowing stops after the adhesion, and the first component of the mold is axially displaced, and the molten plastic composition in the cavity is exposed to a gas pressure less than the gas pressure that maintains the physical foaming agent dissolved in the polymer, so that the distance between the first surface and the second surface of the mold corresponding to the second zone position increases accordingly, and the first solid skin layer still contacts the first surface at this time, and the central molten plastic composition of the second zone is expanded by foaming to form a honeycomb foam body, and the second solid skin layer contacts the second surface; the plastic composition of the first zone contacts the first surface, and the first zone has been solidified or can only form micro-foams, so the shape and thickness of the first zone remain unchanged or the thickness only increases slightly, and the first zone restricts the second zone to expand only toward the second surface; S6: cooling step, cooling the foamed container product in the mold to shape it; S7: a mold opening step, wherein the first component and the second component of the mold are separated and the container product is taken out.
2. The method for manufacturing a container product according to claim 1, characterized in that: The two first areas are the bottom cavity part and the front end of the annular cavity part from the first end toward the second end; and the second area is the position in the annular cavity part from the first area to the bottom cavity part.
3. The method for manufacturing a container product according to claim 1, characterized in that: The blowing direction of the blowing port corresponds to the bottom cavity part.
4. The method for manufacturing a container product according to claim 1, characterized in that: The blowing port has an air permeable block at a position corresponding to the second surface.
5. The method for manufacturing a container product according to claim 1, characterized in that: The polymer is polypropylene.
6. The method for manufacturing a container product according to claim 1, characterized in that: The physical blowing agent is nitrogen.
7. The method for manufacturing a container product according to claim 1, characterized in that: In the step S4, the first zone and the second zone have the same cooling temperature.
8. The method for manufacturing a container product according to claim 1, characterized in that: In the step S6, the first zone and the second zone have the same cooling temperature or are naturally cooled under normal temperature.