Efficient fracturing cleanup additive and preparation method thereof
By combining ester polymers with fatty alcohol polyoxyethylene ethers, a high-efficiency fracturing discharge aid was prepared, which solved the problem of a wide variety of additives in the prior art, and achieved the dual functions of clay stability and discharge aid, simplifying The work content during oil and gas mining is carried out and excellent performance is shown through detection.
Patent Information
- Application Number
- CN202410999333.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-24
- Publication Date
- 2024-11-12
AI Technical Summary
The existing discharge aids are difficult to play the dual role of clay stabilizer and discharge aids in the oil and gas mining process, resulting in a wide variety of additives and complex work content of staff during the oil and gas mining process.
Using the combination of ester polymers and fatty alcohol polyoxyethylene ethers to prepare a high-efficiency fracturing agent, which can be used as clay stabilizers and as fracturing agents, and can be used as fracturing agents to form ester polymerization through esterification reactions. The mixture of the substance with isopropanol and water forms an efficient fracturing discharge aid.
This high-efficiency fracturing discharge aid can reduce the types of additives in oil and gas mining, streamline the workload of staff, and show good expansion volume, water washing resistance and surface tension performance through performance detection.
Smart Images

Figure BDA0004961123190000034 
Figure BDA0004961123190000042
Abstract
Description
Technical Field
[0001] The invention relates to the field of oil and gas exploitation, and in particular to a high-efficiency fracturing drainage agent and a preparation method thereof. Background Art
[0002] A drainage aid is a chemical that can help the residual fluid in the acidification and fracturing process to return from the formation. Adding a drainage aid to the fracturing fluid can increase the return rate of the fracturing fluid, avoid blockage, and increase oil and gas production. At present, there are many types of drainage aids on the market, such as: oil field acidification fracturing drainage aid disclosed in Chinese patent CN114957108A, an oil and gas field fracturing drainage aid composition disclosed in Chinese patent CN106167697A, a fracturing drainage aid and its preparation method, and an acidification fracturing drainage aid disclosed in Chinese patent CN118272066A. The improvement ideas of these drainage aids are usually to reduce surface tension or increase wettability, while the role of clay stabilizers is to adsorb on the clay surface to prevent water-sensitive minerals from hydrating, expanding, and dispersing and migrating, thereby causing damage to the oil and gas layer. Therefore, developing a product that can act as both a clay stabilizer and a drainage aid can reduce the types of additives in the oil and gas production process and streamline the work content of the staff. Summary of the invention
[0003] The purpose of the present invention is to provide a high-efficiency fracturing drainage agent and a preparation method thereof in view of the deficiencies in the prior art.
[0004] In order to achieve the above object, the technical solution adopted by the present invention is:
[0005] A high-efficiency fracturing drainage agent comprises the following raw materials in parts by weight: 5-15 parts of ester polymer, 1-5 parts of fatty alcohol polyoxyethylene ether, 1-5 parts of isopropanol, and 80-90 parts of water; wherein the ester polymer is prepared from ditrimethyl hydroxypropyl quaternary ammonium salt and carboxylic acid monomer.
[0006] The structural formula of the carboxylic acid monomer is R-COOH, wherein R- is a straight-chain alkyl group, a branched alkyl group, an aromatic group, a halogenated alkyl group or a halogenated aromatic group.
[0007] The preparation steps of the ester polymer include placing ditrimethylhydroxypropyl quaternary ammonium salt, carboxylic acid monomer, catalyst and solvent in a reaction container, fully stirring at 120-140° C., reacting for 5-15 hours, discharging water generated by the esterification reaction in time, filtering and removing the solvent after the reaction is completed to obtain the ester polymer.
[0008] The solvents are trifluoroacetic acid, chloroform, phenol, tetrachloroethane, o-chlorophenol, benzene, chlorobenzene, chloroform, ethyl acetate, ethanol, acetone, and ether.
[0009] The molar ratio of the bistrimethylhydroxypropyl quaternary ammonium salt to the carboxylic acid monomer is 1:(1-3), and the mass ratio of the sum of the mass of the bistrimethylhydroxypropyl quaternary ammonium salt, the carboxylic acid monomer and the catalyst to the solvent is 1:(3-8).
[0010] A method for preparing the highly efficient fracturing drainage agent comprises the following steps:
[0011] Add isopropanol into water, mix well, then add ester polymer and fatty alcohol polyoxyethylene ether, mix well to obtain the product.
[0012] The present invention has outstanding substantial features and significant progress compared to the prior art. Specifically, the present invention provides a high-efficiency fracturing drainage agent and a preparation method thereof. The high-efficiency fracturing drainage agent adopts ester polymers and fatty alcohol polyoxyethylene ether to cooperate with each other, and can be used as a clay stabilizer and a fracturing drainage agent. It can reduce the types of additives in the oil and gas production process and streamline the workload of the staff. DETAILED DESCRIPTION
[0013] The technical solution of the present invention is further described in detail below through specific implementation methods.
[0014] A high-efficiency fracturing drainage agent comprises the following raw materials in parts by weight: 5-15 parts of ester polymer, 1-5 parts of fatty alcohol polyoxyethylene ether, 1-5 parts of isopropanol, and 80-90 parts of water; wherein the ester polymer is prepared from ditrimethyl hydroxypropyl quaternary ammonium salt and carboxylic acid monomer.
[0015] The structural formula of the carboxylic acid monomer is R-COOH, wherein R- is a straight-chain alkyl group, a branched alkyl group, an aromatic group, a halogenated alkyl group or a halogenated aromatic group.
[0016] The preparation steps of the ester polymer include placing ditrimethylhydroxypropyl quaternary ammonium salt, carboxylic acid monomer, catalyst (copper sulfate) and solvent in a reaction container, stirring fully at 120-140° C., reacting for 5-15 hours, discharging water generated by the esterification reaction in time, filtering and removing the solvent after the reaction is completed, and obtaining the ester polymer. The catalyst is a titanium catalyst, a zinc catalyst or a copper catalyst
[0017] The solvents are trifluoroacetic acid, chloroform, phenol, tetrachloroethane, o-chlorophenol, benzene, chlorobenzene, chloroform, ethyl acetate, ethanol, acetone, and ether.
[0018] The molar ratio of the bistrimethylhydroxypropyl quaternary ammonium salt to the carboxylic acid monomer is 1:(1-3), and the mass ratio of the sum of the mass of the bistrimethylhydroxypropyl quaternary ammonium salt, the carboxylic acid monomer and the catalyst to the solvent is 1:(3-8).
[0019] A method for preparing the highly efficient fracturing drainage agent comprises the following steps:
[0020] Add isopropanol into water, mix well, then add ester polymer and fatty alcohol polyoxyethylene ether, mix well to obtain the product.
[0021] Example 1
[0022] This embodiment provides a high-efficiency fracturing drainage agent, which includes the following raw materials in parts by weight: 15 parts of ester polymer, 2 parts of fatty alcohol polyoxyethylene ether, 2 parts of isopropanol, and 90 parts of water; wherein the ester polymer is prepared from ditrimethylhydroxypropyl quaternary ammonium salt and carboxylic acid monomer.
[0023] The structural formula of bistrimethylhydroxypropyl quaternary ammonium salt is: Wherein, R is CH3; the structural formula of the carboxylic acid monomer is
[0024] The preparation steps of the ester polymer include placing a ditrimethyl hydroxypropyl quaternary ammonium salt, a carboxylic acid monomer, a catalyst (copper sulfate) and a chlorobenzene solvent in a reaction container, fully stirring at 130° C., reacting for 5 hours, and discharging water generated by the esterification reaction in time. After the reaction is completed, filtering and removing the solvent to obtain an ester polymer. The molar ratio of the ditrimethyl hydroxypropyl quaternary ammonium salt to the carboxylic acid monomer is 1:2, and the mass ratio of the sum of the mass of the ditrimethyl hydroxypropyl quaternary ammonium salt, the carboxylic acid monomer, and the catalyst to the solvent is 1:5; the amount of the catalyst is 1% of the sum of the mass of the ditrimethyl hydroxypropyl quaternary ammonium salt and the carboxylic acid monomer; and the solvent is chlorobenzene.
[0025] A method for preparing the highly efficient fracturing drainage agent comprises the following steps:
[0026] Add isopropanol into water, mix well, then add ester polymer and fatty alcohol polyoxyethylene ether, mix well to obtain the product.
[0027] Example 2
[0028] This embodiment provides a high-efficiency fracturing drainage agent, which includes the following raw materials in parts by weight: 15 parts of ester polymer, 2 parts of fatty alcohol polyoxyethylene ether, 3 parts of isopropanol, and 90 parts of water; wherein the ester polymer is prepared from ditrimethyl hydroxypropyl quaternary ammonium salt and carboxylic acid monomer.
[0029] The structural formula of bistrimethylhydroxypropyl quaternary ammonium salt is:
[0030] Wherein, R is CH3.
[0031] The structural formula of the carboxylic acid monomer is:
[0032]
[0033] The preparation steps of the ester polymer include placing ditrimethyl hydroxypropyl quaternary ammonium salt, carboxylic acid monomer, catalyst (copper sulfate) and chlorobenzene solvent in a reaction container, stirring fully at 120°C, reacting for 6 hours, discharging water generated by the esterification reaction in time, and purifying after the reaction is completed to obtain a clay stabilizer. The molar ratio of ditrimethyl hydroxypropyl quaternary ammonium salt to carboxylic acid monomer is 1:2, the mass ratio of the sum of the mass of ditrimethyl hydroxypropyl quaternary ammonium salt, carboxylic acid monomer and catalyst to the solvent is 1:5; the amount of the catalyst is 1% of the sum of the mass of ditrimethyl hydroxypropyl quaternary ammonium salt and carboxylic acid monomer; and the solvent is chlorobenzene.
[0034] A method for preparing the highly efficient fracturing drainage agent comprises the following steps:
[0035] Add isopropanol into water, mix well, then add ester polymer and fatty alcohol polyoxyethylene ether, mix well to obtain the product.
[0036] Example 3
[0037] This embodiment provides a high-efficiency fracturing drainage agent, which includes the following raw materials in parts by weight: 15 parts of ester polymer, 4 parts of fatty alcohol polyoxyethylene ether, 1 part of isopropanol, and 90 parts of water; wherein the ester polymer is prepared from ditrimethyl hydroxypropyl quaternary ammonium salt and carboxylic acid monomer.
[0038] The structural formula of bistrimethylhydroxypropyl quaternary ammonium salt is:
[0039] Wherein, R is CH3.
[0040] The structural formula of the carboxylic acid monomer is:
[0041]
[0042] The preparation steps of the ester polymer include placing a bistrimethylhydroxypropyl quaternary ammonium salt, a carboxylic acid monomer, a catalyst (copper sulfate) and a chlorobenzene solvent in a reaction container, fully stirring at 130° C., reacting for 5 hours, discharging water generated by the esterification reaction in time, filtering and removing the solvent after the reaction is completed, and obtaining an ester polymer. The molar ratio of the bistrimethylhydroxypropyl quaternary ammonium salt to the carboxylic acid monomer is 1:2.5, the mass ratio of the sum of the mass of the bistrimethylhydroxypropyl quaternary ammonium salt, the carboxylic acid monomer, and the catalyst to the solvent is 1:6; the amount of the catalyst is 1% of the sum of the mass of the bistrimethylhydroxypropyl quaternary ammonium salt and the carboxylic acid monomer; and the solvent is chlorobenzene.
[0043] A method for preparing the highly efficient fracturing drainage agent comprises the following steps:
[0044] Add isopropanol into water, mix well, then add ester polymer and fatty alcohol polyoxyethylene ether, mix well to obtain the product.
[0045] The performance test was carried out in accordance with the technical requirements of QSH4006 CG0001-2020 foaming aid for fracturing and acidizing and Q / SH125-2017 clay stabilizer technology. The test results are shown in Table 1.
[0046] Table 1 Test results of Examples 1-3
[0047] Expansion volume / ml Washability / ml Surface tension / mN / m Interfacial tension / mN / m Example 1 2.33 0.33 25.1 2.58 Example 2 2.45 0.20 24.3 2.39 Example 3 2.25 0.32 25.5 2.67
[0048] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, ordinary technicians in the field should understand that the specific implementation methods of the present invention can still be modified or some technical features can be replaced by equivalents without departing from the spirit of the technical solution of the present invention, which should be included in the scope of the technical solution for protection of the present invention.
Claims
1. A high-efficiency fracturing drainage agent, comprising the following raw materials in parts by weight: 5-15 parts of ester polymer, 1-5 parts of fatty alcohol polyoxyethylene ether, 1-5 parts of isopropanol, and 80-90 parts of water; wherein: The ester polymer is prepared from ditrimethylhydroxypropyl quaternary ammonium salt and carboxylic acid monomer.
2. The high-efficiency fracturing drainage agent according to claim 1, characterized in that: The structural formula of the carboxylic acid monomer is R-COOH, wherein R- is a straight-chain alkyl group, a branched alkyl group, an aromatic group, a halogenated alkyl group or a halogenated aromatic group.
3. The high-efficiency fracturing drainage agent according to claim 2, characterized in that: The preparation steps of the ester polymer include placing ditrimethylhydroxypropyl quaternary ammonium salt, carboxylic acid monomer, catalyst and solvent in a reaction container, fully stirring at 120-140° C., reacting for 5-15 hours, discharging water generated by the esterification reaction in time, filtering and removing the solvent after the reaction is completed to obtain the ester polymer.
4. The high-efficiency fracturing drainage agent according to claim 3, characterized in that: The solvents are trifluoroacetic acid, chloroform, phenol, tetrachloroethane, o-chlorophenol, benzene, chlorobenzene, chloroform, ethyl acetate, ethanol, acetone, and ether.
5. The high-efficiency fracturing drainage agent according to claim 4, characterized in that: The molar ratio of the bistrimethylhydroxypropyl quaternary ammonium salt to the carboxylic acid monomer is 1:(1-3), and the mass ratio of the sum of the mass of the bistrimethylhydroxypropyl quaternary ammonium salt, the carboxylic acid monomer and the catalyst to the solvent is 1:(3-8).
6. A method for preparing the high-efficiency fracturing drainage agent according to any one of claims 1 to 5, comprising the following steps: Add isopropanol into water, mix well, then add ester polymer and fatty alcohol polyoxyethylene ether, mix well to obtain the product.