Oil-immersed radiating fin processing technology
Through the oil-immersed heat sink processing technology, the problems of low heat dissipation efficiency and insufficient durability in traditional processes are solved. The heat conduction efficiency and durability of the heat sink are improved through uniform oil film and nanocoating, and better heat dissipation performance and Corrosion resistance.
Patent Information
- Application Number
- CN202411157544.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-22
- Publication Date
- 2024-11-12
AI Technical Summary
The traditional heat sink processing technology has limitations in terms of heat dissipation efficiency and durability, especially the problems of surface oxidation and uneven heat conduction, which leads to a degradation of heat dissipation performance.
The oil-immersed heat sink processing technology is adopted, including material selection, milling processing, anodizing treatment, sandblasting treatment, cleaning, drying, oil-immersed treatment and curing treatment. By forming a uniform oil film and nanocoating, the heat conduction efficiency is improved and Corrosion resistance.
It significantly improves the heat conduction efficiency and durability of the heat sink, ensures uniform coverage and firm adhesion of the oil film, enhances mechanical stability and high temperature resistance, and provides additional protection.
Smart Images

Figure CN118932454A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of heat sink processing, in particular to a processing technology for oil-immersed heat sinks. Background Art
[0002] As a key heat dissipation component in electronic devices and other high-heat generating devices, the performance of heat sinks directly affects the stability and life of the equipment. Traditional heat sink processing mainly includes metal processing, surface treatment and installation steps, but these methods have certain limitations in heat dissipation efficiency and durability. At present, the commonly used heat sink materials are mainly aluminum and copper, and the processing techniques used include stamping, extrusion, milling, etc. Although these processes can produce heat sinks with shapes and sizes that meet the requirements, in actual use, the surface of the heat sink often has problems such as oxidation, corrosion and uneven heat conduction, resulting in reduced heat dissipation performance.
[0003] Traditional surface treatment methods can improve the surface performance of heat sinks to a certain extent, but cannot solve the problems of low heat dissipation efficiency and insufficient durability. Summary of the invention
[0004] In view of the shortcomings of the prior art, the present invention provides an oil-immersed heat sink processing technology, which solves the problem that the traditional surface treatment method cannot solve the low heat dissipation efficiency of the heat sink.
[0005] To achieve the above objectives, the present invention is implemented through the following technical solutions: an oil-immersed heat sink processing process comprises the following steps:
[0006] S1: Material selection, select aluminum or copper material according to the thermal conductivity required by the heat sink, measure the thickness and size of the material and check the purity and composition of the material;
[0007] S2: Heat sink production: according to the design drawings, determine the size, shape and structure of the heat sink, use the milling process to process the heat sink, and finally deburr the processed heat sink;
[0008] S3: Surface treatment: prepare sulfuric acid solution, immerse the heat sink in the electrolyte, connect the power supply for electrolysis reaction, set the electrolysis parameters for anodizing to form an oxide film, and then clean the heat sink to remove the residual electrolyte, prepare sandblasting equipment and aluminum oxide sand, set the parameters of the sandblasting equipment to sandblast the heat sink;
[0009] S4: cleaning the heat sink, preparing an alkaline cleaning agent or solvent, soaking the heat sink in the cleaning agent, cleaning the surface of the heat sink with a brush or ultrasonic cleaning equipment, and then rinsing the heat sink with deionized water to remove the residual cleaning agent;
[0010] S5: Dry the heat sink, prepare a dryer or hot air circulation oven, set the drying temperature and time, and put the cleaned heat sink into the drying equipment;
[0011] S6: Oil immersion treatment, select silicone oil or mineral oil, prepare an oil immersion tank, and immerse the preheated heat sink in the heat transfer oil;
[0012] S7: Take out and dry, prepare a drying area or centrifugal equipment, hang the oil-soaked heat sink in a dry area to dry or use a centrifugal device to spin off excess oil.
[0013] Preferably, the heat sink design drawing in step S2 includes a heat sink body, the inner wall of the heat sink body is provided with a positioning lock, the outer wall of the heat sink body is provided with a plurality of diversion layers, the outer wall of the heat sink body is provided with a docking port, and the outer wall of the heat sink body is provided with an anti-collision notch.
[0014] Preferably, in the step S1, the thickness of the aluminum plate is 2 mm to 10 mm, the thickness of the copper plate is 1 mm to 5 mm, and the purity is above 99.5%. In the step S2, the size of the heat sink is 100 mm x 50 mm x 10 mm, the fin spacing is 0.8 mm to 1 mm, the milling speed during processing is 2000 rpm, the feed speed is 100 mm / min, and the deburring is performed using 120# sandpaper or a deburring machine for 2 to 5 minutes. In the step S3, the sulfuric acid concentration is 15% to 20%, and the electrolysis current density is 1.5 A / dm 2 -2.0A / dm 2 , the treatment time is 20-30 minutes, the oxide film thickness is 10-20 microns, the sand particle size is 60-80 aluminum oxide sand, the air pressure is 0.5MPa-0.6MPa, the treatment time is 5-10 minutes, and the surface roughness Ra of the heat sink after treatment is 1.6-3.2 microns. In the step S4, the cleaning agent is selected as 5% alkaline cleaning agent solution or isopropanol solution. When using a brush and a cleaning agent, the cleaning time is 5-10 minutes. When using ultrasonic cleaning, the frequency is set to 40kHz, the cleaning time is 10-15 minutes, and then deionized water is used. Rinse 2-3 times, each time for 3-5 minutes. In the step S5, the temperature of the drying machine is set to 80°C-100°C, the drying time is set to 30-60 minutes, or it is naturally dried for 24 hours. In the step S6, silicone oil or mineral oil with a viscosity of 10-50cSt is selected, and the heat sink is completely immersed in the heat transfer oil for 10-30 minutes. In the step S7, the heat sink after oil immersion is hung in a drying area for 1-2 hours to dry, the speed of the centrifugal equipment is 1000-2000rpm, and the drying time is 5-10 minutes.
[0015] Preferably, a preheating treatment is performed after the step S5, a preheating furnace or a hot air circulation oven is prepared, the preheating temperature and time are set, and the dried heat sink is placed in the preheating device.
[0016] Preferably, the preheating temperature is set to 100° C.-120° C., and the time is set to 15-30 minutes.
[0017] Preferably, after the step S7, heat treatment curing is performed, a heat treatment furnace or oven is prepared, the heat treatment temperature and time are set, and the dried heat sink is placed in the heat treatment equipment for heat treatment.
[0018] Preferably, the temperature of the heat treatment is set to 120° C.-150° C., and the time is set to 1-2 hours.
[0019] Preferably, nano-coating is performed after the step S7, wherein nano-coating materials are selected, spraying or dipping equipment is prepared, parameters of the coating equipment are set, and the surface of the heat sink is coated to form a nano-coating.
[0020] Preferably, the coating material is SiO2 or TiO2 nano-coating material, and the coating thickness is 50-100 nanometers.
[0021] Preferably, after the step S7, repeated oil immersion treatment is performed, and curing treatment is performed after each oil immersion, which is repeated 2-3 times to make the thickness of each oil film uniform and the final total thickness is 5-10 microns.
[0022] The present invention provides a processing technology for oil-immersed heat sinks, which has the following beneficial effects:
[0023] 1. The present invention can evenly cover the surface of the heat sink through the oil film, thereby improving the heat conduction efficiency. The heat sink can effectively transfer heat from the heat source to the surrounding environment. The high thermal conductivity of the heat transfer oil helps to quickly transfer heat from the heat sink to the air, thereby improving the overall heat dissipation effect.
[0024] 2. The present invention can gradually increase the thickness of the oil film of the heat sink through multiple oil immersions to ensure that the design requirements are met. Each oil immersion and curing treatment can achieve the effect of optimizing the uniformity and adhesion of the oil film.
[0025] 3. The present invention can further remove residual moisture inside and on the surface of the heat sink through preheating treatment, thereby increasing the surface temperature of the heat sink and enhancing the adhesion effect of the heat transfer oil.
[0026] 4. The present invention can solidify the oil film through heat treatment and more firmly adhere to the surface of the heat sink. The curing treatment can achieve the effect of improving the mechanical stability and high temperature resistance of the oil film.
[0027] 5. The present invention has excellent thermal conductivity through the nano coating, which can further improve the heat dissipation efficiency of the heat sink, and the nano coating can provide additional protection and enhance the corrosion resistance of the heat sink.
[0028] 6. The oxide film produced by anodizing in the present invention can effectively prevent oxidation and corrosion of the heat sink surface, improve the durability of the heat sink in harsh environments, and increase the adhesion of the oil film on the heat sink surface.
[0029] 7. The present invention can achieve the effect of automatic positioning when the heat sink needs to be flipped 180° for welding through the design of the positioning lock.
[0030] 8. The present invention can achieve the effect of improving the heat dissipation efficiency by designing the diverter layer so that the oil flows through the diverter layer and flows out in layers when the heat sink is in use.
[0031] 9. The present invention can achieve the effect of upper and lower docking when using multiple heat sinks through the design of the docking interface. After docking, the distance between the heat sinks can be kept at 40cm and 45cm, and the docking interface can prevent the deviation of multiple heat sinks when they are used.
[0032] 10. The present invention can prevent the heat sink from being deformed by collision during processing by designing the anti-collision notch. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] Figure 1 The oil-immersed heat sink processing process flow chart of the present invention;
[0034] Figure 2 It is a three-dimensional diagram of the heat sink body of the present invention.
[0035] Among them, 1. heat sink body; 2. positioning lock; 3. diversion layer; 4. docking interface; 5. anti-collision notch. DETAILED DESCRIPTION
[0036] The technical solution of the present invention will be described clearly and completely below in conjunction with the accompanying drawings of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0037] Embodiment 1:
[0038] Please see attached Figure 1 - Attachment Figure 2 The embodiment of the present invention provides a process for processing an oil-immersed heat sink, comprising the following steps:
[0039] S1: Material selection, select aluminum material according to the thermal conductivity required by the heat sink, measure the thickness and size of the material and check the purity and composition of the material;
[0040] S2: Heat sink production: according to the design drawings, determine the size, shape and structure of the heat sink, use the milling process to process the heat sink, and finally deburr the processed heat sink;
[0041] S3: Surface treatment: prepare sulfuric acid solution, immerse the heat sink in the electrolyte, connect the power supply for electrolysis reaction, set the electrolysis parameters for anodizing to form an oxide film, and then clean the heat sink to remove the residual electrolyte, prepare sandblasting equipment and aluminum oxide sand, set the parameters of the sandblasting equipment to sandblast the heat sink;
[0042] S4: Clean the heat sink, prepare an alkaline cleaning agent or solvent, soak the heat sink in the cleaning agent, use a brush to clean the surface of the heat sink, and then rinse the heat sink with deionized water to remove the cleaning agent residue;
[0043] S5: Dry the heat sink, prepare the dryer, set the drying temperature and time, and put the cleaned heat sink into the drying equipment;
[0044] S6: Oil immersion treatment, select silicone oil, prepare an oil immersion tank, and immerse the preheated heat sink in the heat transfer oil;
[0045] S7: Take out and dry, prepare a drying area or centrifugal equipment, and hang the oil-soaked heat sink in a drying area to dry.
[0046] The heat sink design drawing in step S2 includes a heat sink body 1, a positioning lock buckle 2 is provided on the inner wall of the heat sink body 1, a plurality of diversion layers 3 are provided on the outer wall of the heat sink body 1, a docking port 4 is provided on the outer wall of the heat sink body 1, and an anti-collision notch 5 is opened on the outer wall of the heat sink body 1;
[0047] Specifically, the positioning lock 2 is designed to automatically position the heat sink when it needs to be flipped 180° for welding. The diverter layer 3 is designed to allow the oil to flow through the diverter layer and flow out in layers when the heat sink is in use to improve the heat dissipation efficiency. The docking interface 4 is designed to achieve the upper and lower docking effect when multiple heat sinks are used. After docking, the distance between the heat sinks can be maintained at 40cm and 45cm. The docking interface 4 prevents deviation when multiple heat sinks are used. The anti-collision notch 5 is designed to prevent the heat sink from colliding and deforming during processing.
[0048] In step S1, the thickness of the aluminum plate is 3 mm and the purity is 99.5%. In step S2, the size of the heat sink is 100 mm x 50 mm x 10 mm, the fin spacing is 1 mm, the milling speed during processing is 2000 rpm, the feed speed is 100 mm / min, and the deburring is performed using 120 grit sandpaper or a deburring machine for 3 minutes. In step S3, the sulfuric acid concentration is 18%, and the electrolysis current density is 1.5 A / dm 2 , the processing time is 25 minutes, the oxide film thickness is 10-20 microns, the sand particle size is 80 aluminum oxide sand, the air pressure is 0.5MPa, the processing time is 7 minutes, and the surface roughness Ra of the treated heat sink is 1.6-3.2 microns. In step S4, the cleaning agent is selected from 5% alkaline cleaning agent solution or isopropyl alcohol solution. The cleaning time is 8 minutes when using a brush and a cleaning agent. The cleaning time is 8 minutes, and then rinsed with deionized water 3 times, each time for 4 minutes. In step S5, the drying machine temperature is set to 90°C, and the drying time is set to 45 minutes. In step S6, silicone oil with a viscosity of 20cSt is selected to completely immerse the heat sink in the thermal oil for 20 minutes. In step S7, the heat sink after oil immersion is hung in a dry area for 2 hours to dry.
[0049] After step S5, preheating treatment is performed, a preheating furnace or a hot air circulation oven is prepared, the preheating temperature and time are set, and the dried heat sink is placed in the preheating device;
[0050] Specifically, the preheating process can remove residual moisture from the heat sink and improve the oil film adhesion effect.
[0051] The preheating temperature was set to 110°C and the time was set to 20 minutes.
[0052] After step S7, heat treatment curing is performed, a heat treatment furnace or oven is prepared, the heat treatment temperature and time are set, and the dried heat sink is placed in the heat treatment equipment for heat treatment;
[0053] Specifically, the heat treatment curing is used to solidify the oil film and improve the durability of the heat sink.
[0054] The temperature of the heat treatment was set to 130°C and the time was set to 1.5 hours.
[0055] After step S7, nano coating is performed, nano coating materials are selected, spray coating or dipping equipment is prepared, parameters of the coating equipment are set, and the surface of the heat sink is coated to form a nano coating;
[0056] Specifically, the nano coating improves the heat dissipation efficiency and corrosion resistance of the heat sink.
[0057] The coating material is SiO2 nano-coating material, the coating thickness is 80 nanometers, and the coating curing time is 1 hour.
[0058] After step S7, repeated oil immersion treatment is performed, and curing treatment is performed after each oil immersion, which is repeated twice to make the thickness of each oil film uniform, and the final total thickness is 8 microns;
[0059] Specifically, by performing multiple oil immersion treatments and performing curing treatment after each oil immersion, the thickness of the oil film is gradually increased. Multiple oil immersions can ensure that the final oil film reaches the designed thickness requirement, while avoiding uniformity problems caused by excessive oil thickness in one immersion.
[0060] Embodiment 2:
[0061] Please refer to the attached Figure 1 - Attachment Figure 2 The embodiment of the present invention provides a process for processing an oil-immersed heat sink, comprising the following steps:
[0062] S1: Material selection, select copper material according to the thermal conductivity required by the heat sink, measure the thickness and size of the material and check the purity and composition of the material;
[0063] S2: Heat sink production: according to the design drawings, determine the size, shape and structure of the heat sink, use the milling process to process the heat sink, and finally deburr the processed heat sink;
[0064] S3: Surface treatment: prepare sulfuric acid solution, immerse the heat sink in the electrolyte, connect the power supply for electrolysis reaction, set the electrolysis parameters for anodizing to form an oxide film, and then clean the heat sink to remove the residual electrolyte, prepare sandblasting equipment and aluminum oxide sand, set the parameters of the sandblasting equipment to sandblast the heat sink;
[0065] S4: cleaning the heat sink, preparing an alkaline cleaning agent or solvent, soaking the heat sink in the cleaning agent, cleaning the surface of the heat sink with a brush or ultrasonic cleaning equipment, and then rinsing the heat sink with deionized water to remove the residual cleaning agent;
[0066] S5: Dry the heat sink, prepare a dryer or hot air circulation oven, set the drying temperature and time, and put the cleaned heat sink into the drying equipment;
[0067] S6: Oil immersion treatment, select silicone oil or mineral oil, prepare an oil immersion tank, and immerse the preheated heat sink in the heat transfer oil;
[0068] S7: Take out and dry, prepare a drying area or centrifugal equipment, hang the oil-soaked heat sink in a dry area to dry or use a centrifugal device to spin off excess oil.
[0069] The heat sink design drawing in step S2 includes a heat sink body 1, a positioning lock buckle 2 is provided on the inner wall of the heat sink body 1, a plurality of diversion layers 3 are provided on the outer wall of the heat sink body 1, a docking port 4 is provided on the outer wall of the heat sink body 1, and an anti-collision notch 5 is opened on the outer wall of the heat sink body 1;
[0070] Specifically, the positioning lock 2 is designed to automatically position the heat sink when it needs to be flipped 180° for welding. The diverter layer 3 is designed to allow the oil to flow through the diverter layer and flow out in layers when the heat sink is in use to improve the heat dissipation efficiency. The docking interface 4 is designed to achieve the upper and lower docking effect when multiple heat sinks are used. After docking, the distance between the heat sinks can be maintained at 40cm and 45cm. The docking interface 4 prevents deviation when multiple heat sinks are used. The anti-collision notch 5 is designed to prevent the heat sink from colliding and deforming during processing.
[0071] In step S1, the copper plate thickness is 2 mm and the purity is 99.9%. In step S2, the size of the heat sink is 100 mm x 50 mm x 10 mm, the fin spacing is 0.8 mm, the milling speed is 2000 rpm, the feed speed is 100 mm / min, the deburring machine is used for deburring, and the processing time is 4 minutes. In step S3, the sulfuric acid concentration is 20%, and the electrolysis current density is 2.0 A / dm 2 The treatment time is 30 minutes, the oxide film thickness is 10-20 microns, the sand particle size is No. 60 aluminum oxide sand, the air pressure is 0.6MPa, the treatment time is 10 minutes, and the surface roughness Ra of the treated heat sink is 1.6-3.2 microns. In step S4, the cleaning agent is selected as isopropanol solution, and the frequency is set to 40kHz when using ultrasonic cleaning. The cleaning time is 12 minutes, and then rinsed with deionized water 3 times, each time for 5 minutes. In step S5, the drying machine temperature is set to 100°C, and the drying time is set to 60 minutes. In step S6, mineral oil with a viscosity of 30cSt is selected to completely immerse the heat sink in the heat transfer oil for 30 minutes. In step S7, the heat sink after oil immersion uses a centrifugal device with a speed of 1500rpm and a drying time of 8 minutes.
[0072] After step S5, preheating treatment is performed, a preheating furnace or a hot air circulation oven is prepared, the preheating temperature and time are set, and the dried heat sink is placed in the preheating device;
[0073] Specifically, the preheating process can remove residual moisture from the heat sink and improve the oil film adhesion effect.
[0074] The preheating temperature was set to 120°C and the time was set to 25 minutes.
[0075] After step S7, heat treatment curing is performed, a heat treatment furnace or oven is prepared, the heat treatment temperature and time are set, and the dried heat sink is placed in the heat treatment equipment for heat treatment;
[0076] Specifically, the heat treatment curing is used to solidify the oil film and improve the durability of the heat sink.
[0077] The temperature of the heat treatment was set to 150°C and the time was set to 2 hours.
[0078] After step S7, nano coating is performed, nano coating materials are selected, spray coating or dipping equipment is prepared, parameters of the coating equipment are set, and the surface of the heat sink is coated to form a nano coating;
[0079] Specifically, the nano coating improves the heat dissipation efficiency and corrosion resistance of the heat sink.
[0080] The coating material is TiO2 nano-coating material, the coating thickness is 100 nanometers, and the coating curing time is 1.5 hours.
[0081] After step S7, repeated oil immersion treatment is performed, and curing treatment is performed after each oil immersion, which is repeated 3 times to make the thickness of each oil film uniform, and the final total thickness is 10 microns;
[0082] Specifically, by performing multiple oil immersion treatments and performing curing treatment after each oil immersion, the thickness of the oil film is gradually increased. Multiple oil immersions can ensure that the final oil film reaches the designed thickness requirement, while avoiding uniformity problems caused by excessive oil thickness in one immersion.
[0083] Table 1: Main properties of oil-immersed heat sink
[0084] property Embodiment 1 Embodiment 2 Overall cooling efficiency high Very high Corrosion resistance good very good Durability high Very high
[0085] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. The oil-immersed heat sink processing technology is characterized by: The following steps are involved: S1: Material selection, select aluminum or copper material according to the thermal conductivity required by the heat sink, measure the thickness and size of the material and check the purity and composition of the material; S2: Heat sink production: according to the design drawings, determine the size, shape and structure of the heat sink, use the milling process to process the heat sink, and finally deburr the processed heat sink; S3: Surface treatment: prepare sulfuric acid solution, immerse the heat sink in the electrolyte, connect the power supply for electrolysis reaction, set the electrolysis parameters for anodizing to form an oxide film, and then clean the heat sink to remove the residual electrolyte, prepare sandblasting equipment and aluminum oxide sand, set the parameters of the sandblasting equipment to sandblast the heat sink; S4: cleaning the heat sink, preparing an alkaline cleaning agent or solvent, soaking the heat sink in the cleaning agent, cleaning the surface of the heat sink with a brush or ultrasonic cleaning equipment, and then rinsing the heat sink with deionized water to remove the residual cleaning agent; S5: Dry the heat sink, prepare a dryer or hot air circulation oven, set the drying temperature and time, and put the cleaned heat sink into the drying equipment; S6: Oil immersion treatment, select silicone oil or mineral oil, prepare an oil immersion tank, and immerse the preheated heat sink in the heat transfer oil; S7: Take out and dry, prepare a drying area or centrifugal equipment, hang the oil-soaked heat sink in a dry area to dry or use a centrifugal device to spin off excess oil.
2. The oil-immersed heat sink processing technology according to claim 1 is characterized in that: The heat sink design drawing in step S2 comprises a heat sink body (1), the inner wall of the heat sink body (1) is provided with a positioning lock (2), the outer wall of the heat sink body (1) is provided with a plurality of diversion layers (3), the outer wall of the heat sink body (1) is provided with a docking port (4), and the outer wall of the heat sink body (1) is provided with an anti-collision notch (5).
3. The oil-immersed heat sink processing technology according to claim 1 is characterized in that: In the step S1, the thickness of the aluminum plate is 2mm to 10mm, the thickness of the copper plate is 1mm to 5mm, and the purity is above 99.5%. In the step S2, the size of the heat sink is 100mmx50mmx10mm, the fin spacing is 0.8mm-1mm, the milling speed during processing is 2000rpm, the feed speed is 100mm / min, and the deburring is performed using 120# sandpaper or a deburring machine for 2-5 minutes. In the step S3, the sulfuric acid concentration is 15%-20%, and the electrolysis current density is 1.5A / dm2-2.0A / dm 2 , the treatment time is 20-30 minutes, the oxide film thickness is 10-20 microns, the sand particle size is 60-80 aluminum oxide sand, the air pressure is 0.5MPa-0.6MPa, the treatment time is 5-10 minutes, and the surface roughness Ra of the heat sink after treatment is 1.6-3.2 microns. In the step S4, the cleaning agent is selected as 5% alkaline cleaning agent solution or isopropanol solution. When using a brush and a cleaning agent, the cleaning time is 5-10 minutes. When using ultrasonic cleaning, the frequency is set to 40kHz, the cleaning time is 10-15 minutes, and then deionized water is used. Rinse 2-3 times, each time for 3-5 minutes. In the step S5, the temperature of the drying machine is set to 80°C-100°C, the drying time is set to 30-60 minutes, or it is naturally dried for 24 hours. In the step S6, silicone oil or mineral oil with a viscosity of 10-50cSt is selected, and the heat sink is completely immersed in the heat transfer oil for 10-30 minutes. In the step S7, the heat sink after oil immersion is hung in a drying area for 1-2 hours to dry, the speed of the centrifugal equipment is 1000-2000rpm, and the drying time is 5-10 minutes.
4. The oil-immersed heat sink processing technology according to claim 1 is characterized in that: After the step S5, a preheating treatment is performed, a preheating furnace or a hot air circulation oven is prepared, the preheating temperature and time are set, and the dried heat sink is placed in the preheating device.
5. The oil-immersed heat sink processing technology according to claim 4 is characterized in that: The preheating temperature is set to 100° C.-120° C., and the preheating time is set to 15-30 minutes.
6. The oil-immersed heat sink processing technology according to claim 1, characterized in that: After the step S7, heat treatment curing is performed, a heat treatment furnace or oven is prepared, the heat treatment temperature and time are set, and the dried heat sink is placed in the heat treatment equipment for heat treatment.
7. The oil-immersed heat sink processing technology according to claim 6 is characterized in that: The temperature of the heat treatment is set to 120° C.-150° C., and the time is set to 1-2 hours.
8. The oil-immersed heat sink processing technology according to claim 1, characterized in that: After the step S7, nano coating is performed, nano coating materials are selected, spray coating or dipping equipment is prepared, parameters of the coating equipment are set, and the surface of the heat sink is coated to form a nano coating.
9. The oil-immersed heat sink processing technology according to claim 8, characterized in that: The coating material is SiO2 or TiO2 nano coating material, and the coating thickness is 50-100 nanometers.
10. The oil-immersed heat sink processing technology according to claim 1, characterized in that: After the step S7, repeated oil immersion treatment is performed, and curing treatment is performed after each oil immersion, which is repeated 2-3 times to make the thickness of each oil film uniform, and the final total thickness is 5-10 microns.