Aerosol generating material as well as preparation method and application thereof

By designing aerosol-generating materials containing loose skeleton structure materials in the heating cigarette, the problems of insufficient smoke release and poor stability of the heating cigarette are solved, and efficient flue gas release and component synergy are achieved, which improves consumer pumping Enjoy experience.

CN118932789AActive Publication Date: 2024-11-12ZHENGZHOU TOBACCO RES INST OF CNTC
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411334425.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-24
Publication Date
2024-11-12
Estimated Expiration
2044-09-24

AI Technical Summary

Technical Problem

The initial number of mouths of the heating cigarettes is insufficient smoke release, poor stability, and insufficient component synergy, which affects the consumer's suction sensory experience.

Method used

Design an aerosol-generating material, including a base paper layer, atomizer releasing layer and an aroma release layer, which uses loose framework structural materials such as cellulose nanofibers and their derivatives, and is coated by layering. Atomizing agents and fragrance release substances use loose skeleton structure to facilitate uniform dispersion and release of the atomizing agent.

Benefits of technology

It improves the release amount and stability of flue gas, reduces atomizer residue, improves the coordinated release of flue gas components, and enhances consumers' suction sensory experience.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118932789A_ABST
    Figure CN118932789A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of heating cigarettes, and particularly relates to an aerosol generating material and a preparation method and application thereof. The aerosol generating material comprises a base paper layer, an atomizing agent release promoting layer and a fragrance releasing layer, wherein the surface of the base paper layer is loaded with an atomizing agent release promoting layer, and the surface of the atomizing agent release promoting layer is loaded with a fragrance releasing layer; the atomizing agent release promoting layer comprises an atomizing agent and an atomizing agent release promoting material, and the atomizing agent release promoting material is selected from a loose skeleton structure material. In order to facilitate the synergistic release of the atomizing agent and the aroma substance, the atomizing agent and the aroma substance are coated in a layered manner, the atomizing agent is placed at the bottom of the aroma substance, so that the atomized atomizing agent carries the aroma substance to form smoke aerosol, and an atomizing agent release channel is formed in the atomizing agent release promoting layer by using an atomizing agent release promoting material; therefore, the purposes of promoting release of the atomizing agent, reducing residues of the atomizing agent and further promoting release of smoke are achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of heated cigarettes, and in particular relates to an aerosol generating material and a preparation method and application thereof. Background Art

[0002] In recent years, as global tobacco control efforts have gradually increased, heat-not-burn tobacco products have become popular due to their low harm, and major multinational tobacco companies and enterprises have competed to launch heated cigarette products. Heated cigarettes are a type of tobacco product that uses heating devices, physical and chemical reactions, or aerosol heating to heat tobacco materials at low temperatures rather than burning them. Heated cigarettes release nicotine-containing smoke aerosols through low-temperature distillation and evaporation to form smoke aerosols for consumers to inhale; compared with the release of harmful or potentially harmful components caused by the combustion process of traditional cigarettes, their smoke aerosols have significantly reduced release, making heated cigarettes have relatively "harm reduction" characteristics.

[0003] At present, heated cigarettes can be roughly divided into tobacco, reconstituted tobacco and tobacco particles according to the different forms of the core materials. At present, the thermal properties and smoke release laws of reconstituted tobacco and tobacco have been reported in the literature, but because the core material as the smoke release medium of heated cigarettes is heated at a low temperature, there are problems such as poor initial smoke release, puff-by-puff stability needs to be improved, and insufficient component synergy.

[0004] The present invention is proposed to optimize the controlled release of the atomizer and the synergistic release between components and to improve the consumer's sensory experience of smoking. Summary of the invention

[0005] The first aspect of the present application provides an aerosol generating material, the aerosol generating material comprising: a base paper layer, an atomizer release promoting layer, and a fragrance releasing layer;

[0006] Wherein, the surface of the base paper layer is loaded with an atomizer release-promoting layer, and the surface of the atomizer release-promoting layer is loaded with a fragrance release layer;

[0007] The atomizer release-promoting layer comprises: an atomizer and an atomizer release-promoting material, and the atomizer release-promoting material is selected from loose skeleton structure materials.

[0008] Preferably, the upper and lower surfaces of the base paper layer are both loaded with the atomizer release-promoting layer on the base paper layer, and the upper and lower surfaces of the atomizer release-promoting layer are both loaded with the fragrance-releasing layer.

[0009] Preferably, the loose skeleton structure material is selected from: one or more of cellulose nanofibers and their derivatives, such as cellulose nanocrystals (CNC), cellulose nanofibrils (CNF), microcrystalline cellulose (MCC), sodium carboxycellulose, hydroxy cellulose, and one or more of cationic modified cellulose.

[0010] Preferably, the flavor-releasing layer may include tobacco material, tobacco coating liquid and / or extract.

[0011] Preferably, the tobacco material is tobacco powder, and the particle size of the tobacco powder ranges from 20 mesh to 400 mesh.

[0012] Preferably, the extract includes but is not limited to one or more extracts of herbal plants such as tobacco, cocoa, and chicory.

[0013] Preferably, the atomizer is selected from: the atomizer is one or more of glycerol, glyceride and its derivatives, propylene glycol, and ethanol.

[0014] Preferably, the base paper layer has a basis weight range of 20-50 g / m 2 The coating amount of the atomizer release-promoting layer on the base paper layer is 3-30 g / m 2 The mass fraction of the atomizer to promote release of the atomizer is 2-30%, and the mass of the fragrance release layer is 3-30g / m 2 .

[0015] Preferably, the base paper layer has a basis weight range of 30-40 g / m 2 .

[0016] The second aspect of the present application provides a method for preparing the aerosol generating material according to any one of the first aspects, characterized in that it comprises the following steps:

[0017] Step 1, uniformly mixing an atomizer, an atomizer release-promoting material and water to obtain a mixed solution of the atomizer and the atomizer release-promoting material; the atomizer release-promoting material is selected from one or more of cellulose nanofibers and their derivatives, sodium carboxymethyl cellulose, hydroxypropyl cellulose and cationic modified cellulose;

[0018] Step 2: coating the atomizer and the atomizer release-promoting material mixed solution on the surface of the base paper by a coating machine and drying to form an atomizer release-promoting layer;

[0019] Step 3: coating the aroma-releasing substance on the upper part of the atomizer release-promoting layer and drying it to form the aroma-releasing layer; the whole material finally obtained is an aerosol generating material.

[0020] Preferably, in step 1, the mass ratio of the atomizer, the atomizer release-promoting material and water is (80-95):(2-30):(1-10).

[0021] Preferably, the coating amount in step 2 is 3-30 g / m 2 , the drying temperature is 50-80℃, and the drying time is 3-20min.

[0022] Preferably, the coating amount in step 3 is 3-30 g / m 2, the drying temperature is 50-100℃, and the drying time is 5-20min.

[0023] Preferably, the viscosity of the mixed solution of the atomizer and the atomizer release-promoting material after mixing in step 1 is 30-3000 mPa·s (25° C.).

[0024] Preferably, the mixed solution of the atomizer and the atomizer release-promoting material is in a gel state.

[0025] The third aspect of the present application provides use of the aerosol generating material described in any one of the first aspects for promoting smoke release.

[0026] Preferably, the base paper layer is base paper for reconstituted tobacco sheets by a papermaking composite process.

[0027] Compared with the prior art, the present invention has the following beneficial effects:

[0028] 1. In order to facilitate the release of the atomizer in coordination with the aroma-releasing substance, the present invention coats the atomizer and the aroma-releasing substance in layers, and places the atomizer at the bottom of the aroma-releasing substance so that the atomizer can carry the aroma-releasing substance to form a smoke aerosol after being atomized, and uses the atomizer release-promoting material to form an atomizer release channel in the atomizer layer, so as to achieve the purpose of promoting the release of the atomizer, reducing the atomizer residue, and thus promoting the smoke release.

[0029] In particular, the atomizer release-promoting material in the present application selects a loose skeleton structure material, such as cellulose nanofibers and their derivatives, including cellulose nanocrystals (CNC), cellulose nanofibrils (CNF), microcrystalline cellulose (MCC), sodium carboxymethyl cellulose, hydroxypropyl cellulose, and cationic modified cellulose. The reasons are: (1) These substances contain a large number of hydroxyl groups on the surface, which can form a large number of hydrogen bonds with the atomizer molecules, thereby reducing the interaction force inside the atomizer molecules, thereby changing large molecular clusters into small molecular clusters, and the atomizer of the small molecular clusters is easy to release when heated. (2) These substances form a loose skeleton structure after drying, and the skeleton structure is easy to load a large number of small molecular clusters of atomizers so that the atomizer of the small molecular clusters is evenly dispersed, and then evenly heated, which is convenient for the gradual release of the small molecular cluster substances.

[0030] The applicant analyzed the reasons as follows: when no atomizer-promoting release material is added, the atomizer directly penetrates into the pores of plant fibers (such as base paper fibers or tobacco fibers), so the release rate is slow and the residual rate is high. However, after the atomizer-promoting release material is added in the present application, propylene glycol is bound to the loose skeleton structure of the atomizer-promoting release material (rather than penetrating into the pores of plant fibers) and is more easily released.

[0031] 2. In addition, the process flow designed by the present invention is simple and can meet production and preparation requirements using existing production equipment. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] Figure 1 It is a schematic diagram of the self-assembly raw materials of atomizer-promoted heated cigarette.

[0033] Figure 2 This is a schematic diagram of the release promoting principle of the atomizer-promoting release material of the present application, a contains the atomizer-promoting release material, and b does not contain the atomizer-promoting release material.

[0034] Figure 3 It is the thermal weight loss data of the aerosol generating materials of Example 1 and Comparative Sample 1.

[0035] Figure 4 It is a schematic diagram of rolling aerosol generating materials.

[0036] Figure 5 This is a graph showing the atomizer residue data for the cigarettes of Example 2 and Comparative Example 2 in Application Example 2.

[0037] Figure 6 It is the puff-by-puff smoke release of the cigarette of Example 2 and Comparative Example 2 in Application Example 2 and the corresponding atomizer and nicotine release.

[0038] Figure 7 It is the puff-by-puff smoke release of the cigarette of Example 3 and Comparative Example 3 in Application Example 3, as well as the corresponding atomizer and nicotine release.

[0039] Figure 8 This is a graph showing the atomizer residue data for the cigarettes of Example 4 and Comparative Example 4 in Application Example 4. Description of the drawings:

[0041] 1. Fragrance release layer, 2. Atomizer release promoting layer, 3. Base paper layer. DETAILED DESCRIPTION

[0042] The present invention is described below in conjunction with specific examples, but the embodiments of the present invention are not limited thereto. Experimental methods without specific conditions in the examples are usually carried out according to conventional conditions and conditions described in the manual, or according to the conditions recommended by the manufacturer. The general equipment, materials, reagents, etc. used can be obtained from commercial channels unless otherwise specified. The raw materials required in the following examples and comparative examples are all commercially available.

[0043] The following base paper, glycerin, cellulose nanofibers, tobacco concentrate, etc., which are flavor-releasing substances, can all be prepared by conventional means.

[0044] Example 1

[0045] A method for preparing an aerosol generating material comprises the following steps:

[0046] 1. Select the quantitative value of 35±0.5g / m 2 Base paper.

[0047] 2. Use a rapid dispersion device to evenly mix the atomizer glycerol, the atomizer release-promoting material cellulose nanofibrils (CNF) and water in a mass ratio of 85:10:2. The viscosity of the mixed atomizer and atomizer release-promoting material mixture is 80±1.0 mPa·s (20°C).

[0048] 3. Use a coating machine to coat the atomizer and atomizer release promoting material mixture on the surface of the base paper. The coating amount is controlled by controlling the coating machine speed and the coating metering roller depth. The coating amount is 20±0.5g / m 2 The mixed liquid layer of the atomizer and the atomizer release-promoting material is dried by a drying box to form an atomizer release-promoting layer. The drying box temperature is 80°C and the drying time is 3 minutes. The coating is double-sided coating, that is, coating is performed on the upper and lower surfaces.

[0049] 4. Apply the tobacco concentrate liquid, the aroma-releasing substance, on the atomizer release-promoting layer at a coating amount of 20±0.5g / m 2 The coating is double-sided coating. Drying is carried out by a box drying device, the drying temperature is 100°C, and the drying time is 5 minutes. The quantitative value is 75±1.0g / m 2 Aerosol generating material, structural diagram as shown Figure 1 .

[0050] Comparative Example 1

[0051] The only difference from Example 1 is that in step 1, no atomizer-promoting release material cellulose nanofibrils (CNF) is added to obtain aerosol generating material comparison sample 1.

[0052] Application Example 1

[0053] 10 mg of the aerosol generating material prepared in Example 1 and 10 mg of the comparative sample 1 were placed in a thermogravimetric analyzer and heated from room temperature to 250°C and kept warm for 30 minutes. Figure 3 As shown, the thermal weight loss and the fastest thermal weight loss rate of the aerosol generating material of Example 1 with CNF added are much greater than those of the comparative sample 1 without CNF added.

[0054] The fastest thermal weight loss rate of Example 1 is 1.86 times that of Comparative Sample 1, indicating that the addition of cellulose nanofibrils (CNF) can promote the release of atomizers and thus promote the release of smoke.

[0055] Example 2

[0056] A method for preparing an aerosol generating material comprises the following steps:

[0057] 1. Select the quantitative value of 30±0.5g / m 2 Base paper.

[0058] 2. Use a rapid dispersion device to mix the atomizer propylene glycol, the atomizer release-promoting material cellulose nanocrystals (CNC) and water in a mass ratio of 90:15:1. The viscosity of the mixed atomizer and the atomizer release-promoting material mixture is 219±1.0 mPa·s (20°C).

[0059] 3. Use a coating machine to coat the atomizer and atomizer release promoting material mixture on the surface of the base paper. The coating amount is controlled by controlling the coating machine speed and the coating metering roller depth. The coating amount is 25±0.5g / m 2 The mixed liquid layer of the atomizer and the atomizer release-promoting material is dried by using a drying box, the drying box temperature is 50°C, and the drying time is 20 minutes. The coating is double-sided coating, that is, coating is performed on the upper and lower surfaces.

[0060] 4. Apply the tobacco concentrate liquid, which is the aroma-releasing substance, on the atomizer layer at a coating amount of 25 ± 0.5 g / m 2 . Drying was carried out in a box drying device at a drying temperature of 50°C and a drying time of 20 minutes. The obtained quantitative value was 80±1.0g / m 2 Aerosol generating material. The coating is double-sided coating, that is, coating is performed on both the upper and lower surfaces.

[0061] The aerosol generating material is rolled into a smoking section (a schematic diagram of using a cigarette making machine to roll the aerosol generating material into a smoking section Figure 4 The heated cigarette is assembled by wrapping the cigarette paper with the concentric circle material of the pattern.

[0062] Comparative Example 2

[0063] A method for preparing an aerosol generating material, which differs from Example 2 in that the atomizer is applied together with the fragrance-releasing substance, rather than in layers, and the specific steps are as follows:

[0064] 1. Select the quantitative value of 30±0.5g / m 2 Base paper.

[0065] 2. Mix the atomizer propylene glycol and the flavor-releasing substance tobacco concentrate in a mass ratio of 1:1 and apply them on the upper and lower surfaces of the base paper using a coating machine. The coating amount is controlled by controlling the coating machine speed and the coating metering roller depth. The coating amount is 50g / m 2 .

[0066] 3. Dry in a box drying device at 80°C for 15 minutes. The obtained weight is 80±1.0g / m 2 Aerosol generating materials.

[0067] The aerosol generating material is rolled into a smoking section (a schematic diagram of using a cigarette making machine to roll the aerosol generating material into a smoking section Figure 4 The heated cigarette is assembled by wrapping the cigarette paper with the concentric circle material of the pattern.

[0068] Application Example 2

[0069] The cigarettes of Example 2 and Comparative Example 2 were respectively taken, and a circumferentially heated smoking device was used. The cigarettes were smoked at Canadian depth using a smoking machine at heating temperatures of 200°C, 220°C, 240°C, 260°C, 280°C and 300°C. The residue in the cigarette core after 12 puffs was analyzed by chromatography for composition and the residual rate of propylene glycol was calculated.

[0070] The results are as follows Figure 5 As shown in the figure, the residual propylene glycol rate of Example 2 gradually decreases with the increase of temperature and is much lower than that of Comparative Example 2. When the temperature is 220°C, the residual propylene glycol rate of Comparative Example 2 and Example 2 differs the most, and the residual propylene glycol rate of Example 2 is only 64.5% of that of the Comparative Example. The heating temperature is selected to be 260°C, and the samples of Example 2 and Comparative Example 2 are smoked. The smoke release per puff is shown in the figure. Figure 6 As shown, the puff-by-puff smoke release of Example 2 is higher than that of Comparative Example 2. At the same time, the puff-by-puff release of the atomizer and nicotine maintains a consistent release trend. It can be seen that layering the atomizer and adding the atomizer release-promoting material is beneficial to promoting the release of the atomizer, thereby promoting the smoke release.

[0071] Example 3

[0072] A method for preparing an aerosol generating material comprises the following steps:

[0073] 1. Select base paper with a basis weight of 40±0.5g / m2.

[0074] 2. Use a rapid dispersion device to evenly mix the atomizer glycerol, the atomizer release-promoting material microcrystalline cellulose (MCC) and water in a mass ratio of 85:10:2. The viscosity of the mixed atomizer and atomizer release-promoting material mixture is 105±1.0 mPa·s (20°C).

[0075] 3. Use a coating machine to coat the mixed liquid of atomizer and atomizer release-promoting material on the surface of the base paper. Control the coating amount by controlling the coating machine speed and the coating metering roller depth. The coating amount is 22±0.5g / m2. Use a box drying device to dry the mixed liquid layer of atomizer and atomizer release-promoting material to form an atomizer release-promoting layer. The drying box temperature is 70°C and the drying time is 12 minutes. The coating is double-sided coating, that is, coating is performed on the upper and lower surfaces.

[0076] 4. Apply the tobacco concentrate liquid, the aroma-releasing substance, on the atomizer release-promoting layer, with a coating amount of 22±0.5g / m 2The coating is double-sided coating. Drying is carried out by a box drying device, the drying temperature is 80, and the drying time is 20 minutes. The quantitative is 84±1.0g / m 2 Aerosol generating materials.

[0077] Comparative Example 3

[0078] A method for preparing an aerosol generating material, which differs from Example 3 in that the atomizer is applied together with the fragrance releasing substance, rather than in layers, and the specific steps are as follows:

[0079] 1. Select the quantitative value of 40±0.5g / m 2 Base paper.

[0080] 2. Mix the atomizer propylene glycol and the flavor-releasing substance tobacco concentrate in a mass ratio of 1:1 and apply them on the upper and lower surfaces of the base paper using a coating machine. The coating amount is controlled by controlling the coating machine speed and the coating metering roller depth. The coating amount is 44g / m 2 .

[0081] 3. Drying in a box drying device, the drying temperature is 80℃, the drying time is 20min. The quantitative value is 84±1.0g / m 2 Aerosol generating materials.

[0082] The aerosol generating material is rolled into a smoking section (a schematic diagram of using a cigarette making machine to roll the aerosol generating material into a smoking section Figure 4 The heated cigarette is assembled by wrapping the cigarette paper with the concentric circle material of the pattern.

[0083] Application Example 3

[0084] The cigarettes of Example 3 and Comparative Example 3 were taken respectively, and a circumferentially heated smoking device was used. A smoking machine was used for smoking at a heating temperature of 260° C. according to Canadian depth, and a smoking test was performed on the samples of Example 3 and Comparative Example 3 to detect the smoke release of each puff.

[0085] The results are as follows Figure 7 As shown, the puff-by-puff smoke release of Example 3 is higher than that of Comparative Example 3 as a whole. The total smoke release of Example 3 is 2.4 mg more than that of Comparative Example 3. The change trend of the puff-by-puff nicotine release of Example 3 and Comparative Example 3 is consistent with the smoke release. It can be seen that layering the atomizer and adding the atomizer release-promoting material is beneficial to promoting the release of the atomizer, thereby promoting the smoke release.

[0086] Example 4

[0087] A method for preparing an aerosol generating material comprises the following steps:

[0088] 1. Select the quantitative value of 45±0.5g / m 2Base paper.

[0089] 2. Use a rapid dispersion device to mix the atomizer propylene glycol, the atomizer release-promoting material sodium carboxymethyl cellulose (CMC) and water in a mass ratio of 90:15:1. The viscosity of the mixed atomizer and the atomizer release-promoting material mixture is 400±1.0 mPa·s (20°C).

[0090] 3. Use a coating machine to coat the atomizer and atomizer release promoting material mixture on the surface of the base paper. The coating amount is controlled by controlling the coating machine speed and the coating metering roller depth. The coating amount is 20±0.5g / m 2 The mixed liquid layer of the atomizer and the atomizer-promoting release material is dried by using a drying box, the drying box temperature is 50°C, and the drying time is 10 minutes. The coating is double-sided coating, that is, coating is performed on the upper and lower surfaces.

[0091] 4. Apply the tobacco concentrate liquid, which is the aroma-releasing substance, on the atomizer layer at a coating amount of 20 ± 0.5 g / m 2 . Drying was carried out in a box drying device at a drying temperature of 80°C and a drying time of 15 minutes. The obtained quantitative value was 95±1.0g / m 2 Aerosol generating materials.

[0092] Comparative Example 4

[0093] The only difference from Example 4 is that in step 1, no atomizer-promoting release material sodium carboxymethyl cellulose (CMC) is added to obtain aerosol generating material comparison sample 4.

[0094] Application Example 4

[0095] The cigarettes of Example 4 and Comparative Example 4 were respectively taken, and a circumferentially heated smoking device was used. The cigarettes were smoked at Canadian depth using a smoking machine at heating temperatures of 200°C, 220°C, 240°C, 260°C, 280°C and 300°C. The residue in the cigarette core after 12 puffs was analyzed by chromatography for composition and the residual rate of propylene glycol was calculated.

[0096] The results are as follows Figure 8 As shown:

[0097] The propylene glycol residual rate of the cigarettes in Example 4 gradually decreases with increasing temperature and is much lower than that in Comparative Example 4.

[0098] At 260°C, the residual propylene glycol rate of the cigarette in Example 4 is only 36% of that in the comparative example. It can be seen that in the comparative example, when the atomizer-promoting release material sodium carboxymethyl cellulose (CMC) is not added, the residual propylene glycol rate in the cigarette core residue after smoking is higher than that in Example 4. The applicant analyzed that this is because part of the propylene glycol in the comparative example 4 penetrated into the deep pores of the plant fiber (such as the base paper fiber), and thus could not be effectively released. After the atomizer-promoting release material was added in Example 4, the propylene glycol was bound to the skeleton structure of the atomizer-promoting release material (rather than penetrating into the pores of the plant fiber) and was more easily released.

[0099] The above embodiments are only some embodiments of the present invention, not all embodiments.

Claims

1. An aerosol generating material, It is characterized in that The aerosol generating material comprises: a base paper layer, an atomizer release promoting layer, and a fragrance releasing layer; Wherein, the surface of the base paper layer is loaded with an atomizer release-promoting layer, and the surface of the atomizer release-promoting layer is loaded with a fragrance release layer; The atomizer release-promoting layer comprises: an atomizer and an atomizer release-promoting material, and the atomizer release-promoting material is selected from loose skeleton structure materials.

2. The aerosol generating material according to claim 1, It is characterized in that The upper and lower surfaces of the base paper layer are both loaded with the atomizer release-promoting layer, and the upper and lower surfaces of the atomizer release-promoting layer are both loaded with the fragrance-releasing layer.

3. The aerosol generating material according to claim 1, It is characterized in that The aroma-releasing layer contains one or more of tobacco flavor concentrate, nicotine, nicotine salt, and herbal plant extracts.

4. The aerosol generating material according to claim 1, It is characterized in that The atomizer is selected from: the atomizer is one or more of glycerol, glyceride and its derivatives, propylene glycol, and ethanol.

5. The aerosol generating material according to claim 1, It is characterized in that The base paper layer has a basis weight range of 20-50 g / m 2 The coating amount of the atomizer release-promoting layer on the base paper layer is 3-30 g / m 2 The mass fraction of the atomizer to promote release of the atomizer is 2-30%, and the mass of the fragrance release layer is 3-30g / m 2 .

6. The aerosol generating material according to claim 1, It is characterized in that The loose skeleton structure material is selected from: one or more of cellulose nanofibers and their derivatives; The atomizer release-promoting layer is in a gel state.

7. A method for preparing the aerosol generating material according to any one of claims 1 to 6, It is characterized in that The steps include: Step 1, uniformly mixing an atomizer, an atomizer release-promoting material and water to obtain a mixed solution of the atomizer and the atomizer release-promoting material; the atomizer release-promoting material is selected from a loose skeleton structure material; Step 2: coating the atomizer and the atomizer release-promoting material mixed solution on the surface of the base paper by a coating machine and drying to form an atomizer release-promoting layer; Step 3: coating the aroma-releasing substance on the upper part of the atomizer release-promoting layer and drying it to form the aroma-releasing layer; the whole material finally obtained is an aerosol generating material.

8. The preparation method according to claim 7, It is characterized in that In step 1, the mass ratio of the atomizer, the atomizer release-promoting material and water is (80-95):(2-30):(1-10).

9. The preparation method according to claim 7, It is characterized in that The total amount of the atomizer release-promoting layer in step 2 is 3-30 g / m 2 , drying temperature is 50-80℃, drying time is 3-20min; The coating amount of the fragrance release layer in step 3 is 3-30g / m 2 , the drying temperature is 50-100℃, and the drying time is 5-20min.

10. Use of the aerosol generating material according to any one of claims 1 to 6 for promoting smoke release.

Citation Information

Patent Citations

  • Preparation method of tobacco raw material for heating cigarettes and heated cigarette product

    CN113040421A

  • Aerosol generating product in hollow form

    CN116584693A

  • Heat-not-burn composite cigarette sheet and composite cigarette

    CN116831310A

  • An improved process for preparing smoking products of the type to be heated and not burnt

    US20220287357A1