Method for recycling waste lithium batteries through double-electrode gradient oxidation
By using a dual-electrode gradient oxidation method to carry out electrochemical reactions in an electrolytic cell, the problems of low recycling efficiency and insufficient utilization of the cathode area in existing lithium battery recycling have been solved, realizing efficient and simplified lithium battery material recycling and electrical energy utilization.
Patent Information
- Application Number
- CN202411273026.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-11
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2044-09-11
AI Technical Summary
Existing lithium battery recycling methods suffer from low recycling efficiency, ineffective utilization of cathode region reactions, complex coating processes, and the inability to utilize reagent oxidizing properties in a gradient manner, resulting in low recycling efficiency.
The dual-electrode gradient oxidation method is adopted. By setting up a cathode and an anode in the electrolytic cell and separating them with a membrane, and combining ionic liquid and catalyst, the anode and cathode are designed in a segmented combination to form a gradient redox pair. The electrochemical reaction is carried out directly in the electrolytic cell, eliminating the coating process, precisely controlling the current and voltage, and improving the charge utilization rate.
It achieves efficient battery material recycling without coating process, improves the recovery rate of elements such as lithium, cobalt, and manganese, improves power utilization efficiency, and simplifies process flow.
Smart Images

Figure CN118943552A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of lithium battery recycling, and in particular to a method for recycling waste lithium batteries by double-electrode gradient oxidation. Background Art
[0002] At present, there are two methods for recycling waste lithium batteries on the market in my country: wet recycling and pyrometallurgical recycling. Among them, pyrometallurgical recycling requires high-temperature reaction (>1400℃), high energy consumption and will cause element loss. Wet recycling uses acid and alkali reagents to dissolve battery materials and adopts corresponding precipitants to separate precious metal elements step by step, but the use of a large number of chemical reagents and cumbersome processes limit large-scale application. In recent years, the electrochemical recycling method has attracted widespread attention for its low reagent consumption and high product purity. Its core reaction is to apply the crushed waste active material to the anode of the electrolytic cell, and use the anodic oxidation reaction to leach lithium ions into the solution. The remaining reactant waste residue is obtained by separation, and finally the lithium ions in the solution are precipitated by the difference in solubility. During the entire chemical reaction process, most of the recovered chemical substances are concentrated near the positive electrode, so it is called a single electrode recovery reaction.
[0003] Generally speaking, there are the following technical problems in recycling waste lithium batteries using the above method:
[0004] There is a lot of room for improvement in recycling efficiency. According to the "Industry Standards for Comprehensive Utilization of Waste Power Batteries for New Energy Vehicles (2019 Edition)" issued by the Ministry of Industry and Information Technology of the People's Republic of China, the comprehensive recycling rate of nickel, cobalt and manganese should not be less than 98%, and the recycling rate of lithium should not be less than 85%. There is still a lot of room for improvement in single-electrode recycling reactions;
[0005] The single-electrode recovery reaction is concentrated in the anode area, and the reaction in the cathode area is not effectively utilized, resulting in power loss.
[0006] The recovered reactants need to be coated on the electrodes, which involves many steps and the recovery efficiency is greatly affected by the coating quality.
[0007] The oxidizing property of the reagent cannot form a gradient, which means that the reaction in the anode area requires a certain threshold voltage and cannot be adjusted at will, so the efficiency of the recovery reaction is not high. Summary of the invention
[0008] Technical issues solved:
[0009] In view of the shortcomings of the prior art, the present invention provides a method for recycling waste lithium batteries through dual-electrode gradient oxidation, which has the advantages of designing solid-liquid contact to recycle battery materials, eliminating the trouble of coating process; designing anode and cathode bipolar technology to improve charge utilization rate, and using ionic liquid to enhance ion activity; further controllable utilization of electrical energy through the design of anode and cathode segmented combination, and further improving the oxidizability of the prepared gradient redox pair with the help of catalysts, thereby solving the problems of the above-mentioned technologies.
[0010] Technical solution:
[0011] To achieve the above object, the present invention provides the following technical solution: a method for recycling waste lithium batteries by dual-electrode gradient oxidation, comprising the following steps:
[0012] Step 1: Place the cathode and anode at both ends of the electrolytic cell, and separate the positive and negative electrodes with a diaphragm in the middle;
[0013] Step 2: Add the mixed ionic liquid solution to the electrolytic cell in an amount of 10%-80% of the volume of the electrolytic cell, blow gas into the cathode at a gas blowing rate of 0.1L / min-5000L / min, apply a voltage of 1.0-200V between the cathode and the anode, and use an electrochemical cation-cation bipolar method to simultaneously prepare an oxidizing redox pair in the electrolytic cell to form a composite oxidation system;
[0014] Step 3: Add catalyst to the prepared electrolytic cell, the amount of catalyst is (0.1-20)*10 of the power consumption. -8 Coulomb, catalytic time is 0.1-10 hours;
[0015] Step 4: Put the waste lithium battery positive electrode material into the above solution. The strong oxidizing property of the composite redox pair in the solution will oxidize the positive electrode material. The lithium ions in the positive electrode material will escape from the bulk phase of the material and enter the ionic liquid. The corresponding positive electrode material will become positive electrode material residue. At the same time, the redox pair will be reduced to the original solute and continue to participate in the redox reaction. The waste positive electrode material residue is obtained by filtration, and the lithium ions are enriched in the ionic liquid.
[0016] Step 5: adding a precipitant to the solution, and filtering to obtain the desired lithium salt by utilizing the difference in solubility;
[0017] In the step 2, the anode and cathode are designed in a segmented combination, and the precise control of the amount of electricity and the gradient preparation of the redox pair are achieved by adjusting the resistance and surface state of each segment. The electrode arrangement in the electrolytic cell adopts a series segmented electrode, a parallel segmented electrode or a series-parallel combination segmented electrode.
[0018] Preferably, the series segmented electrodes in step 2 are multiple electrodes connected in series, and the voltage between the electrodes is controlled by adjusting the type of electrodes and the type of solution between the electrodes, so as to guide the ions with different oxidizing properties in the solution to react simultaneously on the electrodes, thereby achieving gradient oxidation of the solute.
[0019] Preferably, in step 2, the parallel segmented electrodes are first segmented in series at the cathode or anode, and then paired with the counter electrode to form a cation-cation bipolar system, and the voltage of the cation-cation bipolar system composed of each segmented electrode is the same.
[0020] Preferably, in step 2, the series-parallel combination of segmented electrodes simultaneously controls the voltage and charge distribution.
[0021] Preferably, in step 3, the electric charge of 1 mol of electrons is 96500 coulombs, which is converted from coulombs to electric charge of 1 / 1000000, and the amount of catalyst added is 0.1-20% of the electric charge, and the amount used is (0.1-20)*10 -8 .
[0022] Preferably, the ionic liquid solvent in step 2 is acetic acid-3-methylimidazolium hexafluorophosphate; 1-propyl-3-methylimidazolium hexafluorophosphate; boron pentafluoride anthraquinone ionic liquid; ethylammonium nitrate; 1-ethyl-3-methylimidazolium tetrafluoroborate; 1-ethyl-1-methylpiperidinium peracid salt; 1-propyl-1-methylpiperidinium bromide; 1-propyl-1-methylpiperidinium tetrafluoroborate; 1-propyl-1-methylpiperidinium hexafluorophosphate; 1-propyl-1-methylpiperidinium dihydrogen phosphate; 1-ethyl-1-methylpyrrolidinium bromide salt; 1-ethyl-1-methylpyrrolidine methanesulfonate; 1-ethyl-1-methylpyrrolidine p-toluenesulfonate; 1-ethyl-1-methylpyrrolidine bistrifluoromethanesulfonimide salt; 1-propyl-1-methylpyrrolidine hexafluorophosphate; 1-propyl-1-methylpyrrolidine methanesulfonate; N-butyl, methylpyrrolidine peraminate; N-ethyl, methylmorpholine bromide; N-ethyl, methylmorpholine iodide; N-ethyl, methylmorpholine tetrafluoroborate; N-ethyl, methylmorpholine hexafluorophosphate.
[0023] Preferably, the solute in step 2 is one or a mixture of potassium sulfate, sodium sulfate, ammonium sulfate, sulfuric acid, sodium chloride, potassium chloride, ammonium chloride, hydrochloric acid, sodium carbonate, potassium carbonate, ammonium carbonate, potassium perchlorate, sodium perchlorate, ammonium perchlorate, perchloric acid, sulfur trioxide, sulfur dioxide, ammonium persulfate, sodium persulfate, potassium persulfate, ammonium hydrogen sulfate, sodium hydrogen sulfate, and potassium hydrogen sulfate.
[0024] Preferably, the gas in step 2 is one or more of oxygen, nitrogen, carbon dioxide, and argon; the anode material in step 2 is a complex of one or more of the elements Pt, Ti, TiO2, RuO2, IrO2, SnO2, PbO2, graphite, diamond, Pd, Au, B, Ni, Mn, Co, and C3N4; the cathode material is a complex of one or more of the elements Pt, Ti, Ru, Ir, Sn, Pb, C, B, Ni, Mn, and Co.
[0025] Preferably, the catalyst in step 3 is graphene, Fe, Fe 2+ , Fe 3+ , iron oxide, iron sulfide, MgO, MoO3, carbon material, TiO2 one or more; the positive electrode material of the waste lithium battery in the step four is one or more of lithium iron phosphate, lithium manganese phosphate, lithium manganese oxide, lithium manganese iron phosphate, lithium cobalt oxide, lithium vanadium phosphate, lithium vanadium fluorophosphate, and ternary material products.
[0026] Preferably, the precipitant in step 5 is one or more of sodium fluoride, potassium fluoride, ammonium phosphate, ammonium hydrogen phosphate and diammonium phosphate, sodium carbonate, potassium carbonate, ammonium carbonate, ammonium bicarbonate, sodium bicarbonate, potassium bicarbonate, sodium phosphate and potassium phosphate.
[0027] Compared with the prior art, the present invention provides a method for recycling waste lithium batteries by dual-electrode gradient oxidation, which has the following beneficial effects:
[0028] 1. The present invention creates an effective electrochemical reaction environment by arranging a cathode and an anode in an electrolytic cell and using a diaphragm to separate the cathode and the anode, so that the electrode material is in full contact with the electrolyte, and no additional coating process is required to ensure the contact effect. A gradient oxidation and reduction reaction is carried out in the electrolytic cell, and a redox pair with strong oxidizing properties can be generated in the electrolytic cell. The reaction directly acts on the positive electrode material of the waste lithium battery, and no additional coating treatment is required for the material. In step three, the catalyst is directly added to the mixed ionic liquid solution in the electrolytic cell, so that the waste battery material is in direct contact with the solution and converted in the reaction, eliminating the pretreatment steps such as coating, achieving the beneficial effect of designing solid-liquid contact to recover battery materials and eliminating the trouble of the coating process.
[0029] 2. The present invention uses a cathode and an anode in an electrolytic cell and uses a segmented electrode design to accurately control the current and voltage, which can effectively adjust the resistance and surface state of each electrode segment, thereby optimizing the charge distribution and utilization efficiency, ensuring full utilization and efficient reaction of the charge on the electrode. In step 2, a mixed ionic liquid is used as an electrolyte. The ionic liquid has high electrical conductivity and stability, and can effectively enhance the activity of ions in the solution, making the electrolysis reaction process more efficient, thereby improving the redox reaction rate of the battery material. By generating a composite redox pair in the electrolytic cell and using these redox pairs to carry out electrochemical reactions, the utilization rate of the charge is improved. The formation of the composite system enables the reaction to be carried out within a wider voltage and current range, thereby improving the efficiency of the entire system, and achieving the beneficial effects of designing anode and cathode bipolar technology to improve charge utilization and using ionic liquids to enhance ion activity.
[0030] 3. The present invention guides the ions in the solution to undergo gradient oxidation on different electrodes by adjusting the type of electrodes and the voltage between the electrodes, allowing redox pairs of different strengths to be generated on different electrodes, thereby achieving graded control of the use of electric energy and improving the efficiency of electric energy utilization. The composite salt solution used is consistent with the surface state of the electrode, and can achieve gradient control of the redox pairs at low, medium and high oxidizing properties, achieving the beneficial effect of further controllable utilization of electric energy through the segmented combination design of the anode and cathode, and further improving the oxidizing property of the prepared gradient redox pairs with the help of catalysts. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] Figure 1 This is a schematic diagram of the series segmented electrodes of the present invention;
[0032] Figure 2 It is a schematic diagram of the parallel segmented electrodes of the present invention;
[0033] Figure 3 It is a schematic diagram of the hybrid segmented electrode of the present invention. DETAILED DESCRIPTION
[0034] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0035] See also Figure 1-3 , a method for recycling waste lithium batteries by dual-electrode gradient oxidation, comprising the following steps:
[0036] Step 1: Place the cathode and anode at both ends of the electrolytic cell, and separate the positive and negative electrodes with a diaphragm in the middle;
[0037] Step 2: Add the mixed ionic liquid solution to the electrolytic cell in an amount of 10%-80% of the volume of the electrolytic cell, blow gas into the cathode at a gas blowing rate of 0.1L / min-5000L / min, apply a voltage of 1.0-200V between the cathode and the anode, and use an electrochemical cation-cation bipolar method to simultaneously prepare an oxidizing redox pair in the electrolytic cell to form a composite oxidation system;
[0038] Step 3: Add catalyst to the prepared electrolytic cell. The amount of catalyst is (0.1-20)*10 of the power consumption. -8 Coulomb, catalytic time is 0.1-10 hours;
[0039] Step 4: Put the waste lithium battery positive electrode material into the above solution. The strong oxidizing property of the composite redox pair in the solution will oxidize the positive electrode material. The lithium ions in the positive electrode material will escape from the bulk phase of the material and enter the ionic liquid. The corresponding positive electrode material will become positive electrode material residue. At the same time, the redox pair will be reduced to the original solute and continue to participate in the redox reaction. The waste positive electrode material residue is obtained by filtration, and the lithium ions are enriched in the ionic liquid.
[0040] Step 5: adding a precipitant to the solution, and filtering to obtain the desired lithium salt by utilizing the difference in solubility;
[0041] In step 2, the anode and cathode adopt a segmented combination design, and the precise control of the amount of electricity and the gradient preparation of the redox pairs are achieved by adjusting the resistance and surface state of each segment. The electrode arrangement in the electrolytic cell adopts a series segmented electrode, a parallel segmented electrode or a series-parallel combination segmented electrode.
[0042] Specifically, in step 2, the series segmented electrodes are multiple electrodes connected in series, and the voltage between the electrodes is controlled by adjusting the type of electrodes and the type of solution between the electrodes, so as to guide the ions with different oxidizing properties in the solution to react on the electrodes at the same time, thereby achieving gradient oxidation of the solute.
[0043] The use of ionic liquids as electrolytes enhances the activity of the ions therein and improves the conversion efficiency of electrical energy into chemical energy (redox pairs).
[0044] The use of anode-cathode bipolar technology to prepare redox pairs not only prepares redox pairs at the anode, but also produces the same effect at the cathode, thereby improving the utilization rate of electrical energy.
[0045] The anode and cathode are designed as a segmented combination, and the reaction at the electrode-solution interface is precisely controlled by adjusting the resistance and surface state of each segment, while the surface charge density is more reasonably distributed.
[0046] The composite salt solution used is compatible with the surface state of the electrode, and can achieve gradient control of the redox pair at low, medium and high oxidizability.
[0047] The catalyst added to the electrolytic cell utilizes its highly efficient catalytic reaction to further catalyze the composite redox pair into oxidizing substances with stronger oxidizing properties and larger quantities.
[0048] Bipolar electrode structure: cathode and anode are used in the electrolytic cell, and the current and voltage are precisely controlled through segmented electrode design (including series, parallel and series-parallel combination segmented electrodes). This design can effectively adjust the resistance and surface state of each segment of the electrode, thereby optimizing the charge distribution and utilization efficiency, ensuring full utilization of the charge on the electrode and efficient reaction.
[0049] Improved charge utilization: Through this precisely controlled electrode layout, a gradient distribution of charge and gradient preparation of redox pairs are achieved, thereby improving charge utilization. This means that the charges in the electrolyzer can participate in the reaction more evenly, improving the overall reaction efficiency and the recovery rate of battery materials.
[0050] Advantages of ionic liquids: In step 2, a mixed ionic liquid is used as the electrolyte. Ionic liquids have high electrical conductivity and stability, and can effectively enhance the activity of ions in the solution. This high ion activity makes the electrolysis process more efficient, thereby increasing the redox reaction rate of the battery material.
[0051] Enhanced ion activity: The ions in ionic liquids are highly active, which helps to improve the ion migration rate and reaction efficiency during the electrolysis process. By optimizing the selection of ionic liquids (such as using acetic acid-3-methylimidazolium hexafluorophosphate, etc.), the charge utilization effect and reaction efficiency can be further improved.
[0052] Gas bubbling: In step 2, the gas bubbling technology (such as oxygen, nitrogen, etc.) at the cathode further improves the mixing efficiency of the electrolyte and the reaction rate of the electrode. The gas bubbling helps to fully contact the gas-liquid phase and transfer ions, enhances the utilization of charge and the uniformity of the reaction.
[0053] Specifically, in step 2, the parallel segmented electrodes are first connected in series at the cathode or anode segments, and then paired with the counter electrode to form a cation-cation bipolar system, and the voltage of the cation-cation bipolar system composed of each segmented electrode is the same.
[0054] Specifically, in step 2, the series-parallel combination of segmented electrodes simultaneously controls the voltage and charge distribution.
[0055] Specifically, in step 3, the charge of 1 mol of electrons is 96500 coulombs, which is converted from coulombs to charge of 1 / 1000000. The amount of catalyst added is 0.1-20% of the charge, and the amount used is (0.1-20)*10 -8 .
[0056] Specifically, the ionic liquid solvent in step 2 is acetic acid-3-methylimidazolium hexafluorophosphate; 1-propyl-3-methylimidazolium hexafluorophosphate; boron pentafluoride anthraquinone ionic liquid; ethylammonium nitrate; 1-ethyl-3-methylimidazolium tetrafluoroborate; 1-ethyl-1-methylpiperidinium peracid salt; 1-propyl-1-methylpiperidinium bromide; 1-propyl-1-methylpiperidinium tetrafluoroborate; 1-propyl-1-methylpiperidinium hexafluorophosphate; 1-propyl-1-methylpiperidinium dihydrogen phosphate; 1-ethyl-1-methylpyrrolidinium bromide ; 1-ethyl-1-methylpyrrolidine methanesulfonate; 1-ethyl-1-methylpyrrolidine p-toluenesulfonate; 1-ethyl-1-methylpyrrolidine bistrifluoromethanesulfonimide; 1-propyl-1-methylpyrrolidine hexafluorophosphate; 1-propyl-1-methylpyrrolidine methanesulfonate; N-butyl, methylpyrrolidine peramate; N-ethyl, methylmorpholine bromide; N-ethyl, methylmorpholine iodide; N-ethyl, methylmorpholine tetrafluoroborate; N-ethyl, methylmorpholine hexafluorophosphate.
[0057] Specifically, the solute in step 2 is one or a mixture of potassium sulfate, sodium sulfate, ammonium sulfate, sulfuric acid, sodium chloride, potassium chloride, ammonium chloride, hydrochloric acid, sodium carbonate, potassium carbonate, ammonium carbonate, potassium perchlorate, sodium perchlorate, ammonium perchlorate, perchloric acid, sulfur trioxide, sulfur dioxide, ammonium persulfate, sodium persulfate, potassium persulfate, ammonium hydrogen sulfate, sodium hydrogen sulfate, and potassium hydrogen sulfate.
[0058] Specifically, the gas in step 2 is one or more of oxygen, nitrogen, carbon dioxide, and argon; the anode material in step 2 is a complex of one or more of the elements selected from the group consisting of Pt, Ti, TiO2, RuO2, IrO2, SnO2, PbO2, graphite, diamond, Pd, Au, B, Ni, Mn, Co, and C3N4; and the cathode material is a complex of one or more of the elements selected from the group consisting of Pt, Ti, Ru, Ir, Sn, Pb, C, B, Ni, Mn, and Co.
[0059] Specifically, the catalyst in step 3 is graphene, Fe, Fe 2+ , Fe 3+ , iron oxide, iron sulfide, MgO, MoO3, carbon material, TiO2 one or more; the positive electrode material of the waste lithium battery in the step four is one or more of lithium iron phosphate, lithium manganese phosphate, lithium manganese oxide, lithium manganese iron phosphate, lithium cobalt oxide, lithium vanadium phosphate, lithium vanadium fluorophosphate, and ternary material products.
[0060] Specifically, the precipitant in step five is one or more of sodium fluoride, potassium fluoride, ammonium phosphate, ammonium hydrogen phosphate and diammonium phosphate, sodium carbonate, potassium carbonate, ammonium carbonate, ammonium bicarbonate, sodium bicarbonate, potassium bicarbonate, sodium phosphate, and potassium phosphate.
[0061] Example 1
[0062] like Figure 1 As shown, the series segmented electrode design utilizes multiple electrodes in series. By adjusting the type of electrodes, the type of solution between the electrodes, and the voltage between the electrodes, the ions with different oxidizing properties in the solution are guided to react simultaneously on the electrodes, thereby achieving gradient oxidation of the solute. The redox pair generation rate is increased by 120%, and the electrical energy-chemical energy conversion efficiency is increased to 91%.
[0063] Example 2
[0064] like Figure 2 As shown, the parallel segmented electrodes are first connected in series at the cathode or anode, and then paired with the counter electrode to form a cation-cation bipolar system. The voltage of the cation-cation bipolar system composed of each segmented electrode is the same, but the amount of electricity is different. Therefore, by controlling the amount of electricity, the absorption and catalysis of the electrode surface can be specifically adjusted. Experiments have shown that the parallel segmented electrode redox pair generation rate has increased by 140%, and the electrical energy-chemical energy conversion efficiency has increased to 93.2%.
[0065] Example 3
[0066] like Figure 3 As shown, the series-parallel combination of segmented electrodes simultaneously controls the voltage and charge distribution, more accurately controls the reaction on the electrode surface, increases the redox pair generation rate by 162%, and increases the electrical energy-chemical energy conversion efficiency to 96.7%.
[0067] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and alterations may be made to the embodiments without departing from the principles and spirit of the invention, the scope of which is defined by the appended claims and their equivalents.
Claims
1. A method for recycling waste lithium batteries by dual-electrode gradient oxidation, characterized in that: The following steps are involved: Step 1: Place the cathode and anode at both ends of the electrolytic cell, and separate the positive and negative electrodes with a diaphragm in the middle; Step 2: Add the mixed ionic liquid solution to the electrolytic cell in an amount of 10%-80% of the volume of the electrolytic cell, blow gas into the cathode at a gas blowing rate of 0.1L / min-5000L / min, apply a voltage of 1.0-200V between the cathode and the anode, and use an electrochemical cation-cation bipolar method to simultaneously prepare an oxidizing redox pair in the electrolytic cell to form a composite oxidation system; Step 3: Add a catalyst to the prepared electrolytic cell. The amount of the catalyst is (0.1-20)*10 of the power consumption. -8 , the catalytic time is 0.1-10 hours; Step 4: Put the waste lithium battery positive electrode material into the above solution. The strong oxidizing property of the composite redox pair in the solution will oxidize the positive electrode material. The lithium ions in the positive electrode material will escape from the bulk phase of the material and enter the ionic liquid. The corresponding positive electrode material will become positive electrode material residue. At the same time, the redox pair will be reduced to the original solute and continue to participate in the redox reaction. The waste positive electrode material residue is obtained by filtration, and the lithium ions are enriched in the ionic liquid. Step 5: adding a precipitant to the solution, and filtering to obtain the desired lithium salt by utilizing the difference in solubility; In the step 2, the anode and cathode are designed in a segmented combination, and the precise control of the amount of electricity and the gradient preparation of the redox pair are achieved by adjusting the resistance and surface state of each segment. The electrode arrangement in the electrolytic cell adopts a series segmented electrode, a parallel segmented electrode or a series-parallel combination segmented electrode. The unit of the power consumption in step 3 is coulomb.
2. The method for recycling waste lithium batteries by dual-electrode gradient oxidation according to claim 1, characterized in that: In the step 2, the series segmented electrodes are multiple electrodes connected in series. By adjusting the type of electrodes and the type of solution between the electrodes, the voltage between the electrodes is controlled, and the ions with different oxidizing properties in the solution are guided to react on the electrodes simultaneously, so as to achieve gradient oxidation of the solute.
3. The method for recycling waste lithium batteries by dual-electrode gradient oxidation according to claim 1, characterized in that: In the step 2, the parallel segmented electrodes are first connected in series at the cathode or anode segments, and then paired with the counter electrode to form a cation-cation bipolar system, and the voltage of the cation-cation bipolar system composed of each segmented electrode is the same.
4. The method for recycling waste lithium batteries by dual-electrode gradient oxidation according to claim 1, characterized in that: In step 2, the series-parallel combination of segmented electrodes simultaneously controls the voltage and charge distribution.
5. A method for recycling waste lithium batteries by dual-electrode gradient oxidation according to claim 2, 3 or 4, characterized in that: In the step 3, the electric charge of 1 mol of electrons is 96500 coulombs, which is converted from coulombs to electric charge of 1 / 1000000. The amount of the substance added as the catalyst is 0.1-20% of the electric charge, and the dosage is (0.1-20)*10 -8 .
6. The method for recycling waste lithium batteries by dual-electrode gradient oxidation according to claim 1, characterized in that: The ionic liquid solvent in step 2 is acetic acid-3-methylimidazolium hexafluorophosphate; 1-propyl-3-methylimidazolium hexafluorophosphate; boron pentafluoride anthraquinone ionic liquid; ethylammonium nitrate; 1-ethyl-3-methylimidazolium tetrafluoroborate; 1-ethyl-1-methylpiperidinium peracid salt; 1-propyl-1-methylpiperidinium bromide; 1-propyl-1-methylpiperidinium tetrafluoroborate; 1-propyl-1-methylpiperidinium hexafluorophosphate; 1-propyl-1-methylpiperidinium dihydrogen phosphate; 1-ethyl-1-methylpyrrolidinium bromide; The invention is prepared by mixing one or more of 1-ethyl-1-methylpyrrolidine methanesulfonate; 1-ethyl-1-methylpyrrolidine p-toluenesulfonate; 1-ethyl-1-methylpyrrolidine bistrifluoromethanesulfonimide; 1-propyl-1-methylpyrrolidine hexafluorophosphate; 1-propyl-1-methylpyrrolidine methanesulfonate; N-butyl, methylpyrrolidine peramine salt; N-ethyl, methylmorpholine bromide; N-ethyl, methylmorpholine iodide; N-ethyl, methylmorpholine tetrafluoroborate; and N-ethyl, methylmorpholine hexafluorophosphate.
7. The method for recycling waste lithium batteries by dual-electrode gradient oxidation according to claim 1, characterized in that: In the step 2, the solute is one of potassium sulfate, sodium sulfate, ammonium sulfate, sulfuric acid, sodium chloride, potassium chloride, ammonium chloride, hydrochloric acid, sodium carbonate, potassium carbonate, ammonium carbonate, potassium perchlorate, sodium perchlorate, ammonium perchlorate, perchloric acid, sulfur trioxide, sulfur dioxide, ammonium persulfate, sodium persulfate, potassium persulfate, ammonium hydrogen sulfate, sodium hydrogen sulfate, and potassium hydrogen sulfate, or a mixture of several of them.
8. The method for recycling waste lithium batteries by dual-electrode gradient oxidation according to claim 1, characterized in that: The gas in step 2 is one or more of oxygen, nitrogen, carbon dioxide, and argon; the anode material in step 2 is a composite of one or more of Pt, Ti, TiO2, RuO2, IrO2, SnO2, PbO2, graphite, diamond, Pd, Au, B, Ni, Mn, Co, and C3N4; the cathode material is a composite of one or more of Pt, Ti, Ru, Ir, Sn, Pb, C, B, Ni, Mn, and Co.
9. The method for recycling waste lithium batteries by dual-electrode gradient oxidation according to claim 1, characterized in that: The catalyst in step 3 is graphene, Fe, Fe 2+ , Fe 3+ , iron oxide, iron sulfide, MgO, MoO3, carbon material, TiO2 one or more; the positive electrode material of the waste lithium battery in the step four is one or more of lithium iron phosphate, lithium manganese phosphate, lithium manganese oxide, lithium manganese iron phosphate, lithium cobalt oxide, lithium vanadium phosphate, lithium vanadium fluorophosphate, and ternary material products.
10. The method for recycling waste lithium batteries by dual-electrode gradient oxidation according to claim 1, characterized in that: In the step 5, the precipitating agent is one or more of sodium fluoride, potassium fluoride, ammonium phosphate, ammonium hydrogen phosphate and diammonium phosphate, sodium carbonate, potassium carbonate, ammonium carbonate, ammonium bicarbonate, sodium bicarbonate, potassium bicarbonate, sodium phosphate and potassium phosphate.
Citation Information
Patent Citations
Electrochemical recovery method of lithium in cathode materials of waste lithium batteries
CN106823816A
Method for synchronously recovering valuable metal from cathode and anode of waste ternary lithium battery
CN116790885A
A lithium ion battery materials recycling method
US20210391605A1